Adaptive Thermal-Assisted Cleaning System and Method for the Center Hole of Cylindrical Battery Core

By using adaptive control with controllable heating and real-time resistance feedback, the problem of blockage in the center hole of the core after flattening is solved, achieving thermal softening and mechanical flattening of the separator, improving battery production efficiency and yield, and avoiding separator damage.

CN123120816APending Publication Date: 2026-11-17ZHENGZHOU BAK BATTERY CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202611361338.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-09-03
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In the manufacturing process of cylindrical batteries with all tabs, the center hole of the core after flattening is prone to forming a membrane wrinkle layer that blocks it, which leads to obstruction of electrolyte wetting and difficulty in probe insertion. Moreover, the existing device lacks adaptive cleaning capability, and the rigid through hole at room temperature is prone to compacting blockages or puncturing the membrane. Manual through hole opening is inefficient and unreliable.

Method used

Using a controllable heating through-hole tool combined with a tapered guide surface, and through real-time acquisition of feed resistance for adaptive control, the diaphragm is thermally softened and mechanically flattened. The heating power and feed speed are dynamically adjusted according to the degree of blockage to complete adaptive cleaning.

Benefits of technology

It effectively restores the center aperture of the core, improves electrolyte wetting and probe insertion conditions, increases production yield, ensures no damage to the diaphragm, and adapts to cleaning needs with different degrees of blockage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123120816A_ABST
    Figure CN123120816A_ABST
Patent Text Reader

Abstract

This invention discloses an adaptive thermally assisted cleaning system and method for the center hole of a cylindrical battery core, relating to the field of lithium-ion battery manufacturing technology. This invention adds a thermally assisted active cleaning process after flattening and before electrolyte injection. A controllable heated through-hole tool is used to bring the separator to a critical state of thermal softening. Combined with the mechanical flattening effect of the conical guide surface, it can post-clean up existing separator wrinkles and debris blockages, avoiding the defects of room-temperature rigid through-holes compacting blockages and puncturing or tearing the separator. It flattens separator wrinkles without causing thermal damage to the separator. This invention uses feed resistance as the criterion for determining the end point of the through-hole. After the through-hole is in place, the separator is thermally shaped to suppress rebound. Relying on the synergistic effect of thermal softening, blockage classification, and force feedback closed loop, the diameter of the core center hole can be stably restored, improving the subsequent electrolyte wetting and probe insertion process conditions, and increasing the production yield of all-tab cylindrical batteries.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of lithium-ion battery manufacturing technology, specifically to an adaptive thermal-assisted cleaning system and method for the center hole of a cylindrical battery core. Background Technology

[0002] With the rapid development of power battery technology, improving battery energy density, power density, and cycle life has become a continuous pursuit of the industry. All-tab cylindrical batteries (such as 18650, 21700, and 4680) have become an important development direction for cylindrical battery technology due to their advantages such as low internal resistance of the tabs, large conductive area, and strong power output capability. In the manufacturing process of all-tab cylindrical batteries, the wound electrode assembly needs to be flattened to press the positive and negative tabs towards the end face for subsequent welding to the current collector. However, this process often results in the edge of the separator near the root of the tab being squeezed into the central hole due to vibration of the flattening roller or eccentricity of the positioning pin, forming a separator defect. The membrane wrinkles significantly reduce the effective inner diameter of the center hole from approximately 3.5 mm after winding to approximately 1.5 mm. Furthermore, the uneven inner wall allows electrode debris and diaphragm fragments generated during the smoothing process to fall into the center hole, mixing with the wrinkles to form a complex blockage. This type of center hole blockage defect has multiple adverse effects on subsequent production processes: electrolyte wetting is hindered during injection, prolonging the wetting time and affecting formation efficiency; increased resistance during insertion of the center needle or welding probe can easily damage the diaphragm or cause misalignment. Even with optimized smoothing processes such as lengthening the center needle, reducing the cone angle, and homogenizing the clamping force, approximately 0.03% of the core still has residual blockage, restricting product yield.

