Methods of manufacturing personal protective equipment and resulting personal protection

The integration of a thermoplastic composite material with reinforcing fibers and an overmolded expanded polystyrene layer addresses the issues of weight, cost, and adhesion in helmets, resulting in a stronger, lighter, and more efficient body protection equipment.

JP2023500505A5Inactive Publication Date: 2024-11-12MAT PROD & TECH S L U
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
JP2022525812
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2019-11-04
Filing Date
2020-11-03
Publication Date
2024-11-12
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing body protection equipment, particularly helmets, face challenges with structural shells that are heavy, costly, and have poor adhesion between thermoplastic materials and expanded polystyrene layers, leading to peeling and reduced mechanical properties.

Method used

A manufacturing method involving a thermoplastic material with embedded reinforcing fibers, overmolding an expanded polystyrene layer onto a concave interior of a structural shell, ensuring intimate contact without adhesives, thereby improving structural integrity and reducing thickness.

Benefits of technology

Results in a lightweight, cost-effective helmet with enhanced strength and performance by integrating a thermoplastic composite material with reinforcing fibers, providing improved adhesion and mechanical properties without the need for additional adhesives.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

A method for manufacturing a body protection device and a result of the body protection, comprising: manufacturing a structural shell (10) made of a thermoplastic material and having a thickness of up to 5 mm, defining a concave interior (11) and a convex exterior (12); overmolding an expanded polystyrene layer (20) overlying the concave interior (11) of the structural shell (10); and intimately adhering the expanded polystyrene layer (20) to the structural shell (10), wherein the structural shell (10) is manufactured by dispersing in a mold a mixture of thermoplastic material and reinforcing fibers that are stable at a temperature below the melting point of the thermoplastic material; closing and heating the mold causes the thermoplastic material to melt without damaging the reinforcing fibers; and then cooling the mold to harden the thermoplastic material with the reinforcing fibers embedded therein.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to the field of methods for manufacturing body protection comprising a structural shell and an expanded polystyrene layer, and the resulting body protection of said method, where it will be understood that the shell is the outermost layer of the body protection equipment, i.e. the first layer to be subjected to an impact. [Background technology]

[0002] The structural shell is a rigid element intended to provide substantial protection against an impact, distributing stresses over an area larger than the area of ​​the impact surface, thereby reducing local pressures and therefore the direct damage that said impact may cause to the part of the user's body protected by said personal protective equipment.

[0003] The body protection may be protection for joints such as ankles, knees, elbows or shoulders, protection for the long bones of the legs or arms, protection for limbs such as parts of boots or gloves, or protection for parts of the torso, but the preferred use for the body protection is in the form of a helmet for protection of the user's head.

[0004] Typically, an expanded polystyrene layer is placed within the structural shell of the helmet to absorb the energy of a large impact to protect the head contained within the helmet.

[0005] The distribution of forces over a larger area allows a larger cross-section of the expanded polystyrene layer to act in decelerating the impact, thus homogenizing the mechanical response of the assembly to impacts with a surface of reduced area. The structural shell also has other functions, such as wear resistance.

[0006] The proposed body protection equipment may be, for example, a motor vehicle helmet for a car, motorcycle or other vehicle, a bicycle helmet, a ski helmet, a helmet for adventure activities such as mountain climbing, skydiving, paragliding, a sports helmet for example for hockey, baseball, American football, a work helmet for construction sites or mining, as well as other body protection equipment such as elbow pads, wrist guards, knee pads, ankle guards, shoulder pads, boots or / and gloves, shin guards, arm or forearm protection, groin guards, chest or back protection, etc.

[0007] Known body armor includes a shell with a layer of expanded polystyrene bonded to the inside to absorb impact.

[0008] Based on the helmet typology and the test regulations that have to be met, there are structural shells, which are intended to withstand and protect against impacts, and non-structural shells, which only provide protection against abrasion but not against impacts.

