Coated pads and electrode sheets
By using a coating pad design in the production of lithium battery electrode sheets, the flow of slurry is guided by the separator to form a uniform wetting channel, which solves the problems of uneven distribution and insufficient strength of the wetting channel, and improves battery performance and production yield.
Patent Information
- Application Number
- CN202522416212.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-13
- Publication Date
- 2026-11-17
- Estimated Expiration
- 2035-11-13
AI Technical Summary
The uneven distribution of wetting channels on the surface of existing lithium battery electrode sheets leads to large differences in the degree of electrolyte wetting, and laser etching may result in insufficient electrode sheet strength, affecting production yield.
The coating pad design includes a coating tank and a separator. The separator guides the flow of slurry to form a uniform wetting channel, avoiding laser etching and ensuring uniform wetting and structural strength of the electrode sheet.
This method achieves uniform wetting of all parts of the electrode sheet, improves the uniformity of battery performance and production yield, and avoids the problem of powder falling off during the etching process.
Smart Images

Figure CN224976709U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of electrode preparation technology, specifically to a coated pad and an electrode. Background Technology
[0002] In lithium-ion battery production, electrode sheets are formed by uniformly coating a slurry onto foil using an extrusion coating machine. The coating head of the machine contains a cavity enclosed by two dies, with a coating gasket placed between them to ensure a seal. The shape of the coating gasket matches the surfaces of the two dies, without affecting the slurry flow. This results in a smooth and flat electrode sheet surface after the slurry solidifies, and after rolling, the entire surface of the electrode sheet is uniformly compacted.
[0003] In related technologies, some lithium battery electrode surfaces often feature wetting channels. These channels are grooves on the electrode surface that lack slurry or have areas with minimal slurry thickness. These areas are typically formed by etching before or during rolling to increase the surface area of the electrode where the electrolyte is immersed, thereby improving battery rate performance and other parameters. However, the wetting channels formed by laser etching in these technologies are densely distributed across the electrode surface, resulting in an unreasonable spatial distribution. This can lead to significant differences in the degree of electrolyte immersion across different areas of the electrode, or insufficient electrode strength, thus limiting the yield rate of electrode production. Utility Model Content
[0004] The embodiments of this utility model provide a coating pad and an electrode sheet, which can improve the technical problem of limited product yield caused by the formation of channels during the electrode sheet production process.
[0005] In a first aspect, embodiments of the present invention provide a coated gasket, comprising: The pad portion has a coating groove and an opening groove communicating with one side of the coating groove; Multiple partitions are located within the coating tank and protrude from the tank wall. One end of each partition away from the tank wall is located at the outer edge of the opening groove. The partitions are used to guide the flow of slurry to form wetting channels when slurry is applied to the foil surface. The multiple partitions are spaced apart along a first direction. The width of the partition is between 0.2 mm and 1 mm; the ratio of the minimum distance between the partition and the wall of the coating tank adjacent to the tank wall along the first direction to the distance between adjacent partitions in the first direction is between 0.5 and 2.
[0006] By employing the above scheme and limiting the aforementioned ratio, the size of the area without wetting channels on the edge of the electrode sheet is closer to the size of the area with wetting channels. This ensures that the electrode sheet is uniformly wetted by the electrolyte. Furthermore, limiting the width of the partition prevents excessive unevenness in the surface density of the electrode sheet due to excessive local reduction in surface density. This combined limitation with the aforementioned ratio ensures sufficient wetting of the electrode sheet while maintaining adequate structural strength, guaranteeing a high yield of the formed electrode sheet. Additionally, when the coating pad is integrated into the coating head for coating, the partitions prevent the slurry from flowing out of the opening groove, thus creating the possibility of forming wetting channels during the coating process onto the foil. Subsequent processes do not require etching the electrode sheet, preventing powder from falling into the wetting channels during etching.
[0007] In one embodiment, the end of the partition portion away from the pad portion is adapted to extend to the end face of the coating head where the coating pad is mounted, where the slurry flows out.
[0008] By adopting the above solution, when the coating pad is integrated into the coating head, the end of the separator can guide the slurry out of the coating head, ensuring that the slurry can form a wetting channel after being coated on the foil.
[0009] In one embodiment, the extension direction of the end of the partition away from the pad portion is parallel to the flow direction of the slurry flowing out of the opening groove.
[0010] This scheme can use the partition to guide the flow direction of the slurry out of the opening groove. In a specific scheme, this setting can be used to make the internal stress distribution of the slurry more uniform when it flows onto the foil, reducing the possibility of the slurry spreading outward on the foil, thereby ensuring that the width of the wetting channel is more uniform and reducing the possibility of the wetting channel being blocked.
[0011] In one embodiment, the spacing between adjacent partitions in the first direction ranges from 5 mm to 50 mm; And / or, the spacing between any two adjacent partitions is equal in the first direction.
[0012] By limiting the spacing of the separators in the first direction to a suitable degree, multiple wetting channels can be formed to ensure the wetting effect, while also ensuring that the capacity and other properties of each battery are more balanced after the electrode sheets are integrated into a battery, thereby further improving product yield. Limiting the spacing between the multiple separators can further ensure the uniformity of the areal density between local areas of the manufactured electrode sheets.
