Airtight sealing structure applied to wafer level packaging
By using a combination of concave and convex structures and electroplating layers in the wafer-level packaging of thin film bulk acoustic wave filters to form a three-dimensional sealing ring, the bubble problem and Sn overflow problem in the gold-tin or gold-gold gas sealing method are solved. Achieved higher airtightness and miniaturization effect.
Patent Information
- Application Number
- CN202323447625.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-18
- Publication Date
- 2024-10-18
- Estimated Expiration
- 2033-12-18
AI Technical Summary
In the existing wafer-level packaging of thin-film bulk acoustic wave filters, the gold-tin or gold-gold hermetic sealing method has tiny bubbles that cannot be completely eutectic, causing sealing failure. In addition, the thickness of Sn is too large, causing overflow, which affects the miniaturization and performance of the device. Module integration.
The cap wafer is used to set the concave structure and the functional wafer is set to have the convex structure. By electroplating the Ni-Sn-Ag layer and the Au layer, a three-dimensional sealing ring is formed, which reduces the width of the sealing ring and reduces the possibility of Sn overflow. The concave and convex structure is used Improves air tightness and reduces stress buildup.
It achieves smaller sealing ring width and higher air tightness, reduces Sn overflow and stress mismatch, and improves device reliability and module integration density.
Smart Images

Figure CN221861633U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of packaging, and in particular relates to an airtight sealing structure applied to wafer-level packaging. Background Art
[0002] With the rapid development of wireless communication technology and the multifunctionalization of communication terminals, higher performance requirements are put forward for frequency devices working in the radio frequency band. Compared with traditional dielectric ceramic filters and surface acoustic wave (SAW) filters, film bulk acoustic wave resonators (FBARs) are widely used in the field of wireless communications because of their excellent characteristics such as high operating frequency, low loss, stable temperature characteristics, large power capacity, high quality factor, and small size. Generally speaking, after the processing and preparation of film bulk acoustic wave resonators and filters, they need to be packaged to ensure the reliability of the subsequent devices.
[0003] In recent years, the packaging method commonly used for resonators and filters is wafer-level packaging (WLP) technology, which usually includes bonding two substrates to each other to form a sealed cavity so that the key chip structure is sealed in the sealed cavity. In addition, in order to regulate the performance of the resonator and the filter, passive devices such as capacitors and inductors are usually added to the substrate of the device. The existing wafer-level packaging of thin-film bulk acoustic wave filters mainly uses gold-tin or gold-gold as the metal for airtight sealing. Au-Sn is used as an example later; the current process scheme has several main technical disadvantages: 1. The sealing of Au-Sn is a process of melting eutectic, but due to various defects in preparation, there are many tiny bubbles on the entire sealing ring that cannot be completely eutectic. If these tiny bubbles form a through passage, the airtight seal fails. This determines that the sealing ring needs a certain width to ensure that there is no continuous through passage. 2. In order to ensure the effect of Au-Sn eutectic welding, the thickness of Sn must be large, but this causes Sn to overflow when it melts and enter the working area of the device, causing device failure. The above two disadvantages lead to a further increase in the size of the device, which is not conducive to the miniaturization of the device and further affects the subsequent module integration. Utility Model Content
[0004] In order to solve the problems existing in the above-mentioned prior art, the utility model proposes an airtight sealing structure applied to wafer-level packaging, including a cap wafer and a functional wafer. The cap wafer is provided with a recessed structure, which includes a first step and a second step, and there is an inclined surface between the first step structure and the second step structure; the functional wafer is provided with a protruding structure, and the protruding structure of the functional wafer corresponds to the recessed structure of the cap wafer.
[0005] Preferably, the concave structure of the cap wafer is larger than the convex structure of the functional wafer.
[0006] Preferably, a Ni—Sn—Ag layer is electroplated on the surface of the first terrace and the inclined surface between the first terrace and the second terrace of the cap wafer recess structure.
[0007] Preferably, an Au layer is provided on the surfaces of the terraces and the slopes of the protruding structures of the functional wafer.
[0008] Beneficial effects of the utility model:
[0009] The utility model provides a convex structure on the cap wafer and a concave structure on the functional wafer, thereby reducing the distance occupied by the entire sealing ring in the horizontal direction without changing the actual length of the sealing line, thereby ensuring airtightness. The utility model provides a concave structure on the functional wafer to effectively reduce the overflow effect of Sn. Through capillary phenomenon and gravity, most of the tin is adsorbed near the concave-convex structure; due to the existence of the concave-convex structure, the connection of the entire micro-through hole needs to pass through several bending areas, and the probability of penetration is greatly reduced. Moreover, the structure reduces the horizontal width of the sealing ring without reducing the actual length of the sealing ring, and also reduces the mismatch of wafer stress through the supporting structure, reducing the warping of the wafer; the application makes the originally horizontal sealing ring into a three-dimensional sealing ring, and deposits metal (gold-tin or gold-gold) on the inclined surface, thereby reducing the width of the sealing ring, accommodating more working areas, and reducing the accumulation of stress. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figure 1 The figure is a diagram of the airtight structure of wafer-level packaging in the prior art;
[0011] Figure 2 This is a diagram of the airtight structure of the wafer-level package of the utility model;
[0012] Figure 3 This is a wafer structure diagram of the utility model;
[0013] Figure 4 This is a diagram of the airtight structure of a wafer-level package according to an embodiment of the utility model;
[0014] Among them, 1. The first step, 2. The second step, 3. The inclined plane. DETAILED DESCRIPTION
[0015] The technical solution of the present invention will be fully described below in conjunction with the drawings in the embodiments of the present invention. It should be noted that unless otherwise specifically stated, the names and position descriptions of the components described in the embodiments do not limit the scope of protection of the present invention. At the same time, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by those skilled in the art without making creative efforts belong to the scope of protection of the present invention.
