A pipe tobacco cartridge and its preparation method

By preparing tobacco cartridges with a porosity gradient structure that is tight at the top and loose at the bottom, and combining low-temperature extraction and cross-wrinkling technology, the problems of cumbersome operation and inconsistent experience of traditional pipes have been solved, achieving a convenient and standardized tobacco smoking experience and efficient production.

CN123100883APending Publication Date: 2026-11-17HUBEI CHINA TOBACCO INDUSTRY CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202611615622.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-19
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Traditional heated pipe smoking methods suffer from cumbersome operation, inconsistent user experience, and high technical barriers, making it difficult to achieve convenient and standardized usage.

Method used

The cigarette cartridges are made from frustum-shaped tobacco sheets with a spatial mesh-like porous structure. They have an internal porosity gradient structure that is tighter at the top and looser at the bottom. Combined with low-temperature extraction and cross-wrinkling technology, they form a stable airflow channel. The continuous integrated production process of upper and lower V-shaped rolling wheels and dual-station gradient rolling is adopted.

Benefits of technology

It achieves a convenient and standardized user experience, high draw resistance stability, high volatile oil retention rate, excellent sensory quality, and improved production efficiency, solving the problems of draw resistance fluctuation and uneven combustion caused by uneven filling of traditional pipes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123100883A_ABST
    Figure CN123100883A_ABST
Patent Text Reader

Abstract

This invention discloses a pipe tobacco cartridge and its preparation method. The cartridge is a frustum with a spatial mesh-like porous structure, rolled from tobacco sheets. Its interior has a porosity gradient structure with a tighter upper section and a looser lower section; the upper porosity is 35%-45%, and the lower porosity is 55%-65%. The cartridge is a one-piece molded structure. This invention, employing a tighter upper section and a looser lower section porosity gradient structure and an integrated manufacturing process, systematically solves the core pain points of traditional pipe tobacco use, achieving a synergistic improvement in convenience, stability, sensory experience, and production efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This patent belongs to the field of tobacco product technology, specifically relating to a tobacco cartridge for pipe cigarettes and its preparation method. Background Technology

[0002] As a traditional tobacco smoking tool, the core of the pipe smoking experience lies in the burning of pipe tobacco (usually a specific blend of shredded and conditioned tobacco) in the pipe bowl, allowing the smoke to be inhaled through the stem and mouthpiece. This method of smoking is highly regarded by many enthusiasts because it fully showcases the complex aroma of tobacco and provides a slow, focused sensory experience. The domestic pipe market is experiencing rapid growth, with an average annual compound growth rate of approximately 7.3%. By the end of 2024, the pipe market had reached a size of 16 billion yuan. The current pipe market includes traditional heated pipes and newer heat-not-burn pipes; traditional heated pipes offer an irreplaceable smoking experience.

[0003] However, the smoking method of traditional heated pipes differs from that of traditional cigarettes. It requires a certain level of skill, primarily in the packing technique. If the packing is too tight, it increases the draw resistance, leading to uneven burning and a tendency for the pipe to go out. If the packing is too loose, the pipe will burn too quickly, causing overheating and flavor loss. Neglecting the bottom of the pipe can leave gaps, resulting in a "well" (burning through the center). Mastering this packing technique is challenging, causing many new pipe smokers to give up on pipe smoking altogether.

[0004] Each use requires tedious steps such as weighing, filling, ignition, and pressing, which is time-consuming and does not meet the convenience requirements of modern consumption scenarios. More importantly, due to the non-standardization of the raw material (tobacco) form and filling process, the performance (such as draw resistance and burning rate) and sensory quality of the final product vary greatly from batch to batch and from individual to individual, making it impossible to provide a highly consistent and predictable product experience like cigarettes or e-cigarettes.

[0005] In summary, existing technologies rely on manual filling of pipe tobacco, which suffers from core drawbacks such as inconsistent user experience, cumbersome operation, and high technical barriers. Therefore, there is an urgent need for a new type of pipe tobacco product and its preparation method that can retain the excellent sensory experience of traditional pipe tobacco, provide a convenient and standardized way of use, and be produced with high quality and stability through industrial methods. Summary of the Invention

[0006] To solve the above-mentioned technical problems, this patent provides the following technical solution: In the first aspect, a pipe tobacco cartridge is provided. The cartridge is a truncated cone with a spatial mesh porous structure, which is rolled from tobacco sheets. Its interior has a porosity gradient structure with a tight upper part and a loose lower part. The porosity of the upper part is 35%-45%, and the porosity of the lower part is 55%-65%. The cartridge is a one-piece molded structure.

[0007] Furthermore, the tobacco sheet includes transverse pleats and inclined pleats at 45° to the transverse pleats, with a pleat height of 0.1-0.3 mm and a spacing of 0.5-1 mm.

[0008] Furthermore, the diameter of the e-cigarette cartridge is 10-15mm, and the length is 20-30mm.

[0009] Furthermore, the coefficient of variation of the draw resistance of the cartridge is ≤5%, and the draw resistance under standard vaping conditions is in the range of 950~1050Pa.

[0010] In a second aspect, a method for preparing pipe tobacco cartridges according to the first aspect is provided, comprising the following steps: S1. Raw material pretreatment: The compound tobacco raw materials are crushed and extracted at low temperature to separate the flavor extract and the fiber matrix. The fiber matrix is ​​then decomposed and set aside. S2. Slurry preparation: Add water to the fiber matrix obtained in step S1 to prepare slurry, add auxiliary materials and add back some flavor extract, and stir evenly. S3. Shaping and Dehydration: The slurry is formed into wet sheets and then dehydrated; S4. Cross wrinkling: After drying the dehydrated sheet, cross wrinkling and 45° inclined wrinkling are performed to form a grid of wrinkles. S5. Positioning and pre-processing of upper and lower V-shaped rollers: The thin sheet after cross-wrinkling is pre-processed by positioning through a symmetrical upper and lower V-shaped roller assembly. S6. Dual-station gradient winding: The pre-treated sheet is wound around a tapered winding needle at a certain angle for gradient pressure winding to form a continuous blank. S7. Center Cut: Cut the conjoined blank along the center to obtain two separate cartridges; S8. Post-processing: The cut e-cigarette cartridges are balanced and tested to obtain the finished product.