[0003] To address this issue, existing technologies mostly focus on prevention during the kneading process, rather than proactive cleaning after kneading. For example, existing patents (CN223743703U, CN224318495U) emphasize preventative measures during the kneading process, protecting specific structural features (such as the hot-hole needle passing through the kneading device, the bearing connection between the center needle and the base, etc.), without addressing adaptive cleaning of residual blockages after kneading, nor providing a force feedback-based control method. Furthermore, CN120319859A uses a rotatable connection between the center needle and the kneading base to keep the center needle and the battery cell relatively stationary, thus eliminating dynamic friction damage. CN223513993U sets a bearing at the head of the center needle to transform rigid friction into rolling friction to prevent diaphragm wrinkling. However, these solutions are still limited to the scope of mechanical anti-friction, neither introducing heating functions nor possessing adaptive processing capabilities for different degrees of blockage.

[0004] Regarding cleaning after smoothing, existing methods have obvious drawbacks: rigid through-hole needles at room temperature have high resistance, which easily compacts the blockage rather than removes it, and there is a high risk of puncturing the diaphragm. Manual through-hole cleaning is inefficient and inconsistent, and there is a risk of operational errors. Although there are solutions such as heated coiling needles for smoothing or hot-scalding holes, none of them can achieve adaptive cleaning for different degrees of blockage in the diaphragm folds after smoothing. Based on this, we now provide an adaptive heat-assisted cleaning system and method for the center hole of cylindrical battery cores, which can eliminate the drawbacks of existing devices. Summary of the Invention

[0005] The purpose of this invention is to provide an adaptive thermally assisted cleaning system and method for the center hole of a cylindrical battery core, in order to solve the problems in the background art.

[0006] To achieve the above objectives, the present invention provides the following technical solution: An adaptive thermally assisted cleaning system and method for the center hole of a cylindrical battery core, comprising the following steps: Step S1: Provide a through-hole tool: After the kneading process is completed and before the liquid injection process begins, provide a through-hole tool with a controllable heating function; Step S2: Heat to preset temperature: Heat the through-hole tool to a preset temperature T, where the preset temperature T satisfies: T≥60℃ and T<heat distortion temperature of the diaphragm material; Step S3: Initial advance: Advance the through-hole tool toward the center hole of the core at an initial feed rate V0; Step S4: Real-time resistance acquisition: During the advancement process, the axial feed resistance F(t) of the through-hole tool is acquired in real time. Step S5: Adaptive control: Execute adaptive control based on the change in feed resistance F(t); Step S6: Condition determination: When the feed resistance F(t) decreases from the initial peak value to the stable value F stable When the stable duration exceeds Δt, it is determined that the blockage in the central hole has been cleared; Step S7: Exit the through-hole tool.

[0007] Based on the above technical solutions, the present invention also provides the following optional technical solutions: In one alternative: the through-hole tool in step S1 includes a needle tip and a tapered guide surface located behind the needle tip. The diameter of the needle tip is 1.3 to 1.4 mm, the cone angle θ of the tapered guide surface is 45 to 60°, and the maximum diameter of the tapered guide surface is 2.5 to 3.0 mm.

[0008] In one alternative: the preset temperature T in step S2 is 5 to 15°C lower than the heat distortion temperature of the membrane material. When the membrane is a PE membrane, the preset temperature T is 70 to 80°C, and when the membrane is a PP membrane, the preset temperature T is 85 to 95°C.

[0009] In one alternative: the through-hole tool in step S2 adopts a pulse heating strategy, with a pulse heating power of 200-300W during the insertion and heating stage, a heating duration of 0.3-0.8s, and a pulse heating power of 20-50W during the heat preservation stage.

[0010] In one alternative: the initial feed rate V0 in step S3 ranges from 3 to 20 mm / s, the feed pressure P is negatively correlated with the heating temperature T, and the feed pressure P ranges from 1 to 10 N.

