A polymeric surfactant, its preparation method and application
By preparing a polymeric surfactant with an asymmetric tadpole-shaped twin structure, the problem of underutilization of the function of propylene glycol ether surfactants was solved, achieving high surface activity and low foaming properties. This makes it suitable for applications requiring low foaming characteristics and good low-temperature flowability, which aligns with the development trend of green chemicals.
Patent Information
- Application Number
- CN202611308414.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-08-27
- Publication Date
- 2026-11-17
AI Technical Summary
Existing propylene glycol ether surfactants do not fully function in cleaning and emulsification systems, and their low-foaming and low-temperature fluidity are insufficient, making it difficult to meet the needs of high-end green cleaning.
The polymeric surfactant employs an asymmetric tadpole-shaped twin structure, and introduces a hydrophilic glycoside head by connecting a long-chain alkyl hydrophobic tail and an epoxypropyl group through a propylene glycol oligoether chain. The preparation method includes propoxylation, epoxypropylation, and glycosylation steps, avoiding polyoxyethylene chains and nitrogen and phosphorus elements, which is in line with the development trend of green chemicals.
It achieves high surface activity, low foaming and low temperature flowability, and reduces the critical micelle concentration by about 60%, making it suitable for applications with low foaming properties and good low temperature flowability, and replacing traditional APE-type nonionic surfactants.
Smart Images

Figure SMS_3 
Figure QLYQS_1
Abstract
Description
Technical Field
[0001] This invention relates to the field of nonionic green surfactant technology, specifically to a polymeric surfactant, its preparation method, and its application. Background Technology
[0002] Propylene glycol ethers are a class of high-performance oxygen-containing solvents, characterized by low volatility, strong coupling ability, good biodegradability, and low skin irritation. They are widely used in coatings, inks, and electronic cleaning applications, with typical products including propylene glycol methyl ether, propylene glycol butyl ether, and dipropylene glycol methyl ether. However, propylene glycol ethers themselves have short hydrophobic chains and weak surface activity, typically used only as co-solvents in cleaning and emulsification systems. They require the addition of large amounts of traditional surfactants to achieve the desired effect, thus limiting their functional expansion.
[0003] Currently, surfactants related to propylene glycol ether structures mainly fall into the following categories:
[0004] 1. Propylene glycol block polyethers: Pluronic-type polyethers obtained by block copolymerization of propylene oxide (PO) and ethylene oxide (EO), mainly used as defoamers and demulsifiers. These products have high molecular weight, weak wetting and penetration capabilities, and the polyoxyethylene segments are easily deactivated at high temperatures, resulting in generally poor biodegradability. 2. Fatty alcohol propoxylates: Addition products of long-chain fatty alcohols and propylene oxide. They exhibit better low-temperature fluidity than fatty alcohol polyoxyethylene ethers, but have low cloud points, significantly reduced surface activity at high temperatures, and tend to produce high foaming rates. 3. Alcohol ether glycosides (AEG): Green surfactants obtained by direct glycosylation of fatty alcohol polyoxyethylene ethers, combining the advantages of alkyl glycosides and fatty alcohol ethers, but still suffer from easy crystallization. 4. Gemini glycoside surfactants: Existing reports mostly describe symmetrical structures, i.e., both ends are alkyl hydrophobic ends with a disaccharide hydrophilic group in the middle, or dialkyl disaccharides have a symmetrical structure, making their synthetic routes complex.
[0005] In summary, the existing technology has the following core defects: propylene glycol ethers are only used as solvent additives and are not directly constructed into the molecular skeleton of surfactants, so their functions are not fully utilized; existing propoxylated surfactants have insufficient low foaming properties and low-temperature fluidity, making it difficult to meet the needs of high-end green cleaning. Summary of the Invention
[0006] The purpose of this invention is to provide a polymeric surfactant that combines low foaming properties, low-temperature fluidity, and high surface activity. Accordingly, this invention also provides a method for preparing the aforementioned polymeric surfactant and its applications.
[0007] The specific technical solution of the present invention is as follows:
[0008] In a first aspect, this invention provides a polymeric surfactant with the chemical formula: ;
[0009] Where R is C8~C 16 Straight-chain or branched saturated alkyl group, C3H6O is a propoxy unit, G is a glucose residue, m is 1~1.8, and n is 2~5.
