Image forming apparatus
By setting specific surface roughness parameters for the intermediate transfer belt and using a high hardness coating on the scraper, the apparatus achieves enhanced scratch resistance and durability, addressing the wear issues caused by conventional hardened scrapers.
Patent Information
- Application Number
- JP2023046224
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-23
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2043-03-23
AI Technical Summary
Existing image forming apparatuses face issues with scratch resistance and durability of intermediate transfer belts due to the use of highly hardened scrapers, which accelerate wear and lead to a shortened lifespan, and conventional methods fail to effectively address this problem.
The solution involves specifying surface roughness parameters for the intermediate transfer belt, including Spd (peak density) and Sal (minimum autocorrelation length) such that Spd×Sal² < 5×10⁶, with a high hardness coating on the scraper, to prevent scratches and enhance durability.
This approach significantly reduces the occurrence of scratches on the intermediate transfer belt, ensuring a longer lifespan and improved reliability of the image forming apparatus by maintaining the integrity of the belt surface.
Smart Images

Figure 2024135506000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to an electrophotographic image forming apparatus, such as a light-duty printing machine, a copier, a printer, etc., in which an electrostatic latent image formed on an electrostatic latent image carrier is developed and visualized with a charged toner, and then transferred and fixed to a recording material. More specifically, the present disclosure relates to the scratch resistance of an intermediate transfer belt, which is an image carrier in a transfer section of an electrophotographic process. [Background technology]
[0002] In image forming devices such as light-duty printing machines, copiers, and printers, the toner on the photoconductor, which is an image carrier, is transferred to paper to provide a print image as desired by the user. There are two transfer methods: a direct transfer method in which the toner is transferred from the photoconductor to the paper, and an intermediate transfer method in which the toner is transferred from the photoconductor to an intermediate transfer section, and then transferred from the intermediate transfer section to the paper in a secondary transfer section. The intermediate transfer method is used to transfer a full-color image to paper by overlapping the toner of each color from the developer and photoconductor at the intermediate transfer section. This intermediate transfer method has the advantages of improved image quality and faster operation, and is therefore often used in high-speed full-color machines.
[0003] The image carrier in the intermediate transfer section is generally an intermediate transfer belt. To ensure high transferability, the intermediate transfer belt contains conductive material to make it semi-conductive, while to ensure toughness, it is made of a high-strength resin such as polyimide. The reason for the requirement of toughness is that the intermediate transfer belt is subjected to high tension by rollers on the inside of the belt to stabilize the transfer position. A driving force is applied to the intermediate transfer belt by a driving roller provided on the inside of the belt. Furthermore, the belt surface of the intermediate transfer belt is subjected to load due to contact with the photoconductor, secondary transfer roller, and paper. In particular, high pressure is applied by a cleaning device that removes toner remaining on the intermediate transfer belt after secondary transfer.
[0004] A cleaning device is necessary to obtain sufficient image quality. There are various types of cleaning devices. Generally, a cleaning blade is used for cleaning devices. The cleaning blade is an elastic body such as urethane elastomer, and is brought into contact with the intermediate transfer belt in the counter direction to the rotation direction of the intermediate transfer belt to remove toner from the intermediate transfer belt. There are two main types of cleaning blades: one that is fixed in position and comes into contact with the intermediate transfer belt by pressure due to the blade's bending, and one that comes into contact with the intermediate transfer belt by pressure due to a spring.
[0005] When the cleaning blade comes into counter contact, the edge of the cleaning blade is subjected to a load, which may cause damage. To prevent this damage, toner is always present on the edge of the cleaning blade as a lubricant. In the initial stage of production, the blade is coated with toner before assembly, and a mode for supplying toner is provided during use. Furthermore, to ensure a stable supply of toner, a toner storage roller is placed upstream of the cleaning blade in the forward direction, so that the stored toner can be constantly sent to the cleaning blade even in cases of low printing rates.
[0006] Even if damage to the cleaning blade edge is prevented and wear is suppressed in this way, cleaning failures occur due to foreign matter such as paper dust getting caught in the cleaning blade. In addition, cleaning failures occur when the cleaning blade wears out due to long-term use. Therefore, an image forming apparatus has been proposed in which a cleaning device is provided downstream of the cleaning blade.
[0007] Unlike the first cleaning device, the second cleaning device uses a flexible metal scraper. This is because if the second cleaning device installed downstream of the first cleaning device is made of an elastic body made of urethane elastomer, it will supply less toner to the edge and will be damaged more quickly than the first cleaning device. By using a metal scraper for the second cleaning device, it has become possible to create a cleaning system that is reliable over the long term.
[0008] Prior art documents disclosing the above-described image forming apparatus include JP-A-2018-036287 (Patent Document 1), JP-A-2012-113197 (Patent Document 2), and JP-A-2004-287012 (Patent Document 3). [Prior art documents] [Patent documents]
[0009] [Patent Document 1] JP 2018-036287 A [Patent Document 2] JP 2012-113197 A [Patent Document 3] JP 2004-287012 A Summary of the Invention [Problem to be solved by the invention]
[0010] On the other hand, as a method for improving the scratch resistance and durability of an intermediate transfer belt, it has been proposed to specify the roughness of the belt surface. In addition to the surface roughness of the intermediate transfer belt, a method for further improving the scratch resistance and durability by increasing the hardness of the surface has also been proposed.
[0011] In response to this, the cleaning member on the intermediate transfer belt surface is also hardened at the edge to prevent wear against the hardened belt surface and improve durability. Specifically, the resin surface of the belt is hardened by coating it with glass or the like. As the belt surface is made hard, wear of the metal scraper is accelerated due to durability, shortening its lifespan. Therefore, by using a scraper with a coating harder than the intermediate transfer belt surface, the shortening of lifespan is suppressed.
[0012] However, by making the scraper surface harder, the scraper would scratch the belt surface, and the scratch resistance and durability could not be improved by simply specifying the surface roughness as in the past.
[0013] This disclosure has been made to solve the above-mentioned problems, and aims to provide an image forming device having a scratch-resistant belt by identifying parameters for the surface condition of an intermediate transfer belt that can prevent scratches even with a hardened scraper, and by specifying these parameters. [Means for solving the problem]
[0014] [Configuration 1]: This disclosure relates to an image forming apparatus having an intermediate transfer belt and a member for cleaning residual toner that is in contact with the intermediate transfer belt, and among the physical properties that indicate the surface roughness of the intermediate transfer belt, Spd (peak density) and Sal (minimum autocorrelation length) are Spd × Sal 2 <5×10 6 Satisfies [Equation 1].
[0015] [Configuration 2]: The image forming apparatus according to [Configuration 1], wherein the intermediate transfer belt has a base layer and a coating layer that forms irregularities on the surface of the base layer.
[0016] [Configuration 3]: The image forming apparatus according to [Configuration 2], wherein the coating layer of the intermediate transfer belt is a layer containing Si as a main component.
