AI Technical Summary
【0017】 (6)の石炭灰の嵩上げ方法は、石炭灰の処理の場所及びコストを抑えつつ、更に確実かつ効率的に石炭灰の飛散を防止しながら、より多くの石炭灰を嵩上げできる。
Smart Images

Figure 2026093825000001_ABST
Abstract
Claims
1. A coal ash slurry production process involves mixing coal ash, water, and cement to produce a coal ash slurry, A raising process involves pouring the coal ash slurry produced in the coal ash slurry production process into a raised area on the ground to raise the level of the coal ash, The process includes a coal ash slurry hardening step in which the coal ash slurry raised in the raising step is left to stand for a predetermined time to harden, The cement content of the coal ash slurry produced in the aforementioned coal ash slurry production process is 50 kg / m³. 3 That concludes the explanation of the method for raising the volume of coal ash.
2. The method for raising the level of coal ash according to claim 1, wherein the leveling step includes an upper layer leveling step of further piling coal ash slurry on top of the coal ash slurry hardened in the coal ash slurry hardening step to raise the level.
3. The aforementioned raised section has multiple raised sections, A method for raising the level of coal ash according to claim 1 or 2, wherein, after completing the leveling process in a first leveling section among a plurality of leveling sections, the leveling process is started in a second leveling section different from the first leveling section among a plurality of leveling sections.
4. The method for raising the level of coal ash according to claim 3, wherein the multiple leveling sections are arranged in a horizontal and vertical direction, respectively.
5. A moisture content measurement step for measuring the moisture content of the coal ash slurry after raising the height in the aforementioned raising step, A method for raising the level of coal ash according to claim 1 or 2, further comprising: a scattering suppressant spraying step of spraying a scattering suppressant onto the leveled coal ash slurry whose moisture content was measured in the moisture content measurement step when the moisture content measurement result in the moisture content measurement step is less than or equal to a predetermined moisture content.
6. The method for increasing the volume of coal ash according to claim 5, wherein the predetermined moisture content is set to 6% to 15%.