[0011] Furthermore, in step S4, the conditions for transverse wrinkling are: the scraper and the sheet running direction are at 90°, the pressure is 0.2-0.3MPa, and the difference between the traction speed and the sheet running speed is 15%-20%; the conditions for 45° inclined wrinkling are: the scraper and the sheet running direction are at 40°-50°, the pressure is 0.15-0.25MPa, and the speed difference is 20%-25%.

[0012] Furthermore, in step S6, the gradient pressure rolling specifically involves applying a pressure of 0.7-0.9 MPa when rolling the outer layer and applying a pressure of 0.2-0.4 MPa when rolling the inner layer, thereby forming a density gradient that is tighter at the top and looser at the bottom.

[0013] Furthermore, in step S5, the upper and lower V-shaped roller assemblies are made of silicone with a hardness of 65-75 Shore A and a 2-3mm protrusion in the middle; the upper roller applies a pressure of 0.1-0.15MPa to flatten the upper surface of the sheet, and the lower roller applies a pressure of 0.08-0.12MPa to retain the wrinkles on the lower surface of the sheet.

[0014] Furthermore, in step S8, the conditions for equilibration are a temperature of 25°C, a relative humidity of 60%, and an equilibration time of 48 hours.

[0015] Furthermore, in step S8, the testing standards include: upper porosity 35%-45%, lower porosity 55%-65%, absorption resistance coefficient of variation ≤5%, compressive strength ≥0.5MPa, burning rate 2.5-4.5mm / min, and volatile oil retention rate ≥85%.

[0016] The beneficial effects of this patent include: The cartridges are a one-piece molded structure that is ready to use, eliminating the tedious and experience-dependent manual filling process of traditional pipe smoking, shortening the filling time, lowering the threshold for use, and providing consumers with a highly consistent and predictable standardized product.

[0017] The pipe tobacco cartridge of this invention features a unique gradient porosity structure with a tighter top and looser bottom, simulating an ideal hand-filled state. Combined with a stable spatial mesh porous structure formed by cross-wrinkling, it ensures unobstructed and uniformly distributed airflow channels. This allows the product's draw resistance to be precisely controlled within a suitable range, with a small coefficient of variation, solving problems such as large draw resistance fluctuations, uneven combustion (e.g., slanted burning, uneven combustion), and easy flameout caused by uneven filling in traditional methods.

[0018] The pipe tobacco cartridge of this invention employs a low-temperature extraction process combined with the refilling of flavor extract, achieving a high volatile oil retention rate and effectively preserving the original aroma of tobacco. The stable pore structure and combustion rate allow for the full and uniform release of aroma-producing substances. Sensory evaluation results indicate that its aroma richness, smoke smoothness, and overall comfort are comparable to or even superior to high-quality traditional pipe tobacco.

[0019] This invention employs a continuous integrated process combining upper and lower V-shaped roller positioning with dual-station gradient rolling and centered cutting, achieving efficient and continuous production from thin sheets to finished e-cigarette cartridges, significantly improving production capacity and processing efficiency. Attached Figure Description

[0020] The above content of this patent and the following detailed embodiments will be better understood when read in conjunction with the accompanying drawings. It should be noted that the drawings are merely examples of the claimed technical solution.

[0021] Figure 1 This is a flowchart illustrating a method for preparing pipe tobacco cartridges according to an embodiment of the present invention; Figure 2 A schematic diagram of a pipe tobacco cartridge according to one embodiment of the present invention. Detailed Implementation

[0022] The detailed features and advantages of this application are described below in the specific embodiments. The content of this description is sufficient to enable any person skilled in the art to understand the technical content of this application and implement it accordingly. Based on the specification, claims and drawings disclosed in this specification, a person skilled in the art can easily understand the related objectives and advantages of this application.

[0023] In this specification and claims, several terms will be used, and unless otherwise indicated, these terms will be defined to have the following meanings: All figures used to represent component amounts, properties (e.g., weight-average molecular weight), reaction conditions, etc., should be considered to be modified in all cases by the terms "within the unavoidable margin of error" or "approximately". Therefore, the numerical values ​​presented herein are approximate and may vary depending on the desired properties sought to be obtained by this patent. The principle of equivalents, which is applied to a minimum and not intended to limit the scope of the claims, should be applied, for example, each value should be interpreted at least according to the reported significant digits and by applying conventional rounding techniques.

[0024] All other terms used herein for special definition are intended to have the general meaning understood by one of ordinary skill in the art, and in particular, meaning that one of ordinary skill in the art, upon reading the claims, specification and drawings of this patent, can directly and without doubt determine how the technical solution of this patent can be implemented.

[0025] Even if there are incomplete descriptions, omissions, or ambiguities in the grammar, words, punctuation, graphics, symbols, etc. of the claims, specification, and drawings of this patent, a person skilled in the art can still arrive at the only correct understanding by reading the claims, specification, and drawings as a whole without extensive reasoning or experimentation, and effectively exclude various incorrect interpretations that are not aimed at achieving the purpose of this patent.

[0026] The "range" disclosed herein is defined by a lower limit and an upper limit. A given range is defined by selecting a lower limit and an upper limit, which define the boundaries of a particular range. Ranges defined in this way can include or exclude endpoints and can be arbitrarily combined; that is, any lower limit can be combined with any upper limit to form a range. For example, if ranges of 60-120 and 80-110 are listed for a specific parameter, it is expected that ranges of 60-110 and 80-120 are also expected. Furthermore, if minimum range values ​​of 1 and 2 are listed, and if maximum range values ​​of 3, 4, and 5 are listed, then the following ranges are all expected: 1-3, 1-4, 1-5, 2-3, 2-4, and 2-5. In this application, unless otherwise stated, the numerical range "ab" represents a shortened representation of any combination of real numbers between a and b, where a and b are real numbers. For example, the numerical range "0-5" indicates that all real numbers between "0-5" have been listed in this article; "0-5" is simply a shortened representation of these numerical combinations. Furthermore, when a parameter is stated as an integer ≥2, it is equivalent to disclosing that the parameter is, for example, an integer such as 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, etc.