[0017] [Configuration 4]: An image forming apparatus according to any one of [Configuration 1] to [Configuration 3], wherein the cleaning member is a scraper that is in contact with the intermediate transfer belt so as to scrape off the residual toner on the surface of the intermediate transfer belt.
[0018] [Configuration 5]: The image forming apparatus according to [Configuration 4], wherein the scraper includes a flexible metal scraper.
[0019] [Configuration 6]: The image forming apparatus according to [Configuration 5], wherein the scraper has a high-hardness scraper coat layer at least on a portion of the metal scraper that contacts the intermediate transfer belt.
[0020] [Configuration 7]: An image forming apparatus according to any one of [Configuration 1] to [Configuration 6], wherein there is no member on the inside of the intermediate transfer belt facing the portion where the cleaning member contacts the intermediate transfer belt, and the tension of the intermediate transfer belt and the amount of pressure applied by the contact pressure of the cleaning member are adjusted.
[0021] [Configuration 8]: In the image forming apparatus according to any one of [Configuration 1] to [Configuration 7], when the Sal of the physical properties indicating the surface roughness of the intermediate transfer belt is 20 μm or less (Sal≦20 μm), the relationship between the Spd and the Sal is Spd×Sal 2 <4×10 6 Satisfies [Equation 2].
[0022] [Configuration 9]: An image forming apparatus according to any one of [Configuration 1] to [Configuration 8], wherein the intermediate transfer belt is a belt in which one of the manufacturing conditions for forming the Sal (autocorrelation length) and the Spd (peak density) is the relative humidity during coating, and the intermediate transfer belt is manufactured at a relative humidity of 45% or less.
[0023] [Configuration 10]: The image forming apparatus according to any one of [Configuration 1] to [Configuration 9], wherein, among the physical properties indicating the surface roughness of the intermediate transfer belt, Sa (arithmetic mean height) is 0.2 or less.
[0024] [Configuration 11]: The image forming apparatus according to any one of [Configuration 1] to [Configuration 10], wherein, among the physical properties indicating the surface roughness of the intermediate transfer belt, Sq (root mean square height) is 1 or less.
[0025] [Configuration 12]: The image forming apparatus according to any one of [Configuration 1] to [Configuration 11], wherein, among the physical properties indicating the surface roughness of the intermediate transfer belt, Sdr (interface developed area ratio) is 0.002 or more.
[0026] [Configuration 13]: An image forming apparatus according to any one of [Configuration 1] to [Configuration 12], wherein, among the physical properties indicating the surface roughness of the intermediate transfer belt, Smr1 (the load area ratio separating the protruding peaks and the core) is 10 or less.
[0027] [Configuration 14]: The image forming apparatus according to any one of [Configuration 1] to [Configuration 13], wherein, among the physical properties indicating the surface roughness of the intermediate transfer belt, Vmp (solid volume of the peaks) is 0.004 or more.
[0028] [Configuration 15]: The image forming apparatus according to any one of [Configuration 1] to [Configuration 14], wherein, among the physical properties indicating the surface roughness of the intermediate transfer belt, Vmc (the actual volume of the core portion) is 0.008 or more. Effect of the Invention
[0029] According to this image forming apparatus, by finding parameters for the surface condition of the intermediate transfer belt that can prevent scratches even with a scraper with a high hardness and specifying these parameters, it is possible to provide an image forming apparatus having a belt that is resistant to scratches. [Brief description of the drawings]
[0030] [Figure 1] 1 is a schematic cross-sectional view of an image forming apparatus. [Diagram 2] FIG. 2 is a schematic cross-sectional view of the cleaning device. [Diagram 3] 6 is an enlarged view of a contact portion of the second cleaning device. FIG. [Figure 4] FIG. 11 is a diagram showing the ranges of surface roughness parameters Sal and Spd of the intermediate transfer belt surface. [Diagram 5] FIG. 11 is an enlarged view showing an increase in scratches on the surface of the intermediate transfer belt, which is a problem to be solved. [Figure 6] FIG. 2 is an enlarged view showing the small protrusions of the scraper edge, which are the cause of the problem to be solved. [Figure 7A] FIG. 13 is a diagram showing an observed image of the surface of the intermediate transfer belt according to the embodiment and a profile showing its height (coefficient less than 5, low Sal, high Spd). [Figure 7B] FIG. 13 is a diagram showing an observed image of the surface of an intermediate transfer belt of a comparative example and a profile showing the height (coefficient of 5 or more). [Figure 7C] 1A and 1B are diagrams showing an observed image of the surface of an intermediate transfer belt according to an embodiment and a profile showing its height (coefficient less than 5, high Sal, low Spd). [Figure 8A] 11A and 11B are diagrams illustrating a contact state between the intermediate transfer belt and the scraper in the embodiment (coefficient less than 5, low Sal, high Spd). [Figure 8B] FIG. 13 is a diagram showing a contact state (factor 5 or more) between the intermediate transfer belt and the scraper in the comparative example. [Figure 8C] 11A and 11B are diagrams illustrating a contact state between the intermediate transfer belt and the scraper in the embodiment (coefficient less than 5, high Sal, low Spd). [Figure 9] 6 is a diagram showing coefficients of a relational expression of surface roughness parameters of the intermediate transfer belt surface according to the embodiment; [Figure 10] FIG. 11 is a diagram showing the relationship between the relative humidity when the surface layer of the intermediate transfer belt is applied and the likelihood of scratches occurring. [Figure 11] FIG. 4 is a diagram showing the ranges of surface roughness parameters Sal and Sa of the intermediate transfer belt surface according to the embodiment. [Figure 12] FIG. 4 is a diagram showing the ranges of surface roughness parameters Sal and Sq of the intermediate transfer belt surface according to the embodiment. [Figure 13] 6 is a diagram showing the ranges of surface roughness parameters Sal and Sdr of the intermediate transfer belt surface according to the embodiment; [Figure 14] FIG. 4 is a diagram showing the ranges of surface roughness parameters Sal and Smr1 of the intermediate transfer belt surface according to the embodiment. [Figure 15] 6 is a diagram showing the ranges of surface roughness parameters Sal and Vmp of the intermediate transfer belt surface according to the embodiment; [Figure 16] FIG. 4 is a diagram showing the ranges of surface roughness parameters Sal and Vmc of the intermediate transfer belt surface according to the embodiment. [Figure 17] FIG. 11 is a table showing a list of surface roughness parameter conditions and evaluation results of the intermediate transfer belt surface in Examples and Comparative Examples. [Figure 18]FIG. 4 is a table showing a list of surface roughness parameter conditions of the intermediate transfer belt surface, the presence or absence of coating, and evaluation results of the intermediate transfer belt surface in Examples and Comparative Examples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0031] Hereinafter, an image forming apparatus according to an embodiment will be described with reference to the drawings. In each embodiment described below, when numbers, quantities, etc. are mentioned, the scope of the present invention is not necessarily limited to those numbers, quantities, etc., unless otherwise specified. The same reference numbers are used for the same parts or corresponding parts, and duplicate descriptions may not be repeated.
