Grease composition with low power consumption and excellent self-locking property

The grease composition with calcium sulfonate complex and metal soap additives balances self-locking and startability, addressing the inefficiencies of previous compositions by optimizing friction coefficients for reduced power consumption and gear stability.

JP2024147188APending Publication Date: 2024-10-16KYODO YUSHI CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023060046
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-03
Publication Date
2024-10-16

AI Technical Summary

Technical Problem

Existing grease compositions for lubricating resin and metal parts in automobile components fail to balance high self-locking properties with low power consumption, as increasing static friction coefficient to enhance self-locking often leads to higher power consumption.

Method used

A grease composition using calcium sulfonate complex as a thickener and metal soap as an additive, specifically lithium, calcium, or zinc soap, to achieve a balanced friction coefficient for improved self-locking and startability.

Benefits of technology

The composition achieves both high self-locking properties and excellent startability by optimizing static and dynamic friction coefficients, reducing power consumption and preventing gear reversal.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024147188000001
    Figure 2024147188000001
Patent Text Reader

Abstract

To provide a grease composition having both a high self-locking property and an excellent starting property.SOLUTION: A grease composition is used for lubricating a resin member and a metal member. The grease composition contains a base oil, a calcium sulfonate complex as a thickener, and a powdered metal soap as an additive in an amount of 5 to 20 mass% with respect to the total mass of the composition.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a grease composition that consumes low power and has excellent self-locking properties (i.e., the property of suppressing reverse rotation of gears due to slippage that occurs in a reducer). [Background technology]

[0002] Resin parts are often used instead of metal parts in order to reduce weight in automobile parts, etc. For example, the reduction gear of an automobile's power window motor uses a resin (polyacetal) worm wheel gear and a steel worm gear. The grease used in the lubrication parts of these reducers is required to have a high self-locking property to prevent reverse rotation, and to have a high self-locking property, it is necessary to have a high static friction coefficient. As a conventional technique for reducing the static friction coefficient, Patent Document 1 discloses a grease composition containing at least one thickening agent selected from a urea compound and a metal soap (lithium stearate, lithium 12-hydroxystearate, calcium stearate, calcium 12-hydroxystearate, aluminum stearate, aluminum 12-hydroxystearate, barium stearate, barium 12-hydroxystearate, sodium stearate, sodium 12-hydroxystearate, etc.) as an additive. The grease composition can reduce the static friction coefficient of the lubricated parts and lower the starting voltage. Patent Document 2 discloses a lubricating grease composition containing 0.5 to 40 mass % of a polyolefin wax having an average molecular weight of 900 to 10,000. Patent Document 3 discloses a grease composition for resin lubrication, which is characterized in that montan wax is contained in a grease containing a thickener and a base oil. Patent Document 4 discloses a grease composition for resin lubrication, which is applied to areas where resin and metal come into contact with each other, and is characterized by containing a base oil containing at least one of poly-α-olefin oil, mineral oil, and highly refined mineral oil in a specific ratio, a thickener containing at least one of metal soap and metal complex soap in a specific ratio, and at least one of non-polar wax and polar wax. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2004-314916 A [Patent Document 2] Japanese Patent Application Publication No. 9-194867 [Patent Document 3] JP 2002-371290 A [Patent Document 4] JP 2005-054024 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, the self-locking property cannot be improved by simply increasing the static friction coefficient. On the other hand, in order to meet the recent demand for reduced power consumption, it is necessary to lower the static friction coefficient and lower the starting voltage. Therefore, an object of the present invention is to provide a grease composition that achieves both high self-locking property and excellent starting property. [Means for solving the problem]

[0005] The present invention provides a grease composition comprising a calcium sulfonate complex as a thickener and a metal soap as an additive. 1. A grease composition used for lubricating a resin member and a metal member, comprising: Base oil, As a thickener, calcium sulfonate complex, As an additive, a powdered metal soap in an amount of 5 to 20% by mass based on the total mass of the composition, A grease composition comprising: 2. The grease composition according to 1 above, wherein the metal soap is a lithium soap, a calcium soap, a magnesium soap, a zinc soap, or a mixture thereof. 3. A reducer containing the grease composition described in 1 or 2 above. Effect of the Invention

