A method for designing wet hot pressing process parameters for lithium-ion batteries
By calculating the process parameters of lithium-ion batteries using wet hot-pressing, rheological, and wetting models, the problem of lack of theoretical guidance for parameter design in existing technologies is solved, thereby improving the interfacial bonding force of the cells and the stability of battery performance.
Patent Information
- Application Number
- CN202611102626.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-07-23
- Publication Date
- 2026-11-17
AI Technical Summary
The existing wet hot pressing process parameters for lithium-ion batteries lack theoretical guidance, resulting in insufficient interfacial bonding, which affects cell performance and safety. Furthermore, the parameters have poor adaptability and cannot be adapted to different material systems.
By using wet hot pressing, rheological, and wetting models, combined with the swelling kinetics of the adhesive material in the electrolyte, suitable process parameters, including temperature, time, and pressure windows, are calculated to ensure effective bonding between the adhesive layer and the electrode.
It improves cell consistency and performance, ensures interface bonding, shortens process time, and enhances battery safety and cycle life.
Smart Images

Figure CN123116548A_ABST
Abstract
Description
Technical Field
[0001] This invention belongs to the field of lithium-ion battery technology, and more specifically, this invention relates to a method for designing wet hot pressing process parameters for lithium-ion batteries. Background Technology
[0002] With the increase in battery cell energy density, the material system has undergone significant changes. Currently, the high-capacity, high-nickel ternary cathode system matched with CVD silicon-carbon anode is developing most rapidly. High-nickel ternary materials are sensitive to moisture and prone to lattice distortion during cycling. Furthermore, silicon anode materials exhibit significant volume expansion during charge and discharge. If the adhesion between the electrode and separator interface is insufficient, the electrode is prone to wrinkling and warping, leading to a sharp decline in subsequent cycle performance. In addition, the microscopic unevenness of the high-area-density electrode surface results in extremely slow electrolyte wetting of the micropores inside the electrode after traditional room-temperature electrolyte injection. Poor wetting leads to prolonged lithium-ion transport paths and increased risk of lithium plating. Therefore, using a coated separator to improve the adhesion between the separator and the positive and negative electrodes after electrolyte injection, shorten the lithium-ion migration path, and reduce interfacial charge transfer resistance is crucial for the high-rate charge and discharge performance of high-energy-density batteries. Therefore, hot pressing of the cell after electrolyte injection can force the construction of a stable, uniform, and dense interface environment, which can ensure the first efficiency, cycle life, and safety of the high-energy-density cell, and lay a solid foundation for thousands of subsequent cycles.
[0003] Current technologies focus more on hot-press bonding in the dry cell state. However, during hot-pressing of cells after electrolyte injection, the main driving force for the adhesive layer filling the pores changes from pressure-driven viscous flow to capillary force-driven spontaneous wetting and bonding of the adhesive layer. Both the electrode pores and the adhesive layer surface are filled with electrolyte, forming a solid-liquid-solid three-phase interface. The electrolyte generates capillary action in the micropores, which can either assist the adhesive in being drawn into the pores (when wettability is good) or hinder filling (when wettability is poor). The viscosity of the adhesive layer decreases significantly due to swelling, and the flow resistance is significantly reduced. The adhesive layer material partially swells or dissolves in the electrolyte, diffusing with the electrode binder rather than through simple physical interlocking. Furthermore, if the adhesive layer material swells excessively during hot pressing after electrolyte injection due to prolonged hot pressing time or excessively high temperature, it can easily lead to excessive dilution of the polymer network and a sharp decrease in the cohesive strength of the adhesive layer itself. When the adhesive layer dissolves, the dissolved polymer chains may migrate into the pores of the separator and redeposit, blocking lithium-ion channels and causing a surge in battery internal resistance. Therefore, constructing a wet hot pressing process window is of great guiding significance for hot pressing of high-energy-density systems after electrolyte injection. CN103996877A describes the performance of pressing by specifying the temperature, pressure, and time range for hot and cold pressing of the battery cell after electrolyte injection.
[0004] The aforementioned methods, by providing only empirical parameters for temperature ranges, are biased towards experience and offer no guidance for process windows. Furthermore, they are unsuitable for applications with different numbers of layers and different adhesive layer materials. Designing based on empirical parameters presents the following problems: if the parameters are too low, the binder may not fully diffuse to the electrode surface and interdiffused with the electrode binder at the molecular level, resulting in poor interfacial bonding and affecting cell performance. If the parameters are too high, excessive swelling or even partial dissolution of the polymer on the adhesive layer surface can occur, clogging pores and affecting the cell's internal resistance and ion transport. This invention discloses a method for designing wet hot-pressing process parameters for lithium-ion batteries. Based on a given material system, it analyzes the system's characteristics and uses the thermophysical parameters of the wet positive and negative electrodes and the adhesive separator material as a foundation. Combining the swelling kinetics and wet rheology of the adhesive layer material in the electrolyte, it calculates matching wet process parameters using a wet thermo-rheological-wetting model. It provides a complete wet hot-pressing calculation example, including all input parameters, intermediate calculation results, and final output process parameters, improving cell consistency and final performance. Summary of the Invention
[0005] One object of the present invention is to solve at least the above-mentioned problems and / or defects, and to provide at least the advantages described below.