[0027] Unless otherwise specified, all embodiments and preferred embodiments mentioned herein can be combined to form new technical solutions.

[0028] Unless otherwise specified, all the technical features and preferred features mentioned herein can be combined to form new technical solutions.

[0029] Unless otherwise specified, all steps mentioned herein may be performed sequentially or randomly, but are preferably performed sequentially. For example, the method includes steps (a) and (b), indicating that the method may include steps (a) and (b) performed sequentially, or it may include steps (b) and (a) performed sequentially. For example, the mention that the method may also include step (c) indicates that step (c) may be added to the method in any order; for example, the method may include steps (a), (b), and (c), or it may include steps (a), (c), and (b), or it may include steps (c), (a), and (b), etc.

[0030] Unless otherwise specified, the terms "comprising" and "including" as used herein can be open-ended or closed-ended. For example, "comprising" and "including" may mean that other components not listed may also be included, or that only the listed components may be included.

[0031] In the description of this article, it should be noted that, unless otherwise stated, "above" and "below" include the number itself, and "several" in "one or more" means two or more.

[0032] In this description, unless otherwise stated, the term "or" is inclusive. For example, the phrase "A or B" means "A, B, or both A and B". More specifically, the condition "A or B" is satisfied by any of the following conditions: A is true (or exists) and B is false (or does not exist); A is false (or does not exist) and B is true (or exists); or both A and B are true (or exist).

[0033] Unless otherwise specified, percentages (%) in this document refer to percentages by mass relative to the composition.

[0034] Unless otherwise stated herein, the sum of the contents of the components in the composition is 100%.

[0035] In this document, unless otherwise stated, “combination of” means a multi-component mixture of the elements, such as two, three, four, and up to the maximum possible multi-component mixture.

[0036] Unless otherwise specified, the term "a" as used in this specification means "at least one".

[0037] The terms "first" and "second" are used for descriptive purposes only and should not be construed as indicating or implying relative importance or implicitly specifying the number of technical features indicated. Thus, a feature defined as "first" or "second" may explicitly or implicitly include at least one of that feature. In the description of this invention, "a plurality of" means at least two, such as two, three, etc., unless otherwise explicitly specified.

[0038] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention pertains. The terminology used herein in the description of the invention is for the purpose of describing particular embodiments only and is not intended to be limiting of the invention.

[0039] To make the objectives, technical solutions, and advantages of the present invention clearer, the embodiments of the present invention will be further described in detail below with reference to the accompanying drawings. Unless otherwise specified, the experimental methods described in the embodiments of the present invention are conventional methods, and the materials and reagents used in the following embodiments are commercially available unless otherwise specified.

[0040] The purpose of this invention is to provide a pipe tobacco cartridge, which is a truncated cone with a spatial mesh porous structure, made by rolling tobacco sheets. Its interior has a porosity gradient structure with a tight upper part and a loose lower part. The porosity of the upper part is 35%-45%, and the porosity of the lower part is 55%-65%. The tobacco cartridge is a one-piece molded structure.

[0041] Pipe tobacco, specifically designed for pipe smoking, is a type of tobacco product made from various tobacco leaves (such as flue-cured, burley, and aromatic tobacco) that have been shredded, moistened, and flavored. It is typically in the form of loose, moist shreds or flakes. When used, the smoker must manually layer the tobacco into the bowl of the pipe, employing techniques such as the "three-layer method" to achieve an ideal "tight on top, loose on the bottom" structure. This aims to provide a stable, slow-burning experience with rich flavor profiles after lighting. The core of this traditional method lies in manually controlling the tightness and evenness of the packing to regulate airflow and combustion. However, its effectiveness is highly dependent on individual skill and suffers from inherent technical challenges such as tedious packing, large fluctuations in draw resistance, uneven combustion, and a tendency to extinguish.

[0042] As used in this article, "one-piece molding" means that the tobacco cartridge is a complete, independent component that is processed in one step through physical and chemical methods. Its internal structure is fixed during molding, and it can be directly inserted into the pipe without the user having to fill it with other tobacco materials (such as traditional pipe tobacco).

[0043] As used herein, "sheet rolling" refers to the process by which a sheet-like substrate (such as "paper-reconstituted tobacco sheet") is rolled into a truncated cone. This differs from powder pressing or the direct use of tobacco fiber tows. In this invention, the truncated cone is wider at the top and narrower at the bottom, meaning the cross-sectional area of ​​the upper part is larger than that of the lower part.

[0044] As used in this article, "spatial mesh porous structure" refers to the fact that the interior of the e-cigarette cartridge is not solid, but a three-dimensional network composed of interconnected holes and pores. This structure is not a simple, disordered accumulation of pores, but a three-dimensional porous system with a certain degree of regularity and connectivity formed by specific processes (such as cross-wrinkling) to ensure the stability and uniformity of the airflow channels.

[0045] As used in this article, "porosity gradient structure" refers to the fact that the porosity (the percentage of pore volume to total volume) inside the cartridge changes continuously or in layers from one end to the other (usually from top to bottom), rather than being uniform.

[0046] As used herein, "tight at the top and loose at the bottom" is a specific description of the porosity gradient structure. In this invention, it specifically refers to the following: the upper part of the tobacco cartridge (i.e., the end closer to the ignition point during use) has lower porosity and a denser structure; the lower part (i.e., the end closer to the flue during use) has higher porosity and a looser structure. This design aims to simulate the best practice of "tight at the top and loose at the bottom" when traditional pipe tobacco is manually packed to control the combustion rate and airflow.

