Battery monomer, battery and electric equipment

By setting a first groove and a second groove in the pressure relief component of the battery cell, the area and volume ratio of the pressure relief zone are optimized, solving the problem of poor surface flatness of the pressure relief component, improving the production quality and reliability of the battery cell, and reducing the risk of explosion.

CN221861869UActive Publication Date: 2024-10-18CONTEMPORARY AMPEREX TECHNOLOGY CO LTD
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202323664245.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-29
Publication Date
2024-10-18
Estimated Expiration
2033-12-29

AI Technical Summary

Technical Problem

The pressure relief grooves in existing battery cells result in poor surface flatness, affecting the production quality and reliability of the battery cells.

Method used

A first groove and a second groove are provided in the pressure relief component of the battery cell. The first groove is used for cracking, and the second groove is used to guide the predetermined pressure relief area to flip, satisfying the ratio of 0.05mm≤V/A≤0.5mm, so as to optimize the area and volume ratio of the pressure relief area, reduce the height of the material bulge, and improve the surface flatness and pressure relief rate.

Benefits of technology

This improves the production quality and lifespan of battery cells, while reducing the risk of explosion due to thermal runaway and enhancing the reliability and timely pressure relief of battery cells.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221861869U_ABST
    Figure CN221861869U_ABST
Patent Text Reader

Abstract

The embodiment of the utility model provides a battery monomer, a battery and electric equipment, and belongs to the technical field of batteries. The battery monomer comprises a shell, the shell comprises a first wall part, the first wall part comprises a first groove and a second groove, the first groove and the at least one second groove jointly define at least one preset pressure relief area, the first wall part is configured to be capable of cracking along at least one part of the first groove when the battery monomer is subjected to pressure relief, and the second wall part is configured to be capable of cracking along at least one part of the second groove when the battery monomer is subjected to pressure relief. The second groove is configured to guide at least one part of the preset pressure relief area to turn over so as to open at least one part of the preset pressure relief area. The volume of the first groove is V, the sum of the areas of all the preset pressure relief areas is A, and V / A is larger than or equal to 0.05 mm and smaller than or equal to 0.5 mm. Therefore, the flatness of the surface, provided with the first groove, of the first wall part can be improved, and the service life requirement of the battery monomer in the normal use process and the reliability requirement of the battery monomer during thermal runaway are also considered.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of battery technology, and in particular to a battery cell, a battery and an electrical device. Background Art

[0002] With the development of new energy technology, batteries are used more and more widely, for example, in mobile phones, laptops, electric vehicles, electric cars, electric airplanes, electric ships, electric toy cars, electric toy ships, electric toy airplanes and electric tools, etc.

[0003] For general battery cells, a pressure relief component is provided in the battery cell. When the battery cell is in thermal runaway, the pressure inside the battery cell is released through the pressure relief component to improve the reliability of the battery cell. The pressure relief component can be provided with a pressure relief groove, and the pressure relief component can be cracked along the pressure relief groove when the battery cell is depressurized to release the pressure inside the battery cell. However, the provision of the pressure relief groove may result in poor surface flatness of the pressure relief component, affecting the production quality of the battery cell. Utility Model Content

[0004] The embodiments of the present application provide a battery cell, a battery, and an electrical device, which can effectively improve the production quality of the battery cell.

[0005] In a first aspect, an embodiment of the present application provides a battery cell, comprising a shell and a pressure relief component, the shell comprising a first wall portion, the pressure relief component being arranged on the first wall portion, the pressure relief component comprising a first groove and a second groove, along the thickness direction of the first wall portion, the projection of the first groove and the projection of at least one second groove jointly define at least one predetermined pressure relief area, the pressure relief component being configured to be able to split along at least a portion of the first groove when the battery cell is pressure-released, and the second groove being configured to guide at least a portion of the predetermined pressure relief area to flip over so as to open at least a portion of the predetermined pressure relief area; wherein, the volume of the first groove is V, the sum of the areas of all predetermined pressure relief areas is A, satisfying: 0.05mm≤V / A≤0.5mm.

[0006] In the above technical solution, the pressure relief component includes a first groove, so that the pressure relief component can be split along at least a part of the first groove when the battery cell is depressurized, so as to release the internal pressure of the battery cell. The pressure relief component also includes a second groove, and the first groove and the second groove jointly define at least one predetermined pressure relief area, and the second groove can guide at least a part of the predetermined pressure relief area to flip, so as to open at least a part of the predetermined pressure relief area for pressure relief, and the second groove plays an auxiliary role in the predetermined pressure relief area, making it easier to flip the predetermined pressure relief area, reducing the difficulty of flipping the predetermined pressure relief area, and increasing the opening rate of the predetermined pressure relief area. V / A≤0.5mm, so that when forming the first groove, the excess material squeezed out from the area where the first groove is set in the pressure relief component can be shared by the larger predetermined pressure relief area, reducing the amount of material stacking per unit area in the predetermined pressure relief area, so that the height of the material stacking protrusion formed on the surface of the predetermined pressure relief area due to the squeezing of the material in the area where the first groove is set in the pressure relief component is not too large, on the one hand, the flatness of the surface of the pressure relief component where the first groove is set is improved, and on the other hand, the risk of releasing a large residual stress during normal use of the battery cell due to the excessive height of the material stacking protrusion in the predetermined pressure relief area, resulting in reduced fatigue strength of the pressure relief component, thereby improving the service life of the battery cell; V / A≥0.05mm, so that the height of the material stacking protrusion formed on the surface of the predetermined pressure relief area due to the squeezing of the material in the area where the first groove is set in the pressure relief component is not too small, and the residual stress released by the material stacking protrusion helps the pressure relief component to crack along the first groove more promptly when the battery cell is thermally runaway, thereby improving the timeliness of pressure relief of the battery cell, reducing the risk of explosion of the battery cell, and thus improving the reliability of the battery cell. Therefore, 0.05mm≤V / A≤0.5mm can not only improve the flatness of the surface of the pressure relief component where the first groove is set and improve the production quality of the battery cell, but also take into account the service life requirements of the battery cell during normal use and the reliability requirements of the battery cell during thermal runaway.

[0007] In some embodiments, 0.1mm≤V / A≤0.35mm. V / A≤0.35mm, on the one hand, further improves the flatness of the surface of the first groove of the pressure relief component, and on the other hand, further reduces the influence of the material protrusion in the predetermined pressure relief area on the fatigue strength of the pressure relief component; V / A≥0.1mm, further improves the timeliness of the pressure relief of the battery cell, and further reduces the risk of explosion of the battery cell.

[0008] In some embodiments, 82 mm 3 ≤V≤450mm 3 . V≤450mm 3 , so that the amount of extrusion during the forming of the first groove is not too large, reducing the forming force on the pressure relief component during the forming of the first groove, and reducing the risk of damage to the pressure relief component during the forming of the first groove; V ≥ 82mm 3, so that the amount of extruded material when forming the first groove is not too small, it is easier to meet the depth, width and length requirements of the first groove, and reduce the difficulty of forming the first groove.

[0009] In some embodiments, 115 mm 3 ≤V≤265mm 3 . V≤265mm 3 , further reducing the amount of material extruded during the forming of the first groove, further reducing the forming force on the pressure relief component during the forming of the first groove, and reducing the risk of damage to the pressure relief component during the forming of the first groove; V ≥ 115mm 3 , further increasing the amount of extruded material when forming the first groove, and further reducing the difficulty of forming the first groove.

[0010] In some embodiments, 160 mm 2 ≤A≤1500mm 2 . A≤1500mm 2 , so that the area of ​​the predetermined pressure relief zone is not too large, reducing the risk of the predetermined pressure relief zone being deformed by the pressure change inside the battery cell, causing the pressure relief component to crack prematurely along the first groove; A≥160mm 2 , so that the pressure relief component has a sufficiently large pressure relief area, thereby increasing the pressure relief rate of the battery cell.

[0011] In some embodiments, 400 mm 2 ≤A≤1200mm 2 . A≤1200mm 2 , further reducing the risk of premature cracking of the pressure relief component along the first groove. A≥400mm 2 , further improving the pressure release rate of the battery cell.

[0012] In some embodiments, along the thickness direction of the first wall portion, the pressure relief component has a first surface and a second surface relative to each other, and the second groove is recessed from the second surface toward the direction close to the first surface; along the width direction of the second groove, the second groove includes a first groove side surface and a second groove side surface that are relatively arranged and connected to the second surface, the first groove side surface is closer to the predetermined pressure relief area than the second groove side surface, the angle between the first groove side surface and the second surface is a, and the angle between the second groove side surface and the second surface is b, which satisfies: 90°≤a<b<180°, and the width direction of the second groove is perpendicular to the thickness direction of the first wall portion. In this way, it is equivalent to reducing the angle between the first groove side surface and the second surface, which can reduce the amount of piled material in the predetermined pressure relief area of ​​the excess material extruded when forming the second groove, reduce the height of the piled material protrusion formed on the surface of the predetermined pressure relief area due to the extrusion of the area where the second groove of the pressure relief component is set, and improve the flatness of the surface of the predetermined pressure relief area.

[0013] In some embodiments, 90°≤a≤150°. The angle between the first groove side and the second surface is further reduced, and the inclination angle of the first groove side is further reduced, which is beneficial to reduce the amount of excess material extruded in the predetermined pressure relief area when forming the second groove.

[0014] In some embodiments, 90°<b≤170°. The angle between the side surface of the second groove and the second surface is further reduced, the inclination angle of the side surface of the second groove is further reduced, and the difficulty of forming the second groove is reduced.

[0015] In some embodiments, the pressure relief component is provided with a plurality of second grooves, and along the thickness direction of the first wall portion, the projection of the first groove and the projection of the plurality of second grooves jointly define a plurality of predetermined pressure relief areas, and each predetermined pressure relief area is provided corresponding to one or more second grooves. When the battery cell is in thermal runaway, the plurality of predetermined pressure relief areas can be opened, and when the total pressure relief area of ​​the pressure relief component is constant, the opening rate of the predetermined pressure relief areas can be increased, and pressure relief can be achieved more quickly.

[0016] In some embodiments, along the thickness direction of the first wall portion, the projection of the second groove does not overlap with the projection of the first groove, thereby reducing the mutual influence between the first groove and the second groove during the processing and reducing the risk of the first groove and the second groove being connected to each other during the processing.

[0017] In some embodiments, along the width direction of the second groove, the second groove is spaced apart from the first groove, and the width direction of the second groove is perpendicular to the thickness direction of the first wall portion. In this way, it is possible to achieve that the projection of the second groove along the thickness direction of the first wall portion does not overlap with the projection of the first groove along the thickness direction of the first wall portion, which can further reduce the mutual influence between the first groove and the second groove during the processing, and can reduce the residual stress between the pressure relief component in the area where the first groove is set and the pressure relief component in the area where the second groove is set, and can reduce the risk of cracks caused by the pressure relief component cracking along the first groove spreading to the second groove, thereby causing the pressure relief component to crack along the second groove.

[0018] In some embodiments, along the thickness direction of the first wall portion, two ends of the projection of the second groove along the extension direction respectively extend out of two ends of the projection of the first groove, so that the second groove is longer and the auxiliary flipping effect of the second groove on the predetermined pressure relief area is enhanced.

[0019] In some embodiments, the minimum residual thickness of the first groove is D1, and the minimum residual thickness of the second groove is D2, satisfying: D1<D2. The strength of the area where the first groove is set in the pressure relief component is smaller than the strength of the area where the second groove is set in the pressure relief component, so that the pressure relief component can be preferentially split along the first groove to achieve rapid opening of the predetermined pressure relief area.

[0020] In some embodiments, along the thickness direction of the first wall portion, the maximum groove depth of the first groove is H1, and the maximum groove depth of the second groove is H2, satisfying: H2

[0021] In some embodiments, along the thickness direction of the first wall portion, the maximum groove depth of the first groove is H1, the thickness of the pressure relief component is D, and 0.16≤H1 / D<1. This ensures that the maximum depth of the first groove accounts for a small proportion of the thickness of the pressure relief component, and the bursting pressure of the battery cell is not too high, which is beneficial to improving the timeliness of the pressure relief of the battery cell.

[0022] In some embodiments, 0.4 mm ≤ H1 ≤ 2 mm, 0.8 mm ≤ D ≤ 2.5 mm. The maximum depth of the first groove and the thickness of the pressure relief component are controlled within a reasonable range, which has better economy.

[0023] In some embodiments, along the thickness direction of the first wall portion, the pressure relief component has a first surface and a second surface opposite to each other, the first groove is arranged on the first surface, and the second groove is arranged on the second surface, so that the first groove and the second groove are respectively located on both sides of the pressure relief component along the thickness direction of the first wall portion, so that the first groove and the second groove are respectively processed on both sides of the pressure relief component, which is conducive to reducing the mutual influence of the first groove and the second groove during the processing.

[0024] In some embodiments, along the width direction of the second groove, the projection of the first groove overlaps with the projection of the second groove at least partially, and the width direction of the second groove is perpendicular to the thickness direction of the first wall portion. This makes the projections of the first groove and the second groove in the width direction of the second groove overlap each other, so that on the one hand, the absorption effect of the second groove on the residual material extruded during the molding of the first groove can be improved, and the risk of the extruded residual material of the first groove diffusing to the surface close to the shell along the width direction of the second groove, thereby causing the surface to be uneven, and on the other hand, the absorption effect of the second groove on the deformation energy of the battery cell when the battery cell is subjected to internal and external forces and deformed along the width direction of the second groove can be improved, and the influence of the expansion and deformation of the battery cell along the width direction of the second groove on the pressure relief component can be reduced.

[0025] ​In some embodiments, along the thickness direction of the first wall portion, the bottom surface of the second groove is closer to the first surface than the bottom surface of the first groove. This structure is conducive to achieving more overlapping areas between the projections of the second groove and the first groove in the width direction of the second groove, further improving the absorption effect of the second groove on the excess material squeezed out of the first groove during molding, and further improving the absorption effect of the second groove on the deformation energy of the battery cell when the battery cell is subjected to internal and external forces and deformed along the width direction of the second groove.

[0026] In some embodiments, along the thickness direction of the first wall portion, the maximum groove depth of the second groove is H2, and the minimum residual thickness of the first groove is D1, satisfying: D1<H2. Such a structure is conducive to achieving more overlapping areas of the projections of the second groove and the first groove in the width direction of the second groove, further improving the absorption effect of the second groove on the residual material extruded by the first groove during molding, and further improving the absorption effect of the second groove on the deformation energy of the battery cell when the battery cell is subjected to internal and external forces and deformed along the width direction of the second groove.

[0027] In some embodiments, the first groove includes a plurality of grooves arranged in sequence along the direction from the first surface to the second surface, and along the thickness direction of the first wall, in two adjacent grooves, the first groove away from the first surface is arranged on the groove bottom surface of the first groove close to the first surface; wherein, the first groove arranged on the first surface among the multi-level grooves is the first-level groove, and along the width direction of the second groove, the projection of the second groove overlaps with the projection of the first-level groove at least partially, and the width direction of the second groove is perpendicular to the thickness direction of the first wall. By arranging the first groove in the direction of the thickness of the first wall, the grooves of each level can be processed one by one along the direction from the first surface to the second surface when forming the first groove, thereby reducing the forming depth of each level of groove, reducing the forming force on the pressure relief component when forming the first groove, and reducing the risk of the pressure relief component being damaged when forming the first groove. Since the projection of the first-level groove of the first groove along the width direction of the second groove at least partially overlaps with the projection of the second groove along the width direction of the second groove, the projection of the second groove in the width direction can cover the other levels of grooves in the first groove except the first-level groove, thereby, on the one hand, improving the absorption effect of the second groove on the excess material squeezed out of the first groove when the multi-level groove is formed, and on the other hand, further improving the absorption effect of the second groove on the deformation energy of the battery cell when the battery cell is subjected to internal and external impact forces and deformed, thereby reducing the influence of the expansion and deformation of the battery cell along the width direction of the second groove on the pressure relief component.

[0028] In some embodiments, along the thickness direction of the first wall portion, the bottom surface of the second groove is flush with the bottom surface of the first-stage groove, or the bottom surface of the second groove is closer to the first surface than the bottom surface of the first-stage groove. In this way, the projection of the second groove in the width direction can cover the grooves of all stages except the first-stage groove in the first groove, thereby, on the one hand, improving the absorption effect of the second groove on the excess material squeezed out of the first groove when the multi-stage groove is formed, and on the other hand, improving the absorption effect of the second groove on the deformation energy of the battery cell when the battery cell is subjected to internal and external impact forces and deformed, thereby reducing the influence of the expansion and deformation of the battery cell along the width direction of the second groove on the pressure relief component.

[0029] In some embodiments, along the thickness direction of the first wall portion, the pressure relief component has a first surface and a second surface opposite to each other, and the first groove and the second groove are both recessed from the second surface toward the first surface. In this way, the first groove and the second groove are arranged on the same side of the pressure relief component in the thickness direction, which makes it easier to process the first groove and the second groove on the pressure relief component, and the first groove and the second groove can be processed without turning the pressure relief component over, which is conducive to optimizing the production rhythm of the battery cell.

[0030] In some embodiments, the first groove includes a multi-stage groove arranged in sequence along the direction from the second surface to the first surface, and along the thickness direction of the first wall portion, in two adjacent stages of grooves, the first stage groove away from the second surface is arranged at the groove bottom surface of the first stage groove close to the second surface; wherein, the first stage groove arranged on the second surface in the multi-stage groove is the first stage groove, and along the thickness direction of the first wall portion, the groove bottom surface of the first stage groove is closer to the second surface than the groove bottom surface of the second groove. By arranging the first groove in the thickness direction of the first wall portion to arrange the multi-stage groove, when forming the first groove, each stage of the groove can be processed one by one along the direction from the second surface to the first surface, thereby reducing the forming depth of each stage of the groove, reducing the forming force on the pressure relief component when forming the first groove, and reducing the risk of the pressure relief component being damaged when forming the first groove. Since the bottom surface of the first-level groove is closer to the second surface than the bottom surface of the second groove, the projection of the second groove along the width direction at least covers the first-level groove of the first groove, so that the second groove has a deeper depth, so that the second groove can have a good absorption effect on the excess material squeezed out when the first-level groove is formed, and the second groove can have a good absorption effect on the deformation energy of the battery cell when the battery cell is subjected to internal and external impact forces and deformed.

[0031] In some embodiments, along the thickness direction of the first wall portion, the maximum groove depth of the second groove is H2, and the maximum groove depth of the first-level groove is H3, satisfying: H3<H2. The second groove has a deeper depth, so that the second groove can have a good absorption effect on the excess material squeezed out when the first-level groove is formed, and the second groove can have a good absorption effect on the deformation energy of the battery cell when the battery cell is subjected to internal and external impact forces and deformed.

[0032] In some embodiments, the first surface is the surface of the pressure relief component facing the outside of the battery cell, and the second surface is the surface of the pressure relief component facing the inside of the battery cell. The first surface is the surface of the pressure relief component facing the outside of the battery cell. When the first groove is set on the first surface, the first groove is set on the outside of the pressure relief component, which is convenient for processing and forming the first groove on the outside of the battery cell, which is conducive to reducing the difficulty of forming the first groove and improving the production efficiency of the battery cell. The second surface is the surface of the pressure relief component facing the inside of the battery cell. When the second groove is set on the second surface, the second groove is set on the inside of the pressure relief component. On the one hand, when the predetermined pressure relief area is turned outward and opened, the two groove sides in the width direction of the second groove are not easy to abut against each other, which is conducive to increasing the opening area of ​​the predetermined pressure relief area; on the other hand, the second groove is not exposed to the outside of the battery cell, reducing the risk of oxidation and corrosion of the pressure relief component in the second groove area.

[0033] In some embodiments, along the thickness direction of the first wall, the projection of the first groove, the projection of the second groove, and the projection of the extension line of the second groove jointly enclose a predetermined pressure relief area; or, along the thickness direction of the first wall, the projection of the first groove, the projection of the extension line of the first groove, and the projection of the second groove jointly enclose a predetermined pressure relief area; or, along the thickness direction of the first wall, the projection of the first groove, the projection of the extension line of the first groove, the projection of the second groove, and the projection of the extension line of the second groove jointly enclose a predetermined pressure relief area. This structure ensures that the projection of the second groove along the thickness direction of the first wall and the projection of the first groove along the thickness direction of the first wall do not form a closed structure, thereby reducing the mutual influence between the first groove and the second groove during the processing process.

[0034] In some embodiments, the first groove extends along an arc track; and / or the second groove extends along a straight track. The first groove extends along an arc track, that is, the first groove is an arc groove. The first groove of this structure only includes one groove segment, which simplifies the structure of the first groove. The second groove extends along a straight track, that is, the second groove is a straight groove, which has a simple structure and is easy to process and form.

[0035] In some embodiments, the first groove includes a first groove section and a second groove section, the first groove section is connected to the second groove section; along the thickness direction of the first wall, the projection of the first groove section, the projection of the second groove section, the projection of the second groove and the projection of the extension line of the second groove together enclose a predetermined pressure relief area; or, along the thickness direction of the first wall, the projection of the first groove section, the projection of the extension line of the first groove section, the projection of the second groove section, the projection of the extension line of the second groove section and the projection of the second groove together enclose a predetermined pressure relief area; or, along the thickness direction of the first wall, the projection of the first groove section, the projection of the extension line of the first groove section, the projection of the second groove section, the projection of the extension line of the second groove section, the projection of the second groove and the projection of the extension line of the second groove together enclose a predetermined pressure relief area. The first groove of this structure has a simple structure, and the stress at the position where the first groove section is connected to the second groove section is more concentrated, weaker, and easier to crack, so that the pressure relief component can quickly crack from the first groove section and the second groove section after cracking from the position where the first groove section is connected to the second groove section when the battery cell is thermally runaway, so that the predetermined pressure relief area is opened more quickly and the pressure is released in time.

[0036] In some embodiments, the first groove includes a first groove section, a second groove section and a third groove section, the second groove section and the third groove section are arranged opposite to each other, the first groove section connects the second groove section and the third groove section, and the first groove section and the second groove are arranged opposite to each other; along the thickness direction of the first wall portion, the projection of the first groove section, the projection of the second groove section, the projection of the third groove section, the projection of the second groove and the projection of the extension line of the second groove together enclose a predetermined pressure relief area; or, along the thickness direction of the first wall portion, the projection of the first groove section, the projection of the second groove section, the projection of the extension line of the second groove section, the projection of the third groove section, the projection of the extension line of the third groove section and the projection of the second groove together enclose a predetermined pressure relief area; or, along the thickness direction of the first wall portion, the projection of the first groove section, the projection of the second groove section, the projection of the extension line of the second groove section, the projection of the third groove section, the projection of the extension line of the third groove section, the projection of the second groove and the projection of the extension line of the second groove together enclose a predetermined pressure relief area. The first groove with this structure makes the intersection of the first groove segment and the second groove segment and the connection position of the first groove segment and the third groove segment weaker, which is easier to crack and open the predetermined pressure relief area for pressure relief, and can further increase the opening area of ​​the predetermined pressure relief area, thereby increasing the pressure relief area of ​​the battery cell and improving the pressure relief rate of the battery cell.

[0037] In some embodiments, the connection position of the second groove section and the first groove section deviates from the two ends of the second groove section, and the connection position of the third groove section and the first groove section deviates from the two ends of the third groove section, so that predetermined pressure relief areas are formed on both sides of the first groove section. In this way, the first groove section of the first groove is located between the two predetermined pressure relief areas, and after the pressure relief component is split along the first groove section, the two predetermined pressure relief areas can be opened in a split manner to relieve pressure when the battery cell is relieved of pressure, so that the two predetermined pressure relief areas can be opened quickly, which is conducive to improving the pressure relief rate of the battery cell.

[0038] In some embodiments, the first slot segment extends along a straight line or an arc track; and / or, the second slot segment extends along a straight line or an arc track; and / or, the third slot segment extends along a straight line or an arc track. If the first slot segment extends along a straight line track, the first slot segment is a straight slot, which can reduce the difficulty of forming the first slot segment. If the first slot segment extends along an arc track, the first slot segment is an arc-shaped slot, and the pressure relief component is more likely to split along the first slot segment when the battery cell is depressurized, so that the predetermined pressure relief area is opened more quickly. If the second slot segment extends along a straight line track, the second slot segment is a straight line slot, which can reduce the difficulty of forming the second slot segment. If the second slot segment extends along an arc track, the second slot segment is an arc-shaped slot, and the pressure relief component is more likely to split along the second slot segment when the battery cell is depressurized, so that the predetermined pressure relief area is opened more quickly. If the third slot segment extends along a straight line track, the third slot segment is a straight slot, which can reduce the difficulty of forming the third slot segment. If the third groove section extends along an arc trajectory, the third groove section is an arc-shaped groove, and the pressure relief component is more likely to split along the third groove section when the battery cell releases pressure, thereby achieving faster opening of the predetermined pressure relief area.

[0039] In some embodiments, the pressure relief component is integrally formed with the first wall portion, so that the first groove and the second groove can be directly formed on the first wall portion to form an integrated pressure relief structure, which has higher reliability, saves the installation process of the pressure relief component, and has better economy.

[0040] In some embodiments, the first groove is stamped and formed on the first wall; and / or the second groove is stamped and formed on the first wall. If the first groove is stamped and formed on the first wall, the first groove is formed in a simple manner, which is conducive to reducing the production cost of the battery cell. If the second groove is stamped and formed on the first wall, the second groove is formed in a simple manner, which is conducive to reducing the production cost of the battery cell.

[0041] In some embodiments, the pressure relief component is separately arranged from the first wall portion, and the pressure relief component is installed on the first wall portion. The pressure relief component is a component independent of the housing, and the pressure relief component and the housing can be produced and assembled separately, with low production difficulty and high efficiency.

