Radiation detection method, radiation detection liquid manufacturing method, and radiation detection device
A radiation detection method using a tungsten oxide and iron ion-containing liquid offers a simple, fast, and reversible means to detect multiple types of radiation, including ionizing and non-ionizing radiation, without external power or heating, addressing the limitations of existing technologies.
Patent Information
- Application Number
- JP2021031480
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-03-01
- Publication Date
- 2024-09-24
- Estimated Expiration
- 2041-03-01
AI Technical Summary
Existing radiation detection methods require external power sources, high-temperature treatments, or laser irradiation, and are not suitable for repeated measurements, especially for detecting multiple types of radiation including ionizing and non-ionizing radiation like ultraviolet rays.
A radiation detection method using a liquid containing tungsten oxide particles and iron ions that changes color upon radiation exposure, allowing for rapid, reversible detection without external power or heating, and suitable for detecting various types of radiation.
The method provides a simple, fast, and reliable means to detect ionizing radiation and ultraviolet rays through color changes, enabling repeated measurements and clear identification of radiation presence or absence.
Smart Images

Figure 0007555074000004 
Figure 0007555074000005 
Figure 0007555074000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a method for detecting radiation, a method for producing a radiation detecting liquid, and a radiation detecting device. [Background technology]
[0002] When handling radiation such as alpha rays, beta rays, X-rays, gamma rays, and neutron rays in controlled areas such as nuclear power plants and radiation therapy rooms, it is mandatory to manage exposure dose values and working hours within the controlled area.
[0003] In addition, following the Chernobyl nuclear power plant accident in 1986 and the Fukushima Daiichi nuclear power plant accident in 2011, radioactive materials and radiation leaked outside the facilities, making it necessary to continuously measure and manage environmental radiation in nearby areas. In addition, when working on decontamination work following the accidents, it is essential to measure radiation using radiation detection devices in order to manage the workers' own exposure.
[0004] Radiation detection devices are used according to the type of radiation, the purpose of measurement, etc., and examples include Geiger-Muller (GM) counters, scintillation detectors, film badges for personal exposure, pocket dosimeters for personal exposure, thermoluminescence dosimeters, fluorescent glass dosimeters, and optically stimulated luminescence dosimeters. Scintillation detectors come in a wide variety of configurations, including inorganic solids, organic substances, gases, and liquids, and are appropriately selected and used according to the application.
[0005] The characteristics of the radiation detection devices mentioned above each have their own advantages and disadvantages. For example, the GM counter has a high gain and can detect radiation with a strong signal, but the device is complicated because an inert gas is sealed inside the tube, and it has disadvantages such as the inability to measure radiation energy in principle. Among scintillation detectors, those based on inorganic solids such as sodium iodide (NaI), zinc sulfide (ZnS), and cesium iodide (CsI) can be expected to have high output and linearity, but they have issues such as long response time. In addition, liquid scintillation counters (LSCs), which are made by dissolving organic scintillators such as diphenyloxazole (POP) in an organic solvent, can measure samples with multiple nuclides in principle, but depending on the sample, there is a decrease in counting efficiency due to the quenching phenomenon and a decrease in measurement accuracy due to chemiluminescence.
[0006] When the above-mentioned radioactive worker manages radiation exposure dose at the individual level, he / she often carries a pocket dosimeter for personal exposure using high-purity silicon (Si) or germanium (Ge) semiconductors, and a film badge as a backup dosimeter. The reason for this is that the actual dose value and actual working hours cannot be grasped due to the pocket dosimeter's dead battery or malfunction. On the other hand, when managing radiation exposure dose with a film badge, the film is developed and the radiation dose is measured by a specialized measurement company, but the frequency of replacing the film badge is usually on a monthly basis, and it takes at least several days for the results of the exposure amount to be known, making it difficult to grasp the actual dose value and actual working hours on a daily basis.
