Friction stir welding device
By designing a tapered stirring section and a spiral groove structure in the friction stir welding device, the problems of hook-shaped defects and stirring pin breakage in friction stir welding were solved, achieving higher welding quality and stirring pin reliability.
Patent Information
- Application Number
- CN202520676359.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-04-10
- Publication Date
- 2026-04-17
- Estimated Expiration
- 2035-04-10
AI Technical Summary
During friction stir welding, the asymmetric plastic flow caused by the rotation and axial movement of the stirring pin forms hook-shaped defects, which reduces the welding quality and the working reliability of the stirring pin. Especially when welding high-strength aluminum alloys or dissimilar metals, the stirring pin is prone to breakage, affecting process stability and tool life.
The design of the stirring pin adopts a gradually decreasing cross-section of the first stirring section and a constant cross-section of the second stirring section. Combined with the spiral groove and arc-shaped outer peripheral wall structure, it improves the uniformity of material flow, reduces stress concentration, and improves welding quality and structural strength of the stirring pin.
It improves the hook-shaped defects in friction stir welding, enhances the working reliability and service life of the stirring pin, and improves the welding quality and fatigue resistance.
Smart Images

Figure CN224128823U_ABST
Abstract
Description
Technical Field
[0001] This application relates to the field of welding technology, and in particular to a friction stir welding apparatus. Background Technology
[0002] Friction stir welding (FSW), as a solid-state joining technology, utilizes the frictional heat generated by a high-speed rotating stirring pin against the workpiece to induce localized plasticity in the material, forming a dense metallurgical weld under mechanical stirring and forging pressure. Compared to traditional fusion welding, its significant advantages lie in the fact that the material does not reach its melting point during welding, avoiding metallurgical defects such as porosity and slag inclusions common in traditional fusion welding. Furthermore, it features low residual stress and minimal welding deformation, making it highly popular in precision welding of lightweight materials such as aluminum alloys and magnesium alloys, as well as in joining dissimilar materials.
[0003] However, in the penetration welding process of friction stir welding, the asymmetric plastic flow at the lap interface induced by the rotation and axial movement of the stirring pin (on the advancing side, the material is dominated by upward shear force because the tangential direction of the stirring pin rotation is consistent with the welding direction; while on the retreating side, the material is dominated by downward shear force because the tangential direction of the rotation is opposite to the welding direction, resulting in a difference in plastic metal flow between the advancing and retreating sides) leads to the formation of hook-shaped defects at the interface on both sides of the weld nugget. These hook-shaped defects manifest as local warping of the lap interface. This warping not only reduces the effective load-bearing thickness of the workpiece but also easily forms a stress concentration source at the lap interface, becoming a preferred path for crack initiation and propagation under cyclic loading, severely weakening the fatigue performance and static mechanical strength of the joint. Furthermore, the stirring pin in the penetration welding process must withstand higher thermo-mechanical coupling loads, especially when welding high-strength aluminum alloys or dissimilar metals. The stirring pin is prone to fracture failure due to local stress concentration and thermal softening effects, leading to decreased process stability and reliability, and shortened tool life. Therefore, improving the hook-shaped defects in friction stir welding and enhancing the operational reliability of the stirring pin is of great significance. Utility Model Content
[0004] This application provides a friction stir welding apparatus that can improve the working reliability of the stirring pin while improving the hook-shaped defects in friction stir welding.
[0005] To achieve the above objectives, the embodiments of this application adopt the following technical solutions:
[0006] This application provides a friction stir welding apparatus, which includes a frame, a drive unit connected to the frame, a stirring head connected to the drive unit, and a platform for placing the workpiece to be welded. The drive unit is used to drive the stirring head to rotate. The stirring head includes a connector and a stirring pin connected to the connector. The connector protrudes towards the outer periphery of the stirring pin, and the surface of the connector facing the stirring pin is used to abut the workpiece to be welded.
[0007] The stirring needle includes a first stirring section and a second stirring section. The first stirring section is fixed between the second stirring section and the connector. Along the direction from the first stirring section to the second stirring section, the cross-section of the first stirring section gradually decreases, while the cross-section of the second stirring section remains unchanged.
[0008] In the friction stir welding apparatus disclosed in this application, the stirring pin is configured as a first stirring section and a second stirring section, and the cross-section of the first stirring section gradually decreases along the direction from the first stirring section to the second stirring section, while the cross-section of the second stirring section remains unchanged. Thus, when using the friction stir welding apparatus to perform through-welding of a workpiece including a first workpiece and a second workpiece, part of the second stirring section extends into the upper second workpiece and another part extends into the lower first workpiece. Due to the axisymmetric characteristic of its diameter (i.e., the radial dimension of the second stirring section remains constant along the arrangement direction of the first and second stirring sections, and the second stirring pin exhibits axisymmetry), the material contact interface of the second stirring section maintains circumferential continuity during rotation, avoiding periodic cross-sectional changes caused by diameter variations. This results in a more uniform distribution of shear rate and contact pressure when the plastic material flows circumferentially along the second stirring section. This geometric continuity weakens the shear force vector offset caused by the difference in tool rotation direction between the advancing and retreating sides. This allows the softened plastic material to form a stable viscoplastic laminar flow under the forging pressure at the connection between the connector and the first stirring section (i.e., at the shoulder), improving the kinetic energy accumulation or eddy separation phenomenon caused by sudden changes in local flow velocity. Simultaneously, the uniform diameter structure maintains a constant axial migration channel cross-sectional area, reducing the kinetic-potential energy conversion imbalance caused by cross-sectional contraction or expansion along the flow path, thus reducing the tendency for material accumulation on the advancing side induced by local energy accumulation. The mechanical structural characteristics of the second stirring section, combined with the continuous forging pressure of the shoulder, distribute plastic deformation energy more evenly across the weld cross-section, thereby reducing the upward accumulation of plastic material on the advancing side, improving hook-shaped defects caused by asymmetric accumulation of plastic material at the weld interface, and reducing the risk of interface warping.
