AMOLED panel module with glass coating film
By designing a ring-shaped frame, partitions, and protective components in the AMOLED panel module, the problem of glass cover breakage when dropped is solved, achieving optimization of glass cover protection and display effect. The protective components are replaceable, enhancing aesthetics.
Patent Information
- Application Number
- CN202423146978.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-12-19
- Publication Date
- 2025-12-16
- Estimated Expiration
- 2034-12-19
AI Technical Summary
The glass cover of the AMOLED display in wearable smart products is easily damaged when dropped, affecting the normal use of the display.
Design an AMOLED panel module with glass coating, including a ring-shaped frame, partitions, a photosensitive color-changing film layer, and protective elements. The protective elements provide support and cushioning when the glass cover is dropped, preventing direct contact with the ground.
It effectively protects the glass cover from damage, ensuring the normal operation of the AMOLED screen components. The light-sensitive color-changing film layer optimizes the display effect, and the protective component is replaceable, enhancing the aesthetics.
Smart Images

Figure CN223681451U_ABST
Abstract
Description
TECHNICAL FIELD
[0001] The utility model relates to AMOLED technical field especially relates to a kind of AMOLED panel module with glass coating. BACKGROUND
[0002] AMOLED, Chinese translation: active-matrix organic light-emitting diode or active-matrix organic light-emitting diode) is a kind of display screen technology.OLED (organic light-emitting diode) is a specific type of thin film display technology: organic electroluminescent display;AM (active-matrix body or called active matrix body) refers to the pixel addressing technology behind.
[0003] At present, wearable intelligent products also have many applications for AMOLED, such as smart watches with AMOLED display screens. Most of the outermost layers of conventional smart watches with AMOLED display screens are provided with glass cover plates for protecting the internal AMOLED display screens. However, since wearable devices need to be frequently removed and worn during daily use, there is a risk of falling during actual application. If a fall occurs, the glass cover plate may directly contact the ground and be damaged, thereby affecting the display of the AMOLED display screen or even causing the display to fail. Therefore, an AMOLED panel module with glass coating is proposed. SUMMARY
[0004] Therefore, it is necessary to provide an AMOLED panel module with glass coating for the above technical problems. The protective element is designed on the surface of the conventional wearable product, so that the glass cover plate can be supported when it falls to the ground, avoiding direct contact with the ground, which is beneficial to the protection of the AMOLED screen assembly.
[0005] To solve the above technical problems, the utility model adopts the following technical solutions:
[0006] An AMOLED panel module with glass coating includes an annular middle frame, a partition table extends inside the annular middle frame, an AMOLED screen assembly and a PCB control assembly are respectively located on the upper and lower sides of the partition table, a bottom cover is embedded and installed at the bottom of the annular middle frame, a glass cover plate is embedded and installed at the top of the annular middle frame, a light-sensitive color-changing film layer is provided between the glass cover plate and the AMOLED screen assembly, and a protective element is provided at the edge of the top of the annular middle frame to protect the glass cover plate.
[0007] Further, the partition table separates the annular middle frame into an upper mounting cavity and a lower mounting cavity.
[0008] The PCB control assembly is located in the lower mounting cavity, and the AMOLED screen assembly is located in the upper mounting cavity.
[0009] Further, the top of the AMOLED screen assembly is attached to an upper glass plate, and the light-sensing color-changing film layer is coated on the surface of the upper glass plate.
[0010] Further, the glass cover plate has a visible area corresponding to the opening at the top of the annular middle frame body, and a non-visible area outside the visible area on the glass cover plate is arranged on the top of the annular middle frame body and is bonded by optical glue.
[0011] The bottom of the non-visible area is printed with a black ink layer.
[0012] Further, the protection element comprises a threaded inner ring fixed to the outer side of the annular middle frame body, a threaded outer ring is threadedly assembled on the threaded inner ring, and a protection member is mounted on the threaded outer ring.
[0013] The top of the inner side of the threaded outer ring has a limiting boss, and the height of the limiting boss from the bottom of the threaded outer ring is greater than the height of the threaded inner ring.
[0014] Further, the protection member comprises a support ring body fixedly connected to one side of the top of the threaded outer ring, and the surface of the support ring body is wrapped with an annular rubber ring body.
