A device for preparing textured layers of high-temperature superconducting double-sided tapes

By employing a thermal field control component and a winding and unwinding system in the high-temperature superconducting tape texture layer preparation device, multi-pass double-sided alternating deposition of the tape in a single deposition chamber was achieved, solving the problem of heat distribution asymmetry, improving the orientation consistency and uniformity of the texture layer, and enhancing preparation efficiency and product quality.

CN123108729APending Publication Date: 2026-11-17SONGSHAN LAKE MATERIALS LAB +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611610722.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-10-19
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In the preparation of double-sided textured layers of high-temperature superconducting tapes, the asymmetric heat distribution leads to a decrease in the uniformity of crystal orientation and fluctuations in texture stability, making it difficult to achieve continuous preparation of long tapes and uniformity of alternating deposition on both sides.

Method used

A high-temperature superconducting double-sided tape texture layer preparation device is adopted. By setting up a thermal field control component and a winding and unwinding system, the tape is deposited in multiple passes of alternating double-sided deposition in a single deposition chamber. By using the cooperation of the guide reversing wheel and the main reversing wheel, the front and back sides of the tape are repeatedly entered into the deposition zone under different thermal history conditions. The thermal field control component controls the temperature within a preset range to eliminate thermal asymmetry and local thermal history accumulation effects.

Benefits of technology

It improves the orientation consistency and overall uniformity of the double-sided texture, ensures the quality stability of the texture layer in the length and width directions of the strip, and improves the preparation efficiency and the yield of finished products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123108729A_ABST
    Figure CN123108729A_ABST
Patent Text Reader

Abstract

This invention discloses a high-temperature superconducting double-sided tape textured layer preparation apparatus, comprising a box, an ion beam assisted deposition system, and a take-up / unwinding system. The box defines a deposition chamber; the ion beam assisted deposition system forms a deposition zone; the take-up / unwinding system includes an unwinding reel, a guide reversing wheel, a main reversing wheel, and a take-up reel. The take-up / unwinding system is configured such that the tape, in the travel path between the unwinding and take-up reels, passes the guide reversing wheel at least once and the main reversing wheel at least twice, so that both sides of the tape pass through the deposition zone at least twice with an orientation towards the particle exit. The tape undergoes multiple passes of alternating double-sided deposition within a single, isothermal deposition zone, effectively improving the orientation consistency of the double-sided texture.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of superconducting material production technology, and in particular to a device for preparing a textured layer of a high-temperature superconducting double-sided tape. Background Technology

[0002] Ion beam assisted deposition (IBAD) is one of the main techniques for fabricating textured MgO layers in second-generation high-temperature superconducting tapes. This technique uses an auxiliary ion beam to bombard amorphous or non-textured substrates at a specific angle during deposition, causing the film to form a biaxial texture on the substrate, providing a template for the subsequent growth of transition and superconducting layers. To improve material utilization and reduce process costs, existing techniques have proposed double-sided or flip-side deposition structures, such as using a spiral-wound flip-side method or a cavity-based double-sided deposition method to achieve double-sided textured substrate fabrication, while combining multi-ion source structures to improve deposition efficiency and film uniformity.

[0003] Although the above technologies have improved the efficiency of texture preparation to some extent, the existing flipping or double-sided deposition paths are mostly single or limited deposition processes. Under the premise of continuous preparation of long strips and alternating deposition on both sides, the heat will increase along the strip due to the continuous action of the heat source. The front and back sections and the two sides of the strip are in different thermal histories. The cumulative effect of local thermal histories is difficult to balance and adjust in time, resulting in asymmetrical heat distribution, which directly leads to a decrease in crystal orientation consistency and fluctuation in texture stability. Summary of the Invention

[0004] The purpose of this invention is to provide a high-temperature superconducting double-sided tape textured layer preparation device, which can effectively improve the orientation consistency of the double-sided texture.

[0005] To achieve this objective, the present invention adopts the following technical solution: a high-temperature superconducting double-sided tape textured layer preparation device, comprising: a box, an ion beam assisted deposition system, and a take-up and unwinding system, wherein the box defines a deposition chamber; the ion beam assisted deposition system is installed in the deposition chamber, the ion beam assisted deposition system includes a particle beam generating component and a thermal field control component, the particle beam generating component and the thermal field control component are spaced apart to form a deposition zone through which the tape to be processed passes, the particle beam generating component has a particle outlet on one side facing the deposition zone for the particle beam to pass through, and the thermal field control component is used to adjust the temperature of the deposition zone; the take-up and unwinding system is installed in the deposition chamber, the take-up and unwinding system includes an unwinding reel, a guide reversing wheel, a main reversing wheel, and a take-up reel; wherein the take-up and unwinding system is configured such that the tape passes through the guide reversing wheel at least once and the main reversing wheel at least twice in the tape path between the unwinding reel and the take-up reel, so that both sides of the tape pass through the deposition zone at least twice in an orientation facing the particle outlet.

[0006] Preferably, the outer periphery of the guide reversing wheel is provided with at least one first reversing groove, and the outer periphery of the main reversing wheel is provided with one more second reversing groove than the number of the first reversing grooves. Both the first reversing groove and the second reversing groove are used to drive the strip to change direction.