[0009] Furthermore, this application, by gradually reducing the cross-section of the first stirring section connected between the second stirring section and the connector, allows for the gradual axial release of stress at the connection between the connector and the stirring pin. This reduces stress concentration at the connection point, improves the fatigue resistance of the stirring head, and reduces the lateral resistance experienced by the stirring pin during rotation, compression, and movement. This reduces the torque borne by the stirring pin, increases its overall structural strength, and lowers the risk of breakage during welding. Through these design features, this application improves the hook-like defects in friction stir welding while enhancing the reliability and service life of the stirring pin.
[0010] In one feasible embodiment, the workpieces to be welded include a first workpiece and a second workpiece, with the second workpiece located on the side of the first workpiece facing away from the stage. The surface of the connector facing the stirring pin is used to abut against the second workpiece; in the arrangement direction of the first and second stirring sections, the sum of the dimensions of the first and second stirring sections is greater than the dimension of the second workpiece, and the dimension of the first stirring section is smaller than the dimension of the second workpiece.
[0011] With the above-described configuration, during friction stir welding, the surface of the connector facing the stirring pin abuts against the second workpiece. The first stirring section extends into the second workpiece, a portion of the second stirring section extends into the second workpiece, and the other portion extends into the first workpiece. Thus, the second stirring section is located at the lap joint of the first and second workpieces, enabling it to play a primary stirring role. Using a second stirring section with a constant radial dimension can improve hook-like defects, reduce warping at the weld interface, and improve weld quality.
[0012] In one possible implementation, the end face of the first stirring section facing the second stirring section coincides with the end face of the second stirring section facing the first stirring section. By aligning the end faces as described above, this application can mitigate the abrupt change in radial dimensions between the first and second stirring sections, improve stress concentration at the connection between the first and second stirring sections, and enhance the structural strength of the stirring pin.
[0013] In one possible implementation, the stirring needle further includes a third stirring section fixed between the first and second stirring sections; the cross-section of the third stirring section gradually decreases along the direction from the first stirring section to the second stirring section. The end face of the third stirring section facing the first stirring section coincides with the end face of the first stirring section facing the third stirring section; the end face of the third stirring section facing the second stirring section coincides with the end face of the second stirring section facing the third stirring section.
[0014] This application provides a third stirring section located between the first and second stirring sections, and ensures that the third stirring section meets the above conditions. In this way, the third stirring section can serve as a transition between the first and second stirring sections, allowing the first stirring section to smoothly transition to the second stirring section after passing through the third stirring section. This can improve the stress concentration phenomenon at the connection between different stirring sections and enhance the structural strength of the stirring pin.
[0015] In one feasible embodiment, the first stirring section is frustum-shaped, and the second stirring section is cylindrical. This application achieves this by making the first and second stirring sections frustum-shaped and cylindrical, respectively, which not only improves hook-shaped defects and enhances welding quality but also facilitates manufacturing and reduces the difficulty of preparing the stirring pin.
[0016] In one possible implementation, the outer peripheral wall of the first stirring section and / or the outer peripheral wall of the second stirring section are provided with spiral grooves that spiral along the arrangement direction of the first and second stirring sections.
[0017] This application incorporates spiral grooves on the outer peripheral walls of the first and / or second stirring sections. During welding, the centrifugal pump effect generated by these spiral grooves allows the softened plastic material to be transported along the spiral trajectory of the grooves, promoting the migration and filling of thermoplastic material from the front to the rear of the stirring pin, forming a continuous material flow layer. Furthermore, the geometric features of the spiral grooves increase the contact area between the stirring pin and the material, enhancing local heat input efficiency through frictional shearing, accelerating material plasticization, and refining dynamically recrystallized grains, thereby improving the tensile strength of the joint.
[0018] In one possible implementation, the outer peripheral wall of the first stirring section and / or the outer peripheral wall of the second stirring section includes multiple planes and multiple arc surfaces, which are arranged alternately along the circumference of the stirring pin.
[0019] This application employs multiple planar surfaces. The planar areas utilize sharp edges to directionally cut and break up the oxide film on the base material of the workpiece to be welded. Multiple curved surfaces, through a curvature-induced centrifugal force gradient field, drive the softened plastic material to flow in layers, forming a continuous material migration layer. The alternating arrangement of planar and curved surfaces creates a periodic shear-extrusion composite field during the rotation of the stirring pin, refining the dynamically recrystallized grains. Thus, the combined planar and curved surface design of the stirring pin's outer peripheral wall improves welding quality through multi-dimensional mechanical coupling.
[0020] In one feasible approach, multiple arc surfaces each have multiple first grooves, the arrangement of which is parallel to the arrangement of the first stirring section and the second stirring section.
[0021] This application incorporates multiple first grooves on an arc surface. These grooves generate localized turbulent fields during rotation, enhancing the radial-axial composite flow of the softened plastic material and increasing its migration rate. Furthermore, the micro-shearing effect generated at the edges of the first grooves further breaks down oxide film particles. The plastic material accumulated within the first grooves undergoes periodic micro-forging under rotational extrusion, promoting further refinement of the dynamic recrystallized grain size and thus improving the fatigue resistance of the welded joint.
[0022] In one possible implementation, the end face of the second stirring section opposite to the first stirring section has a protrusion; the cross-section of the protrusion gradually decreases along the direction from the first stirring section toward the second stirring section.
[0023] Along the direction from the first stirring section to the second stirring section, the cross-section of the protrusion gradually decreases, which means that the protrusion gradually becomes sharper from the first stirring section to the second stirring section. In this way, the protrusion is designed to facilitate penetration of the workpiece to be welded and reduce penetration resistance during penetration welding.