[0007] Thermoluminescence dosimeters detect radiation by the emission of visible light due to heating (thermoluminescence) after radiation interacts with an element made of calcium fluoride (CaF) or lithium fluoride (LiF). Fluorescent glass dosimeters detect radiation by the excitation and emission due to ultraviolet light irradiation (radiophotoluminescence) after radiation interacts with an element made of silver (Ag) ion-containing phosphate glass. These methods can repeatedly measure various types of radiation, but require high-temperature treatment during measurement or initialization, which may cause deterioration of the element over time.
[0008] As a next-generation dosimeter that solves the problems of the thermoluminescence dosimeter and the fluorescent glass dosimeter, an optically stimulated luminescence (OSL) dosimeter may be used. Patent Documents 1 and 2 describe a method for detecting and measuring radiation using an OSL dosimeter. In the OSL dosimeter, stable alumina (Al2O3) is used as the base element, and radiation is detected by irradiating it with a laser beam to emit fluorescence after interacting with radiation. Since the OSL dosimeter does not require heating during measurement or initialization, the device can be made compact and the influence of heat can be eliminated. However, since laser beams are irradiated to detect radiation, external energy (power source) is required, as with the thermoluminescence dosimeter and the fluorescent glass dosimeter.
[0009] By the way, ultraviolet rays have almost no ionizing effect like the above-mentioned alpha rays, beta rays, X-rays, gamma rays, and neutron rays, so they are sometimes called non-ionizing radiation like radio waves, infrared rays, and visible light, but in a broad sense they belong to the category of radiation. Among ultraviolet rays, UV-A (wavelength range 315nm to 400nm) and UV-B (wavelength range 285nm to 315nm) can damage the skin and cause spots, wrinkles, and skin cancer. Therefore, from the perspective of health management, it is important to measure / monitor ultraviolet rays as well as ionizing radiation.
[0010] Known methods for detecting ultraviolet rays include, for example, those based on diamond or silicon semiconductors, and Schottky contact type ultraviolet sensors mainly made of zinc oxide (ZnO) with a large band gap, as described in Patent Document 3. In addition, ultraviolet detection devices using materials that exhibit so-called photochromic properties, in which the molecular structure changes due to ultraviolet light and the absorption spectrum in the visible light region changes accordingly, are commercially available, and the strength of ultraviolet rays can be grasped depending on the degree of coloration.
[0011] However, the above-mentioned ultraviolet detection devices are not compatible with the detection of ionizing radiation. Furthermore, some photochromic materials have problems such as being unable to be used repeatedly because the coloring (discoloration) is irreversible. [Prior art documents] [Patent documents]
[0012] [Patent Document 1] Special Publication No. 2000-503396 [Patent Document 2] Special Publication No. 2000-503759 [Patent Document 3] JP 2007-201393 A Summary of the Invention [Problem to be solved by the invention]
[0013] A method for detecting radiation is preferred that does not require any auxiliary equipment such as an external power source, high-temperature treatment, laser irradiation, etc., has a simple structure, has a fast response speed, is clearly identifiable, allows repeated measurements, and is compatible with several types of radiation including ultraviolet light.
[0014] One of several objects of the present disclosure is to provide a novel method for detecting radiation, a radiation detecting liquid used in the method for detecting radiation, and a radiation detecting device used in the method for detecting radiation. [Means for solving the problem]
[0015] The gist of the present disclosure is as follows. [1] A method for detecting radiation, comprising: preparing a radiation detecting liquid containing tungsten oxide particles and iron ions; and detecting radiation based on a color change of the radiation detecting liquid when radiation is irradiated to the radiation detecting liquid. [2] A method for detecting radiation, comprising: preparing a support to which a radiation detecting liquid containing tungsten oxide particles and iron ions has been applied; and detecting radiation based on a color change of the support when the support is irradiated with radiation. [3] The radiation detection method according to [2], wherein the support is in a dry state. [4] The radiation detection method according to any one of [1] to [3], wherein the tungsten oxide particles have a particle diameter of 1.0 μm or less when their accumulated volume is 50.0%. [5] The radiation detection method according to any one of [1] to [4], wherein the elemental concentration of tungsten in the radiation detection liquid is higher than the elemental concentration of iron. [6] The radiation detection method according to any one of [1] to [5], which detects at least one type of radiation selected from the group consisting of X-rays, gamma rays, alpha rays, beta rays, and ultraviolet rays.