[0013] In one embodiment, the partition has an extension surface group along the direction protruding from the wall of the coating tank, the extension surface group being polygonal in shape or a closed curve formed by straight lines and curves; The extended surface group is connected to the end face of the partition near the opening groove.
[0014] The above configuration makes the partition protrude from the surface of the coating tank in a planar shape so as to fit tightly with the coating die head, ensuring that the impregnation channel can be formed smoothly after subsequent coating, and ensuring that the extension surface group can be used to block and guide the slurry out of the opening tank, so that the impregnation channel can be formed smoothly.
[0015] In one embodiment, the thickness of the partition is less than the thickness of the pad portion.
[0016] By limiting the thickness of the pad portion, the sealing performance of the coating head, which integrates the coating gasket, can be guaranteed.
[0017] In one embodiment, the width of the coating groove along the first direction is greater than the width of the opening groove along the first direction.
[0018] This setup utilizes the walls of the guide groove to collect the slurry. The width of the opening groove is designed according to different electrode sheet sizes to ensure that the slurry can fully coat all areas of the foil surface. Other parts of the coating head do not need to be adjusted, making it easy for the coating head to adapt to the manufacturing of batteries of different specifications.
[0019] In one embodiment, the pad portion includes: a connecting section, a side section, and a width-limiting section; The connecting segment is connected to a side section at each of its opposite ends along the first direction, and the width limiting segment protrudes from the side section along the first direction; the coating groove is located between the connecting segment, the side sections at both ends of the connecting segment, and the width limiting segment; the opening groove is located between the end faces of the two width limiting segments that protrude from one end of the corresponding side section.
[0020] In this way, the width of the opening groove is defined between two opposing width-limiting segments, such that in the first direction, the width of the opening groove is smaller than the width of the coating groove.
[0021] In one embodiment, at one end of the width-limiting section that protrudes from the side panel section, the side of the width-limiting section away from the coating tank is provided with a first chamfered surface.
[0022] This design allows the slurry fluid to flow out more dispersedly near the groove wall where the opening is formed during the extrusion and coating of the foil. This prevents the slurry from becoming excessively thicker at the periphery compared to the center due to leveling effects; in fact, it can even make the periphery thinner than the center. This design results in a more uniform slurry distribution on the electrode sheet, or a smaller thickness at the outer edge of the slurry area. When the electrode sheet is integrated into a battery, this reduces the likelihood of slurry chipping from the edges of the slurry-coated areas on the electrode sheet surface due to assembly stress or other external forces.
[0023] In one embodiment, at one end of the width-limiting section that protrudes from the side panel section, the width-limiting section has a second chamfered surface on the side near the coating tank.
[0024] The second chamfered surface is designed so that the width of at least one section of the opening groove gradually decreases on the side of the opening groove near the coating groove. This helps to reduce the stress exerted on the slurry by the width-limiting section. By reducing the internal pressure of the slurry, the possibility of the slurry continuing to flow under the action of internal pressure and blocking the wetting channel after being coated onto the foil is reduced.
[0025] In one embodiment, the width-limiting segment and the dividing portion are spaced apart along the first direction.
[0026] This design eliminates the presence of wetting channels in the areas near the edges of the electrode sheet. Since the edges of the electrode sheet are more likely to come into contact with the electrolyte in a battery, they are more easily wetted, thus eliminating the need for wetting channels. This design makes the distribution of wetting channels on the electrode sheet more suitable for the actual use requirements of the electrode sheet.
[0027] Secondly, embodiments of this utility model provide an electrode sheet, comprising: foil layer; A coating layer is applied to the surface of the foil layer; The electrode sheet is provided with a wetting channel, which is recessed into the surface of the coating layer on the side away from the foil layer, and a plurality of the wetting channels are distributed at intervals along a first direction; The width of the wetting channel ranges from 0.2 mm to 1 mm; the ratio of the minimum distance between the boundary of the wetting channel adjacent to the edge of the coating layer along the first direction and the edge of the coating layer to the distance between adjacent wetting channels ranges from 0.5 to 2.
[0028] Using the above scheme, the edge of the electrode sheet is more likely to come into contact with the wetting channel, and the area near the middle of the electrode sheet can also be fully wetted by the electrolyte due to the formation of the wetting channel. By limiting the above ratio, the area of the electrode sheet with the wetting channel and the edge area of the coating layer can have a closer size, so that the electrode sheet can be wetted more uniformly.
[0029] In one embodiment, the ratio of the depth of the wetting channel to the maximum thickness of the coating layer ranges from 0.1 to 0.5; And / or, the depth of the immersion channel ranges from 5 μm to 100 μm; And / or, the spacing between adjacent wetting channels in the first direction ranges from 5 mm to 50 mm; And / or, any two adjacent wetting channels are equally spaced in the first direction.