[0009] Non-structural shells usually have a very limited thickness, generally less than 1 mm. Generally, these non-structural shells are manufactured by a thermoforming process of straight thin sheets (or plates). This type of non-structural shell relies on the structural resistance to impacts on the underside of the helmet, which is made of a material suitable for absorbing the impact, generally expanded polystyrene or polystyrene foam.

[0010] In the field of bicycle helmets it is common to use a non-structural shell onto which is overmolded an expanded polystyrene layer which, thanks to this overmolding process, is attached in intimate contact with the non-structural shell. DISCLOSURE OF THEINVENTION [Problem to be solved by the invention]

[0011] The non-structural shells are also often made of polycarbonate, which has a much higher melting temperature than that reached during the expanded polystyrene overmolding process, and as a result, while the material is not altered during the overmolding process, the expanded polystyrene often has limited adhesion to the polycarbonate and eventually delaminates over time.

[0012] The structural shell has a high thickness, usually several millimeters, In the most common embodiment the structural shell is made of a plastic material, generally a thermoplastic material, which can be easily manufactured by injection, allowing for cheap and quick production, but requires a significant thickness to achieve sufficient structural strength, producing a heavy structural shell that may be uncomfortable to wear for long periods of time or has disadvantages in competitive sports or high performance situations.

[0013] In cases where a low weight structural shell is required, structural shells made from composite materials are known to provide sufficient structural protection at a smaller thickness and therefore less weight.

[0014] These composite structural shells include glass and / or carbon fiber combined with a thermosetting matrix, such as epoxy resin, polyester, or vinyl ester, which cannot be melted or softened by the application of heat after curing, and therefore when these structural shells are used in an expanded polystyrene overmolding process, the adhesion to the thermosetting matrix is ​​not high, and the adhesion achieved is not very good and delamination is likely to occur, but this is not altered.

[0015] Furthermore, the production of said composite structural shells is more expensive than the production of structural shells made of plastic materials that do not contain reinforcing fibers, and as a result there is a need for solutions that make it possible to reduce these costs.

[0016] In the field of personal protective equipment with structural shells constituting full-face helmets, due to the closed shape that these helmets have, the moulds required are so complex that the expanded polystyrene is not overmolded onto the inside of the structural shell, but rather the expanded polystyrene layer is produced separately and then brought and glued into the concave interior of the structural shell. This solution makes the contact between the structural shell and the expanded polystyrene layer limited to only a few places where the glue is placed, so that said layer is not glued over its entire surface and therefore in this type of helmet the strength and rigidity of the structural shell is not improved when it includes the expanded polystyrene layer. In other words, the mechanical properties of the assembly formed by the structural shell and the impact absorbing material are typical of a system made of two overlapping materials that are not glued together. Moreover, the insertion and gluing process of the two components cannot be automated, which increases the final cost of the helmet.

[0017] If the expanded polystyrene layer is manufactured separately and then proceeds to be bonded to a structural shell made of synthetic material by means of an adhesive, there is the aforementioned limitation of not improving the mechanical properties of the structural shell, which are those of a typical system made of two overlapping materials that are not bonded to each other.

[0018]

[0019]

[0020] There is therefore a need for a solution which makes it possible to obtain a helmet with a high-strength, light-weight and low-cost structural shell which can be securely attached to the expanded polystyrene layer and whose strength is further improved.

[0021] This and other advantages are obtained from the following proposed products: [Means for solving the problem]

[0022] The present invention relates according to a first embodiment to a method for the manufacture of personal protective equipment, known per se to the prior art, comprising the following steps: · manufacturing a structural shell of up to 5mm thickness made of thermoplastic material and defining a concave interior and a convex exterior; Overmold an expanded polystyrene layer so that it overlaps the concave interior of the structural shell and creates an intimate bond to the structural shell.

