Semiconductor devices and their manufacturing methods

By optimizing the layout and material selection of the active region and contacts, the problems of bridging and increased contact resistance in semiconductor devices were solved, thereby improving device reliability and processing efficiency.

CN123124343APending Publication Date: 2026-11-17SK HYNIX INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202511834147.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2025-05-14
Filing Date
2025-12-08
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

In the manufacturing process of semiconductor devices, bridging occurs between adjacent active regions, leading to a decrease in reliability. Furthermore, when the size of the contact area where the bit line contact or memory node contact overlaps with the active region decreases, the contact resistance increases.

Method used

The layout of multiple active areas, word line structures, bit line pad areas, and memory node pad areas was designed. Pad areas of different materials and heights were used, and active areas were defined by forming relatively shallow cell isolation areas to prevent bridging and improve the stability of contact resistance.

Benefits of technology

It improves the operating speed of semiconductor devices, reduces leakage current, enhances device reliability and ease of processing, and reduces process complexity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124343A_ABST
    Figure CN123124343A_ABST
Patent Text Reader

Abstract

This application relates to semiconductor devices and methods for manufacturing the same. The semiconductor device includes: word line structures extending along a first direction and spaced apart from each other in a second direction; active regions extending along a diagonal direction at an acute angle to the first direction, overlapping the word line structures, and spaced apart from each other in the first direction; bit line pad regions, each bit line pad region overlapping one end of a corresponding active region, contacting one side of a corresponding word line structure, and comprising a first material; memory node pad regions, each memory node pad region overlapping the other end of a corresponding active region, contacting the other side of a corresponding word line structure, and comprising a second material different from the first material; and pad insulating regions, each pad insulating region disposed between the corresponding bit line pad regions and each memory node pad region spaced apart in the first direction.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Cross-references to related applications

[0002] This patent document claims priority and benefit to Korean Patent Application No. 10-2025-0062249, filed on May 14, 2025, the entire contents of which are incorporated herein by reference as part of the disclosure of this patent document. Technical Field

[0003] The embodiments of this disclosure generally relate to semiconductor devices and methods of manufacturing the same, and more specifically to semiconductor devices comprising a plurality of active regions. Background Technology

[0004] Among various semiconductor devices, those with storage capabilities, used for storing information, may include an array comprising multiple memory cells, each memory cell including a transistor. For example, a semiconductor device with storage capabilities may include Dynamic Random Access Memory (DRAM). DRAM may include bit lines and word lines that may intersect each other in a vertical direction. The bit lines and word lines may extend across the array comprising memory cells. The bit lines and word lines can be used to access individual memory cells.

[0005] Memory performance, cell stability and reliability, power efficiency, ease of fabrication, and cost can vary depending on how individual memory cells are designed and placed. Therefore, research on cell array design and manufacturing processes for memory devices is actively underway. Summary of the Invention

[0006] Various embodiments of this disclosure relate to a semiconductor device that addresses the existing problem of bridging in adjacent active regions during semiconductor device manufacturing processes, leading to decreased reliability of the semiconductor device.

[0007] Various embodiments of this disclosure relate to a semiconductor device that addresses the existing problem that increases contact resistance when the size of the contact area where the bit line contact or memory node contact overlaps with the active region decreases.

[0008] According to one embodiment of this disclosure, a semiconductor device may include: a plurality of word line structures configured to extend along a first direction and spaced apart from each other in a second direction; a plurality of active regions configured to extend along a diagonal direction at an acute angle to the first direction and overlap with the plurality of word line structures and spaced apart from each other in the first direction; a plurality of bit line pad regions, each bit line pad region overlapping one end of a corresponding active region among the plurality of active regions, contacting one side of a corresponding word line structure among the plurality of word line structures, and including a first material; a plurality of memory node pad regions, each memory node pad region overlapping the other end of a corresponding active region among the plurality of active regions, contacting the other side of a corresponding word line structure among the plurality of word line structures, and including a second material different from the first material; and a plurality of pad insulating regions, each pad insulating region being disposed between a corresponding bit line pad region among the plurality of bit line pad regions spaced apart from each other in the first direction and each memory node pad region among the plurality of memory node pad regions.

[0009] In some implementations, the concentration of impurities in the first material may be higher than the concentration of impurities in the second material.

[0010] In some implementations, the first material may be polycrystalline silicon containing impurities; the second material may be monocrystalline silicon.

[0011] In some implementations, the height of each bit line pad area among the plurality of bit line pad areas may be equal to the height of each memory node pad area among the plurality of memory node pad areas; and the height of each bit line pad area among the plurality of bit line pad areas may be equal to the height of each pad insulation area among the plurality of pad insulation areas.

[0012] In some implementations, each of the plurality of bit line pad areas, each of the plurality of memory node pad areas, and each of the plurality of pad insulation areas may be disposed on the same plane as the surface of the plurality of active areas.

[0013] In some implementations, the second direction may be perpendicular to the first direction; and the second direction may form an acute angle with the diagonal direction.

[0014] In some implementations, the angle between the diagonal direction and the first direction can be in the range of 30 to 60 degrees.

[0015] In some implementations, the semiconductor device may further include: a plurality of bit line contact regions, each bit line contact region contacting the top surface of a corresponding bit line pad region among the plurality of bit line pad regions; a plurality of bit line electrode layers, each bit line electrode layer disposed above a corresponding bit line contact region among the plurality of bit line contact regions, overlapping with a corresponding bit line pad region among the plurality of bit line pad regions, and extending along a second direction; a plurality of bit line spacers, each bit line spacer contacting two sides of a corresponding bit line electrode layer among the plurality of bit line electrode layers, and extending along the second direction; and a plurality of memory node contact regions, each memory node contact region contacting the top surface of a corresponding memory node pad region.

[0016] In some implementations, the plurality of active regions may be further arranged to be spaced apart from each other in a second direction and also spaced apart from each other in a diagonal direction.

[0017] In some implementations, the plurality of bit line pad areas may be arranged to be spaced apart from each other in a second direction; the plurality of memory node pad areas may also be arranged to be spaced apart from each other in a second direction.

[0018] According to another embodiment of this disclosure, a method of manufacturing a semiconductor device may include: forming a plurality of active regions, the plurality of active regions being repeatedly spaced apart from each other in a first direction and a second direction, extending along a diagonal direction relative to the first direction, and surrounded by a cell isolation region; forming a plurality of first pad regions, each first pad region overlapping one end of a corresponding active region among the plurality of active regions and extending along the second direction; forming a plurality of pad insulating regions, each pad insulating region contacting two sides of each of the plurality of first pad regions and extending along the second direction; and forming a plurality of second pad regions, the plurality of second pad regions overlapping the other end of a corresponding active region among the plurality of active regions, extending along the second direction, and spaced apart from the plurality of first pad regions.

[0019] In some implementations, the method may further include: forming an active layer over the plurality of active regions and cell isolation regions, wherein forming the plurality of first pad regions includes: removing a portion of the active layer.

[0020] In some implementations, the method may further include: forming a plurality of fill regions between the plurality of first pad regions, wherein forming the plurality of pad insulating regions includes: removing a portion of each of the plurality of fill regions.

[0021] In some implementations, the method may further include: forming a plurality of word line structures that overlap with the center of the plurality of active regions, extend along a first direction, and are repeatedly spaced apart from each other in a second direction.

[0022] In some implementations, forming the plurality of word line structures may include cutting a portion of each of the plurality of first pad areas, a portion of each of the plurality of second pad areas, and a portion of each of the plurality of pad insulating areas.

[0023] In some implementations, the method may further include: forming a plurality of bit line electrode layers that overlap with the plurality of first pad regions and extend along a second direction; and forming a plurality of memory node contact regions that overlap with the plurality of second pad regions.

[0024] In some implementations, the method may further include: forming a plurality of bit line contact regions, each bit line contact region being disposed between a corresponding bit line electrode layer among the plurality of bit line electrode layers and a corresponding first pad region among the plurality of first pad regions; forming a plurality of bit line spacers, each bit line spacer contacting two sides of each bit line electrode layer among the plurality of bit line electrode layers and extending along a second direction; forming a plurality of bit line cover layers, each bit line cover layer contacting the top surface of a corresponding bit line electrode layer among the plurality of bit line electrode layers; and forming a plurality of contact insulation regions, each contact insulation region being disposed between the plurality of memory node contact regions adjacent to each other in the second direction.

[0025] It should be understood that the above general description of this disclosure and the following detailed description are exemplary and explanatory, and are intended to further explain this disclosure. Attached Figure Description

[0026] The above and other features and advantages of this disclosure will become apparent from the following detailed description taken in conjunction with the accompanying drawings.

[0027] Figure 1 This is a circuit diagram illustrating an example of a modeling circuit for a unit cell of a semiconductor device according to an embodiment of the present disclosure.

[0028] Figure 2 This is a first plan view illustrating a portion of a semiconductor device according to an embodiment of the present disclosure.

[0029] Figure 3 This is a second plan view illustrating a portion of a semiconductor device according to an embodiment of the present disclosure.

[0030] Figure 4 This illustrates an embodiment of the present disclosure. Figure 2 and Figure 3 A cross-sectional view of an example structure of a semiconductor device, taken by line A-A'.

[0031] Figure 5This illustrates an embodiment of the present disclosure. Figure 2 and Figure 3 A cross-sectional view of an example structure of a semiconductor device, taken by the B-B' line.

[0032] Figure 6 This illustrates an embodiment of the present disclosure. Figure 2 and Figure 3 A cross-sectional view of an example structure of a semiconductor device taken by the C-C' line.

[0033] Figure 7 This illustrates an embodiment of the present disclosure. Figure 2 and Figure 3 A cross-sectional view of an example structure of a semiconductor device, taken by the D-D' line.

[0034] Figure 8 This illustrates an embodiment of the present disclosure. Figure 2 and Figure 3 A cross-sectional view of an example structure of a semiconductor device taken by the E-E' line.

[0035] Figure 9 This is a flowchart illustrating an example of a method for manufacturing a semiconductor device according to an embodiment of the present disclosure.

[0036] Figure 10A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S10 in the diagram.

[0037] Figure 10B This illustrates an embodiment of the present disclosure. Figure 10A A cross-sectional view of an example structure of a semiconductor device, taken by line A-A'.

[0038] Figure 10C This illustrates an embodiment of the present disclosure. Figure 10A A cross-sectional view of an example structure of a semiconductor device, taken by the B-B' line.

[0039] Figure 10D This illustrates an embodiment of the present disclosure. Figure 10A A cross-sectional view of an example structure of a semiconductor device taken by the C-C' line.

[0040] Figure 10E This illustrates an embodiment of the present disclosure. Figure 10A A cross-sectional view of an example structure of a semiconductor device, taken by the D-D' line.

[0041] Figure 10F This illustrates an embodiment of the present disclosure. Figure 10A A cross-sectional view of an example structure of a semiconductor device taken by the E-E' line.

[0042] Figure 11A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S20.

[0043] Figure 11B This illustrates an embodiment of the present disclosure. Figure 11A A cross-sectional view of an example structure of a semiconductor device, taken by line A-A'.

[0044] Figure 11C This illustrates an embodiment of the present disclosure. Figure 11A A cross-sectional view of an example structure of a semiconductor device, taken by the B-B' line.

[0045] Figure 11D This illustrates an embodiment of the present disclosure. Figure 11A A cross-sectional view of an example structure of a semiconductor device taken by the C-C' line.

[0046] Figure 11E This illustrates an embodiment of the present disclosure. Figure 11A A cross-sectional view of an example structure of a semiconductor device, taken by the D-D' line.

[0047] Figure 11F This illustrates an embodiment of the present disclosure. Figure 11A A cross-sectional view of an example structure of a semiconductor device taken by the E-E' line.