[0030] In one embodiment, the coating layer includes a main body and an edge portion; the edge portion is formed at both ends of the main body opposite to each other along the first direction; the thickness of the edge portion is less than the thickness of the main body.
[0031] In one embodiment, the wetting channel is formed in the body portion.
[0032] The beneficial effects of the embodiments of this utility model are as follows: In the embodiments of this utility model, when the coating pad is integrated into the coating head for coating, the slurry is blocked by the set partition. When the slurry flows out from the opening groove, the slurry is diverted, so that the slurry forms an impregnation channel during the coating process onto the foil. In subsequent processes, there is no need to etch the electrode sheet, thereby avoiding the powder falling into the impregnation channel during the etching process. Attached Figure Description
[0033] To more clearly illustrate the technical solutions in the embodiments of this utility model, the drawings used in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of this utility model. For those skilled in the art, other drawings can be obtained based on these drawings without creative effort.
[0034] Figure 1 This is a three-dimensional schematic diagram of the coated pad provided in an embodiment of this utility model; Figure 2 yes Figure 1 A schematic diagram of the coated pad structure from another perspective; Figure 3 yes Figure 1 A magnified view of a section at point A in the middle; Figure 4 yes Figure 1 A magnified view of a portion of the coated pad near the separator shown; Figure 5 This is a schematic diagram of the structure of the electrode sheet provided in an embodiment of this utility model; Figure 6 yes Figure 5 A magnified view of a section at point B in the middle; Figure 7 yes Figure 5 The diagram shows the structure of the electrode sheet from another perspective.
[0035] Explanation of reference numerals in the attached figures: 100. Coated gaskets; 110. Pad body; 100a. Coating tank; 100b. Opening groove; 111. Connecting section; 112. Side wall section; 113. Width limiting section; 113a. First chamfered surface; 113b. Second chamfered surface; 120. Separator; 121. Extension surface assembly; 122. End face of the separator near the opening slot; 200, Electrode sheet; 200a, Immersion channel; 210. Foil layer; 220. Coating layer; 221. Main body; 222. Edges; a. Width of the partition; b. Spacing between adjacent partitions in the first direction; c. Thickness of the partition; d. Thickness of the pad; e. Width of the coating tank along the first direction; f. Width of the opening groove along the first direction; g. Minimum spacing between the partition adjacent to the tank wall of the coating tank along the first direction and the tank wall of the coating tank; h. Width of the wetting channel; i. Minimum spacing between the boundary of the wetting channel adjacent to the edge of the coating layer along the second direction and the edge of the coating layer; j. Spacing between adjacent wetting channels; k. Depth of the wetting channel; l. Maximum thickness of the coating layer; X1, First direction; X2, Second direction. Detailed Implementation
[0036] The technical solutions of the present utility model will be clearly and completely described below with reference to the accompanying drawings of the embodiments. Obviously, the described embodiments are only some embodiments of the present utility model, and not all embodiments. Based on the embodiments of the present utility model, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of the present utility model. In addition, it should be understood that the specific embodiments described herein are only for illustration and explanation of the present utility model and are not intended to limit the present utility model. In the present utility model, unless otherwise stated, directional terms such as "upper" and "lower" generally refer to the upper and lower positions of the device in actual use or operation, specifically the drawing directions in the accompanying drawings; while "inner" and "outer" refer to the outline of the device.
[0037] The coating pad 100 provided in the first aspect of this application can be used in the coating head of a coating equipment to coat a slurry on a foil in the battery manufacturing process. In subsequent manufacturing processes, the foil coated with the slurry can be further processed into an electrode sheet 200.
[0038] The coating gasket 100 is placed between the two dies in the coating head during use, providing a certain degree of sealing. For details, please refer to... Figure 1 As shown, the coated pad 100 includes a pad body portion 110 and a separator portion 120.
[0039] The pad portion 110 has a coating tank 100a and an opening groove 100b communicating with one side of the coating tank 100a. The coating tank 100a and the opening groove 100b can contain slurry and guide the slurry to flow out from the opening groove 100b. The wall of the opening groove 100b can limit the area where the slurry flows out.
[0040] The separator 120 is located inside the coating tank 100a and protrudes from the tank wall of the coating tank 100a. One end of the separator 120 away from the tank wall of the coating tank 100a is located at the outer edge of the opening groove 100b.
[0041] The term "separator 120" as used in this application refers to the end of the separator 120 away from the wall of the coating tank 100a located at the outer edge of the opening tank 100b. This does not mean that one end of the separator 120 is in contact with the edge of the wall of the opening tank 100b, but rather that one end of the separator 120 is located near the opening of the opening tank 100b where the slurry flows out, along its own extending direction.