[0042] In some embodiments, the first wall portion is a rectangular wall portion, and the first groove and the second groove are arranged along the width direction of the first wall portion. In this way, the second groove is closer to the edge of the first wall portion in the width direction of the first wall portion, so that the area where the second groove is set in the pressure relief component has a higher strength, reducing the risk of the pressure relief component cracking along the second groove when the battery cell is depressurized. In addition, during the use of the battery cell, the expansion amount of the battery cell in the width direction of the first wall portion is greater than the expansion amount in the length direction of the first wall portion, and the expansion of the battery cell in the width direction of the first wall portion has a greater impact on the pressure relief component, and the first groove and the second groove are arranged along the width direction of the first wall portion, and the second groove can have a good absorption effect on the deformation energy of the battery cell when the battery cell expands and deforms along the width direction of the first wall portion, reducing the impact of the expansion of the battery cell along the width direction of the first wall portion on the pressure relief component.

[0043] In some embodiments, the housing includes a shell and an end cover; an opening is formed at least at one end of the shell; the end cover corresponds to the opening one by one, and the end cover closes the opening; wherein at least one end cover is a first wall portion; and / or at least one wall portion in the shell is a first wall portion. If at least one end cover is a first wall portion, so that at least one end cover has a pressure relief function, the difficulty of forming the first groove and the second groove on the end cover or the difficulty of installing the pressure relief component is lower. If at least one wall portion in the shell is a first wall portion, so that the shell has a pressure relief function, when the battery cell is depressurized, the emissions discharged from the inside of the battery cell are not likely to affect the external components outside the end cover, reducing the risk of external components being damaged by emissions.

[0044] In some embodiments, the shell has an opening at only one end, and the wall portion of the shell opposite to the end cap is the first wall portion. The shell has an opening at one end, which makes the structure of the entire battery cell simpler. The first wall portion is the wall portion of the shell opposite to the end cap, which can achieve directional pressure relief from the bottom of the shell.

[0045] In some embodiments, openings are formed at both opposite ends of the shell, and at least one wall portion in the shell is a first wall portion. The shell is a structure with openings formed at both opposite ends, and the electrode assembly can be assembled into the shell through any opening, which can reduce the difficulty of assembling the battery cell and improve the assembly quality of the battery cell. The shell of this structure can make the length (openings are formed at both ends of the shell in the length direction) larger, which is conducive to increasing the capacity of the battery cell.

[0046] In some embodiments, the material of the pressure relief component includes steel. Steel has the characteristic of high strength, and the pressure relief component made of steel has better strength. Under the condition of a certain bursting pressure of the battery cell, the pressure relief component can be made thinner to reduce the volume of the pressure relief component.

[0047] In some embodiments, the steel material is carbon steel or stainless steel.

[0048] In some embodiments, the pressure relief component is made of aluminum alloy, which has the characteristics of light weight and good ductility, and it is easier to process the first groove and the second groove on the pressure relief component.

[0049] In some embodiments, the aluminum alloy includes the following components in mass percentage: aluminum ≥ 99.6%, copper ≤ 0.05%, iron ≤ 0.35%, magnesium ≤ 0.03%, manganese ≤ 0.03%, silicon ≤ 0.25%, titanium ≤ 0.03%, vanadium ≤ 0.05%, zinc ≤ 0.05%, and other single elements ≤ 0.03%. This aluminum alloy has lower hardness, better forming ability, reduces the difficulty of processing the first groove and the second groove, is conducive to improving the processing accuracy of the first groove and the second groove, and improves the pressure relief consistency of the pressure relief component.

[0050] In some embodiments, the aluminum alloy includes the following components in percentage by mass: aluminum ≥ 96.7%, 0.05% ≤ copper ≤ 0.2%, iron ≤ 0.7%, manganese ≤ 1.5%, silicon ≤ 0.6%, zinc ≤ 0.1%, other single element components ≤ 0.05%, and other elements in total ≤ 0.15%. The pressure relief component made of such an aluminum alloy has higher hardness, greater strength, and good anti-destruction ability.

[0051] In a second aspect, an embodiment of the present application provides a battery, comprising a battery cell provided by any embodiment of the first aspect.

[0052] In a third aspect, an embodiment of the present application provides an electrical device, comprising a battery cell provided by any one embodiment of the first aspect, wherein the battery cell is used to provide electrical energy to the electrical device. BRIEF DESCRIPTION OF THE DRAWINGS

[0053] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present application and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.

[0054] Figure 1 A schematic diagram of the structure of a vehicle provided in some embodiments of the present application;

[0055] Figure 2 An exploded view of a battery provided for some embodiments of the present application;

[0056] Figure 3 An exploded view of a battery cell provided for some embodiments of the present application;

[0057] Figure 4 for Figure 3 An assembly diagram of a battery cell is shown;

[0058] Figure 5 for Figure 4 A partial view of the housing is shown;

[0059] Figure 6 for Figure 5 AA section view of the housing shown;

[0060] Figure 7 for Figure 6 A partial enlarged view of point B in the middle;

[0061] Figure 8 Assembly diagrams of battery cells provided for other embodiments of the present application;

[0062] Fig. 9 for Figure 8 A partial view of the housing is shown;

[0063] Fig.10 for Fig. 9 A CC section view of the housing shown;

[0064] Fig.11 for Fig.10 A partial enlarged view of point D in the middle;

[0065] Fig.12 A partial cross-sectional view of a housing provided for some embodiments of the present application;

[0066] Fig.13 for Fig.12 A partial enlarged view of point E in the middle;

[0067] Fig.14 A partial view of a housing (the first groove is an arc-shaped groove) provided for some embodiments of the present application;

[0068] Fig.15 for Fig.14 FF section view of the housing shown;

[0069] Fig.16 A partial view of a housing (the first groove is an arc-shaped groove) provided for some other embodiments of the present application;

[0070] Fig.17 A partial view of a housing (the first groove is an arc-shaped groove) provided for some other embodiments of the present application;

[0071] Fig.18 A partial view of a housing (the first groove is a V-shaped groove) provided for some embodiments of the present application;

[0072] Fig.19 for Fig.18 GG section view of the housing shown;

[0073] Fig. 20 A partial view of a housing (the first groove is a V-shaped groove) provided for some other embodiments of the present application;

[0074] Fig.21 A partial view of a housing (the first groove is a V-shaped groove) provided for some other embodiments of the present application;

[0075] Fig. 22 A partial view of a housing (the first groove is an H-shaped groove) provided for some other embodiments of the present application;

[0076] Fig.23 A partial view of a housing (the first groove is an H-shaped groove) provided for some other embodiments of the present application;

[0077] Fig.24 An exploded view of a housing (an opening is formed at one end of the housing, the housing includes a first wall portion, and the pressure relief component is the first wall portion) provided in some embodiments of the present application;

[0078] Fig.25 An exploded view of a housing (an opening is formed at one end of the housing, the housing includes a first wall portion, and a pressure relief component is installed on the first wall portion) provided in some embodiments of the present application;

[0079] Fig.26 An exploded view of a housing (an opening is formed at one end of the housing, and the end cover is a pressure relief component) provided in some embodiments of the present application;

[0080] Fig. 27 An exploded view of a housing (an opening is formed at one end of the housing, the end cover is a first wall portion, and a pressure relief component is installed on the first wall portion) provided in some embodiments of the present application;

[0081] Fig.28 Exploded diagrams of battery cells provided for some other embodiments of the present application.

[0082] Icons: 1-housing; 11-housing; 12-end cover; 13-first wall; 131-pressure relief hole; 14-second wall; 15-third wall; 2-electrode assembly; 21-ear; 3-electrode terminal; 4-current collecting member; 5-insulating member; 6-pressure relief member; 61-first groove; 61a-extension line of the first groove; 611-first groove section; 612-second groove section; 613-third groove section; 614-bottom surface of the first groove; 615-first groove; 62-second groove; 62a-second groove Extension line of the groove; 621-side of the first groove; 622-side of the second groove; 623-first end; 624-second end; 625-bottom surface of the groove of the second groove; 63-predetermined pressure relief area; 64-first surface; 65-second surface; 10-battery cell; 20-housing; 201-first part; 202-second part; 100-battery; 200-controller; 300-motor; 1000-vehicle; X-thickness direction of the first wall; Y-extension direction of the second groove; Z-width direction of the second groove. DETAILED DESCRIPTION

[0083] In order to make the purpose, technical solution and advantages of the embodiments of the present application clearer, the technical solution in the embodiments of the present application will be clearly described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0084] Unless otherwise defined, all technical and scientific terms used in this application have the same meaning as those commonly understood by technicians in the technical field of this application; the terms used in the specification of this application are only for the purpose of describing specific embodiments and are not intended to limit this application; the terms "including" and "having" in the specification and claims of this application and the above-mentioned drawings and any variations thereof are intended to cover non-exclusive inclusions. The terms "first", "second", etc. in the specification and claims of this application or the above-mentioned drawings are used to distinguish different objects, rather than to describe a specific order or a primary and secondary relationship.

[0085] Reference to "embodiment" in this application means that a particular feature, structure, or characteristic described in conjunction with the embodiment may be included in at least one embodiment of the present application. The appearance of the phrase in various places in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments.

[0086] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", and "attached" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be the internal communication of two elements. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0087] The term "and / or" in this application is only a description of the association relationship of associated objects, indicating that there can be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this application generally indicates that the associated objects before and after are in an "or" relationship.

[0088] In the embodiments of the present application, the same reference numerals represent the same components, and for the sake of brevity, detailed descriptions of the same components are omitted in different embodiments. It should be understood that the thickness, length, width and other dimensions of various components in the embodiments of the present application shown in the drawings, as well as the overall thickness, length, width and other dimensions of the integrated device are only exemplary descriptions and should not constitute any limitation to the present application.

[0089] The term "plurality" used in the present application refers to two or more (including two).

[0090] In the embodiment of the present application, the battery cell may be a secondary battery. A secondary battery refers to a battery cell that can be continuously used by activating active materials by charging after the battery cell is discharged.

[0091] Battery cells include, but are not limited to, lithium-ion batteries, sodium-ion batteries, sodium-lithium-ion batteries, lithium metal batteries, sodium metal batteries, lithium-sulfur batteries, magnesium-ion batteries, nickel-hydrogen batteries, nickel-cadmium batteries, lead-acid batteries, and the like.

[0092] A battery cell generally includes an electrode assembly. The electrode assembly includes a positive electrode, a negative electrode, and a separator. During the charge and discharge process of the battery cell, active ions (such as lithium ions) are embedded and removed between the positive electrode and the negative electrode. The separator is set between the positive electrode and the negative electrode to reduce the risk of short circuit between the positive and negative electrodes, while allowing active ions to pass through.

[0093] In some embodiments, the positive electrode may be a positive electrode sheet, and the positive electrode sheet may include a positive electrode current collector and a positive electrode active material disposed on at least one surface of the positive electrode current collector.

[0094] As an example, the positive electrode current collector has two surfaces facing each other in its thickness direction, and the positive electrode active material is disposed on either or both of the two facing surfaces of the positive electrode current collector.

[0095] As an example, the positive electrode current collector may be a metal foil or a composite current collector. For example, as the metal foil, aluminum with a silver-plated surface, stainless steel with a silver-plated surface, stainless steel, copper, aluminum, nickel, carbon electrode, carbon, nickel or titanium, etc. may be used. The composite current collector may include a polymer material base and a metal layer. The composite current collector may be formed by forming a metal material (aluminum, aluminum alloy, nickel, nickel alloy, titanium, titanium alloy, silver and silver alloy, etc.) on a polymer material substrate (such as a substrate of polypropylene, polyethylene terephthalate, polybutylene terephthalate, polystyrene, polyethylene, etc.).

[0096] As an example, the positive electrode active material may include at least one of the following materials: lithium-containing phosphates, lithium transition metal oxides and their respective modified compounds. However, the present application is not limited to these materials, and other traditional materials that can be used as positive electrode active materials for batteries can also be used. These positive electrode active materials can be used alone or in combination of two or more. Among them, examples of lithium-containing phosphates may include, but are not limited to, at least one of lithium iron phosphate (such as LiFePO4 (also referred to as LFP)), a composite material of lithium iron phosphate and carbon, lithium manganese phosphate (such as LiMnPO4), a composite material of lithium manganese phosphate and carbon, lithium iron manganese phosphate, and a composite material of lithium iron manganese phosphate and carbon. Examples of lithium transition metal oxides may include, but are not limited to, lithium cobalt oxide (such as LiCoO2), lithium nickel oxide (such as LiNiO2), lithium manganese oxide (such as LiMnO2, LiMn2O4), lithium nickel cobalt oxide, lithium manganese cobalt oxide, lithium nickel manganese oxide, lithium nickel cobalt manganese oxide (such as LiNi 1 / 3 Co 1 / 3 Mn 1 / 3 O2 (also referred to as NCM 333 )、LiNi 0.5 Co 0.2 Mn 0.3 O2 (also referred to as NCM 523 )、LiNi 0.5 Co 0.25 Mn 0.25 O2 (also referred to as NCM 211 )、LiNi 0.6 Co 0.2 Mn 0.2 O2 (also referred to as NCM 622 )、LiNi 0.8 Co 0.1 Mn 0.1 O2 (also referred to as NCM 811 ), lithium nickel cobalt aluminum oxide (such as LiNi 0.85 Co 0.15 Al 0.05O2) and its modified compounds, etc.

[0097] In some embodiments, the positive electrode may be a foamed metal. The foamed metal may be a nickel foam, a copper foam, an aluminum foam, an alloy foam, or a carbon foam. When the foamed metal is used as the positive electrode, the positive electrode active material may not be provided on the surface of the foamed metal, but of course, the positive electrode active material may also be provided. As an example, a lithium source material, potassium metal or sodium metal may also be filled or / and deposited in the foamed metal, and the lithium source material is lithium metal and / or a lithium-rich material.

[0098] In some embodiments, the negative electrode may be a negative electrode sheet, and the negative electrode sheet may include a negative electrode current collector.

[0099] As an example, the negative electrode current collector may be a metal foil, a foamed metal or a composite current collector. For example, as the metal foil, aluminum or stainless steel, stainless steel, copper, aluminum, nickel, carbon electrode, carbon, nickel or titanium, etc., treated with silver surface, may be used. The foamed metal may be a nickel foam, a copper foam, an aluminum foam, an alloy foam, etc. The composite current collector may include a polymer material base and a metal layer. The composite current collector may be formed by forming a metal material (copper, copper alloy, nickel, nickel alloy, titanium, titanium alloy, silver and silver alloy, etc.) on a polymer material substrate (such as a substrate of polypropylene, polyethylene terephthalate, polybutylene terephthalate, polystyrene, polyethylene, etc.).

[0100] As an example, the negative electrode sheet may include a negative electrode current collector and a negative electrode active material disposed on at least one surface of the negative electrode current collector.

[0101] As an example, the negative electrode current collector has two surfaces facing each other in its thickness direction, and the negative electrode active material is disposed on either or both of the two facing surfaces of the negative electrode current collector.

[0102] As an example, the negative electrode active material may adopt the negative electrode active material for battery cells known in the art. As an example, the negative electrode active material may include at least one of the following materials: artificial graphite, natural graphite, soft carbon, hard carbon, silicon-based materials, tin-based materials, lithium titanate, etc. The silicon-based material may be selected from at least one of elemental silicon, silicon oxide compounds, silicon-carbon composites, silicon-nitrogen composites, and silicon alloys. The tin-based material may be selected from at least one of elemental tin, tin oxide compounds, and tin alloys. However, the present application is not limited to these materials, and other traditional materials that can be used as negative electrode active materials for batteries may also be used. These negative electrode active materials may be used alone or in combination of two or more.

[0103] In some embodiments, the material of the positive electrode current collector may be aluminum, and the material of the negative electrode current collector may be copper.

[0104] In some embodiments, the separator is a separator membrane, which can be any known porous separator membrane with good chemical stability and mechanical stability.

[0105] As an example, the material of the separator may include at least one of glass fiber, non-woven fabric, polyethylene, polypropylene and polyvinylidene fluoride. The separator may be a single-layer film or a multi-layer composite film. When the separator is a multi-layer composite film, the materials of each layer may be the same or different. The separator may be a separate component located between the positive and negative electrodes, or may be attached to the surface of the positive and negative electrodes.

[0106] In some embodiments, the separator is a solid electrolyte, which is disposed between the positive electrode and the negative electrode and serves to transmit ions and isolate the positive and negative electrodes.

[0107] In some embodiments, the battery cell further includes an electrolyte, which plays a role in conducting ions between the positive and negative electrodes. The electrolyte can be liquid, gel or solid. Among them, the liquid electrolyte includes an electrolyte salt and a solvent.

[0108] In some embodiments, the electrolyte salt may include at least one of lithium hexafluorophosphate, lithium tetrafluoroborate, lithium perchlorate, lithium hexafluoroarsenate, lithium bisfluorosulfonyl imide, lithium bistrifluoromethanesulfonyl imide, lithium trifluoromethanesulfonate, lithium difluorophosphate, lithium difluorooxalatoborate, lithium dioxalatoborate, lithium difluorodioxalatophosphate, and lithium tetrafluorooxalatophosphate.

[0109] In some embodiments, the solvent may include at least one of ethylene carbonate, propylene carbonate, ethyl methyl carbonate, diethyl carbonate, dimethyl carbonate, dipropyl carbonate, methyl propyl carbonate, ethyl propyl carbonate, butylene carbonate, fluoroethylene carbonate, methyl formate, methyl acetate, ethyl acetate, propyl acetate, methyl propionate, ethyl propionate, propyl propionate, methyl butyrate, ethyl butyrate, 1,4-butyrolactone, cyclopentane, dimethyl sulfone, methyl ethyl sulfone and diethyl sulfone. The solvent may also be an ether solvent. The ether solvent may include one or more of ethylene glycol dimethyl ether, ethylene glycol diethyl ether, diethylene glycol dimethyl ether, triethylene glycol dimethyl ether, tetraethylene glycol dimethyl ether, 1,3-dioxolane, tetrahydrofuran, methyltetrahydrofuran, diphenyl ether and crown ether.

[0110] Among them, the gel electrolyte includes a skeleton network with a polymer as the electrolyte, combined with an ionic liquid-lithium salt.

[0111] Among them, solid electrolytes include polymer solid electrolytes, inorganic solid electrolytes, and composite solid electrolytes.

[0112] As an example, the polymer solid electrolyte may be polyether (polyethylene oxide), polysiloxane, polycarbonate, polyacrylonitrile, polyvinylidene fluoride, polymethyl methacrylate, a single ion polymer, polyionic liquid-lithium salt, cellulose, and the like.

[0113] As an example, the inorganic solid electrolyte may include an oxide solid electrolyte (crystalline perovskite, sodium superconducting ion conductor, garnet, amorphous LiPON film), a sulfide solid electrolyte (crystalline lithium superion conductor (lithium germanium phosphosulfide, silver germanium sulfide), amorphous sulfide) and one or more of a halide solid electrolyte, a nitride solid electrolyte and a hydride solid electrolyte.

[0114] As an example, the composite solid electrolyte is formed by adding an inorganic solid electrolyte filler to a polymer solid electrolyte.

[0115] In some embodiments, the electrode assembly is a wound structure, wherein the positive electrode sheet and the negative electrode sheet are wound into the wound structure.

[0116] In some embodiments, the electrode assembly is a laminate structure.

[0117] As an example, a plurality of positive electrode sheets and a plurality of negative electrode sheets may be provided respectively, and the plurality of positive electrode sheets and the plurality of negative electrode sheets may be alternately stacked.

[0118] As an example, a plurality of positive electrode sheets may be provided, and the negative electrode sheet may be folded to form a plurality of stacked folded segments, with a positive electrode sheet being sandwiched between adjacent folded segments.

[0119] As an example, both the positive electrode sheet and the negative electrode sheet are folded to form a plurality of folded sections that are stacked.

[0120] As an example, a plurality of separators may be provided, each of which is provided between any adjacent positive electrode sheets or negative electrode sheets.

[0121] As an example, the separator may be disposed continuously, and may be disposed between any adjacent positive electrode sheets or negative electrode sheets by folding or winding.

[0122] In some embodiments, the shape of the electrode assembly can be cylindrical, flat, or polygonal.

[0123] In some embodiments, the electrode assembly is provided with tabs, which can lead current out of the electrode assembly. The tabs include a positive tab and a negative tab.

[0124] In some embodiments, the battery cell may include a housing. The housing is used to encapsulate components such as the electrode assembly and the electrolyte. The housing may be a steel housing, an aluminum housing, a plastic housing (such as polypropylene), a composite metal housing (such as a copper-aluminum composite housing), or an aluminum-plastic film.

[0125] As an example, the battery cell may be a cylindrical battery cell, a prismatic battery cell, a soft-pack battery cell or a battery cell of other shapes. The prismatic battery cell includes a square-shell battery cell, a blade-shaped battery cell, a polygonal battery, such as a hexagonal battery.

[0126] The battery mentioned in the embodiments of the present application refers to a single physical module including one or more battery cells to provide higher voltage and capacity.

[0127] In some embodiments, the battery may be a battery module. When there are multiple battery cells, the multiple battery cells are arranged and fixed to form a battery module.

[0128] In some embodiments, the battery may be a battery pack, which includes a case and battery cells, wherein the battery cells or battery modules are accommodated in the case.

[0129] In some embodiments, the box body can be used as a part of the chassis structure of the vehicle. For example, part of the box body can become at least a part of the floor of the vehicle, or part of the box body can become at least a part of the cross beam and longitudinal beam of the vehicle.

[0130] In some embodiments, the battery may be an energy storage device, which includes an energy storage container, an energy storage cabinet, and the like.

[0131] The development of battery technology must take into account many design factors at the same time, such as energy density, cycle life, discharge capacity, charge and discharge rate and other performance parameters. In addition, battery reliability must also be considered.

[0132] In order to improve the reliability of the battery cell, a pressure relief component can generally be provided in the battery cell. The pressure relief component can be a part of the outer shell of the battery cell or a component installed on the outer shell. When the battery cell thermally runs away, the pressure inside the battery cell can be released through the pressure relief component.

[0133] In order to achieve timely pressure relief of the battery cell, a pressure relief groove can be provided on the pressure relief component so that the pressure relief component can be split along at least a portion of the pressure relief groove when the battery cell is relieved of pressure, so that the pressure relief area of ​​the pressure relief component can be quickly opened to release the pressure inside the battery cell more quickly.

[0134] In order to make the pressure relief area of ​​the pressure relief component easier to open, a flip groove can be set on the pressure relief component to help the pressure relief area of ​​the pressure relief component open, thereby reducing the difficulty of opening the pressure relief area. The setting of the flip groove weakens the ability of the residual material squeezed out of the pressure relief groove to diffuse to the outer surface of the battery cell along the width direction of the flip groove, so that a large part of the residual material squeezed out of the area where the pressure relief groove is set in the pressure relief component will accumulate in the predetermined pressure relief area defined by the flip groove and the pressure relief groove, forming a pile bulge on the surface of the predetermined pressure relief area, which will affect the flatness of the surface of the pressure relief groove set in the pressure relief component, affect the production quality of the battery cell, and even affect the performance of the battery cell.

[0135] Based on the above considerations, in order to solve the problem of low production quality of battery cells, an embodiment of the present application provides a battery cell, the battery cell includes a shell and a pressure relief component, the shell includes a first wall portion, the pressure relief component is arranged on the first wall portion, the pressure relief component includes a first groove (pressure relief groove) and a second groove (flip groove), along the thickness direction of the first wall portion, the projection of the first groove and the projection of at least one second groove jointly define at least one predetermined pressure relief area, the pressure relief component is configured to be able to split along at least a portion of the first groove when the battery cell is depressurized, and the second groove is configured to guide at least a portion of the predetermined pressure relief area to flip, so as to open at least a portion of the predetermined pressure relief area. Wherein, the volume of the first groove is V, the sum of the areas of all predetermined pressure relief areas is A, and the following is satisfied: 0.05mm≤V / A≤0.5mm.

[0136] In such a battery cell, V / A≤0.5mm, so that when forming the first groove, the excess material squeezed out from the area where the first groove is set in the pressure relief component can be shared by the larger predetermined pressure relief area, reducing the amount of material stacking per unit area in the predetermined pressure relief area, so that the height of the material stacking protrusion formed on the surface of the predetermined pressure relief area due to the squeezing of the material in the area where the first groove is set in the pressure relief component is not too large, on the one hand, the flatness of the surface of the pressure relief component where the first groove is set is improved, and on the other hand, the risk of releasing a large residual stress during normal use of the battery cell due to the excessive height of the material stacking protrusion in the predetermined pressure relief area, resulting in reduced fatigue strength of the pressure relief component, thereby improving the service life of the battery cell; V / A≥0.05mm, so that the height of the material stacking protrusion formed on the surface of the predetermined pressure relief area 63 due to the squeezing of the material in the area where the first groove is set in the pressure relief component is not too small, and the residual stress released by the material stacking protrusion helps the pressure relief component to crack along the first groove more promptly when the battery cell is thermally runaway, thereby improving the timeliness of pressure relief of the battery cell, reducing the risk of explosion of the battery cell, and thus improving the reliability of the battery cell. Therefore, 0.05mm≤V / A≤0.5mm can not only improve the flatness of the surface of the pressure relief component where the first groove is set and improve the production quality of the battery cell, but also take into account the service life requirements of the battery cell during normal use and the reliability requirements of the battery cell during thermal runaway.

[0137] The battery cells described in the embodiments of the present application are suitable for batteries and electrical equipment using the battery cells.