[0007] Preferably, the winding and unwinding system further includes a first guide wheel and a second guide wheel symmetrically arranged on both sides of the deposition zone. The outer periphery of the first guide wheel and the second guide wheel is provided with a third reversing groove, which is twice the number of the second reversing groove. The strip in two adjacent third reversing grooves faces the particle outlet from different sides.

[0008] Preferably, the unwinding and rewinding system further includes a vertical guide wheel located below the guide reversing wheel. The vertical guide wheel is configured to guide the strip along a vertical direction. The inner wall of the deposition chamber is provided with a movable RHEED scanning probe, which is arranged facing the vertical strip to detect the deposition quality on both sides of the strip.

[0009] Preferably, the take-up and unwinding system further includes a tensioning wheel that abuts against the strip, the tensioning wheel being connected to an encoder; and / or, the tensioning wheel being able to adjust the tension of the strip by means of magnetic powder.

[0010] Preferably, the particle beam generating assembly includes a first support base, a target assembly, and an ion source assembly. The particle outlet is located on the top wall of the first support base. The first guide wheel and the second guide wheel are located on opposite sides of the top of the first support base. The first support base has a mounting cavity. The target assembly is mounted in the mounting cavity. The target assembly has a particle generating surface that is inclined toward the particle outlet. The ion source assembly is mounted on the housing and is horizontally arranged toward the particle generating surface.

[0011] Preferably, the top of the first support is provided with a plate, which is located above the particle generating surface, and the plate has the particle outlet.

[0012] Preferably, the top wall of the first support is provided with a protrusion, the protrusion including a horizontal top plate and two vertical side plates, the two side plates being connected to the two sides of the top plate respectively, the protrusion having a plurality of particle outlets corresponding one-to-one with the third reversing groove, the particle outlets penetrating the top plate and penetrating the two side plates, the strip passing through the particle outlets through the side plates and being flush with the top plate.

[0013] Preferably, the thermal field control component is configured as a radiation cooling mechanism or a gas cooling mechanism, and the distance between the thermal field control component and the strip is 3mm to 5mm in the vertical direction.

[0014] Preferably, the ion beam assisted deposition system further includes a temperature sensor, which is installed in the housing, with its detection end extending into the deposition area and located above the strip.

[0015] The beneficial effects of this invention are as follows: In the initial state, the strip is wound on the take-up and unwinding system with its front side facing down towards the particle outlet. When the preparation device is in use, the deposition chamber is evacuated, the ion beam-assisted deposition system is started and sputters a magnesium oxide particle beam, and the thermal field control component synchronously controls the reaction temperature of the deposition zone to a preset temperature. After the ion sputtering stabilizes, the take-up and unwinding system starts to move the strip. The strip first passes around the guide reversing wheel and passes through the deposition zone with its front side facing the particle outlet for a first front deposition. Then, the strip passes around the main reversing wheel and flips over, passing through the deposition zone with its back side facing the particle outlet for a first back deposition. Then, the strip passes around the guide reversing wheel and flips over a second time, repeating the above deposition steps, so that the front and back sides of the strip are deposited with magnesium oxide thin films at least twice towards the particle outlet. After the strip deposition is completed, it is wound into the take-up reel through the guide reversing wheel to complete the coating. By setting up a thermal field control component and a winding and unwinding system, the guide reversing wheel and the main reversing wheel work together to flip the front and back sides of the strip when it passes through the deposition zone twice in adjacent times in the strip path. This allows the strip to undergo multiple rounds of alternating double-sided deposition in a single deposition chamber, and the same strip area can be repeatedly entered into the deposition zone under different thermal history conditions. The thermal field control component controls the temperature of the deposition zone to remain constant within a low preset range, transforming the originally uncontrollable cumulative temperature rise of thermal history into controllable cyclic thermal processing. This ensures that the total thermal shock experienced by each segment of the strip tends to be consistent in the cumulative multiple depositions, eliminating the asymmetry of heat distribution and the local thermal history accumulation effect caused by single deposition or simple flipping. This effectively improves the orientation consistency of the double-sided texture and significantly enhances the uniformity of the texture layer in the length and width directions of the strip. Attached Figure Description

[0016] Figure 1 This is a schematic diagram of the high-temperature superconducting double-sided tape texture layer preparation device according to an embodiment of this application;

[0017] Figure 2 This is a schematic diagram of the particle outlet structure according to one embodiment of this application;

[0018] Figure 3 This is a schematic diagram of the particle outlet structure according to another embodiment of this application.

[0019] In the figure: 1. Box; 11. Deposition chamber; 111. Second support; 12. Movable RHEED scanning probe; 2. Ion beam assisted deposition system; 21. Particle beam generating assembly; 211. First support; 2111. Mounting cavity; 2112. Flat plate; 2113. Protrusion; 212. Target assembly; 2121. Particle generating surface; 2122. First main target; 2123. Second main target; 22. Deposition zone; 23. Particle outlet; 24. Temperature sensor; 241. Temperature display; 3. Unwinding and rewinding system; 31. Unwinding reel; 32. Guide reversing wheel; 33. First guide wheel; 331. Third reversing groove; 34. Second guide wheel; 35. Main reversing wheel; 36. Rewinding reel; 37. Vertical guide wheel; 38. Tensioning wheel; 4. Strip. Detailed Implementation

[0020] The present invention will now be described in further detail with reference to the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are merely illustrative of the invention and not intended to limit it. Furthermore, it should be noted that, for ease of description, the accompanying drawings show only the parts relevant to the present invention, and not all of the structures.