[0042] Specifically, one end of the separator 120 may be flush with the edge of the opening groove 100b away from the coating groove 100a, or the separator 120 may extend out of the opening groove 100b, thereby restricting the area through which the slurry flows as it flows out of the opening groove 100b. Considering that the slurry has a certain flow velocity when it flows out of the opening groove 100b, the end of the separator 120 away from the coating groove 100a can also be located inside the opening groove 100b, but near the edge of the groove wall of the opening groove 100b away from the coating groove 100a. For example, in the flow direction of the slurry flowing out of the opening groove 100b, the distance between the end face of the separator 120 away from the coating groove 100a and the edge of the groove wall of the opening groove 100b away from the coating groove 100a is less than 2.5mm. At this time, although the slurry is not blocked by the separator 120 at the moment of flowing out of the opening groove 100b, it can still be diverted and coated onto the foil surface to form an impregnation channel due to its own flow velocity. That is, the separator 120 is used to guide the flow of slurry to form an impregnation channel when coating the foil surface with slurry.
[0043] In this application, reference is made to Figure 2 As shown, the width 'a' of the separator ranges from 0.2 mm to 1 mm. The width 'a' of the separator defines the spacing between the slurry particles coated on the foil, meaning the width of the wetting channels on the manufactured electrode sheet is constrained by the width 'a' of the separator. During the manufacturing of the electrode sheet using a coating head integrated with a coating pad 100, if the width 'a' of the separator is too small, the resulting wetting channels will be too narrow. Furthermore, during slurry coating and rolling, the slurry may block the wetting channels during flow, reducing the wetting effect of the manufactured electrode sheet and hindering the improvement of parameters such as the rate performance of the electrode sheet. If the width 'a' of the separator is too large, the resulting wetting channels will be wider, which can easily lead to excessive reduction in the local areal density of the manufactured electrode sheet. Uneven areal density of the electrode sheet is detrimental to the stable conductivity of the electrode sheet.
[0044] More specifically, the width 'a' of the partition can range from 0.2mm to 0.4mm, 0.4mm to 0.6mm, 0.6mm to 0.8mm, 0.8mm to 1.0mm, etc.
[0045] Reference Figure 2 As shown, the coating pad 100 is provided with a plurality of partitions 120 to form more wetting channels. The plurality of partitions 120 are distributed at intervals along a first direction X1, which can be a measuring direction for defining the width a of the aforementioned partitions, that is, the width of the partitions 120 in the first direction X1 can be in the range of 0.2 mm to 1 mm.
[0046] In this application, reference is made to Figure 2 As shown, the minimum distance g (hereinafter referred to as the gasket distance for ease of description) between the partition portion adjacent to the wall of the coating tank along the first direction and the wall of the coating tank, and the distance b of the adjacent partition portion in the first direction, ranges from 0.5 to 2.
[0047] As an example, the ratio of the gasket edge distance to the spacing b of the adjacent partition in the first direction can be in the range of 0.5 to 0.8, 0.8 to 1, 1 to 1.2, 1.2 to 1.4, 1.4 to 1.6, 1.6 to 1.8, 1.8 to 2.0, etc.
[0048] The gasket edge distance defines the width of the area where the electrode edge does not have wetting channels. Since the electrode edge is more easily contacted and wetted by the electrolyte, wetting channels do not need to be formed at the edge of the electrode. The spacing b between adjacent separators in the first direction defines the width of the thicker portion of the slurry coating in the area where the electrode has wetting channels. It can be understood that the above-mentioned limitation on the ratio of the gasket edge distance to the spacing b between adjacent separators in the first direction makes the electrolyte distribution in the edge and middle areas of the electrode more uniform, and can also reduce the stress concentration problem in local areas of the electrode. By adopting the above scheme, by limiting the ratio of the gasket edge distance to the distance b between adjacent partitions in the first direction, the size of the area without wetting channels on the edge of the electrode sheet is closer to the size of the area with wetting channels. As a result, the electrode sheet can be more uniformly wetted by the electrolyte. Furthermore, limiting the width a of the partition can prevent the electrode sheet from becoming excessively uneven in surface density due to excessive reduction in local surface density. The combined limitation of the ratio ensures that the electrode sheet is fully wetted while also giving it sufficient structural strength, thus guaranteeing the yield of the formed electrode sheet.
[0049] It is understandable that the solution of forming wetting channels using laser etching technology in related technologies requires an additional laser etching process after the rolling process. Furthermore, dust that is difficult to remove is easily generated in the area where the wetting channels are formed during the etching process. This dust remaining on the electrode surface increases the short circuit rate during electrode processing and testing.
[0050] The coating pad 100 provided in this application, when integrated into the coating head for coating, uses a partition 120 to block the slurry. This partition diverts the slurry as it flows out from the opening groove 100b, thus forming a wetting channel during the coating process onto the foil. Subsequent electrode etching is unnecessary, preventing powder from falling into the wetting channel during etching. Furthermore, by limiting the width 'a' of the partition, the formed wetting channel is ensured to have sufficient width, preventing the slurry from flowing out and blocking the channel. This also prevents excessive unevenness in the surface density of the formed electrode due to excessive reduction in local surface density, ensuring a high yield of the formed battery electrode.