[0032] (Image forming apparatus 100) 1 shows a schematic configuration diagram of a main part of an electrophotographic process of a full-color tandem type electrophotographic image forming apparatus 100. FIG.
[0033] This image forming apparatus 100 performs image formation by transferring and fixing a toner image formed on a photoconductor 1 by a dry electrophotographic method onto a recording medium T such as paper.
[0034] This image forming apparatus 100 has a photoconductor 1 for forming and carrying an electrostatic latent image on its surface. Around the photoconductor 1, the following are arranged in order along the rotation direction of the photoconductor 1: a charging device 2 for uniformly charging the photoconductor 1; an exposure device 3 for exposing the surface of the photoconductor 1 to form an electrostatic latent image; a developing device 4 for visualizing the electrostatic latent image with charged toner by electric field force; a primary transfer roller 6 for transferring each color toner image developed on the photoconductor 1 onto an intermediate transfer belt 5 by electric field force; a photoconductor cleaning device 7 for removing residual toner on the photoconductor 1; and a lubricant application device 8 for the photoconductor.
[0035] A secondary transfer roller 10 is disposed downstream in the moving direction of the intermediate transfer belt 5, facing the secondary transfer opposing roller 9, and transfers the toner image on the intermediate transfer belt 5 to the recording medium T by electric field force. The toner image transferred onto the recording medium T is melted by heat and pressure applied by a fixing device 11, and is fixed onto the recording medium T. Residual toner on the intermediate transfer belt 5 is cleaned and removed by a first cleaning device 12 for the first intermediate transfer belt and a second cleaning device 13 for the second intermediate transfer belt.
[0036] The intermediate transfer belt 5 is made of a material in which conductive material is added to polyimide. The intermediate transfer belt cleaning device is composed of a first cleaning device and a second cleaning device. The first cleaning device is a cleaning blade made of solid rubber such as polyurethane or NBR. The second cleaning device is a scraper 13 made of flexible metal such as stainless steel.
[0037] The photoconductor, charging device, exposure device, developing device, cleaning device, fixing device, conveying device, and the like used in the image forming apparatus 100 may use any known electrophotographic technology. The image carrier may be a photoconductor or an intermediate transfer belt. Depending on the system, it may be a secondary transfer belt. The materials of the intermediate transfer belt 5 and the first cleaning device 12 are not limited to those mentioned above.
[0038] (Cleaning device) A schematic configuration diagram of a cleaning device according to an embodiment is shown in Fig. 2. Fig. 2 is a schematic cross-sectional view of the cleaning device. This cleaning device removes residual toner from the intermediate transfer belt 5 by a cleaning blade 12, which is a first cleaning device, and further removes the residual toner from the intermediate transfer belt 5 by a scraper 13, which is a second cleaning device.
[0039] The cleaning blade 12 has an elastic blade 12-1 and a support member 12-2. The cleaning blade 12 may be a spring-pressure-type cleaning blade using a spring (not shown), or a fixed-pressure-type cleaning blade fixed to the cleaning unit housing 15 by screws (not shown) or the like. The scraper 13 has a flexible metal scraper 13-1, a first support member 13-2, and a second support member 13-3. Like the cleaning blade 12, the scraper 13 may be a spring-pressure-type scraper or a fixed-pressure-type scraper.
[0040] At the contact position of the cleaning blade 12, which is the first cleaning device, a cleaning facing roller 19 is required on the back side of the intermediate transfer belt 5. The presence of the cleaning facing roller 19 causes the elastic blade 12-1 to bend and obtain a contact force. The edge of the elastic blade 12-1 fits closely along the surface of the intermediate transfer belt 5 to form a stable nip for cleaning.
[0041] On the other hand, the contact position of the scraper 13, which is the second cleaning device, must be such that there is nothing on the back side of the intermediate transfer belt 5. However, the scraper 13 is designed to contact the intermediate transfer belt 5 at a portion where sufficient tension is applied between rollers such as the cleaning opposing roller 19 and the drive roller 20. By contacting the tensioned intermediate transfer belt 5, the flexible metal scraper 13-1 bends and a contact force is obtained. The intermediate transfer belt 5 comes into close contact with the edge of the metal scraper 13-1, enabling cleaning.
[0042] The toner on the intermediate transfer belt 5 is removed by the cleaning blade 12, enters the cleaning unit 15, and is transported by the transport screw 14 into a waste toner bottle (not shown). Toner that could not be removed due to damage or wear of the cleaning blade 12 through use, or due to the accidental ingestion of foreign matter, is removed by the metal scraper 13-1, enters the cleaning unit 15, and is transported by the transport screw 14 into a waste toner bottle (not shown).
[0043] Some of the toner removed by cleaning blade 12 is accumulated in toner reservoir 18 by toner reservoir roller 16. A constant amount of toner layer is formed on toner reservoir roller 16 by regulating member 17, and the toner is transferred at the position where it contacts intermediate transfer belt 5 and supplied to cleaning blade 12. This toner reservoir roller 16 constantly supplies toner as a lubricant to the edge of cleaning blade 12, thereby preventing damage to the edge of cleaning blade 12 and achieving a long life.
[0044] On the other hand, only toner that cannot be removed by cleaning blade 12 reaches metal scraper 13-1, so a cleaning blade cannot be used, which would be damaged if there is no toner on the edge as a lubricant, and scraper 13 is used instead. Therefore, there is no need to store the toner removed by metal scraper 13-1, and all the removed toner is transported by transport screw 14 into a waste toner bottle (not shown).
[0045] The toner storage roller 16 is a foam roller made of NBR or the like, but the material and configuration are not limited to this. The regulating member 17 is a flexible metal member made of SUS or the like, but the material and configuration are not limited to this. Similarly, the materials of the parts used in the cleaning unit are not particularly limited. The configuration is also not limited to the above, and a roller or brush that adjusts the toner polarity may be used.
[0046] FIG. 3 shows a schematic diagram of the scraper 13, which is the second cleaning device. FIG. 3 is an enlarged view of the contact portion of the second cleaning device. In FIG. 3, the intermediate transfer belt 5 has a base layer 5-1, and the surface of the base layer 5-1 is coated with a high-hardness belt surface layer 5-2 mainly composed of Si for the purpose of improving transferability and durability. On the other hand, the belt contact portion surface of the metal scraper 13-1, which is the second cleaning device, is coated with a high-hardness scraper coat layer 13-4 mainly composed of carbon for the purpose of improving durability. The materials and configurations of the coating of the intermediate transfer belt 5 and the scraper are not limited to those described above.
[0047] Fig. 4 shows the relationship between parameters Sal (minimum autocorrelation length) and Spd (peak density) representing the state of the surface layer of the intermediate transfer belt. Fig. 4 shows the ranges of the surface roughness parameters Sal and Spd of the intermediate transfer belt surface.
