Functional optical fiber, its production processes, and its uses, particularly for the in-situ measurement of lithium concentration in the electrolyte of a battery

A functionalized optical fiber with specific surface groups enables real-time, cost-effective lithium concentration measurement in battery electrolytes, addressing the limitations of conventional systems by providing detailed, non-invasive monitoring for improved battery performance and safety.

FR3140179B1Active Publication Date: 2024-09-20COMMISSARIAT A LENERGIE ATOMIQUE ET AUX ENERGIES ALTERNATIVES
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
FR2022009695
Authority / Receiving Office
FR · FR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-09-23
Publication Date
2024-09-20
Estimated Expiration
2042-09-23

AI Technical Summary

Technical Problem

Conventional battery management systems lack the ability to provide detailed, real-time measurements of lithium concentration in the electrolyte of batteries, which is crucial for optimizing performance and safety, as existing techniques are expensive, invasive, and do not allow in situ or operando measurements.

Method used

A functionalized optical fiber with specific surface groups is used to measure lithium concentration in situ or operando, utilizing fluorescence to provide real-time data without disrupting battery operation, and can be easily implemented using common materials.

Benefits of technology

The optical fiber sensor offers a cost-effective, non-invasive method for precise lithium concentration monitoring, enhancing battery performance and safety by providing detailed, real-time data to battery management systems.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000028_0000
    Figure 00000028_0000
  • Figure 00000029_0000
    Figure 00000029_0000
  • Figure 00000029_0001
    Figure 00000029_0001
Patent Text Reader

Abstract

The present invention relates to a functionalized optical fiber, by grafting onto at least a portion of its surface a plurality of groups comprising a probe, and methods for obtaining such a fiber. The present invention also relates to the uses of said optical fiber, particularly for measuring lithium concentration, specifically for in situ, or even in operando, measurement of lithium concentration in the electrolyte of a battery.
Need to check novelty before this filing date? Find Prior Art

Description

Description Title of the invention: FUNCTIONALIZED OPTICAL FIBER, SES METHODS OF OBTAINING, AND ITS USES, PARTICULARLY FOR IN SITU MEASUREMENT OF LITHIUM CONCENTRATION IN THE ELECTROLYTE OF A BATTERY

[0001] — The present invention relates to a functionalized optical fiber, by grafting onto at least one of the following: at least a portion of its surface of a plurality of groups comprising a probe, and its methods of obtaining. The present invention also relates to the uses of said optical fiber, in particular for measuring lithium concentration, in particular for the in situ, or even in operando, measurement of the lithium concentration in the electrolyte of a battery.

[0002] = The advantages of electrochemical propulsion of electric vehicles and the need for efficient large-scale energy storage, particularly in transport, have led to a growing demand for high-performance batteries, that is to say, in particular, safe, efficient and reliable, in electronic devices laptops and electric vehicles. The development of larger batteries, with higher energy density and stricter safety requirements are thus crucial.

[0003] In this context, Li-ion batteries have progressed considerably over the recent decades, particularly on issues ranging from thermal safety to cycling stability.

[0004] — However, to reach the next level of battery innovations Li-ion, there is a need to develop sensors that can be used to probe the real-time and operando batteries, in order to optimize performance and to determine the state of the cells more precisely.

[0005] — Conventional battery management systems, which generally rely on parameters such as current, voltage and temperature, provide in- limited training on the chemical and physical processes that take place in the battery during operation. Understanding the degradation processes and their evolution over time is also limited due to the nature battery complex. In order to improve the lifespan, safety and reliability of current batteries as well as emerging battery technologies, information more detailed information from the cells is needed.