[0010] In some preferred embodiments, R is C8~C 16 Straight-chain saturated alkyl groups, preferably C 10 Straight-chain saturated alkyl, C 12 Straight-chain saturated alkyl or C 16 Straight-chain saturated alkyl group.
[0011] In some preferred embodiments, m is 1.4 to 1.7, preferably 1.4, 1.5 or 1.7.
[0012] In some preferred embodiments, n is 2 or 3.
[0013] In a second aspect, the present invention provides a method for preparing the above-mentioned polymeric surfactant, comprising the following steps:
[0014] (1) In an inert atmosphere, C8~C 16 Fatty alcohols and propylene oxide react at 120-140°C under the action of an alkali metal catalyst until the system pressure no longer decreases, while the system pressure is controlled to be ≤0.4MPa, to obtain propylene glycol monoalkyl ethers;
[0015] (2) Propylene glycol monoalkyl ether, epichlorohydrin and alkaline solution are reacted at 40~50℃ for 2~8h under the action of phase transfer catalyst to obtain epioxypropyl propylene glycol alkyl ether;
[0016] (3) Glycidyl propylene glycol alkyl ether reacts with reducing sugar under the action of an acidic catalyst at 100~120℃ and 10~20kPa for 3~7h to obtain a high molecular surfactant;
[0017] Among them, C8~C 16 The molar ratio of fatty alcohol to propylene oxide is 1:1 to 100;
[0018] The molar ratio of propylene glycol monoalkyl ether to epichlorohydrin is 1:1.1~1.5;
[0019] The alkaline solution is composed of potassium hydroxide solution, sodium hydroxide solution, ammonia solution, sodium hypochlorite solution, sodium carbonate solution, and sodium bicarbonate solution, wherein the molar ratio of alkali to epichlorohydrin in the alkaline solution is 1~1.5:1;
[0020] The reducing sugar is glucose and / or maltodextrin, and the molar ratio of reducing sugar to glycidyl glycol alkyl ether is 1~1.8:1.
[0021] In some preferred embodiments, the alkali metal catalyst is an alkali metal hydroxide and / or an alkali metal C1-C4 alkoxide, preferably at least one of sodium methoxide, sodium ethoxide and potassium hydroxide.
[0022] The addition amount of alkali metal catalyst is C8~C 16 0.5~1.2wt% of fatty alcohols.
[0023] In some preferred embodiments, the phase transfer catalyst is tetrabutylammonium bromide and / or benzyltriethylammonium chloride.
[0024] In some preferred embodiments, the amount of phase transfer catalyst added is 0.3 to 0.8 wt% of the total mass of the system.
[0025] In some preferred embodiments, the alkaline solution is a 40-50 wt% NaOH solution.
[0026] In some preferred embodiments, the acidic catalyst is p-toluenesulfonic acid and / or dodecylbenzenesulfonic acid.
[0027] In some preferred embodiments, the amount of acidic catalyst added is 0.5 to 2.0 wt% of the reducing sugar.
[0028] In a third aspect, the present invention provides the use of the above-described polymeric surfactant or the polymeric surfactant prepared by the above-described preparation method in the preparation of a surface-active composition.
[0029] In a fourth aspect, the present invention provides a surface-active composition comprising the above-described polymeric surfactant or a polymeric surfactant prepared by the above-described preparation method.
[0030] In a fifth aspect, the present invention provides the application of the above-mentioned polymeric surfactant, the polymeric surfactant prepared by the above-mentioned preparation method, or the above-mentioned surface-active composition in industrial hard surface cleaning, textile printing and dyeing auxiliaries, and pesticide emulsifiers.
[0031] According to the above technical solution, the present invention has at least the following beneficial effects:
[0032] 1. The polymeric surfactant provided by this invention uses propylene glycol oligoether chains as flexible linkers, with one end being a long-chain alkyl hydrophobic tail and the other end being a glycoside hydrophilic head introduced through glycidyl ring opening. The overall structure is an asymmetric tadpole-shaped twin structure of "single hydrophobic - linker chain - single hydrophilic", which takes into account high surface activity, low foaming and low temperature fluidity, and the critical micelle concentration is reduced by about 60% compared with traditional alkyl glycosides.