[0138] Electrical equipment may be vehicles, mobile phones, portable devices, laptops, ships, spacecraft, electric toys, electric tools, and the like. Vehicles may be fuel vehicles, gas vehicles, or new energy vehicles, and new energy vehicles may be pure electric vehicles, hybrid vehicles, or extended-range vehicles, and the like; spacecraft include airplanes, rockets, space shuttles, and spacecraft, and the like; electric toys include fixed or mobile electric toys, such as game consoles, electric car toys, electric ship toys, and electric airplane toys, and the like; electric tools include metal cutting electric tools, grinding electric tools, assembly electric tools, and railway electric tools, such as electric drills, electric grinders, electric wrenches, electric screwdrivers, electric hammers, impact drills, concrete vibrators, and electric planers, and the like. The embodiments of the present application do not impose any special restrictions on the above-mentioned electrical equipment.

[0139] For the convenience of description, the following embodiments are described by taking the electric device as a vehicle as an example.

[0140] Please refer to Figure 1 , Figure 1The schematic diagram of the structure of the vehicle 1000 provided in some embodiments of the present application. The vehicle 1000 is provided with a battery 100 inside, and the battery 100 can be provided at the bottom, head or tail of the vehicle 1000. The battery 100 can be used to power the vehicle 1000, for example, the battery 100 can be used as an operating power source of the vehicle 1000.

[0141] The vehicle 1000 may further include a controller 200 and a motor 300 , wherein the controller 200 is used to control the battery 100 to supply power to the motor 300 , for example, to meet the power requirements of starting, navigating, and driving the vehicle 1000 .

[0142] In some embodiments of the present application, the battery 100 can not only serve as an operating power source for the vehicle 1000, but also serve as a driving power source for the vehicle 1000, replacing or partially replacing fuel or natural gas to provide driving power for the vehicle 1000.

[0143] Please refer to Figure 2 , Figure 2 The exploded view of the battery 100 provided in some embodiments of the present application. The battery 100 includes a battery cell 10 and a box body 20, and the battery cell 10 is accommodated in the box body 20.

[0144] Among them, the box body 20 is a component for accommodating the battery cell 10. The box body 20 provides a storage space for the battery cell 10. The box body 20 can adopt a variety of structures. In some embodiments, the box body 20 may include a first part 201 and a second part 202, and the first part 201 and the second part 202 cover each other to define a storage space for accommodating the battery cell 10. The first part 201 and the second part 202 may be in a variety of shapes, such as a rectangular parallelepiped, a cylindrical shape, etc. The first part 201 may be a hollow structure with one side open, and the second part 202 may also be a hollow structure with one side open, and the open side of the second part 202 covers the open side of the first part 201, so as to form a box body 20 with a storage space. It is also possible that the first part 201 is a hollow structure with one side open, and the second part 202 is a plate-like structure, and the second part 202 covers the open side of the first part 201, so as to form a box body 20 with a storage space. The first part 201 and the second part 202 can be sealed by a sealing element, and the sealing element can be a sealing ring, a sealant, etc.

[0145] In the battery 100, there may be one or more battery cells 10. If there are more than one battery cell 10, the battery cells 10 may be connected in series, in parallel, or in a mixed connection. A mixed connection means that the battery cells 10 are both connected in series and in parallel. The battery modules may be connected in series, in parallel, or in a mixed connection to form a battery module, and then the battery modules may be connected in series, in parallel, or in a mixed connection to form a whole, and accommodated in the box 20. Alternatively, all the battery cells 10 may be directly connected in series, in parallel, or in a mixed connection, and then the whole formed by all the battery cells 10 may be accommodated in the box 20.

[0146] Please refer to Figure 3 , Figure 3 An exploded view of a battery cell 10 provided in some embodiments of the present application. The battery cell 10 may include a housing 1 and an electrode assembly 2, wherein the electrode assembly 2 is accommodated in the housing 1.

[0147] In some embodiments, the housing 1 may include a shell 11 and an end cover 12 , wherein the shell 11 has an opening and the end cover 12 closes the opening of the shell 11 .

[0148] The shell 11 is a component for accommodating the electrode assembly 2. The shell 11 may be a hollow structure with an opening formed at one end, or a hollow structure with openings formed at opposite ends. The shell 11 may be in various shapes, such as a cylindrical shape, a rectangular parallelepiped shape, etc. The shell 11 may be made of various materials, such as copper, iron, aluminum, steel, aluminum alloy, etc.

[0149] The end cap 12 is a component that closes the opening of the shell 11 to isolate the internal environment of the battery cell 10 from the external environment. The end cap 12 and the shell 11 together define a receiving space for accommodating the electrode assembly 2, the electrolyte and other components. The end cap 12 can be connected to the shell 11 by welding or crimping to close the opening of the shell 11. The shape of the end cap 12 can be adapted to the shape of the shell 1. For example, the shell 11 is a rectangular parallelepiped structure, and the end cap 12 is a rectangular plate structure adapted to the shell 1. For another example, the shell 11 is a cylindrical structure, and the end cap 12 is a circular plate structure adapted to the shell 11. The material of the end cap 12 can also be a variety of materials, such as copper, iron, aluminum, steel, aluminum alloy, plastic, etc. The material of the end cap 12 and the shell 11 can be the same or different.

[0150] In the embodiment where the housing 11 is opened at one end, one end cap 12 may be provided. In the embodiment where the housing 11 is opened at two opposite ends, two end caps 12 may be provided, and the two end caps 12 respectively close the two openings of the housing 11, and the two end caps 12 and the housing 11 together define a receiving space.

[0151] In some embodiments, the battery cell 10 may further include an electrode terminal 3, which is disposed on the housing 1 and is used to electrically connect to the tab 21 of the electrode assembly 2 to input or output the electrical energy of the battery cell 10. The electrode terminal 3 may be disposed on the shell 11 of the housing 1 or on the end cover 12 of the housing 1. The electrode terminal 3 and the tab 21 may be directly connected, for example, the electrode terminal 3 and the tab 21 are directly welded. The electrode terminal 3 and the tab 21 may also be indirectly connected, for example, the electrode terminal 3 and the tab 21 are indirectly connected through a current collecting member 4. The current collecting member 4 may be a metal conductor, for example, copper, iron, aluminum, steel, aluminum alloy, etc.

[0152] As an example, Figure 3 As shown, an opening is formed at one end of the shell 11, and there is one end cap 12 in the shell 1, and one end cap 12 closes one opening of the shell 11. Two electrode terminals 3 are arranged on the end cap 12, and the two electrode terminals 3 are respectively a positive electrode terminal and a negative electrode terminal. A positive electrode ear and a negative electrode ear are formed at one end of the electrode assembly 2 facing the end cap 12, and the positive electrode terminal is connected to the positive electrode ear through a current collecting component 4, and the negative electrode terminal is connected to the negative electrode ear through another current collecting component 4.

[0153] In some embodiments, please refer to Figure 3 The battery cell 10 may further include an insulating member 5, which is a component that separates the housing 11 from the electrode assembly 2, and the insulating member 5 is used to achieve insulation isolation between the housing 11 and the electrode assembly 2. The insulating member 5 is made of insulating material, and the material of the insulating member 5 includes but is not limited to: plastic, rubber, etc.

[0154] As an example, the insulating member 5 is wrapped around the outside of the electrode assembly 2 along the circumferential direction of the opening of the shell 11. The electrode assembly 2 in the shell 1 can be one or more. If there is one electrode assembly 2, the insulating member 5 is wrapped around the electrode assembly 2; if there are multiple electrode assemblies 2, one insulating member 5 can be set corresponding to one electrode assembly 2, and each insulating member 5 is wrapped around one electrode assembly 2, or multiple electrode assemblies 2 can be used as an integral component, and the insulating member 5 is wrapped around the integral component.

[0155] Please refer to Figure 4-Figure 6 , Figure 4 for Figure 3 The assembly diagram of the battery cell 10 shown in FIG. Figure 5 for Figure 4 A partial view of the housing 1 is shown; Figure 6 for Figure 5AA cross-sectional view of the housing 1 is shown. The embodiment of the present application provides a battery cell 10, including a housing 1 and a pressure relief component 6, the housing 1 includes a first wall portion 13, the pressure relief component 6 is arranged on the first wall portion 13, the pressure relief component 6 includes a first groove 61 and a second groove 62, along the thickness direction of the first wall portion 13, the projection of the first groove 61 and the projection of at least one second groove 62 jointly define at least one predetermined pressure relief area 63, the pressure relief component 6 is configured to be able to split along at least a portion of the first groove 61 when the battery cell 10 is depressurized, and the second groove 62 is configured to guide at least a portion of the predetermined pressure relief area 63 to flip, so as to open at least a portion of the predetermined pressure relief area 63.

[0156] The volume of the first groove 61 is V, and the sum of the areas of all the predetermined pressure relief zones 63 is A, satisfying: 0.05 mm ≤ V / A ≤ 0.5 mm.

[0157] The housing 1 includes a plurality of walls, which together define a receiving space inside the housing 1 to accommodate the electrode assembly 2, the electrolyte and other components, and the other components may be current collecting components 4, insulating components 5 and other components. Among the plurality of walls of the housing 1, one wall may be the first wall 13, or a plurality of walls may be the first wall 13. It is understandable that, taking the housing 1 as a rectangular parallelepiped as an example, there are six walls in the housing 1, and one, two, three, four, five or six walls may be the first wall 13. In the housing 1, at least one end cap 12 may be the first wall 13, or at least one wall in the shell 11 may be the first wall 13.

[0158] The pressure relief component 6 is a component in the battery cell 10 for releasing the pressure inside the battery cell 10. The pressure relief component 6 can be integrally formed with the outer shell 1. It can be understood that a part of the outer shell 1 can be used as the pressure relief component 6. For example, the pressure relief component 6 is integrally formed with the end cover 12 of the outer shell 1; for another example, the pressure relief component 6 is integrally formed with a wall portion of the shell 11 of the outer shell 1. The pressure relief component 6 can also be separately provided from the outer shell 1. The pressure relief component 6 and the outer shell 1 are two components produced separately, and the pressure relief component 6 is installed on the outer shell 1. For example, the pressure relief component 6 is installed on the end cover 12 of the outer shell 1; for another example, the pressure relief component 6 is installed on the shell 11.

[0159] The first groove 61 is a pressure relief groove provided in the pressure relief component 6. When the pressure inside the battery cell 10 reaches the bursting pressure of the pressure relief component 6, the pressure relief component 6 can be split along at least a portion of the first groove 61 to open the predetermined pressure relief area 63. It is understandable that when the battery cell 10 is depressurized, the pressure relief component 6 can be split along the entire first groove 61, or can be split along a portion of the first groove 61. The first groove 61 can be formed in a variety of ways, such as stamping, milling, etc. The first groove 61 may include at least one groove segment, and the cross-section of the groove segment may have a variety of shapes, such as a rectangle, a trapezoid, etc. The cross-section of the groove segment is perpendicular to the extension direction of the groove segment. The shape of the first groove 61 may be various, for example, the first groove 61 is a groove extending along an arc trajectory, and for another example, the first groove 61 includes a plurality of groove segments, and the plurality of groove segments may form a U-shaped, H-shaped, V-shaped, Y-shaped, X-shaped, T-shaped, and other structures.

[0160] The second groove 62 is a flip groove provided on the pressure relief component 6. When the pressure relief component 6 is split along at least a portion of the first groove 61, the second groove 62 can guide at least a portion of the predetermined pressure relief area 63 to flip. That is, the second groove 62 plays a role in helping the predetermined pressure relief area 63 to flip, making it easier for the predetermined pressure relief area 63 to flip toward the outside of the battery cell 10, thereby quickly opening the predetermined pressure relief area 63. The second groove 62 can guide the entire flipping of the predetermined pressure relief area 63, or the second groove 62 can only guide the flipping of a portion of the predetermined pressure relief area 63. During the pressure relief process of the battery cell 10, the pressure relief component 6 can be split along at least a portion of the first groove 61, and generally will not be split along the second groove 62. The minimum thickness of the residual portion of the pressure relief component 6 in the area where the first groove 61 is set may be less than the minimum thickness of the residual portion of the pressure relief component 6 in the area where the second groove 62 is set, so that the pressure relief component 6 in the area where the first groove 61 is set is easier to split than the pressure relief component 6 in the area where the second groove 62 is set. The second groove 62 can be formed in various ways, such as stamping, milling, etc. The second groove 62 can have various shapes, such as the second groove 62 is a groove extending along an arc track, and the second groove 62 is a groove extending along a straight track. The cross-section of the second groove 62 can have various shapes, such as a rectangle, a trapezoid, etc.

[0161] The second groove 62 not only has the function of facilitating the flipping of the predetermined pressure relief area 63, but also has a buffering function. The second groove 62 can absorb the excess material extruded when the first groove 61 is formed, reducing the risk of the extruded excess material of the first groove 61 spreading to the surface close to the shell 1 along the width direction Z of the second groove, and improving the flatness of the surface of the shell 1 along the width direction Z of the second groove. When the shell 1 of the battery cell 10 is subjected to internal and external impact forces and deformed along the width direction Z of the second groove, the second groove 62 can also absorb the deformation energy of the shell 1, reducing the influence of the expansion deformation of the battery cell 10 along the width direction Z of the second groove on the pressure relief component 6.

[0162] The second groove 62 and the first groove 61 can be arranged on the same surface of the pressure relief component 6 along the thickness direction X of the first wall portion, or the second groove 62 and the first groove 61 can be arranged on two opposite surfaces of the pressure relief component 6 along the thickness direction X of the first wall portion. The second groove 62 and the first groove 61 can be directly connected, or the second groove 62 and the first groove 61 can not contact each other. If the second groove 62 and the first groove 61 are directly connected, the second groove 62 and the first groove 61 can be arranged on the same surface of the pressure relief component 6, or the second groove 62 and the first groove 61 can jointly enclose a predetermined pressure relief area 63. If the second groove 62 and the first groove 61 do not contact each other, along the thickness direction X of the first wall portion, the projection of the second groove 62 and the projection of the first groove 61 can partially overlap or not overlap. If the projection of the second groove 62 does not overlap with the projection of the first groove 61 along the thickness direction X of the first wall portion, the projection of the second groove 62, the projection of the extension line 62a of the second groove and the projection of the first groove 61 may together enclose a predetermined pressure relief area 63; or the projection of the first groove 61, the projection of the extension line 61a of the first groove and the projection of the second groove 62 may together enclose a predetermined pressure relief area 63; or the projection of the first groove 61, the projection of the extension line 61a of the first groove, the projection of the second groove 62 and the projection of the extension line 62a of the second groove may together enclose a predetermined pressure relief area 63.

[0163] The predetermined pressure relief area 63 is an area of ​​the pressure relief component 6 defined by the projection of the first groove 61 and at least one second groove 62 along the thickness direction X of the first wall. Along the thickness direction X of the first wall, the projection of the first groove 61 and the projection of one second groove 62 may define a predetermined pressure relief area 63, for example, the first groove 61 is a V-shaped groove, and the second groove 62 is a linear groove; along the thickness direction X of the first wall, the projection of the first groove 61 and the projection of one second groove 62 may define multiple predetermined pressure relief areas 63, for example, the first groove 61 is an H-shaped groove, the second groove 62 is an annular groove, and the first groove 61 is located in the circular area defined by the second groove 62; along the thickness direction X of the first wall, the projection of the first groove 61 and the projection of one second groove 62 may define multiple predetermined pressure relief areas 63. The projection of the groove 61 and the projection of the plurality of second grooves 62 define a predetermined pressure relief area 63, for example, the first groove 61 is an H-shaped groove, the second groove 62 is a linear groove, the plurality of second grooves 62 are arranged at intervals along the extension direction of the second groove 62, and are located on the same side of the first groove 61; along the thickness direction X of the first wall portion, the projection of the first groove 61 and the projection of the plurality of second grooves 62 may also define three or more predetermined pressure relief areas 63, for example, the first groove 61 is an H-shaped groove, the second groove 62 is a linear groove, and the first groove 61 is located between two second grooves 62.

[0164] The predetermined pressure relief area 63 may be in a triangular, rectangular, trapezoidal, semicircular, etc. Along the thickness direction X of the first wall portion, the pressure relief component 6 has a first surface 64 and a second surface 65 opposite to each other, one of the first surface 64 and the second surface 65 being the outer surface of the pressure relief component 6, and the other being the inner surface of the pressure relief component 6. Taking the first groove 61 being provided on the first surface 64 as an example, the portion of the first surface 64 located in the predetermined pressure relief area 63 is the measurement surface of the predetermined pressure relief area 63. The area of ​​the predetermined pressure relief area 63 is the area of ​​the measurement surface of the predetermined pressure relief area 63. Taking the projection of the first groove 61, the projection of the extension line 61a of the first groove and the projection of the second groove 62 together enclosing the predetermined pressure relief area 63 as an example, the edge of the measurement surface of the predetermined pressure relief area 63 can be formed by the projection of the inner edge of the notch of the second groove 62 (the edge of the notch of the second groove 62 on the side close to the predetermined pressure relief area 63) in the first surface 64, the projection of the inner edge of the notch of the first groove 61 (the edge of the notch of the first groove 61 on the side close to the predetermined pressure relief area 63) in the first surface 64 and the projection of the extension line of the inner edge of the notch of the first groove 61 in the first surface 64, and the area of ​​the predetermined pressure relief area 63 can be obtained by measuring the measurement surface area of ​​the predetermined pressure relief area 63. Taking the first groove 61 set on the second surface 65 as an example, the part of the second surface 65 located in the predetermined pressure relief area 63 is the measurement surface of the predetermined pressure relief area 63. The area of ​​the predetermined pressure relief area 63 is the area of ​​the measurement surface of the predetermined pressure relief area 63. Taking the projection of the first groove 61, the projection of the extension line 61a of the first groove and the projection of the second groove 62 together enclosing the predetermined pressure relief area 63 as an example, the edge of the measuring surface of the predetermined pressure relief area 63 can be formed by the projection of the inner edge of the notch of the second groove 62 (the edge of the notch of the second groove 62 on the side close to the predetermined pressure relief area 63) on the second surface 65, the projection of the inner edge of the notch of the first groove 61 (the edge of the notch of the first groove 61 on the side close to the predetermined pressure relief area 63) on the second surface 65 and the projection of the extension line of the inner edge of the notch of the first groove 61 on the second surface 65. The area of ​​the predetermined pressure relief area 63 can be obtained by measuring the area of ​​the measuring surface of the predetermined pressure relief area 63. It should be noted that if the first groove 61 and the second groove 62 are both arranged on the first surface 64, the notch of the first groove 61 and the notch of the second groove 62 are both formed on the first surface 64; if the first groove 61 and the second groove 62 are both arranged on the second surface 65, the notch of the first groove 61 and the notch of the second groove 62 are both formed on the second surface 65; if the first groove 61 is arranged on the first surface 64 and the second groove 62 is arranged on the second surface 65, the notch of the first groove 61 is formed on the first surface 64, and the notch of the second groove 62 is formed on the second surface 65; if the first groove 61 is arranged on the second surface 65 and the second groove 62 is arranged on the first surface 64, the notch of the first groove 61 is formed on the second surface 65, and the notch of the second groove 62 is formed on the first surface 64.

[0165] As an example, in Figure 4-Figure 6 In the illustrated embodiment, the thickness direction X of the first wall portion is parallel to the first direction, the wall portion of the shell 11 opposite to the end cover 12 is the first wall portion 13, the first wall portion 13 serves as a pressure relief component 6, the first groove 61 and the second groove 62 are respectively arranged on two surfaces of the pressure relief component 6 opposite to each other along the thickness direction X of the first wall portion, the first groove 61 is H-shaped, the second groove 62 extends along a straight trajectory, the extension direction Y of the second groove is parallel to the second direction, the width direction Z of the second groove is parallel to the third direction, and the first direction, the second direction and the third direction are perpendicular to each other. The first direction is the height direction of the battery cell 10, the second direction is the length direction of the battery cell 10, and the third direction is the thickness direction of the battery cell 10. Figure 5 In the example, there are two predetermined pressure relief areas 63. Figure 5 The sum of the areas of the two shaded parts shown in is the sum of the areas of the two predetermined pressure relief areas 63 .

[0166] The volume of the first groove 61 is the volume of the internal space of the first groove 61. If the first groove 61 includes only one groove section, the volume of the groove section is the volume of the first groove 61; if the first groove 61 includes multiple groove sections, the sum of the volumes of the multiple groove sections is the volume of the first groove 61. Taking the first groove 61 including multiple groove sections as an example, the volume of each groove section can be measured first, and then the volume of all the groove sections can be added to calculate the volume of the first groove 61. For a single groove section, the length of the groove section can be measured first, and then the pressure relief component 6 can be cut along the extension direction perpendicular to the groove section, and the cross-sectional area of ​​the groove section can be measured on the cut surface of the pressure relief component 6 (the cut surface is as close as possible to the midpoint of the groove section in the extension direction), and then the length of the groove section and the cross-sectional area of ​​the groove section can be multiplied to calculate the volume of the groove section. Taking the cross-sectional shape of the slot segment as a rectangle as an example, the slot depth and slot width of the slot segment can be measured on the upper side of the cross-section of the pressure relief component 6, and then the slot depth and slot width of the slot segment can be multiplied to calculate the cross-sectional area of ​​the slot segment. It should be noted that if the slot segment has rounded corners or chamfers at both ends of the extension direction, the volume of the slot segment is calculated by multiplying the length of the slot segment by the cross-sectional area of ​​the slot segment as the calculated volume. The actual volume of the slot segment will be slightly smaller than the calculated volume, but the calculated volume of the slot segment can still be obtained by multiplying the length of the slot segment by the cross-sectional area of ​​the slot segment, and the calculated volume is approximately equal to the actual volume of the slot segment. In other words, when actually measuring the volume of the slot segment, the calculated volume of the slot segment obtained by calculation can be regarded as the actual volume of the slot segment.

[0167] It should be noted that in the embodiment of the present application, the sum of the areas of all the predetermined pressure relief zones 63 is A, which does not limit the number of predetermined pressure relief zones 63 to multiple. The predetermined pressure relief zones 63 may be one or multiple. If there is one predetermined pressure relief zone 63, the area of ​​the predetermined pressure relief zone 63 is the sum of the areas of all the predetermined pressure relief zones 63.

[0168] V / A can take any point value among 0.05mm, 0.06mm, 0.08mm, 0.1mm, 0.15mm, 0.2mm, 0.25mm, 0.3mm, 0.35mm, 0.38mm, 0.4mm, 0.42mm, 0.45mm, 0.46mm, 0.48mm, 0.5mm, etc., or a range value between any two of them.

[0169] In the embodiment of the present application, the pressure relief component 6 is provided with a first groove 61, so that the pressure relief component 6 can be split along at least a portion of the first groove 61 when the battery cell 10 is depressurized, so as to release the internal pressure of the battery cell 10. The pressure relief component 6 is also provided with a second groove 62. The first groove 61 and the second groove 62 jointly define at least one predetermined pressure relief area 63. The second groove 62 can guide at least a portion of the predetermined pressure relief area 63 to flip, so as to open at least a portion of the predetermined pressure relief area 63 for pressure relief. The second groove 62 plays an auxiliary role in the predetermined pressure relief area 63, making it easier to flip the predetermined pressure relief area 63, reducing the difficulty of flipping the predetermined pressure relief area 63, and increasing the opening rate of the predetermined pressure relief area 63. V / A≤0.5mm, so that when forming the first groove 61, the excess material squeezed out from the area where the first groove 61 is set in the pressure relief component 6 can be shared by the larger predetermined pressure relief area 63, reducing the amount of material piled per unit area of ​​the predetermined pressure relief area 63, so that the height of the material piled bulge formed on the surface of the predetermined pressure relief area 63 due to the material squeezed in the area where the first groove 61 is set in the pressure relief component 6 is not too large, on the one hand, the flatness of the surface of the pressure relief component 6 where the first groove 61 is set is improved, and on the other hand, the excessive height of the material piled bulge in the predetermined pressure relief area 63 during normal use of the battery cell 10 is reduced. The risk of reducing the fatigue strength of the pressure relief component 6 by releasing a large residual stress during the process increases the service life of the battery cell 10; V / A ≥ 0.05mm, so that the height of the material pile bulge formed on the surface of the predetermined pressure relief area 63 due to the squeezing of the area where the first groove 61 of the pressure relief component 6 is set is not too small, and the residual stress released by the material pile bulge helps the pressure relief component 6 to crack along the first groove 61 more timely when the battery cell 10 is in thermal runaway, thereby improving the timeliness of the pressure relief of the battery cell 10, reducing the risk of explosion of the battery cell 10, and thus improving the reliability of the battery cell 10. Therefore, 0.05mm ≤ V / A ≤ 0.5mm can not only improve the flatness of the surface where the first groove 61 of the pressure relief component 6 is set, improve the production quality of the battery cell 10, but also take into account the service life requirements of the battery cell 10 in normal use and the reliability requirements of the battery cell 10 in thermal runaway.

[0170] In some embodiments, 0.1 mm ≤ V / A ≤ 0.35 mm.

[0171] In this embodiment, V / A can take any point value among 0.1mm, 0.11mm, 0.12mm, 0.13mm, 0.14mm, 0.15mm, 0.16mm, 0.17mm, 0.18mm, 0.19mm, 0.2mm, 0.21mm, 0.22mm, 0.23mm, 0.24mm, 0.25mm, 0.26mm, 0.27mm, 0.28mm, 0.29mm, 0.3mm, 0.31mm, 0.32mm, 0.33mm, 0.34mm, 0.35mm, etc., or a range value between any two of them.

[0172] In the present embodiment, V / A≤0.35mm, which, on the one hand, further improves the flatness of the surface of the first groove 61 of the pressure relief component 6, and on the other hand, further reduces the influence of the pile protrusion of the predetermined pressure relief area 63 on the fatigue strength of the pressure relief component 6; V / A≥0.1mm, further improves the timeliness of the pressure relief of the battery cell 10, and further reduces the risk of explosion of the battery cell 10.