[0006] — In particular, it is important to be able to know the local ion concentration lithium within the electrolyte of these batteries. This concentration varies during charge and discharge cycles, especially as the cell ages. The loss of active lithium through internal cell degradation processes, such as the growth of the solid-electrolyte interface (SEI), will cause a loss of performance. Many attempts have been made to observe lithium distributions in electrodes using techniques such as X-ray absorption near-threshold spectroscopy (XANES), nuclear magnetic resonance (NMR), X-ray diffraction, neutron diffraction, particle-induced gamma / x-ray emission (PIGF / PIXE), Raman microspectroscopy, and hard X-ray photoelectron spectroscopy (HX-PES). However, these techniques cannot directly measure the lithium concentration in the electrolyte. Furthermore, these techniques do not allow in situ or even in operando measurements, or even require disassembly of the battery to be analyzed. They are also very expensive. They are, in fact, laboratory techniques that cannot be used for monitoring a battery pack in operation. An objective of the invention is thus to provide a sensor making it possible to measure locally, in situ or even in operando, the lithium concentration at the heart of the battery, in the electrolyte and to provide in particular real-time information that can be used by the battery management system (BMS). To this end, the sensor of the invention is stable in electrolytes, in particular in organic carbonates, and does not disrupt the operation of the battery. Another objective of the invention is to provide a sensor which can be easily obtained from common materials (namely optical fibers). Yet another objective of the invention is to provide a sensor that can easily be implemented in a simple, rapid and inexpensive method for measuring lithium concentration. This is a simple fluorescence measurement, which therefore meets the aforementioned criteria. Thus, according to a first aspect, the invention relates to an optical fiber carrying on at least part of its surface a plurality of groups of formula (I) below: [Chem.1] O oO / A pvÉ we 655 (wi °NXN NE R #H #H {I}, in which: W and Y are independently selected from O and NH; iet j are independently chosen from 0 and 1; X represents a group of the following formula (ID): [Chem.2] L xt HR OH H24 K (ID, X, and X. are independently chosen from: the groups X,; being linear and branched C,-C;2 alkane diyls, in par- in particular groups of formula —(CH»),- with n from 1 to 12, or alkene diyls linear and branched in C--C,,, the groups X,, being in particular alkanes linear and branched diyles in C,-C;> ; the groups of formula -X,-NH-X,1-, Where X,1 is at each occurrence inde- pending as defined above, in particular groups of formula —(CH»),-NH-—(CH>).- with n and m being independently from 1 to 12; groups of formula -X,-NHC(=O)-NH-X,1- or -X,-NHC(=0)-NH-X;1 - NHC(=0)-NH-X,-, Where X,1 is at each occurrence independently such that defined above, in particular the groups of formula —(CH»), - NHC(=0)-NH-(CH,),- with n and m being independently from 1 to 12; X, is chosen from: linear and branched C,-C, alkane diyls, in particular the groups of formula CH>),- with n from 1 to 12, the alkane triyls branched in C,-C,, the linear and branched C,-C;> alkene diyls, the X groups being in particular linear and branched C;-C;> divalent or trialkyl alkanes; carrying option- ally, in particular in terminal position(s), at least one group —(O-CHz-CHz),- or —(O-CH,-C(CH3)H),-, with p being an integer from | to 3; arene diyls and heteroarene diyls; X, being optionally substituted by a group A of the following formula (III): [Chem.3] oO oO H A Xe À z ONONCON y}, R (On, X.. Y, j, Z and R being as defined above or below, Z is absent or selected from linear and branched C1-C2 alkane diyls and linear and branched C1-Cy alkene diyls, Z being in particular a linear C7 alkane or alkene diyl, said group Z being optionally substituted by a -COOH group; R is an aryl or heteroaryl group substituted by at least two vicinal groups chosen from -OH and C,-C; alkoxy groups, in particular -OMe, said vicinal groups being more particularly -OH. Said at least part of the surface is for example located at the end of the fiber, or along the fiber ([Fig.3]). According to a particular embodiment, R is chosen from the following groups: [Chem.4] qe NE On OH > 0H VA 0H According to a particular embodiment, (Y)ZR is chosen from the following groups: [Chem.5] HO.20 em0H a ; "NAA Fo (Sy Ra OH | + AP OH Hk a " WT these OH Re 0e 1 0 ae OH È LOH di R Cu NT OH and in particular among the following groups: [Chem.6] HOLLO —22-0H 72, 0H _ OL LL I [ 0 SE n to Sr; Let N OH °NT- OH a OH According to a particular embodiment, X is chosen from the following groups: [Chem.7] F5 “f4 HAS BP To NN From LA # AAN A and p being as defined previously. According to a particular embodiment, the groups of formula (I) are chosen from the groups of the following formula: [Chem.8] Oo oO take ITR HOOH* (Ia). O oO oO Oo HHH Hi # | { I À Xa- À, Xp. À Xe Je y2- AW NT EN TONTPNON NUVOUR ww} NH OH HW BR {Ib}, z- R OP 1 1 NH Xe HHN-—-X, The OO NH NH 9 A Xann AX A en Ses Xp wi NHNH uN- *R of). According to a particular embodiment, the optical fiber according to the present invention is chosen from mineral optical fibers, in particular silica optical fibers, or optical fibers carrying a layer of oxide chosen from TiO,,ZrO;, SnO; or HfO,, preferably modified by a compound comprising a phos- acid group phonic as well as a primary amine, in particular a compound of formula (HO), P(=0)-(CH2),NH, with x = 2, 3 or 4; organic optical fibers, in particular fibers made of or comprising polymethyl methacrylate (PMMA), optionally partially chlorinated polymethyl methacrylate, said polymethyl methacrylate optionally carrying carboxylic acid groups; and optical fibers carrying chains of functional oligomers, in particular chains of PVA, optionally partially acetylated. According to a particular embodiment, the optical fiber according to the present invention is chosen from mineral optical fibers, in particular silica optical fibers, with i = 1 and W representing O, or optical fibers carrying an oxide layer chosen from TiO,,ZrO;, SnO; or HfO;, preferably modified by a compound comprising a phosphonic acid group as well as a primary amine, in particular a compound of formula (HO),P(=O)-(CH,),NH, with x = 2, 3 or 4, with i = 1 and W representing N; organic optical fibers, in particular fibers made of or comprising polymethyl methacrylate (PMMA), optionally partially chlorinated polymethyl methacrylate, said polymethyl methacrylate optionally carrying carboxylic acid groups, with i = 0; and optical fibers carrying chains of functional oligomers, in particular chains of PVA, possibly partially acetylated, with i = 1 and W representing 0. According to a particular embodiment, the optical fiber according to the present invention is solid or hollow, at least on said part of its surface. The compounds of the present invention may be prepared by a number of methods well known to those skilled in the art, including, but not limited to, those described below, or by modifications of these methods by applying standard techniques known to those skilled in the art of organic synthesis. Appropriate modifications and substitutions will be readily apparent and well known or may be readily obtained from the scientific literature by those skilled in the art. In particular, such methods may be found in RC Larock, Comprehensive Organic Transformations, Wiley-VCH Publishers, 1999. All methods disclosed in association with the present invention may be carried out at any scale, including milligram, gram, multigram, kilogram, multikilogram, or commercial industrial scale. It will be understood that the compounds of the present invention may contain one or more