[0011] In one alternative: prior to step S3, the through-hole tool pre-contacts the end face of the core center hole to obtain initial feed resistance F. initial Based on the initial feed resistance F initial Classify the degree of congestion: When F initial When the current is less than 3N, it indicates a slight blockage. The system will automatically select the fast mode and set the feed rate to 15-20 mm / s. When 3N≤F initial When the feed rate is <8N, it indicates moderate blockage. The standard mode is automatically selected, and the feed rate is 8-12 mm / s. When F initial When the pressure is ≥8N, it is considered a severe blockage. The system will automatically select the high-power mode, with a feed rate of 3-5 mm / s, and apply ±30° circumferential reciprocating rotation assistance while advancing axially. During the execution of steps S3 to S5, the cleaning operation is carried out according to the working mode of feed speed and feed pressure matched with the blockage level.

[0012] In one alternative approach: the adaptive control in step S5 specifically includes: If F(t) exceeds the first threshold F1, the heating power will be automatically increased to raise the temperature by ΔT. If F(t) is lower than the second threshold F2, the feed rate will be automatically increased; If F(t) fluctuates within the preset range, then the current parameters are maintained; The first threshold F1 has a value of 8 to 12N, and the second threshold F2 has a value of 2 to 4N.

[0013] In one alternative: the stabilization duration Δt in step S6 is 1 to 5 seconds. After the through-hole tool reaches the target position, it is held for 1 to 5 seconds to achieve thermal setting of the diaphragm and suppress diaphragm rebound.

[0014] An adaptive thermally assisted cleaning system for the center hole of a cylindrical battery core, the system being used to perform the above method, including: The through-hole tool has a controllable heating function and is used to perform heat-assisted through-hole cleaning of the core center hole after the flattening process and before the liquid injection process begins. The force detection module is used to collect the feed resistance F(t) of the through-hole tool during the axial feed process in real time. The temperature control module is used to automatically adjust the heating power and heating temperature according to the change of the feed resistance F(t); The feed drive module is used to automatically adjust the feed speed of the through hole tool according to the change of feed resistance F(t), and can also realize the circumferential reciprocating rotation of the through hole tool; The main control unit is used to communicate with the force detection module, temperature control module, and feed drive module.

[0015] Compared with the prior art, the beneficial effects of the present invention are as follows: 1. This invention adds a heat-assisted active cleaning process after kneading and before liquid injection. It uses a controllable heated through-hole tool to bring the diaphragm to a critical state of thermal softening. Combined with the mechanical flattening effect of the conical guide surface, it can clean the diaphragm wrinkles and debris blockages after the process. This avoids the defects of room temperature rigid through-hole compaction of blockages and puncture and tearing of the diaphragm. It flattens the diaphragm wrinkles without causing thermal damage to the diaphragm.

[0016] 2. This invention uses the feed resistance as the criterion for determining the end point of the through hole. After the through hole is in place, the separator is heat-set to suppress springback. Relying on the synergistic effect of thermal softening, blockage classification, and force feedback closed loop, the diameter of the core center hole can be stably restored, improving the subsequent electrolyte wetting and probe insertion process conditions, and increasing the production yield of all-tab cylindrical batteries.

[0017] 3. This invention classifies the blockage level and matches the corresponding working mode by collecting the initial feed resistance through pre-contact acquisition. At the same time, it collects the axial feed resistance in real time during the feeding process to build a closed-loop adaptive control, dynamically adjusts the heating power and feed speed, and uses pulse heating to reduce the heat input of the core. It can achieve adaptive processing of different blockage conditions of light, medium and heavy blockage, taking into account both cleaning yield and production efficiency. Attached Figure Description

[0018] Figure 1 This is a schematic diagram of the process flow of the adaptive thermal cleaning method of the present invention.

[0019] Figure 2 This is a schematic diagram of the closed-loop logic steps of the force feedback adaptive control of the present invention.

[0020] Figure 3 This is a schematic diagram of the F(t) curve structure of the present invention.

[0021] Figure 4This is a schematic diagram showing the comparison of F(t) curves under different conditions according to the present invention.