[0048] Figure 4 shows the Sal and Spd measurements of the intermediate transfer belt with a scratch-prone surface layer and the intermediate transfer belt with a scratch-resistant surface layer in model A, and similarly the intermediate transfer belt with a scratch-prone surface layer and the scratch-resistant surface layer in model B, plotted on a graph. To classify the intermediate transfer belt into scratch-prone and scratch-resistant intermediate transfer belts, a belt scratch test was conducted and the scratch susceptibility was quantified. Details will be described later.
[0049] Sal and Spd of the surface layer of the intermediate transfer belt are surface roughness parameters that indicate the surface condition, and were measured by the following method. The measuring device was a Keyence VK-3100, a violet laser type of the VK-X3000 series laser microscope, and the surface roughness of the intermediate transfer belt surface was measured without contact. Since the surface layer is transparent, a 10x white interference objective lens (CF IC EPIPlan DI 10X) was used to measure the height and roughness by observing the interference fringes of light. The field of view was 1394 x 1045 μm, and each surface roughness parameter was measured over the entire area. The intermediate transfer belt was measured at six locations in total, two in the circumferential direction, and three locations at the center and both ends in the longitudinal direction (approximately 50 mm from the ends of the intermediate transfer belt), and the average value was calculated.
[0050] The 24 parameters measured are as follows: Sa (arithmetic mean height), Sz (maximum height roughness), Str (aspect ratio of surface texture), SPc (arithmetic mean curvature of peaks), Sdr (ratio of developed area of interface), Sq (root mean square height), Ssk (skewness), Sku (kurtosis), Sp (maximum peak height), Sv (maximum valley depth), Sal (minimum autocorrelation length), Std (direction of surface texture), Sdq (root mean square root slope), Spd (peak density), Sk (level difference in the core), Spk (protruding peak height), Svk (protruding valley height), Smr1 (area material ratio separating the protruding peak and core), Smr2 (area material ratio separating the core and protruding valley), Sxp (pole height), Vvv (spatial volume of the protruding valley), Vvc (spatial volume of the core), Vmp (actual volume of the peak), Vmc (actual volume of the core).
[0051] When the correlation between each parameter and scratch susceptibility was checked, several highly correlated parameters were extracted, but an index that could clearly determine scratch susceptibility with a single parameter could not be found. Therefore, when checking for a relationship between two parameters that could indicate scratch susceptibility, an index that could determine scratch susceptibility was found from the relationship between Sal (minimum autocorrelation length) and Spd (peak density).
[0052] Sal (minimum autocorrelation length) indicates the shortest distance that is consistent when the coordinates are shifted horizontally, and indicates the period of the unevenness. Its unit is μm. Meanwhile, Spd (peak density) indicates the number of peaks present per unit area. Its unit is pieces / mm 2 These two parameters affect each other. For example, if we assume that the bumps are arranged in an orderly fashion, Spd = (1000 / Sal) 2 However, in reality, the unevenness of the surface is not arranged in an orderly fashion, and the shape may be distorted or the arrangement of the unevenness may be uneven. If we express this variation as the coefficient K, it is Spd=(1000 / Sal) 2 × K, so K × 10 6 =Spd×Sal 2 In other words, if the belt surface is coated uniformly, the coefficient K will be close to 1, and if the coating is uneven and clumped, the coefficient K will be larger.
[0053] As shown in Figure 4, the Sal of intermediate transfer belts that are less susceptible to scratches varies greatly depending on the model, but is close to the line with coefficient 1 and at least smaller than the line with coefficient 5. On the other hand, intermediate transfer belts that are more susceptible to scratches are larger than the line with coefficient 5, indicating that they have an uneven coating. The surface layers of models A and B have different shapes, but the poor model A has a large Sal, with a coefficient of 5 or more. The poor model B has a large Spd, with a coefficient of 5 or more.
[0054] As shown in FIG. 4, the coefficient of the relation between Sal and Spd of the surface layer of the intermediate transfer belt that is resistant to scratches is less than 5. 2 <5×10 6 It is specified as [Formula 1].
[0055] The present disclosure is directed to an embodiment shown in the schematic configuration diagrams of Figures 2 and 3, the surface roughness parameters of the surface layer of the intermediate transfer belt in Figure 4, and [Formula 1]. In contrast, a conventional cleaning system for an intermediate transfer belt has the same schematic configuration as that shown in Figures 2 and 3 of the present disclosure, but differs in that it does not satisfy the surface roughness parameters of the surface layer of the intermediate transfer belt in Figure 4 and [Formula 1].
[0056] This difference can also be seen in Figure 4. For example, if only model A is used, the susceptibility to scratches can be determined using Sal alone. However, if model B is added, the susceptibility to scratches cannot be determined using Sal alone. Similarly, if only model B is used, the susceptibility to scratches can be determined using Spd alone, but if model A is added, the susceptibility to scratches cannot be determined using Spd alone. Although not shown, the same is true for other surface roughness parameters and line roughness parameters.
[0057] This corresponds to JP 2012-113197 A (Patent Document 1) and JP 2004-287012 A (Patent Document 2), which specify a line roughness parameter for scratches on the surface of an intermediate transfer belt. While it may be possible to determine the susceptibility to scratches with one parameter under certain belt surface conditions, it is not possible to determine the susceptibility to scratches for all belt surfaces, and therefore it is not possible to solve the problem of scratches on the intermediate transfer belt.
[0058] Here, a description will be given of scratches on the intermediate transfer belt that occur when a new scraper 13 is mounted, which is a problem to be solved by the present disclosure, with reference to Fig. 5. Fig. 5 is an enlarged view showing an increase in scratches on the surface of the intermediate transfer belt, which is a problem to be solved.
[0059] Figure 5 shows scratches on the surface of the intermediate transfer belt 5 observed under a microscope at 1000x magnification. As shown in Figure 5, these scratches are thin and shallow, each about 1 μm wide and 1 μm deep, and as the intermediate transfer belt 5 rotates many times due to its drive, the number of scratches increases in the width direction, and when the collection of thin scratches reaches a width of several tens to several hundreds of μm in total, they become noticeable to the naked eye. Since each scratch is thin and shallow, it does not affect the image, but since the scratches are visible to the naked eye, they will be recognized by inspectors during pre-shipment inspections, and by users and service personnel when inserting and removing the unit.
[0060] Since these scratches are indistinguishable from scratches caused by long-term use or other abnormalities, inspectors may determine that the belt is defective, and users or service personnel may determine that the belt should be replaced. As a result, the belt is discarded even though it was only used for a short period of time and does not cause image noise. During manufacturing, this leads to an increase in the defect rate, which increases costs, and users incur large losses due to the replacement of belts and units.
