Method for raising the level of coal ash

The method of using embankment material and controlled coal ash slurry layers with scattering suppressants addresses storage limitations, allowing efficient and cost-effective disposal of coal ash without scattering.

JP2026093852APending Publication Date: 2026-06-09THE CHUGOKU ELECTRIC POWER CO INC

Patent Information

Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
THE CHUGOKU ELECTRIC POWER CO INC
Filing Date
2024-11-28
Publication Date
2026-06-09

AI Technical Summary

Technical Problem

Existing methods for disposing of coal ash face limitations in storage capacity, necessitating costly expansion of ash disposal sites to prevent scattering, which increases land acquisition and construction costs.

Method used

A method involving the production of embankment material from clinker ash, fly ash, and cement, followed by sequential construction and hardening of embankments and coal ash slurry layers, with controlled moisture content and application of scattering suppressants, to raise and stabilize coal ash without scattering.

Benefits of technology

Enables the stacking of larger amounts of coal ash while minimizing location and cost, ensuring structural integrity and preventing scattering, even over extensive areas.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2026093852000001_ABST
    Figure 2026093852000001_ABST
Patent Text Reader

Abstract

To provide a method for raising coal ash that can raise a larger volume of coal ash while reducing the location and cost of raising the coal ash, and while preventing the scattering of coal ash. [Solution] The method comprises an embankment material generation step (step S10) for generating embankment material, a first embankment construction step (step S11) for forming a first embankment with the embankment material, a first embankment hardening step (step S12) for hardening the first embankment, a coal ash slurry generation step (step S13), a first layer raising step (step S14) for raising the coal ash slurry A, a coal ash slurry hardening step (step S15) for hardening the coal ash slurry A, a second embankment construction step (step S16) for forming a second embankment, a second embankment hardening step (step S17) for hardening the second embankment, and a second layer raising step (step S18) for raising the coal ash slurry A within the second embankment, wherein the cement content of the coal ash slurry A is 50 kg / m³ 3 That's all.