[0048] Figure 12A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S30 in the diagram.

[0049] Figure 12B This illustrates an embodiment of the present disclosure. Figure 12A A cross-sectional view of an example structure of a semiconductor device, taken by line A-A'.

[0050] Figure 12C This illustrates an embodiment of the present disclosure. Figure 12A A cross-sectional view of an example structure of a semiconductor device, taken by the B-B' line.

[0051] Figure 12D This illustrates an embodiment of the present disclosure. Figure 12A A cross-sectional view of an example structure of a semiconductor device taken by the C-C' line.

[0052] Figure 12E This illustrates an embodiment of the present disclosure. Figure 12A A cross-sectional view of an example structure of a semiconductor device, taken by the D-D' line.

[0053] Figure 12F This illustrates an embodiment of the present disclosure. Figure 12A A cross-sectional view of an example structure of a semiconductor device taken by the E-E' line.

[0054] Figure 13A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S40 in the diagram.

[0055] Figure 13B This illustrates an embodiment of the present disclosure. Figure 13A A cross-sectional view of an example structure of a semiconductor device, taken by line A-A'.

[0056] Figure 13C This illustrates an embodiment of the present disclosure. Figure 13A A cross-sectional view of an example structure of a semiconductor device, taken by the B-B' line.

[0057] Figure 13D This illustrates an embodiment of the present disclosure. Figure 13A A cross-sectional view of an example structure of a semiconductor device taken by the C-C' line.

[0058] Figure 13E This illustrates an embodiment of the present disclosure. Figure 13A A cross-sectional view of an example structure of a semiconductor device, taken by the D-D' line.

[0059] Figure 13F This illustrates an embodiment of the present disclosure. Figure 13A A cross-sectional view of an example structure of a semiconductor device taken by the E-E' line.

[0060] Figure 14A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S50 in the diagram.

[0061] Figure 14B This illustrates an embodiment of the present disclosure. Figure 14A A cross-sectional view of an example structure of a semiconductor device, taken by line A-A'.

[0062] Figure 14C This illustrates an embodiment of the present disclosure. Figure 14A A cross-sectional view of an example structure of a semiconductor device, taken by the B-B' line.

[0063] Figure 14D This illustrates an embodiment of the present disclosure. Figure 14A A cross-sectional view of an example structure of a semiconductor device taken by the C-C' line.

[0064] Figure 14E This illustrates an embodiment of the present disclosure. Figure 14A A cross-sectional view of an example structure of a semiconductor device, taken by the D-D' line.

[0065] Figure 14F This illustrates an embodiment of the present disclosure. Figure 14A A cross-sectional view of an example structure of a semiconductor device taken by the E-E' line.

[0066] Figure 15A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S60 in the diagram.

[0067] Figure 15B This illustrates an embodiment of the present disclosure. Figure 15A A cross-sectional view of an example structure of a semiconductor device, taken by line A-A'.

[0068] Figure 15C This illustrates an embodiment of the present disclosure. Figure 15A A cross-sectional view of an example structure of a semiconductor device, taken by the B-B' line.

[0069] Figure 15D This illustrates an embodiment of the present disclosure. Figure 15A A cross-sectional view of an example structure of a semiconductor device taken by the C-C' line.

[0070] Figure 15E This illustrates an embodiment of the present disclosure. Figure 15A A cross-sectional view of an example structure of a semiconductor device, taken by the D-D' line.

[0071] Figure 15F This illustrates an embodiment of the present disclosure. Figure 15A A cross-sectional view of an example structure of a semiconductor device taken by the E-E' line.

[0072] Figure 16A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S70 in the diagram.

[0073] Figure 16B This illustrates an embodiment of the present disclosure. Figure 16A A cross-sectional view of an example structure of a semiconductor device, taken by line A-A'.

[0074] Figure 16C This illustrates an embodiment of the present disclosure. Figure 16A A cross-sectional view of an example structure of a semiconductor device, taken by the B-B' line.

[0075] Figure 16D This illustrates an embodiment of the present disclosure. Figure 16A A cross-sectional view of an example structure of a semiconductor device taken by the C-C' line.

[0076] Figure 16E This illustrates an embodiment of the present disclosure. Figure 16A A cross-sectional view of an example structure of a semiconductor device, taken by the D-D' line.

[0077] Figure 16F This illustrates an embodiment of the present disclosure. Figure 16A A cross-sectional view of an example structure of a semiconductor device taken by the E-E' line.

[0078] Figure 17A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of example results of operation S80 in the diagram.

[0079] Figure 17B This illustrates an embodiment of the present disclosure. Figure 17A A cross-sectional view of an example structure of a semiconductor device, taken by line A-A'.

[0080] Figure 17C This illustrates an embodiment of the present disclosure. Figure 17A A cross-sectional view of an example structure of a semiconductor device, taken by the B-B' line.

[0081] Figure 17D This illustrates an embodiment of the present disclosure. Figure 17A A cross-sectional view of an example structure of a semiconductor device taken by the C-C' line.

[0082] Figure 17E This illustrates an embodiment of the present disclosure. Figure 17A A cross-sectional view of an example structure of a semiconductor device, taken by the D-D' line.

[0083] Figure 17F This illustrates an embodiment of the present disclosure. Figure 17A A cross-sectional view of an example structure of a semiconductor device taken by the E-E' line.

[0084] Figure 18A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S90 in the diagram.

[0085] Figure 18B This illustrates an embodiment of the present disclosure. Figure 18A A cross-sectional view of an example structure of a semiconductor device, taken by line A-A'.

[0086] Figure 18C This illustrates an embodiment of the present disclosure. Figure 18A A cross-sectional view of an example structure of a semiconductor device, taken by the B-B' line.

[0087] Figure 18D This illustrates an embodiment of the present disclosure. Figure 18A A cross-sectional view of an example structure of a semiconductor device taken by the C-C' line.

[0088] Figure 18E This illustrates an embodiment of the present disclosure. Figure 18A A cross-sectional view of an example structure of a semiconductor device, taken by the D-D' line.

[0089] Figure 18F This illustrates an embodiment of the present disclosure. Figure 18A A cross-sectional view of an example structure of a semiconductor device taken by the E-E' line. Detailed Implementation

[0090] This disclosure provides embodiments and examples of semiconductor devices comprising multiple active regions and methods for manufacturing the semiconductor device, which can be used in a variety of configurations to substantially solve one or more technical or engineering problems and mitigate limitations or disadvantages encountered in some semiconductor devices in the art. Some embodiments of this disclosure relate to a semiconductor device that addresses existing problems such as bridging between adjacent active regions and reduced reliability of the semiconductor device when word lines are misaligned during the manufacturing process. Some embodiments of this disclosure relate to a semiconductor device that addresses existing problems such as increased contact resistance when the size of the contact area where bit line contacts or memory node contacts overlap with active regions decreases. In view of the above problems, this disclosure may provide a semiconductor device in which bridging that may occur between adjacent active regions can be prevented. This disclosure may provide a semiconductor device with improved operating speed and reduced leakage current. This disclosure may provide a semiconductor device in which active regions are defined by forming relatively shallow cell isolation regions, thereby reducing process complexity.

[0091] The embodiments of this disclosure will now be described in detail with reference to examples shown in the accompanying drawings. In the drawings, the same reference numerals are used wherever possible to refer to the same or similar parts. While various modifications and alternative forms may be made to this disclosure, specific embodiments are shown in the drawings by way of example only. However, this disclosure should not be construed as being limited to the embodiments described herein.

[0092] Various embodiments will be described below with reference to the accompanying drawings. However, it should be understood that this disclosure is not limited to the specific embodiments, but includes various modifications, equivalents, and / or alternatives. The embodiments of this disclosure can provide a variety of effects, which can be directly or indirectly identified by this disclosure.

[0093] In describing the components of embodiments of this disclosure, terms such as "first" and "second" are used only to distinguish different components, but the nature, order, and sequence of the components are not limited to these terms. Unless otherwise specified, all terms used in this disclosure, including technical and scientific terms, shall have the meanings commonly understood by one of ordinary skill in the art to which this disclosure pertains. Furthermore, it should be understood that terms defined in common dictionaries should have the same meaning as those in the relevant technical field and in this disclosure, and should not be interpreted in an idealized or overly formal manner unless expressly defined herein.

[0094] Figure 1 This is a circuit diagram illustrating a modeling circuit of a unit cell (UC) of a semiconductor device according to an embodiment of the present disclosure.

[0095] refer to Figure 1 According to one embodiment of the present disclosure, a unit cell (UC) of a semiconductor device may include a transistor (TX) and a capacitor (CAP). The unit cell (UC) may be a unit in the semiconductor device used for storing data. The semiconductor device according to one embodiment of the present disclosure can be used as a data storage device and may be included in various electronic devices (e.g., computers). In some implementations, the semiconductor device may be a volatile memory device (e.g., dynamic random access memory (DRAM)) or a non-volatile memory device (e.g., NAND memory).

[0096] A transistor (TX) can be a switching element between a bit line (BL) and a capacitor (CAP). A transistor (TX) can be, for example, a metal-oxide-semiconductor field-effect transistor (MOSFET). A transistor (TX) can operate by an electric field generated by a voltage applied to its gate terminal. When the transistor (TX) is turned on, the bit line (BL) and the capacitor (CAP) are electrically connected to each other. When the transistor (TX) is turned off, the electrical connection between the bit line (BL) and the capacitor (CAP) is prevented.

[0097] The word line (WL) adjusts (controls) the on / off state of the transistor (TX). For example, when the word line signal applied to the word line (WL) has a logic high level, the transistor (TX) can be turned on. On the other hand, when the word line signal applied to the word line (WL) has a logic low level, the transistor (TX) can be turned off.

[0098] Bit lines (BLs) can be interconnect structures designed to transmit data. When a transistor (TX) is turned on, the bit line (BL) can transfer charge to a capacitor (CAP). When a bit line signal applied to the bit line (BL) is high and the transistor (TX) is on, data "1" can be stored in the capacitor (CAP). When a bit line signal applied to the bit line (BL) is low and the transistor (TX) is on, data "0" can be stored in the capacitor (CAP).

[0099] A capacitor (CAP) can be a data storage device. For example, a second capacitor (CAP) may include, but is not limited to, at least one of a metal-insulator-metal (MIM) capacitor, a metal-oxide-metal (MOM) capacitor, or a metal-oxide-semiconductor (MOS) capacitor. When the charge stored in the capacitor (CAP) reaches or exceeds a predetermined level, the unit cell (UC) may be in a state storing data "1". When the charge stored in the capacitor (CAP) is less than or equal to the predetermined level, the unit cell (UC) may be in a state storing data "0".

[0100] In the operation of writing the data "1" to the unit cell (UC), a high-level bit line signal can be applied to the bit line (BL) and a high-level word line signal can be applied to the word line (WL). When the transistor (TX) is turned on by the high-level word line signal, the bit line (BL) can act as the drain terminal of the transistor (TX), and the capacitor (CAP) can act as the source terminal of the transistor (TX). The potential level of the capacitor (CAP) can be raised (or increased) by the high-level bit line signal, thereby writing the data "1" to the unit cell (UC).

[0101] In the operation of writing the data "0" to the unit cell (UC), a low-level bit line signal can be applied to the bit line (BL), and a high-level word line signal can be applied to the word line (WL). When the transistor (TX) is turned on, the bit line (BL) can act as the source terminal of the transistor (TX), the capacitor (CAP) can act as the drain terminal, and the potential level of the capacitor (CAP) can be reduced (or lowered) by the low-level bit line signal, thereby writing the data "0" to the unit cell (UC).