[0022] Figure 5 This is a schematic diagram of the through-hole device structure of the present invention. Detailed Implementation

[0023] To make the objectives, technical solutions, and advantages of this invention clearer, the invention will be further described in detail below with reference to the accompanying drawings and embodiments. Example

[0024] like Figures 1-5 As shown, the adaptive thermal-assisted cleaning system and method for the center hole of a cylindrical battery core includes the following steps: Step S1: Provide through-hole tools After the kneading process is completed and before the liquid injection process begins, a through-hole tool is provided. The through-hole tool has a controllable heating function. The through-hole tool includes a needle tip section and a tapered guide surface located behind the needle tip section. The diameter of the needle tip section is 1.3 to 1.4 mm, the cone angle θ of the tapered guide surface is 45 to 60°, and the maximum diameter of the tapered guide surface is 2.5 to 3.0 mm. Step S2: Heat to the preset temperature The through-hole tool is heated to a preset temperature T, which satisfies the following conditions: T≥60℃ and T<heat distortion temperature of the diaphragm material. In this embodiment, a PE diaphragm system is used, and the heat distortion temperature of the PE diaphragm is about 80℃. The preset temperature T is set to 75℃±3℃. The through-hole tool adopts a pulse heating strategy. During the insertion and heating stage, the pulse heating power is 200W and the heating duration is 0.5s. During the heat preservation stage, the pulse heating power is 20W. Step S3: Initial Propulsion The initial feed resistance F is obtained by pre-contacting the end face of the center hole of the winding core with the through-hole tool. initial In this embodiment F initial If the pressure is 5-7N, it is determined to be a moderate blockage. Select the standard mode and push the through-hole tool toward the center hole of the core with an initial feed speed of V0=10mm / s and a feed pressure of P=3N. Step S4: Real-time resistance acquisition During the advancement process, the axial feed resistance F(t) of the through-hole tool is collected in real time through the force detection module. Step S5: Adaptive Control Adaptive control is executed based on the change in feed resistance F(t): If F(t) exceeds the first threshold F1 (in this embodiment, F1 is 10N), the heating power will be automatically increased to raise the temperature by ΔT. After the temperature rise, the temperature of the through-hole tool is still less than the heat deformation temperature of the diaphragm material. If F(t) is lower than the second threshold F2 (in this embodiment, F2 is 3N), the feed rate will be automatically increased. If F(t) fluctuates within the preset range, then the current parameters are maintained; Step S6: Condition Determination When the feed resistance F(t) decreases from the initial peak value to the stable value F stable When the stable duration exceeds Δt (Δt is 3s in this embodiment), it is determined that the blockage of the central hole has been cleared. After the through-hole tool reaches the target position, it is held for 3s to allow the flattened diaphragm to be shaped under the residual heat and suppress the diaphragm rebound. Step S7: Exit the through-hole tool After the diaphragm is shaped, remove the through-hole tool; In this embodiment, after kneading, the central hole was found to be moderately blocked, and the initial feed resistance F initial The resistance is 5-7 N. The diaphragm wrinkles result in an effective inner diameter of about 1.5 mm. During the through-hole process, the feed resistance F(t) drops rapidly from the initial peak of about 6.6 N. After penetrating the diaphragm wrinkles, it drops to 2.4 N. Subsequently, when advancing in the hole, it fluctuates slightly (about 2.3-2.6 N) due to local diaphragm wrinkles. After thermal softening, it stabilizes at about 1.1 N. When withdrawing, the resistance returns to zero. Disassembly and inspection after pore opening: The diaphragm wrinkles inside the central hole were completely flattened, the effective inner diameter was restored to about 2.7 mm, the diaphragm was undamaged, the pore opening time was 2 seconds, the success rate was 100% (10 / 10), and the diaphragm damage rate was 0%. Example