asymmetrically substituted carbon atoms, and may be isolated in optically active or racemic forms. Thus, all chiral, diastereomeric, racemic, isomeric forms of a structure are intended, unless the ste- reochemistry or the specific isomeric form is not specifically indicated. How to prepare and isolate these optically active forms is well known to those skilled in the art. For example, mixtures of stereoisomers can be separated by standard techniques including, but not limited to, resolution of racemic forms, conventional, reversed-phase and chiral chromatography, preferential salt formation, recrystallization and the like, or by chiral synthesis, either from chiral starting materials or by targeted synthesis of the corresponding chiral centers. The compounds of the present invention can be prepared by a variety of synthetic routes. The reagents and starting materials are commercially available, or readily synthesized by techniques well known to those skilled in the art. All substituents, unless otherwise indicated, are as defined above. More particularly, the optical fibers of the invention, carrying a plurality of groups of formula (I), comprise the groups -NH-C(=O)-NH- (urea), - NH-C(=O)-O- or -OC(=O)-NH- (urethane), and / or -NH-C(=O)- or -C(=O)-NH- (amide). The -NH-C(=O)-NH- group may be formed by any method well known to those skilled in the art, in particular by bringing a compound bearing an -NH; group (primary amine) into contact with a compound bearing an -N=C=O group (isocyanate). This reaction may in particular be carried out in an anhydrous solvent, in particular an anhydrous aprotic solvent, for example dimethyl sulfoxide (DMSO), tetrahydrofuran (THF), 1,4-dioxane, acetone. This reaction may be carried out at a temperature of from 15 to 80°C, in particular from 20 to 60°C, and / or for a period of from 30 minutes to 24 hours, in particular from 1 to 10 hours. The group -NH-C(=O)-O- or -OC(=O)-NH can be formed by any method well known to those skilled in the art, in particular by bringing a compound bearing an -OH group (primary alcohol) into contact with a compound bearing an -N=C=O group (isocyanate), in particular in the presence of a catalyst, in particular chosen from triethylamine, 1,4-diazabicyclo[2,2,2]octane (DABCO), 1,5-diazabicyclo[4.3.0]non-5-ene (DBN), dibutyltin dilaurate (DBTDL), 1,8-diazabicylo[5,4,0]undec-7-ene (DBU), 3,4-dihydro-2H-pyrimido[2,1-b]benzothiazole (DHPB), di-isopropylethylamine (DIPEA), 4-dimethylaminopyridine (DMAP), 1,8-bis(dimethylamino)naphthalene (DMAN), for example triethylamine. This reaction can in particular be carried out in an anhydrous solvent, in particular an anhydrous aprotic solvent, for example dimethyl sulfoxide (DMSO).This reaction can be carried out at a temperature of from 15 to 80°C, in particular from 20 to 60°C, and / or for a period of from 30 minutes to 24 hours, in particular from 1 to 10 hours. When the -OH group is a silanol, in particular of an optical fiber of an optical fiber, this reaction can in particular be carried out at a temperature of from 15 to 30°C, in particular 20 to . 25°C, and / or for a period of 30 minutes to 2 hours, in particular 1 hour. The NH-C(=0)- or -C(=O)-NH- group may be formed by any method well known to those skilled in the art, in particular by bringing a compound bearing a -COOH group (carboxylic acid) into contact with a compound bearing a -N=C=0 group (isocyanate), in particular in the presence of a catalyst, in particular chosen from triethylamine, 1,4-diazabicyclo[2,2,2]octane (DABCO), 1,5-diazabicyclo[4.3.0]non-5-ene (DBN), dibutyltin dilaurate (DBTDL), 1,8-diazabicylo[S,4,0]undec-7-ene (DBU), 3,4-dihydro-2H-pyrimido[2,1-b]benzothiazole (DHPB), di-isopropylethylamine (DIPEA), 4-dimethylaminopyridine (DMAP), 1,8-bis(dimethylamino)naphthalene (DMAN), for example triethylamine. This reaction can in particular be carried out in an anhydrous solvent, in particular an anhydrous aprotic solvent, for example dimethyl sulfoxide (DMSO).This reaction can be carried out at a temperature of 15 to 80°C, in particular 20 to 60°C, and / or for a period of 30 minutes to 24 hours, in particular 1 to 10 hours. According to another aspect, the present invention also relates to a method for preparing an optical fiber as defined above, comprising the following step: (i) Contacting at least a portion of the surface of an optical fiber bearing -OH, -NH, or -COOH groups with a compound (A) of the following formula: [Chem.9] Oo {HAS} o-cn-xy IFR in which X, Y, j, Z and R are as defined above. By "optical fiber carrying -OH, -NH; or -COOH groups" is meant in particular that the optical fiber directly carries -OH, -NH, or -COOH groups on its surface, or that the fiber is functionalized by groups themselves carrying one or more -OH, -NH; or -COOH groups. When the optical fiber carries -OH groups, i = | and W represents -O-. When the optical fiber carries -NH; groups, i = 1 and W represents -NH-. When the optical fiber carries -COOH groups, i = 0. According to a particular embodiment, the optical fiber according to the present invention is chosen from mineral optical fibers, in particular silica optical fibers, with i= 1 and W representing O, or optical fibers carrying a layer of oxide chosen from TiO,, ZrO,, SnO, or HfO,, preferably modified by a compound comprising a phosphonic acid group and a primary amine, in particular a compound of formula (HO),P(=0)-(CH,),NH, with x = 2, 3 or 4, with i = | and W representing N; organic optical fibers, in particular fibers made of or comprising polymethyl methacrylate (PMMA), optionally partially chlorinated polymethyl methacrylate, said polymethyl methacrylate optionally carrying carboxylic acid groups, with i = 0; and optical fibers carrying chains of functional oligomers, in particular chains of PVA, optionally partially acetylated, with i = 1 and W representing 0. According to another aspect, the present invention also relates to a method for preparing an optical fiber as defined above, comprising the following step: (l) bringing into contact at least a portion of the surface of an optical fiber bearing -OH, -NH, or -COOH groups, with a compound (B) of the following formula: [Chem.10] Q=C=NXN=C=0 (B, in which X is as defined previously, to obtain an optical fiber carrying on at least part of its surface a plurality of groups of formula (C) below: [Chem.11] oO IL -ÉW} PN-XN:C=0 i H H (Oo, in which W, i and X are as defined previously, (ii) bringing the fiber obtained in the previous step (i') into contact with a compound of the following formula (D): [Chem.12] Es VOOR (Dk+ in which Z and R are as defined above, and in which Y' is: a -NH group; when j = 1 and Y is -NH-; an -OH group when j = 1 and Y is -O-; a -COOH group when j =0. By "optical fiber carrying -OH, -NH, or -COOH groups" is meant in particular that the optical fiber directly carries -OH, -NH, or -COOH groups on its surface, or that the fiber is functionalized by groups themselves carrying one or more -OH, -NH; or -COOH groups. When the optical fiber carries -OH groups, i = | and W represents -O-. When the optical fiber carries -NH, groups, i = 1 and W represents -NH-. When the optical fiber carries -COOH groups, i = 0. The steps defined above are optionally carried out in the presence of a catalyst, notably chosen from triethylamine, 1,4-diazabicyclo[2,2,2]octane (DABCO), 1,5-diazabicyclo[4.3.0]non-S-ene (DBN), dibutyltin dilaurate (DBTDL), 1,8-diazabicylo[5,4,0]undec-7-ene (DBU), 3,4-dihydro-2H-pyrimido[2,1-b]benzothiazole (DHPB), di-isopropylethylamine (DIPEA), 4-dimethylaminopyridine (DMAP), 1,8-bis(dimethylamino)naphthalene (DMAN), e.g. triethylamine, preferably when a urethane or amide group is formed. The steps defined above are in particular carried out in an anhydrous solvent, in particular an anhydrous aprotic solvent, for example dimethyl sulfoxide (DMSO). The steps defined above are in particular