[0102] In the operation of reading data from a unit cell (UC), the reference level of the bit line signal can be between high and low, while the word line signal can be high. When data "1" is written (stored) into the unit cell (UC) and the transistor (TX) is turned on, the potential level of the capacitor (CAP) is high, so the level of the bit line signal can become higher than the reference level. When data "0" is recorded in the unit cell (UC) and the transistor (TX) is turned on, the potential level of the capacitor (CAP) is low, so the level of the bit line signal can become lower than the reference level. The semiconductor device can determine whether the level of the bit line signal has become higher than the reference level and can read the data from the unit cell (UC) based on the determination result.

[0103] Figure 2 This is a first plan view illustrating a portion of a semiconductor device 1 according to an embodiment of the present disclosure.

[0104] Figure 3 This is a second plan view illustrating a portion of a semiconductor device 1 according to an embodiment of the present disclosure.

[0105] refer to Figure 1 , Figure 2 and Figure 3 The first and second plan views exemplarily illustrate the positional relationship between the plurality of active regions 100 and the peripheral structures. The first plan view shows the positional relationship between the plurality of active regions 100, the plurality of word line structures 300, and the peripheral structures disposed on the surface of a predetermined semiconductor layer. The second plan view shows the positional relationship between the plurality of active regions 100 and the peripheral structures disposed below the surface of the predetermined semiconductor layer.

[0106] Semiconductor device 1 may include the plurality of active regions 100, cell isolation regions 200, the plurality of word line structures 300, the plurality of bit line electrode layers 410, the plurality of bit line spacers 420, the plurality of bit line pad regions 430, the plurality of memory node pad regions 530, the plurality of memory node contact regions 540, and the plurality of pad insulating layers 700.

[0107] Each of the plurality of active regions 100 may include a semiconductor material (e.g., silicon (Si), silicon carbide (SiC), etc.). Each of the plurality of active regions 100 may be surrounded by a cell isolation region 200. For example, the plurality of active regions 100 may be arranged in a matrix structure. The plurality of active regions 100 may be arranged in an (m×n) matrix structure (where "m" is an integer greater than or equal to 2, and "n" is an integer greater than or equal to 2). Each of the plurality of active regions 100 may extend along a diagonal direction (DG). The diagonal direction (DG) may be a diagonal direction relative to a first direction (X). The angle between the diagonal direction (DG) and the first direction (X) may be an acute angle. Some of the plurality of active regions 100 may be repeated to be spaced apart from each other in the first direction (X). Some of the plurality of active regions 100 may be repeated to be spaced apart from each other in a second direction (Y) perpendicular to the first direction (X). Some of the plurality of active regions 100 may be arranged repeatably to be spaced apart from each other in a diagonal direction (DG). The angle between the diagonal direction (DG) and the second direction (Y) may be an acute angle. The acute angle between the first direction (X) and the diagonal direction (DG) may be in the range of about 30 degrees to about 60 degrees. Each of the plurality of active regions 100 may overlap with the word line structure 300. Although the shape of each active region 100 is similar to a parallelogram for illustrative purposes, the scope of this disclosure is not limited thereto. For example, each of the four corner regions of the active region 100 may be circular. Each of the plurality of active regions 100 may include a region of a channel forming a transistor (TX) of a unit cell (UC). Each of the plurality of active regions 100 may be surrounded by a cell isolation region 200. One end of each of the plurality of active regions 100 may overlap with the bit line electrode layer 410. One end of each of the plurality of active regions 100 may overlap with the storage node contact area 540. One end of each of the plurality of active regions 100 may overlap with the bit line pad area 430. The other end of each of the plurality of active regions 100 may overlap with the storage node pad area 530.

[0108] The unit isolation region 200 may include an insulating material. For example, the unit isolation region 200 may include at least one of silicon oxide or silicon-on-insulator (SOI) structures. The unit isolation region 200 may surround each of the plurality of active regions 100. The unit isolation region 200 may provide electrical insulation between the plurality of active regions 100 that are spaced apart from each other.

[0109] Each of the plurality of word line structures 300 may extend along a first direction (X). The plurality of word line structures 300 may be spaced apart from each other in a second direction (Y). Each of the plurality of word line structures 300 may include a predetermined electrode layer to which a word line signal is applied. When the word line signal in the electrode layer included in the word line structure 300 has a high level, a predetermined channel may be formed within the active region 100 overlapping with the word line structure 300. Each of the plurality of word line structures 300 may overlap with each of the plurality of active regions 100 spaced apart from each other in the first direction (X). Although each of the plurality of word line structures 300 may be formed to pass through the center of each of the plurality of active regions 100 spaced apart from each other in the first direction (X), other implementations may also be provided according to this disclosure. Because the center of each word line structure 300 extends closer to the center of the active region 100 along the first direction (X), the overlap between the active region 100 and each of the bit line pad region 430 and the memory node pad region 530 can be reliably ensured, thereby improving the reliability of the semiconductor device 1. The internal structure of the word line structure 300 will be referenced. Figure 4 And will be described below.

[0110] Each of the plurality of bit line electrode layers 410 may include a conductive material. For example, each of the plurality of bit line electrode layers 410 may include a metallic material, such as aluminum (Al), copper (Cu), or tungsten (W). Each of the plurality of bit line electrode layers 410 may extend along a second direction (Y). The plurality of bit line electrode layers 410 may be spaced apart from each other in a first direction (X). The first direction (X) and the second direction (Y) may be perpendicular to each other. Each of the plurality of bit line electrode layers 410 may be an electrode layer for applying bit line signals. Each of the plurality of bit line electrode layers 410 may overlap with the plurality of bit line pad areas 430 arranged spaced apart from each other in the second direction (Y). Each of the plurality of bit line electrode layers 410 may intersect (cross) with the plurality of word line structures 300. Two sides of each of the plurality of bit line electrode layers 410 may contact the bit line spacers 420. Each of the plurality of bit line electrode layers 410 may overlap one end of each active region 100.

[0111] Each of the plurality of bit line spacers 420 may include an insulating material. For example, each of the plurality of bit line spacers 420 may include an insulating material such as silicon oxide or silicon nitride. Each of the plurality of bit line spacers 420 may extend along a second direction (Y). The plurality of bit line spacers 420 may be spaced apart from each other in a first direction (X). The plurality of bit line spacers 420 may prevent electrical interaction between the spaced-apart bit line electrode layers 410. The plurality of bit line spacers 420 may be formed in a pair, and a pair of bit line spacers 420 may contact two sides of the bit line electrode layer 410.

[0112] Each of the plurality of bit line pad regions 430 may include a conductive material. For example, each of the plurality of bit line pad regions 430 may include polysilicon. For example, the polysilicon may include predetermined impurities to improve conductivity. In another embodiment, each of the plurality of bit line pad regions 430 may include silicide. Each of the plurality of bit line pad regions 430 may be configured to transmit a bit line signal applied to the bit line electrode layer 410 to the active region 100. When the plurality of bit line pad regions 430 include polysilicon or silicide doped with predetermined impurities, the carrier concentration may increase, thereby improving conductivity and reducing junction resistance, and thus improving the operating characteristics of the semiconductor device 1. Each of the plurality of bit line pad regions 430 may be disposed between two adjacent word line structures 300. For example, each of the plurality of bit line pad regions 430 may contact two sides of two adjacent word line structures 300 facing each other. Bit line pad areas 430 may overlap with one end of active region 100. In any active region 100, bit line pad areas 430 may contact one side of word line structure 300 covering active region 100. Bit line pad areas 430 may also contact word line structures 300 that are spaced apart from active region 100 in a direction opposite to the second direction (Y) and covering active region 100. Some of the plurality of bit line pad areas 430 may be spaced apart from each other in the first direction (X). Others of the plurality of bit line pad areas 430 may be spaced apart from each other in the second direction (Y).

[0113] Each of the plurality of memory node pad regions 530 may include a material different from that of the bit line pad region 430. For example, each of the plurality of memory node pad regions 530 may include silicon. For example, each of the plurality of memory node pad regions 530 may include, for example, monocrystalline silicon formed from the active region 100 by an epitaxial growth process. Each of the plurality of memory node pad regions 530 may include impurity-free silicon.

[0114] As the number of charge traps in the storage node pad area 530 increases, the charge stored in the capacitor (CAP) may leak into the charge traps of the storage node pad area 530 and may not be able to be stored in the capacitor (CAP) again, leading to the possibility of data loss. Therefore, when the storage node pad area 530 includes a material with low charge trap density (e.g., impurity-free monocrystalline silicon), charge leakage from the capacitor (CAP) can be reduced, thereby improving data reliability and extending data retention time.

[0115] Each of the plurality of memory node pad areas 530 may be disposed between two adjacent word line structures 300. For example, each of the plurality of memory node pad areas 530 may contact two facing sides of two adjacent word line structures 300. The memory node pad area 530 may overlap with another end of the active region 100, which is opposite to one end of the active region 100. In any given active region 100, the memory node pad area 530 may contact one side of the word line structure 300 that overlaps with the active region 100. The memory node pad area 530 may also contact word line structures 300 that are spaced apart from and overlap with the active region 100 in a second direction (Y). Some of the plurality of memory node pad areas 530 may be arranged to be spaced apart from each other in a first direction (X). Others of the plurality of memory node pad areas 530 may be arranged to be spaced apart from each other in a second direction (Y).

[0116] Each of the plurality of memory node contact areas 540 may include a conductive material. For example, each of the plurality of memory node contact areas 540 may include at least one of polysilicon, aluminum, copper, or titanium. The polysilicon may include predetermined impurities to improve conductivity. Each memory node contact area 540 may be disposed between two adjacent bit lines. The memory node contact areas 540 may overlap with the other end of the active region 100. Some memory node contact areas 540 may overlap with the word line structure 300 covering the active region 100. The plurality of memory node contact areas 540 may be spaced apart from each other in a first direction (X). The plurality of memory node contact areas 540 may be spaced apart from each other in a second direction (Y).

[0117] Each of the plurality of pad insulating regions 700 electrically isolates adjacent bit line pad regions 430 from memory node pad regions 530. Each of the plurality of pad insulating regions 700 may be disposed between adjacent bit line pad regions 430 and memory node pad regions 530. For example, each of the plurality of pad insulating regions 700 may be disposed between bit line pad regions 430 and memory node pad regions 530 spaced apart in a first direction (X). The plurality of pad insulating regions 700 may be repeatedly spaced apart from each other in the first direction (X) and the second direction (Y). Each of the plurality of pad insulating regions 700 may include an insulating material. For example, each of the plurality of pad insulating regions 700 may include an insulating material such as silicon oxide or silicon nitride.

[0118] Figure 4 According to an embodiment of this disclosure Figure 2 and Figure 3 The cross-sectional view of an example structure of semiconductor device 1 taken by line A-A' in the figure.

[0119] refer to Figure 2 , Figure 3 and Figure 4 The first cross section (CS1) may include a substrate region 10, an active region 100, a cell isolation region 200, a word line structure 300, a bit line structure 400, a memory node pad region 530, a memory node contact region 540, and a pad insulation region 700.

[0120] The substrate region 10 may be a semiconductor region disposed below the active region 100. The substrate region 10 may include a semiconductor material. For example, the substrate region 10 may include at least one of silicon, silicon-germanium, or a combination thereof.

[0121] Active region 100 may be disposed above substrate region 10 and may extend to the surface of semiconductor layer (SL) (i.e., the top surface shown in the figure). Active region 100 may contact the side and bottom surfaces of word line structure 300. For example, active region 100 may surround the side and bottom surfaces of word line insulating layer 340. When a channel is formed in active region 100, charge carriers may move from bit line electrode layer 410 to bit line contact region 440, bit line pad region 430, active region 100, memory node pad region 530 and memory node contact region 540, and may ultimately move to a capacitor (not shown) connected above memory node contact region 540. Figure 1 (CAP in the text). Furthermore, these charge carriers can also move from the capacitor to the bit line electrode layer 410 in the opposite direction to the aforementioned movement direction. Two sides of the active region 100 can contact the cell isolation region 200. When moving towards the word line (reference... Figure 1 When the operating voltage is applied to the WL in the word line, a channel can be formed near the word line insulation layer 340.

