Device for preventing edge tearing of ultrathin copper foil

By setting a second anode on the left and right sides of the electrolytic cell to increase the electric field to form a thickened layer, the problem of tearing the edge of the ultra-thin copper foil is solved, ensuring the stability of the thickness and width of the copper foil, and removing the excess thickened layer through the cutting device, realizing the Efficient rolling and secondary utilization of copper foil.

CN222119418UActive Publication Date: 2024-12-06GUANGDONG FINE YUAN SCI TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323439539.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-18
Publication Date
2024-12-06
Estimated Expiration
2033-12-18

AI Technical Summary

Technical Problem

Ultra-thin copper foil is prone to tear edges when peeled off the surface of the cathode roller, resulting in a reduced width and may cause a short circuit of the cathode roller, which in turn damages the equipment.

Method used

The second anode is arranged on the left and right sides of the electrolytic cell. By increasing the electric field, the copper foil forms a thickened layer at the outer edge of the cathode roller to avoid tearing the edges, and the excess thickened layer is removed by the cutting device to ensure that the size of the copper foil meets the standard. .

Benefits of technology

It effectively prevents the edge tearing of copper foil, ensures the stability of the thickness and width of copper foil, reduces cathode roller damage and copper waste, and achieves efficient rolling and 100% secondary utilization of copper foil.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222119418U_ABST
    Figure CN222119418U_ABST
Patent Text Reader

Abstract

The utility model discloses a device for preventing edge tearing of ultrathin copper foil, which relates to the field of copper foil production equipment and comprises an electrolytic bath, a first anode arranged at the bottom of the electrolytic bath, electrolyte filled in the electrolytic bath, a cathode roller partially immersed in the electrolyte and arranged at an interval with the first anode, and two second anodes arranged at the bottom of the electrolytic bath. The second anodes are located on the left side and the right side of part of the cathode roller immersed in the electrolyte respectively, are close to the outer edge of the cathode roller and can enable the copper foil to generate thickening layers on the two sides of the second anodes; and the second anode is fixedly arranged on the inner side wall of the electrolytic bath through a connecting rod. Second anodes are additionally arranged on the left side and the right side of a cathode roller in electrolyte, the second anodes increase the copper ion adsorption capacity of the outer edge of the cathode roller in a mode of increasing an electric field, in the rotating process of the cathode roller, the positions of the two sides of a copper foil become thick due to increase of the copper ion adsorption capacity, and the middle of the copper foil normally forms the needed copper foil thickness. Edge tearing of the copper foil is avoided by thickening the two sides of the copper foil to form the thickening layers.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of copper foil production equipment, in particular to a device for preventing edge tearing of ultra-thin copper foil. Background Art

[0002] In order to meet the needs of lithium batteries to increase energy density, copper foil is gradually developing in the direction of lightness and thinness. At present, the thickness of ultra-thin copper foil is generally 6um, 4um or even lower. When the thickness of copper foil is too low, edge tearing will occur. Edge tearing refers to when the copper foil is peeled off from the surface of the cathode roller, affected by the adhesion between the copper foil and the cathode roller, the copper foil is torn from both sides to the middle direction, resulting in a reduction in the width of the copper foil. At the same time, the remaining copper foil after edge tearing is still adhered to the surface of the cathode roller and rotates continuously with the cathode roller. It is easy to fall into the electrolyte and cause a short circuit between the cathode roller and the anode plate, and then break through the surface of the cathode roller, causing the cathode roller to be scrapped. When the thickness of the copper foil is greater than 6um, because the copper foil is thicker and the structural strength is relatively high, it can bear the adhesion between the copper foil and the cathode roller, and it is not easy to cause edge tearing.

[0003] In view of this, how to provide a device that can prevent the edge of ultra-thin copper foil from being torn is a technical problem that people in this field need to solve urgently. Utility Model Content

[0004] The utility model aims to provide a device for preventing edge tearing of ultra-thin copper foil, so as to solve the problems existing in the prior art.

[0005] To achieve the above object, the utility model provides the following solution: The utility model provides a device for preventing edge tearing of ultra-thin copper foil, comprising:

[0006] An electrolytic cell, wherein a first anode is disposed at the bottom of the electrolytic cell and the electrolytic cell is filled with an electrolyte;

[0007] a cathode roller, the cathode roller being partially immersed in the electrolyte and spaced apart from the first anode, the cathode roller being capable of rotating in the electrolyte;

[0008] The second anode has two parts, which are respectively located on the left and right sides of the cathode roller immersed in the electrolyte. The second anode is close to the outer edge of the cathode roller and is spaced apart from the first anode. The second anode can cause the copper foil to form thickened layers on both sides thereof. The second anode is fixed on the inner wall of the electrolytic cell by a connecting rod.