[0016] [7] A method for producing a radiation detecting liquid used in the radiation detection method according to any one of [1] to [6], the method comprising: dissolving metallic tungsten in an aqueous hydrogen peroxide solution to prepare a tungsten-containing solution; preparing an iron-containing solution containing iron ions; mixing the tungsten-containing solution with the iron-containing solution; and irradiating the obtained mixed solution with light. [8] The method for producing a radiation detecting liquid according to [7], wherein preparing the iron-containing solution includes extracting at least a portion of acidic water obtained by contacting the positive electrode with a first water and a second water separated from each other and an iron-containing positive electrode and an iron-containing negative electrode electrically connected to each other, in a configuration in which at least a portion of the positive electrode is immersed in the first water and at least a portion of the negative electrode is immersed in the second water. [9] The method for producing a radiation detecting liquid according to [7] or [8], wherein the light irradiated to the mixed solution has a wavelength of maximum intensity in the light spectrum of less than 400 nm.
[10] A method for producing a support for use in the radiation detection method described in [2], comprising: preparing a radiation detecting liquid in accordance with the method described in any one of [7] to [9]; applying the radiation detecting liquid to a support; and drying the support to remove moisture.
[11] A radiation detection device for use in the radiation detection method described in [1], comprising a container and the radiation detecting liquid contained in the container.
[12] The radiation detection device described in
[11] , wherein the container further comprises an openable and closable lid.
[13] A radiation detection device for use in the radiation detection method according to [2], comprising a support on which the radiation detection liquid is applied.
[14] The radiation detection device according to
[13] , wherein the support is in a dry state.
[15] A radiation detection device for use in the radiation detection method according to [2], comprising a support, and tungsten oxide particles and iron ions supported on the support.
[16] A radiation detection device for use in the radiation detection method according to [2], comprising: a support; and a radiation detection layer formed on the support and containing tungsten oxide particles and iron ions. Effect of the Invention
[0017] According to the present disclosure, it is possible to provide a novel radiation detection method, a radiation detecting liquid used in the radiation detection method, and a radiation detection device used in the radiation detection method. [Brief description of the drawings]
[0018] [Figure 1] FIG. 1 is a schematic diagram (perspective view) showing a radiation detection method according to one embodiment. [Diagram 2] FIG. 2 is a schematic diagram (perspective view) showing a radiation detection method according to another embodiment. [Diagram 3] FIG. 3 is a schematic diagram showing the crystal structure of a perovskite-type oxide. [Figure 4] FIG. 4 is a schematic cross-sectional view illustrating an example of a method for producing an iron-containing solution. [Diagram 5] FIG. 5 is a schematic cross-sectional view showing an example of an electrical connector for a positive electrode and a negative electrode. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] Hereinafter, several embodiments of the present invention will be described in detail. However, the present invention is not limited to the following embodiments. Not only an independent process, but also a process that cannot be clearly distinguished from other processes is implied in the term "process" as long as its purpose is achieved. A numerical range indicated using "to" includes the numerical values before and after "to" as the minimum and maximum values, respectively. In the drawings, equivalent components are given the same symbols.
[0020] In this specification, the term "positive electrode" refers to an electrically connected member in which an anodic reaction occurs to generate metal ions and electrons, and in this specification, the term "negative electrode" refers to an electrically connected member in which a cathodic reaction occurs to generate hydroxide ions.
[0021] The radiation detection method of the present embodiment can include preparing a radiation detection liquid containing tungsten oxide particles and iron ions, and detecting radiation based on a color change of the radiation detection liquid when radiation is irradiated to the radiation detection liquid. A radiation detection device that can be preferably used in this radiation detection method can include a container and a radiation detecting liquid contained in the container.