[0025] An adaptive thermally assisted cleaning system and method for the center hole of a cylindrical battery core, comprising the following steps: The overall process steps are consistent with those in Example 1, except that: this example uses a PP diaphragm system, the heat distortion temperature of the PP diaphragm is about 100℃, the preset temperature T is set to 85℃±3℃, the pulse heating power is 220W, the heating duration is 0.6s, the pulse heating power during the heat preservation stage is 30W, the initial feed speed V0 is 8mm / s (the PP diaphragm is slightly hard, so the speed is reduced), the feed pressure P is 2N, the holding time is set to 4s (PP softens slowly, so the holding time is extended), Δt is 4s, F1 is 11N, and F2 is 3N; In this embodiment, after kneading, the central hole was found to be moderately blocked, and the initial feed resistance F initial The resistance is 6-8 N. The diaphragm wrinkles result in an effective inner diameter of about 1.5 mm. During the through-hole process, the feed resistance F(t) drops rapidly from the initial peak of about 7.5 N. After penetrating the diaphragm wrinkles, it drops to 3.0 N. Subsequently, when advancing in the hole, it fluctuates slightly (about 2.4-3.2 N) due to local diaphragm wrinkles. After thermal softening, it stabilizes at about 1.3 N. When withdrawing, the resistance returns to zero. Disassembly and inspection after pore opening: The diaphragm wrinkles inside the central hole were completely flattened, the effective inner diameter was restored to about 2.5 mm, the diaphragm was undamaged, the pore opening time was 2.2 seconds, the success rate was 100% (10 / 10), and the diaphragm damage rate was 0%. Example

[0026] An adaptive thermally assisted cleaning system and method for the center hole of a cylindrical battery core, comprising the following steps: The overall process steps are consistent with those of Example 1, except that: this example uses a PE diaphragm system, which, after being flattened, was found to have severe blockage in the central hole, resulting in an initial feed resistance F. initial The effective inner diameter is approximately 1.0 mm due to the diaphragm pleats, with a preset temperature T of 75℃±3℃. The pulse heating power is 250W, the heating duration is 0.6s, the pulse heating power during the heat preservation stage is 40W, the initial feed speed V0 is 5mm / s (reduced compared to moderate blockage to prevent impact damage), the feed pressure P is 2N, the holding time is set to 5s, Δt is 5s, F1 is 12N, and F2 is 3N. During the execution of steps S3 to S5, the cleaning operation is carried out according to the working mode of feed speed and feed pressure matched with the blockage level. The through-hole tool is pushed axially and then subjected to circumferential reciprocating rotation auxiliary motion (rotation angle of ±30°, frequency of 5Hz) to help fold and unfold the diaphragm. During the through-hole process, the feed resistance F(t) changes with time: the initial peak value of about 12N at the first diaphragm fold drops rapidly, and after penetrating the diaphragm fold layer, it drops to about 5N. Then, when advancing in the hole, due to the second diaphragm fold, the second peak value is about 6.2N. After penetration, the resistance drops to about 4.5N. After thermal softening, it stabilizes at about 1.2N. When exiting, the resistance returns to zero. Disassembly and inspection after through-hole: The effective inner diameter was restored from about 1.0 mm to about 2.5 mm, and many diaphragm wrinkles / folds were completely flattened. The through-hole time was 2.7 seconds, the success rate was 100% (10 / 10), and the diaphragm damage rate was 0%. After passing through the second diaphragm fold, the control unit automatically reduced the feed speed to allow the diaphragm to soften more fully before flattening.

[0027] Comparative Example 1 The overall process steps are consistent with those of Example 1, except that: this comparative example uses a room temperature rigid through-hole needle for cleaning, and the through-hole needle does not have a heating function. The other parameters (feed speed 10mm / s, feed pressure 3N) are consistent with those of Example 1. During the through-hole process, because the diaphragm is less flexible at room temperature, the wrinkled layer is compacted by the rigid needle tip instead of flattened, and the feed resistance remains high (about 8 to 12N), and the resistance curve does not show a significant downward trend. Disassembly and inspection after opening the hole: The diaphragm wrinkles inside the central hole were not effectively flattened, and the diaphragm in some areas was punctured. The effective inner diameter was still about 1.5 mm. The cleaning success rate was 83.3%, and the diaphragm damage rate was about 4%.