[0006] To achieve these objectives and other advantages according to the present invention, a method for designing wet hot pressing process parameters for lithium-ion batteries is provided, comprising the following steps: S1. Collect the specific heat capacity, density, thickness and thermal conductivity of the coated diaphragm, positive electrode, negative electrode, positive current collector and negative current collector in the electrolyte wetted state. S2. The process window for wet hot pressing is calculated sequentially using the wet adhesive layer interface temperature thermal model, wet rheological model, and wet wetting model, specifically including: S21. Calculate the temperature history of the interface of the adhesive layer inside the cell after liquid injection using the wet adhesive layer interface temperature thermal model, determine the heating time required for the adhesive layer to reach the target activation temperature, and obtain the temperature process window. S22. By combining the swelling kinetics of the adhesive layer in the electrolyte, the gel content of the adhesive layer and the wet rheological properties, a wet rheological model is established, the effective viscosity of the adhesive layer at the target temperature is calculated, the holding time required to ensure the interpenetration bonding between the adhesive layer and the electrode adhesive is determined, and the minimum total hot-pressing time window is obtained by combining the heating time. S23. Based on the capillary effect under wet force, establish a wet wetting model, calculate the minimum external pressure process window required to ensure that the adhesive layer fills the pores on the surface of the positive and negative electrode sheets within the holding pressure time, and obtain the hot pressing pressure window by combining the upper limit of the material's compressive strength. S3. Based on the obtained process window, prepare small sample cells for wet hot pressing verification. Use electrode peel strength as the core indicator to verify the accuracy of the model. Adjust the process parameters and iteratively calculate according to the verification results to finally obtain the wet hot pressing process parameters that are suitable for the target material system.
[0007] Preferably, in step S1, the active material in the positive electrode sheet is one or more of single crystal, polycrystalline, or monocrystalline / polycrystalline materials; the surface capacity of the positive electrode sheet is 4~7 mAh / cm². 2 The ratio of the negative electrode surface area capacity to the positive electrode surface area capacity is 1.03~1.15; the active material of the negative electrode is one or more of graphite or silicon carbide materials; The adhesive-coated diaphragm is made of polyethylene or polypropylene, and the coating is one or more of adhesive coating or ceramic adhesive coating. The adhesive layer facing the positive electrode side includes one or more of poly(vinylidene fluoride-hexafluoropropylene) and polyvinylidene fluoride; The adhesive layer facing the negative electrode side includes one or more of polyacrylic acid and lithium polyacrylate that are interpenetrating with sodium carboxymethyl cellulose, a negative electrode binder, and polyimide, polyurethane / polyacrylonitrile, and styrene-butadiene rubber that are interpenetrating with polyacrylic acid, a negative electrode binder. The adhesive layer is applied by one or more of the following methods: spraying, dot coating, and roller coating.
[0008] Preferably, in S1, the specific heat capacity of the coated separator, positive electrode, negative electrode, positive current collector, and negative current collector in the electrolyte-wetted state is... C p Obtained by DSC measurement; Thermal conductivity of the coated separator, positive electrode, negative electrode, positive current collector, and negative current collector in the electrolyte-wetted state k The thermal conductivity is obtained by laser flare test and calculated using the formula "thermal conductivity = thermal diffusivity × specific heat capacity × bulk density"; The density of the coated separator, positive electrode material, negative electrode material, positive current collector, and negative current collector under electrolyte wetting. r Density after the porosity is fully filled, thickness d The thickness of the materials in each part of a lithium-ion battery.
[0009] Preferably, in step S21, the adhesive layer interface temperature is... T interface The thermal model prediction is based on the temperature history of heat transfer from the hot press plate to the interface of the adhesive layer at the center of the cell under liquid injection conditions. T wet interface ( t This allows for the determination of the hot-pressing time required to reach the target activation temperature; based on the wet physical properties of each layer, the wet thermal resistance of each layer is calculated. Rwet th,i =d i / k wet i With wet heat capacity C wet th,i : C wet th,i = r wet i C wet p,i d i Based on the number of cell layers n Calculate the total thermal resistance ∑ from the hot press plate to the interface of the adhesive layer at the center of the battery cell. i ( R wet th,i ) and total heat capacity ∑ i ( C wet th,i The wet characteristic time constant was obtained. t wet : t wet = α wet 2∑ i ( R wet th,i )∑ i ( C wet th,i ) α wet As a specific correction factor, since heat is transferred from both sides to the center, a temperature gradient exists, therefore it is introduced. α wet Make corrections; Using the temperature history formula: T wet interface ( t ) =T 0 + ( T p -T 0)[1 - exp( -t / t wet )] Predict the change in adhesive layer interface temperature over time and calculate the target activation temperature of the adhesive layer interface. T wet target Time required t , T wet interface ( t )for t The temperature of the adhesive layer interface at any given time. T 0 is the starting temperature. T p Set the temperature for the hot press plate.
[0010] Preferably, the specific correction factor α wet The method, derived through experimental fitting, includes: fabricating a thin-layer battery cell and implanting a thermocouple at the interface of the central adhesive layer; performing hot pressing under low-pressure conditions after electrolyte injection; collecting data on the change of interface temperature over time; and obtaining the characteristic time through linear regression fitting. t Then, using the following formula: α wet = 2τ / [∑ i ( R th,i )∑ i ( C th,i )] Back-reaming to obtain a specific correction factor α wet .