carried out at a temperature of 15 to 80°C, in particular 20 to 60°C, and / or for a duration of 30 minutes to 24 hours, in particular 1 to 10 hours. According to another aspect, the present invention also relates to the use of an optical fiber as defined above, for measuring the concentration of a monovalent ion, in particular of an alkali metal ion, more particularly of lithium ion. The presence of one or more urea functions, in particular aliphatic or linked to aromatic or heteroaromatic cycles, urethane linked to aromatic or heteroaromatic cycles and / or amide linked to aromatic or heteroaromatic cycles, by virtue of their own fluorescence, makes it possible to generate a reference peak during fluorescence, insensitive to the presence or absence of lithium. According to a particular embodiment, the present invention relates to the use as defined above, for measuring the lithium ion concentration in a Li-ion battery, in particular within the electrolyte of said battery. According to another aspect, the present invention also relates to a method for measuring the concentration of a monovalent ion, in particular an alkali metal ion, more particularly lithium ion, comprising the following steps: i A step of bringing into contact the groups of formula (I) carried by at least a part of the surface of the optical fiber as defined previously with the medium in which the monovalent ion concentration is to be measured; ii. A step of excitation by transmission of light in said optical fiber; iii. A step of measuring the fluorescence emitted and transmitted by said fiber optical. According to a particular embodiment, the light of step (ii) is UV light or violet visible light, and in particular has a wavelength of 350 to 450 nm. When said at least one part of the surface is for example located at the end of the fiber, the fluorescence measurement can be done by reflectance ([Fig.3], case 1). When said at least part of the surface is for example located along the fiber, evanescent wave measurement points can be created. In this case, the measurement can be made by transmittance through the fiber, the excitation being sent to one end and the measurement being made at the other end. It is also possible to make a measurement by reflectance, but in this case, it is preferable to add a reflective deposit at the end of the fiber in order to maximize the reflectance ([Fig.3], case 2). Definitions As used herein, the value ranges of "xy" or "from x to y" OR "between x and y" include the bounds x and y as well as the integers between these bounds. For example, "1-5", or "from 1 to 5" or "between 1 and 5" denote the integers 1, 2, 3, 4 and 5. Preferred embodiments include each individual integer in the value range, as well as any subcombination of these integers. For example, preferred values ​​for "1-5" may include the integers 1, 2, 3, 4, 5, 1-2, 1-3, 1-4, 1-5, 2-3, 2-4, 2-5, etc. As used herein, the term “alkyl” means a straight or branched chain, especially straight, alkyl group having the number of carbon atoms indicated before said term, especially 1 to 4 carbon atoms, such as methyl, ethyl, propyl, isopropyl, butyl, isobutyl, sec-butyl, tert-butyl, etc. Thus, a term such as “C1-C3 alkyl” means an alkyl radical containing from 1 to 3 carbon atoms. The same is true for the term "alkane". By "diyl" is meant in particular a residue linked to two groups by a single bond between the residue and each of these two groups. As used herein, the term “arene” means a mono- or bicyclic, substituted or unsubstituted aromatic hydrocarbon ring system having 6 to 10 carbon atoms in the ring. Examples include benzene and naphthalene. Preferred arenes include unsubstituted or substituted benzene and naphthalene. Included within the definition of “arene” are fused ring systems, including, for example, ring systems in which an aromatic ring is fused to a cycloalkyl ring. Examples of such fused ring systems include, for example, indane, indene and tetrahydronaphthalene. As used herein, the term "heteroarene" means a cyclic aromatic system containing 5 to 10 carbon atoms in which one or more ring carbon atoms are replaced by at least one heteroatom such as -O-, -N- or -S-, especially -N- and / or —O-. Examples of heteroarenes include pyrrole, furan, thiophene, pyrazole, imidazole, thiazole, isothiazole, isoxazole, oxazole, oxathiol, oxadiazole, triazole, oxatriazole, furazan, tetrazole, pyridine, pyrazine, pyrimidine, pyridazine, triazine, indole, isoindole, indazole, benzofuran, isobenzofuran, purine, quinazoline, quinoline, isoquinoline, benzoimidazole, benzothiazole, benzo- thiophene, thianaphthene, benzoxazole, benzisoxazole, cinnoline, phthalazine, naphthyridine and quinoxaline. Included in the definition of "heteroarene" are fused ring systems, including, for example, ring systems in which an aromatic ring is fused to a heterocycloalkyl ring.Examples of such fused ring systems include, for example, phthalamide, phthalic anhydride, indoline, isoindoline, tetrahydroisoquinoline, chromane, isochromane, chromene, and isochromene. FIGURES [Fig.1] corresponds to the emission spectra for excitation at 350 nm of compound (4) (example 4) in an electrolyte solution composed of ethylene carbonate (EC) and diethylene carbonate (DEC) in proportion |:1 with different concentrations of lithium ion (LiPF6), as follows: (1) in the absence of lithium (reference); (2) reference + 75 mg Li; (3) reference + 252 mg Li; (4) reference + 379 mg Li; (5) reference + 529 mg Li. [Fig.2] corresponds to the emission spectra for excitation at 320 nm and excitation for emission at 360 nm of the compound (2”) (example 2) in an electrolyte solution composed of Ethylene Carbonate (EC) and Diethylene Carbonate (DEC) in proportion 1:1 with different concentrations of lithium ion (LiPF6), as follows: (1) in the absence of lithium (reference); (2) reference + 70 mg Li; (3) reference + 210 mg Li. [Fig.3] corresponds to the fluorescence measurements using an optical fiber according to the invention as described in Example 5. EXAMPLES Example 1: Preparation of a functionalized silica optical fiber according to the invention The density of silanol groups on the surface of a glass can be estimated at 5 groups per square nm. It can also be estimated that generally, about 10% of these sites are likely to be grafted. Thus, the concentration of the reagents to be used can be determined by knowing the section of the optical core of the glass fiber to be functionalized. Generally, syntheses are carried out in anhydrous DMSO. Still generally, anything that is not grafted by a covalent bond is removed by rinsing in DMSO, then by rinsing in an ethylene carbonate / diethylene carbonate mixture. These rinses remove all impurities adsorbed on the surface of the optical fiber. The hydroxylated surfaces were first dehydrated. This can be done, for example, at 150°C in anhydrous DMSO under argon sparging. 