[0023] It will be understood that the structural shell is the outermost layer of the body protection equipment that is directly impacted in the event of an accident. The structural shell is defined as the concave interior corresponding to the interior of the helmet intended to accommodate the body part of the user to be protected.

[0024] The recessed interior is overlaid with an expanded polystyrene layer which, beneath the structural shell, surrounds the occupant's body part.

[0025] The expanded polystyrene layer distorts and crushes in the event of a severe impact, absorbing energy that is not transferred to the user's body parts, as well as managing the stroke deceleration so as to reduce the maximum acceleration experienced by the head, thus protecting it.

[0026] The process of fabricating the expanded polystyrene layer on the inner surface of the structural shell by overmolding produces adhesion of the expanded polystyrene layer to the concave interior of the structural shell by intimate contact, i.e., all of the outer surface of the expanded polystyrene layer facing and connected to the concave interior of the shell, without gaps or separations or intervening materials such as adhesives between the surfaces, and the expanded polystyrene layer adheres to any of the concave interior surfaces of the structural shell. dent (corner / recessed place / nook) , Ups and downs ( Relief / relief) , or texture (rough surface / texture) is included inside.

[0027] This intimate adhesion is achieved by a process of overmolding a polystyrene foam layer onto the inner surface (or arch web / intrados) of the structural shell. This manufacturing method includes producing the structural shell, placing it in a mold, closing the mold, and placing inside the closed mold a substance consisting of pre-expanded polystyrene and steam at a temperature comprised between 100°C and 130°C, the expanding agent causing the expansion of the expanded polystyrene which molds to conform itself to the concave inner surface of the structural shell, thus remaining intimately bonded without adhesive.

[0028] This feature that the expanded polystyrene layer and the structural shell remain intimately attached despite the absence of adhesive between them makes it possible, on the one hand, to reduce manufacturing costs, since no assembly steps or application of adhesive are required, saving labor and time.

[0029] Furthermore, the close contact between both elements also allows them to cooperate structurally, which makes it possible to increase the final strength of the helmet, improving its functionality, or to reduce the thickness of the structural shell without losing strength thanks to the structural reinforcement provided by the close attachment with the expanded polystyrene layer, which makes it possible to reduce material and weight, thus reducing costs and improving its performance, especially for competitive or high performance applications.

[0030] The present invention proposes, in a manner not known in the prior art, that the steps of manufacturing the structural shell include distributing in a mould a mixture of reinforcing fibres and thermoplastic material, which is stable at or below the melting temperature of the thermoplastic material, closing and heating the mould above the melting temperature of the thermoplastic material to cause melting of the thermoplastic material without damaging the reinforcing fibres, followed by cooling of the mould and hardening of the thermoplastic material with the reinforcing fibres embedded therein to form a composite material.

[0031] Thermoplastics, which are plastics that can be repeatedly melted by heating, exhibit great adhesion to expanded polystyrene, and as a result, the structural integrity of the helmet is greatly improved when this type of thermoplastic material is used.

[0032] The reinforcing fibers increase the strength of the structural shell, which allows the strength of the structural shell to be increased again or maintained, and reduces the thickness of the structural shell, making it lighter and less expensive.

[0033] Thus, the use of a structural shell made from a composite material including thermoplastic and reinforcing fibers, in combination with the use of an expanded polystyrene layer bonded by intimate contact to the concave interior of the structural shell, makes it possible to obtain a helmet having a structural shell that is exactly the same strength as other known helmets but which is thinner and lighter, or makes it possible to obtain a helmet that is stronger than other known helmets at the same weight, all of which at a moderate manufacturing cost, thus providing a helmet that has better performance and a better price than known helmets of the prior art.

[0034] According to a further embodiment of the method, the thermoplastic material is applied to the mould in the form of strands and / or in the form of a coating of reinforcing fibres. Preferably, the thermoplastic material and the reinforcing fibres are applied to the mould in a woven or non-woven fabric.