[0021] In the description of this invention, unless otherwise explicitly specified and limited, the terms "connected," "linked," and "fixed" should be interpreted broadly. For example, they can refer to a fixed connection, a detachable connection, or an integral part; they can refer to a mechanical connection or an electrical connection; they can refer to a direct connection or an indirect connection through an intermediate medium; they can refer to the internal communication of two components or the interaction between two components. Those skilled in the art can understand the specific meaning of the above terms in this invention based on the specific circumstances.

[0022] In this invention, unless otherwise explicitly specified and limited, "above" or "below" the second feature can include direct contact between the first and second features, or contact between the first and second features through another feature between them. Furthermore, "above," "over," and "on top" of the second feature includes the first feature directly above or diagonally above the second feature, or simply indicates that the first feature is at a higher horizontal level than the second feature. "Below," "below," and "under" the second feature includes the first feature directly below or diagonally below the second feature, or simply indicates that the first feature is at a lower horizontal level than the second feature.

[0023] In the description of this embodiment, the terms "upper," "lower," "right," etc., refer to the orientation or positional relationship shown in the accompanying drawings. They are used only for ease of description and simplification of operation, and do not indicate or imply that the device or element referred to must have a specific orientation, or be constructed and operated in a specific orientation. Therefore, they should not be construed as limitations on the present invention. In addition, the terms "first" and "second" are used only for distinction in description and have no special meaning.

[0024] Reference Figures 1 to 3 As shown, a high-temperature superconducting double-sided tape textured layer preparation device (hereinafter referred to as the preparation device) provided according to an embodiment of this application includes: a box 1, an ion beam assisted deposition system 2 and a winding and unwinding system 3. The box 1 defines a deposition chamber 11. Along a first direction, two chamber doors are provided and symmetrically connected to the two sides of the box 1. The chamber doors can be sealed to the box 1. Both chamber doors are used to open or close the deposition chamber 11. The inner wall of the deposition chamber 11 is also provided with a vacuum port, which is connected to an external mechanical pump group.

[0025] An ion beam-assisted deposition system 2 is installed in the deposition chamber 11. The ion beam-assisted deposition system 2 includes a particle beam generating component 21 and a thermal field control component. The particle beam generating component 21 and the thermal field control component are arranged opposite each other in the vertical direction. A deposition zone 22 is formed between the particle beam generating component 21 and the thermal field control component for the strip 4 to be processed to pass through. The particle beam generating component 21 has a particle outlet 23 on the side facing the deposition zone 22 for the particle beam to pass through. The thermal field control component is used to adjust the temperature of the deposition zone 22.

[0026] The unwinding and rewinding system 3 is installed in the sedimentation chamber 11. The unwinding and rewinding system 3 includes an unwinding reel 31, a guide reversing wheel 32, a main reversing wheel 35, and a rewinding reel 36. The unwinding reel 31 and the rewinding reel 36 are both connected to a drive motor. The guide reversing wheel 32 and the main reversing wheel 35 are respectively connected to a rotating shaft on the inner wall of the sedimentation chamber 11. After the strip 4 is drawn out from the unwinding reel 31, it passes around the guide reversing wheel 32 and the main reversing wheel 35 and then enters the rewinding reel 36. The strip 4 is in a horizontal position in the sedimentation zone 22. When the strip 4 passes around the main reversing wheel 35, it flips on both sides. The first direction and the second direction are two mutually perpendicular directions in the horizontal plane.

[0027] The preparation apparatus also includes a control system, which is connected to the ion source of the particle beam generating component 21, the thermal field control component, and the drive motor of the winding and unwinding system 3. The control system can be installed in the housing 1 or arranged remotely.

[0028] The unwinding and rewinding system 3 is configured such that the strip 4 passes through the guide reversing wheel 32 at least once and the main reversing wheel 35 at least twice in the belt path between the unwinding reel 31 and the rewinding reel 36, so that both sides of the strip 4 pass through the deposition zone 22 at least twice in an orientation toward the particle outlet 23.

[0029] In this embodiment, the strip 4 is a Hastelloy base strip or an iron-based alloy base strip. The side of the strip 4 facing the particle outlet 23 in its initial winding state is defined as the front side, and the other side as the back side. This is specifically stated to avoid misunderstanding. The control system can be a centralized or distributed controller. For example, the controller can be a single microcontroller or a combination of multiple distributed microcontrollers. The microcontroller can run a control program to control the particle beam generating component 21, the thermal field control component, and the winding / unwinding system 3 to achieve their functions.