[0122] Cell isolation region 200 may contact the side surface of active region 100. The top surface of cell isolation region 200 may contact pad insulating region 700. Cell isolation region 200 may form a recess at a predetermined distance from the surface of semiconductor layer (SL). The predetermined distance of the cell isolation region 200 from the surface of semiconductor layer (SL) may be, for example, about 1600 Å to about 1900 Å, but embodiments of this disclosure are not limited thereto. In an exemplary embodiment, if the thickness of bit line pad region 430 or memory node pad region 530 in the horizontal direction (e.g., in the X direction or DG direction) is greater than... Figure 3 and Figure 4 If the thickness is greater, the top surface of the cell isolation area 200 can also contact the bit line pad area 430 or the storage node pad area 530.

[0123] The word line structure 300 may include a first word line electrode layer 310, a second word line electrode layer 320, a word line cover layer 330, and a word line insulating layer 340. The word line structure 300 may extend (or be recessed) in the third direction (Z) from the same plane as the top surface of the bit line pad region 430 into the semiconductor layer (SL) to a predetermined depth. The X, Y, and Z directions may be orthogonal to each other, for example, forming a Cartesian coordinate system. The word line structure 300 is preferably formed in the central region of the active region 100, but may vary depending on manufacturing process limitations, variables, and defects. Here, the predetermined depth may be, for example, from about 1000 Å to about 1300 Å, but embodiments of this disclosure are not limited thereto. In this disclosure, the surface of the semiconductor layer (SL) may be defined as being in the same plane as the top surface of the active region 100 or the top surface of the cell isolation region 200.

[0124] The first word line electrode layer 310 may include a conductive material. For example, the first word line electrode layer 310 may include tungsten, aluminum, copper, tungsten nitride, tungsten silicide, cobalt silicide, titanium silicide, tantalum nitride, or a combination thereof. The first word line electrode layer 310 may be disposed below the second word line electrode layer 320. The sides and bottom of the first word line electrode layer 310 may be surrounded by a word line insulating layer 340.

[0125] The second word line electrode layer 320 may include a conductive material. For example, the second word line electrode layer 320 may include tungsten, aluminum, copper, tungsten nitride, tungsten silicide, cobalt silicide, titanium silicide, tantalum nitride, or a combination thereof. The second word line electrode layer 320 may be a region implanted with predetermined impurities (e.g., phosphorus, germanium, etc.). The second word line electrode layer 320 may be disposed above the first word line electrode layer 310. The second word line electrode layer 320 may be disposed below the word line cover layer 330. Two sides of the second word line electrode layer 320 may contact the word line insulating layer 340.

[0126] Although not shown in the figure, a predetermined antioxidant layer may be provided between the first word line electrode layer 310 and the second word line electrode layer 320. The predetermined antioxidant layer may capture (or collect) impurities (e.g., oxygen) contained in the first and second word line electrode layers (310, 320).

[0127] Both the first and second word line electrode layers (310, 320) can receive word line signals as input. When the word line signal is high, a channel for charge movement can be formed around the word line structure 300 within the active region 100. When the word line signal is low, the channel may not be formed. When the channel is formed, the bit line electrode layer 410 and the memory node contact area 540 can be electrically connected to each other. For example, in the operation of recording data "1", when a high-level bit line signal is applied to the bit line electrode layer 410 and word line signals are applied to the first and second word line electrode layers (310, 320), charge can move to the memory node contact area 540 via the bit line contact area 440, the bit line pad area 430, the channel, and the memory node pad area 530 according to the bit line signal of the bit line electrode layer 410. Since the memory node contact area 540 can be electrically connected to a predetermined capacitor structure (not shown), charge can be stored in the capacitor structure through the memory node contact area 540. The capacitor structure can be modeled as a circuit diagram, such as... Figure 1 Capacitors (CAPs) in the system.

[0128] The word line overlay 330 may include an insulating material. For example, the word line overlay 330 may include silicon nitride, silicon oxide, silicon oxynitride, or a combination thereof. The word line overlay 330 may be disposed above the second word line electrode layer 320. The word line overlay 330 may be a region filled with insulating material located between the surface of the semiconductor layer (SL) and the top surface of the second word line electrode layer 320. The word line overlay 330 may electrically isolate the first word line electrode layer (310) and the second word line electrode layer (320) from the bit line structure 400. The word line overlay 330 may electrically isolate the first word line electrode layer (310) and the second word line electrode layer (320) from the memory node contact region 540. Although, for ease of description, the depth of the word line overlay 330 to the surface of the semiconductor layer (SL) shown in the figures is shallower than the depth of the bit line pad region 430 or the depth of the memory node pad region 530, other embodiments may be provided according to this disclosure. According to another embodiment, the depth of the word line overlay 330 may also be deeper than the depth of the bit line pad area 430 and the depth of the memory node pad area 530.

[0129] The word line insulating layer 340 may include an insulating material. For example, the word line insulating layer 340 may include silicon oxide, hafnium oxide, hafnium silicon oxide, hafnium silicon oxynitride, or a combination thereof. The word line insulating layer 340 may be formed along the side and bottom surfaces of the word line structure 300. The word line insulating layer 340 may physically isolate the first and second word line electrode layers (310, 320) from the active region 100. The word line insulating layer 340 may electrically isolate the first and second word line electrode layers (310, 320) from the memory node pad region 530. The word line insulating layer 340 may also electrically isolate the first and second word line electrode layers (310, 320) from the memory node pad region 530.

[0130] The bitline structure 400 may include a bitline electrode layer 410, a bitline spacer 420, a bitline pad area 430, a bitline contact area 440, and a bitline cover layer 450.

[0131] Bit line electrode layer 410 may include a conductive material. For example, bit line electrode layer 410 may include tungsten, aluminum, copper, tungsten nitride, tungsten silicide, cobalt silicide, titanium silicide, tantalum nitride, or combinations thereof. Bit line electrode layer 410 may be spaced apart from the surface of semiconductor layer (SL). Bit line electrode layer 410 may be spaced apart from bit line pad area 430. When viewed along a third direction (Z), bit line electrode layer 410 may overlap with bit line pad area 430. Bit line electrode layer 410 may also overlap with word line structure 300. Each side of bit line electrode layer 410 may contact bit line spacer 420. Bit line electrode layer 410 may be disposed below bit line cover layer 450.

[0132] Bit line spacer 420 may include an insulating material. For example, bit line spacer 420 may include at least one of silicon oxide, silicon nitride, silicon oxynitride, or combinations thereof. Bit line spacer 420 may contact two sides of bit line electrode layer 410. Bit line spacer 420 may contact two sides of bit line contact region 440. Bit line spacer 420 may also contact two sides of bit line cover layer 450. Bit line spacer 420 may electrically isolate bit line electrode layer 410 from memory node contact region 540. Bit line spacer 420 may also electrically isolate bit line contact region 440 from memory node contact region 540.

[0133] Bit line pad area 430 may include a conductive material. For example, bit line pad area 430 may include polysilicon. Polysilicon may include predetermined impurities. Bit line pad area 430 may include silicide. Bit line pad area 430 may be disposed above a semiconductor layer (SL). Bit line pad area 430 may be disposed on the same plane as the surface of the semiconductor layer (SL). The top surface of bit line pad area 430 may be disposed on the same plane as the top surface of pad insulating area 700 or word line structure 300. The bottom surface of bit line pad area 430 may contact active area 100. One side of bit line pad area 430 may contact word line structure 300. The other side of bit line pad area 430 may contact pad insulating area 700. The top surface of bit line pad area 430 may contact bit line contact area 440.

[0134] Without the bit line pad area 430, when the word line structure 300 is misaligned from the center of the active area 100 to the bit line contact area 440 (according to...) Figure 4 When the word line structure 300 is offset (or biased) to the left, the contact area between the bit line contact area 440 and the active region 100 may be reduced, and various problems may occur, such as increased contact resistance, reduced current capacity, and performance degradation due to increased temperature. However, when the bit line pad area 430 is formed, the upper surface of the bit line pad area 430 ensures a sufficient contact area with the bit line contact area 440, and the lower surface of the bit line pad area 430 ensures a sufficient contact area with the active region 100, thereby reducing contact resistance, increasing current capacity, reducing temperature rise, and thus improving the performance of the semiconductor device 1.

[0135] Bit line contact region 440 may include a conductive material. For example, bit line contact region 440 may include at least one of polysilicon, copper, aluminum, titanium, titanium nitride, or combinations thereof. Bit line contact region 440 may be formed of the same material as bit line electrode layer 410 or of a different material. For example, when bit line contact region 440 is formed of a different material from bit line electrode layer 410, it may be more advantageous for bit line electrode layer 410 to be formed of a highly conductive metallic material, while it may be more advantageous for bit line contact region 440 to be formed of a material that helps reduce the contact resistance between bit line electrode layer 410 and bit line pad region 430. Bit line contact region 440 may contact the bottom surface of bit line electrode layer 410. Each side surface of bit line contact region 440 may contact bit line spacer 420. The bottom surface of bit line contact region 440 may contact bit line pad region 430. Bit line contact region 440 may be disposed on semiconductor layer (SL).

[0136] Bit line capping layer 450 may include an insulating material. For example, bit line capping layer 450 may include silicon oxide, silicon nitride, silicon oxynitride, or a combination thereof. Bit line capping layer 450 may contact the top surface of bit line electrode layer 410. Bit line capping layer 450 may contact bit line spacer 420. Bit line capping layer 450 and bit line spacer 420 work together to prevent electrical interaction between bit line electrode layer 410 and bit line contact region 420 and components surrounding bit line structure 400.

[0137] The memory node pad region 530 may include silicon. For example, the memory node pad region 530 may include impurity-free single-crystal silicon. The memory node pad region 530 may be disposed above a semiconductor layer (SL). The bottom surface of the memory node pad region 530 may be disposed on the same plane as the surface of the semiconductor layer (SL). The top surface of the memory node pad region 530 may be disposed at a position equal to or lower than the top surface of the bit line pad region 430. The bottom surface of the memory node pad region 530 may contact the active region 100. One side of the memory node pad region 530 may contact the pad insulating region 700. The other side of the memory node pad region 530 may contact the word line structure 300. The top surface of the memory node pad region 530 may contact the memory node contact region 540.

[0138] In the absence of the memory node pad area 530, when the word line structure 300 is misaligned from the center of the active area 100 to the memory node contact area 540 (e.g.) Figure 4 As shown, when the word line structure 300 is offset (or biased) to the right, the contact area between the memory node contact area 540 and the active region 100 may decrease, potentially leading to various problems such as increased contact resistance, reduced current capacity, and performance degradation due to increased temperature. However, when the memory node pad area 530 is formed, the top surface of the memory node pad area 530 ensures sufficient contact area with the memory node contact area 540, and the bottom surface of the memory node pad area 530 ensures sufficient contact area with the active region 100, thereby reducing contact resistance, increasing current capacity, and reducing temperature rise, thus improving the performance of the semiconductor device 1.

[0139] Unlike bit line pad area 430, storage node pad area 530 may include undoped material with relatively low charge trap density, thereby preventing storage in capacitors ( Figure 1 This addresses charge leakage in CAP and enables data to be retained for a relatively long time.