[0011] Preferably, the hot press plate is set to a specific temperature. T p Target activation temperature T wet target The wet glass transition temperature of the adhesive layer after swelling equilibrium T wet g and wet melting point T wet m Sure, T wet g and T wet m The target activation temperature was obtained by DSC testing of the adhesive layer after swelling equilibrium. T wet target Compare T wet g or Twet m The temperature of the hot press plate is set at 5~15℃. T p Compare T wet target The temperature ranges from 5°C to 25°C; within a limited hot-pressing time, the process of transferring heat from the hot-press plate to the internal adhesive layer interface must overcome the temperature drop caused by the thermal resistance of the multi-layer materials and not affect the overall performance. T wet interface Reach quickly T wet target .
[0012] Preferably, in step S22, the swelling kinetics are obtained by the following method: immersing the adhesive sample in an excess electrolyte, placing it in a constant temperature environment, removing it periodically, quickly drying the surface, and weighing it. m ( t Record the time for mass to remain constant. t With quality m To measure the weight and time at different times, use the following formula: SD ( t , T )= SD ∞ ( T )[1 - exp( -t / t swell ( T ))] The equilibrium swelling degree was obtained by fitting. SD ∞ ( T and swelling characteristic time t swell ( T ), where SD ( t , T )for t The swelling degree of the adhesive layer at any given time is calculated as follows: SD ( t,T ) = ( m(t)-m 0 ) / m 0 , m 0 This represents the initial sample mass of the adhesive layer.
[0013] Preferably, in step S23, the gel content of the adhesive layer is... GC The residue weight was obtained by Soxhlet extraction, specifically by placing the swollen gel layer into a Soxhlet extractor.m after ,use GC =( m after / m 0 Calculate by multiplying 100%. m 0 The initial sample mass of the gel layer, and the gel content of the gel layer. GC The lower the value, the more severe the dissolution of the adhesive layer and the less stable the structure. The gel content of the adhesive layer should be ≥70% to avoid excessive dissolution of the adhesive layer, which could lead to negative effects. In step S22, the specific method for establishing the wet rheological model includes: immersing the gel disc sample in a rheometer solvent cup containing electrolyte, changing the temperature, and measuring the change in sample viscosity over time at a fixed temperature. or ( t ), through the Arrhenius equation or ( T,t ) = A·exp ( E a / RT The activation energy under wet conditions was obtained by fitting. E a wet and pre-finger factor A wet ; By correlating swelling degree with viscosity, a wet rheological model is constructed: or eff ( T,t ) =h 0 ( T )exp( -k s SD ( t )) The sensitivity of the viscosity of the quantified adhesive layer to the decrease with increasing swelling degree after absorbing electrolyte is expressed by the formula. or 0 ( T ) represents temperature T The dry reference viscosity of the lower adhesive layer is the viscosity at which it swells. k s The swelling attenuation constant is SD ( t )for t The degree of swelling at any given time; Holding time after the adhesive layer reaches the target activation temperature t dwell The minimum total hot pressing time is 10~300s. t wet min =t 1+ t dwell ,in t 1 represents the heating time required for the adhesive layer interface to reach the target activation temperature.
[0014] Preferably, in step S22, the wet wetting model is obtained by calculating the dry pressure driving term and the capillary force term. The dry pressure driving model is as follows: P base min =η(T wet interface ) R a 2 / ( t wet dwell h g 2 ) in P base min This is the minimum pressure window for the upper and lower hot platens. or ( T wet interface (The adhesive layer is on the bottom) T wet interface Viscosity R a The surface roughness of the electrode is measured using a roughness tester. t wet dwell For the pressure holding time, h g This refers to the thickness of the adhesive layer. Calculation of capillary force using the Young-Laplace equation P cap : P cap =2c LV cos θ / r pore In the formula c LV For the surface tension of the electrolyte, i Contact angle, r pore The average radius of the pores on the electrode surface; Will P base min and P capSubtraction yields the wet wetting model: P wet min = P base min - P cap in P wet min This is the minimum thermal pressure under wet conditions; The upper pressure limit is determined by combining the compressive strength of the diaphragm substrate and the electrode. P max The hot-pressing pressure window is obtained. P wet min ≤ P ≤ P max , P This refers to the pressure applied during hot pressing.
[0015] Preferably, in step S3, the peel strength is obtained using a tensile testing machine. Based on the temperature process window, minimum total hot-pressing time window, minimum applied pressure process window, and hot-pressing pressure window, within the process window range of wet hot pressing, prioritizing increasing the set temperature of the hot-pressing plate while ensuring higher peel strength. T p With hot pressing pressure P shorten the total hot pressing time t Improve process efficiency; Minimum electrode peel strength σ min The target activation temperature is 1 N / m. If the peel strength is not up to standard, adjust the target activation temperature of the adhesive layer according to the interpenetration state of the adhesive layers. T wet target Or holding time t wet dwell Return to S2 to recalculate the process window and iterate to verify.
[0016] The present invention has at least the following beneficial effects: Following the method described in this application, based on the thermophysical parameters of the wet material and combined with the swelling kinetics and wet rheological characteristics of the adhesive layer material in the electrolyte, matching wet process parameters are calculated using a wet rheology-wetting model. This provides a complete example of wet hot pressing calculations, realizing the transformation from "empirical adjustment" to "theoretical design." It includes all input parameters, intermediate calculation results, and final output process parameters, improving cell consistency and final performance.
[0017] In a multivariable, strongly coupled system, this invention constructs the relationship between the cell pressing temperature, time, and pressure process windows after liquid injection. Through a wet thermal model → wet rheological model → wet wetting model → verification iterative process, it strives to find the global optimal solution, providing theoretical guidance for the optimization of wet hot pressing parameters.