[0024] In one feasible manner, along the arrangement direction of the first and second stirring sections, the protrusion facing the end face of the second stirring section coincides with the end face of the second stirring section away from the first stirring section.
[0025] Through the above-mentioned configuration, this application enables a smooth and uniform transition at the connection between the second stirring section and the protrusion, thereby improving the stress concentration phenomenon at the connection between the second stirring section and the protrusion. Attached Figure Description
[0026] Figure 1 This is a schematic diagram of the structure of the friction stir welding apparatus provided in the embodiments of this application;
[0027] Figure 2 A schematic diagram of the rotating shaft, stirring head, and workpiece to be welded provided in an embodiment of this application;
[0028] Figure 3 This is a schematic diagram of the structure of the stirring head and the workpiece to be welded provided in the embodiments of this application;
[0029] Figure 4 This is one of the structural schematic diagrams of the stirring head provided in the embodiments of this application;
[0030] Figure 5 This is a second schematic diagram of the structure of the stirring head provided in the embodiments of this application;
[0031] Figure 6 for Figure 5 A bottom view of the stirring head in the middle;
[0032] Figure 7 This is the third schematic diagram of the structure of the stirring head provided in the embodiments of this application;
[0033] Figure 8 This is one of the metallographic microstructure images obtained after friction stir welding using a conical stirring needle;
[0034] Figure 9 The second image shows the metallographic microstructure obtained after friction stir welding using a conical stirring needle.
[0035] Figure 10 One of the metallographic microstructure images obtained after friction stir welding using the friction stir welding apparatus provided in the embodiments of this application;
[0036] Figure 11The second metallographic microstructure image obtained after friction stir welding using the friction stir welding apparatus provided in this application embodiment.
[0037] Figure label:
[0038] 100 - Friction stir welding device;
[0039] 10-Rack;
[0040] 21-Drive component; 22-Rotating shaft;
[0041] 30-Stirring head; 31-Connector; 311-Second groove; 32-Stirring needle; 321-First stirring section; 322-Second stirring section; 323-Third stirring section; 324-Spiral groove; 33-Flat surface; 34-Arc surface; 341-First groove; 35-Protrusion;
[0042] 40 - Stage;
[0043] 50 - Workpiece to be welded; 51 - First workpiece; 52 - Second workpiece; a - First direction; b - Second direction. Detailed Implementation
[0044] The technical solutions of the embodiments of this application will be clearly and completely described below with reference to the accompanying drawings. Obviously, the described embodiments are only some embodiments of this application, not all embodiments. Based on the embodiments of this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.
[0045] The terms "first," "second," and similar terms used in this article do not indicate any order, quantity, or importance, but are merely used to distinguish different components. Similarly, "one" or similar terms do not indicate a quantity limitation, but rather indicate the existence of at least one.
[0046] In the embodiments of this application, the words "exemplarily" or "for example" are used to indicate examples, illustrations, or descriptions. Any embodiment or design described as "exemplarily" or "for example" in the embodiments of this application should not be construed as being more preferred or advantageous than other embodiments or design solutions. Specifically, the use of the words "exemplarily" or "for example" is intended to present the relevant concepts in a specific manner. In the description of the embodiments of this application, unless otherwise stated, "a plurality of" means two or more.
[0047] To facilitate understanding of the embodiments of this application, the technical terms involved in this application will be explained before the embodiments are described in detail.
[0048] 1. Advancing Side (AS): The weld is divided into two sides by the centerline of the friction stir weld, namely the advancing side and the retreating side. The advancing side and the retreating side are determined by the rotation direction and the advancing direction of the welding tool. On the advancing side of the weld, the rotation direction of the welding tool is usually the same as the advancing direction of the welding tool.
[0049] 2. Retreating Side (RS): On the retreating side of the weld, the direction of rotation of the welding tool is usually opposite to the direction of advance of the welding tool.
[0050] 3. Weld Nugget Zone (WNZ): Located in the center of the weld, this is the area subjected to intense stirring during friction stir welding. Within this zone, the material undergoes significant plastic deformation and dynamic recrystallization, ultimately forming a microstructure with fine, equiaxed grains.
[0051] This application provides a friction stir welding apparatus 100, which can be applied to metal sheet welding scenarios in fields such as new energy, aerospace, and rail transportation, and is particularly suitable for through-welding processes of lightweight materials such as aluminum alloys and magnesium alloys. For example, the friction stir welding apparatus 100 can be used for welding large die-cast parts, forgings, or profiles; or, it can be used for internal or external welding of liquid-cooled electronic control housings; or, it can be used for welding on liquid-cooled radiators.
[0052] The friction stir welding device 100 achieves solid-state connection through the synergistic effect of mechanical stirring and frictional heat generation, which can effectively avoid defects such as porosity and cracks in traditional fusion welding processes, and shows significant technical advantages in thin plate welding and dissimilar metal connection. Figure 1 For a schematic diagram of the friction stir welding apparatus 100 provided in this application embodiment, please refer to... Figure 1 The friction stir welding apparatus 100 of this application includes a frame 10, a drive system, and a stirring head 30, etc.
[0053] For example, rack 10 can adopt a frame structure, or it can adopt a structure such as... Figure 1 The column-like structure shown, frame 10, is used to support or fix the various components of the friction stir welding apparatus 100, providing stable mechanical support for the welding process. The drive system is used to drive and control the stirring head 30 through servo motors and transmission mechanisms, so as to achieve precise positioning of the stirring head 30 and the workpiece 50 to be welded, and to provide a constant feed speed for the stirring head 30.
[0054] For example, the friction stir welding apparatus 100 also includes a pressure control system for monitoring and adjusting the welding pressure in real time to avoid welding defects caused by pressure fluctuations.