[0047] As used in this article, "upper porosity / lower porosity" refers to the average porosity values ​​of the upper and lower sections of the cartridge, respectively. The division between the upper and lower sections is generally based on the volume average.

[0048] In some embodiments, the tobacco sheet includes transverse pleats and inclined pleats at a 45° angle to the transverse pleats, with a pleat height of 0.1-0.3 mm and a spacing of 0.5-1 mm. Pleat height refers to the vertical distance from the apex to the trough of the pleat protrusion formed on the sheet surface during the cross-creaming process. Pleat spacing refers to the average distance between two adjacent parallel pleat ridges.

[0049] In some implementations, the cartridge has a diameter of 10-15 mm and a length of 20-30 mm. The diameter of the cartridge is the average diameter of the cross-section of the frustum, and the length refers to the height of the frustum.

[0050] In some implementations, the coefficient of variation of the draw resistance of the cartridge is ≤5%, and the draw resistance under standard vaping conditions is in the range of 950~1050 Pa.

[0051] As used in this article, the coefficient of variation of draw resistance is a statistical indicator that measures the stability of the draw resistance of a tobacco cartridge. The calculation formula is: (standard deviation of draw resistance / average draw resistance) × 100%. "≤5%" indicates a high degree of consistency in draw resistance across different parts of a batch or a single cartridge, a key indicator of superior product performance. Standard vaping conditions refer to the conditions under which testing is conducted in a laboratory environment using specified, simulated human vaping patterns (such as vaping volume, duration, frequency, etc.). Draw resistance values ​​are measured under these conditions.

[0052] The purpose of this invention is to provide a method for preparing pipe tobacco cartridges, comprising the following steps: S1. Raw material pretreatment: The compound tobacco raw materials are crushed and extracted at low temperature to separate the flavor extract and the fiber matrix. The fiber matrix is ​​then decomposed and set aside. S2. Slurry preparation: Add water to the fiber matrix obtained in step S1 to prepare slurry, add auxiliary materials and add back some flavor extract, and stir evenly. S3. Shaping and Dehydration: The slurry is formed into wet sheets and then dehydrated; S4. Cross wrinkling: After drying the dehydrated sheet, cross wrinkling and 45° inclined wrinkling are performed to form a grid of wrinkles. S5. Positioning and pre-processing of upper and lower V-shaped rollers: The thin sheet after cross-wrinkling is pre-processed by positioning through a symmetrical upper and lower V-shaped roller assembly. S6. Dual-station gradient winding: The pre-treated sheet is wound around a tapered winding needle at a certain angle for gradient pressure winding to form a continuous blank. S7. Center Cut: Cut the conjoined blank along the center to obtain two separate cartridges; S8. Post-processing: The cut e-cigarette cartridges are balanced and tested to obtain the finished product.

[0053] As used in this article, "blended tobacco raw materials" refers to raw materials made by mixing two or more different types (such as flue-cured tobacco, burley tobacco, aromatic tobacco, etc.) or tobacco from different origins in a certain proportion, with the aim of obtaining specific flavor characteristics.

[0054] As used in this article, "low-temperature extraction" refers to the extraction of broken tobacco raw materials by soaking them in water or other solvents at a relatively low temperature (e.g., 40-60°C). The aim is to maximize the extraction and retention of volatile aroma components in the tobacco, while minimizing the formation of undesirable flavor compounds or aroma loss that may result from high temperatures.

[0055] As used in this article, "fiber matrix" refers to the solid portion, mainly composed of plant fibers, remaining after the tobacco raw material has been extracted and separated into solid and liquid components. It is the main material constituting the structural framework of the tobacco cartridge.

[0056] As used in this article, "splitting" refers to breaking down and separating fiber bundles in a fiber matrix through mechanical action (such as a twin-screw splitter) to make them shorter and more uniform individual fibers, which is beneficial for subsequent pulp preparation and molding.

[0057] As used in this article, “auxiliary materials” refers to various functional materials added in the preparation of slurry other than the fiber matrix and water, such as binders (sodium carboxymethyl cellulose), fillers or combustion modifiers (calcium carbonate powder), pore-forming agents (porous starch), etc.

[0058] As used in this article, “refilling” refers to adding back the flavor-rich extract separated in step (1) in a subsequent process (slurry preparation) so that the flavor substances are loaded onto the fiber.

[0059] In some embodiments, in step S4, the conditions for transverse wrinkling are: the scraper and the sheet running direction are at 90°, the pressure is 0.2-0.3MPa, and the difference between the traction speed and the sheet running speed is 15%-20%; the conditions for 45° inclined wrinkling are: the scraper and the sheet running direction are at 40°-50°, the pressure is 0.15-0.25MPa, and the speed difference is 20%-25%.

[0060] In some implementations, step S6 specifically involves applying a pressure of 0.7-0.9 MPa when rolling the outer layer and applying a pressure of 0.2-0.4 MPa when rolling the inner layer, thereby forming a density gradient that is tighter at the top and looser at the bottom.

[0061] In some embodiments, in step S5, the upper and lower V-shaped roller assemblies are made of silicone with a hardness of 65-75 Shore A and a 2-3mm protrusion in the middle; the upper roller applies a pressure of 0.1-0.15MPa to flatten the upper surface of the sheet, and the lower roller applies a pressure of 0.08-0.12MPa to retain the wrinkles on the lower surface of the sheet.

[0062] The inclined wire forming machine is a commonly used forming equipment in the production of paper sheets. The pulp flows onto the inclined forming wire and is dehydrated under vacuum, initially forming a wet sheet.

[0063] As used herein, "cross-wrinkling" is a key process step in this invention. It refers to sequentially wrinkling the sheet in two different directions: first, horizontal wrinkling (the wrinkle direction is perpendicular to the sheet's running direction), and then inclined wrinkling (the wrinkle direction forms an angle of approximately 45° with the sheet's running direction). The two wrinkling processes are superimposed to form a stable three-dimensional mesh-like fold structure.