[0006] As described above, in order to achieve both high self-locking properties and excellent starting properties, it is necessary to increase the dynamic friction coefficient without lowering the static friction coefficient too much. According to the present invention, by using a metal soap and a calcium sulfonate complex in combination, it is possible to obtain a friction coefficient that achieves both high self-locking properties and excellent starting properties. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0007] [Base oil] As the base oil of the grease composition of the present invention, mineral lubricating oils and synthetic lubricating oils can be used. The type is not particularly limited, but as the mineral lubricating oils, paraffinic mineral oils, naphthenic mineral oils, and mixtures thereof can be used. As the synthetic lubricating oils, synthetic hydrocarbon oils, ether oils, ester oils, fluorine oils, etc. can be used. Synthetic oils are preferred, synthetic hydrocarbon oils are more preferred, and poly-alpha-olefins are even more preferred. The synthetic oil may be a so-called biomass oil produced from biological resources derived from animals and plants. For example, biomass ester oils synthesized from various fatty acids and alcohols using vegetable oils as raw materials, and biomass hydrocarbon oils using vegetable oils such as palm oil, corn oil, and soybean oil can also be used. The kinematic viscosity of the base oil of the present invention at 40° C. is from 15 to 450 mm from the viewpoints of low temperature properties and durability. 2 / s, 15 to 200 mm 2 / s is preferable, and 15 to 70 mm 2 / s is even more preferable. The content of the base oil in the grease composition of the present invention is an amount normally used for producing grease, for example, 45 to 90 mass %, and from the viewpoint of low temperature properties, it is preferably 47.5 to 87 mass %, more preferably 50 to 82 mass %.

[0008] [Calcium sulfonate complex thickener] The calcium sulfonate complex of the present invention is a complex (complex soap) containing calcium sulfonate and a calcium salt of an acid other than sulfonic acid. Examples of sulfonic acids constituting calcium sulfonate include dodecylbenzenesulfonic acid, dinonylnaphthalenesulfonic acid, petroleum sulfonic acid, etc. As the sulfonic acid, dodecylbenzenesulfonic acid is preferred. Acids other than sulfonic acids include 12-hydroxystearic acid, acetic acid, carbonic acid and boric acid. As the calcium sulfonate complex used in the present invention, a complex formed from calcium dodecylbenzenesulfonate, calcium 12-hydroxystearate, calcium carbonate and / or calcium acetate is particularly preferred. More particularly, a complex formed from calcium dodecylbenzenesulfonate, calcium 12-hydroxystearate, calcium carbonate and calcium acetate is preferred. The complex of the present invention may also contain calcium borate and calcium carbonate. The content of the calcium sulfonate complex thickener in the composition of the present invention is an amount capable of adjusting the consistency of the grease composition of the present invention to the range of 235 to 415, for example, and is usually 5 to 40 mass%, preferably 8 to 35 mass%, and more preferably 10 to 33 mass%, based on the total mass of the composition. In the present invention, the calcium sulfonate complex can also function as an anti-wear agent and an anti-rust agent. In this specification, the term "penetration" refers to 60 times worked penetration, which can be measured in accordance with JIS K2220 7. The penetration of the grease composition of the present invention is preferably 235 to 415, more preferably 280 to 415, from the viewpoint of low temperature properties.

[0009] [Metal soap] The grease composition of the present invention contains a powdered metal soap as an additive. Examples of the metal soap include lithium soap, calcium soap, magnesium soap, zinc soap, or a mixture thereof. Among these, lithium soap and zinc soap are preferred from the viewpoint of starting performance because they further reduce the static friction coefficient. Metal soaps are often used as thickeners for grease. In general, thickeners can retain the liquid base oil and turn it into a solid or semi-solid (i.e., grease) by forming a network structure in the base oil. The metal soap used in the present invention contains powdered metal soap, so it does not form a network structure and does not act as a thickener. The content of the metal soap in the grease composition of the present invention is 5 to 20 mass %, and from the viewpoint of starting performance, it is preferably 8 to 20 mass %, and more preferably 13 to 20 mass %.

[0010] [Optional Additives] The grease composition of the present invention may further contain additives that are commonly used in greases, such as antioxidants, metal corrosion inhibitors, oiliness agents, solid lubricants, etc. Examples of the antioxidant include amine-based antioxidants and phenol-based antioxidants. The metal corrosion inhibitor includes, for example, benzotriazole. Examples of oily agents include fatty acids, fatty acid esters, and phosphate esters. Examples of solid lubricants include metal oxides such as CaO, ZnO, and MgO, metal carbonates such as CaCO3 and ZnCO3, molybdenum disulfide, graphite, PTFE, MCA, etc. Among these, CaCO3 is preferred from the viewpoint of extending the seizure life. The amount of these additives to be added is not particularly limited as long as it does not impair the object of the present invention, and is, for example, 0 to 15% by mass, preferably 0 to 12% by mass, based on the total mass of the composition. The grease composition of the present invention also preferably does not contain any thickeners other than the calcium sulfonate complex. The grease composition of the present invention also preferably does not contain wax as an additive.