[0061] The cause of the scratches that are the problem to be solved by this disclosure is that minute protrusions on the edge scratch the surface of the intermediate transfer belt. Fig. 6 is an enlarged view showing the minute protrusions on the scraper edge that are the cause of the problem to be solved. Fig. 6 shows an observation of the edge of the scraper 13 on the contact side at a magnification of 4000 times at the position where the scratch occurred on the intermediate transfer belt. As shown in Fig. 6, the protrusion is 10 to 20 μm wide and about 5 μm high, and force is concentrated on a part of the tip of the protrusion, causing a scratch of 1 μm wide on the belt.
[0062] There are many such protrusions on the edge of the metal scraper 13-1, and they cannot be eliminated by improving the manufacturing precision of the metal scraper 13-1. The manufacturing process of the metal scraper 13-1 involves masking the parts of a rolled thin metal plate that are to remain with photoresist, and then dissolving the unmasked parts by etching to create the desired shape. Even when the rolling direction or etching method was changed, it was not possible to eliminate the tiny protrusions on the edge.
[0063] Even if the metal scraper 13-1 is coated, if there are such minute protrusions on the undercoat layer, the protrusions will remain as they are with a coating of about 1 μm thickness, causing scratches. Since these scratches depend on the waviness of the scraper 13 as a whole, the state of the surface layer on the intermediate transfer belt 5 side, and the contact state between the intermediate transfer belt and the scraper 13, it is not possible to identify and remove which minute protrusions cause scratches by observation or inspection. In terms of the magnification of the microscope, the inspection takes too much time and is not practical. Furthermore, large protrusions such as edge abnormalities and dents do not concentrate force, so they do not cause a cluster of fine scratches, which is the subject of this disclosure. From this point of view, it is also difficult to identify the protrusions that cause scratches.
[0064] It is difficult to remove the minute protrusions on the edge of the scraper 13 during manufacturing. Therefore, we considered an improvement plan to make the intermediate transfer belt less susceptible to scratches. To this end, we decided to investigate how the surface conditions of belts that are easily scratched and belts that are not easily scratched differ.
[0065] First, intermediate transfer belts that are easily scratched and intermediate transfer belts that are not easily scratched were classified. The method was to rub the intermediate transfer belt and conduct a test to evaluate how easily it is scratched. The details are as follows. An intermediate transfer belt cut into a circular shape on a disk was set on a Rhesca friction player FPR2200. The part to be rubbed was a metal plate with a width of 15 mm and an angle of 30°, which was installed so as to be in counter contact, and a wrapping film (3M, grain size 320) was placed on the surface and rubbed. The conditions for the rubbing were a load of 150 g, a rotation radius of 38 mm, a rotation speed of 400 mm / s, and 1000 rotations. After rubbing, the scratches on the surface of the intermediate transfer belt were photographed and binarized, and the area ratio of the scratches was calculated, and intermediate transfer belts that are easily scratched and intermediate transfer belts that are not easily scratched were classified. Belts with a scratch area ratio of about 8 to 10% were classified as easily scratched belts, and belts with a scratch area ratio of about 4 to 6% were classified as not easily scratched belts.
[0066] Next, the surfaces of the easily scratched and not easily scratched belts were measured using the above-mentioned white light interference laser microscope to measure 24 surface roughness parameters: Sa, Sz, Str, Spc, Sdr, Sq, Ssk, Sku, Sp, Sv, Sal, Std, Sdq, Spd, Sk, Spk, Svk, Smr1, Smr2, Sxp, Vvv, Vvc, Vmp, and Vmc.
[0067] For each parameter and the scratch area ratio, multiple regression analysis was performed with the scratch area ratio as the objective variable and the surface roughness parameters as the explanatory variables to extract the parameters with the greatest influence. The following eight parameters were extracted: Sa (arithmetic mean height), Sq (root mean square height), Sal (minimum autocorrelation length), Sdr (interface developed area ratio), Spd (peak density), Smr1 (area ratio of the surface area that separates the protruding peak and core), Vmp (actual volume of the peak), and Vmc (actual volume of the core).
[0068] The correlation between these parameters reveals the characteristics of belts that are resistant to scratches. For example, Sa and Sq show that belts with low height and little variation are resistant to scratches. Sdr and Spd show that belts with some unevenness but few peaks are resistant to scratches. Smr1 shows that belts with a high ratio of peaks are resistant to scratches. Vmp and Vmc show that belts with large volumes of peaks and core are resistant to scratches.
[0069] Although each parameter indicates the tendency of the belt to be less susceptible to scratches, none of the parameters could be used alone to determine how easily the belt is scratched. Therefore, the correlation between two of the eight extracted parameters was confirmed by exhaustive testing. As a result, it was found that only the combination of Sal (minimum autocorrelation length) and Spd (peak density) can draw a boundary line that separates the intermediate transfer belt group that is easily scratched from the intermediate transfer belt group that is not easily scratched. The result is shown in Figure 4, where the line with coefficient 5 in the aforementioned relationship between Sal and Spd corresponds to the boundary line that separates the intermediate transfer belt group that is easily scratched from the intermediate transfer belt group that is not easily scratched.
[0070] As described above, we found that scratches on the intermediate transfer belt can be suppressed by using an intermediate transfer belt with surface roughness parameters Sal and Spd within a specified range. By closely observing and considering the state of the belt surface and the contact state of the scraper, we can explain the phenomenon of scratches on the intermediate transfer belt.
[0071] Figures 7A, 7B, and 7C show typical observation results of the intermediate transfer belt surface layer from Sal and Spd shown in Figure 4. The images in Figures 7A, 7B, and 7C show the height of the intermediate transfer belt surface photographed with a laser microscope using a white interference lens. Shown below the images is a profile showing the height of the center of the image (cross section taken along the arrow SS line).
[0072] FIG. 7A is a diagram showing an observation image of the intermediate transfer belt surface and a profile showing its height (coefficient less than 5, low Sal, high Spd) (the range surrounded by VII(A) in FIG. 4). FIG. 7A shows the observation results of an intermediate transfer belt in an area with few scratches for model A. Since Sal is small and Spd is large, the cycle is short and there are many peaks, and the profile also shows a similar tendency.
[0073] Fig. 7B is a diagram showing an observed image of the intermediate transfer belt surface and a profile showing the height (coefficient 5 or more) (the range surrounded by VII(B) in Fig. 4). Fig. 7B is the result of observation of the intermediate transfer belt in the range with many scratches for model A. Because Sal and Spd are large, the period is long, but there are many peaks, and the profile also shows a similar tendency.
[0074] Figure 7C shows an observation image of the intermediate transfer belt surface and a profile showing its height (coefficient less than 5, high Sal, low Spd) (the range surrounded by VII(C) in Figure 4). Figure 7C shows the results of observation of the intermediate transfer belt in the range with few scratches for model B. The cycle is long and there are few peaks, and the profile also shows a similar trend.