[0033] 2. The polymeric surfactant provided by this invention does not contain polyoxyethylene chains or nitrogen and phosphorus elements, has low skin irritation, and conforms to the development trend of green chemicals.
[0034] 3. The polymeric surfactant provided by this invention has a wide range of applications: its low foaming properties are suitable for spray and ultrasonic cleaning processes, and its good low-temperature fluidity and high surface activity are suitable for low-temperature dyeing processes and antifreeze, etc. It can replace traditional APE-type nonionic surfactants. Detailed Implementation
[0035] To enable those skilled in the art to better understand the technical solutions of the present invention, some non-limiting embodiments are further disclosed below to provide a more detailed description of the present invention.
[0036] It is important to note that, in the context of this invention, all figures disclosed herein are approximate values, regardless of whether words such as "approximately" or "about" are used. The value of each figure may vary by 1%, 2%, 5%, 7%, 8%, 10%, 15%, or 20%, etc. Whenever a figure with a value of N is disclosed, any figure having a value of N±1%, N±2%, N±3%, N±5%, N±7%, N±8%, N±10%, N±15%, or N±20% is explicitly disclosed, where "±" refers to addition or subtraction. Whenever a lower limit, RL, and an upper limit, RU, of a numerical range are disclosed, any value within that disclosed range is explicitly disclosed. In particular, the following value is included within this range: R = RL + K * (RU - RL), where K is a variable increasing in 1% increments from 1% to 100%. For example: 1%, 2%, 3%, 4%, 5%, 50%, 51%, 52%, 95%, 96%, 97%, 98%, 99%, or 100%. In addition, the numerical ranges defined by the two R numbers disclosed herein are also specifically included.
[0037] The maltodextrin mentioned in this invention refers to a mixture of oligosaccharides and glucose monosaccharides consisting of 2 to 10 glucose units linked by α-1,4-glycosidic bonds. The average degree of polymerization (DP) of the mixture is 1 < DP ≤ 10, based on the number of glucose units and glucose residues.
[0038] The general structural formula of the polymeric surfactant provided by this invention is as follows:
[0039] .
[0040] Example 1
[0041] The polymeric surfactant provided in this embodiment is dodecyl dipropylene glycol ether glucoside (R=C 12 (n=2, m≈1.4), its preparation method includes the following steps:
[0042] 1. Propoxylation:
[0043] Add 186g (1mol) of n-dodecyl alcohol and 1.5g of sodium methoxide to a 1L high-pressure reactor. After sealing, purge with nitrogen three times and start stirring to raise the temperature to 130℃. Slowly introduce 116g (2mol) of propylene oxide, controlling the pressure inside the reactor to ≤0.4MPa. After the material is introduced, keep it at the temperature for 1 hour until the pressure no longer drops. Then, cool it down to 60℃ and discharge the material to obtain approximately 298g of dodecyl dipropylene glycol ether.
[0044] 2. Epioxypropylation:
[0045] Add 298g of the above intermediate dodecyl dipropylene glycol ether (1mol), 111g (1.2mol) epichlorohydrin, and 3g tetrabutylammonium bromide to a 1L four-necked flask, stir and heat to 45℃; slowly add 96g of 50wt% NaOH solution over 2h, and continue to keep the reaction at the temperature for 4h after the addition is complete; allow to stand and separate the layers, separate the lower brine layer, wash the organic phase with deionized water until neutral, and remove unreacted epichlorohydrin by vacuum distillation to obtain approximately 335g of epichlorohydrin dodecyl dipropylene glycol ether;
[0046] 3. Glycosylation:
[0047] Add 335g of the above product, glycidyl dodecyl dipropylene glycol ether (0.9mol), 216g (1.2mol) of anhydrous glucose, and 1.5g of p-toluenesulfonic acid to a 1L reaction flask. Start stirring and evacuate the system to an absolute pressure of 15kPa. Heat to 110℃ and react for 5h, continuously separating the water generated during the reaction. After the reaction is complete, cool to 70℃, neutralize with triethanolamine to pH=6.5, add 1w% activated carbon and keep warm for decolorization for 1h. Filter under pressure to obtain approximately 490g of the pale yellow, viscous, transparent product, dodecyl dipropylene glycol ether glucoside, with a yield of 75.81%.