2 hours are generally sufficient to remove the water. Diisocyanate, for example hexane diisocyanate, was then added to the anhydrous DMSO at room temperature, along with triethylamine (1 mol% relative to the diisocyanate used) as a catalyst. This addition can be done, for example, with 15 ml of a 0.1 M solution of diisocyanate in anhydrous DMSO. After typically 1 hour at room temperature, the urethane function is formed between the surface silanols and one of the isocyanate groups. Finally, 3,4-dihydroxy-L-phenylalanine, particularly in a stoichiometric amount relative to the diisocyanate as mentioned above, was added to a solution of the chain-grafted intermediate bearing an isocyanate group in anhydrous DMSO at a temperature of 50°C, for 3 hours. The following optical fiber (1) was thus obtained: [Chem.13] H ox, NN. _cooH 0” NN Ta "ax Oh -OH Se x B SP OH OH ©. Other products of the invention were obtained by replacing the 3,4-dihydroxy-L-phenylalanine with dopamine or caffeic acid, according to a procedure notably described in the following example. Optionally, before contact with the compound of type 3,4-dihydroxy-L-phenylalanine, dopamine or caffeic acid, the chain-grafted intermediate carrying an isocyanate group can be hydrolyzed by adding at room temperature a quantity of stoichiometric water corresponding to half the molar of the diisocyanate involved. Anhydrous DMSO washing is then carried out to remove traces of catalyst and unattached by-products. Then anhydrous DMSO was added, and the resulting mixture was heated to 150°C under argon sparging to remove any adsorbed water. Diisocyanate, with at most 1 molar of the second isocyanate relative to the first grafted, for example hexane diisocyanate, is then added to the anhydrous DMSO at room temperature. This optional sequence therefore makes it possible to lengthen the chain linking the surface of the optical fiber to the catechol-type group. This optional sequence can optionally be repeated to obtain longer chains. Alternatively, the surface of the silica optical fiber can be directly brought into contact, at room temperature, with a medium comprising an intermediate prepared for example according to one of the following operating methods: in 50ml of anhydrous DMSO, 0.1 molar of is added 3,4-dihydroxy-L-Phenylalanine, then 0.1 molar of hexane diisocyanate. The reaction medium is left stirring for 3 hours at 50°C; in 50ml anhydrous DMSO, 0.1 molar of dopamine hydrochloride is added . The mixture is then transferred onto an inversion frit containing 1.5g of NaOH pearl (Alfa Aesar) previously dried for 5 hours under primary vacuum at 50°C and packaged under argon. The solution is left in contact with the soda then filtered, The filtrate obtained contains, in the anhydrous DMSO, dopamine. The filtrate is kept away from light, then added 0.08 molar of hexane diisocyanate. The reaction medium is then left stirring for 3 hours at 50°C; in 50ml of anhydrous DMSO, 0.1 molar of caffeic acid is added, then 0.1 molar of hexane diisocyanate and 0.01 molar of triethylamine. The The reaction medium is then left stirring for 5 hours at 50°C. Example 2: Preparation of another functionalized silica optical fiber according to the invention An optical fiber carrying longer chains than those described in the previous example was also obtained. In a manner analogous to that described in Example 1, the hydroxylated surfaces were first dehydrated. Then, again in a manner analogous to that described in Example 1, diisocyanate, for example hexane diisocyanate, was added. First operating mode: To a solution of the chain-grafted intermediate bearing an isocyanate group in DMSO, a stoichiometric amount of water corresponding to half the molar amount of the diisocyanate involved is added at room temperature. This results in a silanol surface covered with a pendant hexyl group covalently bearing a function primary amine of formula -OC(=O)NH(CH);,NH. Anhydrous DMSO washing was then carried out to remove traces of catalyst and unattached by-products. Then anhydrous DMSO was added, and the resulting mixture was heated to 150°C under argon sparging to remove any adsorbed water. Second method of operation: Alternatively, to a solution of the chain-grafted intermediate bearing an isocyanate group in DMSO, a stoichiometric amount of ethylenediamine is added at room temperature, this amount corresponding to half the molar amount of the diisocyanate involved. A silanol surface covered with hexyl groups covalently bearing a primary amine function of the following formula: -OC(=O)NH(CH 2)eNH(CH.),NH,, was thus obtained. Anhydrous DMSO washing was then carried out to remove traces of catalyst and unattached by-products. Then anhydrous DMSO was added, and the resulting mixture was heated to 150°C under argon sparging to remove any adsorbed water. The chain formed can optionally be extended by repeating the treatment with the diisocyanate then the first or second procedure below, with at most 1 molar of the second isocyanate compared to the first grafted. Whether the operating method used is the first or the second, moreover, an intermediate is prepared for example according to one of the following operating methods: in 50ml of anhydrous DMSO, 0.1 molar of is added 3,4-dihydroxy-L-Phenylalanine, then 0.1 molar of hexane diisocyanate. The reaction medium is left stirring for 3 hours at 50°C; in 50ml anhydrous DMSO, 0.1 molar of dopamine hydrochloride is added . The mixture is then transferred onto an inversion frit containing 1.5g of NaOH pearl (Alfa Aesar) previously dried for 5 hours under primary vacuum at 50°C and packaged under argon. The solution is left in contact with the soda and then filtered. The filtrate obtained contains, in anhydrous DMSO, dopamine. The filtrate is kept away from light, then added 0.08 molar of hexane diisocyanate. The reaction medium is then left stirring for 3 hours at 50°C; in 50ml of anhydrous DMSO, 0.1 molar of caffeic acid is added, then 0.1 molar of hexane diisocyanate and 0.01 molar of triethylamine. The The reaction medium is then left stirring for 5 hours at 50°C. These different reaction media were added to the supported grafts carrying pendant amine functions, as obtained at the end of the first or second mode. described above. To do this, a quantity of 1 molar of catechol grafts versus the theoretical number of pendant amine grafts was added. The reaction mixture is stirred for at least | hour at room temperature. The product obtained is washed thoroughly with anhydrous DMSO to remove impurities, followed by washing in EC / DC medium. The preservation of covalent grafted products can be done in particular in EC / DC medium. A silica optical fiber (2) carrying chains of the following formula was thus obtained: [Chem.14] OH ' 0H # # Vas > ; Te Se NS ES ON Ÿ NON -COOH } H Oo HO H -OH a. A silica optical fiber (2') carrying chains of the following formula was obtained in a similar manner: [Chem.15] OxM 222.08 {© # Read To see HQ rod Hu L LAS ET AN SATA 0 NN ç oO breakdowns PS }-OH @) Example 3: Functionalization of other optical fibers according to the invention In a first embodiment, the optical fiber is functionalized by hydrolysis of a silane coupling agent. In the case of silane coupling agents of the type (OR);Si(CHz);NH; with R=Me,Et or (OR).SiX(CH;),NH; with R= Et, Me and X=Me, there is no need to add an acid or basic catalyst to initiate the hydrolysis. The anhydrous solvent can be acetone, ethanol, THF. Water is added to the formulation at 0.1 mol% relative to the silane coupling agent titer which is between 0.1M and 0.5M. The reaction is rapid (typically 0.5 to 1h at room temperature) for the former, longer for the latter. At the end of the reaction, the fiber is covered with NH graft, pendant. In the case of silane coupling agents of the type (OR);Si(CH,),NCO with R=Et,Me and (OR),SiX(CHz),NCO with R=Et,Me and X=Me, the hydrolysis is carried out in an aprotic solvent without acid or base catalysis and typically takes 4 or 5 hours at room temperature. The concentration of silane coupling agent is notably between 0.2M and 0.5M. The fiber thus treated is stored in a controlled atmosphere for the rest of the grafting. In a second embodiment, a functional oligomer was grafted onto the optical fiber. It may in particular be an oligomer comprising a monomer carrying at least one -OH group. PVA (fully hydrolyzed (PVOH) or partially hydrolyzed (PVOH-PVOAc type)) was thus used. The PVA was contacted with diisocyanate, for example hexane diisocyanate, in a manner analogous to that described in Example 1. The amount of diisocyanate used can be calculated from the molecular weight of the PVA used. For example, with a molecular weight of 10000, PVA has 227 graftable OH sites, knowing that a maximum of 50% of these sites are actually grafted (above this, insoluble particles are likely to be formed). Then, the functionalized PVA was grafted onto an optical fiber. For example, 1.36g of PVA (PM=18000) was added to 75g of anhydrous 1,4-dioxane. The medium was heated to 150°C for SH on a Sohxlet containing a cartridge of anhydrous MgSO. After 5 hours, a clear solution of anhydrous PVA in dioxane was obtained. Previously, 0.4g of diisocyanate and 0.36g of caffeic acid were reacted in 60g of anhydrous dioxane. 