[0064] As used in this article, "upper and lower V-shaped roller positioning pretreatment" refers to the pretreatment of the cross-wrinkled sheet using a pair of rollers with specific V-shaped profiles before rolling. The main function of the upper roller is to locally flatten the upper surface of the sheet to facilitate alignment and interlayer bonding during subsequent rolling; the lower roller contacts with less pressure to maintain the wrinkled texture of the lower surface of the sheet (i.e., the outer surface of the future cartridge) while preventing the sheet from deviating during transport.

[0065] As used in this article, "dual-station gradient winding" refers to winding a thin sheet onto a tapered needle at a specific angle on a device with two parallel winding stations (dual-station). The gradient is manifested in the application of different winding pressures to different parts of the cartridge (outer / inner layer, corresponding to the upper / lower part) during the winding process, thereby directly forming the desired density and porosity gradient.

[0066] As used in this article, "conical mandrel" refers to a rolling mandrel whose diameter gradually changes from one end to the other. Using a conical mandrel helps to smoothly demold the rolled cartridge blank.

[0067] In some embodiments, in step S8, the equilibration conditions are a temperature of 25°C, a relative humidity of 60%, and an equilibration time of 48 hours. As used in this article, "equilibrium treatment" refers to placing the cut e-cigarette cartridges in a constant temperature and humidity environment for a certain period of time to allow the internal moisture to be evenly distributed and reach a stable state of equilibrium with the external environment, thereby ensuring the stability of the product's physical properties.

[0068] In some embodiments, the testing criteria in step S8 include: upper porosity 35%-45%, lower porosity 55%-65%, absorption resistance coefficient of variation ≤5%, compressive strength ≥0.5MPa, burning rate 2.5-4.5mm / min, and volatile oil retention rate ≥85%.

[0069] As used in this article, "volatile oil retention rate" is an indicator that measures the degree to which low-temperature impregnation and subsequent processes retain the original aroma substances of tobacco. It is usually calculated by comparing the content of specific volatile aroma components in the finished product and the raw materials. ≥85% indicates that the process of this invention can effectively retain most of the natural aroma.

[0070] In one specific embodiment, the method for preparing the pipe tobacco cartridge of the present invention includes the following specific steps: (1) Raw material pretreatment: A variety of aged tobacco raw materials are blended (including but not limited to flue-cured tobacco, Maryland tobacco, Burley tobacco, sun-cured tobacco, cigar tobacco, aromatic tobacco, blackboard tobacco, etc.), crushed to 1-3mm and then extracted at low temperature (40-60℃, solid-liquid ratio 1:5, extraction for 50min), separating the flavor extract from the fiber matrix; the fiber matrix is ​​decomposed by a twin-screw decomposition machine (80-100℃, 300-500r / min) for 20-30min to a fiber length of 0.5-2mm, and directly used as molding raw material to replace traditional tobacco shreds; (2) Slurry preparation: Add water to the fiber matrix to adjust the slurry concentration to 5%-15%, stir and disperse for 10 min; add auxiliary materials (sodium carboxymethyl cellulose 1%-2%, calcium carbonate powder 5%-8%, porous starch 1%-2%), and continue stirring for 20 min; add back 10%-15% of the raw material mass of flavor extract (35% solid content 25-40%), and stir for 15 min until uniform; (3) Forming and dewatering: The slurry is formed into wet sheets (thickness 0.3-0.5mm, quantity 30-50g / m²) by an 80-100 mesh inclined screen forming machine (vacuum degree -0.04~-0.06MPa); the wet sheets are dewatered to a moisture content of 50%-55% by a press roller (0.3-0.5MPa, linear speed 3-6m / min); (4) Cross-folding: The wet sheet is dried with hot air at 80-90℃ and 2-3m / s until the moisture content is 15%-20%; first, cross-folding is performed, with the drying cylinder at 110-130℃ and 3-6m / min, the scraper at 90° to the running direction and 0.2-0.3MPa, the traction at 3-7m / min and the speed difference at 15%-20%; then, cross-folding is performed at 45°, with the scraper at 40°-50° to the running direction, the guide rollers tilted synchronously, the pressure at 0.15-0.25MPa and the speed difference at 20%-25%, forming a "cross-fold + 45°" grid fold with a height of 0.1-0.3mm and a spacing of 0.5-1mm. The moisture content after folding is 8%-10%. (5) Pre-treatment of upper and lower V-shaped rollers for positioning: The cross-wrinkled sheet is conveyed to the symmetrical upper and lower V-shaped roller assembly, which is made of silicone with a hardness of 65-75 Shore A, a 2-3mm bulge in the middle, and an inclination of 5°-8° at both ends, with a 0.1-0.2mm anti-slip texture on the surface; the upper roller applies pressure of 0.1-0.15MPa to flatten the upper surface, with a flattening rate ≥80%, and the lower roller applies pressure of 0.08-0.12MPa to retain the wrinkles on the lower surface, with a retention rate ≥90%; the rotation speed of the upper and lower rollers is 3-7m / min, which matches the sheet conveying speed of 3-7m / min, and the deviation rate is ≤3%; (6) Dual-station gradient winding: The pre-treated sheet is simultaneously wound with two sets of parallel conical winding needles at a 45° angle (diameter 8mm→12mm, center spacing 20-30mm); the outer layer (upper part of the cartridge) is pressurized with 0.7-0.9MPa to obtain a density of 0.4-0.5g / cm³, and the inner layer (lower part of the cartridge) is pressurized with 0.2-0.4MPa to obtain a density of 0.2-0.3g / cm³; the winding speed is 3-5r / s to form a double cartridge integrated blank with a total length of 40-60mm and a diameter of 10-15mm, and a thickness of 1-1.5mm at the integrated part; (7) Centered cutting: Use a circular blade cutting machine (high-speed steel / carbide blade, cutting edge Ra≤0.4μm) to cut along the 1 / 2 of the integral blank, with a rotation speed of 300-500r / min, cutting pressure of 0.05-0.1MPa, and speed of 10-15mm / s; equipped with an elastic pressing component (silicone pressure roller, hardness 50-60ShoreA, pressure 0.03-0.05MPa), the cutting accuracy is ±0.1mm, resulting in two 20-30mm independent tobacco cartridges with structural integrity ≥98%; (8) Post-processing: The e-cigarette cartridges are equilibrated at 25℃ and 60% humidity for 48 hours. The qualified test standards are: upper porosity 35%-45%, lower porosity 55%-65%, suction resistance variation coefficient ≤5%, compressive strength ≥0.5MPa, burning rate 2.5-4.5mm / min, and volatile oil retention rate ≥85%.