[0011] The grease composition of the present invention can be used for lubrication between resin members and metal members, for example, for lubrication between a resin (polyacetal, polyamide) worm wheel gear and a steel worm gear, which are part of the reducer of an automobile power window motor, and in the reducers of power seat motors and sunroof motors. EXAMPLES

[0012] <Raw materials for test grease composition> (Thickener) Dodecylbenzenesulfonic acid, 12-hydroxystearic acid, acetic acid, boric acid, calcium carbonate, calcium hydroxide (Base oil) Poly-α-olefin (Kinematic viscosity at 40°C: 38.7mm 2 / s) (Additives) Li soap Lithium stearate (powder) Calcium soap Calcium stearate (powder) Zn soap Zinc stearate (powder) PE wax Molecular weight: Weight average molecular weight 17, 500 Physical properties: Dropping point 132-138℃, acid value 0mgKOH / g, melt viscosity approx. 25,000mPa·s (140℃) Sold by: Clariant Chemicals Co., Ltd. Product Name:LICOWAX PE190 P PP wax Molecular weight: Weight average molecular weight 28, 200 Physical properties: Softening point 112℃, melt viscosity approx. 9,300mPa·s (170℃) Sold by: Clariant Chemicals Co., Ltd. Product Name:LICOCENE PP 3602 Montan wax Physical properties: Dropping point 96-102℃, acid value 9-14mgKOH / g, saponification value 102-122mgKOH / g Sold by: Clariant Chemicals Co., Ltd. Product name: LICOWAX OP FL

[0013] <Preparation of Test Grease Compositions> Dodecylbenzenesulfonic acid, 12-hydroxystearic acid, acetic acid, calcium carbonate, and calcium hydroxide were stirred in the base oil and heated to 72°C. Then, boric acid and calcium hydroxide were added, further stirred, and heated to 163°C. After that, the mixture was cooled to 100°C or less while stirring to obtain a base grease. Metal soap or wax was added to the mixture in the ratio shown in Table 1, and the mixture was dispersed using a three-roll mill to prepare a test grease composition. The consistency of the test grease compositions was standardized to 350. The consistency was measured according to JIS K 2220 7.

[0014] <Test Method> If the static friction coefficient is high, a large force is required to start the motor, resulting in high power consumption. By lowering the maximum static friction coefficient with grease, it is possible to operate the motor with less force, reducing power consumption and resulting in good starting performance (low starting voltage). In other words, starting performance can be evaluated based on the maximum static friction coefficient. The smaller the maximum static friction coefficient, the better the starting performance. On the other hand, by increasing the maximum static friction coefficient, it is possible to prevent the gears from reversing due to slippage, and by increasing the maximum dynamic friction coefficient, it is possible to minimize the gears from reversing. In other words, the self-locking property can be evaluated by the maximum dynamic friction coefficient. The larger the maximum dynamic friction coefficient, the better the self-locking property. Therefore, the starting property and self-locking property were evaluated by determining the maximum static and dynamic friction coefficients by the Bowden test. Specifically, the test grease composition was applied to the lower test piece, a specified load was applied to the upper test piece, and after leaving it to stand for a specified time, the lower test piece was slid to determine the maximum static and dynamic friction coefficients. The results are shown in Table 1. [Test conditions] Upper specimen: POM Lower test piece: Steel S45C Test speed: 0.06mm / s Test load: 39.2N Test temperature: 80℃ Standing time: 5 minutes [Acceptance criteria] Maximum static friction coefficient: 0.083 or less Maximum dynamic friction coefficient: 0.043 or more

[0015] [Table 1]

[0016] In Examples 1, 2, 3, and 4, in which 5 to 20% lithium soap was blended, the maximum static friction coefficients were 0.083, 0.074, 0.060, and 0.048, respectively, which were lower than Comparative Example 1, and a reduction in the starting voltage was observed. Furthermore, the maximum dynamic friction coefficients were 0.093, 0.081, 0.060, and 0.043, which were not too low, and the self-locking properties were also good. In Examples 5 and 6, in which 5% Ca soap and 5% Zn soap were mixed, the maximum static friction coefficients were 0.08 and 0.067, and the maximum dynamic friction coefficients were 0.080 and 0.081, respectively, and the same effects as in Example 1, in which 5% Li soap was mixed, were obtained. In Comparative Example 2, in which 4% of lithium soap was mixed, the maximum static friction coefficient was 0.093, which was higher than those in Examples 1 to 4, and the reduction in starting voltage was insufficient. In Comparative Example 3, in which 25% lithium soap was mixed, the maximum dynamic friction coefficient was 0.035, which was lower than those of Examples 1 to 4, and the self-locking property was insufficient. In Comparative Examples 4, 5 and 6, in which PE wax, PP wax and montan wax were mixed at 5%, the maximum static friction coefficients were 0.092, 0.106 and 0.102, respectively, which were higher than those in Examples 1 to 4, and the reduction in starting voltage was insufficient.

Claims

1. A grease composition used for lubricating a resin member and a metal member, Base oil, As a thickener, calcium sulfonate complex, As an additive, a powdered metal soap in an amount of 5 to 20% by mass based on the total mass of the composition, A grease composition comprising:

2. 2. The grease composition according to claim 1, wherein the metal soap is a lithium soap, a calcium soap, a magnesium soap, a zinc soap, or a mixture thereof.

3. A reducer containing the grease composition according to claim 1 or 2.

Citation Information

Patent Citations

  • Lubricating grease composition

    JP1997194867A

  • Grease composition for lubricating resin

    JP2002371290A

  • Electric power steering device

    JP2004314916A

  • Grease composition for lubricating resin and electric power steering device

    JP2005054024A