Anti-overturning photovoltaic welding strip delivery structure

By using auxiliary laminating tapes of PET or PE material with bright aluminum foil in the photovoltaic welding ribbon shipping structure, the problem of the welding ribbon turning over during the winding and unwinding process is solved, improving the welding quality and reducing the cost.

CN222387761UActive Publication Date: 2025-01-24SHENZHEN HUAGUANGDA TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420399019.7
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-01
Publication Date
2025-01-24
Estimated Expiration
2034-03-01

AI Technical Summary

Technical Problem

Photovoltaic welding tapes are easily flipped during rolling and unwinding, resulting in poor welding and bulging and fragmentation of the battery cells.

Method used

The anti-flip photovoltaic welding belt shipment structure is adopted, including the welding belt and the auxiliary laminating belt. The welding belt is close to the auxiliary laminating belt. The material of the auxiliary laminating belt is PET or PE, with bright aluminum foil, and the outer side of the aluminum foil. Painted in logo color.

Benefits of technology

Through the design of the auxiliary fit band, the structural resistance is strengthened, and the flipping of the welding zone during the collection and the volume of the welding zone is avoided, the welding quality is ensured, and the cost is reduced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222387761U_ABST
    Figure CN222387761U_ABST
Patent Text Reader

Abstract

The utility model provides an anti-overturning photovoltaic welding strip delivery structure which comprises a welding strip and an auxiliary attaching belt, the welding strip is tightly attached to the auxiliary attaching belt, the auxiliary attaching belt is made of PET or PE, the welding strip is attached to the PET belt through hot rolling, a bright aluminum foil is attached to the face, not attached to the welding strip, of the PET belt, and the face, facing outwards, of the aluminum foil is coated with marked colors. PET and PE are used as transparent materials, the bright aluminum foil is attached to one side, the photovoltaic welding strip is attached to the other side, light reflection of the bright aluminum foil facilitates visual inspection of a machine for whether the width of the welding strip changes or not, then whether the welding strip is turned over or not is judged, the anti-turning performance of the structure can be enhanced through the auxiliary attaching strip, the structure is not prone to turning over in the winding and unwinding process, and the service life of the structure is prolonged. The color of the mark coated on the outward surface of the aluminum foil can mark whether the welding strip is turned over or not, the welding strip is attached to the PET strip and the PE strip through hot rolling, the welding strip can be conveniently separated during use, meanwhile, the auxiliary attaching strip can be repeatedly used, and the cost is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of photovoltaics, and in particular to an anti-flipping photovoltaic welding belt delivery structure. Background Art

[0002] With the large-scale application of photovoltaic cells, the welding of photovoltaic ribbons is almost entirely completed by automated equipment. During the process of winding and unwinding the ribbon, the ribbon is prone to flipping, and the flipped part will bulge, which can easily cause poor welding and bulging and broken battery cells. Therefore, it is necessary to invent a new ribbon delivery structure to avoid flipping. Utility Model Content

[0003] In view of the deficiencies in the prior art, the present invention attempts to overcome the above defects, and thus provides an anti-flipping photovoltaic welding ribbon delivery structure, which prevents the welding ribbon from flipping by tightly attaching the welding ribbon to the auxiliary bonding tape.

[0004] To achieve the above purpose, the utility model is implemented through the following technical solutions: an anti-flip photovoltaic welding tape shipping structure, including a welding tape and an auxiliary bonding tape, the welding tape is tightly attached to the auxiliary bonding tape, the material of the auxiliary bonding tape is PET or PE, the welding tape is bonded to the auxiliary bonding tape by hot roller pressing, and the side of the auxiliary bonding tape that is not bonded to the welding tape is affixed with bright aluminum foil, and the outward side of the aluminum foil is painted with a logo color.

[0005] Furthermore, the thickness of the auxiliary bonding tape is 0.5-3 times the thickness of the welding tape.

[0006] Furthermore, the width of the auxiliary bonding tape is 1.5-3 times the width of the welding tape.