[0022] In one embodiment of the radiation detection method, when radiation is irradiated to a radiation detecting liquid contained in a container, radiation can be detected by a color change of the radiation detecting liquid. This radiation detecting liquid contains tungsten oxide particles and iron ions. The mechanism by which the radiation detecting liquid changes color upon irradiation with radiation will be described below. It is believed that the radiation detecting liquid changes color as a result of the tungsten oxide particles becoming colored upon irradiation with radiation. Note that the mechanism by which the radiation detecting liquid becomes colored upon irradiation with radiation is not limited to the mechanism described below.
[0023] Figure 3 is a schematic diagram showing the crystal structure of a typical perovskite oxide, represented as ABO3. Tungsten oxide (WO3) belongs to the perovskite oxide type, and in the tungsten oxide crystal, the A site is a vacancy and the B site is tungsten (W). That is, in the tungsten oxide crystal, oxygen (O) is coordinated six times around the tungsten (W) ion to form an octahedron. In addition, tungsten oxide is connected by sharing the oxygen at the vertices of the octahedron. Furthermore, tungsten oxide can accommodate many elements in the vacant A site.
[0024] Tungsten oxide acts as a semiconductor when it is excited by high energy such as radiation or light, and electrons (e - ) and holes (h + ) is then generated. + ) reacts with water to produce hydrogen ions (H +) is produced. As shown in the following reaction formula (3), tungsten bronze (H x Generally, the color of WO3 as a bulk material is ochre, and H x The color of WO3 is deep blue. WO3+hν→WO3(e - +h + ) (1) h + +(1 / 2)H2O→H + +(1 / 4)O2(2) WO3+xH + +xe - →H x WO3(3)
[0025] Tungsten bronze (H x The reason why tungsten oxide (WO3) is dark blue is thought to be as follows. The electrons (e - ) converts some of the tungsten ions to hexavalent (W 6+ ) to 5-valent (W 5+ ), W 6+ / W 5+ A mixed valence state occurs. As a result, W 6+ and W 5+ Tungsten bronze absorbs visible light in the range of about 600 to 800 nm due to valence transfer absorption by electrons transitioning between H and H. x WO3) appears dark blue.
[0026] The radiation detecting liquid of this embodiment is colorless and transparent when not irradiated with radiation, and turns tungsten bronze (H x The reason why the radiation detecting liquid is colorless and transparent when not irradiated with radiation is explained in more detail below.
[0027] <Radiation detection liquid> One embodiment of the radiation detecting liquid may contain tungsten oxide particles and iron ions. The radiation detecting liquid preferably contains water as a dispersion medium. The content of water in the total mass of the radiation detecting liquid is preferably 50 mass % or more, more preferably 80 mass % or more, and more preferably 95 mass % or more. The radiation detecting liquid preferably contains tungsten oxide particles dispersed in the dispersion medium and iron ions dissolved therein. The iron ions in the radiation detecting liquid are Fe 2+ It is preferred that the compound contains The radiation detecting liquid can be obtained by mixing a tungsten-containing solution obtained by dissolving metallic tungsten in an aqueous hydrogen peroxide solution with an iron-containing solution containing iron ions, and irradiating the resulting mixed liquid with light. The color of the radiation detecting liquid obtained in this way is not the ochre color of WO3 as a bulk material, but is colorless and transparent when not irradiated with radiation. This can be considered, for example, as follows.
[0028] In the radiation detection liquid, iron ions (Fe 2+ ) is supported (hereinafter referred to as "WO3(Fe 2+ As described below, by dissolving metallic tungsten in a hydrogen peroxide solution, a tungsten-containing solution is obtained, in which tungstate ions (WO4 2- When a tungsten-containing solution is mixed with an iron-containing solution that contains iron ions, and light is irradiated to produce a radiation detecting liquid, iron ions (Fe 2+ ) inhibits the growth of WO3 particles, making the radiation detection liquid colorless and transparent.