[0018] Other advantages, objectives and features of the present invention will become apparent in part from the following description, and in part from those skilled in the art through study and practice of the invention. Attached Figure Description
[0019] Figure 1 A schematic flowchart illustrating the method for designing wet hot pressing process parameters for lithium-ion batteries provided by this invention. Detailed Implementation
[0020] The present invention will now be described in further detail with reference to the accompanying drawings, so that those skilled in the art can implement it based on the description.
[0021] It should be understood that terms such as “having,” “comprising,” and “including” as used herein do not exclude the presence or addition of one or more other elements or combinations thereof. Example: like Figure 1 As shown, a method for designing process parameters for wet hot pressing of lithium-ion batteries includes the following steps: S1. Use DSC to test the glass transition temperature T of the wet coating material. wet g and melting point information T wet m The specific heat capacity of materials such as the coated separator, positive electrode material, negative electrode material, positive current collector, and negative current collector in the electrolyte-wet state of a battery. C p The thermal conductivity of the coated separator, positive electrode material, negative electrode material, positive current collector, and negative current collector was tested using the laser scintillation method. k The compaction densities of the coated separator, positive electrode material, negative electrode material, positive current collector, and negative current collector were tested. r and thickness d Parameters such as these.
[0022] S2. The process window for wet hot pressing is calculated sequentially using the wet adhesive layer interface temperature thermal model, wet rheological model, and wet wetting model, specifically including: S21. Calculate the temperature history of the interface of the adhesive layer inside the cell after liquid injection using the wet adhesive layer interface temperature thermal model, determine the heating time required for the adhesive layer to reach the target activation temperature, and obtain the temperature process window. adhesive layer interface temperature Tinterface The thermal model prediction is based on the temperature history of heat transfer from the hot press plate to the interface of the adhesive layer at the center of the cell under liquid injection conditions. T wet interface ( t This allows for the determination of the hot-pressing time required to reach the target activation temperature; based on the wet physical properties of each layer, the wet thermal resistance of each layer is calculated. R wet th,i =d i / k wet i With wet heat capacity C wet th,i : C wet th,i = r wet i C wet p,i d i Based on the number of cell layers n Calculate the total thermal resistance ∑ from the hot press plate to the interface of the adhesive layer at the center of the battery cell. i ( R wet th,i ) and total heat capacity ∑ i ( C wet th,i The wet characteristic time constant was obtained. t wet : t wet = α wet 2∑ i ( R wet th,i )∑ i ( C wet th,i ) α wet As a specific correction factor, since heat is transferred from both sides to the center, a temperature gradient exists, therefore it is introduced. α wet Make corrections; Using the temperature history formula: T wetinterface ( t ) =T 0 + ( T p -T 0)[1 - exp( -t / t wet )] Predict the change in adhesive layer interface temperature over time and calculate the target activation temperature of the adhesive layer interface. T wet target Time required t , T wet interface ( t )for t The temperature of the adhesive layer interface at any given time. T 0 is the starting temperature. T p Set the temperature for the hot press plate.
[0023] The specific correction factor α wet The method, derived through experimental fitting, includes: fabricating a thin-layer battery cell and implanting a thermocouple at the interface of the central adhesive layer; performing hot pressing under low-pressure conditions after electrolyte injection; collecting data on the change of interface temperature over time; and obtaining the characteristic time through linear regression fitting. t Then, using the following formula: α wet = 2 t / [∑ i ( R th,i )∑ i ( C th,i )] Back-reaming to obtain a specific correction factor α wet .
[0024] Hot press plate set temperature T p Target activation temperature T wet target The wet glass transition temperature of the adhesive layer after swelling equilibrium T wet g and wet melting point T wet m Sure, T wet g and Twet m The target activation temperature was obtained by DSC testing of the adhesive layer after swelling equilibrium. T wet target Compare T wet g or T wet m The temperature of the hot press plate is set at 5~15℃. T p Compare T wet target Temperatures range from 5 to 25°C.
[0025] S22. By combining the swelling kinetics of the adhesive layer in the electrolyte, the gel content of the adhesive layer and the wet rheological properties, a wet rheological model is established, the effective viscosity of the adhesive layer at the target temperature is calculated, the holding time required to ensure the interpenetration bonding between the adhesive layer and the electrode adhesive is determined, and the minimum total hot-pressing time window is obtained by combining the heating time. Swelling kinetics were obtained by immersing the gel sample in an excess electrolyte, placing it in a constant temperature environment, removing it periodically, quickly drying the surface, and weighing it. m ( t Record the time for mass to remain constant. t With quality m To measure the weight and time at different times, use the following formula: SD ( t , T )= SD ∞ ( T )[1 - exp( -t / t swell ( T ))] The equilibrium swelling degree was obtained by fitting. SD ∞ ( T and swelling characteristic time t swell ( T ), where SD ( t , T )for t The swelling degree of the adhesive layer at any given time is calculated as follows: SD ( t,T ) = ( m(t)-m 0 ) / m 0 , m 0This represents the initial sample mass of the adhesive layer.