[0035] Said woven and / or nonwoven fabrics may be placed in a mould to form overlapping layers, in which case it is proposed to produce a structural shell in which at least the layers constituting the outer side of the structural shell are constituted exclusively by strands made of thermoplastic material, the structural shell having a higher density of reinforcing fibres in its concave inner side than in its convex outer side.

[0036] The reinforcing fibers are fibers longer than 30 mm. It is preferred .

[0037] The reinforcing fibers are preferably selected from glass fibers, carbon fibers, aramid fibers, or combinations thereof.

[0038] It is also proposed that the thermoplastic material is preferably polyethylene terephthalate having a melting point comprised between 165° C. and 190° C., or a low-grade melting polyethylene terephthalate.

[0039] It has also been proposed that the reinforcing fibres constitute between 45% and 65% of the total weight of the structural shell.

[0040] According to one embodiment of the method, following production of the structural shell, without removing the structural shell from the production mold, the portion of the mold defining the concave interior is removed and replaced with a new portion of the mold defining an overmolded chamber containing the structural shell, along with the portion of the mold that formed the convex exterior of the structural shell, and an expanded polystyrene layer is overmolded onto the concave interior of the structural shell in the overmolded chamber.

[0041] This may require less tooling in manufacture, reduce the number of operations required in manufacture, and therefore speed up said manufacture.

[0042] According to a second aspect of the invention, a method for producing a medicament for the treatment of a disease, which is known per se and which is obtained by the method described above, A structural shell, maximum thickness 5 mm, made of thermoplastic material and defining a concave inner side and a convex outer side; Expanded polystyrene layers overlap and bond over the entire surface by intimate contact with the concave interior of the structural shell This relates to personal protective equipment having the following features:

[0043] The proposed personal protective equipment further comprises, in a manner not known in the prior art, the following features:

[0044] The structural shell is made from a composite material that includes a thermoplastic material having a pre-set melting temperature that is stable below or at the melting temperature of the thermoplastic material and reinforcing fibers embedded therein.

[0045] According to another embodiment of the body protection equipment, it is proposed that the structural shell may have a higher density of reinforcing fibers in its concave inner side than in its convex outer side, which allows the reinforcing fibers to be exposed on the surface of the concave inner side, or at least to affect the surface finish of said concave inner side, creating small protrusions or holes that make it possible to improve the adhesion of the expanded polystyrene layer, while said defects are avoided on the convex outer side of the structural shell.

[0046] This can be achieved, for example, by producing a structural shell starting from two overlapping layers with different reinforcing fiber densities, typically placing said layers in a mold before closing it, and proceeding to melt the thermoplastic material.

[0047] According to one embodiment of the present invention, the thermoplastic material is polyethylene terephthalate, commonly known by the acronym PET.

[0048] Preferably, it has a melting point comprised between 165°C and 190°C. low grade Molten polyethylene terephthalate is used, which is advantageous to the molding process of the shell, speeding up its manufacture and reducing its costs.

[0049] Polyethylene terephthalate or low grade A structural shell made of molten polyethylene terephthalate would be subject to distortion due to the heat applied during the overmolding process of the expanded polystyrene layer, which is necessary to achieve intimate adhesion. However, the inclusion of reinforcing fibers within said thermoplastic material prevents this problem, thus allowing the use of said thermoplastic material in combination with an expanded polystyrene layer attached by intimate contact, without an adhesive in between.

[0050] The reinforcing fibers can preferably be chosen from glass fibers, carbon fibers, aramid fibers, or combinations thereof, this type of fiber remaining unchanged even during the manufacturing process of the structural shell, which requires melting of a thermoplastic material, said reinforcing fibers being embedded in a mould for shaping the structural shell.

[0051] Preferably, the reinforcing fibres are long fibres, for example having a length greater than 30mm, allowing greater reinforcement of the structural shell.