[0075] Figures 8A, 8B, and 8C are simplified diagrams showing the contact state between the intermediate transfer belt surface and the scraper edge in Figures 7A, 7B, and 7C. Figure 8A is a diagram showing the contact state between the intermediate transfer belt and the scraper (coefficient less than 5, low Sal, high Spd), Figure 8B is a diagram showing the contact state between the belt and the scraper (coefficient 5 or more), and Figure 8C is a diagram showing the contact state between the intermediate transfer belt and the scraper (coefficient less than 5, high Sal, low Spd).
[0076] 8A, 8B, and 8C are enlarged views of the edge of the metal scraper 13-1. The protrusions 13-5 on the edge of the metal scraper 13-1 are minute protrusions of about 5 μm as shown in FIG. 6. The shape of the belt surface in FIG. 8A has many peaks at short intervals as shown in FIG. 7A. In such a case, the protrusions 13-5 on the edge of the metal scraper 13-1 that come into contact with the intermediate transfer belt 5 do not penetrate into the valleys of the surface layer of the intermediate transfer belt 5 and do not scrape the peaks of the peaks, so the intermediate transfer belt 5 is less likely to be scratched.
[0077] The surface shape of the intermediate transfer belt 5 in Fig. 8B has a long period but many peaks, as shown in Fig. 7B. This is a state similar to the state in which the coating agent in Fig. 7A has aggregated. In such a case, the protrusions 13-5 on the edge of the abutting metal scraper 13-1 penetrate into the valleys of the intermediate transfer belt 5 and scrape off the peaks of the peaks, making it easy to scratch the intermediate transfer belt 5.
[0078] The surface shape of the intermediate transfer belt 5 in Fig. 8C has a long period and few peaks, as shown in Fig. 7C. In such a case, the protrusions 13-5 of the edge of the abutting metal scraper 13-1 penetrate into the valleys of the surface layer of the intermediate transfer belt 5, but since each peak is a large lump, it is difficult to scrape the peaks and to scratch the intermediate transfer belt 5. As a result, the above-mentioned phenomena can be explained as the cause of the values of Sal and Spd and the occurrence of scratches.
[0079] As described above, the present disclosure relates to the configuration of the image forming apparatus 100 shown in FIGS. 2 and 3, in which the scraper 13 has a high hardness, and by using an intermediate transfer belt whose surface roughness parameters Sal and Spd are within a predetermined range as shown in FIG. 4, belt scratches can be suppressed.
[0080] The above is mainly the content described in [Configuration 1]. However, some other [Configurations] are also included. Each [Configuration 1] is described below.
[0081] In [Configuration 2], a high-hardness coating is applied to the surface of the intermediate transfer belt 5. In the above explanation, in order to make the background of this disclosure easier to understand, the explanation was given using FIG. 3 in which a high-hardness coating is applied, but in reality, because of the relationship between surface roughness and scratches, [Configuration 1] also includes the case where no high-hardness coating is applied. [Configuration 2] specifies the high-hardness coating.
[0082] In [Configuration 3], the coating layer of the intermediate transfer belt 5 is made mainly of Si. In the above explanation, in order to make the background of this disclosure easier to understand, it was explained that the high-hardness coating is made mainly of Si, but in reality, it is a relationship between surface roughness and scratches, so in [Configuration 1], no particular material is specified. In [Configuration 3], the material is specified.
[0083] In [Configuration 4], the cleaning member is a scraper. In the above explanation, in order to make the background of this disclosure easier to understand, the cleaning member is described as a scraper, but in reality, since it is a relationship between surface roughness and scratches, the form of the cleaning member is not particularly specified in [Configuration 1]. In [Configuration 4], it is specified that the cleaning member is a scraper.
[0084] In [Configuration 5], the cleaning member is a scraper, and the scraper is flexible metal. In the above explanation, the scraper is described as being flexible metal in order to make it easier to understand how the present invention was made, but in reality, the relationship is between surface roughness and scratches, so in [Configuration 1], the material of the scraper is not particularly specified. In [Configuration 5], it is specified that the scraper is flexible metal.
[0085] In [Configuration 6], the cleaning member is a scraper, the scraper is made of flexible metal, and a high-hardness coating is formed on the contact portion. In the above explanation, in order to make the background of this disclosure easier to understand, it was explained that a high-hardness coating is formed on the scraper, but in reality, since it is a relationship between surface roughness and scratches, [Configuration 1] does not particularly specify the coating of the scraper. In [Configuration 6], it is specified that a high-hardness coating is formed on the contact portion of the scraper.
[0086] In [Configuration 7], there is no component on the inside of the belt that faces the scraper's contact part, and the pushing amount is flexibly set by the tension of the belt and the contact pressure of the scraper. Although a similar description is made in the above explanation, it is not specified in [Configuration 1], but is specified in [Configuration 7].
[0087] In [Configuration 8], when Sal (minimum autocorrelation length), which is one of the physical properties that indicate the surface roughness of the intermediate transfer belt, is 20 μm or less, the coefficient of the relational equation between Sal (autocorrelation length) and Spd (peak density) is 4. This is because, as shown in FIG. 9, the scratch-resistant belt of model A has Sal smaller than 20 μm, and the coefficient of the relational equation is 4 or less. Therefore, by narrowing the range by the Sal value, it is possible to set the conditions for a surface layer that is less susceptible to scratches.
[0088] Figure 10 is a diagram showing the relationship between the relative humidity when the surface layer of the intermediate transfer belt is applied and the susceptibility to scratches. In [Configuration 9], one of the manufacturing conditions for forming Sal (autocorrelation length) and Spd (peak density) is the relative humidity during coating, which is set to 45% or less. As shown in Figure 10, if the relative humidity when applying the coating layer is 45% or less, an intermediate transfer belt with a low scratch area rate and resistance to scratches can be obtained.
[0089] However, the correlation between Sal and Spd is not completely consistent. This is thought to be due to factors other than relative humidity that affect the coating layer application conditions. Factors that change Sal and Spd include, for example, changing the ratio of each material in the coating agent, or changing the application speed or number of applications. There are also various other factors, such as the type and shape of the application device and the temperature during application. At least, relative humidity is found to be one of the factors that change Sal and Spd, and is specified in [Configuration 9].
[0090] Figure 11 is a diagram showing the ranges of the surface roughness parameters Sal and Sa of the intermediate transfer belt surface. From [Configuration 10] onwards, the relationships with other parameters are stipulated based on the relationship between Sal and Spd. [Configuration 10] stipulates that Sa (arithmetic mean height) be 0.2 or less. The smaller Sa is, the smaller the ridges that are scraped off, making the belt less susceptible to scratches. As shown in Figure 11, even when Sal is 15 or less, which shortens the cycle, a Sa of 0.2 or less will make the belt less susceptible to scratches.
[0091] Fig. 12 is a diagram showing the ranges of surface roughness parameters Sal and Sq of the intermediate transfer belt surface. [Configuration 11] specifies that Sq (root mean square height) is 1 or less. The smaller Sq is, the smaller the variation in height is, and the less susceptible the belt is to scratches. As shown in Fig. 12, even when Sal is 15 or less, which shortens the cycle, the belt is less susceptible to scratches if Sq is 1 or less.