[0026] gel content of the gel layer GC through The Soxhlet extraction method was used to determine the residue weight, specifically by placing the swollen gel layer into a Soxhlet extractor. m after ,use GC =( m after / m 0 Calculate by multiplying 100%. m 0 The initial sample mass of the adhesive layer is ≥70%; The specific method for establishing a wet rheological model includes: immersing the gel disc sample in a rheometer solvent cup containing electrolyte, changing the temperature, and measuring the change in sample viscosity over time at a fixed temperature. or ( t ), through the Arrhenius equation or ( T,t ) = A·exp ( E a / RT The activation energy under wet conditions was obtained by fitting. E a wet and pre-finger factor A wet ; By correlating swelling degree with viscosity, a wet rheological model is constructed: or eff ( T,t ) =h 0 ( T )exp( -k s SD ( t )) The sensitivity of the viscosity of the quantified adhesive layer to the decrease with increasing swelling degree after absorbing electrolyte is expressed by the formula. or 0 ( T ) represents temperature T The dry reference viscosity of the lower adhesive layer is the viscosity at which it swells. k s The swelling attenuation constant is SD ( t )for t The degree of swelling at any given time; Holding time after the adhesive layer reaches the target activation temperature t wet dwellThe minimum total hot pressing time is 10~300s. t wet min = t 1+ t dwell ,in t 1 represents the heating time required for the adhesive layer interface to reach the target activation temperature; S23. Based on the capillary effect under wet force, establish a wet wetting model, calculate the minimum external pressure process window required to ensure that the adhesive layer fills the pores on the surface of the positive and negative electrode sheets within the holding pressure time, and obtain the hot pressing pressure window by combining the upper limit of the material's compressive strength. The wet wetting model is obtained by calculating the dry pressure driving term and the capillary force term. The dry pressure driving model is as follows: P base min =η(T wet interface ) R a 2 / ( t wet dwell h g 2 ) in P base min This is the minimum pressure window for the upper and lower hot platens. or ( T wet interface (The adhesive layer is on the bottom) T wet interface Viscosity R a The surface roughness of the electrode is measured using a roughness tester. t wet dwell For the pressure holding time, h g This refers to the thickness of the adhesive layer. Calculation of capillary force using the Young-Laplace equation P cap : P cap =2c LV cos θ / r pore In the formula c LV For the surface tension of the electrolyte, iContact angle, r pore The average radius of the pores on the electrode surface; Will P base min and P cap Subtraction yields the wet wetting model: P wet min = P base min - P cap in P wet min This is the minimum thermal pressure under wet conditions; The upper pressure limit is determined by combining the compressive strength of the diaphragm substrate and the electrode. P max The hot-pressing pressure window is obtained. P wet min ≤ P ≤ P max , P This refers to the pressure applied during hot pressing. S3. Based on the obtained process window, small-sample cells were prepared for wet hot pressing verification. The accuracy of the model was verified using electrode peel strength as the core indicator. Peel strength was obtained using a tensile testing machine. According to the temperature process window, minimum total hot pressing time window, minimum applied pressure process window, and hot pressing pressure window, within the wet hot pressing process window range, prioritizing increasing the hot pressing plate temperature while ensuring higher peel strength was achieved. T p With hot pressing pressure P shorten the total hot pressing time t Improve process efficiency; Minimum electrode peel strength σ min The target activation temperature is 1 N / m. If the peel strength is not up to standard, adjust the target activation temperature of the adhesive layer according to the interpenetration state of the adhesive layers. T wet target Or holding time t wet dwell Return to S2 to recalculate the process window and iterate to verify. Once the solution is determined, it can be extended to the same formulation system, establishing a standardized process parameter library for different material systems.
[0027] The wet hot pressing process parameters for lithium-ion batteries are designed and calculated using the above method, specifically including: S1. The positive electrode is a ternary nine-series pure single crystal material, the negative electrode is a silicon-carbon material (10% silicon content), the negative electrode binder is polyacrylic acid, styrene-butadiene rubber, and sodium carboxymethyl cellulose, the positive electrode current collector is a 12µm aluminum foil, the negative electrode current collector is a 6µm copper foil, the base film is a 16µm polyethylene, the coating is with one side of the base film facing the positive electrode and the other side of the 2µm polyacrylic acid facing the negative electrode, the electrolyte is 1.2M LiPF6, the volume ratio of ethylene carbonate (EC), ethyl methyl carbonate (EMC), and diethyl carbonate (DEC) in the electrolyte is 3:5:2, the electrolyte also includes 6wt% fluoroethylene carbonate (FEC) and 1wt% lithium difluorooxalate borate (LiDFOB), and the dry glass transition temperature of the coating material is... T g The melting point is 106℃. T m It is amorphous, and its wet glass transition temperature is... T wet g The temperature is 40℃. The battery is a Z-layer cell with a total of 41 positive electrode layers, 42 battery layers, and 85 separator layers. The specific heat capacity of the wet-coated separator, positive electrode material, negative electrode material, positive current collector, and negative current collector materials in the positive and negative cells is... C p ,density r ,thickness d and thermal conductivity k The parameters and test data are shown in Table 1. Table 1. Relevant Parameters of Lithium-ion Batteries The adhesive layer material, polyacrylic acid, is a highly swellable material, so it is necessary to focus on interfacial interpenetration. The adhesive layer material and the negative electrode adhesive can form an interpenetrating network through hydrogen bonding and esterification crosslinking, and are physically entangled. S2, First set the target activation temperature T wet target Set to 55℃, set the temperature of the hot press plate. T p At 80℃, using a small battery cell with three positive electrodes, four negative electrodes, and nine separators, the battery was placed in the hot pressing station of a flatbed hot press machine, and a pressure of 0.05MPa was applied to approximate pure heat conduction conditions. A thermocouple was implanted in the middle layer of the second positive electrode. After the pressurization started, the time was recorded at a frequency of 1Hz. t and measured interface temperature T interface ; The thermal resistance of a single layer is: R wet th =R th正 +R th负+R th隔 = 1.5293×10 -4 m 2 K / W The heat capacity of a single layer is: C wet th =C th正 +C th负 +C th隔 = 546.84 J / (m 2 k) The product of total thermal resistance and total heat transfer is: [ ∑ i ( R th,i ) ∑ i (C th,i )] = 0.5666s Use ln[1 − ( T interface ( t ) −T 0) / ( T p −T 0)] =−t / τ , with ln[1−( T interface ( t )− T 0) / ( T p - T [0)] is the ordinate. t Using the x-axis as the x-axis, a linear regression is performed on the data, and the resulting slope is −1 / t The wet characteristic time constant was calculated. t wet =0.7213s, specific correction factor α wet = 2 t / [∑ i ( R th,i )×∑ i ( C th,i )] = 2.55.