[0051] As a specific embodiment, when the coating pad 100 is integrated into the coating head, the end of the separator 120 away from the pad 110 is adapted to extend to the end face of the coating head where the coating pad 100 is installed, where the slurry flows out. That is, one end of the separator 120 can extend to be flush with the end face of the coating head where the slurry flows out, or protrude from the end face of the coating head where the slurry flows out. Considering that the velocity of the slurry flowing out of the coating head is greater than 0, the separator 120 can also be located inside the coating head, that is, the separator 120 does not protrude from the end face of the coating head where the slurry flows out, and there is a certain distance between the separator 120 and the end face of the coating head where the slurry flows out in the flow direction when the slurry flows out of the coating head. For example, the distance between the end of the separator 120 away from the pad 110 and the end face of the coating head where the slurry flows out is less than 2.5 mm, and the slurry can still form an impregnation channel at the foil under the influence of its own flow velocity.
[0052] As an example, when the coating pad 100 is integrated into the coating head, at least a portion of the surface of the separator 120 can be made to adhere to the coating die head. The slurry is blocked by the separator 120 when it flows, so that when the slurry is coated on the foil, areas on the foil that are not coated with slurry or are coated with less slurry corresponding to the separator 120 are formed. After the foil coated with slurry is subjected to processes such as rolling, these areas that are not coated with slurry or are coated with less slurry form wetting channels.
[0053] By adopting the above solution, when the coating pad 100 is integrated into the coating head, the end of the separator 120 can guide the slurry to flow out of the coating head, ensuring that the slurry can form an impregnation channel after being coated on the foil.
[0054] In some designs, the extension direction of the end of the separator 120 away from the pad portion 110 is parallel to the direction of the slurry outflow opening trough 100b. The direction of the slurry outflow opening trough 100b can be obtained through various experimental methods. As an example, the coating head with the integrated coating pad 100 can be placed vertically, that is, the opening formed at the end of the opening trough 100b away from the coating tank 100a faces downward. In this case, the slurry flows vertically downward, and at least one end of the separator 120 at the end away from the pad portion 110 (that is, the end of the separator 120 away from the tank wall of the coating tank 100a) extends in a vertical direction.
[0055] This configuration guides the direction of the slurry flow out of the opening groove 100b, allowing the slurry to flow out of the coating head in a relatively defined direction. By using the separator 120 to guide the flow direction of the slurry out of the opening groove 100b, in a specific embodiment, this configuration ensures a more uniform distribution of internal stress in the slurry when it flows onto the foil, reducing the possibility of the slurry spreading outwards on the foil. This ensures a more uniform width of the wetting channel, reducing the possibility of the wetting channel being blocked by the slurry due to disordered flow, and thus ensuring that the manufactured electrode sheet is fully wetted by the electrolyte.
[0056] The separator 120 and the pad 110 can be integrally formed, for example, by casting, stamping or other means. This can reduce the assembly gap between the separator 120 and the pad 110 and reduce the possibility of slurry adhering to and remaining on the coating pad 100 and affecting the subsequent coating effect.
[0057] Reference Figure 2 As shown, in this application, the value range of the spacing b between adjacent partitions in the first direction X can be limited to 5mm to 50mm. For example, the value range of the spacing b between adjacent partitions in the first direction can be 5mm to 15mm, 15mm to 20mm, 20mm to 25mm, 25mm to 30mm, 30mm to 35mm, 35mm to 40mm, 40mm to 45mm, 45mm to 50mm, etc.
[0058] The spacing between wetting channels affects the performance of the electrode sheet. Specifically, a spacing b of less than 5 mm between adjacent separators in the first direction results in an overly dense distribution of wetting channels, leading to uneven slurry surface density across the electrode sheet. A spacing b of more than 50 mm between adjacent separators in the first direction has a significant impact on the wetting effect of the electrode sheet. By limiting the spacing of the separators 120 to an appropriate distance in the first direction X1, multiple wetting channels can be fabricated to ensure a good wetting effect, while also ensuring that the capacity and other performance characteristics of each battery are more balanced after the electrode sheets are integrated into the battery, further improving product yield.
[0059] Furthermore, the spacing b between any two adjacent partitions in the first direction can be set to be equal. It is understood that this setting can further ensure the uniformity of surface density between local areas of the manufactured electrode sheet.
[0060] The thickness of the separator 120 does not need to be exactly the same as that of the pad 110, as this would increase the difficulty of manufacturing the coating pad 100. Since the pad 110 is mainly located between the two coating dies of the coating head, if the manufacturing precision is insufficient and the thickness c of the separator exceeds the thickness d of the pad by a certain value, the pad 110 may affect the sealing effect due to a large gap between it and the coating die.
[0061] In some embodiments, the thickness c of the partition is less than the thickness d of the pad, and the thickness d of the pad can satisfy the following relationship: d = N1 - N2 + N0 Among them, reference Figure 2As shown, d represents the thickness of the pad portion; N1 represents the slurry thickness, i.e., the thickness of the coating applied to the foil surface by the coating die head; N2 represents the rolling thickness, i.e., the reduction in slurry thickness during the subsequent rolling process to compact the slurry; and N0 is a constant, specifically, the value of N0 can range from 0.05 mm to 1.0 mm. By limiting the thickness d of the pad portion, the sealing performance of the coating head integrating the coating pad 100 can be guaranteed, and the slurry will not completely fill the areas on the foil surface that were not coated with slurry during the slurry application process due to the use of the separator 120 due to the subsequent rolling process. This ensures that the electrode surface formed under rolling and subsequent processes can smoothly form wetting channels.