[0071] Example

[0072] Table 1. Names of Raw Materials and Suppliers

[0073] Table 2. Instruments used in the experiment and their suppliers

[0074] In addition to those listed in the table above, all other materials and reagents used in the following examples are commercially available unless otherwise specified.

[0075] Example 1:

[0076] The cigarette cartridge is prepared using the following steps: ① Raw material pretreatment: The compounded tobacco raw materials, in which the ratio of flue-cured tobacco, burley tobacco, aromatic tobacco and black tobacco is 4:1:2:3, are crushed to 1-3mm; extracted at an extraction temperature of 70-80℃ and a solid-liquid ratio of 1:5 for 50min, and the extract is separated from the fiber matrix; the fiber matrix is ​​delaminated in a twin-screw delaminator at 90-100℃ and a high delaminating speed of 500r / min for 25min, so that the fiber length is 0.8-1.2mm.

[0077] ② Slurry preparation: Add water to the fiber matrix to adjust the concentration to 12% and stir for 10 min; add 1.5% sodium carboxymethyl cellulose, 7% calcium carbonate powder and 1.5% porous starch and stir for 20 min; add back 13% of the raw material mass of flavor extract, the solid content of which is 38%, and stir for 15 min.

[0078] ③ Forming and Dehydration: Using an 80-mesh inclined screen forming machine, wet sheets are prepared under a vacuum of -0.05 to -0.06 MPa. The thickness of the wet sheets is 0.4-0.5 mm, and the basis weight is 45-50 g / m². Then, the sheets are dehydrated using a press roller at a pressure of 0.4-0.5 MPa and a linear speed of 5-6 m / min, so that the moisture content of the sheets is reduced to 53-55%.

[0079] ④ Cross-folding: First, hot air drying is performed at a temperature of 85-90℃ and a wind speed of 2.5-3m / s to dry the sheet to a moisture content of 18-20%. Next, transverse folding is performed on the sheet with a drying cylinder of 120-130℃ and a speed of 5-6m / min, a scraper at 90° and a pressure of 0.25-0.3MPa, a traction speed of 6-7m / min, and a speed difference of 18-20%. Then, the sheet is folded at a 45° angle with the scraper at 45° and the guide rollers tilted synchronously, a pressure of 0.2-0.25MPa, and a speed difference of 23-25%, forming a grid of folds with a fold height of 0.2-0.3mm and a fold spacing of 0.8-1mm. The final moisture content is 9-10%.

[0080] ⑤ V-shaped positioning pretreatment: The wrinkled sheet is pretreated using upper and lower V-shaped rollers. The silicone hardness is 70-75 Shore A, the middle protrusion is 2.5-3mm, the V-angle is 5°, and the surface texture is 0.15-0.2mm. The upper roller applies a pressure of 0.12-0.15MPa, and the flattening rate is ≥85%. The lower roller applies a pressure of 0.1-0.12MPa, and the retention rate is ≥92%. The rotation speed is 6-7m / min, and the deviation rate is ≤2%.

[0081] ⑥ Dual-station winding: The thin sheet is wound around a conical winding needle at a 45° angle, with the needle diameter gradually increasing from 8mm to 12mm and the spacing between the needles being 25-30mm; a pressure of 0.8-0.9MPa is applied to the outer layer to achieve a density of 0.45-0.5g / cm³; a pressure of 0.3-0.4MPa is applied to the inner layer to achieve a density of 0.25-0.3g / cm³; the winding speed is 4-5r / s, resulting in a double-smoke cartridge integrated blank with a length of 55-60mm, a diameter of 13-15mm, and a thickness of 1.2-1.5mm at the integrated section.

[0082] ⑦ Centered Cutting: A circular cutter is used, equipped with a carbide blade with a surface roughness Ra≤0.4μm, cutting along the 1 / 2 mark; the cutting speed is 450-500r / min, the pressure is 0.08-0.1MPa, and the speed is 13-15mm / s; the elastic pressing component uses a silicone pressure roller with a hardness of 60 Shore A and a pressure of 0.04-0.05MPa; the cutting accuracy is ±0.1mm, resulting in two e-cigarette cartridges with a length of 27-30mm and a structural integrity ≥99%.

[0083] ⑧ Post-processing: Equilibrate at 25℃ and 60% humidity for 48 hours to obtain the finished e-cigarette cartridge.

[0084] The quality inspection results meet the following parameter ranges: upper porosity 40-42%, lower porosity 60-62%, absorption resistance coefficient of variation ≤4.2%, compressive strength ≥0.6MPa, burning rate 3.5-4.0mm / min, and volatile oil retention rate ≥88%.

[0085] Example 2:

[0086] Following the same method as in Example 1, the extraction temperature was lowered to 60-70℃, while other conditions remained unchanged, to obtain the finished e-cigarette cartridge.

[0087] Example 3:

[0088] Following the same method as in Example 1, the extraction temperature was lowered to 40-60℃, while other conditions remained unchanged, to obtain the finished e-cigarette cartridge.

[0089] Example 4:

[0090] Following the same method as in Example 3, only the horizontal wrinkling method was used, without the subsequent 45° inclined wrinkling process, and other conditions remained unchanged, to obtain the finished e-cigarette cartridge.