100mg of trimethylamine was added as a catalyst. The mixture was heated for 4 hours at 50°C. The two products are mixed and left for 5 hours at 70°C with a second addition of 100mg of trimethylamine. Finally, the catechol residue was introduced as described in Example 1, for example using caffeic acid. Alternatively, the PVA functionalized by the chains carrying a diisocyanate group can be reacted with the compound carrying the catechol, for example caffeic acid, under conditions analogous to those described above, before grafting the PVA thus obtained onto the optical fiber. In a third embodiment, the optical fiber was a mineral optical fiber with a TiO,, ZrO,, SnO, or HfO, surface. The surface of this fiber was first modified with a compound comprising a functional phosphonic acid as well as a chain carrying a pendant free primary amine, in particular of the following formula: (HO);P(=O)-(CH,),-NH> with x = 2, 3 or 4. An optical fiber was thus obtained carrying pendant free primary amine type groups, on which an isocyanate group can react, as indicated above, in particular in example 1. An aluminum or alkaline earth salt or a titanium or zirconium alkoxide can also be hydrolyzed on a silica optical fiber. The optical fiber is then coated with the following functions: Al-OH, Mg-OH, Ti-OH or Zr-OH, on which a phosphonic acid carrying a primary amine function can be reacted, as for example mentioned above. In a fourth embodiment, the optical fiber was an organic optical fiber, in particular based on PMMA, optionally halogenated. The optical fiber was treated to form free carboxylic acid functions on its surface, which will form an amide bond by reaction with an isocyanate group, as indicated above, in particular in example 1. To form free COOH functions on PMMA, for example, the PMMA fiber is immersed in a 1M aqueous HCl solution containing 0.1% by mass of butanol for 10 minutes. After 10 minutes, the fiber is rinsed and dehydrated by immersing it in an anhydrous dioxane solution. A 0.1 molar solution of diisocyanate in anhydrous DMSO containing 1% by mass of trimethylamine is added. The pendant carboxylic acid functions react with an isocyanate function forming an amide function with the release of CO. Typically, the reaction takes place at 50°C and lasts 4 hours. Example 4: Preparation of functionalized optical fibers carrying chains comprising a multivalent platform In a manner similar to that described in Example 1, the hydroxylated surfaces were first dehydrated. Then, again in a manner similar to that described in Example 1, diisocyanate, for example hexane diisocyanate, was added to anhydrous DMSO at room temperature, as well as triethylamine (1 mol% relative to the diisocyanate used), as a catalyst. This addition can, for example, be made with 15 ml of a 0.1 M solution of diisocyanate in anhydrous DMSO. After typically 1 hour at room temperature, the urethane function is formed between the surface silanols and one of the isocyanate groups. The pendant isocyanate-modified fiber is thoroughly rinsed with anhydrous DMSO and finally stored in anhydrous DMSO. Then 1 molar equivalent is added relative to the diisocyanate introduced in the first step: of 1,5-Diaminonaphthalene or Melamine (,3,5-triazine-2,4,6-triamine). This step takes place at 30°C in anhydrous DMSO without catalyst and lasts 1 hour. The modified fibers are washed with anhydrous DMSO and the fibers are stored in anhydrous DMSO. 0.4g of hexyl diisocyanate and 0.36g of caffeic acid were reacted in 60g of anhydrous DMSO. 100mg of trimethylamine are added as a catalyst. The mixture is heated for 4 hours at 50°C. Then, respectively, 1 molar equivalent of caffeic acid-grafted hexyl isocyanate is added relative to the 1,5-Diaminonaphthalene grafted onto the fiber or 2 molar equivalents of caffeic acid-grafted hexyl isocyanate relative to the melamine grafted onto the fiber. This step takes place at 30°C in anhydrous DMSO and is carried out without a catalyst. The optical fibers thus modified are washed thoroughly with anhydrous DMSO and are stored in a mixture of organic carbonates. [Chem.16] OH ME © A L0H # TO, gs mé N US y 755 3 WHERE HR { ae TO THE a. 08” Fox ARR, Ke PAT ON: 1-0 N ï OH (3) oxH { ° 0H a » 4, PP: 7 À ï Ns< CN nd CR © { o Lu Hoi He Lo N° EE, ' HY À ÊE ô * OH (4) # > y FO 8 7 “OH ÔôH « Example 5: Fluorescence measurements Fluorescence measurements, emission spectrum and excitation spectrum, were recorded with a Horiba Jobin Yvon model Fluorolog-3 model FL3-22 spectrometer having the R928 Hamamatsu detector and a 450W Xenon lamp as excitation source. The emission spectrum is obtained by exciting the sample with an absorbed wavelength, usually the absorption (or excitation) peak of maximum intensity. The emission monochromator scans the luminescence over a wavelength interval. The generally most important parameters are i) the excitation wavelength and ii) the slit width, and can easily be determined by the person skilled in the art. The emission spectra were corrected for the spectral response of the monochromators and detector, using typical correction spectra provided by the manufacturer. The excitation spectrum is measured by fixing the emission monochromator at a given emission wavelength (e.g., the one corresponding to the maximum of the emission spectrum). The excitation monochromator is then scanned in a given wavelength interval and the luminescence intensity corresponding to the monitored emission wavelength is measured. The most important parameters are usually i) the monitoring wavelength and ii) the slit width, and can easily be determined by the person skilled in the art. The excitation spectra were corrected from 240 to 600 nm for the spectral distribution of the lamp intensity using a silicon photodiode reference detector (Figures 1 and 2). To assess the sensitivity of the sensor to lithium concentration, the emission and excitation spectrum of the "probe" molecule in solution (EC+DEC) was measured. This is a reference measurement. Then different concentrations of lithium in solution (EC+DEC+LiPF6) were added to the reference / initial solution and the emission and excitation spectra recorded for each concentration. For the dopamine-based probe, the emission spectrum was measured by exciting at a wavelength of 320 nm and with 1.5 mm slits for the emission spectrometer and 0.3 mm slits for the excitation spectrometer. The excitation spectrum was measured by monitoring at a wavelength of 360 nm and with 0.4 mm slits for the emission spectrometer and 0.8 mm slits for the excitation spectrometer. For the melamine-based probe the emission spectrum was measured by exciting at a wavelength of 350 nm and with 1.5 mm slits for the emission spectrometer and 0.3 mm slits for the excitation spectrometer. This example was obtained with optical fibers with grafting of probe molecules at the end of the fiber, for a measurement by reflectance, as presented in particular in [Fig.3], case 1. It is also possible to graft molecules along the fiber on areas where the cladding has been removed in order to create evanescent wave measurement points, as shown in [Fig.3], case 2. In this case, the measurement is made by transmittance through the fiber. The excitation is sent to one end and the measurement is made at the other end. It is also possible in case 2 to make a measurement by reflectance, but in this case it is preferable to add a reflective deposit at the end of the fiber in order to maximize the reflectance.