[0028] Comparative Example 2 The overall process steps are consistent with those of Example 1, except that: this comparative example uses a heated through-hole needle (heating temperature 75℃±3℃) for cleaning, but does not perform force feedback adaptive control. That is, the heating power, feed speed, and feed pressure are kept constant throughout the through-hole process (constant power 200W, constant speed 10mm / s, constant pressure 3N), and no adjustment is made according to the change of feed resistance F(t). During the through-hole process, when encountering local stubborn wrinkles, the resistance peak is high (about 9-11N) because the heating power cannot be increased or the feed speed cannot be decreased automatically. After penetration, the overall through-hole time is extended to 4-5 seconds because the feed speed cannot be increased automatically. Disassembly and inspection after opening the hole: The diaphragm wrinkles in the center hole are basically flattened, but there are local areas where the wrinkles are more severe and the flattening is insufficient. The effective inner diameter is restored to about 2.0 to 2.3 mm. The cleaning success rate is 90% and the diaphragm damage rate is about 0%.

[0029] Comparative Example 3 The overall process steps are consistent with those of Example 1, except that: this comparative example uses force feedback adaptive control for through-hole cleaning, but the through-hole needle is not heated (at room temperature). The other parameters are consistent with those of Example 1. During the through-hole process, although the feed speed can be adjusted according to the change in resistance, the diaphragm is not softened by heat, and the wrinkled layer is difficult to flatten effectively under mechanical action. The resistance curve shows repeated fluctuations but no significant decrease. The overall resistance is maintained between 6 and 9 N, and the through-hole time is extended to 4.8 seconds. Disassembly and inspection after opening the hole: The diaphragm wrinkles inside the central hole are in a compressed state rather than a flattened state, the effective inner diameter is only restored to about 1.8mm, and there are local diaphragm tears. The cleaning success rate is 86.7%, and the diaphragm damage rate is about 3.3%.