[0055] For example, the friction stir welding apparatus 100 also includes a rotating shaft 22. The stirring head 30, a core functional component of the friction stir welding apparatus 100, is fixedly connected to the rotating shaft 22. The drive system includes a drive component 21 for driving the stirring head 30 to rotate. The drive component 21 of the drive system drives the rotating shaft 22 to rotate, thereby causing the stirring head 30 to rotate. The stirring head 30 can be detachably installed within the rotating shaft 22. This detachable installation allows for quick replacement of the stirring head 30, enabling it to adapt to the welding requirements of plates of different thicknesses.
[0056] The stirring head 30 has a shoulder and a stirring pin 32. The diameter of the shoulder is designed according to the thickness of the workpiece to be welded. In the penetration welding process, the stirring pin 32 needs to completely penetrate the upper workpiece 50 to be welded and partially insert into the lower workpiece 50 to be welded. This deep-penetration operation places stringent requirements on the structural strength of the stirring head 30 and the distribution of shear force on the material by the stirring head 30. In practical applications, it has been found that traditional stirring heads 30 are prone to hook-shaped defects on both sides of the weld nugget during penetration welding, and the stirring pin 32 is prone to pin breakage during operation. Based on this, the new friction stir welding device 100 proposed in this application optimizes the structure of the stirring pin 32, which can improve the hook-shaped defects in friction stir welding while improving the working reliability of the stirring pin 32.
[0057] The following application will provide a detailed description of the specific structure of the friction stir welding apparatus 100.
[0058] Figure 2 This is a schematic diagram of the structure of the rotating shaft 22, stirring head 30, and workpiece 50 to be welded provided in the embodiments of this application. Please refer to the following: Figure 1 and Figure 2 The friction stir welding apparatus 100 includes a frame 10, a drive unit 21 connected to the frame 10, a stirring head 30 connected to the drive unit 21, and a platform 40 for placing the workpiece 50 to be welded. The drive unit 21 is used to drive the stirring head 30 to rotate.
[0059] Among them, the frame 10 can be a frame structure or a [type of frame structure]. Figure 1 The column-shaped structure shown in this application does not limit the structural form of the frame 10, as long as the frame 10 can support or fix the corresponding components of the friction stir welding device 100 and can meet the strength requirements.
[0060] The driving component 21 is used to drive the stirring head 30 to rotate. The driving component 21 can drive the stirring head 30 directly or indirectly. This application does not limit the driving form or specific structural form of the driving component 21. For example, the driving component 21 can be a combination of a servo motor and a transmission mechanism, or a combination of a hydraulic cylinder or a pneumatic cylinder and a transmission mechanism.
[0061] The stage 40 is used to support the workpiece 50 to be welded. The stage 40 can be fixed relative to the frame 10 or movable relative to the frame 10 (for example, the stage 40 can move relative to the frame 10 along the length of the weld). For example, when performing friction stir welding, if the stirring head 30 needs to move along the length of the weld to be formed under the driving action of the drive system, then the stage 40 is fixed relative to the frame 10; if the stirring head 30 does not need to move along the length of the weld to be formed, then the stage 40 moves along the length of the weld to be formed under the driving action of the drive system.
[0062] Additionally, as an example, the stage 40 is provided with a clamping mechanism for clamping the workpiece 50 to be welded, so as to fix the workpiece 50 to be welded on the stage 40 and prevent the workpiece to be welded from shifting during the welding process.
[0063] For example, the stage 40 can be a conveyor belt or a support plate, etc.
[0064] For example, the friction stir welding apparatus 100 also includes a rotating shaft 22, and a stirring head 30 is detachably connected to the rotating shaft 22 (e.g., the stirring head 30 is threaded into the rotating shaft 22). The drive member 21 drives the rotating shaft 22 to rotate, which in turn drives the stirring head 30 to rotate. The detachable installation of the stirring head 30 allows for quick replacement of the stirring head 30, so that different specifications of stirring heads 30 can be replaced according to the welding requirements of plates of different thicknesses, thereby improving the versatility of the friction stir welding apparatus 100.
[0065] In some embodiments, the stirring head 30 includes a connector 31 and a stirring pin 32 connected to the connector 31. The connector 31 protrudes toward the outer periphery of the stirring pin 32, and the surface of the connector 31 toward the stirring pin 32 is used to abut against the workpiece 50 to be welded.
[0066] The surface of the connector 31 protruding towards the outer periphery of the stirring pin 32 serves to abut against the workpiece 50 to be welded. The side of the connector 31 facing the stirring pin 32 forms a shoulder of the stirring head 30, which generates heat through high-speed friction with the surface of the workpiece 50 during welding, thereby increasing the temperature of the welding area and creating sufficient heat input to maintain plastic deformation of the material and promote metallurgical bonding. Furthermore, the shoulder applies axial pressure during welding to confine the softened plastic material within the weld area, preventing material from overflowing from the surface.
[0067] The stirring needle 32 includes a first stirring section 321 and a second stirring section 322. The first stirring section 321 is fixed between the second stirring section 322 and the connecting member 31. Along the direction from the first stirring section 321 to the second stirring section 322, the cross-section of the first stirring section 321 gradually decreases, while the cross-section of the second stirring section 322 remains unchanged.
[0068] Wherein, the cross-section of the first stirring section 321 refers to the cross-section of the first stirring section 321 along the first direction a, and the cross-section of the second stirring section 322 refers to the cross-section of the second stirring section 322 along the first direction a. The first direction a is perpendicular to the arrangement direction of the first stirring section 321 and the second stirring section 322 (i.e., the second direction b). That is, the first direction a is the radial direction of the stirring needle 32, corresponding to... Figure 2 In the orientation shown, the first direction a is horizontal, and the arrangement direction of the first stirring section 321 and the second stirring section 322 is vertical (i.e., the second direction b). In other words, the cross-section of the first stirring section 321 and the cross-section of the second stirring section 322 are both perpendicular to the arrangement direction of the first stirring section 321 and the second stirring section 322 (i.e., the second direction b).