[0015] Further, one end of the annular rubber ring body extends outwardly with a side protection portion, and the other end extends outwardly with a top protection portion, the top protection portion covers the connection between the glass cover plate and the annular middle frame body, and the side protection portion covers the bottom of the threaded outer ring.
[0016] Further, the end of the top protection portion has a top elastic convex rib, and the end of the side protection portion has a side elastic convex rib.
[0017] Further, an arc chamfer table is formed on the outer side of the annular rubber ring body, and a hollow deformation cavity is formed in the inner part of the annular rubber ring body corresponding to the arc chamfer table.
[0018] Further, the top elastic convex rib and the side elastic convex rib are both left with a gap between the corresponding glass cover plate and annular middle frame body.
[0019] Compared with the prior art, the present application has the following advantages:
[0020] The AMOLED panel module with glass coating provided by the utility model has the design of the protection element at the connecting position of the annular middle frame body and the glass cover plate, so that the glass cover plate can be protected when the wearable equipment falls, and the glass cover plate is prevented from being directly contacted with the ground to cause breakage and affect the normal use of the AMOLED screen assembly in the wearable equipment.
[0021] Through cooperation of the threaded inner ring and the threaded outer ring, the threaded outer ring can be rotated on the surface of the threaded inner ring, so that the threaded outer ring is separated from the threaded inner ring, and the protection element can be taken out and replaced.
[0022] Through the design of the side protection part and the top protection part, the connecting position between the glass cover plate and the annular middle frame body can be covered and protected, and when the glass cover plate on the module falls and is about to contact the ground, the glass cover plate can be supported, the side protection part and the top protection part are preferentially contacted with the ground, and the impact force during the falling is buffered, so that the AMOLED screen assembly in the wearable equipment is protected. BRIEF DESCRIPTION OF DRAWINGS
[0023] Figure 1 The utility model provides a structure schematic diagram of AMOLED panel module with glass coating provided by the utility model;
[0024] Figure 2 The utility model provides a part structure schematic diagram of AMOLED panel module with glass coating provided by the utility model;
[0025] Figure 3 The utility model provides a protection element structure schematic diagram of AMOLED panel module with glass coating provided by the utility model;
[0026] Figure 4 The utility model provides a protection element part structure schematic diagram of AMOLED panel module with glass coating provided by the utility model;
[0027] Figure 5 The utility model provides a support ring body structure schematic diagram of AMOLED panel module with glass coating provided by the utility model;
[0028] Figure 6 The utility model provides a threaded inner ring and threaded outer ring structure schematic diagram of AMOLED panel module with glass coating provided by the utility model.
[0029] Marking in the drawing is as follows:
[0030] Annular middle frame body 1, partition table 11, upper installation cavity 12, lower installation cavity 13, bottom cover 14;
[0031] AMOLED screen assembly 2, light-sensitive color film layer 21, upper glass 22;
[0032] PCB control assembly 3;
[0033] Glass cover plate 4, visible area 41, non-visible area 42, black ink layer 43;
[0034] Protection element 5, threaded inner ring 51, threaded outer ring 52, limiting boss 53, support ring body 54, annular rubber ring body 55, side protection part 56, top protection part 57;
[0035] Arc chamfer table 550, hollow deformation cavity 551;
[0036] Side elastic ribs 560;
[0037] Top elastic ribs 570. DETAILED DESCRIPTION
[0038] In order to make the person skilled in the art better understand the technical scheme of the present application, the technical scheme in the embodiments of the present application will be described clearly and completely below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only a part of the embodiments of the present application, not all the embodiments. Based on the embodiments in the present application, all other embodiments obtained by the person skilled in the art without creative labor should belong to the protection scope of the present application.
[0039] As described in the background, the conventional AMOLED wearable device is likely to cause the glass cover plate to directly contact the ground and be damaged when falling, thereby affecting the display of the AMOLED display screen or even unable to display.
[0040] In order to solve this technical problem, the present application provides an AMOLED panel module with glass coating, which is applied to an AMOLED module.