[0173] In some embodiments, 82 mm 3 ≤V≤450mm 3 .

[0174] In this embodiment, V can be 82 mm 3 、90mm 3 , 100mm 3 、115mm 3 , 120mm 3 , 150mm 3 、153mm 3 、180mm 3 、184mm 3 , 200mm 3 , 210mm 3 , 250mm 3 、265mm 3 、285mm 3 、300mm 3 、350mm 3 , 400mm 3 , 450mm 3 Any point value or any range between the two.

[0175] In this embodiment, V≤450mm 3 , so that the amount of material extruded during the forming of the first groove 61 is not too large, the forming force on the pressure relief component 6 during the forming of the first groove 61 is reduced, and the risk of the pressure relief component 6 being damaged during the forming of the first groove 61 is reduced; V ≥ 82 mm 3, so that the amount of extruded material when forming the first groove 61 is not too small, it is easier to meet the depth, width and length requirements of the first groove 61, and the difficulty of forming the first groove 61 is reduced.

[0176] In some embodiments, 115 mm 3 ≤V≤265mm 3 .

[0177] In this embodiment, V can be 115 mm 3 , 120mm 3 , 125mm 3 、130mm 3 、135mm 3 、140mm 3 、145mm 3 , 150mm 3 、153mm 3 、155mm 3 、160mm 3 、165mm 3 、170mm 3 、175mm 3 、180mm 3 、184mm 3 、185mm 3 、190mm 3 、195mm 3 , 200mm 3 、205mm 3 , 210mm 3 , 215mm 3 、220mm 3 , 225mm 3 、230mm 3 、235mm 3 , 240mm 3 、245mm 3 , 250mm 3 、255mm 3 , 260mm 3 、265mm 3 Any point value or any range between the two.

[0178] In this embodiment, V≤265mm 3 , further reducing the amount of material extruded when forming the first groove 61, further reducing the forming force on the pressure relief component 6 when forming the first groove 61, and reducing the risk of the pressure relief component 6 being damaged when forming the first groove 61; V≥115mm 3, further increasing the amount of extruded material when forming the first groove 61, and further reducing the difficulty of forming the first groove 61.

[0179] In some embodiments, 160 mm 2 ≤A≤1500mm 2 .

[0180] In this embodiment, A can be 160 mm 2 , 200mm 2 , 250mm 2 、300mm 2 、320mm 2 , 400mm 2 , 450mm 2 , 500mm 2 、550mm 2 、600mm 2 、650mm 2 、700mm 2 , 750mm 2 , 800mm 2 、850mm 2 、875mm 2 、890mm 2 , 900mm 2 、950mm 2 , 1000mm 2 、1050mm 2 、1100mm 2 、1150mm 2 , 1200mm 2 、1250mm 2 、1300mm 2 、1350mm 2 、1400mm 2 、1437mm 2 、1450mm 2 、1500mm 2 Any point value or any range between the two.

[0181] In this embodiment, A≤1500mm 2 , so that the area of ​​the predetermined pressure relief zone 63 is not too large, reducing the risk of the predetermined pressure relief zone 63 being deformed by the pressure change inside the battery cell 10 and causing the pressure relief component 6 to crack prematurely along the first groove 61; A≥160mm 2 , so that the pressure relief component 6 has a sufficiently large pressure relief area, thereby increasing the pressure relief rate of the battery cell 10.

[0182] In some embodiments, 400 mm 2≤A≤1200mm 2 .

[0183] In this embodiment, A can be 400 mm 2 、425mm 2 , 450mm 2 、475mm 2 , 500mm 2 、525mm 2 、550mm 2 、575mm 2 、600mm 2 、625mm 2 、650mm 2 、675mm 2 、700mm 2 、725mm 2 , 750mm 2 、775mm 2 , 800mm 2 、825mm 2 、850mm 2 、857mm 2 、875mm 2 、880mm 2 , 900mm 2 、925mm 2 、950mm 2 、975mm 2 , 1000mm 2 、1025mm 2 、1050mm 2 、1075mm 2 、1100mm 2 、1125mm 2 、1150mm 2 、1175mm 2 , 1200mm 2 Any point value or any range between the two.

[0184] In this embodiment, A≤1200mm 2 , further reducing the risk of premature cracking of the pressure relief component 6 along the first groove 61. A≥400mm 2 , further improving the pressure release rate of the battery cell 10.

[0185] In some embodiments, please refer to Figure 6 and Figure 7 , Figure 7 for Figure 6A partial enlarged view of the B in the figure. Along the thickness direction X of the first wall portion, the pressure relief component 6 has a first surface 64 and a second surface 65 opposite to each other, and the second groove 62 is recessed from the second surface 65 toward the direction close to the first surface 64. Along the width direction Z of the second groove, the second groove 62 includes a first groove side surface 621 and a second groove side surface 622 that are oppositely arranged and connected to the second surface 65, the first groove side surface 621 is closer to the predetermined pressure relief area 63 than the second groove side surface 622, the first groove side surface 621 and the second surface 65 form an angle a, and the second groove side surface 622 and the second surface 65 form an angle b, which satisfies: 90°≤a<b<180°, and the width direction Z of the second groove is perpendicular to the thickness direction X of the first wall portion.

[0186] When measuring the angle a and the angle b, the pressure relief component 6 can be cut along the direction perpendicular to the extension direction of the second groove 62, and then the angle between the first groove side surface 621 and the second surface 65 and the angle between the second groove side surface 622 and the second surface 65 can be measured on the cut surface by a measuring tool. Alternatively, the first groove side surface 621, the second groove side surface 622 and the second surface 65 can be scanned and imaged on the cut surface by a CT scanning device, and then the angle between the first groove side surface 621 and the second surface 65 and the angle between the second groove side surface 622 and the second surface 65 can be measured.

[0187] One of the first surface 64 and the second surface 65 may be the outer surface of the pressure relief component 6, and the other may be the inner surface of the pressure relief component 6. The outer surface of the pressure relief component 6 faces the outside of the battery cell 10, and the inner surface of the pressure relief component 6 faces the inside of the battery cell 10. The first surface 64 and the second surface 65 may be planes. The first surface 64 and the second surface 65 may be arranged in parallel or at a non-zero angle. The second groove 62 is recessed from the second surface 65 toward the direction close to the first surface 64, that is, the second groove 62 is arranged on the second surface 65. In this case, the first groove 61 can be arranged on the second surface 65 or on the first surface 64. As an example, in Figure 7 In the illustrated embodiment, the first surface 64 is the outer surface of the pressure relief component 6 , the first groove 61 is disposed on the first surface 64 , and the second groove 62 is disposed on the second surface 65 .

[0188] The first groove side surface 621 can be a plane or an arc surface. If the first groove side surface 621 is an arc surface, the angle between the line connecting the two ends of the first groove side surface 621 along the depth direction of the second groove 62 and the second surface 65 is the angle a between the first groove side surface 621 and the second surface 65. The second groove side surface 622 can be a plane or an arc surface. If the second groove side surface 622 is an arc surface, the angle between the line connecting the two ends of the second groove side surface 622 along the depth direction of the second groove 62 and the second surface 65 is the angle b between the second groove side surface 622 and the second surface 65. The first groove side surface 621 and the second surface 65 can be directly connected or indirectly connected, for example, the first groove side surface 621 and the second surface 65 smoothly transition through an arc surface; the second groove side surface 622 and the second surface 65 can be directly connected or indirectly connected, for example, the second groove side surface 622 and the second surface 65 smoothly transition through an arc surface. As an example, in Figure 7 In the illustrated embodiment, the second surface 65 , the first groove side surface 621 , and the second groove side surface 622 are all planes.

[0189] The first groove side surface 621 and the second surface 65 may be arranged at an obtuse angle or a right angle, and the second groove side surface 622 and the second surface 65 may be arranged at an obtuse angle. As an example, ba≥3°.

[0190] The second groove 62 may further include a groove bottom surface, the groove bottom surface 625 of the second groove connects the first groove side surface 621 and the second groove side surface 622, the groove bottom surface 625 of the second groove may be a plane, or the groove bottom surface 625 of the second groove may be an arc surface. As an example, the width of the second groove 62 gradually decreases along the depth direction of the second groove 62, and the groove bottom surface 625 of the second groove is a plane parallel to the second surface 65.

[0191] In this embodiment, a<b, is equivalent to reducing the angle between the first groove side 621 and the second surface 65, which can reduce the amount of piled material in the predetermined pressure relief area 63 of the excess material squeezed out when forming the second groove 62, and reduce the height of the piled material protrusion formed on the surface of the predetermined pressure relief area 63 due to the squeezing of material in the area where the second groove 62 is set in the pressure relief component 6, thereby improving the flatness of the surface of the predetermined pressure relief area 63, reducing the influence of the piled material protrusion on the predetermined pressure relief area 63, and reducing the risk of the predetermined pressure relief area 63 opening prematurely due to the uneven surface of the predetermined pressure relief area 63.

[0192] In some embodiments, 90°≤a≤150°.

[0193] In this embodiment, a can be any point value among 90°, 100°, 110°, 120°, 130°, 135°, 140°, 150°, etc., or a range value between any two of them.

[0194] In this embodiment, 90°≤a≤150°, which further reduces the angle between the first groove side 621 and the second surface 65, and further reduces the inclination angle of the first groove side 621, which is beneficial to reducing the amount of excess material extruded in the predetermined pressure relief area when forming the second groove 62.

[0195] In some embodiments, 90°<b≤170°.

[0196] In this embodiment, b can be any point value among 91°, 95°, 100°, 105°, 110°, 115°, 120°, 125°, 130°, 135°, 140°, 145°, 150°, 155°, 160°, 165°, 170°, etc., or a range value between any two of them.

[0197] In this embodiment, 90°<b<170°, which further reduces the angle between the second groove side surface 622 and the second surface 65 , further reduces the inclination angle of the second groove side surface 622 , and reduces the difficulty of forming the second groove 62 .

[0198] In some embodiments, please refer to Figure 5 The pressure relief component 6 is provided with a plurality of second grooves 62 . Along the thickness direction X of the first wall portion, the projection of the first groove 61 and the projection of the plurality of second grooves 62 jointly define a plurality of predetermined pressure relief areas 63 . Each predetermined pressure relief area 63 is provided corresponding to one or more second grooves 62 .

[0199] Along the thickness direction X of the first wall portion, the projection of the first groove 61 and the projection of the plurality of second grooves 62 together define two, three, four, five or more predetermined pressure relief areas 63. Each predetermined pressure relief area 63 may be arranged corresponding to at least one second groove 62, that is, each predetermined pressure relief area 63 may be arranged corresponding to one second groove 62, or may be arranged corresponding to a plurality of second grooves 62.

[0200] As an example, in Figure 5 In the illustrated embodiment, the predetermined pressure relief areas 63 correspond one to one with the second grooves 62 , and along the thickness direction X of the first wall portion, the projection of the first groove 61 and the projections of the two second grooves 62 jointly define two predetermined pressure relief areas 63 , and the two predetermined pressure relief areas 63 are symmetrically arranged.

[0201] In this embodiment, the first groove 61 and the plurality of second grooves 62 jointly define a plurality of predetermined pressure relief areas 63. When the battery cell 10 thermally runs away, the plurality of predetermined pressure relief areas 63 can all be opened. When the total pressure relief area of ​​the pressure relief component 6 is constant, the opening rate of the predetermined pressure relief areas 63 can be increased, thereby achieving faster pressure relief.

[0202] In some embodiments, please refer to Figure 5-Figure 7 , along the thickness direction X of the first wall portion, the projection of the second groove 62 does not overlap with the projection of the first groove 61 .

[0203] It can be understood that, along the thickness direction X of the first wall portion, the projection of the second groove 62 has no overlapping portion with the projection of the first groove 61 .

[0204] Along the thickness direction X of the first wall portion, the projection of the extension line 62a of the second groove may be connected to the projection of the first groove 61, or the projection of the extension line 61a of the first groove may be connected to the projection of the second groove 62, or the projection of the extension line 61a of the first groove may be connected to the projection of the extension line 62a of the second groove.

[0205] The second groove 62 and the first groove 61 can be arranged on the same side of the pressure relief component 6 in the thickness direction X of the first wall portion, for example, the second groove 62 and the first groove 61 are both arranged on the first surface 64, and for another example, the second groove 62 and the first groove 61 are both arranged on the second surface 65; the second groove 62 and the first groove 61 can also be arranged on different sides of the pressure relief component 6 in the thickness direction X of the first wall portion, for example, the first groove 61 is arranged on the first surface 64, and the second groove 62 is arranged on the second surface 65.

[0206] In this embodiment, the projection of the second groove 62 along the thickness direction X of the first wall portion does not overlap with the projection of the first groove 61 along the thickness direction X of the first wall portion, which can reduce the mutual influence between the first groove 61 and the second groove 62 during the processing process and reduce the risk of the first groove 61 and the second groove 62 being connected to each other during the processing.

[0207] In some embodiments, please refer to Figure 5-Figure 7 , along the width direction Z of the second groove, the second groove 62 is spaced apart from the first groove 61, and the width direction Z of the second groove is perpendicular to the thickness direction X of the first wall portion.

[0208] The second groove 62 and the first groove 61 are spaced apart in the width direction Z of the second groove, that is, the projection of the second groove 62 in the thickness direction X of the first wall portion and the projection of the first groove 61 in the thickness direction X of the first wall portion are spaced apart in the width direction Z of the second groove. In this embodiment, the second groove 62 and the first groove 61 can be located on the same side of the pressure relief component 6 in the thickness direction X of the first wall portion, or can be located on two opposite sides of the pressure relief component 6 in the thickness direction X of the first wall portion. It can be understood that the projection of the second groove 62 in the thickness direction X of the first wall portion and the projection of the first groove 61 in the thickness direction X of the first wall portion are spaced apart in the width direction Z of the second groove.

[0209] As an example, in Figure 6In the illustrated embodiment, the housing 1 includes a first wall portion 13, a second wall portion 14 and a third wall portion 15. Along the width direction Z of the second groove, the second wall portion 14 and the third wall portion 15 are arranged opposite to each other. The first wall portion 13 connects the second wall portion 14 and the third wall portion 15. The first wall portion 13 is a pressure relief component 6. The first wall portion 13 is provided with two second grooves 62. Along the width direction Z of the second groove, one second groove 62 is located between the first groove 61 and the second wall portion 14, and the other second groove 62 is located between the first groove 61 and the third wall portion 15.

[0210] In this embodiment, the second groove 62 and the first groove 61 are spaced apart in the width direction Z of the second groove, so that the projection of the second groove 62 along the thickness direction X of the first wall portion and the projection of the first groove 61 along the thickness direction X of the first wall portion do not overlap. On the one hand, the mutual influence between the first groove 61 and the second groove 62 during the processing can be reduced. On the other hand, the residual stress influence between the pressure relief component 6 in the area where the first groove 61 is set and the area where the second groove 62 is set can be reduced, and the risk of cracks generated by the pressure relief component 6 cracking along the first groove 61 spreading to the second groove 62, thereby causing the pressure relief component 6 to crack along the second groove 62, can be reduced.

[0211] In some embodiments, please refer to Figure 5 Along the thickness direction X of the first wall portion, two ends of the projection of the second groove 62 along the extension direction respectively extend out of two ends of the projection of the first groove 61 .

[0212] Along the thickness direction X of the first wall portion, the projection of the second groove 62 has two opposite ends in the extension direction, namely, a first end 623 and a second end 624. The two ends of the projection of the second groove 62 along the extension direction extend out of the two ends of the projection of the first groove 61, that is, the two ends of the projection of the first groove 61 are located between the first end 623 and the second end 624 along the extension direction of the projection of the second groove 62. The extension direction of the projection of the second groove 62 along the thickness direction X of the first wall portion is parallel to the extension direction Y of the second groove. Along the extension direction Y of the second groove, the length of the second groove 62 is greater than the length of the first groove 61 (the maximum span of the first groove 61 along the extension direction Y of the second groove).

[0213] In the present embodiment, the two ends of the projection of the second groove 62 along the thickness direction X of the first wall portion along the extension direction respectively extend out of the two ends of the projection of the first groove 61 along the thickness direction X of the first wall portion, so that the second groove 62 is longer, and the auxiliary flipping effect of the second groove 62 on the predetermined pressure relief area 63 is enhanced. In addition, this structure can also improve the separation effect of the second groove 62 on the surface of the battery cell 10 in the width direction Z of the second groove (the outer surface of the second wall portion 14 or the outer surface of the third wall portion 15) and the first groove 61, improve the absorption effect of the second groove 62 on the excess material extruded during the molding of the first groove 61, improve the flatness of the surface of the battery cell 10 in the width direction Z of the second groove, and can improve the blocking effect of the second groove 62 on the deformation energy of the battery cell 10 when the battery cell 10 is subjected to internal and external impact forces, thereby reducing the influence of the expansion of the battery cell 10 on the pressure relief component 6.

[0214] In some embodiments, please refer to Figure 7 , the minimum residual thickness of the first groove 61 is D1, and the minimum residual thickness of the second groove 62 is D2, satisfying: D1<D2.

[0215] The minimum residual thickness of the first groove 61 is the minimum thickness of the residual part after the pressure relief component 6 is provided with the first groove 61, and the residual part may be the groove bottom wall of the first groove 61. The thickness of the groove bottom wall of the first groove 61 may be uniform or uneven. If the thickness of the groove bottom wall of the first groove 61 is uneven, the thickness of the thinnest position of the groove bottom wall of the first groove 61 is the minimum residual thickness of the first groove 61. In the embodiment where the first groove 61 includes a plurality of groove sections, the minimum residual thickness of all groove sections may be equal, and the minimum residual thickness of any groove section is the minimum residual thickness of the first groove 61; if the minimum residual thickness of at least two groove sections is not equal, the minimum residual thickness of the groove section with the smallest minimum residual thickness is the minimum residual thickness of the first groove 61. Among them, the minimum residual thickness of a groove section is the minimum thickness of the residual part after the pressure relief component 6 is provided with the groove section, and the residual part may be the groove bottom wall of the groove section.

[0216] The minimum residual thickness of the second groove 62 is the minimum thickness of the residual portion of the pressure relief component 6 after the second groove 62 is provided, and the residual portion may be the groove bottom wall of the second groove 62. The thickness of the groove bottom wall of the second groove 62 may be uniform or non-uniform. If the thickness of the groove bottom wall of the second groove 62 is non-uniform, the thickness of the thinnest position of the groove bottom wall of the second groove 62 is the minimum residual thickness of the second groove 62.

[0217] In this embodiment, D1<D2 makes the strength of the area where the first groove 61 of the pressure relief component 6 is set smaller than the strength of the area where the second groove 62 of the pressure relief component 6 is set, so that the pressure relief component 6 can preferentially break along the first groove 61 to achieve rapid opening of the predetermined pressure relief area 63.

[0218] In some embodiments, please refer to Figure 7 Along the thickness direction X of the first wall portion, the maximum groove depth of the first groove 61 is H1, and the maximum groove depth of the second groove 62 is H2, satisfying: H2

[0219] The maximum distance between the notch of the first groove 61 and the groove bottom surface 614 of the first groove along the thickness direction X of the first wall portion is the maximum groove depth of the first groove 61; the maximum distance between the notch of the second groove 62 and the groove bottom surface 625 of the second groove along the thickness direction X of the first wall portion is the maximum groove depth of the second groove 62.

[0220] As an example, the first surface 64 is parallel to the second surface 65 , the distance between the first surface 64 and the second surface 65 is D, the thickness of the pressure relief component 6 is D, and D= D1 + H1 = D2 + H2 .

[0221] In this embodiment, H2

[0222] In some embodiments, along the thickness direction X of the first wall portion, the maximum groove depth of the first groove 61 is H1, the thickness of the pressure relief component 6 is D, and 0.16≤H1 / D<1.

[0223] H1 / D can take any point value among 0.16, 0.18, 0.2, 0.22, 0.25, 0.28, 0.3, 0.32, 0.35, 0.38, 0.4, 0.42, 0.45, 0.48, 0.5, 0.62, 0.65, 0.68, 0.7, 0.72, 0.75, 0.78, 0.8, 0.82, 0.85, 0.88, 0.9, 0.92, 0.95, 0.98, 0.99, etc., or a range of values ​​between any two of them.

[0224] It is understandable that if the pressure relief component 6 and the first wall portion 13 are formed integrally, the first wall portion 13 can serve as the pressure relief component 6 , and the thickness of the pressure relief component 6 is the thickness of the first wall portion 13 .

[0225] ​​In this embodiment, 0.16≤H1 / D<1, so that the maximum depth of the first groove 61 accounts for a small proportion of the thickness of the pressure relief component 6, and the bursting pressure of the battery cell 10 is not too high, which is beneficial to improving the timeliness of the pressure relief of the battery cell 10.

[0226] In some embodiments, 0.4 mm ≤ H1 ≤ 2 mm, 0.8 mm ≤ D ≤ 2.5 mm.

[0227] H1 can be any point value among 0.4mm, 0.45mm, 0.5mm, 0.55mm, 0.6mm, 0.65mm, 0.7mm, 0.75mm, 0.8mm, 0.85mm, 0.9mm, 0.95mm, 1mm, 1.05mm, 1.1mm, 1.15mm, 1.2mm, 1.25mm, 1.3mm, 1.35mm, 1.4mm, 1.45mm, 1.5mm, 1.55mm, 1.6mm, 1.65mm, 1.7mm, 1.75mm, 1.8mm, 1.85mm, 1.9mm, 1.95mm, 2mm, etc., or any range value between any two of them.

[0228] D can be any point value among 0.8mm, 0.85mm, 0.9mm, 0.95mm, 1mm, 1.05mm, 1.1mm, 1.15mm, 1.2mm, 1.25mm, 1.3mm, 1.35mm, 1.4mm, 1.45mm, 1.5mm, 1.55mm, 1.6mm, 1.65mm, 1.7mm, 1.75mm, 1.8mm, 1.85mm, 1.9mm, 1.95mm, 2mm, 2.05mm, 2.1mm, 2.15mm, 2.2mm, 2.25mm, 2.3mm, 2.35mm, 2.4mm, 2.45mm, 2.5mm, etc., or a range value between any two of them.

[0229] In this embodiment, 0.4mm≤H1≤2mm, 0.8mm≤D≤2.5mm, so that the maximum depth of the first groove and the thickness of the pressure relief component 6 are within a reasonable range, which has better economy. In the embodiment where the first wall portion 13 is used as the pressure relief component 6, the thickness of the first wall portion 13 is 0.8mm~2.5mm, and the thickness of the first wall portion 13 is greater than or equal to 0.8mm, so that the first wall portion 13 has sufficient strength, and the thickness of the first wall portion 13 is less than or equal to 2mm, so that the thickness of the first wall portion 13 is not too thick. Under the condition that the volume of the shell 1 is constant, the internal space of the shell 1 can be increased to make more space for the electrode assembly 2. When the thickness of the first wall portion 13 is controlled within the range of 0.8mm~2.5mm, the maximum groove depth of the first groove 61 is controlled within the range of 0.4mm~2mm, so that the maximum groove depth of the first groove 61 is more matched with the thickness of the pressure relief component 6, so that the pressure relief component 6 has good pressure relief ability.

[0230] In some embodiments, along the thickness direction X of the first wall portion, the pressure relief component 6 has a first surface 64 and a second surface 65 opposite to each other, the first groove 61 is disposed on the first surface 64 , and the second groove 62 is disposed on the second surface 65 .

[0231] The first surface 64 and the second surface 65 are two surfaces of the pressure relief component 6 that are opposite to each other along the thickness direction X of the first wall portion. The first groove 61 is arranged on the first surface 64, that is, the first groove 61 is recessed from the first surface 64 to the direction close to the second surface 65; the second groove 62 is arranged on the second surface 65, that is, the second groove 62 is recessed from the second surface 65 to the direction close to the first surface 64. One of the first surface 64 and the second surface 65 may be the outer surface of the pressure relief component 6, and the other is the inner surface of the pressure relief component 6. The outer surface of the pressure relief component 6 faces the outside of the battery cell 10, and the inner surface of the pressure relief component 6 faces the inside of the battery cell 10. The first surface 64 and the second surface 65 may be planes, and the first surface 64 and the second surface 65 may be arranged in parallel or at a non-zero angle. As an example, in Figure 7 In the illustrated embodiment, the first surface 64 is parallel to the second surface 65 .

[0232] As an example, the minimum distance between the groove bottom surface 614 of the first groove and the second surface 65 along the thickness direction X of the first wall portion is equal to the minimum residual thickness of the first groove 61, and the minimum distance between the groove bottom surface 625 of the second groove and the first surface 64 along the thickness direction X of the first wall portion is equal to the minimum residual thickness of the second groove 62. The maximum groove depth of the first groove 61 is equal to the maximum distance between the first surface 64 and the groove bottom surface 614 of the first groove along the thickness direction X of the first wall portion, and the maximum groove depth of the second groove 62 is equal to the maximum distance between the second surface 65 and the groove bottom surface 625 of the second groove along the thickness direction X of the first wall portion.

[0233] In this embodiment, the first groove 61 and the second groove 62 are respectively arranged on the first surface 64 and the second surface 65, and the first groove 61 and the second groove 62 are respectively located on both sides of the pressure relief component 6 along the thickness direction X of the first wall portion, so that the first groove 61 and the second groove 62 can be processed on both sides of the pressure relief component 6, which is beneficial to reduce the mutual influence of the first groove 61 and the second groove 62 during the processing.

[0234] In some embodiments, please refer to Figure 7 Along the width direction Z of the second groove, the projection of the first groove 61 and the projection of the second groove 62 at least partially overlap, and the width direction Z of the second groove is perpendicular to the thickness direction X of the first wall portion.