[0016] The existing wafer-level packaging airtight structure is as follows Figure 1 As shown, the device structure includes a cap wafer and a functional wafer. The cap is prepared by magnetron sputtering at the sealing ring position to form a Ti-Cu seed layer, and then a thick Ni-Sn-Ag layer is formed by electroplating. A thick layer of Au is evaporated at the sealing ring position of the functional wafer. In the prior art, an airtight seal is formed by Au-Sn fusion.
[0017] A hermetic sealing structure for wafer level packaging, such as Figure 2 As shown, the device structure includes: a cap wafer and a functional wafer; the cap wafer is provided with a protruding structure, which is evenly distributed at the edge position of the bottom of the cap wafer; the functional wafer is provided with a recessed structure, which is arranged on the upper surface of the functional wafer and corresponds to the protruding structure at the bottom of the cap wafer.
[0018] In this embodiment, the convex structure of the cap wafer is smaller than the concave structure of the functional wafer, so that the convex structure of the cap wafer can perfectly match the concave structure of the functional wafer. By providing a concave structure with grooves on the functional wafer to reduce the horizontal distance of the sealing ring and the width of the sealing ring, it is beneficial to high-density integrated packaging.
[0019] The surface of the raised structure of the cap wafer is electroplated with a Ni-Sn-Ag layer, and the surface of the recessed structure of the functional wafer is provided with an Au layer.
[0020] In another embodiment of the present invention, a gas-tight structure is disclosed, such as Figure 4 As shown, the packaging structure includes: a cap wafer and a functional wafer; wherein the cap wafer is provided with a recessed structure, the recessed structure includes a first step 1 and a second step 2, and a slope 3 is provided between the first step structure and the second step structure; the functional wafer is provided with a protruding structure, and the protruding structure of the functional wafer corresponds to the recessed structure of the cap wafer.
[0021] In this embodiment, the concave structure of the cap wafer is larger than the convex structure of the functional wafer. This structure allows the originally horizontal sealing ring to be made into a three-dimensional sealing ring during the airtight packaging process of the device, thereby reducing the width of the sealing ring, accommodating more working areas, and reducing the accumulation of stress.
[0022] In this embodiment, a Ni—Sn—Ag layer is electroplated on the surface of the first terrace and the inclined surface between the first terrace and the second terrace of the cap wafer recess structure.
[0023] In this embodiment, an Au layer is provided on the terrace and the inclined surface of the protruding structure of the functional wafer. Since there are many devices that need to make such a structure on a wafer, about 16,000 devices / wafer, the traditional wafer structure will expand and contract due to temperature changes during the process, and the stress is mainly in the horizontal direction. Since there are multiple such structures on a wafer, after some thermal processes, the stress will be accumulated, resulting in the warping of the entire wafer; Figure 3 As shown, the wafer structure designed by the utility model optimizes the stress distribution and can effectively reduce the warping of the wafer. That is, during thermal expansion and contraction, the stress at A / B is always balanced, the main forces are offset, the stress accumulation is very small, and the unbalanced force that causes the wafer warping is also very small. The force at C is similar to the original structure and has some effect on the warping, but its own size has been reduced, and the thermal mismatch is greatly reduced; at the same time, due to the existence of A / B, part of its force will be eliminated by the structure. In other words, this mechanism reduces the horizontal width of the sealing ring without reducing the actual length of the sealing ring, and also reduces the mismatch of wafer stress through the supporting structure, thereby reducing the warping of the wafer.
[0024] The above embodiments further illustrate the purpose, technical solutions and advantages of the present invention in detail. It should be understood that the above embodiments are only preferred implementation modes of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made to the present invention within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. An airtight sealing structure for wafer-level packaging, comprising a cap wafer and a functional wafer, characterized in that: The cap wafer is provided with a recessed structure, which includes a first step and a second step, and there is an inclined plane between the first step structure and the second step structure; the functional wafer is provided with a convex structure, and the convex structure of the functional wafer corresponds to the recessed structure of the cap wafer.
2. The airtight sealing structure for wafer-level packaging according to claim 1, characterized in that: The concave structure of the cap wafer is larger than the convex structure of the functional wafer.
3. The airtight sealing structure for wafer-level packaging according to claim 1, characterized in that: A Ni-Sn-Ag layer is electroplated on the surface of the first terrace and the inclined surface between the first terrace and the second terrace of the cap wafer recess structure.
4. The airtight sealing structure for wafer-level packaging according to claim 1, characterized in that: The Au layer is disposed on the terrace surface and the inclined surface of the protruding structure of the functional wafer.
Citation Information
Cited By
Air-tight sealing structure applied to wafer level packaging and manufacturing method of air-tight sealing structure
CN117525002A