[0028] In a normal electrolyte-filled battery cell system: ∑i ( R th,i )×∑ i ( C th,i )=∑ i ( d i / k i )×∑ i ( r i C p,i d i )=(3.21153×10 -3 ) × 11483.64 = 36.88s This lithium-ion battery t wet = α wet ×∑ i ( R wet th,i )×∑ i ( C wet th,i ) / 2 = 2.55 × 36.88 / 2 = 47.022 s, from which the interface temperature of the wet adhesive layer is obtained. T wet interface Thermal model formula: T wet interface ( t ) =+ ( T p -T 0)×[ 1- exp( - t / 47.022)] Used to predict the temperature of the adhesive layer inside the battery cell at different times in this system. T wet target It is 55℃. T p For 80℃ T wet interface At 55 ℃, t 1 = -47.022×ln(1-(55-25) / (80-25))=37.08s. t wetdwell Setting it to 200 seconds, the resulting time window is: t wet min =t 1 +t wet dwell = 237.08s. The diaphragm adhesive layer was hot-pressed into a disc approximately 25mm in diameter and 1mm thick using a mold, at a time of 0.1s. -1 The shear rate was tested within a temperature range of 25 ℃ to 70 ℃ (incrementing in 10 ℃ increments, with each temperature point held constant for 5 min to eliminate thermal history), and the static shear viscosity after stabilization was recorded. or The data is shown in Table 2: Table 2. Dry viscosity and wet viscosity versus temperature test data With 1 / T ln( ) is the x-coordinate or Using y as the ordinate, a linear fit is performed to calculate... E dry a =35 kJ / mol, A=2.1×10 5 Pa·s; The rheological model of the adhesive layer is obtained: or ( T interface ) = 2.1×10 5 ×exp[35000 / ( RT interface )] or 0 (55℃) = 7.81 × 10 10 Pa·s.
[0029] Based on the swelling kinetics model SD ∞ (55℃) = 85%, t swell (55℃) = 190s, at this time the kinetic model of the adhesive layer swelling is: SD ( t dwell ) = 85%×[1-exp(- t dwell / 190] Sol content under these conditions GC The value is 78%, which meets the lower limit requirement of 70%, and the adhesive layer can maintain structural stability during hot pressing.
[0030] Table 3 shows the solubility and characteristic swelling time data at different temperatures after injection: Table 3. Solubility and characteristic swelling time at different temperatures after injection. The wet effective viscosity model is as follows: or eff ( T , t ) = 1.2×10 -9 ×exp[85 / (RT interface )]×exp(-0.025×85%×[1-exp(- t dwell / 190]) or eff (55℃, 200s) = 1.96 × 10 10 Pa·s.
[0031] The surface roughness of the negative electrode sheet was measured using a surface roughness tester and SEM. R a =1.5um, h g =6um, yielding the dry-state pressure-driven model. P base min = 1.96×10 10 ×1.5 2 ×10 -12 / (200×6 2 ×10 -12 =6MPa, measured c LV =0.65N / m, contact angle i The angle is 10°, the average radius of the pores on the electrode surface is 0.3 μm, and the capillary force model is: P cap = 2 c LV cos θ / r pore = (2×0.65×cos10×10) 6 ) / (3×10 -5 =4.27MPa Wet infiltration model: P wet min = Pbase min - P cap = 1.73MPa S3. According to the time and pressure windows, hot-press the battery at 2MPa pressure and 80℃ for 250 seconds. Disassemble the cell, check the adhesive layer condition, and determine if adjustments are needed. T target or t dwell The peel force between the outer and middle layers of the electrode and the diaphragm. s The result is 1.2 N / m, which meets the requirements. Based on this model, the pressure and temperature can be adjusted according to the production line process rhythm to optimize the hot pressing time, and the model can be further adjusted based on the obtained peel strength.
[0032] Using the above-mentioned lithium-ion battery hot pressing process parameter design method, a complete wet hot pressing calculation example is provided in a multivariable and strongly coupled system to construct the relationship between the cell pressing temperature, time and pressure process windows after liquid injection. The goal is to find the global optimal solution as much as possible, and to provide theoretical guidance for wet hot pressing parameter optimization to improve cell consistency and final performance.
[0033] The number of devices and processing scale described herein are for the purpose of simplifying the description of the invention. Applications, modifications, and variations of the invention will be readily apparent to those skilled in the art.
