Raw sheet

A raw sheet composition of high-density polyethylene, linear low-density polyethylene, calcium carbonate, and antistatic agent addresses the strength-weight trade-off in newspaper packaging bags, resulting in a lightweight bag with sufficient strength and reduced carbon dioxide emissions.

JP3249376UActive Publication Date: 2024-12-05CREW CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2024003345U
Authority / Receiving Office
JP · JP
Patent Type
Utility models
Current Assignee / Owner
Filing Date
2024-10-09
Publication Date
2024-12-05
Estimated Expiration
2034-10-09

AI Technical Summary

Technical Problem

Conventional newspaper packaging bags made of thin polyethylene face a trade-off between maintaining strength to prevent damage during transportation and reducing weight for cost efficiency, with calcium carbonate mixtures failing to provide sufficient strength when thinned to 7 μm.

Method used

A raw sheet composition comprising high-density polyethylene, linear low-density polyethylene, calcium carbonate, barium sulfate, and an antistatic agent, blended and processed at specific ratios, is used to create a lightweight packaging bag with sufficient strength, achieved through a thickness of 5 to 10 μm and an inflation molding method.

Benefits of technology

The solution results in a lightweight newspaper packaging bag that maintains necessary strength and reduces carbon dioxide emissions when incinerated, achieving a balance between strength and weight reduction.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0003249376000001_ABST
    Figure 0003249376000001_ABST
Patent Text Reader

Abstract

To provide a raw sheet for producing a bag-shaped newspaper packaging bag, capable of maintaining a required strength and realizing a reduction in weight. [Solution] The raw sheet for making newspaper packaging bags 10 is formed to a thickness of approximately 7.0 μm and contains 100 parts by weight of high density polyethylene (HDPE), 5 to 10 parts by weight of linear low density polyethylene (LLDPE), 5 to 15 parts by weight of calcium carbonate admixture, 2 to 8 parts by weight of barium sulfate admixture, and 1.5 to 3.5 parts by weight of an antistatic admixture.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a raw sheet used for making bag-shaped newspaper packaging bags that contain newspapers inside. [Background technology]

[0002] Conventionally, when newspapers are delivered during rainy weather, the newspapers are sealed in a thin polyethylene bag to prevent the newspapers from getting wet. This type of bag is rectangular, with all four edges sealed (see Patent Document 1). The newspapers are delivered to readers with the newspapers contained in such a bag. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2006-335426 A Summary of the Invention [Problem to be solved by the invention]

[0004] Incidentally, a packaging bag for containing newspapers needs to have sufficient strength to prevent damage or tearing due to friction or external pressure during transportation. On the other hand, when transporting or delivering a newspaper package containing newspapers, the packaging bag needs to be lightweight in order to reduce the transportation cost and the burden on the delivery person. In general, it is known to mix calcium carbonate into a sheet member whose main raw material is polyethylene in order to reduce the weight. However, when a conventional packaging bag used for containing newspapers is to be formed into a thin packaging bag of, for example, about 7 μm, the mixing of calcium carbonate does not provide sufficient strength, and there is a risk of the bag being broken due to insufficient strength during transportation or delivery.

[0005] The present invention has been made in consideration of the above-mentioned circumstances, and its purpose is to provide a base sheet for creating bag-shaped newspaper packaging bags that can maintain the necessary strength while achieving lightweight construction. [Means for solving the problem]

[0006] (1) The raw sheet of the present invention is a raw sheet used for producing a newspaper packaging bag formed into a rectangular shape in which newspapers are contained. The raw sheet is formed to a thickness of 5 to 10 μm, and is characterized in that it contains 100 parts by weight of high-density polyethylene, 5 to 10 parts by weight of linear low-density polyethylene, 5 to 15 parts by weight of a calcium carbonate admixture containing calcium carbonate and the high-density polyethylene, 2 to 8 parts by weight of a barium sulfate admixture containing barium sulfate and the high-density polyethylene, and 1.5 to 3.5 parts by weight of an antistatic admixture containing an antistatic agent and the high-density polyethylene.