[0235] The projection of the first groove 61 along the width direction Z of the second groove and the projection of the second groove 62 along the width direction Z of the second groove may partially overlap or completely overlap. If the two completely overlap, a first protrusion may be provided at a position corresponding to the first surface 64 and the second groove 62, so that the second groove 62 does not penetrate the pressure relief component 6 along the thickness direction X of the first wall, and a second protrusion may be provided at a position corresponding to the second surface 65 and the first groove 61, so that the first groove 61 does not penetrate the pressure relief component 6 along the thickness direction X of the first wall.

[0236] It can be understood that the projections of the first groove 61 and the second groove 62 along the width direction Z of the second groove have an overlapping area. It can also be understood that the projections of the groove wall surface (groove bottom surface and groove side surface) of the first groove 61 and the groove wall surface (groove bottom surface and groove side surface) of the second groove 62 in the width direction Z of the second groove at least partially overlap.

[0237] It should be noted that if the groove bottom surface 614 of the first groove and the groove bottom surface 625 of the second groove are exactly flush, the projections of the groove bottom surface 614 of the first groove and the groove bottom surface 625 of the second groove along the width direction Z of the second groove overlap, and the overlapping area is a line. In this case, the projection of the first groove 61 and the projection of the second groove 62 also partially overlap.

[0238] In this embodiment, the projections of the first groove 61 and the second groove 62 along the width direction Z of the second groove at least partially overlap, so that the projections of the first groove 61 and the second groove 62 in the width direction Z of the second groove have overlapping areas, thereby, on the one hand, improving the absorption effect of the second groove 62 on the residual material squeezed out of the first groove 61 during molding, and reducing the risk of the extruded residual material of the first groove 61 diffusing to the surface close to the shell 1 along the width direction Z of the second groove, thereby causing the surface to be uneven; on the other hand, improving the absorption effect of the second groove 62 on the deformation energy of the battery cell 10 when the battery cell 10 is subjected to internal and external forces and deformed along the width direction Z of the second groove, and reducing the influence of the expansion deformation of the battery cell 10 along the width direction Z of the second groove on the pressure relief component 6.

[0239] In some embodiments, please refer to Figure 7 Along the thickness direction X of the first wall portion, the groove bottom surface 625 of the second groove is closer to the first surface 64 than the groove bottom surface 614 of the first groove.

[0240] It can be understood that, along the thickness direction X of the first wall portion, the minimum distance between the groove bottom surface 625 of the second groove and the first surface 64 is smaller than the minimum distance between the groove bottom surface 614 of the first groove and the first surface 64 .

[0241] The bottom surface 614 of the first groove can be a plane or a curved surface; the bottom surface 625 of the second groove can be a plane or a curved surface. Figure 7 In the illustrated embodiment, the groove bottom surface 614 of the first groove and the groove bottom surface 625 of the second groove are both planes and are parallel to the first surface 64 and the second surface 65 .

[0242] In this embodiment, the groove bottom surface 625 of the second groove is closer to the first surface 64 than the groove bottom surface 614 of the first groove. This structure is conducive to achieving that the projections of the second groove 62 and the first groove 61 in the width direction Z of the second groove have more overlapping areas, further improving the absorption effect of the second groove 62 on the residual material squeezed out of the first groove 61 during molding, and further improving the absorption effect of the second groove 62 on the deformation energy of the battery cell 10 when the battery cell 10 is subjected to internal and external forces and deformed along the width direction Z of the second groove.

[0243] In some embodiments, along the thickness direction X of the first wall portion, the maximum groove depth of the second groove 62 is H2, and the minimum residual thickness of the first groove 61 is D1, satisfying: D1<H2.

[0244] As an example, the first surface 64 is parallel to the second surface 65, the notch of the second groove 62 is located on the second surface 65, and along the thickness direction X of the first wall portion, the portion between the groove bottom surface 614 of the first groove and the second surface 65 is the residual portion of the first groove 61, the minimum thickness of the residual portion is the minimum residual thickness of the first groove 61, and the maximum distance between the groove bottom surface 625 of the second groove and the second surface 65 is the maximum groove depth of the second groove 62. The second surface 65 is a measurement reference surface for the maximum groove depth of the second groove 62 and the minimum residual thickness of the first groove 61.

[0245] In the present embodiment, D1<H2. This structure is conducive to achieving more overlapping areas between the projections of the second groove 62 and the first groove 61 in the width direction Z of the second groove, further improving the absorption effect of the second groove 62 on the residual material squeezed out of the first groove 61 during molding, and further improving the absorption effect of the second groove 62 on the deformation energy of the battery cell 10 when the battery cell 10 is subjected to internal and external forces and deformed along the width direction Z of the second groove.

[0246] In some embodiments, please refer to Figure 8-Figure 11 As shown, Figure 8 Assembly diagrams of battery cells 10 provided for other embodiments of the present application; Fig. 9 for Figure 8 A partial view of the housing 1 is shown; Fig.10 for Fig. 9 The CC cross-sectional view of the housing 1 is shown; Fig.11 for Fig.10 The first groove 61 includes a multi-stage groove arranged in sequence along the direction from the first surface 64 to the second surface 65. Along the thickness direction X of the first wall portion, in two adjacent stages of grooves, the first stage groove away from the first surface 64 is arranged on the groove bottom surface of the first stage groove close to the first surface 64. Among them, the first stage groove arranged on the first surface 64 in the multi-stage groove is the first stage groove 615. Along the width direction Z of the second groove, the projection of the second groove 62 at least partially overlaps with the projection of the first stage groove 615. The width direction Z of the second groove is perpendicular to the thickness direction X of the first wall portion.

[0247] The first groove 61 can be a two-stage groove, a three-stage groove, a four-stage groove, a five-stage groove, etc. It can be understood that the first groove 61 is a stepped groove. Along the direction from the first surface 64 to the second surface 65, the groove width of each stage of the groove gradually decreases. The volume of the first groove 61 is equal to the sum of the volumes of the grooves at each stage. Fig.11 As shown, taking the first groove 61 as a two-level groove as an example, the two-level grooves are respectively a first-level groove 615 and a second-level groove. During processing, a first-level groove 615 with a larger width can be processed on the first surface 64 first, and then a second-level groove with a smaller width can be processed on the bottom surface of the first-level groove 615.

[0248] The first-level groove 615 is a first-level groove disposed on the first surface 64 in the first groove 61. In the embodiment where the first groove 61 includes a plurality of groove sections, it can be understood that each groove section is a multi-level groove, and the first-level grooves of all groove sections disposed on the first surface 64 constitute the first-level groove 615. In the multi-level grooves of the first groove 61, the groove bottom surface of the first-level groove farthest from the first surface 64 is the groove bottom surface 614 of the first groove, the minimum residual thickness of the first-level groove farthest from the first surface 64 is the minimum residual thickness of the first groove 61, and the maximum distance between the groove bottom surface of the first-level groove farthest from the first surface 64 and the first surface 64 is equal to the maximum groove depth of the first groove 61. When calculating the volume of the first groove 61, the volume of each groove section can be calculated first. Since each groove section is a multi-level groove structure, when calculating the volume of each groove section, the volume of each level groove in each groove section can be calculated separately. For each level of groove in each groove section, the length and cross-sectional area of ​​each level of groove in each groove section can be measured first, and the length and the cross-sectional area can be multiplied to calculate the volume of each level of groove in each groove section. Taking the cross-sectional area of ​​the first-level groove in the groove section as a rectangle as an example, the pressure relief component 6 can be cut along the direction perpendicular to the extension of the groove section, and the groove depth and groove width of the first-level groove in the groove section can be measured on the upper side of the cut surface of the pressure relief component 6 (the cut surface is as close as possible to the midpoint position of the groove section in the extension direction), and then the groove depth and groove width can be multiplied to calculate the cross-sectional area of ​​the first-level groove in the groove section. It should be noted that if the first-level groove in the groove section has rounded corners or chamfers at both ends in the extension direction, the calculated volume calculated by multiplying the length of the first-level groove and the cross-sectional area can be regarded as the actual volume of the first-level groove.

[0249] The projection of the second groove 62 along the width direction Z of the second groove may partially overlap or completely overlap with the projection of the first-stage groove 615 along the width direction Z of the second groove. If the two completely overlap, a first protrusion may be provided at a position corresponding to the second groove 62 on the first surface 64, so that the second groove 62 does not penetrate the pressure relief component 6 along the thickness direction X of the first wall, and a second protrusion may be provided at a position corresponding to the first-stage groove 615 on the second surface 65, so that the first groove 61 does not penetrate the pressure relief component 6 along the thickness direction X of the first wall.

[0250] It can be understood that the projections of the second groove 62 and the first-stage groove 615 along the width direction Z of the second groove have an overlapping area. It can also be understood that the projections of the groove wall surface (groove bottom surface and groove side surface) of the second groove 62 and the groove wall surface (groove bottom surface and groove side surface) of the first-stage groove 615 in the width direction Z of the second groove at least partially overlap.

[0251] In this embodiment, by setting the first groove 61 as a multi-level groove arranged along the thickness direction X of the first wall portion, when forming the first groove 61, each level of groove can be processed one by one along the direction from the first surface 64 to the second surface 65, thereby reducing the forming depth of each level of groove, reducing the forming force exerted on the pressure relief component 6 when forming the first groove 61, and reducing the risk of the pressure relief component 6 being damaged when forming the first groove 61. Since the projection of the first-stage groove 615 of the first groove 61 along the width direction Z of the second groove at least partially overlaps with the projection of the second groove 62 along the width direction Z of the second groove, the projection of the second groove 62 in the width direction can not only cover a part of the first groove 61, but also cover the grooves of other stages in the first groove 61 except the first-stage groove 615. Therefore, on the one hand, the absorption effect of the second groove 62 on the residual material squeezed out of the first groove 61 during the multi-stage groove forming process can be further improved. On the other hand, the absorption effect of the second groove 62 on the deformation energy of the battery cell 10 when the battery cell 10 is subjected to internal and external impact forces and deformed can be further improved, thereby reducing the influence of the expansion deformation of the battery cell 10 along the width direction Z of the second groove on the pressure relief component 6.

[0252] In some embodiments, please refer to Fig.11 Along the thickness direction X of the first wall portion, the groove bottom surface 625 of the second groove is closer to the first surface 64 than the groove bottom surface of the first-level groove 615 .

[0253] It can be understood that, along the thickness direction X of the first wall portion, the minimum distance between the groove bottom surface 625 of the second groove and the first surface 64 is smaller than the minimum distance between the groove bottom surface of the first-level groove 615 and the first surface 64 .

[0254] The bottom surface 625 of the second groove can be a plane or a curved surface; the bottom surface of the first-stage groove 615 can be a plane or a curved surface. Fig.11 In the illustrated embodiment, the groove bottom surface of the first-stage groove 615 and the groove bottom surface 625 of the second groove are both planes and are parallel to the first surface 64 and the second surface 65 .

[0255] In this embodiment, the projection of the second groove 62 in the width direction can cover the other levels of grooves in the first groove 61 except the first-level groove 615, and can cover more parts of the first-level groove 615. On the one hand, it can improve the absorption effect of the second groove 62 on the excess material squeezed out of the first groove 61 when the multi-level groove is formed. On the other hand, it can improve the absorption effect of the second groove 62 on the deformation energy of the battery cell 10 when the battery cell 10 is subjected to internal and external impact forces and deformed, thereby reducing the influence of the expansion deformation of the battery cell 10 along the width direction Z of the second groove on the pressure relief component 6.

[0256] In some other embodiments, along the thickness direction X of the first wall portion, the groove bottom surface 625 of the second groove is flush with the groove bottom surface of the first-stage groove 615 .

[0257] As an example, the groove bottom surface 625 of the second groove and the groove bottom surface of the first-level groove 615 are both flat and coplanar.

[0258] In this embodiment, the projection of the second groove 62 in the width direction can cover the other levels of grooves in the first groove 61 except the first-level groove 615. On the one hand, it can improve the absorption effect of the second groove 62 on the excess material squeezed out of the first groove 61 during the processing of multi-level groove forming. On the other hand, it can further improve the absorption effect of the second groove 62 on the deformation energy of the battery cell 10 when the battery cell 10 is subjected to internal and external impact forces and deformed, thereby reducing the influence of the expansion deformation of the battery cell 10 along the width direction Z of the second groove on the pressure relief component 6.

[0259] In some embodiments, please refer to Fig.12 and Fig.13 , Fig.12 A partial cross-sectional view of a housing 1 provided in some embodiments of the present application; Fig.13 for Fig.12 The partial enlarged view at E. Along the thickness direction X of the first wall portion, the pressure relief component 6 has a first surface 64 and a second surface 65 opposite to each other, and the first groove 61 and the second groove 62 are both recessed from the second surface 65 to the first surface 64 .

[0260] It can be understood that the first groove 61 and the second groove 62 are both arranged on the second surface 65. The second surface 65 can be the outer surface of the external component, or can be the inner surface of the external component.

[0261] In this embodiment, the first groove 61 and the second groove 62 are arranged on the same side of the pressure relief component 6 in the thickness direction X of the first wall portion, which makes it easier to process the first groove 61 and the second groove 62 on the pressure relief component 6. The first groove 61 and the second groove 62 can be processed without flipping the pressure relief component 6, which is beneficial to optimizing the production rhythm of the battery cell 10.

[0262] In some embodiments, please refer to Fig.13 The first groove 61 includes a plurality of grooves sequentially arranged along the direction from the second surface 65 to the first surface 64. Along the thickness direction X of the first wall portion, in two adjacent grooves, the first groove far from the second surface 65 is arranged at the groove bottom surface of the first groove close to the second surface 65. Among them, the first groove arranged on the second surface 65 of the multi-stage groove is the first groove 615. Along the thickness direction X of the first wall portion, the groove bottom surface of the first groove 615 is closer to the second surface 65 than the groove bottom surface 625 of the second groove.

[0263] The first-level groove 615 is a first-level groove disposed on the second surface 65 in the first groove 61. Among the multi-level grooves of the first groove 61, the groove bottom surface of the first-level groove farthest from the second surface 65 is the groove bottom surface 614 of the first groove, the minimum residual thickness of the first-level groove farthest from the second surface 65 is the minimum residual thickness of the first groove 61, and the maximum distance between the groove bottom surface of the first-level groove farthest from the second surface 65 and the second surface 65 is equal to the maximum groove depth of the first groove 61. Along the thickness direction X of the first wall portion, the minimum distance between the groove bottom surface 625 of the second groove and the first surface 64 is equal to the minimum residual thickness of the second groove 62, and the minimum distance between the groove bottom surface of the first-level groove farthest from the second surface 65 and the first surface 64 is equal to the minimum residual thickness of the first groove 61.

[0264] It can be understood that, along the thickness direction X of the first wall portion, the minimum distance between the groove bottom surface of the first-level groove 615 and the second surface 65 is smaller than the minimum distance between the groove bottom surface 625 of the second groove and the second surface 65 .

[0265] The bottom surface 625 of the second groove can be a plane or a curved surface; the bottom surface of the first-stage groove 615 can be a plane or a curved surface. Fig.13 In the illustrated embodiment, the groove bottom surface of the first-stage groove 615 and the groove bottom surface 625 of the second groove are both planes and are parallel to the first surface 64 and the second surface 65 .

[0266] In this embodiment, by arranging the first groove 61 with multiple grooves along the thickness direction X of the first wall, when forming the first groove 61, each groove can be processed one by one along the direction from the second surface 65 to the first surface 64, thereby reducing the forming depth of each groove, reducing the forming force to which the pressure relief component 6 is subjected when forming the first groove 61, and reducing the risk of the pressure relief component 6 being damaged when forming the first groove 61. Since the groove bottom surface of the first groove 615 is closer to the second surface 65 than the groove bottom surface 625 of the second groove, the projection of the second groove 62 along the width direction at least covers the first groove 615 of the first groove 61, so that the second groove 62 has a deeper depth, so that the second groove 62 can have a good absorption effect on the residual material squeezed out when forming the first groove 615, and the second groove 62 can have a good absorption effect on the deformation energy of the battery cell 10 when the battery cell 10 is subjected to internal and external impact forces and deformed.

[0267] In some embodiments, please refer to Fig.13 Along the thickness direction X of the first wall portion, the maximum groove depth of the second groove 62 is H2, and the maximum groove depth of the first-level groove 615 is H3, satisfying: H3<H2.

[0268] As an example, the maximum distance between the groove bottom surface 625 of the second groove and the second surface 65 along the thickness direction X of the first wall portion is the maximum groove depth of the second groove 62, and the maximum distance between the groove bottom surface of the first-level groove 615 and the second surface 65 along the thickness direction X of the first wall portion is the maximum groove depth of the first-level groove 615. The maximum groove depth of the second groove 62 is greater than the maximum groove depth of the first-level groove 615, so that the groove bottom surface of the first-level groove 615 is closer to the second surface 65 than the groove bottom surface 625 of the second groove.

[0269] In this embodiment, H3<H2, so that the second groove 62 has a deeper depth, so that the second groove 62 can have a good absorption effect on the residual material squeezed out when the first-level groove 615 is formed, and the second groove 62 can have a good absorption effect on the deformation energy of the battery cell 10 when the battery cell 10 is subjected to internal and external impact forces and deformed.

[0270] In some embodiments, please refer to Figure 6 , Figure 7 and Figure 10-13 The first surface 64 is the surface of the pressure relief component 6 facing the outside of the battery cell 10 , and the second surface 65 is the surface of the pressure relief component 6 facing the inside of the battery cell 10 .

[0271] The first surface 64 is the outer surface of the pressure relief component 6 , and the second surface 65 is the inner surface of the pressure relief component 6 .

[0272] The first surface 64 is the surface of the pressure relief component 6 facing the outside of the battery cell 10. When the first groove 61 is set on the first surface 64, the first groove 61 is set on the outside of the pressure relief component 6, which is convenient for processing and forming the first groove 61 on the outside of the battery cell 10, which is conducive to reducing the difficulty of forming the first groove 61, so as to improve the production efficiency of the battery cell 10. The second surface 65 is the surface of the pressure relief component 6 facing the inside of the battery cell 10. When the second groove 62 is set on the second surface 65, the second groove 62 is set on the inside of the pressure relief component 6. On the one hand, when the predetermined pressure relief area 63 is turned outward and opened, the two groove side surfaces (the first groove side surface 621 and the second groove side surface 622) in the width direction of the second groove 62 are not easy to abut against each other, which is conducive to increasing the opening area of ​​the predetermined pressure relief area 63; on the other hand, the second groove 62 is not exposed to the outside of the battery cell 10, reducing the risk of oxidation corrosion of the pressure relief component 6 in the second groove 62 area. In addition, the second surface 65 is the surface of the pressure relief component 6 facing the interior of the battery cell 10. When the first groove 61 is arranged on the second surface 65, the first groove 61 is arranged on the inner side of the pressure relief component 6, which can reduce the risk of oxidation corrosion of the pressure relief component 6 in the first groove 61 area.

[0273] In other embodiments, the first surface 64 may be the surface of the pressure relief component 6 facing the interior of the battery cell 10 , and the second surface 65 may be the surface of the pressure relief component 6 facing the exterior of the battery cell 10 .

[0274] In some embodiments, please refer to Fig.14 and Fig.15 , Fig.14 A partial view of the housing 1 (the first groove 61 is an arc-shaped groove) provided in some embodiments of the present application; Fig.15 for Fig.14 The FF cross-sectional view of the housing 1 is shown. Along the thickness direction X of the first wall portion, the projection of the first groove 61 , the projection of the extension line 61 a of the first groove and the projection of the second groove 62 together enclose a predetermined pressure relief area 63 .

[0275] The first groove 61 may include only one groove section, and the first groove 61 may be a groove extending along a non-linear trajectory, for example, the first groove 61 is a groove extending along an arc trajectory, a parabolic trajectory, etc. Both ends of the first groove 61 may have extension lines, and along the thickness direction X of the first wall portion, the projections of the extension lines at both ends of the first groove 61 intersect with the projection of the second groove 62; or only one end of the first groove 61 may have an extension line, and along the thickness direction X of the first wall portion, the projection of the extension line at one end of the first groove 61 intersects with the projection of the second groove 62, and the projection of the first groove 61 and the projection of the second groove 62 intersect at the projection of the other end of the first groove 61.

[0276] The first groove 61 may include a plurality of groove segments, and the plurality of groove segments may form a U-shaped, H-shaped, V-shaped, Y-shaped, X-shaped, T-shaped, and other structures. The extension line 61a of the first groove may be one groove segment or the extension line of a plurality of groove segments. For example, the first groove 61 includes three groove segments, and the three groove segments form a U-shaped structure. In the two groove segments located at both ends of the first groove 61, both groove segments may have extension lines, and along the thickness direction X of the first wall, the projections of the extension lines of the two groove segments intersect with the projection of the second groove 62; or only one groove segment may have an extension line, and along the thickness direction X of the first wall, the projection of the extension line of one groove segment intersects with the projection of the second groove 62, and the projection of the other groove segment intersects with the projection of the second groove 62.

[0277] Whether the first groove 61 includes only one groove segment or multiple groove segments, the extension line 61a of the first groove is a portion that continues to extend from the end of the groove segment along the extension direction of the groove segment located at the end of the first groove 61. It can be understood that if the groove segment extends along an arc trajectory, the extension line 61a of the first groove also extends along the arc trajectory; if the groove segment extends along a straight trajectory, the extension line 61a of the first groove also extends along the straight trajectory.

[0278] As an example, in Fig.14and Fig.15 In the illustrated embodiment, the first groove 61 is an arc groove, the first groove 61 is arranged on the first surface 64, and the second groove 62 is arranged on the second surface 65. Along the width direction Z of the second groove, the second groove 62 is arranged at intervals from the first groove 61. Along the thickness direction X of the first wall portion, the projection of the second groove 62 extends out of the two ends of the projection of the first groove 61 at both ends along the extension direction. The edge of the measurement surface of the predetermined pressure relief area 63 is formed by the projection of the inner edge of the notch of the second groove 62 (the edge of the notch of the second groove 62 on the side close to the predetermined pressure relief area 63) on the first surface 64, the projection of the inner edge of the notch of the first groove 61 (the edge of the notch of the first groove 61 on the side close to the predetermined pressure relief area 63) on the first surface 64, and the projection of the extension line of the two ends of the inner edge of the notch of the first groove 61 on the first surface 64. The area of ​​the measurement surface of the predetermined pressure relief area 63 is the area of ​​the predetermined pressure relief area 63. When measuring the area of ​​the predetermined pressure relief zone 63, a first straight line can be drawn on the first surface 64 so that the projection of the inner edge of the notch of the second groove 62 on the first surface 64 is located within the first straight line, and then an extension line of the inner edge of the notch of the first groove 61 is drawn on the first surface 64 along the extension direction of the inner edge and intersects with the first straight line, thereby defining a measuring surface, the edge of which is composed of an arc line and a straight line.

[0279] In this embodiment, the projection of the first groove 61 along the thickness direction X of the first wall portion, the projection of the extension line 61a of the first groove along the thickness direction X of the first wall portion, and the projection of the second groove 62 along the thickness direction X of the first wall portion jointly enclose a predetermined pressure relief area 63. This structure ensures that the projection of the second groove 62 along the thickness direction X of the first wall portion and the projection of the first groove 61 along the thickness direction X of the first wall portion do not form a closed structure, thereby reducing the mutual influence between the first groove 61 and the second groove 62 during the processing process, and reducing the risk of the predetermined pressure relief area 63 falling off and splashing during pressure relief.

[0280] In some embodiments, please refer to Fig.16 , Fig.16 Partial view of the housing 1 (the first groove 61 is an arc groove) provided in some other embodiments of the present application. Along the thickness direction X of the first wall portion, the projection of the first groove 61, the projection of the second groove 62 and the projection of the extension line 62a of the second groove together enclose a predetermined pressure relief area 63.

[0281] The first groove 61 may include only one groove segment, and the first groove 61 may be a groove extending along a non-linear trajectory, for example, the first groove 61 is a groove extending along an arc trajectory, a parabolic trajectory, etc. The first groove 61 may include multiple groove segments, and the multiple groove segments may form a U-shaped, H-shaped, V-shaped, Y-shaped, X-shaped, T-shaped, etc. structure.

[0282] The extension line 62a of the second groove is the part that continues to extend from the end of the second groove 62 along the extension direction Y of the second groove. If the second groove 62 extends along an arc trajectory, the extension line 62a of the second groove also extends along the arc trajectory; if the second groove 62 extends along a straight trajectory, the extension line 62a of the second groove also extends along the straight trajectory. Both ends of the second groove 62 may have extension lines, and along the thickness direction X of the first wall portion, the projections of the extension lines at both ends of the second groove 62 intersect with the projection of the first groove 61; or only one end of the second groove 62 may have an extension line, and along the thickness direction X of the first wall portion, the projection of the extension line of one end of the second groove 62 intersects with the projection of the first groove 61, and the projection of the second groove 62 intersects with the projection of the first groove 61 at the projection of the other end of the second groove 62.

[0283] As an example, in Fig.16 In the illustrated embodiment, the first groove 61 is an arc-shaped groove, and the first groove 61 is disposed on the first surface 64 ( Fig.16 The second groove 62 is provided on the second surface 65 ( Fig.16 The second groove 62 is located in the area enclosed by the line connecting the two ends of the first groove 61 and the first groove 61. The edge of the measuring surface of the predetermined pressure relief zone 63 is formed by the projection of the inner edge of the notch of the second groove 62 (the edge of the notch of the second groove 62 close to the predetermined pressure relief zone 63) in the first surface 64, the projection of the extended line of the two ends of the inner edge of the notch of the second groove 62 in the first surface 64, and the projection of the inner edge of the notch of the first groove 61 (the edge of the notch of the first groove 61 close to the predetermined pressure relief zone 63) in the first surface 64. The area of ​​the measuring surface of the predetermined pressure relief zone 63 is the area of ​​the predetermined pressure relief zone 63. When measuring the area of ​​the predetermined pressure relief zone 63, a first straight line can be drawn on the first surface 64, so that the projection of the inner edge of the notch of the second groove 62 on the first surface 64 is located in the first straight line, and the two ends of the first straight line extend to the inner edge of the notch of the first groove 61, respectively, so as to define the measuring surface, and the edge of the measuring surface is composed of an arc and a straight line.