[0062] As a specific plan, refer to Figure 3 As shown, the partition 120 has an extension surface group 121 along the direction protruding from the wall of the coating tank 100a. The shape of the extension surface group 121 is polygonal, or a closed curve formed by straight lines and curves. That is, this application does not impose specific restrictions on the cross-sectional shape of the partition 120 protruding from the wall of the coating tank 100a. However, in order to ensure that the wetting channel can be formed smoothly after subsequent coating, the surface of the partition 120 protruding from the coating tank 100a and extending is planar so as to fit tightly with the coating die head. More specifically, the extension surface group 121 is connected to the end face 122 of the partition near the opening groove, so as to ensure that the extension surface group 121 can block and guide the slurry to flow out of the opening groove 100b, so that the wetting channel can be formed smoothly.
[0063] Reference Figure 4 As shown, the width e of the coating tank along the first direction can be set to be greater than the width f of the opening tank along the first direction. During the process of the slurry flowing from the coating tank 100a to the opening tank 100b, this setting can utilize the tank wall of the guide tank to collect the slurry. The width of the opening tank 100b is designed according to different electrode sheet sizes so that the slurry can be fully coated on all parts of the foil surface, while other parts of the coating head do not need to be adjusted, making it easy for the coating head to adapt to the manufacturing of batteries of different specifications.
[0064] In one embodiment, reference is made to Figure 2 As shown, the pad body 110 is provided with: a connecting section 111, a side section 112, and a width limiting section 113.
[0065] The connecting segment 111 is connected to a side wall segment 112 at each of its opposite ends along the first direction X1. A width-limiting segment 113 protrudes from the side wall segment 112 along the first direction X1. The coating tank 100a is located between the connecting segment 111, the side wall segments 112 at both ends of the connecting segment 111, and the width-limiting segment 113. That is, the connecting segment 111, the side wall segment 112, and the width-limiting segment 113 each form a portion of the tank wall of the coating tank 100a. The opening slot 100b is located between the end faces of the two width-limiting segments 113 protruding from one end of the corresponding side wall segment 112. In this way, the width of the opening slot 100b is defined between the two opposite width-limiting segments 113, and the width of the opening slot 100b is smaller than the width of the coating tank 100a in the first direction.
[0066] For more specific solutions, refer to Figure 2 As shown, at one end of the width-limiting section 113 protruding from the side section 112, the side of the width-limiting section 113 away from the coating tank 100a is provided with a first chamfered surface 113a. That is, on the side of the opening groove 100b away from the coating tank 100a, the width of the opening groove 100b gradually increases. This arrangement allows the slurry fluid to flow out more dispersedly near the wall of the opening groove 100b formed by the width-limiting section 113 during the process of being extruded from the opening groove 100b and coated onto the foil. This prevents the slurry from being too thick at the periphery compared to the middle area due to the leveling effect of the slurry, and may even make the slurry thickness at the periphery thinner than the middle area. This arrangement makes the slurry distribution on the electrode sheet more uniform, or makes the outer edge of the slurry-coated area on the electrode sheet have a smaller thickness dimension. When the electrode sheet is integrated into the battery, it can reduce the possibility of the edge of the slurry-coated area on the electrode sheet losing material when the electrode sheet is subjected to stress during assembly or other external forces.
[0067] Reference Figure 2 As shown, considering the setting of the width limiting section 113, during the process of the slurry flowing from the wider coating tank 100a to the narrower opening tank 100b, the slurry will be squeezed by the width limiting section 113. It can be limited to one end of the width limiting section 113 that protrudes from the side wall section 112. The side of the width limiting section 113 near the coating tank 100a is provided with a second chamfered surface 113b. That is, on the side of the opening tank 100b near the coating tank 100a, the width of at least one section of the opening tank 100b gradually decreases. This helps to reduce the stress applied to the slurry by the width limiting section 113. By reducing the internal pressure of the slurry, the possibility of the slurry continuing to flow under the action of internal pressure and blocking the wetting channel after being coated onto the foil is reduced.
[0068] Reference Figure 2As shown, in the first direction X1, the width-limiting section 113 can be configured to be separated from the partition 120, that is, the slurry is not restricted by the partition 120 during the flow of the slurry in the opening groove 100b on both sides near the width-limiting section 113. This configuration makes it so that there are no wetting channels in the area near the two side edges of the electrode sheet. Since the two side edge areas of the electrode sheet are more likely to come into contact with the electrolyte in the battery, they are more likely to be wetted, so it is not necessary to set the wetting channels. The above configuration makes the distribution of the wetting channels formed on the electrode sheet more suitable for the actual use requirements of the electrode sheet.