[0041] Specifically, please refer to Figures 1-6 As shown in the figure, the AMOLED panel module with glass coating specifically includes an annular middle frame body 1, a separation table 11 extends in the annular middle frame body 1, an AMOLED screen assembly 2 and a PCB control assembly 3 are respectively arranged on the upper and lower sides of the separation table 11, a bottom cover 14 is embedded and installed at the bottom of the annular middle frame body 1, a glass cover plate 4 is embedded and installed at the top of the annular middle frame body 1, a light-sensitive color-changing film layer 21 is arranged between the glass cover plate 4 and the AMOLED screen assembly 2, and a protection element 5 is further arranged at the edge of the top of the annular middle frame body 1 for protecting the glass cover plate 4.
[0042] The AMOLED panel module with glass coating provided by the utility model has the design of the protection element 5 at the connecting position of the annular middle frame body 1 and the glass cover plate 4, so that the glass cover plate 4 can be protected when the wearable device falls, and the glass cover plate 4 is prevented from being directly contacted with the ground to cause breakage and affect the normal use of the AMOLED screen assembly 2 in it.
[0043] In order for those skilled in the art to better understand the utility model scheme, the technical scheme in the utility model embodiment will be clearly and completely described below in combination with the drawings.
[0044] It should be noted that the embodiments in the utility model and the features and technical schemes in the embodiments can be combined with each other without conflict.
[0045] It should be noted that: similar signs and letters represent similar items in the following drawings, so once an item is defined in one drawing, it does not need to be further defined and explained in the subsequent drawings.
[0046] Embodiment one
[0047] Please refer to Figures 1-6 As shown in the figure, an AMOLED panel module with glass coating comprises an annular middle frame body 1, a partition table 11 extends in the annular middle frame body 1, an AMOLED screen assembly 2 and a PCB control assembly 3 are arranged on the upper and lower sides of the partition table 11 respectively, a bottom cover 14 is embedded and installed at the bottom of the annular middle frame body 1, a glass cover plate 4 is embedded and installed at the top of the annular middle frame body 1, a light-sensitive color-changing film layer 21 is arranged between the glass cover plate 4 and the AMOLED screen assembly 2, and a protection element 5 is arranged at the edge of the top of the annular middle frame body 1 for protecting the glass cover plate 4.
[0048] The annular middle frame body 1 in the embodiment is a circular shell of a conventional smart watch, and the protection element 5 is additionally arranged on the surface of the annular middle frame body 1 in the embodiment, so that when the glass cover plate 4 on the module falls towards the ground, the glass cover plate 4 can be prevented from directly contacting the ground, and the protection element 5 can play a supporting role to protect the glass cover plate 4 and the AMOLED screen assembly 2 in it.
[0049] Embodiment two
[0050] The AMOLED panel module with glass coating provided by embodiment one is further optimized, and specifically, as shown in the figure, the partition table 11 divides the annular middle frame body 1 into an upper mounting cavity 12 and a lower mounting cavity 13, wherein the PCB control assembly 3 is arranged in the lower mounting cavity 13, and the AMOLED screen assembly 2 is arranged in the upper mounting cavity 12. Figure 1
[0051] The top of the AMOLED screen assembly 2 is attached with an upper glass 22, and the light-sensitive color-changing film layer 21 is coated on the surface of the upper glass 22.
[0052] In this embodiment, due to the design of the light-sensitive color-changing film layer 21 above the AMOLED screen assembly 2, the molecular structure of the light-sensitive color-changing film layer 21 can change under the irradiation of light of different intensity or wavelength, thereby causing color change, for example, the originally transparent glass becomes dark in the environment with strong ultraviolet light, and the color returns to transparent or original state when the ultraviolet light becomes weak or disappears, so as to sharpen the details of the environment, optimize the color and weaken the interference by cooperating with the light-sensitive color-changing film layer 21, and finally achieve the experience of optimizing the picture for vision through the filtering and adjustment of light.