[0030] Experimental Example Test conditions: Cylindrical battery cores (PE separator system, moderate clogging, F) ​​from the same batch were used after being flattened. initial =5~7N, effective inner diameter of the central hole is about 1.5mm), randomly divided into 6 groups, 30 samples in each group, and processed by the methods of Example 1, Example 2, Example 3, Comparative Example 1, Comparative Example 2, and Comparative Example 3 respectively; After each group was processed, the cleaning success rate, diaphragm damage rate, average through-hole time, and effective inner diameter after through-hole were statistically analyzed. The cleaning success rate was judged by the diaphragm wrinkles in the center hole being completely flattened after through-hole, the effective inner diameter being ≥2.4mm, and the diaphragm being undamaged. The diaphragm damage rate was judged by the diaphragm being punctured, torn, or obviously scratched after disassembly and inspection after through-hole. The through-hole time was the total time from the start of axial feeding of the through-hole tool to its complete withdrawal. The effective inner diameter was obtained by measuring the center hole of the core after through-hole using an image measuring instrument. The average value of 30 samples in each group was taken. The specific test results are shown below: Performance indicators diaphragm system degree of congestion Cleanup success rate Diaphragm damage rate Average through-hole time (s) Effective inner diameter after through hole (mm) Adaptability Example 1 PE moderate 100%(30 / 30) 0%(0 / 30) 2.0 2.7 It has (automatic classification and closed-loop feedback). Example 2 PP moderate 100%(30 / 30) 0%(0 / 30) 2.2 2.5 It has (automatic classification and closed-loop feedback). Example 3 PE Severe 100%(30 / 30) 0%(0 / 30) 2.7 2.5 It has (automatic classification and closed-loop feedback). Comparative Example 1 PE moderate 83.3%(25 / 30) 3.3%(1 / 30) 1.8 1.5~1.7 none Comparative Example 2 PE moderate 90.0%(27 / 30) 0%(0 / 30) 4.3 2.0~2.3 none Comparative Example 3 PE moderate 86.7%(26 / 30) 3.3%(1 / 30) 4.8 1.8~2.0 Yes (feedback only indicates no heating) Results analysis: The cleaning success rate of Examples 1 to 3 all reached 100% (30 / 30), the diaphragm damage rate was 0%, and the effective inner diameter after the pore was restored to more than 2.5 mm. This shows that the method of the present invention can achieve stable and reliable cleaning effect under different diaphragm systems (PE / PP) and different degrees of blockage (medium / severe). Comparative Example 1 (Rigid through-hole needle at room temperature) lacks heating function, so the diaphragm cannot be softened. The wrinkled layer is compacted by the rigid needle tip instead of being flattened. The cleaning success rate is only 83.3%, and the diaphragm damage rate is 3.3%. The effective inner diameter is still about 1.5 mm, and the cleaning effect is the worst. Comparative Example 2 (heated through-hole needle without force feedback adaptive control) has a heating function, but it cannot dynamically adjust the through-hole parameters according to the change of feed resistance. The cleaning success rate is 90.0%, the overall through-hole time is extended to 4.3 seconds, and the effective inner diameter recovery is insufficient (2.0~2.3mm). This shows that without force feedback adaptive control, the cleaning effect and efficiency are significantly reduced. Comparative Example 3 (force feedback adaptive control without heating) can adjust the feed speed according to the change of resistance, but because the diaphragm is not softened by heat, the mechanical flattening effect is limited, the cleaning success rate is only 86.7%, the diaphragm damage rate is 3.3%, and the effective inner diameter is only restored to 1.8-2.0 mm. This shows that without the heating function, force feedback adaptive control alone cannot effectively flatten the diaphragm wrinkles. The comparison between Example 1 and Comparative Examples 2 and 3 shows that there is a significant synergistic effect between heating and force feedback adaptive control: neither of these technologies alone can achieve the desired cleaning effect; only the synergistic effect of the two can achieve high success rate and zero damage adaptive cleaning. The hole-through time of Example 1 (2.0s) is significantly better than that of Comparative Example 2 (4.3s), Comparative Example 3 (4.8s) and artificial hole-through (5-10s), indicating that the adaptive control of the present invention not only improves the cleaning success rate, but also greatly improves the cleaning efficiency; The above experimental data fully demonstrate that the adaptive thermal-assisted cleaning system and method for the center hole of cylindrical battery core provided by this invention, through the synergistic effect of heating and softening the diaphragm and force feedback adaptive control, can completely remove the blockage in the center hole without damaging the diaphragm. It effectively solves the technical problems of low cleaning success rate, easy damage to the diaphragm, and inability to adapt to different degrees of blockage in the prior art, and has significant technological progress and industrial application value.

[0031] The above description is merely a specific embodiment of this disclosure, but the scope of protection of this disclosure is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in this disclosure should be included within the scope of protection of this disclosure. Therefore, the scope of protection of this disclosure should be determined by the scope of the claims.

Claims

1. A method for using a cylindrical battery roll core center hole self-adaptive heat-assisted cleaning system, characterized in that, Includes the following steps: Step S1: Provide a through-hole tool: After the kneading process is completed and before the liquid injection process begins, provide a through-hole tool with a controllable heating function; Step S2: Heat to preset temperature: Heat the through-hole tool to a preset temperature T, where the preset temperature T satisfies: T≥60℃ and T<heat distortion temperature of the diaphragm material; Step S3: Initial advance: Advance the through-hole tool toward the center hole of the core at an initial feed rate V0; Step S4: Real-time resistance acquisition: During the advancement process, the axial feed resistance F(t) of the through-hole tool is acquired in real time. Step S5: Adaptive control: Execute adaptive control based on the change in feed resistance F(t); Step S6: Condition determination: When the feed resistance F(t) decreases from the initial peak value to the stable value F stable When the stable duration exceeds Δt, it is determined that the blockage in the central hole has been cleared; Step S7: Exit the through-hole tool.