[0030] Understandably, in the initial state, after the strip 4 is drawn out from the unwinding reel 31, it successively passes around the guide reversing wheel 32, the main reversing wheel 35, and finally around the take-up reel 36. The strip 4 repeatedly passes around the main reversing wheel 35 and the guide reversing wheel 32 between the unwinding reel 31 and the take-up reel 36. At this time, it is arranged with its front side facing down towards the particle outlet 23. When the preparation device is in use, the mechanical pump group is first started to generate negative pressure at the vacuum port, so that the deposition chamber 11 forms a 10 -4 A vacuum environment of approximately Pa is created, followed by the activation of the ion beam-assisted deposition system 2. The main ion source emits an ion beam to bombard the target and sputter out a particle beam (in this application, the ion beam is an Ar ion beam, the target is a magnesium oxide target, the particle beam generated on the target is a magnesium oxide particle beam, and a magnesium oxide thin film is deposited on the strip 4). The magnesium oxide particle beam passes through the particle outlet 23 and is deposited on the surface of the strip 4. At the same time, the auxiliary ion bombards the magnesium oxide thin film during deposition, and the thermal field control component synchronously controls the reaction temperature of the deposition zone 22 to the preset temperature. After the ion sputtering stabilizes, the unwinding and rewinding system 3 is started, and the strip 4 begins to move at a preset speed. The strip 4 first passes around the guide reversing wheel 32 in sequence, and passes through the deposition zone 22 with the front side facing the particle outlet 23 for the first front deposition. Then, the strip 4 passes around the main reversing wheel 35 for the first flip, and passes through the deposition zone 22 with the back side facing the particle outlet 23 for the first reverse deposition (the strip 4 undergoes two deposition passes in total). Then, the strip 4 passes around the guide reversing wheel 32 for the second flip and repeats the above deposition steps, so that the front and back sides of the strip 4 are deposited with magnesium oxide film at least twice with the particle outlet 23. After the deposition is completed, the strip 4 is wound into the take-up reel 36 through the guide reversing wheel 32 to complete the double-sided coating of the ultra-long strip 4.

[0031] By setting up a thermal field control component and a winding and unwinding system 3, the guide reversing wheel 32 and the main reversing wheel 35 cooperate to cause the front and back sides of the strip 4 to flip when it passes through the deposition zone 22 twice in adjacent times in the belt path. This allows the strip 4 to undergo multiple passes of alternating double-sided deposition within a single deposition zone 22, thereby enabling the same area of ​​the strip 4 to repeatedly enter the deposition zone 22 under different thermal history conditions. The temperature of the deposition zone 22 is kept constant within a low preset range under the control of the thermal field control component and does not change with the belt 4. This transforms the originally uncontrollable cumulative temperature rise due to thermal history into a stable and controllable cyclic thermal processing, ensuring that the total thermal shock experienced by each segment of the strip 4 in the cumulative multiple depositions tends to be consistent. This eliminates the asymmetry of heat distribution and the local thermal history accumulation effect caused by single deposition or simple flipping, thereby effectively improving the orientation consistency of the double-sided texture and significantly improving the uniformity of the texture layer in the length and width directions of the strip 4.

[0032] Reference Figure 1 and Figure 2 As shown, it can be understood that the outer periphery of the guide reversing wheel 32 is provided with guide grooves for guiding the movement of the strip 4 and at least one first reversing groove for guiding the strip 4 to change direction. The first reversing groove is located between two guide grooves. The outer periphery of the main reversing wheel 35 is provided with a second reversing groove, which is one more than the number of the first reversing grooves. Both the first and second reversing grooves are used to drive the strip 4 to change direction. After the strip 4 first passes around the second reversing groove on the main reversing wheel 35, it undergoes its first flip. In the subsequent belt path, it flips every time it passes through the first or second reversing groove. Therefore, the number of third reversing grooves 331 is twice the number of second reversing grooves. Since the strip 4 does not flip during the first frontal deposition, the number of second reversing grooves is set to be one more than the number of first reversing grooves, so that the number of flips is odd, ensuring that the number of depositions on both sides of the strip 4 is the same.

[0033] Understandably, by setting guide grooves, the guide grooves can provide lateral restraint before and after the strip 4 enters and exits the deposition zone 22, effectively preventing lateral slippage or deviation of the strip 4 during high-speed conveying, and improving the accuracy and repeatability of multi-pass conveying paths. By setting first and second reversing grooves, automatic alternating exposure of the front and back sides of the strip 4 can be achieved without the need for additional reversing mechanisms, simplifying the equipment structure and reducing layout costs.

[0034] Optionally, the winding and unwinding system 3 also includes a first guide wheel 33 and a second guide wheel 34 symmetrically arranged on both sides of the deposition zone 22. The outer periphery of the first guide wheel 33 and the outer periphery of the second guide wheel 34 are provided with a third reversing groove 331, which is twice the number of the second reversing grooves. The strip 4 in two adjacent third reversing grooves 331 faces the particle outlet 23 from different sides.

[0035] Before and after flipping, the strip 4 is guided through the deposition zone 22 by the adjacent third reversing groove 331, so that the strips 4 in each pass maintain a fixed spacing and relative position, avoiding mutual interference or obstruction between adjacent strips 4, and ensuring that the particle beam bombards the surface of the strip 4 uniformly and consistently during each deposition process.