[0069] Based on the inventive concept of this application, and referring to Figure 5 As shown, a second aspect of this application also provides an electrode sheet 200, including a foil layer 210 and a coating layer 220 disposed on the surface of the foil layer 210. Specifically, the coating layer 220 is formed by the coagulation of a slurry, or more specifically, the coating layer 220 is formed, for example, by the coagulation of a slurry applied to the surface of the foil layer 210 by a coating head integrated with the aforementioned coating pad 100.
[0070] Among them, reference Figure 5 and Figure 6 As shown, the electrode sheet 200 is provided with a plurality of wetting channels 200a. The wetting channels 200a are recessed into the surface of the coating layer 220 on the side away from the foil layer 210. The wetting channels 200a can penetrate the coating layer 220 or not. The plurality of wetting channels 200a are distributed at intervals along the second direction X2. It can be understood that when the coating pad 100 participates in the formation process of the coating layer 220, the second direction X2 is the same as the first direction X1.
[0071] In this application, reference is made to Figure 6 As shown, the width h of the immersion channel ranges from 0.2 mm to 1 mm. Specifically, the width h of the immersion channel can range from 0.2 mm to 0.4 mm, 0.4 mm to 0.6 mm, 0.6 mm to 0.8 mm, 0.8 mm to 1.0 mm, etc.
[0072] Furthermore, referring to Figure 7 As shown, the ratio of the minimum distance i between the boundary of the wetting channel adjacent to the edge of the coating layer along the second direction and the edge of the coating layer (hereinafter referred to as the coating edge distance) to the distance j between adjacent wetting channels ranges from 0.5 to 2. Here, the distance j between adjacent wetting channels is the distance between wetting channels 200a in the second direction X2. Specifically, the ratio of the coating edge distance to the distance j between adjacent wetting channels ranges, for example, from 0.5 to 0.8, 0.8 to 1, 1 to 1.2, 1.2 to 1.4, 1.4 to 1.6, 1.6 to 1.8, 1.8 to 2.0, etc.
[0073] It is understandable that by limiting the ratio of the coating edge distance to the distance j between adjacent wetting channels of adjacent partitions, the size of the area of the electrode sheet 200 without wetting channels 200a is closer to the size of the area with wetting channels 200a. As a result, the electrode sheet 200 can be more uniformly wetted by the electrolyte. Moreover, limiting the width h of the wetting channel can prevent the electrode sheet 200 from becoming excessively uneven in surface density due to excessive reduction in local surface density. At the same time, the combined limitation of the width h of the wetting channel and the ratio of the coating edge distance to the distance j between adjacent wetting channels of adjacent partitions ensures that the electrode sheet 200 is fully wetted while also giving the electrode sheet 200 sufficient structural strength, thus ensuring the yield of the electrode sheet 200 during forming and its stability during use.
[0074] In some embodiments, refer to Figure 6 As shown, the ratio of the depth k of the wetting channel to the maximum thickness l of the coating layer can be limited to a range of 0.1 to 0.5. It can be understood that the maximum thickness of the coating layer 220 occurs in the area where the coating layer 220 does not have a wetting channel 200a. This limitation makes the depth k of the wetting channel match the overall thickness of the coating layer 220. While ensuring that the wetting channel 200a can accommodate enough electrolyte, the coating layer 220 also has sufficient thickness at the location of the wetting channel 200a to ensure the overall structural strength of the electrode sheet 200.
[0075] Specifically, the ratio of the depth k of the wetting channel to the maximum thickness l of the coating layer ranges, for example, from 0.1 to 0.2, 0.2 to 0.3, 0.3 to 0.4, 0.4 to 0.5, etc.
[0076] More specifically, the depth k of the wetting channel can range from 5 μm to 100 μm. For example, the depth k could range from 5 μm to 15 μm, 15 μm to 30 μm, 30 μm to 45 μm, 45 μm to 60 μm, 60 μm to 75 μm, 75 μm to 90 μm, 90 μm to 100 μm, etc. This specific limitation on the depth k of the wetting channel further ensures sufficient contact between the electrode sheet 200 and the electrolyte, while the structural strength of the electrode sheet 200 itself is less affected by the formation of the wetting channel 200a.
[0077] In practical applications, the spacing j between any two adjacent wetting channels can also be configured to be equal, so that the degree of wetting and structural strength of a large number of areas of the electrode sheet 200 are relatively similar.
[0078] In some embodiments, refer to Figure 5As shown, the coating layer 220 includes a main body 221 and an edge portion 222. The main body 221 has edge portions 222 formed at both ends opposite to each other along the second direction X2. That is, the edge portions 222 are located on the periphery of the main body 221. During the coating of slurry on the surface of the foil layer 210 and subsequent rolling processes, the slurry will be subjected to some external forces or internal stresses. These forces may cause problems such as cracking at the edge of the coating layer 220. In some embodiments of this application, the thickness of the edge portion 222 can be limited to be less than the thickness of the main body 221. That is, the edge of the electrode sheet 200 along the second direction X2 can be thinned. This setting is beneficial to reduce the stress at the slurry or coating layer 220, and also beneficial to make the electrolyte and the electrode sheet 200 more fully in contact.