[0009] Preferably, the distance between the second anode and the outer edge of the cathode roller is 20-45 mm.

[0010] Furthermore, the second anode is adapted to the shape of the outer edge of the portion of the cathode roller immersed in the electrolyte.

[0011] Furthermore, the connecting rod is hollow inside and is provided with a connecting wire, and the second anode is connected to an external power source through the connecting wire.

[0012] Furthermore, it also includes: a stripping roller, which is arranged adjacent to the cathode roller. When the cathode roller rotates, the copper foil adhered to the surface of the cathode roller is stripped by the stripping roller and then led to the winding roller for winding.

[0013] Furthermore, it also includes a cutting device, which is arranged between the stripping roller and the curling roller, and the cutting device corresponds to the thickened layer and can cut the thickened layer from the copper foil.

[0014] Furthermore, the cutting device is a copper foil trimming air knife.

[0015] Furthermore, it also includes a recovery roller, and the thickened layer is rolled onto the recovery roller after being cut.

[0016] The utility model discloses the following technical effects:

[0017] 1. A second anode is added on the left and right sides of the cathode roller in the electrolyte. The second anode increases the copper ion adsorption capacity at the outer edge of the cathode roller (corresponding to the two sides of the copper foil) by increasing the electric field. During the rotation of the cathode roller, the copper foil on both sides becomes thicker due to the increase in the amount of copper ion adsorption, while the required copper foil thickness is formed normally in the middle. The copper foil tearing is avoided by forming a thickened layer on both sides of the copper foil.

[0018] 2. The distance between the second anode and the cathode roller can directly affect the width of the thickened layer. If the width of the thickened layer is too high, more material needs to be cut later. In order to ensure that the final width of the copper foil meets the standard, a larger cathode roller is required, and the cost will also increase; if the thickened layer is too narrow, it will be difficult to cut the thickened layer later. Therefore, the present application prefers that the distance between the second anode and the outer edge of the cathode roller is 20-45mm.

[0019] 3. The present invention removes the excess thickened layer before the copper foil is rolled up to ensure that the size of the copper foil after rolling up meets the standard. At the same time, the removed thickened layer is rolled up by a recovery roller and can be 100% reused after processing, without causing the problem of copper material waste. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0021] Figure 1 It is a schematic diagram of the overall structure of the utility model;

[0022] Figure 2 Schematic diagram of the internal structure of the electrolytic cell;

[0023] Figure 3 for Figure 2 Side view of

[0024] Among them, 1. electrolytic cell; 2. first anode; 3. electrolyte; 4. cathode roller; 5. second anode; 6. copper foil; 7. thickening layer; 8. connecting rod; 9. stripping roller; 10. winding roller; 11. cutting device; 12. recovery roller. DETAILED DESCRIPTION

[0025] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0026] In order to make the above-mentioned purposes, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods.

[0027] Reference Figure 1-Figure 3 The utility model provides a device for preventing the edge of ultra-thin copper foil from being torn, comprising: an electrolytic cell 1, a first anode 2 is arranged at the bottom of the electrolytic cell 1, and the electrolytic cell 1 is filled with an electrolyte 3; a cathode roller 4, the cathode roller 4 is partially immersed in the electrolyte 3 and is spaced apart from the first anode 2, and the cathode roller 4 can rotate in the electrolyte 3; there are two second anodes 5, which are respectively located on the left and right sides of the part of the cathode roller 4 immersed in the electrolyte 3, the second anode 5 is close to the outer edge of the cathode roller 4 and is spaced apart from the first anode 2, and the second anode 5 can make the copper foil 6 produce thickening layers 7 on both sides thereof; the second anode 5 is fixedly arranged on the inner wall of the electrolytic cell 1 through a connecting rod 8.

[0028] The distance between the second anode 5 and the outer edge of the cathode roller 4 can be 20-45 mm. Under the current conditions of the conventional ultra-thin copper foil 6 raw foil and the speed conditions of the cathode roller 4, when the distance between the second anode 5 and the outer edge of the cathode roller 4 is 20 mm, the generated thickened layer 7 is about 3 um thick and 20 mm wide, and when the distance between the second anode 5 and the outer edge of the cathode roller 4 is 45 mm, the generated thickened layer 7 is about 1 um thick and 5 mm wide. In this embodiment, the distance between the second anode 5 and the outer edge of the cathode roller 4 is 20 mm.

[0029] like Figure 2 and Figure 3 As shown, the second anode 5 is adapted to the outer edge shape of the portion of the cathode roller 4 immersed in the electrolyte 3. The connecting rod 8 is hollow inside and is provided with a connecting wire, and the second anode 5 is connected to the external power supply through the connecting wire. After being led out of the electrolytic cell 1, the connecting wire of the second anode 5 can be connected to the same power distribution cabinet together with the first anode 2, and form an independent circuit with the cathode roller 4 respectively.