[0140] The memory node contact area 540 may include a conductive material. For example, the memory node contact area 540 may include at least one of polysilicon, copper, aluminum, titanium, titanium nitride, or combinations thereof. The bottom surface of the memory node contact area 540 may contact the memory node pad area 530. One side of the memory node contact area 540 may contact the bit line spacer 420.

[0141] The pad insulating region 700 may include an insulating material. For example, the pad insulating region 700 may include silicon oxide or silicon nitride. The pad insulating region 700 may be disposed on a semiconductor layer (SL). The bottom surface of the pad insulating region 700 may be disposed on the same plane as the surface of the semiconductor layer (SL). The top surface of the pad insulating region 700 may be disposed on the same plane as the top surface of the bit line pad region 430 or the word line structure 300. The bottom surface of the pad insulating region 700 may contact the cell isolation region 200 (or structure). One side of the pad insulating region 700 may contact the bit line pad region 430. The other side of the pad insulating region 700 may contact the memory node pad region 530. The top surface of the pad insulating region 700 may contact the bit line spacer 420 or the memory node contact region 540.

[0142] In the following Figures 5 to 18F In the description, for the sake of brevity and clarity, and Figures 1 to 4 Overlapping descriptions will be omitted here.

[0143] Figure 5 According to an embodiment of this disclosure Figure 2 and Figure 3 A cross-sectional view of an example structure of a semiconductor device, taken by the B-B' line.

[0144] refer to Figure 2 , Figure 3 , Figure 4 and Figure 5 The second cross section (CS2) may include a substrate region 10, an active region 100, a cell isolation region 200, a first word line electrode layer 310, a second word line electrode layer 320, a word line cover layer 330, a word line insulating layer 340, a bit line electrode layer 410, a bit line spacer 420, a bit line contact region 440, a bit line cover layer 450, and a contact insulating region 600.

[0145] The first word line electrode layer 310 can extend along a first direction (X). The first word line electrode layer 310 can be disposed on the word line insulating layer 340. The second word line electrode layer 320 can extend along the first direction (X). The second word line electrode layer 320 can be disposed on the first word line electrode layer 310. The word line cover layer 330 can extend along the first direction (X). The word line cover layer 330 can be disposed on the second word line electrode layer 320. The word line insulating layer 340 can extend along the first direction (X). The bottom surface of the word line insulating layer 340 can contact both the cell isolation region 200 and the active region 100.

[0146] exist Figure 5In this embodiment, the bottom surface of the word line insulating layer 340 is shown to be formed horizontally, but other embodiments are also possible. Alternatively, depending on the process method, the etching rate of the active region 100 and the etching rate of the cell isolation region 200 may be different from each other, and the bottom surface of the word line insulating layer 340 may be positioned lower above the cell isolation region 200 than above the active region 100 (i.e., the position of the word line insulating layer 340 above the cell isolation region 200 may be deeper than the position above the active region 100). Hereinafter, this disclosure will describe by way of example an embodiment in which the bottom surface of the word line insulating layer 340 is formed horizontally.

[0147] Multiple bit line electrode layers 410 may be arranged spaced apart from each other in a first direction (X). Both sides of each bit line electrode layer 410 may contact the bit line spacer 420. Contact insulation areas 600 may be provided between the bit line spacers 420 arranged on one side of different bit line electrode layers 410.

[0148] Contact insulation region 600 may include an insulating material. For example, contact insulation region 600 may include at least one of silicon oxide, silicon nitride, silicon oxynitride, or combinations thereof. Contact insulation regions 600 may be disposed between adjacent bit line spacers 420. Contact insulation regions 600 may be arranged in a repeating, spaced-apart arrangement in a first direction (X). Reference will be made below. Figure 8 A more detailed description is given of the contact insulation zone 600.

[0149] Figure 6 According to an embodiment of this disclosure Figure 2 and Figure 3 A cross-sectional view of an example structure of a semiconductor device taken by the C-C' line.

[0150] refer to Figure 2 , Figure 3 , Figure 4 and Figure 6 The third section (CS3) may include a substrate region 10, an active region 100, a cell isolation region 200, a bit line electrode layer 410, a bit line spacer 420, a bit line pad region 430, a bit line contact region 440, a bit line cover layer 450, a memory node pad region 530, a memory node contact region 540, and a pad insulation region 700.

[0151] The bottom surface of the bit line pad area 430 can contact the active area 100 and the cell isolation area 200. Both sides of the bit line pad area 430 can contact the pad insulation area 700. The top surface of the bit line pad area 430 can contact the bit line contact area 440.

[0152] The storage node pad area 530 can contact the top surface of the active area 100. Both sides of the storage node pad area 530 can contact the pad insulation area 700. The top surface of the storage node pad area 530 can contact the storage node contact area 540.

[0153] Each bit line pad region 430 and each memory node pad region 530 may be arranged alternately in a first direction (X). The height of the bit line pad region 430 may differ from the height of the memory node pad region 530, but the scope of this disclosure is not limited thereto. For example, the height of the bit line pad region 430 may be the same as the height of the memory node pad region 530. In the process of forming the memory node contact region 540, when the memory node contact region 540 is in complete contact with the memory node pad region 530 and no portion of the memory node pad region 530 is etched, the height of the memory node pad region 530 may be the same as the height of the bit line pad region 430.

[0154] Each of the plurality of bit line pad areas 430, each of the plurality of memory node pad areas 530, and each of the plurality of pad insulation areas 700 may be disposed on the same plane as the surface of the active area 100.

[0155] Each of the plurality of bit line contact areas 440 may contact the top surface of the bit line pad area 430. On the other hand, each of the plurality of memory node contact areas 540 may contact the top surface of the memory node pad area 530.

[0156] The pad insulation region 700 may be disposed between the storage node pad region 530 and the adjacent bit line pad region 430. The bottom surface of the pad insulation region 700 may contact the cell isolation region 200. For example, the top surface of the pad insulation region 700 may be disposed on the same plane as the top surface of the bit line pad region 430.

[0157] Figure 7 This illustrates an embodiment of the present disclosure. Figure 2 and Figure 3 A cross-sectional view of an example structure of semiconductor device 1 taken by the D-D' line in the diagram.

[0158] refer to Figure 2 , Figure 3 , Figure 4 and Figure 7 The fourth section (CS4) may include a substrate region 10, an active region 100, a cell isolation region 200, a bit line pad region 430, a first word line electrode layer 310, a second word line electrode layer 320, a word line cover layer 330, a word line insulating layer 340, a bit line electrode layer 410, a bit line contact region 440, and a bit line cover layer 450.

[0159] Bit line electrode layer 410 may extend along the second direction (Y). Bit line contact region 440 may extend along the second direction (Y). Bit line cover layer 450 may extend along the second direction (Y).

[0160] A portion (e.g., the lower part) of the bottom surface of the word line structure 300 may contact the active region 100. Another portion of the bottom surface of the word line structure 300 may contact the cell isolation region 200. A portion (e.g., the lower part) of one side of the word line structure 300 may contact the active region 100. Another portion (e.g., the upper part) of one side of the word line structure 300 may contact the bit line pad region 430. A portion (e.g., the lower part) of the other side of the word line structure 300 may contact the cell isolation region 200. Another portion (e.g., the upper part) of the other side of the word line structure 300 may contact the bit line pad region 430.

[0161] Each of the plurality of bit line pad areas 430 may be located between adjacent word line structures 300.

[0162] Figure 8 This illustrates an embodiment of the present disclosure. Figure 2 and Figure 3 A cross-sectional view of an example structure of semiconductor device 1 taken by the E-E' line.

[0163] refer to Figure 2 , Figure 3 , Figure 4 and Figure 8 The fifth section (CS5) may include a substrate region 10, an active region 100, a cell isolation region 200, a word line structure 300, a memory node pad region 530, a memory node contact region 540, and a contact insulation region 600.

[0164] Each of the plurality of storage node contact areas 540 may have its side surface in contact with the contact insulation area 600. Each of the plurality of contact insulation areas 600 may have its side surface in contact with the storage node contact area 540. The plurality of storage node contact areas 540 and the plurality of contact insulation areas 600 may be arranged in alternating rows along a second direction (Y).

[0165] The active region 100 may interact with a portion of the bottom surface of the word line structure 300 and a side surface of the word line structure 300 (e.g., Figure 8 The left side (e.g., the lower part) of the word line structure 300 may contact another part of the bottom surface of the word line structure 300 and another side of the word line structure 300 (e.g., the lower part). Figure 8 The right side (e.g., the lower part) of the middle is in contact.

[0166] The storage node pad area 530 may contact a portion (e.g., the upper part) of one side of the word line structure 300. The storage node pad area 530 may contact a portion (e.g., the upper part) of the other side of the word line structure 300.

[0167] The contact insulation area 600 may be disposed on the word line structure 300. For example, the contact insulation area 600 may be in contact with the top surface of the word line cover layer 330.

[0168] Figure 9 This is a flowchart illustrating an example of a method for manufacturing a semiconductor device 1 according to an embodiment of the present disclosure.

[0169] refer to Figure 2 , Figure 3 and Figure 9 A method of manufacturing a semiconductor device 1 (hereinafter referred to as "the manufacturing method") may include forming (S10) a plurality of active regions 100 and a cell isolation region 200 surrounding the plurality of active regions 100.

[0170] A method of manufacturing semiconductor device 1 may include depositing an active layer over the plurality of active regions 100 and cell isolation regions 200 (S20). The active layer may include the same material as the bit line pad region 430 or the memory node pad region 530. In one example, when the active layer includes the same material as the bit line pad region 430, the manufacturing method may include first forming the bit line pad region 430 and then forming the memory node pad region 530. In another example, when the active layer includes the same material as the memory node pad region 530, the manufacturing method may include first forming the memory node pad region 530 and then forming the bit line pad region 430.

[0171] The manufacturing method may include forming a plurality of first pad regions by removing portions of the active layer (S30). In an example of a manufacturing method in which the active layer comprises the same material as the bit line pad region 430, the first pad regions may correspond to the bit line pad region 430. In an example of a manufacturing method in which the active layer comprises the same material as the memory node pad region 530, the first pad regions may correspond to the memory node pad region 530.

[0172] The operation of depositing the active layer (S20) and the operation of removing part of the active layer (S30) can be considered as included in the operation of forming the plurality of first pad areas.

[0173] The manufacturing method may include forming a fill region between the plurality of first pad regions (S40). The fill region may include the same material as the pad insulating region 700.

[0174] The manufacturing method may include forming a plurality of pad insulating areas 700 (S50) by removing a portion of the filling area (i.e., partial removal).

[0175] The operations of forming the fill area (S40) and removing a portion of the fill area (S50) can be considered as part of the operations of forming the plurality of pad insulating areas 700. However, the scope of the operations of forming the pad insulating areas 700 is not limited thereto. For example, as a representative method of forming sidewalls on both sides of each first pad area, the method of forming the pad insulating areas 700 can also be included in the operations of forming the pad insulating areas 700 according to this disclosure.

[0176] The manufacturing method may include forming a plurality of second pad areas (S60). Each second pad area may be located within a space where fill has been removed. In one embodiment, if the first pad area corresponds to the bit line pad area 430, then the second pad area may represent the storage node pad area 530.

[0177] The manufacturing method may include forming a plurality of word line structures 300 (S70). The manufacturing method may also include forming a plurality of bit line electrode layers 410, a plurality of bit line spacers 420, a plurality of bit line contact areas 440, and a plurality of bit line cover layers 450 (S80). The manufacturing method may further include forming a plurality of memory node contact areas 540 and a plurality of contact insulation areas 600 (S90).

[0178] The following will be referenced Figure 10A The manufacturing method is described in more detail using multiple cross-sectional views.