[0091] Specifically, refer to Example 3. The specific procedures are as follows: ① Raw material pretreatment, ② Slurry preparation, ③ Molding and dewatering stages are consistent with Example 3. ④ In the cross-creeping stage, the 45° inclined creeping process is cancelled. Specifically, hot air drying (85-90℃, wind speed 2.5-3m / s) is carried out until the moisture content is 18-20%; first, transverse creeping is carried out (drying cylinder 120-130℃, 5-6m / min, scraper 90°, 0.25-0.3MPa, traction 6-7m / min, speed difference 18-20%); moisture content is 9-10%. ⑤ V-shaped positioning pretreatment: ⑥ Dual-station rolling: ⑦ Center cutting: ⑧ Post-processing is consistent with Example 3.

[0092] Subsequent experimental results showed that the combustion uniformity fluctuated and there was a certain proportion of slanted burning.

[0093] Example 5: Following the same method as in Example 3, but without performing the V-shaped positioning pretreatment, and with other conditions remaining unchanged, the finished e-cigarette cartridge was obtained.

[0094] Without using V-shaped positioning pretreatment, there are two main reasons: first, there is a certain degree of deviation; second, it is somewhat misleading for the traditional layout of pipe smoking, which is tight at the top and loose at the bottom; and third, it can lead to the accumulation and blockage of some substances later on, resulting in excessive suction and thus affecting the smoking experience.

[0095] suction resistance test

[0096] Experimental subjects: 5 people with more than 1 year of experience in using pipes (numbered 1-5).

[0097] Tobacco shreds parameters: uniform batch, humidity 55%±2%, shred diameter 0.8-1.2mm, after pretreatment, clumps of tobacco shreds are removed to ensure that the basic condition of the tobacco shreds is consistent.

[0098] Pipe specifications: Briar wood, bowl volume 9cm³, flue diameter 3mm. The flue was cleaned with a cleaning rod before the experiment to eliminate any residual effects.

[0099] Measuring instruments: The instruments were calibrated once every 5 experiments using a suction resistance measuring instrument (modified from the i TDR100 prototype of Zhengzhou Tobacco Research Institute, with a range of 0-3000Pa and an accuracy of ±10Pa), an electronic balance (accuracy 0.01g), and a sub-analytical balance (accuracy 0.001g). The instruments were calibrated once every 5 experiments to ensure data accuracy.

[0100] Experimental description: (1) Conventional pipe tobacco (self-filling): The testers did not weigh the tobacco when filling it, but operated according to their daily habits (including pressing force, layering filling method, etc.). Each person completed 25 repeated experiments, with a total of 12 sets of initial data. One set of abnormal data was removed due to instrument failure (sucking resistance fluctuation exceeding ±30Pa) and tobacco blockage (sucking resistance >2500Pa), and finally 124 sets of valid data were retained.

[0101] (2) The tobacco cartridge of the present invention (the finished tobacco cartridge obtained in Example 1): The draw resistance was tested with reference to conventional pipe tobacco experiments.

[0102] (3) Comparison of patented tobacco cartridges: CN120419702A was used, and the draw resistance was tested with reference to conventional pipe tobacco experiments.

[0103] Deviation judgment criteria: If the absolute value of the draw resistance deviation (difference from the average value of the same weight) is >50Pa, and after excluding the differences in the properties of the tobacco itself (such as the diameter fluctuation) and instrument error (and after being confirmed by the smoke evaluation that there are large changes in draw resistance at each node), it is judged as a large draw resistance deviation caused by uneven filling.

[0104] The experimental results are as follows: Table 3 Results of the inhalation resistance test of conventional pipe tobacco by the No. 1 evaluator

[0105] Table 4. Results of the inhalation resistance test of conventional pipe tobacco by the second evaluator.

[0106] Table 5. Results of the inhalation resistance test of conventional pipe tobacco by three evaluators.

[0107] Table 6. Results of the inhalation resistance test on conventional pipe tobacco by test takers No. 4

[0108] Table 7 Results of the inhalation resistance test of conventional pipe tobacco by the No. 5 evaluator

[0109] Table 8. Results of the inhalation resistance test of the present invention's cartridge by the first evaluator.

[0110] Table 9. Results of the inhalation resistance test on the present invention's cigarette cartridge by the second evaluator.

[0111] Table 10. Results of the inhalation resistance test of the present invention's tobacco cartridge by three evaluators.

[0112] Table 11 Results of the inhalation resistance test of the present invention's tobacco cartridge by four evaluators.

[0113] Table 12 Results of the inhalation resistance test of the present invention's tobacco cartridge by the fifth evaluator

[0114] Table 13 Comparison of Inhalation Resistance Test Results of Patented Tobacco Cartridges by Tester No. 1

[0115] Table 14 Results of the comparative test on the draw resistance of the patented e-cigarette cartridges by the second evaluator.

[0116] Table 15 Results of the comparative test on the draw resistance of the patented e-cigarette cartridges by three evaluators.

[0117] Table 16 Results of the comparative test on the draw resistance of the patented e-cigarette cartridges by four evaluators.

[0118] Table 17 Comparison of Inhalation Resistance Test Results of Patented Tobacco Cartridges by Test Participant No. 5

[0119] Sensory experiments

[0120] Sensory evaluation tests were conducted on samples of conventional pipe tobacco, comparative patented tobacco cartridges, and tobacco cartridges of the present invention (Example 1). Five groups of experimental samples with good filling conditions (draw resistance close to 1000 Pa) were selected from each group for evaluation, and the results were averaged. Specific experimental results are as follows: Table 18 Results of Sensory Evaluation Experiment

[0121] This tobacco cartridge retains volatile oils and other substances to the maximum extent through low-temperature extraction technology, resulting in a stable and controllable burning rate and a sensory experience that is on par with or even better than traditional products. At the same time, through fiber decomposition optimization and elastic structure design, the cartridge has good resistance to compression deformation. Its size covers 10-15mm in diameter and 20-30mm in length, making it widely compatible with various mainstream pipes. It has achieved a four-fold breakthrough in efficiency, stability, experience, and compatibility, providing consumers with a higher quality, more convenient, and more controllable pipe smoking solution.