[0284] In this embodiment, the projection of the first groove 61 along the thickness direction X of the first wall portion, the projection of the second groove 62 along the thickness direction X of the first wall portion, and the projection of the extension line 62a of the second groove along the thickness direction X of the first wall portion jointly enclose a predetermined pressure relief area 63. This structure ensures that the projection of the second groove 62 along the thickness direction X of the first wall portion and the projection of the first groove 61 along the thickness direction X of the first wall portion do not form a closed structure, thereby reducing the mutual influence between the first groove 61 and the second groove 62 during the processing process, and reducing the risk of the predetermined pressure relief area 63 falling off and splashing during pressure relief.

[0285] In some embodiments, please refer to Fig.17 , Fig.17 A partial view of the housing 1 (the first groove 61 is an arc groove) provided in some other embodiments of the present application. Along the thickness direction X of the first wall portion, the projection of the first groove 61, the projection of the extension line 61a of the first groove, the projection of the second groove 62 and the projection of the extension line 62a of the second groove together enclose a predetermined pressure relief area 63.

[0286] The first groove 61 may include only one groove section, and the first groove 61 may be a groove extending along a non-linear trajectory, for example, the first groove 61 is a groove extending along an arc trajectory, a parabolic trajectory, etc. Both ends of the first groove 61 may have extension lines, and both ends of the second groove 62 may also have extension lines, and along the thickness direction X of the first wall portion, the projections of the extension lines at both ends of the first groove 61 intersect with the projections of the extension lines at both ends of the second groove 62 respectively; or only one end of the first groove 61 may have an extension line, and only one end of the second groove 62 may have an extension line, and along the thickness direction X of the first wall portion, the projection of the extension line of one end of the first groove 61 intersects with the projection of the extension line of one end of the second groove 62, and the projection of the other end of the first groove 61 is connected to the projection of the other end of the second groove 62.

[0287] The first groove 61 may include multiple groove segments, and the multiple groove segments may form a U-shaped, H-shaped, V-shaped, Y-shaped, X-shaped, T-shaped, etc. structure. The extension line of one groove segment or multiple groove segments may be the extension line 61a of the first groove. For example, the first groove 61 includes three groove segments, and the three groove segments form a U-shaped structure. In the two groove segments located at both ends of the first groove 61, both groove segments may have extension lines, and along the thickness direction X of the first wall, the projections of the extension lines of the two groove segments intersect with the projections of the extension lines at both ends of the second groove 62 respectively; or only one groove segment may have an extension line, and along the thickness direction X of the first wall, the projection of the extension line of one groove segment intersects with the projection of the extension line 62a of the second groove, and the projection of the other groove segment intersects with the projection of the second groove 62.

[0288] Whether the first groove 61 includes only one groove segment or multiple groove segments, the extension line 61a of the first groove is a portion that continues to extend from the end of the groove segment along the extension direction of the groove segment located at the end of the first groove 61. The extension line 62a of the second groove is a portion that continues to extend from the end of the second groove 62 along the extension direction Y of the second groove.

[0289] As an example, in Fig.17 In the illustrated embodiment, the first groove 61 is an arc-shaped groove, and the first groove 61 is disposed on the first surface 64 ( Fig.17 The second groove 62 is provided on the second surface 65 ( Fig.17(not shown), along the width direction Z of the second groove, the second groove 62 is spaced from the first groove 61, and along the thickness direction X of the first wall portion, the two ends of the projection of the second groove 62 along the extension direction do not extend beyond the two ends of the projection of the first groove 61. The edge of the measurement surface of the predetermined pressure relief zone 63 is formed by the projection of the inner edge of the notch of the second groove 62 (the edge of the notch of the second groove 62 on the side close to the predetermined pressure relief zone 63) on the first surface 64, the projection of the extension line of the inner edge of the notch of the second groove 62 on the first surface 64, the projection of the inner edge of the notch of the first groove 61 (the edge of the notch of the first groove 61 on the side close to the predetermined pressure relief zone 63) on the first surface 64, and the projection of the extension line of the inner edge of the notch of the first groove 61 on the first surface 64. The area of ​​the measurement surface of the predetermined pressure relief zone 63 is the area of ​​the predetermined pressure relief zone 63. When measuring the area of ​​the predetermined pressure relief zone 63, a first straight line can be drawn on the first surface 64 so that the projection of the inner edge of the notch of the second groove 62 on the first surface 64 is located within the first straight line, and then the extension lines of the two ends of the inner edge of the notch of the first groove 61 are drawn on the first surface 64 along the extension direction of the inner edge and intersected with the first straight line, thereby defining a measuring surface, the edge of which is composed of an arc line and a straight line.

[0290] In this embodiment, the projection of the first groove 61 along the thickness direction X of the first wall portion, the projection of the extension line of the first groove 61 along the thickness direction X of the first wall portion, the projection of the second groove 62 along the thickness direction X of the first wall portion, and the projection of the extension line of the second groove 62 along the thickness direction X of the first wall portion jointly enclose a predetermined pressure relief area 63. This structure ensures that the projection of the second groove 62 along the thickness direction X of the first wall portion and the projection of the first groove 61 along the thickness direction X of the first wall portion do not form a closed structure, thereby reducing the mutual influence between the first groove 61 and the second groove 62 during the processing process, and reducing the risk of the predetermined pressure relief area 63 falling off and splashing during pressure relief.

[0291] In some embodiments, please refer to Figure 14-17 , the first groove 61 extends along an arc trajectory.

[0292] The central angle of the first groove 61 may be less than 15°, 30°, 45°, 60°, 90°, 120°, 150°, 180°, 210°, 240°, 270°, 300°, 330°, etc.

[0293] exist Figure 14-17 In the illustrated embodiment, the central angle of the first groove 61 is greater than 180° and less than 270°.

[0294] In this embodiment, the first groove 61 extends along an arc track. The first groove 61 is an arc-shaped groove. The first groove 61 of this structure only includes one groove segment, which simplifies the structure of the first groove 61.

[0295] In some embodiments, the second groove 62 extends along a straight line. The second groove 62 is a straight groove with a simple structure and is easy to process and shape.

[0296] In some embodiments, please refer to Fig.18 and 19 , Fig.18 A partial view of the housing 1 (the first groove 61 is a V-shaped groove) provided in some embodiments of the present application; Fig.19 for Fig.18 The GG cross-sectional view of the housing 1 is shown. The first groove 61 includes a first groove section 611 and a second groove section 612, and the first groove section 611 is connected to the second groove section 612. Along the thickness direction X of the first wall portion, the projection of the first groove section 611, the projection of the extension line of the first groove section 611, the projection of the second groove section 612, the projection of the extension line of the second groove section 612, and the projection of the second groove 62 together enclose a predetermined pressure relief area 63.

[0297] The first slot section 611 and the second slot section 612 are two slot sections in the first groove 61. The first slot section 611 and the second slot section 612 can be a linear slot extending along a linear trajectory, or a non-linear slot extending along a non-linear trajectory, for example, an arcuate slot extending along an arc trajectory. If the first slot section 611 and the second slot section 612 both extend along a linear trajectory, the first slot section 611 and the second slot section 612 can be arranged at an acute angle, a right angle, or an obtuse angle. The first slot section 611 and the second slot section 612 can be connected at their ends to form a V-shaped, L-shaped, or other structure. The first groove 61 of this structure can define a predetermined pressure relief area 63 with a second groove 62. The first slot section 611 and the second slot section 612 can also be arranged crosswise to form an X-shaped structure. The first groove 61 of this structure can define two predetermined pressure relief areas 63 with two second grooves 62, or can define four predetermined pressure relief areas 63 with four second grooves 62. The extension line of the first slot segment 611 is the portion that continues to extend from the end of the first slot segment 611 along the extension direction of the first slot segment 611. The extension line of the second slot segment 612 is the portion that continues to extend from the end of the second slot segment 612 along the extension direction of the second slot segment 612. The extension line of the first slot segment 611 and the extension line of the second slot segment 612 are both extension lines 61a of the first groove.

[0298] As an example, in Fig.18 and Fig.19In the illustrated embodiment, the first groove section 611 is connected to the second groove section 612 to form a V-shaped structure, the first groove 61 is arranged on the first surface 64, the second groove 62 is arranged on the second surface 65, along the width direction Z of the second groove, the second groove 62 is spaced apart from the first groove 61, and along the thickness direction X of the first wall portion, the projection of the second groove 62 extends out of the two ends of the projection of the first groove 61 at both ends along the extension direction. The edge of the measuring surface of the predetermined pressure relief zone 63 is formed by the projection of the inner edge of the notch of the second groove 62 (the edge of the notch of the second groove 62 on the side close to the predetermined pressure relief zone 63) on the first surface 64, the projection of the inner edge of the notch of the first groove section 611 (the edge of the notch of the first groove section 611 on the side close to the predetermined pressure relief zone 63) on the first surface 64, the projection of the extended line of the inner edge of the notch of the first groove section 611 on the first surface 64, the projection of the inner edge of the notch of the second groove section 612 (the edge of the notch of the second groove section 612 on the side close to the predetermined pressure relief zone 63) on the first surface 64, and the projection of the extended line of the inner edge of the notch of the second groove section 612 on the first surface 64. The area of ​​the measuring surface of the predetermined pressure relief zone 63 is the area of ​​the predetermined pressure relief zone 63, and the predetermined pressure relief zone 63 is a triangle. When measuring the area of ​​the predetermined pressure relief zone 63, a first straight line can be drawn on the first surface 64 so that the projection of the inner edge of the notch of the second groove 62 on the first surface 64 is located within the first straight line, and then an extension line of the inner edge of the notch of the first groove section 611 is drawn on the first surface 64 along the extension direction of the inner edge of the notch and intersects with the first straight line, and then an extension line of the inner edge of the notch of the second groove section 612 is drawn on the first surface 64 along the extension direction of the inner edge and intersects with the first straight line, thereby defining a triangular measuring surface, and the area of ​​the predetermined pressure relief zone 63 can be calculated by measuring the base and height of the triangle and multiplying the base by the height.

[0299] It should be noted that in the embodiment where the first groove 61 is a multi-stage groove structure, both the first groove section 611 and the second groove section 612 are multi-stage groove structures.

[0300] In this embodiment, the first groove 61 has a simple structure, and the stress at the position where the first groove section 611 and the second groove section 612 are connected is more concentrated, weaker, and easier to crack, so that when the battery cell 10 thermally runs away, the pressure relief component 6 can quickly crack from the first groove section 611 and the second groove section 612 after cracking from the position where the first groove section 611 and the second groove section 612 are connected, so that the predetermined pressure relief area 63 is opened more quickly to release pressure in time.

[0301] In some embodiments, please refer to Fig. 20 , Fig. 20Partial view of the housing 1 (the first groove 61 is a V-shaped groove) provided in some other embodiments of the present application. The first groove 61 includes a first groove section 611 and a second groove section 612, and the first groove section 611 is connected to the second groove section 612. Along the thickness direction X of the first wall portion, the projection of the first groove section 611, the projection of the second groove section 612, the projection of the second groove 62, and the projection of the extension line of the second groove 62 together enclose a predetermined pressure relief area 63.

[0302] As an example, in Fig. 20 In the illustrated embodiment, the first groove section 611 and the second groove section 612 are connected to form a V-shaped structure, and the first groove 61 is provided on the first surface 64 ( Fig. 20 The second groove 62 is provided on the second surface 65 ( Fig. 20 (not shown), the second groove 62 is located in the area enclosed by the line connecting one end of the first groove section 611 and one end of the second groove section 612 and the first groove 61. The edge of the measuring surface of the predetermined pressure relief zone 63 is formed by the projection of the inner edge of the notch of the second groove 62 (the edge of the notch of the second groove 62 on the side close to the predetermined pressure relief zone 63) on the first surface 64, the projection of the extended line of the inner edge of the notch of the second groove 62 on the first surface 64, the projection of the inner edge of the notch of the first groove section 611 (the edge of the notch of the first groove section 611 on the side close to the predetermined pressure relief zone 63) on the first surface 64, and the projection of the inner edge of the notch of the second groove section 612 (the edge of the notch of the second groove section 612 on the side close to the predetermined pressure relief zone 63) on the first surface 64. The area of ​​the measuring surface of the predetermined pressure relief zone 63 is the area of ​​the predetermined pressure relief zone 63, and the predetermined pressure relief zone 63 is a triangle. When measuring the area of ​​the predetermined pressure relief zone 63, a first straight line can be drawn on the first surface 64 so that the projection of the inner edge of the notch of the second groove 62 on the first surface 64 is located within the first straight line, and the two ends of the first straight line extend to the inner edge of the notch of the first groove section 611 and the inner edge of the notch of the second groove section 612, respectively, thereby defining a triangular measuring surface. The area of ​​the predetermined pressure relief zone 63 can be calculated by measuring the base and height of the triangle and multiplying the base by the height.

[0303] In this embodiment, the first groove 61 has a simple structure, and the stress at the position where the first groove section 611 and the second groove section 612 are connected is more concentrated, weaker, and easier to crack, so that when the battery cell 10 thermally runs away, the pressure relief component 6 can quickly crack from the first groove section 611 and the second groove section 612 after cracking from the position where the first groove section 611 and the second groove section 612 are connected, so that the predetermined pressure relief area 63 is opened more quickly to release pressure in time.

[0304] In some embodiments, please refer to Fig.21 , Fig.21Partial view of the housing 1 (the first groove 61 is a V-shaped groove) provided in some other embodiments of the present application. The first groove 61 includes a first groove section 611 and a second groove section 612, and the first groove section 611 is connected to the second groove section 612. Along the thickness direction X of the first wall portion, the projection of the first groove section 611, the projection of the extension line of the first groove section 611, the projection of the second groove section 612, the projection of the extension line of the second groove section 612, the projection of the second groove 62, and the projection of the extension line 62a of the second groove together enclose a predetermined pressure relief area 63.

[0305] As an example, in Fig.21 In the illustrated embodiment, the first groove section 611 and the second groove section 612 are connected to form a V-shaped structure, and the first groove 61 is provided on the first surface 64 ( Fig.21 The second groove 62 is provided on the second surface 65 ( Fig.21 (not shown), along the width direction Z of the second groove, the second groove 62 is spaced apart from the first groove 61, and along the thickness direction X of the first wall portion, the two ends of the projection of the second groove 62 along the extension direction do not extend beyond the two ends of the projection of the first groove 61. The edge of the measuring surface of the predetermined pressure relief zone 63 is formed by the projection of the inner edge of the notch of the second groove 62 (the edge of the notch of the second groove 62 on the side close to the predetermined pressure relief zone 63) on the first surface 64, the projection of the extended line of the inner edge of the notch of the second groove 62 on the first surface 64, the projection of the inner edge of the notch of the first groove section 611 (the edge of the notch of the first groove section 611 on the side close to the predetermined pressure relief zone 63) on the first surface 64, the projection of the extended line of the inner edge of the notch of the first groove section 611 on the first surface 64, the projection of the inner edge of the notch of the second groove section 612 (the edge of the notch of the second groove section 612 on the side close to the predetermined pressure relief zone 63) on the first surface 64, and the projection of the extended line of the inner edge of the notch of the second groove section 612 on the first surface 64. The area of ​​the measuring surface of the predetermined pressure relief zone 63 is the area of ​​the predetermined pressure relief zone 63, and the predetermined pressure relief zone 63 is a triangle. When measuring the area of ​​the predetermined pressure relief zone 63, a first straight line can be drawn on the first surface 64 so that the projection of the inner edge of the notch of the second groove 62 on the first surface 64 is located within the first straight line, and then an extension line of the inner edge of the notch of the first groove section 611 is drawn on the first surface 64 along the extension direction of the inner edge of the notch and intersects with the first straight line, and then an extension line of the inner edge of the notch of the second groove section 612 is drawn on the first surface 64 along the extension direction of the inner edge and intersects with the first straight line, thereby defining a triangular measuring surface, and the area of ​​the predetermined pressure relief zone 63 can be calculated by measuring the base and height of the triangle and multiplying the base by the height.

[0306] In this embodiment, the first groove 61 has a simple structure, and the stress at the position where the first groove section 611 and the second groove section 612 are connected is more concentrated, weaker, and easier to crack, so that when the battery cell 10 thermally runs away, the pressure relief component 6 can quickly crack from the first groove section 611 and the second groove section 612 after cracking from the position where the first groove section 611 and the second groove section 612 are connected, so that the predetermined pressure relief area 63 is opened more quickly to release pressure in time.

[0307] In some embodiments, please refer to Fig. 9 and Fig.10 The first groove 61 includes a first groove section 611, a second groove section 612 and a third groove section 613. The second groove section 612 and the third groove section 613 are arranged opposite to each other. The first groove section 611 connects the second groove section 612 and the third groove section 613. The first groove section 611 is arranged opposite to the second groove 62. Along the thickness direction X of the first wall portion, the projection of the first groove section 611, the projection of the second groove section 612, the projection of the extension line of the second groove section 612, the projection of the third groove section 613, the projection of the extension line of the third groove section 613 and the projection of the second groove 62 together enclose a predetermined pressure relief area 63.

[0308] The first slot section 611, the second slot section 612 and the third slot section 613 are three slot sections in the first groove 61. The first slot section 611, the second slot section 612 and the third slot section 613 can be straight slots extending along a straight track, or non-straight slots extending along a non-straight track, for example, arc slots extending along an arc track. If the first slot section 611, the second slot section 612 and the third slot section 613 all extend along a straight track, the first slot section 611 and the second slot section 612 can be arranged at an acute angle, a right angle or an obtuse angle, the first slot section 611 and the third slot section 613 can be arranged at an acute angle, a right angle or an obtuse angle, the second slot section 612 and the third slot section 613 can be arranged in parallel, or the extension line of the second slot section 612 and the extension line of the third slot section 613 can intersect.

[0309] The first slot section 611 connects the second slot section 612 and the third slot section 613. The two ends of the first slot section 611 may be connected to the second slot section 612 and the third slot section 613 respectively, or at least one of the second slot section 612 and the third slot section 613 may be connected to a position deviated from the end of the first slot section 611, so that at least one of the second slot section 612 and the third slot section 613 is located between the two ends of the first slot section 611. The position where the second slot section 612 is connected to the first slot section 611 may be located at one end of the second slot section 612 or between the two ends of the second slot section 612. The position where the third slot section 613 is connected to the first slot section 611 may be located at one end of the third slot section 613 or between the two ends of the third slot section 613. The first slot section 611, the second slot section 612, and the third slot section 613 may form a U-shaped structure, an H-shaped structure, or the like. If the first groove section 611, the second groove section 612, and the third groove section 613 form a U-shaped structure, the first groove 61 of this structure can define a predetermined pressure relief area 63 with a second groove 62. If the first groove section 611, the second groove section 612, and the third groove section 613 form an H-shaped structure, the first groove 61 of this structure can define two predetermined pressure relief areas 63 with two second grooves 62.

[0310] The extension line of the second slot segment 612 is the portion that continues to extend from the end of the second slot segment 612 along the extension direction of the second slot segment 612. The extension line of the third slot segment 613 is the portion that continues to extend from the end of the third slot segment 613 along the extension direction of the third slot segment 613. The extension line of the second slot segment 612 and the extension line of the third slot segment 613 are both extension lines 61a of the first groove.

[0311] As an example, in Fig. 9 and Fig.10In the illustrated embodiment, the first slot section 611, the second slot section 612 and the third slot section 613 form an H-shaped structure, there are two predetermined pressure relief areas 63, a part of the second slot section 612, a part of the third slot section 613, the first slot section 611 and a second groove 62 together define a predetermined pressure relief area 63, another part of the second slot section 612, another part of the third slot section 613, the first slot section 611 and another second groove 62 together define another predetermined pressure relief area 63. The first groove 61 is provided on the first surface 64, and the second groove 62 is provided on the second surface 65. Along the width direction Z of the second groove, the second groove 62 is spaced apart from the first groove 61, and along the thickness direction X of the first wall portion, the projection of the second groove 62 extends from the two ends of the projection of the first groove 61 along the extension direction. The edge of the measuring surface of the predetermined pressure relief zone 63 is formed by the projection of the inner edge of the notch of the second groove 62 (the edge of the notch of the second groove 62 on the side close to the predetermined pressure relief zone 63) on the first surface 64, the projection of the inner edge of the notch of the first groove section 611 (the edge of the notch of the first groove section 611 on the side close to the predetermined pressure relief zone 63) on the first surface 64, the projection of the inner edge of the notch of the second groove section 612 (the edge of the notch of the second groove section 612 on the side close to the predetermined pressure relief zone 63) on the first surface 64, the projection of the extended line of the inner edge of the notch of the second groove section 612 on the first surface 64, the projection of the inner edge of the notch of the third groove section 613 (the edge of the notch of the third groove section 613 on the side close to the predetermined pressure relief zone 63) on the first surface 64 and the projection of the extended line of the inner edge of the notch of the third groove section 613 on the first surface 64, and the predetermined pressure relief zone 63 is a rectangle. When measuring the area of ​​the predetermined pressure relief zone 63, a first straight line can be drawn on the first surface 64 so that the projection of the inner edge of the notch of the second groove 62 on the first surface 64 is located within the first straight line. Then, an extension line of the inner edge of the notch of the second groove section 612 is drawn on the first surface 64 along the extension direction of the inner edge and intersects with the first straight line. Then, an extension line of the inner edge of the notch of the third groove section 613 is drawn on the first surface 64 along the extension direction of the inner edge and intersects with the first straight line, thereby defining a rectangular measurement surface. By measuring the length and width of the rectangle and multiplying the length by the width, the area of ​​the predetermined pressure relief zone 63 can be calculated.

[0312] In this embodiment, the second groove section 612 and the third groove section 613 are arranged opposite to each other, the first groove section 611 and the second groove 62 are arranged opposite to each other along the width direction of the second groove 62, the first groove section 611 connects the second groove section 612 and the third groove section 613, the intersection position of the first groove section 611 and the second groove section 612 and the connection position of the first groove section 611 and the third groove section 613 are weaker, and are more likely to crack and open the predetermined pressure relief area 63 for pressure relief, and can further increase the opening area of ​​the predetermined pressure relief area 63, thereby increasing the pressure relief area of ​​the battery cell 10 and improving the pressure relief rate of the battery cell 10.

[0313] In some embodiments, please refer to Fig. 22 , Fig. 22 Partial view of the housing 1 (the first groove 61 is an H-shaped groove) provided for other embodiments of the present application. The first groove 61 includes a first groove section 611, a second groove section 612 and a third groove section 613. The second groove section 612 and the third groove section 613 are arranged opposite to each other. The first groove section 611 connects the second groove section 612 and the third groove section 613. Along the width direction of the second groove 62, the first groove section 611 and the second groove 62 are arranged opposite to each other. Along the thickness direction X of the first wall portion, the projection of the first groove section 611, the projection of the second groove section 612, the projection of the third groove section 613, the projection of the second groove 62 and the projection of the extension line 62a of the second groove together enclose a predetermined pressure relief area 63.

[0314] As an example, in Fig. 22 In the illustrated embodiment, the first slot section 611, the second slot section 612 and the third slot section 613 form an H-shaped structure, and there are two predetermined pressure relief areas 63. A portion of the second slot section 612, a portion of the third slot section 613, the first slot section 611 and a second groove 62 together define a predetermined pressure relief area 63, and another portion of the second slot section 612, another portion of the third slot section 613, the first slot section 611 and another second groove 62 together define another predetermined pressure relief area 63. The first groove 61 is provided on the first surface 64 ( Fig. 22 For illustration), the second groove 62 is provided on the second surface 65 ( Fig. 22The second groove 62 is located in the area enclosed by the line connecting one end of the second groove section 612 and one end of the third groove section 613 and the first groove 61. The edge of the measuring surface of the predetermined pressure relief area 63 is formed by the projection of the inner edge of the notch of the second groove 62 (the edge of the notch of the second groove 62 on the side close to the predetermined pressure relief area 63) on the first surface 64, the projection of the extended line of the inner edge of the notch of the second groove 62 on the first surface 64, the projection of the inner edge of the notch of the first groove section 611 (the edge of the notch of the first groove section 611 on the side close to the predetermined pressure relief area 63) on the first surface 64, the projection of the inner edge of the notch of the second groove section 612 (the edge of the notch of the second groove section 612 on the side close to the predetermined pressure relief area 63) on the first surface 64, and the projection of the inner edge of the notch of the third groove section 613 (the edge of the notch of the third groove section 613 on the side close to the predetermined pressure relief area 63) on the first surface 64, and the predetermined pressure relief area 63 is rectangular. When measuring the area of ​​the predetermined pressure relief zone 63, a first straight line can be drawn on the first surface 64 so that the projection of the inner edge of the notch of the second groove 62 on the first surface 64 is located within the first straight line, and the two ends of the first straight line extend to the inner edge of the notch of the second groove section 612 and the inner edge of the notch of the third groove section 613, respectively, thereby defining a rectangular measuring surface. By measuring the length and width of the rectangle and multiplying the length by the width, the area of ​​the predetermined pressure relief zone 63 can be calculated.