[0034] Although embodiments of the present invention have been disclosed above, they are not limited to the applications listed in the specification and embodiments. They can be applied to various fields suitable for the present invention. For those skilled in the art, other modifications can be easily made. Therefore, without departing from the general concept defined by the claims and their equivalents, the present invention is not limited to the specific details and illustrations shown and described herein.
Claims
1. A method for designing process parameters for wet hot pressing of lithium-ion batteries, characterized in that, Includes the following steps: S1. Collect the specific heat capacity, density, thickness and thermal conductivity of the coated diaphragm, positive electrode, negative electrode, positive current collector and negative current collector in the electrolyte-wetted state. S2. The process window for wet hot pressing is calculated sequentially using the wet adhesive layer interface temperature thermal model, wet rheological model, and wet wetting model, specifically including: S21. Calculate the temperature history of the interface of the adhesive layer inside the cell after liquid injection using the wet adhesive layer interface temperature thermal model, determine the heating time required for the adhesive layer to reach the target activation temperature, and obtain the temperature process window. S22. By combining the swelling kinetics of the adhesive layer in the electrolyte, the gel content of the adhesive layer and the wet rheological properties, a wet rheological model is established, the effective viscosity of the adhesive layer at the target temperature is calculated, the holding time required to ensure the interpenetration bonding between the adhesive layer and the electrode adhesive is determined, and the minimum total hot-pressing time window is obtained by combining the heating time. S23. Based on the capillary effect under wet force, establish a wet wetting model, calculate the minimum external pressure process window required to ensure that the adhesive layer fills the pores on the surface of the positive and negative electrode sheets within the holding pressure time, and obtain the hot pressing pressure window by combining the upper limit of the material's compressive strength. S3. Based on the obtained process window, prepare small sample cells for wet hot pressing verification. Use electrode peel strength as the core indicator to verify the accuracy of the model. Adjust the process parameters and iteratively calculate according to the verification results to finally obtain the wet hot pressing process parameters that are suitable for the target material system.
2. The method for designing process parameters for wet hot pressing of lithium-ion batteries according to claim 1, characterized in that, In step S1, the active material in the positive electrode sheet is one or more of single crystal, polycrystalline, or monocrystalline / polycrystalline materials; the surface capacity of the positive electrode sheet is 4~7 mAh / cm². 2 The ratio of the negative electrode surface area capacity to the positive electrode surface area capacity is 1.03~1.15; the active material of the negative electrode is one or more of graphite or silicon carbide materials; The coated diaphragm is made of polyethylene or polypropylene, and the coating is one or more of the following: adhesive coating or ceramic adhesive mixed coating. The adhesive layer facing the positive electrode side includes one or more of poly(vinylidene fluoride-hexafluoropropylene) and polyvinylidene fluoride; The adhesive layer facing the negative electrode side includes one or more of polyacrylic acid and lithium polyacrylate that are interpenetrating with sodium carboxymethyl cellulose, a negative electrode binder, and polyimide, polyurethane / polyacrylonitrile, and styrene-butadiene rubber that are interpenetrating with polyacrylic acid, a negative electrode binder. The adhesive layer is applied by one or more of the following methods: spraying, dot coating, and roller coating.
3. The method for designing process parameters for wet hot pressing of lithium-ion batteries according to claim 1, characterized in that, In S1, the specific heat capacity of the coated diaphragm, positive electrode, negative electrode, positive current collector, and negative current collector in the electrolyte-wetted state is... C p Obtained by DSC measurement; Thermal conductivity of the coated separator, positive electrode, negative electrode, positive current collector, and negative current collector in the electrolyte-wetted state k The thermal conductivity is obtained by testing with the laser flare method and calculated using the formula "thermal conductivity = thermal diffusivity × specific heat capacity × bulk density". The density of the coated separator, positive electrode material, negative electrode material, positive current collector, and negative current collector under electrolyte wetting. ρ Density after the porosity is fully filled, thickness d The thickness of the materials in each part of a lithium-ion battery.
4. The method for designing process parameters for wet hot pressing of lithium-ion batteries according to claim 1, characterized in that, In step S21, the interface temperature of the adhesive layer T interface The thermal model prediction is based on the temperature history of heat transfer from the hot press plate to the interface of the adhesive layer at the center of the cell under liquid injection conditions. T wet interface ( t This allows for the determination of the hot-pressing time required to reach the target activation temperature; Calculate the wet thermal resistance of each layer based on the wet physical properties of each layer. R wet th,i =d i / k wet i With wet heat capacity C wet th,i : C wet th,i = ρ wet i C wet p,i d i Based on the number of cell layers n Calculate the total thermal resistance ∑ from the hot press plate to the interface of the adhesive layer at the center of the battery cell. i ( R wet th,i ) and total heat capacity ∑ i ( C wet th,i The wet characteristic time constant was obtained. τ wet : τ wet = α wet 2∑ i ( R wet th,i )∑ i ( C wet th,i ) α wet As a specific correction factor, since heat is transferred from both sides to the center, a temperature gradient exists, therefore it is introduced. α wet Make corrections; Using the temperature history formula: T wet interface ( t ) =T 0 + ( T p -T 0)[1 - exp( -t / τ wet )] Predict the change in adhesive layer interface temperature over time and calculate the target activation temperature of the adhesive layer interface. T wet target Time required t , T wet interface ( t )for t The temperature of the adhesive layer interface at any given time. T 0 is the starting temperature. T p Set the temperature for the hot press plate.