Claims

Claims

1. Optical fiber carrying on at least one part of its surface a plurality of groups of the following formula (I): [Chem.17] oO oO ; pe ccchiart "açae WI PN-X-NT TR HO H: ®. in which: W and Y are independently selected from O and NH; iet j are independently chosen from 0 and 1; X represents a group of the following formula (II): [Chem.18] oO G 7 i ; | A “n°Xe4. HHHHA ”k (In. X, and X, are independently chosen from: the X groups,; being linear and branched alkane diyls C,-C,,, in particular the groups of formula —CH),- with n from | to 12, or linear and branched C,-C;, alkene diyls the X groups, being in particular linear alkane diyls and connected in C,-C;> ; the groups of formula -X,-NH-X;,1-, where X,1 is at each oc- independently as defined above, in par- in particular the groups of formula —(CH,),-NH—(CH>),- with n and m being independently from 1 to 12; groups of formula -X,-NHC(=O)-NH-X,;- or -X;1 - NHC(=0)-NH-X,-NHC(=0)-NH-X,1-, where X, is at each oc- independently as defined above, in par- in particular the groups of formula —(CH,),-NHC(=0)-NH-—(CH»>)m - with n and m being independently from 1 to 12; X, is chosen from: linear and branched C;-C;2 alkane diyls, in particular groups of formula —(CH»),- with n from 1 to 12, alkanes C,-C, branched triyls, linear alkene diyls and branched in C--C,, the X groups being in particular alkanes linear and branched C,-C;> diyls or triyls; bearing op- tionally, in particular in terminal position(s), at minus one group —O-CH--CH,),- or —“(O-CH,-C(CH,)H),-, with p being an integer from 1 to 3; arene diyls and heteroarene diyls; X, being optionally substituted by a group A of the following formula (III): [Chem.19] oO oO Lx. 442 NT N7X { y RH OH N y (IN), Xe, Y, J, Z and R being as defined above or below, Z is absent or selected from linear and branched C, -Cy alkane diyls and linear and branched C;-C;2 alkene diyls, Z being in particular a linear C> alkane or alkene diyl, said group Z being optionally substituted by a -COOH group; R is an aryl or heteroaryl group substituted by at least two vicinal groups chosen from -OH and C1-C12 alkoxy groups, in particular -OMe, said vicinal groups being more particularly -OH.