[0315] In this embodiment, the second groove section 612 and the third groove section 613 are arranged opposite to each other, the first groove section 611 and the second groove 62 are arranged opposite to each other along the width direction of the second groove 62, the first groove section 611 connects the second groove section 612 and the third groove section 613, the intersection position of the first groove section 611 and the second groove section 612 and the connection position of the first groove section 611 and the third groove section 613 are weaker, and are more likely to crack and open the predetermined pressure relief area 63 for pressure relief, and can further increase the opening area of ​​the predetermined pressure relief area 63, thereby increasing the pressure relief area of ​​the battery cell 10 and improving the pressure relief rate of the battery cell 10.

[0316] In some embodiments, please refer to Fig.23 , Fig.23Partial view of the housing 1 (the first groove 61 is an H-shaped groove) provided for some other embodiments of the present application. The first groove 61 includes a first groove section 611, a second groove section 612 and a third groove section 613. The second groove section 612 and the third groove section 613 are arranged opposite to each other. The first groove section 611 connects the second groove section 612 and the third groove section 613. Along the width direction of the second groove 62, the first groove section 611 and the second groove 62 are arranged opposite to each other. Along the thickness direction X of the first wall portion, the projection of the first groove section 611, the projection of the second groove section 612, the projection of the extension line of the second groove section 612, the projection of the third groove section 613, the projection of the extension line of the third groove section 613, the projection of the second groove 62 and the projection of the extension line 62a of the second groove together enclose a predetermined pressure relief area 63.

[0317] As an example, in Fig.23 In the illustrated embodiment, the first slot section 611, the second slot section 612 and the third slot section 613 form an H-shaped structure, and there are two predetermined pressure relief areas 63. A portion of the second slot section 612, a portion of the third slot section 613, the first slot section 611 and a second groove 62 together define a predetermined pressure relief area 63, and another portion of the second slot section 612, another portion of the third slot section 613, the first slot section 611 and another second groove 62 together define another predetermined pressure relief area 63. The first groove 61 is provided on the first surface 64 ( Fig.23 The second groove 62 is provided on the second surface 65 ( Fig.23(not shown), along the width direction Z of the second groove, the second groove 62 is spaced apart from the first groove 61, and along the thickness direction X of the first wall portion, the two ends of the projection of the second groove 62 along the extension direction do not extend beyond the two ends of the projection of the first groove 61. The edge of the measuring surface of the predetermined pressure relief zone 63 is formed by the projection of the inner edge of the notch of the second groove 62 (the edge of the notch of the second groove 62 on the side close to the predetermined pressure relief zone 63) on the first surface 64, the projection of the extended line of the inner edge of the notch of the second groove 62 on the first surface 64, the projection of the inner edge of the notch of the first groove section 611 (the edge of the notch of the first groove section 611 on the side close to the predetermined pressure relief zone 63) on the first surface 64, the projection of the inner edge of the notch of the second groove section 612 (the edge of the notch of the second groove section 612 on the side close to the predetermined pressure relief zone 63) on the first surface 64, the projection of the extended line of the inner edge of the notch of the second groove section 612 on the first surface 64, the projection of the inner edge of the notch of the third groove section 613 (the edge of the notch of the third groove section 613 on the side close to the predetermined pressure relief zone 63) on the first surface 64 and the projection of the extended line of the inner edge of the notch of the third groove section 613 on the first surface 64, and the predetermined pressure relief zone 63 is a rectangle. When measuring the area of ​​the predetermined pressure relief zone 63, a first straight line can be drawn on the first surface 64 so that the projection of the inner edge of the notch of the second groove 62 on the first surface 64 is located within the first straight line. Then, an extension line of the inner edge of the notch of the second groove section 612 is drawn on the first surface 64 along the extension direction of the inner edge and intersects with the first straight line. Then, an extension line of the inner edge of the notch of the third groove section 613 is drawn on the first surface 64 along the extension direction of the inner edge and intersects with the first straight line, thereby defining a rectangular measurement surface. By measuring the length and width of the rectangle and multiplying the length by the width, the area of ​​the predetermined pressure relief zone 63 can be calculated.

[0318] In this embodiment, the second groove section 612 and the third groove section 613 are arranged opposite to each other, the first groove section 611 and the second groove 62 are arranged opposite to each other along the width direction of the second groove 62, the first groove section 611 connects the second groove section 612 and the third groove section 613, the intersection position of the first groove section 611 and the second groove section 612 and the connection position of the first groove section 611 and the third groove section 613 are weaker, and are more likely to crack and open the predetermined pressure relief area 63 for pressure relief, and can further increase the opening area of ​​the predetermined pressure relief area 63, thereby increasing the pressure relief area of ​​the battery cell 10 and improving the pressure relief rate of the battery cell 10.

[0319] In some embodiments, please refer to Fig. 22 and Fig.23The connection position of the second slot section 612 and the first slot section 611 deviates from the two ends of the second slot section 612 , and the connection position of the third slot section 613 and the first slot section 611 deviates from the two ends of the third slot section 613 , so that a predetermined pressure relief area 63 is formed on both sides of the first slot section 611 .

[0320] The connection position between the second slot segment 612 and the first slot segment 611 deviates from the two ends of the second slot segment 612, that is, the connection position between the second slot segment 612 and the first slot segment 611 is not located at any one of the two ends of the second slot segment 612, and along the extension direction of the second slot segment 612, the connection position between the second slot segment 612 and the first slot segment 611 is located between the two ends of the second slot segment 612. The connection position between the second slot segment 612 and the first slot segment 611 can be located at the midpoint of the second slot segment 612, or can be deviated from the midpoint of the second slot segment 612.

[0321] The connection position between the third slot segment 613 and the first slot segment 611 deviates from the two ends of the third slot segment 613, that is, the connection position between the third slot segment 613 and the first slot segment 611 is not located at any one of the two ends of the third slot segment 613, and along the extension direction of the third slot segment 613, the connection position between the third slot segment 613 and the first slot segment 611 is located between the two ends of the third slot segment 613. The connection position between the third slot segment 613 and the first slot segment 611 can be located at the midpoint of the third slot segment 613, or can be deviated from the midpoint of the third slot segment 613.

[0322] It should be noted that in the embodiment where the first groove 61 is a multi-stage groove structure, the first groove section 611 , the second groove section 612 and the third groove section 613 are all multi-stage groove structures.

[0323] In this embodiment, the connection position of the second slot section 612 and the first slot section 611 deviates from the two ends of the second slot section 612. During the pressure relief process, after the pressure relief component 6 is cracked at the connection position of the second slot section 612 and the first slot section 611, the crack can spread along the second slot section 612 to the two ends of the second slot section 612, thereby shortening the time for the pressure relief component 6 to be cracked along the second slot section 612. The connection position of the third slot section 613 and the first slot section 611 deviates from the two ends of the third slot section 613. During the pressure relief process, after the pressure relief component 6 is cracked at the connection position of the third slot section 613 and the first slot section 611, the crack can spread along the third slot section 613 to the two ends of the third slot section 613, thereby shortening the time for the pressure relief component 6 to be cracked along the third slot section 613. In such a structure, the first groove section 611 of the first groove 61 is located between two predetermined pressure relief areas 63. After the pressure relief component 6 is split along the first groove section 611, the two predetermined pressure relief areas 63 can be opened in a split manner to relieve pressure when the battery cell 10 is depressurized, so that the two predetermined pressure relief areas 63 can be opened quickly, which is beneficial to improving the pressure relief rate of the battery cell 10.

[0324] In some embodiments, the first slot segment 611 extends along a straight line or an arc trajectory; and / or, the second slot segment 612 extends along a straight line or an arc trajectory; and / or, the third slot segment 613 extends along a straight line or an arc trajectory.

[0325] As an example, in Fig. 22 and Fig.23 In the illustrated embodiment, the first slot segment 611 , the second slot segment 612 , and the third slot segment 613 all extend along a straight line, and the second slot segment 612 and the third slot segment 613 are both perpendicular to the first slot segment 611 .

[0326] If the first groove section 611 extends along a straight trajectory, the first groove section 611 is a straight groove, which can reduce the difficulty of forming the first groove section 611. If the first groove section 611 extends along an arc trajectory, the first groove section 611 is an arc groove, and the pressure relief component 6 is more likely to split along the first groove section 611 when the battery cell 10 is depressurized, so that the predetermined pressure relief area 63 is opened more quickly. If the second groove section 612 extends along a straight trajectory, the second groove section 612 is a straight groove, which can reduce the difficulty of forming the second groove section 612. If the second groove section 612 extends along an arc trajectory, the second groove section 612 is an arc groove, and the pressure relief component 6 is more likely to split along the second groove section 612 when the battery cell 10 is depressurized, so that the predetermined pressure relief area 63 is opened more quickly. If the third groove section 613 extends along a straight trajectory, the third groove section 613 is a straight groove, which can reduce the difficulty of forming the third groove section 613. If the third groove section 613 extends along an arc trajectory, the third groove section 613 is an arc-shaped groove, and the pressure relief component 6 is more likely to split along the third groove section 613 when the battery cell 10 releases pressure, so that the predetermined pressure relief area 63 is opened more quickly.

[0327] In some embodiments, please refer to Fig.24 , Fig.24 An exploded view of a housing 1 (an opening is formed at one end of the housing 11 , the housing 11 includes a first wall portion 13 , and the pressure relief component 6 is the first wall portion 13 ) provided in some embodiments of the present application. The pressure relief component 6 is integrally formed with the first wall portion 13 .

[0328] The first wall portion 13 may be the entire pressure relief component 6, or a part of the first wall portion 13 may be the pressure relief component 6, so that the pressure relief component 6 and the first wall portion 13 are integrally formed. The first groove 61 and the second groove 62 are both provided in the first wall portion 13. One of the first surface 64 and the second surface 65 of the pressure relief component 6 is the inner surface of the first wall portion 13, and the other is the outer surface of the first wall portion 13.

[0329] In this embodiment, the pressure relief component 6 is integrally formed with the first wall portion 13, and the first groove 61 and the second groove 62 can be directly formed on the first wall portion 13 to form an integrated pressure relief structure, which has higher reliability, eliminates the installation process of the pressure relief component 6, and has better economy.

[0330] In some embodiments, the first groove 61 is stamped and formed on the first wall portion 13 ; and / or the second groove 62 is stamped and formed on the first wall portion 13 .

[0331] If the first groove 61 is a primary groove structure, when the first groove 61 is formed on the first wall portion 13, the first wall portion 13 can be punched once to punch out the first groove 61 on the first wall portion 13; if the first groove 61 is a multi-stage groove structure, when the first groove 61 is formed on the first wall portion 13, the first wall portion 13 can be punched multiple times to punch out a primary groove each time, and the first groove 61 is finally formed after multiple stampings.

[0332] In this embodiment, if the first groove 61 is stamped and formed on the first wall portion 13, the first groove 61 is simply formed, which is beneficial to reducing the production cost of the battery cell 10. If the second groove 62 is stamped and formed on the first wall portion 13, the second groove 62 is simply formed, which is beneficial to reducing the production cost of the battery cell 10.

[0333] In some embodiments, please refer to Fig.25 , Fig.25 An exploded view of a housing 1 (an opening is formed at one end of the housing 11, the housing 11 includes a first wall portion 13, and a pressure relief component 6 is installed on the first wall portion 13) provided in some embodiments of the present application. The pressure relief component 6 is separately provided from the first wall portion 13, and the pressure relief component 6 is installed on the first wall portion 13.

[0334] The pressure relief component 6 and the housing 1 are two separate components, and the pressure relief component 6 is produced separately and then installed on the first wall portion 13. The pressure relief component 6 can be installed on the first wall portion 13 by welding, riveting, bonding, etc. As an example, the first wall portion 13 is provided with a pressure relief hole 131, the pressure relief component 6 covers the pressure relief hole 131, and the pressure relief component 6 is welded to the first wall portion 13.

[0335] In this embodiment, the pressure relief component 6 is a component independent of the housing 1 , and the pressure relief component 6 and the housing 1 can be produced and assembled separately, with low production difficulty and high efficiency.

[0336] In some embodiments, the first wall portion 13 is a rectangular wall portion, and the first groove 61 and the second groove 62 are arranged along the width direction of the first wall portion 13 .

[0337] The housing 1 may be in a rectangular parallelepiped shape, and the first wall portion 13 may be any rectangular wall portion in the housing 1. The first wall portion 13 is a rectangular wall portion, that is, the first wall portion 13 is substantially in a rectangular shape when viewed along the thickness direction of the first wall portion 13. The length of the first wall portion 13 is greater than the width of the first wall portion 13.

[0338] The first groove 61 and the second groove 62 are arranged along the width direction of the first wall portion 13. The first groove 61 and the second groove 62 may be spaced apart along the width direction of the first wall portion 13, or the projection of the first groove 61 along the thickness direction X of the first wall portion and the projection of the second groove 62 along the thickness direction X of the first wall portion may be just connected in the width direction of the first wall portion 13. Taking the H-shaped first groove 61 as an example, the second groove section 612 and the third groove section 613 of the first groove 61 may both be at a certain distance from the second groove 62 along the width direction of the first wall portion 13, so that the first groove 61 and the second groove 62 are spaced apart along the width direction of the first wall portion 13. Alternatively, the projection of at least one of the second groove section 612 and the third groove section 613 of the first groove 61 along the thickness direction X of the first wall portion at one end of the extension direction just extends along the width direction of the first wall portion 13 to the projection of the second groove 62 along the thickness direction X of the first wall portion, so that the projection of the first groove 61 along the thickness direction X of the first wall portion and the projection of the second groove 62 along the thickness direction X of the first wall portion are just connected in the width direction of the first wall portion 13.

[0339] As an example, the width direction of the first wall portion 13 is parallel to the width direction Z of the second groove.

[0340] In this embodiment, the first groove 61 and the second groove 62 are arranged along the width direction of the first wall portion 13, so that the second groove 62 is closer to the edge of the first wall portion 13 in the width direction of the first wall portion 13, so that the area where the second groove 62 is arranged in the pressure relief component 6 has a higher strength, reducing the risk of the pressure relief component 6 being cracked along the second groove 62 when the battery cell 10 releases pressure. In addition, during the use of the battery cell 10, the expansion amount of the battery cell 10 in the width direction of the first wall portion 13 is greater than the expansion amount in the length direction of the first wall portion 13, and the expansion of the battery cell 10 in the width direction of the first wall portion 13 has a greater impact on the pressure relief component 6, and the first groove 61 and the second groove 62 are arranged along the width direction of the first wall portion 13, and the second groove 62 can absorb the deformation energy of the battery cell 10 when the battery cell 10 expands and deforms along the width direction of the first wall portion 13, thereby reducing the impact of the expansion of the battery cell 10 in the width direction of the first wall portion 13 on the pressure relief component 6.

[0341] In some embodiments, please refer to Figure 24-Figure 27 , Fig.26An exploded view of a housing 1 (an opening is formed at one end of the housing 11 and the end cover 12 is a pressure relief component 6) provided in some embodiments of the present application; Fig. 27 An exploded view of a housing 1 (an opening is formed at one end of the housing 11, the end cover 12 is a first wall portion 13, and the pressure relief component 6 is installed on the first wall portion 13) provided in some embodiments of the present application. The housing 11 has an opening formed at least at one end. The end cover 12 corresponds to the opening one by one, and the end cover 12 closes the opening. Among them, at least one end cover 12 is the first wall portion 13; and / or, at least one wall portion in the housing 11 is the first wall portion 13.

[0342] The shell 11 may have only one opening, for example, the shell 11 has an opening formed at only one end; the shell 11 may also have multiple openings, for example, the shell 11 has openings formed at both opposite ends. The number of end caps 12 is the same as the number of openings of the shell 11. It is understandable that if the shell 11 has only one opening, the end cap 12 is one; if the shell 11 has two openings, the end caps 12 are two. One or more end caps 12 may be the first wall portion 13, or one or more wall portions in the shell 11 may be the first wall portion 13. In the embodiment in which the shell 11 has an opening formed at one end, the positive electrode terminal and the negative electrode terminal may be provided at the end cap 12, and the positive electrode ear and the negative electrode ear may be formed at one end of the electrode assembly 2 facing the end cap 12, so as to be electrically connected to the positive electrode terminal and the negative electrode terminal respectively. In an embodiment in which openings are formed at both opposite ends of the shell 11, the positive electrode terminal can be arranged at one end cover 12, the negative electrode terminal can be arranged at the other end cover 12, and the positive electrode ear and the negative electrode ear can be respectively formed at the opposite ends of the electrode assembly 2 to facilitate electrical connection between the positive electrode ear and the positive electrode terminal and the negative electrode ear and the negative electrode terminal.

[0343] exist Fig.24 In the illustrated embodiment, an opening is formed at one end of the housing 11, a wall portion of the housing 11 opposite to the end cover 12 is a first wall portion 13, and the pressure relief component 6 is the first wall portion 13; Fig.25 In the illustrated embodiment, an opening is formed at one end of the housing 11, and a wall portion of the housing 11 opposite to the end cover 12 is a first wall portion 13, and the pressure relief component 6 is mounted on the first wall portion 13; Fig.26 In the embodiment shown, one end of the housing 11 forms an opening, and the end cover 12 is a first wall portion 13 ( Fig.26 (not shown), the first wall portion 13 is a pressure relief component 6. Fig. 27 In the illustrated embodiment, an opening is formed at one end of the housing 11 , the end cover 12 is a first wall portion 13 , and the pressure relief component 6 is mounted on the first wall portion 13 .

[0344] In this embodiment, if at least one end cap 12 is a first wall portion 13, so that at least one end cap 12 has a pressure relief function, the difficulty of forming the first groove 61 and the second groove 62 on the end cap 12 or the difficulty of installing the pressure relief component 6 is lower. If at least one wall portion in the shell 11 is a first wall portion 13, so that the shell 11 has a pressure relief function, when the battery cell 10 is depressurized, the emissions discharged from the inside of the battery cell 10 are not easy to affect the external components outside the end cap 12, reducing the risk of external components being damaged by emissions. The external components can be a confluence component connected to the electrode terminal 3, a temperature detection component, a voltage detection component, etc. The emissions include but are not limited to: electrolyte, dissolved or split positive and negative plates, fragments of separators, high-temperature and high-pressure gases generated by the reaction, flames, etc.

[0345] In some embodiments, please refer to Fig.24 and Fig.25 The shell 11 has an opening at only one end, and the wall portion of the shell 11 that is opposite to the end cover 12 is a first wall portion 13 .

[0346] As an example, the shell 11 is in a rectangular parallelepiped shape, and the shell 11 further includes four side walls, which are arranged around the first wall portion 13 . The four side walls and the first wall portion 13 together define a space inside the shell 11 .

[0347] In this embodiment, the housing 11 is an open structure at one end, making the structure of the entire battery cell 10 simpler. The first wall 13 is a wall of the housing 11 opposite to the end cover 12, and can achieve directional pressure relief from the bottom of the housing 11.

[0348] In some embodiments, please refer to Fig.28 , Fig.28 The exploded view of the battery cell 10 provided in some other embodiments of the present application. The housing 11 has openings at both opposite ends, and at least one wall portion in the housing 11 is a first wall portion 13 .

[0349] In the housing 11 , one wall portion may be the first wall portion 13 , or a plurality of walls may be the first wall portion 13 . The pressure relief component 6 may be the first wall portion 13 , or the pressure relief component 6 may be installed on the first wall portion 13 .

[0350] exist Fig.28 In the illustrated embodiment, the housing 11 is in a rectangular parallelepiped shape and includes four wall portions, which are connected in sequence at their ends and together define a space inside the housing 11. Among the four wall portions, two opposite wall portions are large-area wall portions, and the other two wall portions are small-area wall portions, and the outer surface area of ​​the large-area wall portion is greater than the outer surface area of ​​the small-area wall portion, and one or two small-area wall portions in the housing 11 are first wall portions 13.

[0351] In this embodiment, the shell 11 is a structure with openings formed at both opposite ends, and the electrode assembly 2 can be assembled into the shell 11 through any opening, which can reduce the difficulty of assembling the battery cell 10 and improve the assembly quality of the battery cell 10. The shell 11 of this structure can be made longer (openings are formed at both ends of the shell 11 in the length direction), which is conducive to increasing the capacity of the battery cell 10.

[0352] In some embodiments, the material of the pressure relief component 6 includes steel.

[0353] The steel material can be carbon steel, alloy steel, stainless steel, etc.

[0354] It is understandable that in the embodiment where the pressure relief component 6 and the first wall portion 13 are integrally formed, the material of the first wall portion 13 includes steel. If the first wall portion 13 is the end cover 12, the end cover 12 can be made of steel; if the first wall portion 13 is a wall portion in the housing 11, the housing 11 can be made of steel.

[0355] In this embodiment, steel has the characteristic of high strength, and the pressure relief component 6 made of steel has better strength. When the bursting pressure of the battery cell 10 is constant, the pressure relief component 6 can be made thinner to reduce the volume of the pressure relief component 6. In the embodiment where the pressure relief component 6 and the first wall portion 13 are integrally formed, the first wall portion 13 is made of steel, and the first wall portion 13 can be made thinner. When the volume of the shell 1 is constant, the volume of the shell 1 can be increased to provide more space for the electrode assembly 2, which is conducive to improving the volume energy density of the battery cell 10.

[0356] In some embodiments, the steel material is carbon steel or stainless steel.

[0357] Carbon steel can be low carbon steel, medium carbon steel or high carbon steel.

[0358] In some embodiments, the pressure relief component 6 is made of aluminum alloy.

[0359] It is understandable that in the embodiment where the pressure relief component 6 and the first wall portion 13 are integrally formed, the material of the first wall portion 13 includes aluminum alloy. If the first wall portion 13 is the end cover 12, the end cover 12 can be made of aluminum alloy; if the first wall portion 13 is a wall portion in the housing 11, the housing 11 can be made of aluminum alloy.

[0360] Aluminum alloy has the characteristics of light weight and good ductility, and it is easier to process the first groove 61 and the second groove 62 on the pressure relief component 6. In the embodiment where the pressure relief component 6 and the first wall portion 13 are integrally formed, the first wall portion 13 is made of aluminum alloy, which can effectively reduce the difficulty of forming the first wall portion 13. Since aluminum alloy has good ductility, it is easier to pile materials in the predetermined pressure relief area 63 when forming the first groove 61. However, controlling V / A at 0.05mm to 0.5mm can effectively reduce the impact of the pile of materials in the predetermined pressure relief area 63 on the performance of the battery cell 10, thereby improving the flatness of the surface of the pressure relief component 6 where the first groove 61 is set, taking into account the service life requirements of the battery cell 10 during normal use and the reliability requirements of the battery cell 10 during thermal runaway.

[0361] In some embodiments, the aluminum alloy includes the following components in mass percentage: aluminum ≥ 99.6%, copper ≤ 0.05%, iron ≤ 0.35%, magnesium ≤ 0.03%, manganese ≤ 0.03%, silicon ≤ 0.25%, titanium ≤ 0.03%, vanadium ≤ 0.05%, zinc ≤ 0.05%, and other single elements ≤ 0.03%.

[0362] This aluminum alloy belongs to the third series aluminum, and has lower hardness and better forming ability, which reduces the difficulty of processing the first groove 61 and the second groove 62, is conducive to improving the processing accuracy of the first groove 61 and the second groove 62, and improves the pressure relief consistency of the pressure relief component 6.

[0363] In some embodiments, the aluminum alloy includes the following components in mass percentage: aluminum ≥ 96.7%, 0.05% ≤ copper ≤ 0.2%, iron ≤ 0.7%, manganese ≤ 1.5%, silicon ≤ 0.6%, zinc ≤ 0.1%, other single element components ≤ 0.05%, and the total composition of other elements ≤ 0.15%.

[0364] This aluminum alloy belongs to the fifth series aluminum, and the pressure relief component 6 made of this aluminum alloy has higher hardness, greater strength, and good anti-destruction ability. The present application embodiment provides a battery 100, including the battery cell 10 provided by any of the above embodiments.

[0365] An embodiment of the present application provides an electrical device, including a battery cell 10 provided by any one of the above embodiments, and the battery cell 10 is used to provide electrical energy to the electrical device.

[0366] The embodiment of the present application also provides a battery cell 10, which includes a housing 1 and an electrode assembly 2, wherein the electrode assembly 2 has a positive electrode ear and a negative electrode ear, and the electrode assembly 2 is accommodated in the housing 1. The housing 1 is in the shape of a rectangular parallelepiped, and includes a shell 11 and an end cover 12, wherein an opening is formed at one end of the shell 11, and the end cover 12 closes the opening, and a positive electrode terminal and a negative electrode terminal are provided on the end cover 12, wherein the positive electrode terminal is electrically connected to the positive electrode ear through a current collecting member 4, and the negative electrode terminal is electrically connected to the negative electrode ear through another current collecting member 4.

[0367] The housing 11 is made of aluminum alloy, the wall of the housing 11 opposite to the end cover 12 is the pressure relief component 6, the pressure relief component 6 is a rectangular wall, the outer surface of the pressure relief component 6 is provided with a first groove 61, the inner surface of the pressure relief component 6 is provided with two second grooves 62, along the width direction of the pressure relief component 6, the first groove 61 is located between the two second grooves 62, and the second groove 62 is spaced from the first groove 61. The minimum residual thickness of the first groove 61 is less than the minimum residual thickness of the second groove 62. The first groove 61 is an H-shaped structure. The first groove 61 includes a first groove section 611, a second groove section 612 and a third groove section 613. The first groove section 611, the second groove section 612 and the third groove section 613 all extend along a straight line. The second groove section 612 and the third groove section 613 are arranged in parallel. The first groove section 611 connects the second groove section 612 and the third groove section 613. The second groove section 612 and the third groove section 613 are both perpendicular to the first groove section 611. The connection position between the first groove section 611 and the second groove section 612 is located at the midpoint of the second groove section 612. The connection position between the first groove section 611 and the third groove section 613 is located at the midpoint of the third groove section 613. Along the thickness direction X of the first wall portion, the projection of the second groove 62 extends the second groove section 612 and the third groove section 613 at both ends of the extension direction. The first groove 61 is a stepped groove. The first groove 61 includes two-stage grooves, and each stage of the groove is an H-shaped structure. Among them, along the thickness direction X of the first wall portion, the projection of the first groove section 611, the projection of the second groove section 612, the projection of the extension line of the second groove section 612, the third groove section 613, the projection of the extension line of the third groove section 613 and the projection of the two second grooves 62 together enclose two predetermined pressure relief areas 63, and the two predetermined pressure relief areas 63 are respectively located on both sides of the first groove section 611. The pressure relief component 6 is configured to be able to split along at least a portion of the first groove 61 when the battery cell 10 is depressurized, and the second groove 62 is configured to be able to guide at least a portion of the predetermined pressure relief area 63 to flip over to open at least a portion of the predetermined pressure relief area 63. The volume of the first groove 61 is V, and the sum of the areas of all the predetermined pressure relief areas 63 is A, which satisfies: 0.05mm≤V / A≤0.5mm, 82mm 3 ≤V≤450mm 3 , 160mm 2 ≤A≤1500mm 2.