[0092] Fig. 13 is a diagram showing the ranges of surface roughness parameters Sal and Sdr for the intermediate transfer belt surface. [Configuration 12] specifies that Sdr (ratio of developed surface area of interface) is 0.002 or more. The larger the Sdr, the more uneven the surface, and a certain degree of unevenness limits the contact points and makes the belt less susceptible to scratches than a smooth surface. As shown in Fig. 13, even when Sal, which shortens the period, is 15 or less, the belt is less susceptible to scratches if Sdr is 0.002 or more.
[0093] Fig. 14 is a diagram showing the ranges of surface roughness parameters Sal and Smr1 for the intermediate transfer belt surface. [Configuration 13] specifies that Smr1 (the load area ratio separating the protruding peaks and the core) is 10 or less. The smaller Smr1 is, the smaller the peak ratio is, and the less the area that is scraped off, making the belt less susceptible to scratches. As shown in Fig. 14, even when Sal is 15 or less, which shortens the cycle, the belt is less susceptible to scratches if Smr1 is 10 or less.
[0094] Fig. 15 is a diagram showing the range of surface roughness parameters Sal and Vmp for the intermediate transfer belt surface. [Configuration 14] specifies that Vmp (the actual volume of the peaks) must be 0.004 or more. The larger Vmp is, the larger the volume of the peaks is, and the less likely each peak is to be worn away, resulting in a belt that is less susceptible to scratches. As shown in Fig. 15, even when Sal, which shortens the cycle, is 15 or less, a Vmp of 0.004 or more will result in a belt that is less susceptible to scratches.
[0095] Fig. 16 is a diagram showing the range of surface roughness parameters Sal and Vmc for the intermediate transfer belt surface. [Configuration 15] specifies that Vmc (the actual volume of the core) must be 0.008 or more. The larger the Vmc, the larger the volume of the middle part of the mountain, and the less likely each mountain is to be worn down, resulting in a belt that is less susceptible to scratches. As shown in Fig. 16, even when Sal, which shortens the cycle, is 15 or less, a Vmc of 0.008 or more results in a belt that is less susceptible to scratches.
[0096] [Comparative Example] Similar to the embodiment, the comparative example is a cleaning system for the intermediate transfer belt 5, which has the intermediate transfer belt 5 and a scraper 13, as shown in Figures 1 and 2. Also, similar to the embodiment, the intermediate transfer belt 5 has a high-hardness coating on its surface as described in [Configuration 2], and the scraper 13 has a coating on its contact portion which is harder than the intermediate transfer belt surface as described in [Configuration 6].
[0097] The difference from the embodiment is that the relationship between Sal and Spd is outside the range of [Formula 1] described in [Configuration 1], and the coefficient K is 5 or more. The difference between Comparative Examples 1 to 3 is the surface roughness parameter of the surface layer of the intermediate transfer belt 5. As in the example, the belt manufacturing conditions and the relative humidity conditions during manufacturing were changed to prepare conditions that result in different combinations of Sal and Spd.
[0098] [Comparative example of evaluation results of the present disclosure] In this disclosure, a new scraper that is prone to belt damage is used, and a new intermediate transfer belt is always used to compare the number of scratches and the state of scratches.
[0099] In the verification method of the present disclosure, a predetermined number of images are formed under predetermined conditions, and scratches on the intermediate transfer belt surface are visually evaluated. The evaluation items for scratches are the number of scratches and the condition of the scratches. The scratches mentioned here do not refer to fine scratches of about 1 μm, but rather a collection of such fine scratches is counted as one. The condition of the scratches is divided into the following three stages. The first stage is a non-occurrence level where there are fine scratches but they are not visible to the naked eye. Of course, since they are not visible, they are not counted as scratches. In the second stage, the width of the scratches is several tens to 200 μm, and they are visible to the naked eye, but are not noticeable to service personnel or users, and are at the OK level. In the third stage, the width of the scratches is 200 μm or more, and they are visible to the naked eye, so they are at the NG level where they are judged to be defective even if they do not affect the image.
[0100] The experimental machine used was an AccurioPress C4080 manufactured by Konica Minolta. The transfer unit was standard except for the belt of the embodiment and the comparative example. The cleaning unit was standard, and the embodiment and the comparative example were evaluated under the same conditions. The environment was normal (23°C, 50%). As described above, the intermediate transfer belt and scraper were always new for each evaluation, and the other units were continuously used with new ones prepared before the evaluation because the number of images formed was not large. Maintenance was performed on the transfer unit and cleaning unit when the intermediate transfer belt and scraper were replaced. In all conditions, the image formation was performed in color mode, with 200 A3 sheets of horizontal band images with a print rate of 5% for each color printed (operated for about 5 minutes), and the number and condition of scratches on the intermediate transfer belt were evaluated.
[0101] (Evaluation Results) The evaluation results shown in Fig. 17 will be examined. Fig. 17 is a diagram showing a list of surface roughness parameter conditions and evaluation results for the intermediate transfer belt surface of the examples and comparative examples. For examples 1 to 7, the overall evaluation was "A" (no scratches or scratches of OK level occurred), and there were no scratches of NG level. For comparative examples 1 to 3, the evaluation was "F" (scratches of NG level occurred).
[0102] The detailed evaluation results are shown below. First, Examples 1 to 3 are compared with Comparative Examples 1 to 3. Examples 1 to 3 have a coefficient K smaller than 5, satisfy [Configuration 1], and are evaluated as "A" for belt damage, whereas Comparative Examples 1 to 3 have a coefficient K of 5 or more, do not satisfy Configuration 1, and are evaluated as "F" for belt damage. Although Example 1 and Comparative Example 1, Example 2 and Comparative Example 2, and Example 3 and Comparative Example 3 are close to each other, the evaluation results are in accordance with the relational formula [Formula 1] described in [Configuration 1].
[0103] Next, the effects are compared among the examples. In Examples 1 to 6, the coefficient K is changed stepwise in a range smaller than 5. Although there is some error in the results of the coefficient K and the number of scratches due to variations in the intermediate transfer belt and scraper, the number of scratches decreases as the coefficient K becomes smaller. In particular, when the coefficient is around 1, no scratches occurred on the intermediate transfer belt. This shows that the occurrence of scratches can be suppressed by making the surface condition more uniform.
[0104] As described above, in each example, the surface roughness parameters of the surface layer of the intermediate transfer belt 5 satisfy the relational expressions described in [Configuration 1], thereby suppressing the occurrence of belt scratches, and all of the evaluation results are "A." In the comparative example, the surface roughness parameters of the surface layer of the intermediate transfer belt 5 do not satisfy the relational expressions described in [Configuration 1], so belt scratches occur, and the evaluation result is "F."