[0069] In the friction stir welding apparatus 100 provided in this application, the stirring pin 32 is configured as a first stirring section 321 and a second stirring section 322, and the cross-section of the first stirring section 321 gradually decreases in the first direction a, while the cross-section of the second stirring section 322 remains unchanged in the first direction a. Thus, when the friction stir welding apparatus 100 is used to perform a through-welding process on a workpiece 50 including a first workpiece 51 and a second workpiece 52, part of the second stirring section 322 extends into the upper second workpiece 52 and another part extends into the lower first workpiece 51. Due to the axisymmetric characteristic of the diameter of the second stirring section 322 (the radial dimension of the second stirring section 322 remains unchanged along the arrangement direction of the first and second stirring sections 321, and the second stirring pin 32 exhibits axisymmetry), the second stirring section 322 maintains circumferential continuity with the material contact interface when rotating, avoiding periodic cross-sectional changes caused by diameter variations. This results in a more uniform distribution of shear rate and contact pressure when the softened plastic material flows circumferentially along the second stirring section 322.
[0070] This geometric continuity weakens the shear force vector offset caused by the difference in tool rotation direction between the advancing and retreating sides, allowing the softened plastic material to form a stable viscoplastic laminar flow under the forging pressure at the connection between the connector 31 and the first stirring section 321 (i.e., at the shoulder), thus improving the phenomenon of kinetic energy accumulation or eddy separation caused by sudden changes in local flow velocity. Simultaneously, the uniform diameter structure, by maintaining a constant cross-sectional area of the axial migration channel, reduces the imbalance in kinetic-potential energy conversion caused by cross-sectional contraction or expansion along the flow path, thereby reducing the tendency for material accumulation on the advancing side induced by local energy accumulation. The mechanical structural characteristics of the second stirring section 322 in this application, in conjunction with the continuous forging pressure of the shoulder, distribute the plastic deformation energy more evenly across the weld cross-section, thereby reducing the upward accumulation of plastic material on the advancing side, improving hook-shaped defects caused by asymmetric accumulation of plastic material at the weld interface, and reducing the risk of interface warping.
[0071] Furthermore, by making the cross-section of the first stirring section 321, which connects the second stirring section 322 and the connector 31, gradually decrease in the first direction a, this application allows the stress at the connection between the connector 31 and the stirring pin 32 to be gradually released axially. This reduces stress concentration at the connection and improves the fatigue resistance of the stirring head 30. Moreover, the gradually decreasing design of the first stirring section 321 reduces the lateral resistance experienced by the stirring pin 32 during rotation, pressing, and movement, thus reducing the torque borne by the stirring pin 32, increasing its overall structural strength, and lowering the risk of breakage during welding. Therefore, through these design features, this application can improve the hook-like defects in friction stir welding while simultaneously enhancing the operational reliability and service life of the stirring pin 32.
[0072] In one possible implementation, the workpiece 50 to be welded includes a first workpiece 51 and a second workpiece 52, with the second workpiece 52 located on the side of the first workpiece 51 facing away from the stage 40. The surface of the connector 31 facing the stirring needle 32 is used to abut against the second workpiece 52; in the arrangement direction of the first stirring section 321 and the second stirring section 322, the sum of the dimensions of the first stirring section 321 and the second stirring section 322 is greater than the dimension of the second workpiece 52, and the dimension of the first stirring section 321 is smaller than the dimension of the second workpiece 52.
[0073] The dimension of the first stirring section 321 along the arrangement direction of the first stirring section 321 and the second stirring section 322 is the axial dimension of the first stirring section 321, and the dimension of the second stirring section 322 along the arrangement direction of the first stirring section 321 and the second stirring section 322 is the axial dimension of the second stirring section 322. The sum of the dimensions of the first stirring section 321 and the second stirring section 322 along the arrangement direction of the first stirring section 321 and the second stirring section 322 is the sum of the axial dimensions of the first stirring section 321 and the second stirring section 322.
[0074] The thickness of the first workpiece 51 is the dimension along the arrangement direction of the first stirring section 321 and the second stirring section 322. The thickness of the second workpiece 52 is the dimension along the arrangement direction of the first stirring section 321 and the second stirring section 322.
[0075] This application achieves this by having the surface of the connector 31 facing the stirring needle 32 abut against the second workpiece 52, and by ensuring that, in the arrangement direction of the first stirring section 321 and the second stirring section 322, the sum of the dimensions of the first stirring section 321 and the second stirring section 322 is greater than the dimension of the second workpiece 52, while the dimension of the first stirring section 321 is smaller than the dimension of the second workpiece 52. Thus, as... Figure 2 As shown, during friction stir welding, the surface of the connector 31 facing the stirring pin 32 abuts against the second workpiece 52. The first stirring section 321 extends into the second workpiece 52, a portion of the second stirring section 322 extends into the second workpiece 52, and the other portion of the second stirring section 322 extends into the first workpiece 51. That is, the second stirring section 322 is located at the lap surface of the first workpiece 51 and the second workpiece 52. The second stirring section 322 can play the main stirring role. Using a second stirring section 322 with a constant radial dimension can improve hook-shaped defects, reduce warping at the weld interface, and improve weld quality.
[0076] like Figure 2 As shown, in one possible implementation, the end face of the first stirring section 321 facing the second stirring section 322 coincides with the end face of the second stirring section 322 facing the first stirring section 321. By aligning the end faces as described above, this application can mitigate the abrupt change in radial dimensions between the first stirring section 321 and the second stirring section 322, improve stress concentration at the connection between the first stirring section 321 and the second stirring section 322, and enhance the structural strength of the stirring pin 32.