[0053] Embodiment Three
[0054] The AMOLED panel module with glass coating provided in Embodiment One or Two is further optimized, as shown in Figure 3 The glass cover plate 4 has a visible area 41 corresponding to the opening at the top of the annular middle frame body 1, and the area outside the visible area 41 on the glass cover plate 4 is a non-visible area 42, which is arranged on the top of the annular middle frame body 1 and bonded by optical glue, wherein the bottom of the non-visible area 42 is silk-screen printed with a black ink layer 43. Through the design of the non-visible area 42, the area on the glass cover plate 4 that does not need to display is uniformly formed black in cooperation with the annular middle frame body 1, so as to form the whole more beautiful and coordinated.
[0055] Embodiment Four
[0056] The AMOLED panel module with glass coating provided in Embodiment Three is further optimized, as shown in Figure 3 , Figure 4 and Figure 5 The protection element 5 includes a threaded inner ring 51 fixed to the outer side of the annular middle frame body 1, a threaded outer ring 52 threadedly assembled on the threaded inner ring 51, and a protection piece installed on the threaded outer ring 52.
[0057] The top of the inner side of the threaded outer ring 52 has a limiting boss 53, and the height of the limiting boss 53 from the bottom of the threaded outer ring 52 is greater than the height of the threaded inner ring 51.
[0058] The threaded outer ring 52 is rotated on the surface of the threaded inner ring 51, so that the threaded outer ring 52 can be separated, so that the threaded outer ring 52 and the protection piece thereon can be taken out on the annular middle frame body 1, so that the worn protection piece can be replaced in the actual use process to ensure the effect of drop protection.
[0059] Example Five
[0060] The AMOLED panel module with glass coating provided in Example Four is further optimized, as shown in Figure 3 、 Figure 4 and Figure 5 , the protective member includes a support ring body 54 fixedly connected to one side of the top of the threaded outer ring 52, and the surface of the support ring body 54 is wrapped with an annular rubber ring body 55;
[0061] One end of the annular rubber ring body 55 extends outward with a side protection portion 56, and the other end extends outward with a top protection portion 57, the top protection portion 57 covers the connection between the glass cover plate 4 and the annular middle frame body 1, and the side protection portion 56 covers the bottom of the threaded outer ring 52;
[0062] Through the design of the side protection portion 56 and the top protection portion 57, the connection between the glass cover plate 4 and the annular middle frame body 1 can be covered and protected, further improving the sealing protection effect of the glass cover plate 4 embedded in the connection, and at the same time, when the glass cover plate 4 on the module falls and is about to contact the ground, the glass cover plate 4 can be supported, so that the side protection portion 56 and the top protection portion 57 preferentially contact the ground and buffer the impact force during the fall, so as to meet the protection of the AMOLED screen assembly therein;
[0063] The end of the top protection portion 57 has a top elastic rib 570, and the end of the side protection portion 56 has a side elastic rib 560;
[0064] When the module falls and acts on the annular rubber ring body 55, the impact force received will cause the side protection portion 56 and the top protection portion 57 to tilt and deform to a certain extent, so that they will disperse the impact force through the gap formed between them and the middle frame body 1, and if the impact force is too large, the top elastic rib 570 and the side elastic rib 560 on the side protection portion 56 and the top protection portion 57 will finally act on the annular middle frame body 1, further dispersing the impact force;
[0065] The outer side of the annular rubber ring body 55 is formed with an arc chamfer table 550, and the inside of the annular rubber ring body 55 is formed with a hollow deformation cavity 551 corresponding to the arc chamfer table 550;
[0066] The top elastic rib 570 and the side elastic rib 560 leave a gap with the corresponding glass cover plate 4 and annular middle frame body 1, and through the design of the hollow deformation cavity 551, when the arc chamfer table 550 contacts the ground, the hollow deformation cavity 551 deforms to buffer the impact force during the fall, thereby comprehensively improving the protection effect of the protective member 5 on the module.
[0067] In the present application, unless otherwise expressly specified and limited, the terms "mounting", "connecting", "connecting", "fixing" and the like should be understood broadly, for example, it can be fixedly connected, or it can be detachably connected, or it can be integrated; it can be mechanically connected, or it can be electrically connected or communicate with each other; it can be directly connected, or it can be indirectly connected through an intermediate medium, it can be the internal communication of two elements or the interaction relationship of two elements, unless otherwise expressly limited. For ordinary skilled in the art, the specific meaning of the above terms in the present application can be understood according to the specific circumstances.