[0052] The use of long fibres prevents the thermoplastic material from being injected into the mould for the manufacture of the structural shell, since due to their length they become entangled with one another and are unable to flow and remain precisely distributed in a uniform manner within the mould. For this reason, the use of this type of fibre requires that the reinforcing fibres are deposited in their final position within the mould before closing the mould and melting the thermoplastic material for the manufacture of the structural shell.

[0053] Typically, the reinforcing fibers form a woven fabric, i.e., a fabric having a weft and warp structure, and thus form the opposite of a nonwoven fabric, although the use of nonwoven fabrics is also contemplated.

[0054] The fabric is laid down in a mold before closing and heating the mold to obtain a structural shell.

[0055] It is also proposed that the fabric, whether woven or non-woven, in addition to the reinforcing fibers comprises a thermoplastic coating or a thermoplastic coating of the reinforcing fibers prior to closing and heating the mould to produce the structural shell. In this way, at the same time as placing the reinforcing fibers in the mould, a thermoplastic material is also placed, which melts to form the structural shell and leave the reinforcing fibers embedded therein.

[0056] It is proposed that the reinforcing fibres should constitute 45% to 65% of the total weight of the structural shell.

[0057] Typically the expanded polystyrene layer has a minimum thickness of 10mm, preferably at least 15mm.

[0058] Preferably, the proposed body protection equipment is a helmet or a full face helmet, elbow pads, wrist guards, knee pads, ankle guards, shoulder pads, boots or at least one pair of gloves, shin guards, arm or forearm protectors, groin guards, chest or back protectors.

[0059] Other features of the present invention will become apparent from the following detailed description of the illustrative embodiments. [Brief description of the drawings]

[0060] These and other advantages and features will be more fully understood from the following detailed description of illustrative embodiments, taken in conjunction with the accompanying drawings, in which: [Figure 1] FIG. 1 shows a perspective view of a proposed structural shell according to an embodiment, where the helmet is a full-face helmet; [Diagram 2] FIG. 2 shows a cross-sectional view of a full-face helmet formed from a structural helmet as shown in FIG. 1, with a layer of expanded polystyrene intimately attached to the recessed interior of the structural shell. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0061] The accompanying drawings show representative embodiments of illustrative and non-limiting features of the present invention. The present invention relates to manufacturing a structural shell (10) of a maximum thickness of 5 mm made of a thermoplastic material and defining a concave interior (11) and a convex exterior (12); overmolding an expanded polystyrene layer (20) overlying the recessed interior (11) of the structural shell (10); A method for manufacturing a personal protective equipment comprising: The structural shell (10) is produced by distributing within a mold a mixture of thermoplastic material and reinforcing fibers that are stable at a temperature below or equal to the melting point of the thermoplastic material, closing the mold with the mixture of thermoplastic material and reinforcing fibers contained therein, heating the mold above the melting point of the thermoplastic material to cause melting of the thermoplastic material without damaging the reinforcing fibers, and then cooling the mold to harden the thermoplastic material with the reinforcing fibers embedded therein to form a composite material. A manufacturing method is proposed. According to the proposed method, the thermoplastic material (10) and reinforcing fibers are integrated into a woven or nonwoven fabric and placed in a mold, and the overlapping layers of woven and / or nonwoven fabric are placed in the mold. At least the woven and / or nonwoven layers making up the outer surface of the structural shell (10) are constructed solely from strands of thermoplastic material prior to melting to produce the structural shell (10), and the reinforcing fibers are present in a higher density in the concave interior (11) of the structural shell (10) than in its convex exterior (12) after melting and curing. The expanded polystyrene layer (20) is overmolded into the concave interior (11) of the structural shell (10) without any gaps or gaps or intervening material therebetween, thereby causing the expanded polystyrene to be contained within any depressions, undulations, or textures of the concave interior (11), thereby causing the expanded polystyrene layer (20) to adhere to the concave interior (11) through intimate contact therebetween.