[0036] In some preferred embodiments, the unwind reel 31 and the take-up reel 36 are spaced apart and positioned below the particle beam generating assembly 21. The guide reversing wheel 32 is located on the side of the unwind reel 31 away from the take-up reel 36 and below the first guide wheel 33. The main reversing wheel 35 is located on the side of the take-up reel 36 away from the unwind reel 31 and below the second guide wheel 34.

[0037] With the above arrangement, the strip 4 is led out from below and passes upward around the guide wheel assembly, making full use of the vertical space of the deposition chamber 11, shortening the overall length of the winding and unwinding system 3, minimizing the volume of the entire winding and unwinding system 3, constructing a complex multi-pass tape path within the limited deposition chamber 11, improving the integration and space utilization of the preparation device, and reducing the manufacturing cost and vacuuming time of the vacuum chamber.

[0038] Furthermore, the unwinding and rewinding system 3 also includes a vertical guide wheel 37, which is located below the guide reversing wheel 32. The vertical guide wheel 37 is configured so that the strip 4 travels vertically. Specifically, a second support base 111 is provided in the deposition chamber 11, and the vertical guide wheel 37 is installed on the second support base 111. On the travel path of the strip 4, the vertical guide wheel 37 is located between the guide reversing wheel 32 and the rewinding reel 36, and the line connecting the center of the vertical guide wheel 37 and the center of the guide reversing wheel 32 is perpendicular to the horizontal plane. After the strip 4 is deposited, it passes through the guide groove on the guide reversing wheel 32, the vertical guide wheel 37, and another guide groove on the guide reversing wheel 32 in sequence, and finally rewinds onto the rewinding reel 36. At this time, the guide reversing wheel 32 is provided with three guide grooves (one of which is used to guide the strip 4 out). The inner wall of the deposition chamber 11 is equipped with a movable RHEED (reflection high-energy electron diffraction) scanning probe 12, which is positioned facing the vertical strip 4 to detect the deposition quality on the surface of the strip 4. During the strip 4's movement, the control system automatically adjusts the electron beam emission angle of the movable RHEED scanning probe 12, thereby detecting the deposition quality on both sides of the strip 4 sequentially.

[0039] By setting up vertical guide wheels 37, the strip 4 forms a vertical detection area within the deposition chamber 11. The movable RHEED scanning probe 12 emits an electron beam horizontally toward the surface of the vertical strip 4. The electron beam bombards the surface of the vertical strip at an extremely small grazing angle, meeting the stringent requirements of RHEED for small-angle grazing incidence. This ensures that the movable RHEED scanning probe 12 acquires a high-resolution diffraction pattern, thereby enabling real-time and accurate characterization of the crystal structure, in-plane orientation, and surface flatness of the magnesium oxide texture layer on both sides of the strip 4. This facilitates accurate judgment of deposition quality by on-site personnel, timely adjustment of the process parameters of the ion beam assisted deposition system 2, and ensures a high yield of finished products.

[0040] Furthermore, the unwinding and take-up system 3 also includes two tensioning rollers 38 that abut against the strip 4. One tensioning roller 38 is connected to an encoder, or the tensioning roller 38 is connected to a magnetic powder adjustment device, thereby enabling the tension of the strip 4 to be adjusted by magnetic powder. Alternatively, the tensioning roller 38 is connected to both an encoder and a magnetic powder adjustment device, automatically adjusting the tension while recording the tape length. In this embodiment, there are two tensioning rollers 38. One tensioning roller 38 is located between the unwinding reel 31 and the guide reversing roller 32 to guide the unwinding reel 31 to lead out the strip 4, and the other tensioning roller 38 is located between the guide reversing roller 32 and the take-up reel 36 to guide the take-up reel 36 to retract the strip 4. One tensioning roller 38 has an encoder, and the other is connected to a magnetic powder adjustment device.

[0041] By setting tensioning wheel 38, the tensioning wheel 38 presses the strip 4 before and after the strip 4 is taken in and out, so that the strip 4 can enter and exit the deposition zone 22 at a smooth angle in the belt path, avoiding mechanical damage to the strip 4 caused by sharp turns or large-angle reversals, and ensuring the surface quality of the texture layer.

[0042] By setting an encoder, the encoder detects the rotational speed of the tension wheel 38 in real time. This rotational speed corresponds precisely to the belt feed speed of the strip 4. The control system can accurately calculate the belt feed length of the strip 4 through the speed signal fed back by the encoder. When the speed deviates from the set value, it can be compensated immediately by adjusting the rotational speed of the drive motors of the unwinding reel 31 and the take-up reel 36 to ensure a constant belt feed speed, thereby avoiding uneven deposition thickness caused by speed fluctuations.

[0043] The winding and unwinding system 3 has a built-in pressure sensor that can detect the pressure of the strip 4 in real time (the pressure is positively correlated with the tension of the strip 4). The control system judges the current tension state of the strip 4 in real time based on the feedback signal of the pressure sensor. When the tension deviates from the set value, the tensioning wheel 38 adjusts the tension of the strip 4 through magnetic powder to ensure that the tension of the strip 4 is constant during the belt running process. This avoids changes in the elongation of the strip 4 and the drift of the deposition zone 22 caused by tension fluctuations, ensuring the consistency of deposition conditions in each pass and further improving the uniformity of the texture layer in the long strip length direction.