[0030] In this embodiment, it also includes: a stripping roller 9, which is arranged adjacent to the cathode roller 4. When the cathode roller 4 rotates, the copper foil 6 adhered to the surface of the cathode roller 4 is stripped by the stripping roller 9 and then led to the winding roller 10 for winding.

[0031] In this embodiment, a cutting device 11 is further included. The cutting device 11 is disposed between the stripping roller 9 and the winding roller 10. The cutting device 11 corresponds to the thickened layer 7 and can cut the thickened layer 7 from the copper foil 6. The cutting device 11 is a copper foil trimming air knife.

[0032] In this embodiment, a recovery roller 12 is further included, and the thickened layer 7 is rolled onto the recovery roller 12 after being cut.

[0033] The specific working process is as follows:

[0034] Start the equipment. During the rotation of the cathode roller 4, the copper ions in the electrolyte 3 are continuously absorbed to form a copper foil 6 on the outer surface of the cathode roller 4. The second anode 5 increases the electric field at the outer edges of both sides of the cathode roller 4, so that a thickened layer 7 is generated on both sides of the copper foil 6. When the cathode roller 4 rotates to the stripping roller 9, the copper foil 6 is stripped from the cathode roller 4 to form a copper foil 6 with a thickness of 4um and a thickened layer 7 with a thickness of 3um.

[0035] The copper foil 6 moves along the stripping roller 9 toward the winding roller 10. When the copper foil 6 passes under the copper foil trimming air knife, the copper foil trimming air knife cuts off the thickened layer 7. The thickened layer 7 bends obliquely downward and is finally rolled into the recovery roller 12. The remaining copper foil 6 after removing the thickened layer 7 is the copper foil 6 that meets the thickness and width requirements, and is finally rolled into the winding roller 10.

[0036] It should be noted that the rotating mechanism of the cathode roller 4 and the stripping principle of the stripping roller 9 are the same as those in the existing foil production machine, and will not be described in detail in this embodiment.

[0037] In the description of the present invention, it should be understood that the terms "longitudinal", "lateral", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside" and "outside" etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention, and do not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as a limitation on the present invention.

[0038] The embodiments described above are only descriptions of the preferred methods of the present invention, and are not intended to limit the scope of the present invention. Without departing from the design spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary technicians in this field should fall within the protection scope determined by the claims of the present invention.

Claims

1. A device for preventing the edge of ultra-thin copper foil from being torn. It is characterized in that include: An electrolytic cell (1), wherein a first anode (2) is arranged at the bottom of the electrolytic cell (1), and the electrolytic cell (1) is filled with an electrolyte (3); a cathode roller (4), wherein the cathode roller (4) is partially immersed in the electrolyte (3) and is spaced apart from the first anode (2), and the cathode roller (4) is capable of rotating in the electrolyte (3); The second anode (5) has two second anodes (5), which are respectively located on the left and right sides of the cathode roller (4) immersed in the electrolyte (3). The second anode (5) is close to the outer edge of the cathode roller (4) and is spaced apart from the first anode (2). The second anode (5) can cause the copper foil (6) to produce thickened layers (7) on both sides thereof. The second anode (5) is fixedly arranged on the inner wall of the electrolytic cell (1) via a connecting rod (8).

2. A device for preventing edge tearing of ultra-thin copper foil according to claim 1, It is characterized in that The distance between the second anode (5) and the outer edge of the cathode roller (4) is 20-45 mm.

3. A device for preventing edge tearing of ultra-thin copper foil according to claim 1, It is characterized in that The second anode (5) is adapted to the outer edge shape of the portion of the cathode roller (4) immersed in the electrolyte (3).

4. A device for preventing edge tearing of ultra-thin copper foil according to claim 1, It is characterized in that The connecting rod (8) is hollow inside and is provided with a connecting wire, and the second anode (5) is connected to an external power source via the connecting wire.

5. A device for preventing edge tearing of ultra-thin copper foil according to claim 1, It is characterized in that Also includes: A stripping roller (9) is arranged adjacent to the cathode roller (4). When the cathode roller (4) rotates, the copper foil (6) adhered to the surface of the cathode roller (4) is stripped by the stripping roller (9) and then led to the winding roller (10) for winding.

6. A device for preventing edge tearing of ultra-thin copper foil according to claim 5, It is characterized in that It also comprises a cutting device (11), wherein the cutting device (11) is arranged between the stripping roller (9) and the curling roller (10), and the cutting device (11) corresponds to the thickened layer (7) and can cut the thickened layer (7) from the copper foil (6).

7. A device for preventing edge tearing of ultra-thin copper foil according to claim 6, It is characterized in that The cutting device (11) is a copper foil trimming air knife.