[0068] Obviously, the above-described embodiments are only a part of the embodiments of the present application, rather than all the embodiments, and the preferred embodiments of the present application are given in the drawings, but do not limit the patent scope of the present application. The present application can be realized in many different forms, and conversely, the purpose of providing these embodiments is to make the disclosure of the present application more thorough and comprehensive. Although the present application has been described in detail with reference to the foregoing embodiments, those skilled in the art can still modify the technical solutions recorded in the foregoing specific embodiments, or equivalently replace some of the technical features. Any equivalent structure made by using the content of the present application specification and drawings, directly or indirectly used in other related technical fields, is also within the patent protection scope of the present application.
Claims
1. A glass-coated AMOLED panel module, comprising a ring-shaped middle frame (1), a partition table (11) extending in the ring-shaped middle frame (1), an AMOLED screen assembly (2) and a PCB control assembly (3) respectively arranged on the upper and lower sides of the partition table (11), and a bottom cover (14) embedded and installed at the bottom of the ring-shaped middle frame (1), characterized in that, The top of the annular middle frame body (1) is embeddedly installed with a glass cover plate (4), a light-sensitive color-changing film layer (21) is arranged between the glass cover plate (4) and the AMOLED screen assembly (2), and a protection element (5) is further arranged at the edge of the top of the annular middle frame body (1) for protecting the glass cover plate (4). 2.The AMOLED panel module with glass coating according to claim 1, wherein, The annular middle frame body (1) is internally partitioned by the partition table (11) into an upper mounting cavity (12) and a lower mounting cavity (13). The PCB control assembly (3) is located in the lower mounting cavity (13), and the AMOLED screen assembly (2) is located in the upper mounting cavity (12). 3.The AMOLED panel module with glass coating according to claim 2, wherein, The top of the AMOLED screen assembly (2) is attached with an upper glass sheet (22), and the light-sensitive color-changing film layer (21) is coated on the surface of the upper glass sheet (22). 4.The AMOLED panel module with glass coating according to claim 1, wherein, The glass cover plate (4) has a visible area (41) corresponding to the opening at the top of the annular middle frame body (1), the area outside the visible area (41) on the glass cover plate (4) is a non-visible area (42), the non-visible area (42) is arranged on the top of the annular middle frame body (1) and is bonded by optical glue; The bottom of the non-visible area (42) is silk-screen printed with a black ink layer (43). 5.The AMOLED panel module with glass coating according to claim 1, wherein, The protection element (5) comprises a threaded inner ring (51) fixed to the outer side of the annular middle frame body (1), a threaded outer ring (52) threadedly assembled on the threaded inner ring (51), and a protection member mounted on the threaded outer ring (52). The top of the inner side of the threaded outer ring (52) has a limiting boss (53), and the height of the limiting boss (53) from the bottom of the threaded outer ring (52) is greater than the height of the threaded inner ring (51). 6.The AMOLED panel module with glass coating according to claim 5, wherein, The protection member comprises a support ring body (54) fixedly connected to one side of the top of the threaded outer ring (52), and the surface of the support ring body (54) is wrapped with an annular rubber ring body (55). 7.The AMOLED panel module with glass coating according to claim 6, wherein, One end of the annular rubber ring body (55) extends outwardly with a side protection portion (56), and the other end extends outwardly with a top protection portion (57), the top protection portion (57) covers the connection between the glass cover plate (4) and the annular middle frame body (1), and the side protection portion (56) covers the bottom of the threaded outer ring (52). 8.The AMOLED panel module with glass coating according to claim 7, wherein, The end of the top protection portion (57) has a top elastic convex rib (570), and the end of the side protection portion (56) has a side elastic convex rib (560). 9.The AMOLED panel module with glass coating according to claim 8, wherein, The outer side of the annular rubber ring body (55) forms an arc chamfer table (550), and the inner side of the annular rubber ring body (55) forms a hollow deformation cavity (551) corresponding to the arc chamfer table (550). 10.The AMOLED panel module with glass coating of claim 8, wherein, The top elastic convex rib (570) and the side elastic convex rib (560) each have a gap with the corresponding glass cover plate (4) and annular middle frame body (1).