[0179] The following will refer to Figures 10A to 18F A representative example of the manufacturing method is described in more detail, wherein the first pad area corresponds to the bit line pad area 430 and the second pad area corresponds to the storage node pad area 530.

[0180] Figures 10A to 18F It is a plan view or a cross-sectional view, with examples provided. Figure 9 The method for manufacturing the semiconductor device 1 shown.

[0181] Figure 10A It is a floor plan showing the execution. Figure 9 Example results of operation S10 in the example.

[0182] refer to Figure 2 , Figure 3 , Figure 9 and Figures 10A to 10F A method of manufacturing a semiconductor device 1 (hereinafter referred to as "the manufacturing method") may include forming (S10) a plurality of active regions 100 and a cell isolation region 200 surrounding the plurality of active regions 100.

[0183] refer to Figure 10ASome of the plurality of active regions 100 may be arranged alternately spaced apart from each other in a first direction (X). Others of the plurality of active regions 100 may be arranged alternately spaced apart from each other in a second direction (Y) perpendicular to the first direction (X). The remaining portions of the plurality of active regions 100 may be arranged alternately spaced apart from each other in a diagonal direction (DG). Each active region 100 may extend along the diagonal direction (DG). The angle between the diagonal direction (DG) and the first direction (X) may be in the range of approximately 30 degrees to approximately 60 degrees.

[0184] Subsequently, a unit isolation region 200 can be formed to fill the remaining blank space other than the plurality of active regions 100 with the gaps of insulating material (e.g., silicon oxide, silicon nitride, silicon oxynitride, etc.).

[0185] Figure 10B According to an embodiment of this disclosure Figure 10A The cross-sectional view of an example structure of semiconductor device 1 taken by line A-A' in the figure.

[0186] refer to Figure 10A and Figure 10B A predetermined trench can be formed on the top surface of a semiconductor layer (SL) comprising a semiconductor material (e.g., silicon, silicon germanium, etc.). The remaining region after trench formation can be an active region 100 or a substrate region 10. In some embodiments, the active region 100 can be defined as a region with the same depth as the predetermined trench. In this disclosure, the substrate region 10 can contact the bottom surface of the active region 100 and can be defined as the remaining region other than the active region 100 after the predetermined trench is formed.

[0187] After the predetermined trench is formed, the unit isolation area 200 can be formed by filling the gaps in the trench with insulating material.

[0188] Figure 10C This illustrates an embodiment of the present disclosure. Figure 10A A cross-sectional view of an example structure of a semiconductor device, taken by the B-B' line.

[0189] Figure 10D This illustrates an embodiment of the present disclosure. Figure 10A A cross-sectional view of an example structure of a semiconductor device taken by the C-C' line.

[0190] refer to Figure 10A , Figure 10C and Figure 10D By forming predetermined trenches, a plurality of active regions 100 can be repeatedly formed in a first direction (X). A unit isolation region 200 can be formed between the plurality of active regions 100.

[0191] Figure 10E This illustrates an embodiment of the present disclosure. Figure 10A A cross-sectional view of an example structure of semiconductor device 1 taken by the D-D' line in the diagram.

[0192] Figure 10F This illustrates an embodiment of the present disclosure. Figure 10A A cross-sectional view of an example structure of semiconductor device 1 taken by the E-E' line.

[0193] refer to Figure 10A , Figure 10E and Figure 10F The plurality of active regions 100 can be repeatedly formed in the second direction (Y) by forming predetermined trenches. A unit isolation region 200 can be formed between the plurality of active regions 100.

[0194] The following will describe Figures 11A to 11F The following embodiments focus on... Figures 10A to 10F Different characteristics.

[0195] Figure 11A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S20.

[0196] refer to Figure 2 , Figure 3 , Figure 9 and Figures 11A to 11F The manufacturing method may include forming an active layer (DAT) that overlaps with each of the plurality of active regions 100 and each unit isolation region 200 (S20).

[0197] The active layer (DAT) may include, for example, at least one of silicide, impurity-containing polysilicon, or combinations thereof. In another embodiment, the storage node pad region 530 is first formed, and the active layer (DAT) may include undoped monocrystalline silicon.

[0198] refer to Figure 10A and Figure 11A It can form an active layer (DAT) that overlaps with each of the plurality of active regions 100 and each unit isolation region 200.

[0199] Figure 11B This illustrates an embodiment of the present disclosure. Figure 11A The cross-sectional view of an example structure of semiconductor device 1 taken by line A-A' in the figure.

[0200] refer to Figure 10A , Figure 11A and Figure 11B The active layer (DAT) can be formed on the semiconductor layer (SL). The active layer (DAT) can be disposed on the semiconductor layer (SL) with a predetermined thickness.

[0201] Figure 11C This illustrates an embodiment of the present disclosure. Figure 11A A cross-sectional view of an example structure of semiconductor device 1 taken by line B-B' in the figure.

[0202] Figure 11D This illustrates an embodiment of the present disclosure. Figure 11A A cross-sectional view of an example structure of semiconductor device 1 taken by the C-C' line.

[0203] refer to Figure 10A , Figure 11A , Figure 11C and Figure 11D The active layer (DAT) can be formed to extend along a first direction (X) on the surface of the semiconductor layer (SL).

[0204] Figure 11E This illustrates an embodiment of the present disclosure. Figure 11A A cross-sectional view of an example structure of semiconductor device 1 taken by the D-D' line in the diagram.

[0205] Figure 11F This illustrates an embodiment of the present disclosure. Figure 11A A cross-sectional view of an example structure of semiconductor device 1 taken by the E-E' line.

[0206] refer to Figure 10A , Figure 11A , Figure 11E and Figure 11F The active layer (DAT) can be formed to extend along a second direction (Y) on the surface of the semiconductor layer (SL).

[0207] The following will describe Figures 12A to 12F The following embodiments focus on... Figures 11A to 11F Different characteristics.

[0208] Figure 12A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S30 in the diagram.

[0209] refer to Figure 2 , Figure 3 , Figure 9 and Figures 12A to 12F This manufacturing method may include removing a portion of the active layer (DAT) to form a plurality of bit line pad regions 430 (S30).

[0210] refer to Figure 11A and Figure 12AAt least one first removal region (DEL1) may refer to the region of the active layer (DAT) to be removed. The first removal region (DEL1) may extend along a second direction (Y). The first removal region (DEL1) may be repeated along a first direction (X).

[0211] The active layer (DAT) may overlap one end of the active region 100 and may form a structure extending along the second direction (Y), thereby making the resulting active layer (DAT) usable as a bit line pad region 430.

[0212] Figure 12B This illustrates an embodiment of the present disclosure. Figure 12A The cross-sectional view of an example structure of semiconductor device 1 taken by line A-A' in the figure.

[0213] Figure 12C This illustrates an embodiment of the present disclosure. Figure 12A A cross-sectional view of an example structure of a semiconductor device, taken by the B-B' line.

[0214] Figure 12D This illustrates an embodiment of the present disclosure. Figure 12A A cross-sectional view of an example structure of a semiconductor device taken by the C-C' line.

[0215] refer to Figure 11A and Figures 12A to 12D The bit line pad area 430 can be located at one end of the active area 100 (e.g., Figure 12B Above the left end of the area. The first removal area (DEL1) can be set on both sides of the bit line pad area 430.

[0216] The first removal region (DEL1) can be located above the center of the active region 100, or at the other end of the active region 100 (e.g., Figure 12B Above the right end of the middle.

[0217] Bit line pad areas 430 may be arranged in a repeating, spaced-apart arrangement in a first direction (X). The gaps between the bit line pad areas 430 spaced apart in the first direction (X) may correspond to a first removal area (DEL1).

[0218] Figure 12E This illustrates an embodiment of the present disclosure. Figure 12A A cross-sectional view of an example structure of semiconductor device 1 taken by the D-D' line in the diagram.

[0219] Figure 12F This illustrates an embodiment of the present disclosure. Figure 12A A cross-sectional view of an example structure of semiconductor device 1 taken by the E-E' line.

[0220] refer to Figure 11A , Figure 12A , Figure 12E and Figure 12F The bit line pad area 430 can extend along the second direction (Y). The first removal area (DEL1) can also extend along the second direction (Y).

[0221] The following will describe Figures 13A to 13F The following embodiments focus on... Figures 12A to 12F Different characteristics.

[0222] Figure 13A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S40 in the diagram.

[0223] refer to Figure 2 , Figure 3 , Figure 9 and Figures 13A to 13F The manufacturing method may include forming at least one fill area (FIL) between the plurality of bit line pad areas 430 (S40).

[0224] The fill area (FIL) can fill the area of ​​the first removal area (DEL1) to fill the gap. Although the first removal area (DEL1) corresponds to the empty space, the fill area (FIL) can include the same material as the pad insulation area (e.g., insulating material) (see reference). Figure 3 (700 in the middle).

[0225] Figures 13A to 13F The filled area (FIL) can be formed in the formation Figures 12A to 12F The location of the first removal zone (DEL1).

[0226] The following will describe Figures 14A to 14F The following embodiments focus on... Figures 13A to 13F Different characteristics.

[0227] Figure 14A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S50 in the diagram.

[0228] refer to Figure 2 , Figure 3 , Figure 9 and Figures 14A to 14F This manufacturing method may include forming a plurality of pad insulating areas 700 (S50) by removing a portion of the fill area (FIL).

[0229] refer to Figure 13A and Figure 14AA second removal area (DEL2) can be formed by removing a portion of the fill area (FIL). After the second removal area (DEL2) is formed, the remaining portion of the fill area (FIL) can be used as the pad insulating area 700.

[0230] The second removal region (DEL2) may be formed at the location where the memory node pad area 530 is formed. For example, the second removal region (DEL2) may be located at the other end of each of the plurality of active regions 100 (e.g., Figure 14B The right end of the first removal area overlaps with the second removal area (DEL2) and can extend along the second direction (Y). The second removal area (DEL2) can be repeatedly spaced apart from each other in the first direction (X).

[0231] The pad insulating region 700 is the remaining portion of the fill region (FIL) after the formation of the second removal region (DEL2) and may be located between the second removal region (DEL2) and the bit line pad region 430. The pad insulating region 700 may overlap with the center of each of the plurality of active regions 100 and may extend along a second direction (Y).

[0232] Figure 14B This illustrates an embodiment of the present disclosure. Figure 14A The cross-sectional view of an example structure of semiconductor device 1 taken by line A-A' in the figure.

[0233] Figure 14C This illustrates an embodiment of the present disclosure. Figure 14A A cross-sectional view of an example structure of semiconductor device 1 taken by line B-B' in the figure.

[0234] Figure 14D This illustrates an embodiment of the present disclosure. Figure 14A A cross-sectional view of an example structure of semiconductor device 1 taken by the C-C' line.

[0235] refer to Figure 13A and Figures 14A to 14D When the second removal region (DEL2) is formed, the bit line pad region 430 is located at one end of the active region 100 (e.g., Figure 14B When the second removal region (DEL2) is located above the left end of the active region 100, it can be set at the other end of the active region 100 (e.g., Figure 14B The second removal area (DEL2) can be located above the right end of the active area 100, and the pad insulating area 700 can be located above the center of the active area 100. The second removal area (DEL2) can be a blank space. Each side of the second removal area (DEL2) can be in contact with the pad insulating area 700. The second removal area (DEL2) can be formed by completely removing the fill area (FIL), thereby fully exposing the active area 100 to the outside.

[0236] When the filler area (FIL) is not completely removed, the contact area between the memory node pad area 530 and the active region 100 formed in subsequent processes may be reduced, which may decrease the reliability of the semiconductor device 1. Therefore, it is necessary to completely remove the portion of the filler area (FIL) that overlaps with the location where the memory node pad area 530 is formed (and this can be completely removed according to embodiments of this disclosure).