[0007] Compared with the prior art, the utility model has the following beneficial effects:

[0008] PET and PE are transparent materials, with bright aluminum foil attached to one side and photovoltaic welding tape attached to the other side. The reflection of the bright aluminum foil facilitates machine vision to check whether the width of the welding tape has changed, and then judge whether the welding tape has flipped. The auxiliary bonding tape can enhance the anti-flip performance of the structure, making it difficult to flip during the winding and unwinding process. The outer side of the aluminum foil is painted with a logo color to indicate whether the shipping structure has flipped. The welding tape is attached to PET and PE tapes by hot roller pressing, which is convenient for separating the welding tape when using it. At the same time, the auxiliary bonding tape can be reused to reduce costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] Figure 1 , a cross-sectional schematic diagram of the first embodiment,

[0010] In the figure: 1. Photovoltaic welding ribbon; 2. PET ribbon; 3. Aluminum foil. DETAILED DESCRIPTION

[0011] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0012] Embodiment 1, the utility model provides a photovoltaic welding ribbon delivery structure that prevents flipping, such as Figure 1 As shown, it includes a welding tape and an auxiliary bonding tape. The welding tape is tightly attached to the auxiliary bonding tape. The material of the auxiliary bonding tape is PET. The welding tape is bonded to the PET tape 2 by hot roller pressing. The side of the PET tape 2 that is not bonded to the welding tape is affixed with a bright aluminum foil 3. The side of the aluminum foil 3 facing outward is painted with a logo color. The thickness of the auxiliary bonding tape is 0.5-3 times the thickness of the welding tape, and the width of the auxiliary bonding tape is 1.5-3 times the width of the welding tape.

[0013] Embodiment 2, the utility model provides an anti-flip photovoltaic welding tape delivery structure, including a welding tape and an auxiliary bonding tape, the welding tape is tightly attached to the auxiliary bonding tape, the material of the auxiliary bonding tape is PE, the welding tape is bonded to the PE tape by hot roller pressing, the side of the PE tape that is not bonded to the welding tape is affixed with a bright aluminum foil 3, and the side of the aluminum foil 3 facing outwards is painted with a marking color, the thickness of the auxiliary bonding tape is 0.5-3 times the thickness of the welding tape, and the width of the auxiliary bonding tape is 1.5-3 times the width of the welding tape.

[0014] Working principle: PET and PE are transparent materials, with bright aluminum foil 3 attached to one side and photovoltaic welding tape 1 attached to the other side. The reflection of the bright aluminum foil 3 facilitates machine vision to check whether the width of the welding tape has changed, and then judge whether the welding tape has flipped. The auxiliary bonding tape can enhance the anti-flip performance of the structure, making it difficult to flip during the winding and unwinding process. The outer side of the aluminum foil 3 is painted with a marking color to indicate whether the shipping structure has flipped. The welding tape is bonded to PET and PE tapes by hot roller pressing, which is convenient for separating the welding tape when used. At the same time, the auxiliary bonding tape can be reused to reduce costs.

[0015] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A photovoltaic welding ribbon delivery structure that prevents flipping, characterized in that: The invention comprises a welding tape and an auxiliary bonding tape, wherein the welding tape is closely attached to the auxiliary bonding tape, the material of the auxiliary bonding tape is PET or PE, the welding tape is attached to the auxiliary bonding tape by hot roller pressing, the side of the auxiliary bonding tape not attached to the welding tape is attached with a bright aluminum foil (3), and the side of the aluminum foil (3) facing outward is painted with a logo color.

2. The anti-flip photovoltaic welding ribbon delivery structure according to claim 1, characterized in that: The thickness of the auxiliary bonding tape is 0.5-3 times the thickness of the welding tape.

3. The anti-flip photovoltaic welding ribbon delivery structure according to claim 1, characterized in that: The width of the auxiliary bonding tape is 1.5-3 times the width of the welding tape.