[0077] Wherein, the end face of the first stirring section 321 facing the second stirring section 322 coincides with the end face of the second stirring section 322 facing the first stirring section 321, meaning that along the arrangement direction of the first stirring section 321 and the second stirring section 322, the projection of the end face of the first stirring section 321 facing the second stirring section 322 on the second stirring section 322 coincides with the position of the end face of the second stirring section 322 facing the first stirring section 321, and the areas of the end face of the first stirring section 321 facing the second stirring section 322 and the end face of the second stirring section 322 facing the first stirring section 321 are equal.
[0078] Figure 3 This is a schematic diagram of the structure of the stirring head 30 and the workpiece 50 to be welded provided in an embodiment of this application. Figure 4 This is one of the structural schematic diagrams of the stirring head 30 provided in the embodiments of this application. Please refer to the attached diagram. Figure 3 and Figure 4 In one embodiment, the stirring needle 32 further includes a third stirring section 323, which is fixed between the first stirring section 321 and the second stirring section 322. Along the direction from the first stirring section 321 to the second stirring section 322, the cross-section of the third stirring section 323 gradually decreases. The end face of the third stirring section 323 facing the first stirring section 321 coincides with the end face of the first stirring section 321 facing the third stirring section 323; the end face of the third stirring section 323 facing the second stirring section 322 coincides with the end face of the second stirring section 322 facing the third stirring section 323.
[0079] Along the direction from the first stirring section 321 toward the second stirring section 322, the cross-section of the third stirring section 323 gradually decreases in the first direction a, that is, the radial cross-section of the third stirring section 323 gradually decreases.
[0080] That is, the third stirring section 323 is fixedly connected between the first stirring section 321 and the second stirring section 322. This application achieves this by aligning the end face of the third stirring section 323 facing the first stirring section 321 with the end face of the first stirring section 321 facing the third stirring section 323, and aligning the end face of the third stirring section 323 facing the second stirring section 322 with the end face of the second stirring section 322 facing the third stirring section 323. Furthermore, the cross-section of the third stirring section 323 gradually decreases along the arrangement direction of the first stirring section 321 and the second stirring section 322. In this way, the third stirring section 323 can serve as a transition between the first stirring section 321 and the second stirring section 322, allowing the first stirring section 321 to smoothly transition to the second stirring section 322 after passing through the third stirring section 323. This improves the stress concentration phenomenon at the connection point of the stirring pin 32 between different stirring sections and enhances the structural strength of the stirring pin 32.
[0081] When the stirring needle 32 includes a third stirring section 323, the area of the end face of the first stirring section 321 facing the third stirring section 323 is greater than the area of the end face of the second stirring section 322 facing the third stirring section 323.
[0082] Furthermore, the aforementioned third stirring section 323 can be obtained by rounding the corners at the connection between the first stirring section 321 and the second stirring section 322; that is, the third stirring section 323 can be a rounded corner structure. The aforementioned third stirring section 323 can also be another stirring section not belonging to the first stirring section 321 and the second stirring section 322. By processing the outer peripheral wall of this stirring section, a smooth transition between the first stirring section 321 and the second stirring section 322 can be achieved through the third stirring section 323.
[0083] like Figures 2 to 4 As shown, in one embodiment, the first stirring section 321 is frustum-shaped, and the second stirring section 322 is cylindrical. The frustum-shaped first stirring section 321 and the cylindrical second stirring section 322 can not only improve the welding quality by reducing hook-shaped defects, but also facilitate processing and manufacturing, thereby reducing the difficulty of preparing the stirring pin 32.
[0084] Figure 5 This is the second schematic diagram of the structure of the stirring head 30 provided in the embodiments of this application. Please refer to... Figure 5 In one possible implementation, the outer peripheral wall of the first stirring section 321 and / or the outer peripheral wall of the second stirring section 322 are provided with spiral grooves 324 that spiral along the arrangement direction of the first stirring section 321 and the second stirring section 322.
[0085] For example, the outer peripheral wall of the first stirring section 321 is provided with a spiral groove 324; as another example, the outer peripheral wall of the second stirring section 322 is provided with a spiral groove 324; and yet another example, both the outer peripheral walls of the first stirring section 321 and the outer peripheral walls of the second stirring section 322 are provided with spiral grooves 324. For example, as... Figure 5 As shown, when the outer peripheral wall of the first stirring section 321 and the outer peripheral wall of the second stirring section 322 are both provided with spiral grooves 324, the spiral grooves 324 of the first stirring section 321 and the spiral grooves 324 of the second stirring section 322 can be continuous spiral grooves 324.
[0086] The spiral groove 324 is arranged in a spiral pattern along the arrangement direction of the first stirring section 321 and the second stirring section 322, for example, spiraling upward or spiraling downward along the arrangement direction of the first stirring section 321 and / or the second stirring section 322.
[0087] This application incorporates spiral grooves 324 on the outer peripheral wall of the first stirring section 321 and / or the outer peripheral wall of the second stirring section 322. During welding, the centrifugal pump effect generated by the spiral grooves 324 allows the softened plastic material to be transported along the spiral trajectory of the spiral grooves 324, promoting the migration and filling of thermoplastic material from the front end to the rear end of the stirring pin 32, forming a continuous material flow layer. Furthermore, the geometric features of the spiral grooves 324 (such as groove depth and pitch) increase the contact area between the stirring pin 32 and the material, enhancing local heat input efficiency through friction shear strengthening, accelerating material plasticization, and refining dynamically recrystallized grains, thereby improving the tensile strength of the joint. In other words, the spiral groove 324 design on the outer peripheral wall of the stirring pin 32 in friction stir welding can improve welding quality by enhancing material flow and thermo-coupling effects.
[0088] Figure 7 This is the third schematic diagram of the structure of the stirring head 30 provided in the embodiments of this application. Please refer to... Figure 7 In one possible implementation, the outer peripheral wall of the first stirring section 321 and / or the outer peripheral wall of the second stirring section 322 includes a plurality of planes 33 and a plurality of arc surfaces 34, the planes 33 and arc surfaces 34 being arranged alternately along the circumference of the stirring needle 32.