[0237] Figure 14E This illustrates an embodiment of the present disclosure. Figure 14A A cross-sectional view of an example structure of semiconductor device 1 taken by the D-D' line in the diagram.

[0238] Figure 14F This illustrates an embodiment of the present disclosure. Figure 14A A cross-sectional view of an example structure of semiconductor device 1 taken by the E-E' line.

[0239] Figure 14E The cross section can be with Figure 13E Their cross-sections are basically the same.

[0240] Figure 14F show, Figure 13F The fill area (FIL) portion has been completely removed, forming the second removal area (DEL2).

[0241] The following will describe Figures 15A to 15F The following embodiments focus on... Figures 14A to 14F Different characteristics.

[0242] Figure 15A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S60 in the diagram.

[0243] refer to Figure 2 , Figure 3 , Figure 9 and Figures 15A to 15F This manufacturing method may include forming a plurality of storage node pad areas 530 between pad insulation areas 700.

[0244] refer to Figure 14A and Figure 15A The memory node pad region 530 may be formed as a gap-filled second removal region (DEL2). The memory node pad region 530 may, for example, comprise impurity-free monocrystalline silicon. In some embodiments, after forming the memory node pad region 530 filled with the second removal region (DEL2), a planarization process may be further performed. The memory node pad region 530 may extend along a second direction (Y). The memory node pad regions 530 may be repeatedly spaced apart from each other in a first direction (X).

[0245] Figure 15BThis illustrates an embodiment of the present disclosure. Figure 15A The cross-sectional view of an example structure of semiconductor device 1 taken by line A-A' in the figure.

[0246] Figure 15C This illustrates an embodiment of the present disclosure. Figure 15A A cross-sectional view of an example structure of semiconductor device 1 taken by line B-B' in the figure.

[0247] Figure 15D This illustrates an embodiment of the present disclosure. Figure 15A A cross-sectional view of an example structure of semiconductor device 1 taken by the C-C' line.

[0248] refer to Figure 14A , Figure 15A and Figure 15B The storage node pad area 530 can be disposed on the active area 100. The storage node pad area 530 can be formed at the end opposite to the bit line pad area 430. The storage node pad area 530 can be electrically and physically isolated from the bit line pad area 430 through the pad insulation area 700.

[0249] The bit line pad area 430 can be located at one end of the active area 100 (e.g., Figure 15B Above the left end of the active area 100. The storage node pad area 530 may be located at the other end of the active area 100 (e.g., on the left end). Figure 15B Above the right end of the active area 100. The pad insulation area 700 can be located between the bit line pad area 430 and the storage node pad area 530. The pad insulation area 700 can be located above the center of the active area 100.

[0250] Bit line pad area 430 may be disposed between two adjacent pad insulation areas 700. Storage node pad area 530 may also be disposed between two adjacent pad insulation areas 700. Bit line pad area 430 and storage node pad area 530 may be arranged alternately and repeatedly in a first direction (X).

[0251] Figure 15E This illustrates an embodiment of the present disclosure. Figure 15A A cross-sectional view of an example structure of semiconductor device 1 taken by the D-D' line in the diagram.

[0252] Figure 15E The cross section can be with Figure 14E Their cross-sections are basically the same.

[0253] Figure 15F This illustrates an embodiment of the present disclosure. Figure 15A A cross-sectional view of an example structure of semiconductor device 1 taken by the E-E' line.

[0254] Figure 15F It can correspond to the formation in Figure 14F The cross section of the storage node pad area 530 in the second removal area (DEL2).

[0255] The following will describe Figures 16A to 16F The following embodiments focus on... Figures 15A to 15F Different characteristics.

[0256] Figure 16A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S70 in the diagram.

[0257] refer to Figure 2 , Figure 3 , Figure 9 and Figures 16A to 16F This manufacturing method may include forming a plurality of word line structures 300 (S70).

[0258] refer to Figure 9 , Figure 10A , Figure 15A and Figure 16A The character line structure 300 can be formed to extend along a first direction (X). The character line structure 300 can be formed to penetrate. Figure 15A The bit line pad area 430 and the storage node pad area 530 are shown.

[0259] In this embodiment, the remaining bit line pad area 430 after patterning can overlap with one end of each active area 100, and can be electrically and physically separated not only from the storage node pad area 530 of other active areas 100 adjacent to each other in the first direction (X), but also from the bit line pad area 430 of other active areas 100 adjacent to each other in the second direction (Y).

[0260] Each of the plurality of bit line pad areas 430 may overlap with one end of the active region 100, and the plurality of bit line pad areas 430 may be repeatedly spaced apart from each other not only in the first direction (X), but also repeatedly spaced apart from each other in the second direction (Y).

[0261] In one embodiment, each remaining memory node pad area 530 after patterning may overlap with the other end of the active region 100, and may be electrically and physically separated not only from the bit line pad areas 430 of the active regions 100 adjacent to each other in the first direction (X), but also from the memory node pad areas 530 of other active regions 100 adjacent to each other in the second direction (Y).

[0262] Each of the plurality of storage node pad areas 530 may overlap with the other end of the active area, and the plurality of storage node pad areas 530 may be repeatedly spaced apart from each other not only in the first direction (X) but also in the second direction (Y).

[0263] The character line structure 300 can also be formed as a through-line. Figure 15A The pad insulation area 700 is shown. Therefore, the plurality of pad insulation areas 700 can be repeatedly spaced apart from each other not only in the first direction (X), but also repeatedly spaced apart from each other in the second direction (Y).

[0264] Figure 16B This illustrates an embodiment of the present disclosure. Figure 16A The cross-sectional view of an example structure of semiconductor device 1 taken by line A-A' in the figure.

[0265] Figure 16C This illustrates an embodiment of the present disclosure. Figure 16A A cross-sectional view of an example structure of semiconductor device 1 taken by line B-B' in the figure.

[0266] refer to Figure 15A , Figure 16A , Figure 16B and Figure 16C Word line trenches (WT) can be formed along a third direction (Z) from the plane containing the top surface of the bit line pad area 430 and the top surface of the memory node pad area 530.

[0267] In this disclosure, the height of the cell isolation region 200 recessed from the surface of the semiconductor layer (SL) along a third direction (Z) can be defined as a first height (H1), the heights of the bit line pad region 430, the memory node pad region 530 and the pad insulation region 700 formed above the surface of the semiconductor layer (SL) can all be defined as a second height (H2), and the height of the word line trench (WT) recessed from the top surface of the bit line pad region 430 can be defined as a third height (H3).

[0268] As described above, the first altitude (H1) may be equal to or greater than 1600 Å and equal to or less than 1900 Å. As described above, the third altitude (H3) may be equal to or greater than 1000 Å and equal to or less than 1300 Å. The second altitude (H2) may be equal to or greater than 200 Å and equal to or less than 400 Å.

[0269] To ensure reliable electrical isolation between adjacent active areas 100, it is necessary to ensure that there is a height difference between the bottom surface of the word line trench (WT) and the bottom surface of the cell isolation area 200, which can be achieved according to the embodiment.

[0270] When the bit line contact area or memory node contact area is disposed on the semiconductor layer surface (SL) without forming the bit line pad area 430, the memory node pad area 530 and the pad insulation area 700, the first height (H1) may need to be relatively large to ensure reliable electrical isolation between adjacent active areas 100.

[0271] However, when the bit line pad area 430, the memory node pad area 530, and the pad insulation area 700 are all formed with a second height (H2), the word line trench (WT) can be recessed from the top surface of the bit line pad area 430 along a third direction (Z). Therefore, the height difference between the bottom surface of the cell isolation area 200 and the bottom surface of the word line trench (WT) can be expressed as "(H1+H2)−H3" instead of "(H1–H3)". Furthermore, even if the first height (H1) is set to a relatively low height, adjacent active areas 100 can be electrically isolated from each other. When the first height (H1) is set to a relatively low height, the additional effect of reducing the difficulty of the etching process used to form the cell isolation area 200 can also be obtained.

[0272] After forming the word line groove (WT), a word line insulating layer 340 extending along a first direction (X) can be formed to contact the bottom and side surfaces of the word line groove (WT). Subsequently, a first word line electrode layer 310 extending along the first direction (X) can be formed on the word line insulating layer 340. Then, a second word line electrode layer 320 extending along the first direction (X) can be formed on the first word line electrode layer 310.

[0273] like Figure 16B and Figure 16C As shown, in this example, the surface of the semiconductor layer (SL) is located above the top surface of the first word line electrode layer 310 and below the top surface of the second word line electrode layer 320, but the scope of this disclosure is not limited thereto. For example, the top surface of the second word line electrode layer 320 may also be located below the surface of the semiconductor layer (SL).

[0274] Figure 16D This illustrates an embodiment of the present disclosure. Figure 16A A cross-sectional view of an example structure of semiconductor device 1 taken by the C-C' line.

[0275] Figure 16D The cross section can be with Figure 15D Their cross-sections are basically the same.

[0276] Figure 16E This illustrates an embodiment of the present disclosure. Figure 16A A cross-sectional view of an example structure of semiconductor device 1 taken by the D-D' line in the diagram.

[0277] refer to Figure 15A , Figure 16A and Figure 16EThe plurality of word line structures 300 may be repeatedly spaced apart from each other in the second direction (Y).

[0278] In addition, one side of each word line structure 300 may contact the bit line pad area 430, which in turn contacts the active area 100, and the active area 100 contacts the bottom and side surfaces of the word line structure 300.

[0279] Figure 16F This illustrates an embodiment of the present disclosure. Figure 16A A cross-sectional view of an example structure of semiconductor device 1 taken by the E-E' line.

[0280] refer to Figure 15A , Figure 16A and Figure 16F The plurality of word line structures 300 may be repeatedly spaced apart from each other in a second direction (Y). One side of a word line structure 300 may contact a memory node pad area 530, which in turn contacts an active area 100, which in turn contacts the bottom and side surfaces of the word line structure 300.

[0281] The following will describe Figures 17A to 17F The following embodiments focus on... Figures 16A to 16F Different characteristics.

[0282] Figure 17A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of example results of operation S80 in the diagram.

[0283] refer to Figure 2 , Figure 3 , Figure 9 and Figures 17A to 17F The manufacturing method may include forming the plurality of bit line electrode layers 410, the plurality of bit line spacers 420, the plurality of bit line contact areas 440 and the plurality of bit line cover layers 450 (S80).

[0284] Figure 17B This illustrates an embodiment of the present disclosure. Figure 17A The cross-sectional view of an example structure of semiconductor device 1 taken by line A-A' in the figure.

[0285] refer to Figure 9 , Figure 10A , Figure 17A and Figure 17BA bitline contact area 440 is formed that contacts the top surface of the bitline pad area 430. Then, a bitline electrode layer 410 is formed on the bitline contact area 440. The bitline electrode layer 410 can extend along a second direction (Y). Next, a bitline cover layer 450 is formed on the bitline electrode layer 410. A bitline spacer 420 is formed that contacts both sides of the bitline electrode layer 410, the bitline contact area 440, and the bitline cover layer 450.

[0286] Figure 17C This illustrates an embodiment of the present disclosure. Figure 17A A cross-sectional view of an example structure of semiconductor device 1 taken by line B-B' in the figure.

[0287] refer to Figure 9 , Figure 10A , Figure 17A and Figure 17C The plurality of bit line contact areas 440 may be spaced apart from each other in the first direction (X). The plurality of bit line electrode layers 410 may be spaced apart from each other in the first direction (X). The plurality of bit line cover layers 450 may be spaced apart from each other in the first direction (X). The plurality of bit line spacers 420 may be in lateral contact with the bit line electrode layers 410 in the first direction (X), or may be in lateral contact with the bit line electrode layers 410 in a direction opposite to the first direction (X).