5. The method for designing process parameters for wet hot pressing of lithium-ion batteries according to claim 4, characterized in that, The specific correction factor α wet The method, derived through experimental fitting, includes: fabricating a thin-layer battery cell and implanting a thermocouple at the interface of the central adhesive layer; performing hot pressing under low-pressure conditions after electrolyte injection; collecting data on the change of interface temperature over time; and obtaining the characteristic time through linear regression fitting. τ Then, using the following formula: α wet = 2 τ / [∑ i ( R th,i )∑ i ( C th,i )] Back-reaming to obtain a specific correction factor α wet .
6. The method for designing process parameters for wet hot pressing of lithium-ion batteries according to claim 4, characterized in that, Hot press plate set temperature T p Target activation temperature T wet target The wet glass transition temperature of the adhesive layer after swelling equilibrium T wet g and wet melting point T wet m Sure, T wet g and T wet m The target activation temperature was obtained by DSC testing of the adhesive layer after swelling equilibrium. T wet target Compare T wet g or T wet m The temperature of the hot press plate is set at 5~15℃. T p Compare T wet target Temperatures range from 5 to 25°C.
7. The method for designing process parameters for wet hot pressing of lithium-ion batteries according to claim 1, characterized in that, In step S22, the swelling kinetics are obtained by the following method: the adhesive sample is immersed in an excess electrolyte, placed in a constant temperature environment, removed periodically, the surface is quickly dried, and the sample is weighed. m ( t Record the time for mass to remain constant. t With quality m To measure the weight and time at different times, use the following formula: SD ( t , T )= SD ∞ ( T )[1 - exp( -t / τ swell ( T ))] The equilibrium swelling degree was obtained by fitting. SD ∞ ( T and swelling characteristic time τ swell ( T ), where SD ( t , T )for t The swelling degree of the adhesive layer at any given time is calculated as follows: SD ( t,T ) = ( m(t)-m 0 ) / m 0 , m 0 This represents the initial sample mass of the adhesive layer.
8. The method for designing process parameters for wet hot pressing of lithium-ion batteries according to claim 1, characterized in that, In S22, the gel content of the adhesive layer GC The residue weight was obtained by Soxhlet extraction, specifically by placing the swollen gel layer into a Soxhlet extractor. m after ,use GC =( m after / m 0 Calculate by multiplying 100%. m 0 The initial sample mass of the adhesive layer is ≥70%; In step S22, the specific method for establishing the wet rheological model includes: immersing the gel disc sample in a rheometer solvent cup containing electrolyte, changing the temperature, and measuring the change in sample viscosity over time at a fixed temperature. η ( t ), through the Arrhenius equation η ( T,t ) = A·exp ( E a / RT The activation energy under wet conditions was obtained by fitting. E a wet and pre-finger factor A wet ; By correlating swelling degree with viscosity, a wet rheological model is constructed: η eff ( T,t ) =η 0 ( T )exp( -k s SD ( t )) The sensitivity of the viscosity of the quantified adhesive layer to the decrease with increasing swelling degree after absorbing electrolyte is expressed by the formula. η 0 ( T ) represents temperature T The dry reference viscosity of the lower adhesive layer is the viscosity at which it swells. k s The swelling attenuation constant is SD ( t )for t The degree of swelling at any given time; Holding time after the adhesive layer reaches the target activation temperature t wet dwell The minimum total hot pressing time is 10~300s. t wet min = t 1+ t dwell ,in t 1 represents the heating time required for the adhesive layer interface to reach the target activation temperature.
9. The method for designing process parameters for wet hot pressing of lithium-ion batteries according to claim 1, characterized in that, In step S23, the wet wetting model is obtained by calculating the dry pressure driving term and the capillary force term. The dry pressure driving model is as follows: P base min =η ( T wet interface ) R a 2 / ( t wet dwell h g 2 ) in P base min This is the minimum pressure window for the upper and lower hot platens. η ( T wet interface (The adhesive layer is on the bottom) T wet interface Viscosity R a The surface roughness of the electrode is measured using a roughness tester. t wet dwell For the pressure holding time, h g This refers to the thickness of the adhesive layer; Calculation of capillary force using the Young-Laplace equation P cap : P cap = 2 γ LV cosθ / r pore In the formula γ LV For the surface tension of the electrolyte, θ Contact angle, r pore The average radius of the pores on the electrode surface; Will P base min and P cap Subtraction yields the wet wetting model: P wet min = P base min − P cap in P wet min This is the minimum thermal pressure under wet conditions; The upper pressure limit is determined by combining the compressive strength of the diaphragm substrate and the electrode. P max The hot-pressing pressure window is obtained. P wet min ≤ P ≤ P max , P This refers to the pressure applied during hot pressing.
10. The method for designing process parameters for wet hot pressing of lithium-ion batteries according to claim 1, characterized in that, In step S3, the peel strength is obtained using a tensile testing machine. Based on the temperature process window, minimum total hot-pressing time window, minimum applied pressure process window, and hot-pressing pressure window, within the wet hot-pressing process window range, prioritizing increasing the hot-pressing platen set temperature while ensuring higher peel strength is achieved. T p With hot pressing pressure P shorten the total hot pressing time t Improve process efficiency; Minimum electrode peel strength σ min The target activation temperature is 1 N / m. If the peel strength is not up to standard, adjust the target activation temperature of the adhesive layer according to the interpenetration state of the adhesive layers. T wet target Or holding time t wet dwell Return to S2 to recalculate the process window and iterate to verify.
Citation Information
Patent Citations
Method for processing lithium ion battery cell by diaphragm coating
CN103996877A