2. The method of claim 1, wherein the method further comprises: The through-hole tool in step S1 includes a needle tip and a tapered guide surface located behind the needle tip. The diameter of the needle tip is 1.3 to 1.4 mm, the cone angle θ of the tapered guide surface is 45 to 60°, and the maximum diameter of the tapered guide surface is 2.5 to 3.0 mm.

3. The method of using the cylindrical battery roll core center hole adaptive thermal-assisted cleaning system according to claim 1, wherein, The preset temperature T in step S2 is 5 to 15°C lower than the heat distortion temperature of the diaphragm material. When the diaphragm is a PE diaphragm, the preset temperature T is 70 to 80°C, and when the diaphragm is a PP diaphragm, the preset temperature T is 85 to 95°C.

4. The method of claim 1, wherein the method further comprises: In step S2, the through-hole tool adopts a pulse heating strategy. During the insertion and heating stage, the pulse heating power is 200-300W and the heating duration is 0.3-0.8s. During the heat preservation stage, the pulse heating power is 20-50W.

5. The method of using the cylindrical battery roll core center hole adaptive thermal-assisted cleaning system of claim 1, wherein, In step S3, the initial feed rate V0 ranges from 3 to 20 mm / s, and the feed pressure P is negatively correlated with the heating temperature T, with the feed pressure P ranging from 1 to 10 N.

6. The method of using the adaptive thermal-assisted cleaning system for the center hole of a cylindrical battery core according to claim 1, characterized in that, Before step S3, the through-hole tool pre-contacts the end face of the core center hole to obtain the initial feed resistance F. initial Based on the initial feed resistance F initial Classify the degree of congestion: When F initial When <3N, it is light blockage, and the automatic selection of fast mode is 15-20 mm / s. When 3N ≤ F initial When 8N < F < 12N, it is a moderate block, and the standard mode is automatically selected, and the feed speed is 8-12 mm / s; When F initial When the pressure is ≥8N, it is considered a severe blockage. The system will automatically select the high-power mode, with a feed rate of 3-5 mm / s, and apply ±30° circumferential reciprocating rotation assistance while advancing axially. During the execution of steps S3 to S5, the cleaning operation is carried out according to the working mode of feed speed and feed pressure matched with the blockage level.

7. The method of using the cylindrical battery roll core center hole adaptive thermal-assisted cleaning system of claim 1, wherein, The adaptive control in step S5 specifically includes: If F(t) exceeds the first threshold F1, the heating power will be automatically increased to raise the temperature by ΔT. If F(t) is lower than the second threshold F2, the feed rate will be automatically increased; If F(t) fluctuates within the preset range, then the current parameters are maintained; The first threshold F1 has a value of 8 to 12N, and the second threshold F2 has a value of 2 to 4N.

8. The method of using the adaptive thermal-assisted cleaning system for the center hole of a cylindrical battery core according to claim 1, characterized in that, The stabilization duration Δt in step S6 is 1 to 5 seconds. After the through-hole tool reaches the target position, it is held for 1 to 5 seconds to achieve thermal shaping of the diaphragm and suppress diaphragm rebound.

9. An adaptive thermal-assisted cleaning system for the center hole of a cylindrical battery core, characterized in that, The system is used to perform the method according to any one of claims 1-8, comprising: The through-hole tool has a controllable heating function and is used to perform heat-assisted through-hole cleaning of the core center hole after the flattening process and before the liquid injection process begins. The force detection module is used to collect the feed resistance F(t) of the through-hole tool during the axial feed process in real time. The temperature control module is used to automatically adjust the heating power and heating temperature according to the change of the feed resistance F(t); The feed drive module is used to automatically adjust the feed speed of the through hole tool according to the change of feed resistance F(t), and can also realize the circumferential reciprocating rotation of the through hole tool; The main control unit is used to communicate with the force detection module, temperature control module, and feed drive module.

Citation Information

Patent Citations

  • Hole ironing and rubbing integrated mechanism for cylindrical battery cell

    CN223743703U

  • Cylindrical battery kneading station center needle assembly and kneading device

    CN224318495U