[0105] The evaluation results shown in FIG. 18 will be examined. FIG. 18 is a diagram showing the surface roughness parameter conditions of the intermediate transfer belt surface of the examples and comparative examples, and a list of evaluation results with and without coating. The evaluation results in FIG. 18 are evaluation results for the configurations with and without coatings described in [Configuration 2], [Configuration 3], [Configuration 5], and [Configuration 6]. In the cases of Examples 8 and 9, the surface layer of the intermediate transfer belt is not coated. In this case, both the surface roughness parameters Sal and Spd are low, and the coefficients are 1 or less. Under these conditions, no scratches were generated, which is the issue. A coefficient of less than 5 in the present disclosure satisfies the absence of scratches. There are no intermediate transfer belts without coatings with a coefficient K of 5 or more, and there are no comparative examples.
[0106] In Example 10 and Comparative Example 4, the surface layer of the intermediate transfer belt is coated, but the scraper contact portion is not coated. In terms of hardness, the belt side is harder and more advantageous, but the scraper edge has minute protrusions, which cause slight scratches. In Example 10, the coefficient K is less than 5, and scratches are generated but are at an OK level, and the overall evaluation is "A." In Comparative Example 4, the coefficient K is 5 or more, and scratches at an NG level are generated, and the overall evaluation is "F." Regardless of whether the intermediate transfer belt and scraper are coated or not, the relational formula and the conditions for scratch generation described in [Configuration 1] are satisfied.
[0107] Based on the results shown in the above Examples 1 to 10 and Comparative Examples 1 to 4, among the physical properties indicating the surface roughness of the intermediate transfer belt, Spd×Sal 2 <5×10 6 When [Formula 1] is satisfied and Sal (minimum autocorrelation length) is 20 μm or less (Sal≦20 μm), it is derived that the relationship between Spd (peak density) and Sal should satisfy the following [Formula 2]: Spd×Sal 2 <4×10 6 ...[Formula 2] (Effects of disclosure) In a cleaning system having a scraper that is harder than the surface of an intermediate transfer belt to accommodate longer life, the relationship between the surface roughness parameters Sal (minimum autocorrelation length) and Spd (peak density) of the intermediate transfer belt surface layer shown in this disclosure is defined, and by using this intermediate transfer belt, it is possible to suppress the occurrence of scratches on the intermediate transfer belt and to suppress the occurrence of scratches at an NG level, thereby improving the problem.
[0108] This will eliminate the need for intermediate transfer belts, which have to be replaced and discarded immediately after starting use, improving production defect rates, reducing service technician man-hours, preventing cost increases, and improving user trust.
[0109] The method of the present disclosure makes it possible to provide an image forming apparatus equipped with a cleaning system that is reliable over a long period of time.
[0110] Although the image forming apparatus has been described above based on each embodiment, the embodiments disclosed herein are illustrative and not restrictive in all respects. The scope of the present invention is defined by the claims, and includes all modifications within the meaning and scope of the claims. [Explanation of symbols]
[0111] 1 photoconductor, 2 charging device, 3 exposure device, 4 developing device, 5 intermediate transfer belt, 5-1 base layer, 5-2 belt surface layer, 6 primary transfer roller, 7 cleaning device, 8 lubricant application device, 9 secondary transfer opposing roller, 10 secondary transfer roller, 11 fixing device, 12 cleaning blade, 12-1 blade, 12-2 support member, 13 scraper, 13-1 metal scraper, 13-2 first support member, 13-3 second support member, 13-4 scraper coat layer, 13-5 protrusion, 14 conveying screw, 15 cleaning unit housing, 16 toner storage roller, 17 regulating member, 18 toner storage section, 19 cleaning opposing roller, 100 image forming apparatus, T recording medium.
Claims
1. An image forming apparatus having an intermediate transfer belt and a cleaning member that is in contact with the intermediate transfer belt and removes residual toner therefrom, Among the physical properties indicating the surface roughness of the intermediate transfer belt, Spd (peak density) and Sal (minimum autocorrelation length) are Spd × Sal 2 <5×10 6 An image forming apparatus that satisfies [Formula 1].
2. The intermediate transfer belt has a base layer and a coating layer that forms irregularities on a surface of the base layer. The image forming apparatus according to claim 1 .
3. The coating layer of the intermediate transfer belt is a layer containing Si as a main component. The image forming apparatus according to claim 2 .
4. the cleaning member is a scraper that is in contact with the intermediate transfer belt so as to scrape off the residual toner on the surface of the intermediate transfer belt; The image forming apparatus according to claim 1 .
5. The scraper comprises a flexible metal scraper. The image forming apparatus according to claim 4 .
6. the scraper has a high-hardness scraper coat layer at least on a portion of the metal scraper that contacts the intermediate transfer belt; The image forming apparatus according to claim 5 .
7. There is no member on the inside of the intermediate transfer belt opposite to the portion where the cleaning member contacts the intermediate transfer belt, The tension of the intermediate transfer belt and the amount of pressure applied by the contact pressure of the cleaning member are adjusted. The image forming apparatus according to claim 1 .
8. Among the physical properties indicating the surface roughness of the intermediate transfer belt, when the Sal is 20 μm or less (Sal≦20 μm), The relationship between the Spd and the Sal is Spd x Sal 2 <4 x 10 6 2. The image forming apparatus according to claim 1, wherein the following formula (2) is satisfied:
9. In the intermediate transfer belt, one of the manufacturing conditions for forming the Sal and the Spd is a relative humidity during coating. The belt is manufactured at a relative humidity of 45% or less. The image forming apparatus according to claim 1 .
10. Among the physical properties indicating the surface roughness of the intermediate transfer belt, Sa (arithmetic mean height) is 0.2 or less. The image forming apparatus according to claim 1 .
11. Among the physical properties indicating the surface roughness of the intermediate transfer belt, Sq (root mean square height) is 1 or less. The image forming apparatus according to claim 1 .
12. Among the physical properties indicating the surface roughness of the intermediate transfer belt, Sdr (interface development area ratio) is 0.002 or more. The image forming apparatus according to claim 1 .
13. Among the physical properties indicating the surface roughness of the intermediate transfer belt, Smr1 (the load area ratio separating the protruding peaks and the core) is 10 or less. The image forming apparatus according to claim 1 .
14. Among the physical properties indicating the surface roughness of the intermediate transfer belt, Vmp (the actual volume of the peaks) is 0.004 or more. The image forming apparatus according to claim 1 .
15. Among the physical properties indicating the surface roughness of the intermediate transfer belt, Vmc (the actual volume of the core portion) is 0.008 or more. The image forming apparatus according to claim 1 .
Citation Information
Patent Citations
Method for manufacturing intermediate transfer belt
JP2011118026A
Intermediate transfer belt and manufacturing method thereof, and image forming apparatus
JP2012113197A
Image forming apparatus
JP2018036287A
Cleaning device, image formation apparatus, and manufacturing method for rigid body blade
JP2018205653A
Cleaning device and image forming apparatus
JP2021051253A