[0044] Continue to refer to Figure 1 As shown, the particle beam generating assembly 21 includes a first support 211, a target assembly 212, and an ion source assembly. The particle outlet 23 is located on the top wall of the first support 211. The first guide wheel 33 and the second guide wheel 34 are located on opposite sides of the top of the first support 211. The first support 211 has a mounting cavity 2111, in which the target assembly 212 is mounted. The target assembly 212 has a particle generating surface 2121, which is inclined at 30°-60° towards the particle outlet 23. The ion source assembly is mounted on the housing 1 and horizontally oriented towards the particle generating surface 2121. The inner wall of the deposition chamber 11 is also provided with an auxiliary ion source inclined towards the strip 4 to allow selective growth of grains in a preset direction, ensuring the deposition of a biaxially textured magnesium oxide layer on both sides of the strip.

[0045] The target assembly 212 is integrated inside the first support 211, making the structure of the entire particle beam generating assembly 21 more compact. The particle generating surface 2121 is tilted at 30°-60° towards the particle outlet 23. The particle beam generated by the horizontally emitted ion beam from the ion source assembly bombarding the target surface is directed vertically towards the surface of the strip 4 in the deposition region 22, maximizing the sputtered particle beam yield of target molecules under ion beam bombardment in the vertical direction and improving the deposition rate of magnesium oxide thin film.

[0046] Specifically, in this application, two mounting cavities 2111 are provided, separated by the same partition. Each mounting cavity 2111 has openings on both sides in a first direction. The target assembly 212 includes a first main target 2122 and a second main target 2123, respectively fixed within the two mounting cavities 2111. Both the first and second main targets 2122 and 2123 have particle generating surfaces 2121, arranged in opposite directions such that the included angle between the two particle generating surfaces 2121 is 60°-120°. The ion source assembly includes a first main ion source facing the particle generating surface 2121 of the first main target 2122 and a second main ion source facing the particle generating surface 2121 of the second main target 2123. The first and second main ion sources are respectively mounted on the cavity doors on both sides of the housing 1. Furthermore, auxiliary ion sources inclined at 45° towards the strip 4 are also provided on the cavity doors on both sides.

[0047] Specifically, the first main ion source horizontally bombards the 30°-60° tilted particle generating surface 2121 of the first main target 2122, and the second main ion source horizontally bombards the 30°-60° tilted particle generating surface 2121 of the second main target 2123, simultaneously generating a magnesium oxide sputtering particle beam required for deposition. The magnesium oxide particles fly towards the surface of the strip 4 with high kinetic energy, forming a dense and uniform magnesium oxide thin film base layer, ensuring the film coverage and thickness. The first main target 2122 and the second main target 2123 work together to simultaneously generate magnesium oxide particle beams and deposit them in different regions of the strip 4, significantly improving the magnesium oxide layer deposition rate and increasing production efficiency. The auxiliary ion source bombards the surface of the strip 4 within the deposition area 22 with a 45° ion beam tilt. The auxiliary ion beam selectively etches and transfers energy to the growing film, resulting in the growth of grains with only c-axis orientation, thus forming a texture with consistent in-plane and out-of-plane heights.

[0048] By setting up a first main target 2122, a second main target 2123, a first main ion source, a second main ion source, and two auxiliary ion sources, the deposition function and the texture control function are decoupled while accelerating the formation of the texture layer. This allows for independent control of the deposition rate and texture quality. Operators can adjust the power, beam density, and working pressure of the first main ion source, the second main ion source, the first auxiliary ion source, and the second auxiliary ion source according to actual process requirements. This improves the controllability and repeatability of deposition, ensuring optimal texture quality while maintaining deposition efficiency.

[0049] Since the side of strip 4 facing away from particle outlet 23 is the surface of the thermal field control component, when the auxiliary ion source is tilted towards strip 4, some high-energy ions may collide with the surface of the thermal field control component, causing secondary sputtering and affecting the other side of strip 4 where a magnesium oxide film has not yet been deposited (in the case of multiple passes, it will affect the quality of the magnesium oxide film already deposited on the other side of strip 4). Existing particle beam control methods mostly use fixed-angle incident or simple shielding structures, which have limited ability to suppress particle beams at non-primary incident angles, resulting in the uniformity of film crystal orientation still being affected. In single-sided deposition, the impact of secondary sputtering of the particle beam is not significant, but in long strip double-sided film deposition, secondary sputtering of ions has a great impact on the texture of the currently non-deposited surface.

[0050] Reference Figure 2 As shown, in some embodiments, the top of the first support 211 is provided with two flat plates 2112, which are located above the first main target 2122 and the second main target 2123, respectively, and the two flat plates 2112 are respectively provided with particle outlets 23.