[0079] It is understandable that when the electrode sheet 200 is manufactured using a coating head that integrates the above-mentioned coating pad, the setting of the first chamfer surface 113a can facilitate the thickness of the formed edge portion 222 being less than that of the main body portion 221.
[0080] The function of the wetting channel 200a is to ensure that the electrode sheet 200 is in full contact with the electrolyte, which is similar to the function of the edge portion 222 having a smaller thickness than the main body portion 221. For a more specific design, refer to... Figure 5 and Figure 7 As shown, the wetting channel 200a can be formed in the main body 221, that is, the wetting channel 200a does not need to be provided at the edge 222. On the one hand, the edge 222 can be fully wetted by the electrolyte, and on the other hand, it also ensures that the edge 222 has sufficient structural strength.
[0081] The embodiments of this utility model have been described in detail above. Specific examples have been used to illustrate the principles and implementation methods of this utility model. The description of the above embodiments is only for the purpose of helping to understand the method and core ideas of this utility model. At the same time, for those skilled in the art, there will be changes in the specific implementation methods and application scope based on the ideas of this utility model. Therefore, the content of this specification should not be construed as a limitation of this utility model.
Claims
1. A coated gasket, characterized by, include: The pad portion has a coating groove and an opening groove communicating with one side of the coating groove; Multiple partitions, at least partially located within the coating tank and protruding from the tank wall, are provided. One end of each partition, away from the tank wall, is located at the outer edge of the opening. The partitions are used to guide the flow of slurry to form wetting channels when slurry is applied to the foil surface. The multiple partitions are spaced apart along a first direction. The width of the partition is between 0.2 mm and 1 mm; the ratio of the minimum distance between the partition and the wall of the coating tank adjacent to the tank wall along the first direction to the distance between adjacent partitions in the first direction is between 0.5 and 2.
2. The coated gasket according to claim 1, characterized in that, The end of the separator away from the pad is adapted to extend to the end face of the coating head where the coating pad is installed, where the slurry flows out.
3. The coated gasket according to claim 1, characterized in that, The extension direction of the end of the separator away from the pad is parallel to the flow direction of the slurry flowing out of the opening groove.
4. The coated gasket according to claim 1, characterized in that, The spacing between adjacent partitions in the first direction ranges from 5 mm to 50 mm; And / or, the spacing between any two adjacent partitions is equal in the first direction.
5. The coated gasket according to claim 4, characterized in that, The partition has an extension surface group along the direction protruding from the wall of the coating tank. The shape of the extension surface group is a polygon or a closed curve surrounded by straight lines and curves. The extended surface group is connected to the end face of the partition near the opening groove.
6. The coated gasket according to claim 1, characterized in that, The thickness of the partition is less than the thickness of the pad.
7. The coated gasket according to any one of claims 1 to 6, characterized in that, The width of the coating groove along the first direction is greater than the width of the opening groove along the first direction.
8. The coated gasket according to any one of claims 1 to 6, characterized in that: The pad body is provided with: a connecting section, a side section, and a width limiting section; The connecting segment is connected to a side section at each of its two opposite ends along the first direction. The width limiting segment protrudes from the side section along the first direction, and the width limiting segment and the partition are spaced apart along the first direction. The coating groove is located between the connecting segment, the side sections at both ends of the connecting segment, and the width limiting segment. The opening groove is located between the end faces of the two width limiting segments that protrude from one end of the corresponding side section.
9. The coated gasket according to claim 8, characterized in that, At one end of the width-limiting section that protrudes from the side panel section, a first chamfered surface is provided on the side of the width-limiting section away from the coating tank.
10. The coated gasket according to claim 8, characterized in that, At one end of the width-limiting section that protrudes from the side panel section, the width-limiting section has a second chamfered surface on the side near the coating tank.
11. An electrode sheet, characterized in that, The electrode sheet includes: foil layer; A coating layer is applied to the surface of the foil layer; The electrode sheet is provided with wetting channels, which are recessed into the surface of the coating layer on the side away from the foil layer. Multiple wetting channels are distributed at intervals along the second direction. The width of the wetting channels ranges from 0.2 mm to 1 mm. The ratio of the minimum distance between the boundary of the wetting channel adjacent to the edge of the coating layer along the second direction and the edge of the coating layer to the distance between adjacent wetting channels ranges from 0.5 to 2.
12. The electrode sheet according to claim 11, characterized in that, The ratio of the depth of the wetting channel to the maximum thickness of the coating layer ranges from 0.1 to 0.
5. And / or, the depth of the immersion channel ranges from 5 μm to 100 μm; And / or, the spacing between adjacent wetting channels ranges from 5 mm to 50 mm; And / or, the spacing between any two adjacent wetting channels is equal.
13. The electrode sheet according to claim 11 or 12, characterized in that, The coating layer includes a main body and an edge portion; the edge portion is formed at both ends of the main body along the second direction; the thickness of the edge portion is less than the thickness of the main body.
14. The electrode sheet according to claim 13, characterized in that, The wetting channel is formed in the main body.