[0048] Example 2
[0049] The polymeric surfactant provided in this embodiment is decyl tripropylene glycol ether glucoside (R=C 10 (n=3, m≈1.5), its preparation method includes the following steps:
[0050] 1. Propoxylation:
[0051] Add 158g (1mol) of n-decyl alcohol and 1.264g of sodium methoxide to a 1L high-pressure reactor. After sealing, purge with nitrogen three times and start stirring to raise the temperature to 120℃. Slowly introduce 174g (3mol) of propylene oxide, controlling the pressure inside the reactor to ≤0.4MPa. After the material is introduced, keep it at the temperature for 2 hours until the pressure no longer drops. Then, cool it down to 60℃ and discharge the material to obtain approximately 328g of decyl tripropylene glycol ether.
[0052] 2. Epioxypropylation:
[0053] Add 328g of the above intermediate decyltripropylene glycol ether (1mol), 129.5g (1.4mol) epichlorohydrin, and 2.69g tetrabutylammonium bromide to a 1L four-necked flask, stir and heat to 40℃; slowly add 156g of 40wt% NaOH solution over 1 hour, and continue to keep the reaction at the temperature for 3 hours after the addition is complete; allow to stand and separate the layers, separate the lower brine layer, wash the organic phase with deionized water until neutral, and remove unreacted epichlorohydrin by vacuum distillation to obtain approximately 370g of epichlorohydrin ether;
[0054] 3. Glycosylation:
[0055] Add 370g of the above product, glycidyl decyl tripropylene glycol ether (1mol), 180g (1mol) of anhydrous glucose, and 0.9g of p-toluenesulfonic acid to a 1L reaction flask. Start stirring and evacuate the system to an absolute pressure of 10kPa. Heat to 100℃ and react for 4h, continuously separating the water generated during the reaction. After the reaction is complete, cool to 70℃, neutralize with triethanolamine to pH=6.5, add 1w% activated carbon and keep warm for decolorization for 1h. Filter under pressure to obtain approximately 476g of the pale yellow, viscous, transparent product, decyl tripropylene glycol ether glucoside, with a yield of 73.85%.
[0056] Example 3
[0057] The polymeric surfactant provided in this embodiment is hexadecyl dipropylene glycol ether maltodextrin (R=C 16 (n=2, m≈1.7), its preparation method includes the following steps:
[0058] 1. Propoxylation:
[0059] Add 242g (1mol) of n-hexadecyl alcohol and 2.18g of sodium methoxide to a 1L high-pressure reactor. After sealing, purge with nitrogen three times and start stirring to raise the temperature to 140℃. Slowly introduce 232g (4mol) of propylene oxide, controlling the pressure inside the reactor to ≤0.4MPa. After the material is introduced, keep it at the temperature for 3 hours until the pressure no longer drops. Then, cool it down to 60℃ and discharge the material to obtain approximately 470g of hexadecyl dipropylene glycol ether.
[0060] 2. Epioxypropylation:
[0061] Add 470g of the above intermediate hexadecyl dipropylene glycol ether (1mol), 120.3g (1.3mol) epichlorohydrin, and 4.25g tetrabutylammonium bromide to a 1L four-necked flask, stir and heat to 50℃; slowly add 134.4g of 50wt% NaOH solution over 3h, and continue to keep the reaction at the temperature for 5h after the addition is complete; allow to stand and separate the layers, separate the lower brine layer, wash the organic phase with deionized water until neutral, and remove unreacted epichlorohydrin by vacuum distillation to obtain approximately 498g of epichlorohydrin hexadecyl dipropylene glycol ether;
[0062] 3. Glycosylation:
[0063] Add 498g of the above product glycidyl hexadecyl dipropylene glycol ether (0.85mol), 270g (1.5mol) of maltodextrin (average degree of polymerization 1.7), and 4.38g of p-toluenesulfonic acid to a 1L reaction flask. Start stirring and evacuate the system to an absolute pressure of 20kPa. Heat to 120℃ and react for 7h, continuously separating the water generated during the reaction. After the reaction is completed, cool to 70℃, neutralize with triethanolamine to pH=6.5, add 1w% activated carbon and keep warm for decolorization for 1h. Filter under pressure to obtain approximately 682g of the pale yellow viscous transparent product hexadecyl dipropylene glycol ether maltodextrin glycoside, with a yield of 79.78%.