[0051] By setting up the plate 2112, the secondary sputtering of high-energy particles and the scattering of sputtered particles can be restricted. The shape and size of the particle outlet 23 on the plate 2112 can be customized for actual production. By geometrically constraining the particle outlet 23, the space of the ion beam and sputtered particle beam is restricted. This ensures that only a portion of the high-energy ions emitted from the auxiliary ion source, the first main target 2122, and the sputtered particles generated by the bombardment of the main ion source ion beam by the second main target 2123 can reach the deposition area 22 to participate in film growth. The remaining ions and particles are blocked by the plate 2112 and deposited on the lower surface of the plate 2112. This effectively controls the boundary and range of the deposition area 22, avoids contamination of non-target areas of the strip 4 and uneven film thickness, and makes the distribution of the particle beam on the surface of the strip 4 more uniform.

[0052] Reference Figure 3 As shown, in some embodiments, the top wall of the first support 211 is provided with two protrusions 2113. The protrusions 2113 include a horizontal top plate and two vertical side plates. The two side plates are arranged at intervals along the second direction and are respectively connected to the two sides of the top plate. Each protrusion 2113 is provided with multiple particle outlets 23 corresponding to the third reversing groove 331. The particle outlets 23 penetrate the top plate and the two side plates. The strip 4 passes through the side plates through the particle outlets 23 and is flush with the top plate.

[0053] By setting the protrusion 2113, on the one hand, after the strip 4 passes through the particle outlet 23, it is flush with the top plate of the protrusion 2113, so that the strip 4 is on the same horizontal plane in the deposition zone 22. This ensures that the vertical distance between the strip 4 and the particle outlet 23 is consistent in each pass, avoiding the difference in deposition rate and bombardment angle caused by the difference in the height of the strip 4, and further improving the uniformity of multi-pass deposition. On the other hand, the top plate and side plate of the protrusion 2113 together form a spatial constraint structure for the ion beam and sputtered particles, so that the ion beam and sputtered particles can only reach the surface of the strip 4 through the particle outlet 23, and cannot hit the surface of the thermal field control component to cause secondary sputtering. This effectively suppresses the radiation and deposition of the ion beam and sputtered particles in non-target areas, effectively blocks the magnesium oxide film on the side of the strip 4 away from the particle outlet 23 from particle defects caused by secondary sputtering of the ion beam, improves the density and purity of the texture layer, and is beneficial to the subsequent epitaxial growth of the superconducting layer. In addition, the multiple particle outlets 23 and multiple third reversing grooves 331 on the protrusion 2113 cooperate with each other to provide precise lateral guidance and positioning for the multi-pass strip 4, ensuring that each pass strip 4 maintains a fixed spacing and posture within the deposition zone 22, avoiding deposition position deviation caused by strip offset, and ensuring the consistency of the texture of each pass under multi-pass deposition conditions.

[0054] The contact cooling method of single-sided deposition may introduce mechanical disturbances such as friction during the thermal management process, which may damage the film surface. At the same time, it is difficult to achieve fine temperature control on the spatial scale of the deposition zone, thus limiting the stable structure formed by particle beam deposition.

[0055] In this application, the thermal field control component is configured as a radiation cooling mechanism or a gas cooling mechanism, and the distance between the thermal field control component and the strip 4 in the vertical direction is 3mm to 5mm.

[0056] The radiation cooling mechanism can quickly remove the heat accumulated in the strip 4 during the deposition process through radiation heat transfer, while the gas cooling mechanism can quickly remove the heat accumulated in the strip 4 during the deposition process through convection heat transfer. Regardless of whether a radiation cooling mechanism or a gas cooling mechanism is set, the heat accumulation effect during the continuous deposition process can be effectively suppressed without contacting the strip 4, and the temperature on the strip is kept low and within an acceptable temperature fluctuation range. It can also eliminate the risk of mechanical damage to the texture layer caused by friction or extrusion from the root, and ensure the structural integrity and crystal orientation stability of the texture layer.

[0057] Setting the distance between the radiating surface or air outlet of the thermal field control component and the strip 4 to 3mm to 5mm can avoid gas friction that may be caused by too small a distance, and provide sufficient tolerance for mechanical tolerance, thermal expansion and error margin of the strip path; at the same time, it can avoid temperature difference between the center and edge of the strip 4 that may be caused by too large a distance, and ensure that each point in the width direction of the strip 4 can exchange heat efficiently with radiation or convection, further suppressing the heat accumulation effect and avoiding texture degradation.

[0058] In some embodiments, the ion beam assisted deposition system 2 further includes a temperature sensor 24, which is mounted on the housing 1 and connected to the control system signal. The detection end of the temperature sensor 24 extends into the deposition zone 22 and is located above the strip 4. Preferably, the temperature sensor 24 is also connected to a temperature display, which is fixed to the outer wall of the housing 1 so that the operator can view the temperature of the deposition zone 22 in real time.

[0059] By setting temperature sensor 24, temperature sensor 24 can collect temperature data of the surface of strip 4 in real time, providing accurate feedback signals for the closed-loop control of thermal field control components. The control system can adjust the temperature, flow rate or gas flow rate of cooling fluid in real time according to the feedback of temperature sensor 24, so that the temperature fluctuation of deposition zone 22 is controlled within ±5℃, ensuring that the texture layer grows in a stable temperature window and avoiding texture degradation caused by temperature drift.