[0007] Because of this configuration, it is possible to realize a newspaper packaging bag that maintains the necessary and sufficient strength and is lightweight. Furthermore, when a newspaper packaging bag made from the raw sheet is incinerated as garbage after use, it is possible to reduce the amount of combustion gases such as carbon dioxide generated compared to conventional products.

[0008] (2) The raw fabric sheet of the present invention is used for producing a rectangular newspaper packaging bag in which newspapers are placed, and is obtained by heating and melting a mixture of 100 parts by weight of high density polyethylene, 5 to 10 parts by weight of linear low density polyethylene, 5 to 15 parts by weight of a calcium carbonate admixture containing calcium carbonate and the high density polyethylene, 2 to 8 parts by weight of a barium sulfate admixture containing barium sulfate and the high density polyethylene, and 1.5 to 3.5 parts by weight of an antistatic agent and an antistatic admixture containing the high density polyethylene, at a temperature of 190 to 210°C, and forming the mixture into a tubular shape having a thickness of 5 to 10 μm by an inflation molding method.

[0009] This structure makes it possible to realize a lightweight newspaper packaging bag that maintains sufficient strength. Also, when used newspaper packaging bags are burned, the amount of combustion gases such as carbon dioxide generated can be reduced compared to conventional products.

[0010] (3) In the raw sheet, the linear low density polyethylene is preferably 7 parts by weight, the calcium carbonate admixture is 10 parts by weight, the barium sulfate admixture is 5 parts by weight, and the antistatic admixture is 2.5 parts by weight. In this case, the calcium carbonate admixture contains 8 parts by weight of the calcium carbonate and 2 parts by weight of the high density polyethylene, the barium sulfate admixture contains 4 parts by weight of the barium sulfate and 1 part by weight of the high density polyethylene, and the antistatic admixture contains 1 part by weight of the antistatic agent and 1.5 parts by weight of the high density polyethylene.

[0011] This configuration allows for optimum strength and weight to be achieved as a bag for wrapping newspapers. Effect of the Invention

[0012] According to this invention, it is possible to realize a newspaper packaging bag that maintains sufficient strength while being lightweight. [Brief description of the drawings]

[0013] [Figure 1] 1 is a diagram showing the configuration of a newspaper packaging bag 10 according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] Hereinafter, the embodiment of the present invention will be described with reference to the drawings as appropriate. Note that the embodiment described below is merely an example of the present invention, and the embodiment of the present invention can be modified as appropriate without departing from the scope of the present invention.

[0015] Fig. 1 is a diagram showing the overall configuration of a newspaper packaging bag 10 according to an embodiment of the present invention. Note that Fig. 1 shows a part of the inside of the newspaper packaging bag 10.

[0016] A newspaper packaging bag 10 according to an embodiment of the present invention is a newspaper packaging bag for storing newspapers 20 therein. The newspaper packaging bag 10 is sealed after storing newspapers 20 therein to prevent the newspapers 20 from getting wet in bad weather such as rain or snow. The newspaper packaging bag 10 shown in Fig. 1 has a bag body 11 in which two thin resin sheets 12, 13 are stacked so as to face each other.

[0017] The bag body 11 of the newspaper packaging bag 10 is made by cooling and stacking raw material sheets, which are made of raw materials including multiple resin materials and additives, formed into a cylindrical shape by a conventionally known inflation molding machine. The raw material sheet is cut to a predetermined length to obtain the bag body 11, which is made of two thin resin sheets 12 and 13.

[0018] The bag body 11 is formed in a rectangular shape, specifically, as shown in Fig. 1. The bag body 11 is formed so that the longitudinal dimension (vertical dimension) is, for example, about 490 mm, and the transverse dimension (horizontal dimension) is about 300 mm. Here, the longitudinal direction is the up-down direction (vertical direction) on the plane of Fig. 1, and the transverse direction is the left-right direction (horizontal direction) on the plane of Fig. 1. The shapes and sizes of the newspaper packaging bag 10 and the bag body 11 are not limited to those described above, and may be any that are suitable for the folded shape of the newspaper 20 to be contained and the size of the newspaper 20.