[0122] In the foregoing description of exemplary embodiments / specific implementations of this patent, various features of this patent are sometimes combined in a single embodiment / specific implementation or its figures and description, with the aim of simplifying the disclosure and aiding in the understanding of one or more of the various aspects of the invention. However, unless expressly stated otherwise or in obvious technical contradiction or exclusion, the descriptive method of this patent should not be construed as reflecting an intention that the claimed features of the invention are more than expressly stated in each claim. Rather, the inventive aspect reflected in the claims lies in not all the features of a single foregoing disclosed embodiment / specific implementation. Therefore, the claims following the detailed description are hereby expressly incorporated into this detailed description, each claim existing independently as a separate embodiment / specific implementation of this patent.

[0123] The terms and expressions used in this specification are for illustrative purposes and not for limitation. Their use is not intended to exclude any equivalents of the shown and described features or portions thereof, but rather to facilitate the understanding that various modifications may be possible within the scope of this patent claim. Therefore, it should be understood that while this patent has been specifically disclosed through preferred embodiments, exemplary embodiments, and optional features, variations or modifications of the concepts disclosed herein may be adopted by those skilled in the art, and such variations and modifications are therefore considered to be within the scope of this patent as defined by the appended claims. The specific embodiments given in this specification are examples of useful embodiments of this patent, and it will be apparent to those skilled in the art that this patent can be implemented using many variations of the devices, device components, and method steps disclosed herein.

[0124] The foregoing description of specific embodiments fully discloses the general features of this patent, enabling others to easily modify and / or adapt such embodiments for various applications by applying knowledge within the scope of the art, without excessive experimentation or deviation from the general concept of this patent. Therefore, based on the teachings and guidance provided herein, it is intended that such modifications and alterations be included within the meaning and scope of equivalents of the disclosed embodiments. It should be understood that the wording or terminology used herein is for descriptive purposes and not intended to be limiting; thus, the wording or terminology in this specification will be interpreted by those skilled in the art based on the foregoing teachings and guidance.

[0125] Furthermore, the scope of this patent should not be limited to any of the exemplary embodiments described above, but only to the appended claims and their equivalents.

Claims

1. A pipe tobacco cartridge, characterized in that, The tobacco cartridge is a truncated cone with a spatial mesh-like porous structure, which is rolled from tobacco sheets. Its interior has a porosity gradient structure with a tighter upper part and a looser lower part. The porosity of the upper part is 35%-45%, and the porosity of the lower part is 55%-65%. The tobacco cartridge is a one-piece molded structure.

2. The pipe tobacco cartridge according to claim 2, characterized in that, The tobacco sheet includes transverse pleats and inclined pleats at 45° to the transverse pleats, the pleats being 0.1-0.3 mm high and 0.5-1 mm apart.

3. The pipe tobacco cartridge according to claim 1, characterized in that, The cartridge has a diameter of 10-15mm and a length of 20-30mm.

4. The pipe tobacco cartridge according to claim 2, characterized in that, The coefficient of variation of the draw resistance of the cartridge is ≤5%, and the draw resistance under standard vaping conditions is in the range of 950~1050Pa.

5. A method for preparing pipe tobacco cartridges as described in any one of claims 1-4, characterized in that, Includes the following steps: S1. Raw material pretreatment: The compound tobacco raw materials are crushed and then extracted at low temperature to separate the flavor extract and the fiber matrix. The fiber matrix is ​​then decomposed and used for later use. S2. Slurry preparation: The fiber matrix obtained in step S1 is mixed with water to form a slurry, and auxiliary materials are added and a portion of the flavor extract is added back. The mixture is stirred evenly. S3. Shaping and Dehydration: The slurry is formed into wet sheets and then dehydrated; S4. Cross wrinkling: After drying the dehydrated sheet, cross wrinkling and 45° inclined wrinkling are performed to form a grid of wrinkles. S5. Positioning and pre-processing of upper and lower V-shaped rollers: The thin sheet after cross-wrinkling is pre-processed by positioning through a symmetrical upper and lower V-shaped roller assembly. S6. Dual-station gradient winding: The pre-treated sheet is wound around a tapered winding needle at a certain angle for gradient pressure winding to form a continuous blank. S7. Center Cut: Cut the conjoined blank along the center to obtain two separate cartridges; S8. Post-processing: The cut e-cigarette cartridges are balanced and tested to obtain the finished product.

6. The method according to claim 5, characterized in that, In step S4, the conditions for transverse wrinkling are: the scraper and the sheet running direction are at 90°, the pressure is 0.2-0.3MPa, and the difference between the traction speed and the sheet running speed is 15%-20%; the conditions for 45° inclined wrinkling are: the scraper and the sheet running direction are at 40°-50°, the pressure is 0.15-0.25MPa, and the speed difference is 20%-25%.

7. The method according to claim 6, characterized in that, In step S6, the gradient pressure rolling specifically involves applying a pressure of 0.7-0.9 MPa when rolling the outer layer and applying a pressure of 0.2-0.4 MPa when rolling the inner layer, thereby forming a density gradient that is tighter at the top and looser at the bottom.

8. The method according to claim 7, characterized in that, In step S5, the upper and lower V-shaped roller assemblies are made of silicone with a hardness of 65-75 Shore A and a 2-3mm protrusion in the middle. The upper roller applies a pressure of 0.1-0.15MPa to flatten the upper surface of the sheet, and the lower roller applies a pressure of 0.08-0.12MPa to retain the wrinkles on the lower surface of the sheet.

9. The method according to claim 9, characterized in that, In step S8, the conditions for the equilibration process are a temperature of 25°C, a relative humidity of 60%, and an equilibration time of 48 hours.

10. The method according to claim 6, characterized in that, In step S8, the testing standards include: upper porosity 35%-45%, lower porosity 55%-65%, absorption resistance coefficient of variation ≤5%, compressive strength ≥0.5MPa, burning rate 2.5-4.5mm / min, and volatile oil retention rate ≥85%.

Citation Information

Patent Citations