[0060] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the implementation of the present invention. Those skilled in the art will be able to make various obvious changes, readjustments, and substitutions without departing from the scope of protection of the present invention. It is neither necessary nor possible to exhaustively describe all embodiments here. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention should be included within the scope of protection of the claims of the present invention.

Claims

1. A high temperature superconducting bi-tape texture layer preparation apparatus, characterized in that, include: The box (1) defines a sedimentation chamber (11) inside; An ion beam-assisted deposition system (2) is installed in the deposition chamber (11). The ion beam-assisted deposition system (2) includes a particle beam generating component (21) and a thermal field control component. The particle beam generating component (21) and the thermal field control component are spaced apart to form a deposition zone (22) through which the strip (4) to be processed passes. The particle beam generating component (21) has a particle outlet (23) on the side facing the deposition zone (22) for the particle beam to pass through. The thermal field control component is used to adjust the temperature of the deposition zone (22). The unwinding and rewinding system (3) is installed in the deposition chamber (11). The unwinding and rewinding system (3) includes an unwinding reel (31), a guide reversing wheel (32), a main reversing wheel (35), and a rewinding reel (36). The unwinding and rewinding system (3) is configured such that the strip (4) passes through the guide reversing wheel (32) at least once and the main reversing wheel (35) at least twice in the belt path between the unwinding reel (31) and the rewinding reel (36), so that both sides of the strip (4) pass through the deposition zone (22) at least twice in a posture toward the particle outlet (23).

2. The high temperature superconducting bi-tape texture layer preparation apparatus of claim 1, wherein, The outer periphery of the guide reversing wheel (32) is provided with at least one first reversing groove, and the outer periphery of the main reversing wheel (35) is provided with one more second reversing groove than the number of the first reversing grooves. Both the first reversing groove and the second reversing groove are used to drive the strip (4) to change direction.

3. The high temperature superconducting bi-tape texture layer preparation apparatus of claim 2, wherein, The winding and unwinding system (3) further includes a first guide wheel (33) and a second guide wheel (34) symmetrically arranged on both sides of the deposition zone (22). The outer periphery of the first guide wheel (33) and the second guide wheel (34) is provided with a third reversing groove (331) twice the number of the second reversing grooves. The strip (4) in two adjacent third reversing grooves (331) faces the particle outlet (23) from different sides.

4. The high temperature superconducting bi-tape texture layer preparation apparatus according to claim 2 or 3, characterized in that, The winding and unwinding system (3) also includes a vertical guide wheel (37) located below the guide reversing wheel (32). The vertical guide wheel (37) is configured to guide the strip (4) to travel vertically. The inner wall of the deposition chamber (11) is provided with a movable RHEED scanning probe (12). The movable RHEED scanning probe (12) is arranged facing the vertical strip (4) to detect the deposition quality on both sides of the strip (4).

5. The high temperature superconducting bi-tape texture layer preparation apparatus according to claim 2 or 3, characterized in that, The winding and unwinding system (3) further includes a tensioning wheel (38) that abuts against the strip (4), the tensioning wheel (38) being connected to an encoder; and / or, the tensioning wheel (38) adjusting the tension of the strip (4) by means of magnetic powder.

6. The high temperature superconducting bi-tape texture layer preparation apparatus of claim 3, wherein, The particle beam generating assembly (21) includes a first support base (211), a target assembly (212), and an ion source assembly. The particle outlet (23) is located on the top wall of the first support base (211). The first guide wheel (33) and the second guide wheel (34) are located on both sides of the top of the first support base (211). The first support base (211) is provided with a mounting cavity (2111). The target assembly (212) is installed in the mounting cavity (2111). The target assembly (212) has a particle generating surface (2121). The particle generating surface (2121) is inclined toward the particle outlet (23). The ion source assembly is installed in the housing (1) and is horizontally arranged toward the particle generating surface (2121).

7. The high temperature superconducting bi-tape texture layer preparation apparatus of claim 6, wherein, The first support base (211) has a plate (2112) on its top, the plate (2112) is located above the particle generating surface (2121), and the plate (2112) has the particle outlet (23).

8. The high temperature superconducting bi-tape texture layer preparation apparatus of claim 6, wherein, The top wall of the first support base (211) is provided with a protrusion (2113), the protrusion (2113) includes a horizontal top plate and two vertical side plates, the two side plates are respectively connected to the two sides of the top plate, the protrusion (2113) is provided with a plurality of particle outlets (23) corresponding one-to-one with the third reversing groove (331), the particle outlets (23) penetrate the top plate and penetrate the two side plates, the strip (4) passes through the side plates through the particle outlets (23) and is flush with the top plate.

9. The high temperature superconducting bi-tape texture layer preparation apparatus of claim 1, wherein, The thermal field control component is configured as a radiation cooling mechanism or a gas cooling mechanism, and the distance between the thermal field control component and the strip (4) in the vertical direction is 3mm to 5mm.

10. The high temperature superconducting bi-tape texture layer preparation apparatus according to claim 1 or 9, characterized in that, The ion beam assisted deposition system (2) also includes a temperature sensor (24), which is installed in the housing (1). The detection end of the temperature sensor (24) extends into the deposition area (22) and is located above the strip (4).