[0019] The thickness of each of the resin sheets 12, 13 of the bag body 11 is approximately 7.0 μm (±0.6 μm). The thickness of the resin sheets 12, 13 may be within a range of 5 to 10 μm, but for packaging newspaper 20, the thickness of the resin sheets 12, 13 is optimally approximately 7.0 μm (±0.6 μm) as described above.

[0020] The newspaper packaging bag 10 has both top and bottom ends closed with the newspaper 20 contained inside the bag body 11. The newspaper packaging bag 10 is produced as follows: The raw sheet is pulled out from a roll (raw sheet roll) (not shown) around which the long cylindrical raw sheet before being cut is wound, and the newspaper 20 (approximately A3 size) folded in four (8P fold) is placed inside the raw sheet, i.e., between the resin sheet 12 and the resin sheet 13, and in this state, the outer portion of the peripheral edge of the newspaper 20 is heat-sealed by a heat-sealing device and cut at the same time.

[0021] The newspaper packaging bag 10 is not limited to the one produced by the above-mentioned method. For example, a method of producing the newspaper packaging bag 10 by overlapping two resin sheets so that the newspaper 20 is placed inside, and then heat-welding the upper, lower, left, and right ends and cutting them may be adopted.

[0022] The newspaper packaging bag 10 can also be made by folding one resin sheet in half, placing the newspaper 20 inside, and then heat-welding the three edges to produce the newspaper packaging bag 10. It can also be made by the method described in the above-mentioned Patent Document 1 (JP Patent Publication 2006-335426 A) or other conventionally known methods.

[0023] 1, seal lines (sealed portions) 21, 22 are formed by heat welding the resin sheets 12, 13 to each other near both ends 101, 102 on one side of the longitudinal direction of the bag body 11. The seal lines 21, 22 are formed at positions spaced a predetermined distance L1 (e.g., about 30 mm) toward the center.

[0024] As described above, the raw sheet for producing the newspaper packaging bag 10 of this embodiment is formed to a thickness of approximately 7.0 μm, and contains 100 parts by weight of high density polyethylene (HDPE), 5 to 10 parts by weight of linear low density polyethylene (LLDPE), 5 to 15 parts by weight of calcium carbonate admixture, 2 to 8 parts by weight of barium sulfate admixture, and 1.5 to 3.5 parts by weight of antistatic admixture.

[0025] Specifically, the raw fabric sheet for the newspaper packaging bag 10 is produced by feeding a blend of 100 parts by weight of high density polyethylene (HDPE), 5 to 10 parts by weight of linear low density polyethylene (LLDPE), 5 to 15 parts by weight of a calcium carbonate admixture, 2 to 8 parts by weight of a barium sulfate admixture, and 1.5 to 3.5 parts by weight of an antistatic admixture into the extruder of the inflation molding machine, where the blended raw fabric is heated, melted, and kneaded at a temperature of 190 to 210°C, extruded through a mold (round die, ring die) by the well-known inflation molding method, and inflated by blowing in air to produce the cylindrical (tube-shaped) raw fabric sheet with a thickness of approximately 7.0 μm that serves as the basis for the newspaper packaging bag 10.

[0026] Here, the calcium carbonate admixture is an admixture containing a predetermined amount of calcium carbonate and a predetermined amount of the high-density polyethylene, and has been sufficiently kneaded in advance so that the calcium carbonate and the high-density polyethylene are well mixed with each other before being mixed with the raw materials.

[0027] In addition, the barium sulfate admixture is an admixture containing a predetermined amount of barium sulfate and a predetermined amount of the high-density polyethylene, and has been thoroughly kneaded in advance so that the barium sulfate and the high-density polyethylene are compatible with each other before being mixed into the raw materials.

[0028] In addition, the antistatic admixture is an admixture containing a predetermined amount of an antistatic agent and a predetermined amount of the high-density polyethylene, and has been sufficiently kneaded in advance so that the antistatic agent and the high-density polyethylene are compatible with each other before being mixed into the raw materials.