[0064] Comparative Example 1
[0065] Preparation of dodecyl glycosides:
[0066] Add 200g C to a 1L pressure-resistant reactor 12 A mixture of fatty alcohol, 180 g of anhydrous glucose, and 1.9 g of p-toluenesulfonic acid catalyst was prepared. The system was evacuated to 12 kPa absolute pressure, stirred, and heated to 115 °C, and the reaction was continued for 6 h, continuously removing water molecules generated during the reaction. After the reaction was completed, the temperature was lowered to 70 °C, and the pH of the system was neutralized to 6.5 using triethanolamine. 1 wt% of powdered activated carbon was added, and the mixture was stirred and kept at this temperature for 1 h for decolorization. Solid impurities were removed by pressure filtration, and excess free fatty alcohol was removed by vacuum distillation to obtain a pale yellow viscous dodecyl glycoside product.
[0067] Comparative Example 2
[0068] Preparation of lauryl alcohol polyoxyethylene ether:
[0069] Add 186 g (1 mol) lauryl alcohol and 1.5 g potassium hydroxide catalyst to a dry high-pressure reactor, start stirring and heat to 90-100°C, dehydrate under a vacuum of -0.09 MPa or higher for 0.5-1 h until the water content of the system is ≤50 ppm; after dehydration, turn off the vacuum, purge the air in the reactor with nitrogen three times, and continue heating to 130-140°C. Then, slowly introduce a total of approximately 396 g (9 mol) ethylene oxide through a metering pump, controlling the reaction temperature throughout the process. At 150℃ and 0.3MPa, the feeding time is controlled at 4h. After feeding, the temperature is maintained and stirring is continued for 1h until the pressure inside the reactor no longer decreases. Then, the system is cooled to below 80℃, and vacuum degassing is performed for 15~30min to remove residual ethylene oxide. Then, glacial acetic acid is slowly added dropwise to neutralize the system to a pH of 6.0~7.0. Finally, the temperature is raised to 100~110℃ and vacuum dehydrated until the moisture content is ≤0.5%. The system is then cooled and filtered to remove insoluble salts, thus obtaining lauryl alcohol polyoxyethylene ether.
[0070] Performance testing
[0071] Examples 1-3 and Comparative Examples 1-2 of this invention were tested for their critical micelle concentration, surface tension, initial foam height, and appearance. The results are shown in Table 1. The specific test methods are as follows:
[0072] Critical micelle concentration: Tested according to standard GB / T11276-2007 "Determination of critical micelle concentration of surfactants";
[0073] Surface tension: Tested according to standard GB / T22237-2008 "Determination of surface tension of surfactants";
[0074] Initial foam height: Tested according to standard GB / T7462-1994 "Determination of foaming power of surfactants - Modified Ross-Miles method";
[0075] Appearance: The surfactants prepared in Examples 1-3 and Comparative Examples 1 and 2 were left to stand at 0°C for 24 hours and their appearance was observed.
[0076] Table 1. Performance test results of Examples 1-3 and Comparative Examples 1 and 2
[0077]
[0078] A lower critical micelle concentration (CMC) indicates that the surfactant can form micelles and exert its effect at a lower concentration, resulting in higher surface activity. The CMC of all three examples is significantly lower than that of Comparative Examples 1 and 2, indicating that the surfactants prepared in these examples have superior micellization capabilities, achieving their effects at lower concentrations, and offering advantages in application cost and efficiency. A lower surface tension value indicates a stronger ability of the surfactant to reduce the surface tension of the solution, resulting in better core surface properties such as wetting, penetration, and emulsification. The surface tension of all three examples is significantly lower than that of Comparative Examples 1 and 2, demonstrating stronger basic surface activity and superior performance in interface-related applications. Initial foam height reflects foaming ability; a higher value indicates stronger foaming. Comparative Examples 1 and 2 have initial foam heights of 150-160 mm, classifying them as high-foaming products; the foam height of the three examples is only 38-51 mm, with foaming ability far lower than the comparative samples, classifying them as low-foaming surfactants. This characteristic offers significant advantages in most industrial scenarios such as industrial cleaning, printing and dyeing, and machining, preventing foam overflow, reducing defoaming processes, and improving the stability and convenience of the application process. All three examples are transparent homogeneous liquids, indicating good solubility and system stability at room temperature, facilitating metering, compounding, and on-site use. Comparative Example 1 is a turbid semi-solid, and Comparative Example 2 is a white paste, exhibiting poor solubility and dispersibility, resulting in weaker ease of use and storage stability compared to the examples.