[0288] refer to Figure 17B and Figure 17C In the process of forming the bit line structure 400, bit line spacers 420 can be formed to surround the two sides of the bit line electrode layer 410, or the space between the bit line electrode layers 410 adjacent to each other in the first direction (X) can be filled with insulating material, and the bit line spacers 420 can be formed by etching the portion corresponding to the position where the memory node contact area 540 is to be formed.

[0289] In this disclosure, an example of a manufacturing method will be described with reference to the accompanying drawings, wherein a portion corresponding to the location where a memory node contact area 540 is to be formed is etched to form a bit line spacer 420.

[0290] Figure 17D This illustrates an embodiment of the present disclosure. Figure 17A A cross-sectional view of an example structure of semiconductor device 1 taken by the C-C' line.

[0291] refer to Figure 9 , Figure 10A , Figure 17A and Figure 17D Bit line spacers 420 may be disposed on pad insulation area 700. The plurality of bit line structures 400 may be arranged in a repeating, spaced-apart arrangement in a first direction (X) (e.g., in a spaced configuration).

[0292] Figure 17E This illustrates an embodiment of the present disclosure. Figure 17A A cross-sectional view of an example structure of semiconductor device 1 taken by the D-D' line in the diagram.

[0293] refer to Figure 9 , Figure 10A , Figure 17A and Figure 17E The bit line contact area 440, bit line electrode layer 410, bit line cover layer 450 and bit line spacer 420 can all be formed to extend along the second direction (Y).

[0294] Figure 17F This illustrates an embodiment of the present disclosure. Figure 17A A cross-sectional view of an example structure of semiconductor device 1 taken by the E-E' line.

[0295] Figure 17F cross section and Figure 16F Their cross-sections are basically the same.

[0296] The following will describe Figures 18A to 18F The following embodiments focus on... Figures 17A to 17F Different characteristics.

[0297] Figure 18A This illustrates the implementation of an embodiment according to the present disclosure. Figure 9 A plan view of the example results of operation S90 in the diagram.

[0298] refer to Figure 2 , Figure 3 , Figure 9 and Figures 18A to 18F The manufacturing method may include forming the plurality of storage node contact areas 540 and the plurality of contact insulation areas 600 (S90).

[0299] Figure 18B This illustrates an embodiment of the present disclosure. Figure 18A The cross-sectional view of an example structure of semiconductor device 1 taken by line A-A' in the figure.

[0300] refer to Figure 9 , Figure 10A , Figure 18A and Figure 18BEach of the plurality of memory node contact areas 540 can be formed to overlap with a portion of the active region 100. One end of the active region 100 can be formed to overlap with the bit line pad region 430. The other end of the active region 100 can be formed to overlap with the memory node contact area 540. Each memory node contact area 540 can contact the top surface of the memory node pad region 530. Each memory node contact area 540 can contact the top surface of the pad insulation region 700.

[0301] The memory node contact area 540 can be formed by performing additional shallow etching on the portion where the memory node contact area 540 is to be formed, to ensure complete contact with the memory node pad area 530. If the top surface of the memory node pad area 530 is completely exposed to the outside, the memory node contact area 540 can be formed without additional etching. In this case, the bottom surface of the memory node contact area 540 can be located on a plane substantially the same as the bottom surface of the bit line contact area 440.

[0302] Figure 18C This illustrates an embodiment of the present disclosure. Figure 18A A cross-sectional view of an example structure of semiconductor device 1 taken by line B-B' in the figure.

[0303] refer to Figure 18C The plurality of contact insulating regions 600 may be disposed between the bit line spacers 420. For example, the contact insulating region 600 may contact the bit line spacer 420 in a first direction (X). The contact insulating region 600 may contact the bit line spacer 420 in a direction opposite to the first direction (X).

[0304] Similar to the memory node contact area 540, the contact insulating area 600 may be formed in the portion of the memory node contact area 540 that is etched simultaneously with some portions of the contact area 540 to be formed. In this case, the bottom surface of the contact insulating area 600 may be lower than the bottom surface of the bit line spacer 420.

[0305] Figure 18D This illustrates an embodiment of the present disclosure. Figure 18A A cross-sectional view of an example structure of a semiconductor device taken by the C-C' line.

[0306] refer to Figure 18D The plurality of memory node contact areas 540 may be disposed between the bit line spacers 420. For example, the memory node contact areas 540 may contact the bit line spacers 420 in a first direction (X). The memory node contact areas 540 may also contact the bit line spacers 420 in a direction opposite to the first direction (X).

[0307] Figure 18E This illustrates an embodiment of the present disclosure. Figure 18AA cross-sectional view of an example structure of semiconductor device 1 taken by the D-D' line in the diagram.

[0308] Figure 18E The cross section can be with Figure 17E Their cross-sections are basically the same.

[0309] Figure 18F This illustrates an embodiment of the present disclosure. Figure 18A A cross-sectional view of an example structure of semiconductor device 1 taken by the E-E' line.

[0310] refer to Figure 18F The plurality of storage node contact areas 540 and the plurality of contact insulating areas 600 may be formed alternately and repeatedly in the second direction (Y). Two sides of each storage node contact area 540 may contact the contact insulating area 600. For example, the storage node contact area 540 may contact the contact insulating area 600 in the second direction (Y). The storage node contact area 540 may contact the contact insulating area 600 in a direction opposite to the second direction (Y). Furthermore, the contact insulating area 600 may contact the storage node contact area 540 in the second direction (Y). The contact insulating area 600 may contact the storage node contact area 540 in a direction opposite to the second direction (Y).

[0311] As can be seen from the above description, embodiments of this disclosure can provide a semiconductor device in which bridging phenomena that may occur between adjacent active regions can be prevented.

[0312] Embodiments of this disclosure may provide semiconductor devices with improved operating speed and reduced leakage current.

[0313] Embodiments of this disclosure may provide a semiconductor device in which the active region is defined by forming a relatively shallow cell isolation region, thereby reducing process complexity.

[0314] The embodiments disclosed herein can provide various effects that can be directly or indirectly identified.

[0315] Those skilled in the art will understand that this disclosure may be made in other specific ways than those described herein. Furthermore, claims not expressly listed in the appended claims may be combined as embodiments or proposed as new claims through subsequent amendments after the application has been filed.

[0316] Although many exemplary embodiments have been described, it should be understood that modifications and improvements may be made to the disclosed embodiments and other embodiments based on the content described and / or illustrated herein.

Claims

1. A semiconductor device, comprising: Multiple character line structures are configured to extend along a first direction and be spaced apart from each other in a second direction; Multiple active regions are configured to extend along a diagonal direction at an acute angle to the first direction, overlap with the multiple word line structures, and be spaced apart from each other in the first direction; Multiple bit line pad areas, each bit line pad area overlapping one end of a corresponding active area among the multiple active areas, contacting one side of a corresponding word line structure among the multiple word line structures, and including a first material; Multiple storage node pad areas, each storage node pad area overlaps with the other end of one of the multiple active areas, contacts the other side of one of the multiple word line structures, and includes a second material different from the first material; and Multiple pad insulation areas, each pad insulation area is disposed between a corresponding bit line pad area among the multiple bit line pad areas spaced apart from each other in the first direction and each memory node pad area among the multiple memory node pad areas.

2. The semiconductor device of claim 1, wherein, The concentration of impurities in the first material is higher than the concentration of impurities in the second material.

3. The semiconductor device according to claim 1, wherein: The first material is polycrystalline silicon containing impurities; and The second material is monocrystalline silicon.

4. The semiconductor device according to claim 1, wherein: The height of each bit line pad area in the plurality of bit line pad areas is equal to the height of each storage node pad area in the plurality of storage node pad areas; and The height of each bit line pad area is equal to the height of each pad insulation area in the plurality of pad insulation areas.

5. The semiconductor device of claim 1, wherein, Each of the plurality of bit line pad areas, each of the plurality of memory node pad areas, and each of the plurality of pad insulation areas is disposed on the same plane as the surface of the plurality of active areas.

6. The semiconductor device according to claim 1, wherein: The second direction is perpendicular to the first direction; and The second direction forms an acute angle with the diagonal direction.

7. The semiconductor device of claim 1, wherein, The angle formed between the diagonal direction and the first direction is in the range of 30 degrees to 60 degrees.

8. The semiconductor device according to claim 1, further comprising: Multiple bit line contact areas, each bit line contact area is in contact with the top surface of a corresponding bit line pad area among the multiple bit line pad areas; Multiple bit line electrode layers, each bit line electrode layer is disposed on a corresponding bit line contact area among the multiple bit line contact areas, overlaps with a corresponding bit line pad area among the multiple bit line pad areas, and extends along the second direction; Multiple bit line spacers, each bit line spacer contacting two sides of a corresponding bit line electrode layer among the multiple bit line electrode layers and extending along the second direction; and Multiple storage node contact areas, each of which is in contact with the top surface of a corresponding storage node pad area.

9. The semiconductor device of claim 1, wherein, The plurality of active regions are further arranged to be spaced apart from each other in the second direction and spaced apart from each other in the diagonal direction.

10. The semiconductor device according to claim 9, wherein: The plurality of bit line pad areas are arranged to be spaced apart from each other in the second direction; and The plurality of storage node pad areas are arranged to be spaced apart from each other in the second direction.

11. A method for manufacturing a semiconductor device, the method comprising: Multiple active regions are formed, which are repeatedly spaced apart from each other in a first direction and a second direction, extend along a diagonal direction relative to the first direction, and are surrounded by a cell isolation region. Multiple first pad areas are formed, each first pad area overlapping one end of a corresponding active area among the multiple active areas and extending along the second direction; Multiple pad insulation areas are formed, each pad insulation area is in contact with two sides of each of the multiple first pad areas and extends along the second direction; as well as Multiple second pad areas are formed, which overlap with the other end of one of the multiple active areas, extend along the second direction, and are spaced apart from the multiple first pad areas.

12. The method of claim 11, further comprising: An active layer is formed above the plurality of active regions and the unit isolation region. Forming the plurality of first pad regions includes removing a portion of the active layer.

13. The method of claim 11, further comprising: Multiple fill areas are formed between the plurality of first pad areas. Forming the plurality of pad insulating regions includes removing a portion of each of the plurality of filling regions.

14. The method of claim 11, further comprising: Multiple word line structures are formed, which overlap with the center of the multiple active regions, extend along the first direction, and are repeatedly spaced apart from each other in the second direction.

15. The method according to claim 14, wherein, Forming the plurality of word line structures includes: cutting a portion of each of the plurality of first pad areas, a portion of each of the plurality of second pad areas, and a portion of each of the plurality of pad insulating areas.

16. The method of claim 14, further comprising: Multiple bit line electrode layers are formed, which overlap with the multiple first pad regions and extend along the second direction; as well as Multiple storage node contact areas are formed, and the multiple storage node contact areas overlap with the multiple second pad areas.

17. The method of claim 16, further comprising: Multiple bit line contact areas are formed, and each bit line contact area is disposed between a corresponding bit line electrode layer among the multiple bit line electrode layers and a corresponding first pad area among the multiple first pad areas. Multiple bit line spacers are formed, each bit line spacer contacting two sides of each bit line electrode layer among the multiple bit line electrode layers and extending along the second direction; Multiple bit line cover layers are formed, and each bit line cover layer is in contact with the top surface of a corresponding bit line electrode layer among the multiple bit line electrode layers; as well as Multiple contact insulation areas are formed, each contact insulation area being disposed between the multiple storage node contact areas that are adjacent to each other in the second direction.

Citation Information

Patent Citations

  • Pick and place device and method for correction of head position thereof

    KR1020250062249A