[0089] This application does not limit the specific number of planes 33 and arc surfaces 34. For example, the outer peripheral wall of the first stirring section 321 and / or the outer peripheral wall of the second stirring section 322 includes two planes 33 and two arc surfaces 34; or, the outer peripheral wall of the first stirring section 321 and / or the outer peripheral wall of the second stirring section 322 includes three planes 33 and three arc surfaces 34; or, the outer peripheral wall of the first stirring section 321 and / or the outer peripheral wall of the second stirring section 322 includes four planes 33 and four arc surfaces 34.
[0090] By setting multiple planes 33, the plane 33 region can use sharp edges to directionally cut and break the oxide film of the base material of the workpiece 50 to be welded; by setting multiple arc surfaces 34, the arc surfaces 34 can drive the softened plastic material to flow in layers through the curvature-induced centrifugal force gradient field, forming a continuous material migration layer. The alternating arrangement of planes 33 and arc surfaces 34 forms a periodic shear-extrusion composite field during rotation, which refines the dynamic recrystallized grains. Thus, the composite design of planes 33 and arc surfaces 34 on the outer peripheral wall of the stirring pin 32 in friction stir welding can improve the welding quality through multi-dimensional mechanical coupling.
[0091] The aforementioned planes 33 and arcs 34 can be obtained by milling the outer periphery of the stirring pin 32. For example, if the plane 33 is only provided on the outer periphery of the first stirring section 321, then only the outer periphery of the first stirring section 321 is milled; if the plane 33 is only provided on the outer periphery of the second stirring section 322, then only the outer periphery of the second stirring section 322 is milled; if the plane 33 is provided on the outer periphery of both the first stirring section 321 and the second stirring section 322, then both the outer periphery of the first stirring section 321 and the second stirring section 322 are milled simultaneously.
[0092] When the outer peripheral wall of the first stirring section 321 and / or the outer peripheral wall of the second stirring section 322 includes multiple planes 33 and multiple arc surfaces 34, in some embodiments, please refer to Figure 7 As shown, each of the multiple arc surfaces 34 has multiple first grooves 341, and the arrangement direction of the multiple first grooves 341 is parallel to the arrangement direction of the first stirring section 321 and the second stirring section 322.
[0093] That is, multiple first grooves 341 are spaced apart on the arc surface 34 along the arrangement direction of the first stirring section 321 and the second stirring section 322.
[0094] This application provides multiple first grooves 341 on the arc surface 34. These grooves 341 create a localized turbulent flow field during rotation, enhancing the radial-axial composite flow of the softened plastic material and increasing its migration rate. This also helps to mitigate the discontinuous laminar flow lines that easily occur at the arc surface 34. Furthermore, the micro-shearing effect generated at the edges of the first grooves 341 further breaks down oxide film particles, and the plastic material accumulated within the first grooves 341 forms a periodic micro-forging effect under rotational extrusion, promoting further refinement of the dynamic recrystallized grain size, which is beneficial for improving the fatigue resistance of the welded joint.
[0095] Figure 6 for Figure 5 Please refer to the bottom view of the stirring head 30. Figure 5 , Figure 6 and Figure 7 For example, the surface of the connector 31 facing the stirring pin 32 is provided with a second groove 311, which extends curvedly from the outer periphery of the stirring pin 32 towards the outer edge of the connector 31. That is, the surface of the connector 31 that abuts against the workpiece 50 to be welded is provided with a vortex groove. By providing a vortex groove at the shoulder, the spiral structure of the vortex groove can increase the frictional contact area between the shoulder and the workpiece 50 to be welded, improve the frictional heat input efficiency, and allow the material in the core area of the weld to continuously soften and maintain a plastic flow state. In addition, the centrifugal force gradient formed by the channel of the vortex groove can guide the plastic material to diffuse outward along the spiral path, which can help eliminate material accumulation at the edge of the shoulder and improve the uniformity of the weld surface.
[0096] Of course, the vortex groove is only one example. In some embodiments, the surface of the connector 31 that abuts against the workpiece 50 to be welded can also be configured as an annular groove.
[0097] Please refer to Figure 3 In one possible implementation, the end face of the second stirring section 322 facing away from the first stirring section 321 has a protrusion 35; the cross-section of the protrusion 35 gradually decreases along the direction from the first stirring section 321 toward the second stirring section 322.
[0098] The gradual reduction in the cross-section of the protrusion 35 along the direction from the first stirring section 321 to the second stirring section 322 means that the cross-section of the protrusion 35 gradually decreases in the first direction a. This gradual reduction in the cross-section of the protrusion 35 implies that the protrusion 35 gradually becomes sharper from the first stirring section 321 to the second stirring section 322. Therefore, during penetration welding, the protrusion 35 facilitates penetration of the workpiece 50 to be welded, reducing penetration resistance.
[0099] In one feasible configuration, along the arrangement direction of the first stirring section 321 and the second stirring section 322, the end face of the protrusion 35 facing the second stirring section 322 coincides with the end face of the second stirring section 322 facing away from the first stirring section 321. This allows for a smooth and uniform transition at the connection between the second stirring section 322 and the protrusion 35, thus mitigating stress concentration at this connection point.
[0100] The following are the welding results when friction stir welding is performed on a liquid-cooled charging module using the friction stir welding apparatus 100 provided in this application and the friction stir welding apparatus 100 with a conical stirring pin 32.