[0079] The above embodiments are only used to illustrate the technical solutions of the present invention, and are not intended to limit it. Although the present invention has been described in detail with reference to the foregoing embodiments, those skilled in the art should understand that modifications can still be made to the technical solutions described in the foregoing embodiments, or equivalent substitutions can be made to some of the technical features. Such modifications or substitutions do not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the embodiments of the present invention.
Claims
1. A polymeric surfactant, characterized in that, Its chemical formula is ; Where R is C8~C 16 Straight-chain or branched saturated alkyl group, C3H6O is a propoxy unit, G is a glucose residue, m is 1~1.8, and n is 2~5.
2. The polymeric surfactant according to claim 1, characterized in that, R is C8~C 16 Straight-chain saturated alkyl groups, preferably C 10 Straight-chain saturated alkyl, C 12 Straight-chain saturated alkyl or C 16 Straight-chain saturated alkyl groups; and / or, m is 1.4~1.7, preferably 1.4, 1.5 or 1.7; and / or, n is 2 or 3.
3. A method for preparing the polymeric surfactant according to claim 1 or 2, characterized in that, Includes the following steps: (1) In an inert atmosphere, C8~C 16 Fatty alcohols and propylene oxide react at 120-140°C under the action of an alkali metal catalyst until the system pressure no longer decreases, while the system pressure is controlled to be ≤0.4MPa, to obtain propylene glycol monoalkyl ethers; (2) The propylene glycol monoalkyl ether, epichlorohydrin and alkaline solution are reacted at 40~50℃ for 2~8h under the action of a phase transfer catalyst to obtain epioxypropyl propylene glycol alkyl ether; (3) The epoxypropyl propylene glycol alkyl ether reacts with reducing sugar at 100~120℃ and 10~20kPa for 3~7h under the action of an acidic catalyst to obtain the polymeric surfactant; Wherein, C8~C 16 The molar ratio of fatty alcohol to propylene oxide is 1:1 to 100; The molar ratio of the propylene glycol monoalkyl ether to the epichlorohydrin is 1:1.1~1.5; The alkaline solution is a potassium hydroxide solution, sodium hydroxide solution, ammonia solution, sodium hypochlorite solution, sodium carbonate solution, or sodium bicarbonate solution, wherein the molar ratio of alkali to epichlorohydrin in the alkaline solution is 1~1.5:1; The reducing sugar is glucose and / or maltodextrin, and the molar ratio of the reducing sugar to the glycidyl glycol alkyl ether is 1~1.8:
1.
4. The preparation method according to claim 3, characterized in that, The alkali metal catalyst is an alkali metal hydroxide and / or an alkali metal C1-C4 alkoxide, preferably at least one of sodium methoxide, sodium ethoxide and potassium hydroxide. The amount of alkali metal catalyst added is C8~C 16 0.5~1.2wt% of fatty alcohols.
5. The preparation method according to claim 3, characterized in that, The phase transfer catalyst is tetrabutylammonium bromide and / or benzyltriethylammonium chloride; and / or The amount of the phase transfer catalyst added is 0.3~0.8 wt% of the total mass of the system.
6. The preparation method according to claim 3, characterized in that, The alkaline solution is a 40-50 wt% NaOH solution.
7. The preparation method according to claim 3, characterized in that, The acidic catalyst is p-toluenesulfonic acid and / or dodecylbenzenesulfonic acid; and / or, The amount of acidic catalyst added is 0.5~2.0 wt% of the reducing sugar.
8. The use of the polymeric surfactant according to claim 1 or 2 or the polymeric surfactant prepared by any one of claims 3 to 7 in the preparation of surface-active compositions.
9. A surface-active composition, characterized in that, Includes the polymeric surfactant as described in claim 1 or 2, or the polymeric surfactant prepared by any one of claims 3 to 7.
10. The application of the polymeric surfactant according to claim 1 or 2, the polymeric surfactant prepared by any one of claims 3 to 7, or the surface-active composition according to claim 9 in industrial hard surface cleaning, textile printing and dyeing auxiliaries, and pesticide emulsifiers.