2. Optical fiber according to claim 1, in which R is chosen from the following groups: [Chem.20] , Ta” (x 0H QT TE oO

3. An optical fiber according to any preceding claim, wherein (Y);ZR is selected from the following groups: [Chem.21] HO.__0 F HO_0 00H H te SL ag” Oi Bi ; "OH > ,-0H C SET SES OH H OH wine has 0. 7% OH c 40H - Î J Î J. SNS OH SSSOÉTOR 07 OH À and in particular among the following groups: [Chem.22] sou 0H EC CE *a A “OH NT "OH SUN “0H NN

4. An optical fiber according to any preceding claim, wherein X is selected from the following groups: [Chem.23] A1; EX ft HAS The sn CU Fr | P y US NN a D ] lo to ; ; there ie At #2 ÊX ( 1 '-o / k 0 FA Xe 9 + ; There to” > 9 A and p being as defined in claim 1.

5. Optical fiber according to any one of the preceding claims, in which the groups of formula (I) are chosen from the groups of the following formula: [Chem.24] oO oO —bwf Sp 07 NN y}, R (Ia). o Oo ÔÈ Oo H At X, +. b { Se Ka ; as I n°* T At x 4 2 N°NT Xe A4 tés ww N NY OR {Ib} 7-R dx O2 J ONH OH o NH à born Lg —w NNNN HN- HH #HH HN-- x. ÊR (Ie).

6. Optical fiber according to any one of the preceding claims, which is chosen from mineral optical fibers, in particular silica optical fibers, or optical fibers carrying an oxide layer chosen from TiO,ZrO,, SnO, or HfO, preferably modified by a compound comprising a phosphonic acid group as well as a primary amine, in particular a compound of formula (HO),P(=O)-(CH,), NH; with x = 2, 3 or 4; organic optical fibers, in particular fibers made of or comprising polymethyl methacrylate (PMMA), optionally partially chlorinated polymethyl methacrylate, said polymethyl methacrylate optionally carrying carboxylic acid groups; and optical fibers carrying chains of functional oligomers, in particular chains of PVA, optionally partially acetylated, said optical fiber being in particular chosen from mineral optical fibers, more particularly silica optical fibers, with i = 1 and W representing O, or optical fibers carrying a layer of oxide chosen from TiO,, ZrO;, SnO, or HfO,, preferably modified by a compound comprising a phosphonic acid group as well as an amine primary, in particular a compound of formula (HO),P(=O)-(CH,),NH, with x = 2, 3 or 4, with i = | and W representing N; optical fibers organic, in particular fibers consisting of or comprising po- methyl methacrylate (PMMA), possibly polyme- partially chlorinated methyl acrylate, said polymethacrylate of methyl optionally bearing carboxylic acid groups, with i =0 ; and optical fibers carrying functional oligomer chains- tional, in particular PV A chains, possibly par- partially acetylated, with i = | and W representing O.

7. An optical fiber according to any preceding claim, which is solid or hollow, at least on said part of its surface.

8. A method of preparing an optical fiber according to any one of the preceding claims, comprising the following step: (i) Contacting at least part of the surface of a fiber optical bearing -OH, -NH, or -COOH groups, with a compound (A) of the following formula: [Chem.25] O {HAS} o-cnx-p" ER wherein X, Y, j, Z and R are as defined in claim L. or the following steps: (the) bringing into contact at least part of the surface of a fiber optical bearing -OH, -NH, or -COOH groups, with a compound (B) of the following formula: [Chem.26] O=C0=NXN=2=0 (B; wherein X is as defined in claim 1, to obtain an optical fiber covering at least part of its surface a plurality of groups of the following formula (C): [Chem.27] Oo j ER min to H (CO), wherein W, 1 and X are as defined in claim 1, (il) bringing the fiber obtained in the previous step (i') into contact with a compound of the following formula (D): [Chem.28] &“ yYR {D} wherein Z and R are as defined in claim 1, and in which Y' is: a -NH group; when j = 1 and Y is -NH-; an -OH group when j = | and Y is -O-; a -COOH group when j =0.

9. Use of an optical fiber according to any one of the claims- indications 1 to 7, to measure the concentration of a monovalent ion, in particular in an alkali metal ion, more particularly in ion lithium.

10. Use according to claim 9 for measuring ion concentration lithium in a Li-ion battery, particularly within the electrolyte of said battery.

11. Method for measuring the concentration of a monovalent ion, in par- particular into an alkali metal ion, more particularly into lithium ion, including the following steps: A step of bringing into contact the groups of formula (I) carried by at least part of the surface of the optical fiber according to any one of claims 1 to 7 with the medium in which the monovalent ion concentration is to be measured; ii. A step of excitation by transmission of light in said optical fiber; lil. A step of measuring the fluorescence emitted and transmitted by said optical fiber.

12. The method of claim 11, wherein the light of step (ii) is UV light or violet visible light, and in particular has a wavelength between 350 and 450 nm.