[0029] As a more preferred example of the weight ratio of each raw material in the blended raw materials, when the high density polyethylene (HDPE) constituting the raw sheet is 100 parts by weight, it is preferable that the linear low density polyethylene is 7 parts by weight, the calcium carbonate admixture is 10 parts by weight, the barium sulfate admixture is 5 parts by weight, and the antistatic admixture is 2.5 parts by weight. In this case, the calcium carbonate admixture contains 8 parts by weight of the calcium carbonate and 2 parts by weight of the high density polyethylene, the barium sulfate admixture contains 4 parts by weight of the barium sulfate and 1 part by weight of the high density polyethylene, and the antistatic admixture contains 1 part by weight of the antistatic agent and 1.5 parts by weight of the high density polyethylene. The weight ratio of each raw material is not limited to such a numerical value, and it is possible to apply a weight ratio arbitrarily determined within the numerical range of each weight ratio of each of the above-mentioned raw materials.

[0030] As described above, the thickness of one of the resin sheets of the raw sheet (the portion corresponding to the resin sheets 12 and 13) is not limited to 7 μm, but may be any thickness within the range of 5 to 10 μm.

[0031] In the case of the base sheet blended in this manner, the resin sheet is foamed by the calcium carbonate and barium sulfate, so when compared to conventional base sheets manufactured using high density polyethylene (HDPE), linear low density polyethylene (LLDPE), and a small amount of antistatic agent as the main raw materials, the amount of resin material (high density polyethylene and linear low density polyethylene) can be reduced by approximately 10% when compared at the same thickness.

[0032] Therefore, by producing the newspaper packaging bag 10 from the raw fabric sheet of this embodiment, it is possible to achieve weight reduction without reducing the strength of the newspaper packaging bag 10. In other words, since the raw fabric sheet is configured with the above-mentioned blending ratio, the newspaper packaging bag 10 produced from this has the best balance between strength and weight reduction.

[0033] In addition, when the newspaper packaging bag 10 made from the raw material sheet of this embodiment is used and incinerated as waste, since the raw materials of the newspaper packaging bag 10 are mixed in the weight ratio described above, not only the weight but also the amount of combustion gases such as carbon dioxide generated can be reduced compared to conventional bags of the same size. [Explanation of symbols]

[0034] 10:Newspaper packaging bag 11: Bag body 12: Resin sheet 13: Resin sheet 20: Newspaper 21: Seal Line 22: Seal Line

Claims

1. A raw sheet used for producing a newspaper packaging bag formed in a rectangular shape in which newspapers are contained, A raw sheet having a thickness of 5 to 10 μm, comprising: 100 parts by weight of high density polyethylene; 5 to 10 parts by weight of linear low density polyethylene; 5 to 15 parts by weight of a calcium carbonate admixture containing calcium carbonate and the high density polyethylene; 2 to 8 parts by weight of a barium sulfate admixture containing barium sulfate and the high density polyethylene; and 1.5 to 3.5 parts by weight of an antistatic admixture containing an antistatic agent and the high density polyethylene.

2. A raw sheet used for producing a newspaper packaging bag formed in a rectangular shape in which newspapers are contained, A raw material mixture of 100 parts by weight of high density polyethylene, 5 to 10 parts by weight of linear low density polyethylene, 5 to 15 parts by weight of a calcium carbonate admixture containing calcium carbonate and the high density polyethylene, 2 to 8 parts by weight of a barium sulfate admixture containing barium sulfate and the high density polyethylene, and 1.5 to 3.5 parts by weight of an antistatic agent and an antistatic admixture containing the high density polyethylene is heated and melted at a temperature of 190 to 210°C, and formed into a cylindrical shape having a thickness of 5 to 10 μm by an inflation molding method.

3. The linear low density polyethylene is 7 parts by weight, the calcium carbonate admixture is 10 parts by weight, the barium sulfate admixture is 5 parts by weight, and the antistatic admixture is 2.5 parts by weight. The calcium carbonate admixture contains 8 parts by weight of the calcium carbonate and 2 parts by weight of the high-density polyethylene, The barium sulfate admixture includes 4 parts by weight of the barium sulfate and 1 part by weight of the high density polyethylene, 3. The raw sheet according to claim 1, wherein the antistatic mixture comprises 1 part by weight of the antistatic agent and 1.5 parts by weight of the high density polyethylene.

Citation Information

Patent Citations

  • Method and device for reusing newspaper packaging bag

    JP2006335426A