[0062] 1 shows a structural shell 10, in this example for a full face helmet, which includes a lower opening through which a user's head is inserted and a visor front opening through which the user can see.

[0063] Obviously, the invention is also applicable to other types of helmets not shown, for example non-full-face helmets, or helmets having ventilation openings, such as bicycle helmets. The body protection equipment may be, for example, elbow pads, wrist guards, knee pads, ankle guards, shoulder pads, boots or gloves, shin guards, arm or forearm guards, groin guards, chest or back protectors.

[0064] The structural shell 10 at least partially faces the head of a helmet user and defines a concave interior 11 intended to surround the head, and a convex exterior 12 which remains exposed and is initially subjected to impact.

[0065] The structural shell 10 is made from a composite material, that is, a composite material incorporating thermoplastic materials with embedded reinforcing fibers.

[0066] The proposed helmet also includes an expanded polystyrene layer 20 located within the structural shell 10, as shown in FIG.

[0067] The expanded polystyrene layer 20 is attached to the recessed interior 11 of the structural shell 10 by a bonding means that does not require an intervening adhesive; i.e., there are no gaps, spaces or separations between the structural shell 10 and the expanded polystyrene layer 20. This is accomplished by overmolding the expanded polystyrene layer 20 onto the structural shell 10.

[0068] In this embodiment, it is proposed that the structural shell has a thickness of 2 mm to 4 mm.

[0069] In accordance with a preferred embodiment, the thermoplastic material that integrates the structural shell 10 is polyethylene terephthalate, commonly known as PET, and the reinforcing fibers are long glass fibers, carbon fibers, or aramid fibers, or a mixture thereof. [Industrial Applicability]

[0070] Polyethylene terephthalate is inexpensive, tough, durable, easy to manufacture, and allows for excellent intimate bonding with the expanded polystyrene layer 20. Reinforcing fibers embedded within the polyethylene terephthalate increase its structural strength and prevent it from being distorted by heat during the overmolding process of the expanded polystyrene layer.

[0071] In addition, low temperature, which is a thermoplastic material having a melting point between 165℃ and 190℃ Grade Melted Polyethylene Terephthalate (low-melt polyethylene terephthalate) It is preferred to use a low melting point polyethylene terephthalate, which allows for lower manufacturing costs and faster production without sacrificing strength. Due to the stability provided by the reinforcing fibers, the low grade molten polyethylene terephthalate does not distort during operation of the expanded polystyrene layer 20.