[0101] When using the friction stir welding apparatus 100 of this application, the parameters of the stirring pin 32 are as follows: the large end diameter of the first stirring section 321 of the stirring pin 32 is 5mm, the small end diameter is 3.2mm, the length of the stirring pin 32 is 4mm (wherein, the stirring pin 32 includes the first stirring section 321 and the second stirring section 322, the length of the first stirring section 321 is 3mm, and the length of the second stirring section 322 is 1mm), the shoulder diameter (i.e., the diameter of the end face of the connector 31 facing the stirring pin 32) is 12mm, the spiral direction of the spiral groove 324 on the outer peripheral wall of the stirring pin 32 is right-handed, the outer peripheral wall of the stirring pin 32 is machined with three milled surfaces, and the end face morphology of the shoulder is provided with a spiral line.
[0102] When using the existing friction stir welding device 100 with only a conical section of stirring pin 32, the parameters of the stirring pin 32 are as follows: the length of the stirring pin 32 is 4mm, the small end diameter of the stirring pin 32 is 3.2mm, and the large end diameter is 5.0mm.
[0103] Figure 8 This is one of the metallographic microstructure images obtained after friction stir welding using a conical stirring pin 32. Figure 9 The second metallographic microstructure obtained after friction stir welding using a conical stirring pin 32; Figure 10 One of the metallographic microstructure images obtained after friction stir welding using the friction stir welding apparatus provided in the embodiments of this application. Figure 11 The second metallographic microstructure image obtained after friction stir welding using the friction stir welding apparatus provided in this application embodiment. At the same welding speed of 500-650 mm / min and rotation speed of 2000 rpm, two sets of plates and two sets of die-cast parts with a thickness of 3.5 mm were welded using the friction stir welding apparatus 100 of this application and the existing friction stir welding apparatus 100, respectively. The metallographic microstructure images show that the warpage heights of the existing ordinary conical stirring pin 32 are 0.463 mm and 0.600 mm, respectively, while the warpage heights of the stirring pin 32 of this application are 0.219 mm and 0.283 mm, respectively. The warpage height after welding with the friction stir welding apparatus 100 of this application is significantly lower. Therefore, the friction stir welding apparatus 100 of this application can indeed reduce warpage and improve hook-shaped defects.
[0104] Furthermore, when using a stirring needle 32 with only a cylindrical section, six needles broke during the welding of five sets of workpieces 50 under the same parameters. However, when using the friction stir welding device 100 of this application, no needle breakage occurred during the welding of five sets of workpieces 50 under the same speed and increased pressure. Therefore, it can be seen that the strength of the friction stir welding device 100 of this application has also been improved.
[0105] In the description of this specification, specific features, structures, materials, or characteristics may be combined in any suitable manner in one or more embodiments or examples. The above description is merely a specific embodiment of this application, but the scope of protection of this application is not limited thereto. Any variations or substitutions that can be easily conceived by those skilled in the art within the scope of the technology disclosed in this application should be included within the scope of protection of this application. Therefore, the scope of protection of this application should be determined by the scope of the claims.
Claims
1. A friction stir welding apparatus characterized by comprising: The device includes a frame, a drive unit connected to the frame, a stirring head connected to the drive unit, and a platform for placing a workpiece to be welded. The drive unit is used to drive the stirring head to rotate. The stirring head includes a connector and a stirring pin connected to the connector. The connector protrudes towards the outer periphery of the stirring pin, and the surface of the connector facing the stirring pin is used to abut against the workpiece to be welded. The stirring needle includes a first stirring section and a second stirring section. The first stirring section is fixed between the second stirring section and the connector. Along the direction from the first stirring section to the second stirring section, the cross-section of the first stirring section gradually decreases, while the cross-section of the second stirring section remains unchanged.
2. The friction stir welding device of claim 1, wherein The workpiece to be welded includes a first workpiece and a second workpiece, with the second workpiece located on the side of the first workpiece facing away from the stage. The surface of the connector facing the stirring needle is used to abut against the second workpiece; In the arrangement direction of the first stirring section and the second stirring section, the sum of the dimensions of the first stirring section and the second stirring section is greater than the dimension of the second workpiece, and the dimension of the first stirring section is smaller than the dimension of the second workpiece.
3. The friction stir welding device of claim 1, wherein The end face of the first stirring section facing the second stirring section coincides with the end face of the second stirring section facing the first stirring section.
4. The friction stir welding device of claim 1, wherein The stirring needle further includes a third stirring section, which is fixed between the first stirring section and the second stirring section; the cross-section of the third stirring section gradually decreases along the direction from the first stirring section to the second stirring section. The end face of the third stirring section facing the first stirring section coincides with the end face of the first stirring section facing the third stirring section; the end face of the third stirring section facing the second stirring section coincides with the end face of the second stirring section facing the third stirring section.
5. The friction stir welding apparatus according to any one of claims 1-4, characterized in that, The first stirring section is frustum-shaped, and the second stirring section is cylindrical.
6. The friction stir welding device of claim 5, wherein, The outer peripheral wall of the first stirring section and / or the outer peripheral wall of the second stirring section are provided with spiral grooves that spiral along the arrangement direction of the first stirring section and the second stirring section.
7. The friction stir welding apparatus of any one of claims 1-4, wherein, The outer peripheral wall of the first stirring section and / or the outer peripheral wall of the second stirring section includes multiple planes and multiple arc surfaces, which are arranged alternately along the circumference of the stirring needle.
8. The friction stir welding device of claim 7, wherein, Each of the multiple arc surfaces has multiple first grooves, and the arrangement direction of the multiple first grooves is parallel to the arrangement direction of the first stirring section and the second stirring section.
9. The friction stir welding apparatus of any one of claims 1-4, wherein, The end face of the second stirring section opposite to the first stirring section has a protrusion; the cross-section of the protrusion gradually decreases along the direction from the first stirring section toward the second stirring section.
10. The friction stir welding device of claim 9, wherein, Along the arrangement direction of the first stirring section and the second stirring section, the end face of the protrusion facing the second stirring section coincides with the end face of the second stirring section away from the first stirring section.