[0368] Along the width direction Z of the second groove, the second groove 62 includes a first groove side surface 621 and a second groove side surface 622 which are arranged opposite to each other and connected to the inner surface of the pressure relief component 6. The first groove side surface 621 is closer to the predetermined pressure relief area 63 than the second groove side surface 622. The angle between the first groove side surface 621 and the inner surface of the pressure relief component 6 is a, and the angle between the second groove side surface 622 and the inner surface of the pressure relief component 6 is b, satisfying: 90°≤a<b<180°.

[0369] In such a battery cell 10, 0.05mm≤V / A≤0.5mm, which can not only improve the flatness of the surface of the first groove 61 of the pressure relief component 6, but also take into account the service life requirements of the battery cell 10 during normal use and the reliability requirements of the battery cell 10 during thermal runaway. a<b, so that the inclination angle of the first groove side 621 is smaller than that of the second groove side 622, which is equivalent to reducing the angle between the first groove side 621 and the second surface 65, which can reduce the amount of piled material in the predetermined pressure relief area 63 of the excess material squeezed out when forming the first groove 61, reduce the height of the piled material protrusion formed on the surface of the predetermined pressure relief area 63 due to the squeezing of the area where the first groove 61 of the pressure relief component 6 is set, and further improve the flatness of the surface of the first groove 61 of the pressure relief component 6.

[0370] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application may be combined with each other.

[0371] The features and performance of the present application are further described in detail below in conjunction with the embodiments.

[0372] The battery cells 10 in each embodiment and comparative example are prepared and tested according to the following method.

[0373] 1. Preparation of Battery Cell 10

[0374] 1. Preparation of positive electrode

[0375] The positive electrode active material LiNi 0.7 Co 0.1 Mn 0.1 O2, conductive agent Super P, and binder polyvinylidene fluoride (PVDF) are used to prepare positive electrode slurry in N-methylpyrrolidone (NMP), wherein the solid content in the positive electrode slurry is 50wt%, and the solid content of LiNi 0.7 Co 0.1 Mn 0.1The mass ratio of O2, Super P and PVDF is 8:1:1. The positive electrode slurry is coated on the upper and lower surfaces of the current collector aluminum foil and dried at 85°C and then cold pressed. Then, it is trimmed, cut and stripped, and then dried at 85°C under vacuum conditions for 4 hours to make the positive electrode sheet.

[0376] 2. Preparation of negative electrode

[0377] Graphite, conductive agent Super P, thickener carboxymethyl cellulose (CMC), and adhesive styrene butadiene rubber (SBR) are mixed evenly in deionized water to prepare a negative electrode slurry, wherein the solid content in the negative electrode slurry is 30wt%, and the mass ratio of graphite, silicon oxide, Super P, CMC and adhesive styrene butadiene rubber (SBR) in the solid component is 88:7:3:2. The negative electrode slurry is coated on the upper and lower surfaces of the current collector copper foil and dried at 85°C, and then cold pressed, trimmed, cut into pieces, and slit, and then dried at 120°C under vacuum conditions for 12 hours to prepare a negative electrode sheet.

[0378] 3. Preparation of Electrolyte

[0379] In an argon atmosphere glove box (H2O<0.1ppm, O2<0.1ppm), the fully dried electrolyte salt LiPF6 was dissolved in a mixed solvent (the mixed solvent included ethylene carbonate (EC) and diethyl carbonate (DEC), and ethylene carbonate (EC) and diethyl carbonate (DEC) were mixed in a mass ratio of 50:50), and after mixing evenly, a liquid electrolyte with a concentration of 1 mol / L was obtained.

[0380] 4. Isolation parts

[0381] A 16 μm polyethylene film was used as a separator.

[0382] 5. Preparation of Battery Cell 10

[0383] The positive electrode sheet, the separator, and the negative electrode sheet are stacked in order, and the separator is placed in the middle of the positive and negative electrode sheets to isolate the positive and negative electrodes. The electrode assembly 2 is wound and placed in an aluminum casing 1. The prepared electrolyte is injected into the dried casing 1, and the battery cell 10 is prepared by packaging, standing, forming, shaping, and capacity testing.

[0384] The battery cells 10 in each embodiment and comparative example are prepared by the above method. The battery cells 10 in each embodiment and comparative example are of the same chemical system. The difference between the battery cells 10 in each embodiment and comparative example is that the volume V of the first groove 61 and the sum A of the areas of all the predetermined pressure relief areas 63 on the first wall 13 are different. In each embodiment and comparative example, the outer shell 1 of the battery cell 10 is a rectangular parallelepiped structure, the shell 11 of the outer shell 1 is a structure with only one end having an opening, the shell 11 is made of aluminum alloy, the wall of the shell 11 opposite to the end cover 12 is the first wall 13, the first wall 13 serves as the pressure relief component 6, the first wall 13 is a rectangular wall, the first groove 61 is an H-shaped structure, and is a two-stage groove, the first groove 61 is arranged on the outer surface of the first wall 13, the second groove 62 is arranged on the inner surface of the first wall 13, and along the width direction of the first wall 13, the first groove 61 is located between the two second grooves 62.

[0385] 2. Performance parameter testing

[0386] 1. Method for measuring cycle fatigue number of battery cell 10

[0387] 1) Prepare a special test fixture. Specifically, the fixture includes three 10 mm steel plates (first steel plate, second steel plate, and third steel plate). Each steel plate can completely cover the large surface of the battery cell 10 (the outer surface of the shell 11 perpendicular to the width direction of the first wall portion 13). The first steel plate and the third steel plate are located at both ends of the fixture and are fixed by bolts. The second steel plate is located between the first steel plate and the third steel plate, and the second steel plate is constrained by a guide rail. The second steel plate can only move in translation along the thickness direction of the second steel plate.

[0388] 2) Install the battery cell 10 between the first steel plate and the second steel plate, place a support structure between the large surface of one side of the battery cell 10 and the first steel plate, and between the large surface of the other side and the second steel plate. The support structure can be an insulation pad or a water-cooling plate (consistent with the material / structure between two adjacent battery cells 10 in the actual battery 100). The support structure can be compressed to provide expansion space for the battery cell 10 during the charge and discharge cycle aging process; the large surface of the battery cell 10 is bonded to the support structure, the first steel plate is bonded to the corresponding support structure, the second steel plate is bonded to the corresponding support structure, and a pressure sensor is provided between the second steel plate and the third steel plate.

[0389] 3) The position of the second steel plate is adjusted by adjusting the pre-tightening force of the bolts, and the pressure sensor is observed so that the initial extrusion force on the battery cell 10 is 2000N, and the positive electrode terminal and the positive electrode terminal of the battery cell 10 are connected to the charging and discharging device.

[0390] 4) Place the battery cell 10 and the fixture in a constant temperature environment of 25±2°C, and start the test after the battery cell 10 reaches temperature equilibrium.

[0391] 5) The test steps are carried out in accordance with Chapter 6.4 "Standard Cycle Life" of "GBT31484-2015 Requirements and Test Methods for Cycle Life of Power Batteries for Electric Vehicles", and the test cycle end condition is changed to "stop the test until the first wall portion 13 is damaged at the first groove 61".

[0392] Specifically, test according to the following steps:

[0393] a) Discharge to 2.8v with 1I1(A) current;

[0394] b) Leave it for no less than 30 minutes;

[0395] c) Charge according to method 6.1.1.3 of GBT31484-2015 Cycle life requirements and test methods for power batteries for electric vehicles;

[0396] d) Leave it for no less than 30 minutes;

[0397] e) Discharge to 2.8v with a current of 1I1(A);

[0398] f) Repeat steps b) to e) until the first wall portion 13 where the first groove 61 is provided is damaged and the test is stopped.

[0399] That is, the test process continuously observes the area where the first groove 61 is set on the first wall portion 13 of the battery cell 10 until the area is damaged and leaks, and the number of cycles is recorded as the cycle fatigue number of the battery cell 10. The more cycle fatigue times the battery cell 10 has, the lower the probability of the battery cell 10 opening the valve and leaking due to gas production during long-term use, and the longer the service life.

[0400] 2. Thermal runaway test method for battery cell 10

[0401] 1. Select the heating plate according to the size of the battery cell 10. The size of the heating plate should cover as much surface of the battery cell 10 as possible (covering area ≥ 60%);

[0402] 2. Before testing, charge the battery cell 10 to 100% SOC and place the battery cell 10 in a constant temperature environment of 25±2°C;

[0403] 3. Sensor layout:

[0404] 1) Arrangement of temperature sensing wires: A layer of Teflon is attached to the center areas of the two large surfaces of the battery cell 10, a temperature sensing wire is arranged above the Teflon, and another layer of Teflon is attached;

[0405] 2) Arrangement of voltage sampling line: a layer of Teflon is attached to the positive electrode terminal of the battery cell 10, the positive electrode terminal and the housing 1, a voltage sampling line is arranged above the Teflon, and another layer of Teflon is attached;

[0406] 3) Air pipe arrangement: Drill a hole in the first wall portion 13 of the battery cell 10. The drilling position is located at the midpoint between the first groove 61 and the side surface of the shell 11 (the outer surface of the wall portion of the shell 11 adjacent to the first wall portion 13 along the length direction of the first wall portion 13). Extend the air pipe into the hole and seal it, and connect the air pipe to the air pressure sensor.

[0407] 4) Connect the temperature sensing wire, voltage sampling wire and air pressure sensor to the data acquisition instrument to collect and analyze data in real time. The collection frequency of the data acquisition instrument is ≤0.1S;

[0408] 4. Assembly fixture: The fixture completely covers the large surface of the battery cell 10 (the outer surface of the housing 11 perpendicular to the width direction of the first wall 13), the clamping force is 3000N, and the arrangement order of the fixture, heating plate and battery cell 10 is: fixture + heating plate + battery cell 10 + fixture;

[0409] 5. Test: Turn on the data acquisition instrument to collect temperature, voltage, and air pressure data, and then turn on the heating plate at a power of 500W to heat the battery cell 10 until the battery cell 10 thermally runs away.

[0410] 6. Obtaining the pressure holding time of the battery cell 10: Determine the thermal runaway moment and the valve opening moment according to the temperature, voltage and air pressure data collected by the data acquisition instrument, and obtain the pressure holding time of the battery cell 10 according to the pressure holding time = valve opening moment - thermal runaway moment.

[0411] Thermal runaway criteria: a) The trigger object generates a voltage drop, and the voltage drops to more than 25% of the initial voltage; b) The temperature at the detection point reaches the maximum operating temperature specified by the manufacturer; c) The temperature rise rate dT / dt at the detection point is ≥1℃ / s and lasts for more than 3s. When a) and c) or b) and c) occur, thermal runaway is determined and the thermal runaway moment is determined.

[0412] Valve opening time determination: When the air pressure drops by more than 25%, it can be determined that the valve is open (the first wall portion 13 is at least partially cracked along the first groove 61), and the moment when the air pressure begins to drop is the valve opening time. Both the valve opening time and the thermal runaway time can be obtained from the data logger.

[0413] 3. Method for measuring the flatness difference of the outer surface of the first wall portion 13

[0414] Four measuring points are taken on the outer surface of the first wall portion 13 in the area near the two ends along the length direction of the first wall portion 13 (the area is not provided with the first groove 61), and the flatness of the four measuring points is measured, and the average flatness of the four measuring points is calculated to obtain a reference value of the flatness. Then, two experimental points are taken on the outer surface of the first wall portion 13 at the predetermined pressure relief area 63 and close to the first groove section 611, the second groove section 612, and the third groove section 613, respectively, and the flatness of the six experimental points is measured, and the average flatness of the six experimental points is calculated to obtain an experimental value of the flatness, and finally the reference value is subtracted from the experimental value to obtain the flatness difference of the outer surface of the first wall portion 13.

[0415] 3. Test Results

[0416] The performance test results of the battery cells 10 in various embodiments and comparative examples are shown in Table 1, and are as follows:

[0417] Table 1

[0418]

[0419] As shown in Table 1, it can be seen from the comparison between Examples 1 to 17 and Comparative Examples 1 to 2 that when V / A ≥ 0.05 mm, the holding time of the battery cell 10 during thermal runaway is shorter, so that the bursting pressure of the battery cell 10 is lower, and the pressure release of the battery cell 10 during thermal runaway is more timely, which can reduce the risk of explosion of the battery cell 10 and improve the reliability of the battery cell 10. It can be seen from the comparison between Examples 1 to 17 and Comparative Examples 3 to 4 that when V / A ≤ 0.5 mm, the flatness difference of the outer surface of the first wall portion 13 (the surface of the first wall portion 13 where the first groove 61 is set) is small, which improves the flatness of the outer surface of the first wall portion 13, and the number of cycle fatigue of the battery cell 10 is large, which improves the fatigue resistance of the area where the first groove 61 is set on the first wall portion 13, and can effectively improve the service life of the battery cell 10.

[0420] From the comparison between Examples 4 to 9 and Examples 1 to 3, it can be seen that when V / A ≥ 0.1 mm, the holding time of the battery cell 10 during thermal runaway is shorter, and the pressure release of the battery cell 10 during thermal runaway is more timely, which can further improve the reliability of the battery cell 10. From the comparison between Examples 4 to 9 and Examples 10 to 17, it can be seen that when V / A ≤ 0.35 mm, the flatness of the outer surface of the first wall portion 13 is further improved, the number of cycle fatigue of the battery cell 10 is greater, and the service life of the battery cell 10 is further improved.

[0421] The above embodiments are only used to illustrate the technical solutions of the present application and are not used to limit the present application. For those skilled in the art, the present application may have various changes and variations. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present application shall be included in the protection scope of the present application. The above embodiments are only used to illustrate the technical solutions of the present application and are not used to limit the present application. For those skilled in the art, the present application may have various changes and variations. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present application shall be included in the protection scope of the present application.

Claims

1. A battery cell, characterized in that: include: The housing comprises a first wall portion, the first wall portion comprises a first groove and a second groove, along the thickness direction of the first wall portion, a projection of the first groove and a projection of at least one of the second grooves jointly define at least one predetermined pressure relief area, the first wall portion is configured to be split along at least a portion of the first groove when the battery cell is depressurized, and the second groove is configured to guide at least a portion of the predetermined pressure relief area to flip, so as to open at least a portion of the predetermined pressure relief area; The volume of the first groove is V, the sum of the areas of all the predetermined pressure relief zones is A, and the following condition is satisfied: 0.05 mm ≤ V / A ≤ 0.5 mm.

2. The battery cell according to claim 1, characterized in that: 0.1mm≤V / A≤0.35mm.

3. The battery cell according to claim 1, characterized in that: 82mm 3 ≤V≤450mm 3 。 4. The battery cell according to claim 3, characterized in that: 115mm 3 ≤V≤265mm 3 。 5. The battery cell according to claim 1, characterized in that: 160mm 2 ≤A≤1500mm 2 。 6. The battery cell according to claim 5, characterized in that: 400mm 2 ≤A≤1200mm 2 。 7. The battery cell according to claim 1, characterized in that: Along the thickness direction of the first wall portion, the first wall portion has a first surface and a second surface opposite to each other, and the second groove is recessed from the second surface toward the first surface; Along the width direction of the second groove, the second groove includes a first groove side surface and a second groove side surface that are oppositely arranged and connected to the second surface. The first groove side surface is closer to the predetermined pressure relief area than the second groove side surface. The angle between the first groove side surface and the second surface is a, and the angle between the second groove side surface and the second surface is b, satisfying: 90°≤a<b<180°, and the width direction of the second groove is perpendicular to the thickness direction of the first wall portion.

8. The battery cell according to claim 7, characterized in that: 90°≤a≤150°。 9. The battery cell according to claim 7, characterized in that: 90°<b≤170°。 10. The battery cell according to claim 1, characterized in that: The first wall portion is provided with a plurality of the second grooves. Along the thickness direction of the first wall portion, the projection of the first groove and the projections of the plurality of the second grooves jointly define a plurality of the predetermined pressure relief areas. Each of the predetermined pressure relief areas is provided corresponding to one or more of the second grooves.

11. The battery cell according to any one of claims 1 to 9, characterized in that: Along the thickness direction of the first wall portion, a projection of the second groove does not overlap with a projection of the first groove.

12. The battery cell according to claim 11, characterized in that: The second groove is spaced apart from the first groove along a width direction of the second groove, and the width direction of the second groove is perpendicular to a thickness direction of the first wall portion.

13. The battery cell according to any one of claims 1 to 9, characterized in that: Along the thickness direction of the first wall portion, two ends of the projection of the second groove along the extension direction respectively extend out of two end portions of the projection of the first groove.

14. The battery cell according to any one of claims 1 to 9, characterized in that: The minimum residual thickness of the first groove is D1, and the minimum residual thickness of the second groove is D2, satisfying: D1<D2.

15. The battery cell according to claim 14, characterized in that: Along the thickness direction of the first wall portion, the maximum groove depth of the first groove is H1, and the maximum groove depth of the second groove is H2, satisfying: H2<H1.

16. The battery cell according to any one of claims 1 to 9, characterized in that: Along the thickness direction of the first wall portion, the maximum groove depth of the first groove is H1, the thickness of the first wall portion is D, and 0.16≤H1 / D<1.

17. The battery cell according to claim 16, characterized in that: 0.4mm≤H1≤2mm, 0.8mm≤D≤2.5mm.

18. The battery cell according to claim 1, characterized in that: The first wall portion has a first surface and a second surface opposite to each other along a thickness direction of the first wall portion, the first groove is arranged on the first surface, and the second groove is arranged on the second surface.

19. The battery cell according to claim 18, characterized in that: Along the width direction of the second groove, the projection of the first groove at least partially overlaps with the projection of the second groove, and the width direction of the second groove is perpendicular to the thickness direction of the first wall portion.

20. The battery cell according to claim 18, characterized in that Along the thickness direction of the first wall portion, a groove bottom surface of the second groove is closer to the first surface than a groove bottom surface of the first groove.

21. The battery cell according to claim 18, characterized in that Along the thickness direction of the first wall portion, the maximum groove depth of the second groove is H2, and the minimum residual thickness of the first groove is D1, satisfying: D1<H2.

22. The battery cell according to claim 18, characterized in that The first groove comprises a plurality of grooves arranged in sequence along the direction from the first surface to the second surface, and along the thickness direction of the first wall portion, in two adjacent grooves, the first groove away from the first surface is arranged at the groove bottom surface of the first groove close to the first surface; Among them, the first-level groove in the multi-level groove arranged on the first surface is a first-level groove, and along the width direction of the second groove, the projection of the second groove at least partially overlaps with the projection of the first-level groove, and the width direction of the second groove is perpendicular to the thickness direction of the first wall portion.

23. The battery cell according to claim 22, characterized in that: Along the thickness direction of the first wall portion, the groove bottom surface of the second groove is flush with the groove bottom surface of the first-stage groove, or the groove bottom surface of the second groove is closer to the first surface than the groove bottom surface of the first-stage groove.

24. The battery cell according to claim 1, characterized in that: Along the thickness direction of the first wall portion, the first wall portion has a first surface and a second surface opposite to each other, and both the first groove and the second groove are recessed from the second surface toward a direction close to the first surface.

25. The battery cell according to claim 24, characterized in that The first groove comprises a plurality of grooves arranged in sequence along a direction from the second surface to the first surface, and along a thickness direction of the first wall portion, in two adjacent grooves, a primary groove away from the second surface is arranged at a groove bottom surface of a primary groove close to the second surface; Among them, the first-level groove in the multi-level grooves arranged on the second surface is a first-level groove, and along the thickness direction of the first wall portion, the groove bottom surface of the first-level groove is closer to the second surface than the groove bottom surface of the second groove.

26. The battery cell according to claim 25, characterized in that Along the thickness direction of the first wall portion, the maximum groove depth of the second groove is H2, and the maximum groove depth of the first-level groove is H3, satisfying: H3<H2.

27. The battery cell according to any one of claims 18 to 26, characterized in that: The first surface is a surface of the first wall portion facing the outside of the battery cell, and the second surface is a surface of the first wall portion facing the inside of the battery cell.

28. The battery cell according to any one of claims 1 to 9, characterized in that: Along the thickness direction of the first wall portion, the projection of the first groove, the projection of the second groove and the projection of the extension line of the second groove jointly enclose the predetermined pressure relief area; or Along the thickness direction of the first wall portion, the projection of the first groove, the projection of the extension line of the first groove and the projection of the second groove jointly enclose the predetermined pressure relief area; or Along the thickness direction of the first wall portion, the projection of the first groove, the projection of the extension line of the first groove, the projection of the second groove and the projection of the extension line of the second groove jointly enclose the predetermined pressure relief area.

29. The battery cell according to claim 28, characterized in that The first groove extends along an arc trajectory; and / or the second groove extends along a straight trajectory.

30. The battery cell according to any one of claims 1 to 9, characterized in that: The first groove comprises a first groove section and a second groove section, wherein the first groove section is connected to the second groove section; Along the thickness direction of the first wall portion, the projection of the first groove section, the projection of the second groove section, the projection of the second groove and the projection of the extension line of the second groove jointly enclose the predetermined pressure relief area; or Along the thickness direction of the first wall portion, the projection of the first groove segment, the projection of the extension line of the first groove segment, the projection of the second groove segment, the projection of the extension line of the second groove segment and the projection of the second groove jointly enclose the predetermined pressure relief area; or Along the thickness direction of the first wall portion, the projection of the first groove section, the projection of the extension line of the first groove section, the projection of the second groove section, the projection of the extension line of the second groove section, the projection of the second groove and the projection of the extension line of the second groove together enclose the predetermined pressure relief area.

31. The battery cell according to any one of claims 1 to 9, characterized in that: The first groove includes a first groove section, a second groove section and a third groove section, the second groove section and the third groove section are arranged opposite to each other, the first groove section connects the second groove section and the third groove section, and the first groove section and the second groove are arranged opposite to each other; Along the thickness direction of the first wall portion, the projection of the first slot segment, the projection of the second slot segment, the projection of the third slot segment, the projection of the second groove and the projection of the extension line of the second groove jointly enclose the predetermined pressure relief area; or Along the thickness direction of the first wall portion, the projection of the first groove segment, the projection of the second groove segment, the projection of the extension line of the second groove segment, the projection of the third groove segment, the projection of the extension line of the third groove segment and the projection of the second groove together enclose the predetermined pressure relief area; or Along the thickness direction of the first wall portion, the projection of the first groove section, the projection of the second groove section, the projection of the extension line of the second groove section, the projection of the third groove section, the projection of the extension line of the third groove section, the projection of the second groove and the projection of the extension line of the second groove together enclose the predetermined pressure relief area.

32. The battery cell according to claim 31, characterized in that The connection position between the second slot section and the first slot section deviates from the two ends of the second slot section, and the connection position between the third slot section and the first slot section deviates from the two ends of the third slot section, so that the predetermined pressure relief area is formed on both sides of the first slot section.

33. The battery cell according to claim 31, characterized in that The first slot segment extends along a straight line or an arcuate trajectory; and / or the second slot segment extends along a straight line or an arcuate trajectory; and / or the third slot segment extends along a straight line or an arcuate trajectory.

34. The battery cell according to claim 1, characterized in that: The first groove is stamped and formed on the first wall portion; and / or the second groove is stamped and formed on the first wall portion.

35. The battery cell according to any one of claims 1 to 9, characterized in that: The first wall portion is a rectangular wall portion, and the first groove and the second groove are arranged along a width direction of the first wall portion.

36. The battery cell according to any one of claims 1 to 9, characterized in that: The housing comprises: A shell having an opening formed at at least one end; An end cover, corresponding to each of the openings, and closing the openings; Wherein, at least one of the end covers is the first wall portion; and / or, at least one wall portion in the shell is the first wall portion.

37. The battery cell according to claim 36, characterized in that The opening is formed at only one end of the shell, and the wall portion of the shell opposite to the end cover is the first wall portion.

38. The battery cell according to claim 36, characterized in that The openings are formed at opposite ends of the shell, and at least one wall portion in the shell is the first wall portion.

39. The battery cell according to any one of claims 1 to 9, characterized in that: The material of the first wall portion includes steel.

40. The battery cell according to claim 39, wherein: The steel material is carbon steel or stainless steel.

41. The battery cell according to any one of claims 1 to 9, characterized in that: The material of the first wall portion includes aluminum alloy.

42. A battery, characterized in that: Comprising the battery cell according to any one of claims 1-41.

43. An electrical device, characterized in that: It comprises a battery cell as described in any one of claims 1 to 41, and the battery cell is used to provide electrical energy to the electrical device.

Citation Information

Cited By

  • Battery cell, battery device and electric device

    WO2026090928A1

  • Battery cell, battery, and electric device

    WO2026199101A1