[0072] The following is an invention described at the beginning of the present application. <Claim 1> - manufacturing a structural shell (10) of a maximum thickness of 5 mm, made of a thermoplastic material and defining a concave interior (11) and a convex exterior (12); overmolding an expanded polystyrene layer (20) overlying the recessed interior (11) of the structural shell (10) to create an intimate contact bond to said structural shell (10); A method for manufacturing a personal protective equipment, comprising: The structural shell (10) comprises: Distributing and arranging in a mold a mixture of a thermoplastic material and a reinforcing fiber that is stable at a temperature equal to or lower than the melting point of the thermoplastic material; heating and closing the mold at a temperature above the melting point of the thermoplastic material to cause melting of the thermoplastic material without damaging the reinforcing fibers; curing said thermoplastic material with said reinforcing fibers embedded therein to form a composite material, followed by cooling of the mold; and A method for producing personal protective equipment, comprising the steps of: <Claim 2> The method of claim 1 , wherein the thermoplastic material is placed in the mold in the form of strands and / or coating the reinforcing fibers. <Claim 3> The method according to claim 2, wherein the thermoplastic material (10) and the reinforcing fibers are integrated into a woven or non-woven fabric and placed in the mold. <Claim 4> The method of claim 3, wherein overlapping layers of woven and / or nonwoven fabric are molded. <Claim 5> 5. The method of claim 4, wherein at least the layers constituting the outer surface of the structural shell (10) are constituted exclusively by strands of thermoplastic material, producing a structural shell (10) having a higher density of reinforcing fibers on its concave inner surface (11) than on its convex outer surface (12). <Claim 6> 5. The method according to claim 1, wherein the reinforcing fibers are long fibers or long fibers having a length exceeding 30 mm. <Claim 7> 3. The method according to claim 1 or 2, wherein the thermoplastic material is polyethylene terephthalate, low-grade melting polyethylene terephthalate, or low-grade melting polyethylene terephthalate having a melting temperature comprised between 165°C and 190°C. <Claim 8> 4. The method according to claim 1, wherein the reinforcing fibers are selected from the group consisting of fiberglass, carbon fibers, aramid fibers, and combinations thereof. <Claim 9> The method of any one of claims 1 to 4, wherein the reinforcing fibers comprise 45% to 65% of the total weight of the structural shell (10). <Claim 10> 7. The method of claim 1, wherein following production of the structural shell, without removing the structural shell from the production mold, the portion of the mold defining the concave interior (11) is removed and replaced by a new mold portion that, together with the portion of the mold that molded the convex exterior (12) of the structural shell (10), defines an overmolded chamber containing the structural shell, and a polystyrene layer is overmolded onto the concave interior (11) of the structural shell (10) in the overmolded chamber. <Claim 11> a structural shell (10) made of a thermoplastic material and having a thickness of up to 5 mm, defining a concave interior (11) and a convex exterior (12); comprising an expanded polystyrene layer (20) overlapping and adhered to said concave interior (11) of said structural shell (10) over its entire surface by intimate contact therewith; A personal protective equipment manufactured by the method of any one of claims 1 to 10. <Claim 12> 12. The body armor of claim 11, wherein the structural shell (10) has a higher density of reinforcing fibers on its inner concave surface (11) than on its outer convex surface (12). <Claim 13> 14. The body protection equipment according to claim 12 or 13, wherein the thermoplastic material is polyethylene terephthalate, low-grade melting polyethylene terephthalate or low-grade melting polyethylene terephthalate having a melting point comprised between 165°C and 190°C. <Claim 14> 14. The personal protective equipment according to claim 11, wherein the reinforcing fibers are selected from glass fibers, carbon fibers, aramid fibers, or combinations thereof. <Claim 15> The personal protective equipment according to any one of claims 11 to 14, wherein the reinforcing fibers are long fibers or long fibers having a length exceeding 30 mm. <Claim 16> The personal protective equipment according to any one of claims 11 to 15, wherein the reinforcing fibers form a woven or nonwoven fabric within the composite material. <Claim 17> 17. The personal protective equipment of claim 11, wherein the reinforcing fibers comprise between 45% and 65% of the total weight of the structural shell (10). <Claim 18> The personal protective equipment according to any one of claims 7 to 11, wherein the personal protective equipment is a helmet, a full-face helmet, an elbow pad, a wrist guard, a knee pad, an ankle guard, a shoulder pad, at least one of a boot or a glove, a shin guard, an arm or forearm protector, a groin guard, or a chest or back protector.

Claims

1. - manufacturing a structural shell (10) made of thermoplastic material and defining a concave interior (11) and a convex exterior (12) with a maximum thickness of 5 mm; overmolding an expanded polystyrene layer (20) overlying the recessed interior (11) of the structural shell (10); A method for manufacturing a personal protective equipment, comprising: The structural shell (10) comprises: Distributing and arranging in a mold a mixture of a thermoplastic material and a reinforcing fiber that is stable at a temperature equal to or lower than the melting point of the thermoplastic material; heating the mold above the melting point of the thermoplastic material to cause melting of the thermoplastic material without damaging the reinforcing fibers and closing the mold; curing said thermoplastic material with said reinforcing fibers embedded therein to form a composite material, followed by cooling of the mold; and Manufactured by The thermoplastic material (10) and the reinforcing fibers are integrated into a woven or nonwoven fabric and placed in the mold; A laminate of woven and / or nonwoven layers is placed in the mold; at least the woven and / or nonwoven layers constituting the outer surface of said structural shell (10) are constituted exclusively by strands of thermoplastic material prior to melting to produce said structural shell (10), said reinforcing fibers being present in a higher density in said concave interior (11) of said structural shell (10) than in said convex exterior (12) thereof after melting and hardening; said expanded polystyrene layer (20) being overmolded onto said concave interior (11) of said structural shell (10) without any gaps or separations or intervening material therebetween, thereby resulting in the inclusion of the expanded polystyrene inside any indentations, undulations or textures of said concave interior (11), thereby resulting in adhesion of said expanded polystyrene layer (20) to said concave interior (11) through intimate contact therebetween; A method for manufacturing personal protective equipment, comprising the steps of:

2. The method of claim 1 , wherein the thermoplastic material is placed in the mold in the form of strands and / or coating the reinforcing fibers.

3. 3. The process according to claim 1 or 2, wherein the thermoplastic material is polyethylene terephthalate or a low-grade melting polyethylene terephthalate having a melting temperature comprised between 165°C and 190°C.

4. The method according to any one of claims 1 to 3, wherein the reinforcing fibers are selected from the group consisting of fiberglass, carbon fibers, aramid fibers, or combinations thereof.

5. The method of any of claims 1 to 4, wherein the reinforcing fibers comprise between 45% and 65% of the total weight of the structural shell (10).

6. 7. The method of claim 1, wherein following production of the structural shell, without removing the structural shell from the production mold, the portion of the mold defining the concave interior (11) is removed and replaced by a new mold part that, together with the portion of the mold that molded the convex exterior (12) of the structural shell (10), defines an overmolded chamber containing the structural shell, and a polystyrene layer is overmolded onto the concave interior (11) of the structural shell (10) in the overmolded chamber.

7. a structural shell (10) made of a thermoplastic material and having a thickness of up to 5 mm, defining a concave interior (11) and a convex exterior (12); 1. A body armor comprising an expanded polystyrene layer (20) overlapping and bonded to all surfaces of the concave interior (11) of the structural shell (10), the structural shell (10) being comprised of a mixture of a thermoplastic material having a predetermined melting point and reinforcing fibers stable at temperatures below the melting point of the thermoplastic material; the reinforcing fibers form a woven or non-woven fabric within the composite material; the reinforcing fibers are present in a higher density in the concave interior (11) of the structural shell (10) than in the convex exterior (12) thereof; said expanded polystyrene layer (20) being in intimate contact with said concave interior (11) of said structural shell (10) without gaps or separations or intervening material therebetween, thereby causing the inclusion of the expanded polystyrene inside any depressions, undulations or textures of said concave interior (11) and bonding said expanded polystyrene layer (20) to said concave interior (11) through the intimate contact therebetween; A body armor manufactured by the method of any one of claims 1 to 6.

8. 8. The body protection equipment according to claim 7, wherein the thermoplastic material is polyethylene terephthalate or a low-grade melting polyethylene terephthalate having a melting point comprised between 165°C and 190°C.

9. 9. The body protection device according to claim 7 or 8, wherein the reinforcing fibers are selected from glass fibers, carbon fibers, aramid fibers, or combinations thereof.

10. The personal protective equipment according to any one of claims 7 to 9, wherein the reinforcing fibers are long fibers having a length exceeding 30 mm.

11. A body protection device according to any one of claims 7 to 10, wherein the reinforcing fibres constitute between 45% and 65% of the total weight of the structural shell (10).

12. The body protector according to any one of claims 7 to 11, wherein the body protector is a helmet, a full-face helmet, an elbow pad, a wrist guard, a knee pad, an ankle guard, a shoulder pad, at least one of a boot or a glove, a shin guard, an arm or forearm protector, a groin guard, or a chest or back protector.