[0029] In the case of a radiation detecting liquid that has become colored by radiation irradiation, it is preferable that the radiation detecting liquid return to being colorless and transparent when the radiation irradiation is stopped. This can be considered, for example, as follows. That is, tungsten bronze (H x When oxygen is dissolved in the radiation detection liquid or supplied from the outside, tungsten oxide (WO3) returns to tungsten oxide as shown in the following reaction formula (4). At this time, the tungsten ions are pentavalent (W 5+) to hexavalent (W 6+ ) is oxidized to H x WO3+xO2→WO3+xH2O (4)
[0030] <Tungsten-containing solution> The tungsten-containing solution can be obtained by dissolving metallic tungsten in an aqueous hydrogen peroxide solution. The tungsten-containing solution contains tungstate ions (WO4 2- ) is dispersed and generated. Metallic tungsten is dissolved in a hydrogen peroxide solution to form tungstate ions (WO4 2- The reaction to produce 2,4-dichlorophenyl ether is represented by the following reaction scheme (5). W+H2O2→WO4 2+ +H + +2H2O (5)
[0031] The shape of the metallic tungsten is not particularly limited. The metallic tungsten is preferably in a bulk or powder form from the viewpoint of solubility in an aqueous hydrogen peroxide solution and workability. For example, the metallic tungsten particles in powder form having an average particle size based on volume in a laser scattering method of 0.1 to 10 μm is preferred, and the metallic tungsten particles in powder form having an average particle size of 0.5 to 1 μm is more preferred.
[0032] The purity of the metallic tungsten is not particularly limited. From the viewpoint of coloring properties as a radiation detecting liquid, the purity of the metallic tungsten is preferably 10.0 to 100.0 mass%, more preferably 15.0 to 100.0 mass%, and even more preferably 20.0 to 100.0 mass%. The higher the purity of the metallic tungsten, the more colorless and transparent the radiation detecting liquid obtained is, and the easier it is to distinguish the degree of coloring upon irradiation with radiation. From this viewpoint, the purity of the metallic tungsten is preferably 50.0 mass%, more preferably 80.0 mass% or more, and even more preferably 95.0 mass% or more.
[0033] The hydrogen peroxide concentration in the aqueous hydrogen peroxide solution is not particularly limited, but from the viewpoints of solubility of metallic tungsten, workability, and versatility, the hydrogen peroxide concentration in the aqueous hydrogen peroxide solution is preferably 1.0 to 50.0 mass%, more preferably 2.0 to 40.0 mass%, and even more preferably 3.0 to 30.0 mass%.
[0034] The content of metallic tungsten per 100 parts by mass of the aqueous hydrogen peroxide solution is preferably 0.1 to 10 parts by mass, and more preferably 1 to 5 parts by mass, from the viewpoints of the solubility of metallic tungsten and the coloring properties as a radiation detecting liquid.
[0035] <Iron-containing solution> The iron-containing solution contains iron ions. The iron-containing solution contains Fe 2+ and water, Fe 2+ and water. The iron-containing solution is preferably used as acidic water obtained by contacting the positive electrode in a configuration in which the first water and the second water are separated from each other and the iron-containing positive electrode and the iron-containing negative electrode are electrically connected to each other, at least a part of the positive electrode is immersed in the first water and at least a part of the negative electrode is immersed in the second water. An example of a method for producing the iron-containing solution will be described below. Note that the method for producing the iron-containing solution is not limited to the following method.
[0036] A schematic diagram showing an example of a method for producing an iron-containing solution is shown in Fig. 4. The apparatus for producing an iron-containing solution shown in Fig. 4 has a container 6, a partition 7, a positive electrode 9a, and a negative electrode 9b, and the container 6 contains a first water 8a and a second water 8b in the spaces separated by the partition 7. The material of the container 6 is not particularly limited and may be glass, quartz glass, resin, ceramics, metal, or the like. The positive electrode 9a and the negative electrode 9b contain iron. The positive electrode 9a and the negative electrode 9b are electrically connected to each other. The positive electrode 9a and the negative electrode 9b are long and preferably extend substantially parallel to the bottom surface of the container 6. The electrical connector between the positive electrode 9a and the negative electrode 9b penetrates the partition material 7. The positive electrode 9a is preferably completely immersed in the first water 8a, and the negative electrode 9b is preferably completely immersed in the second water 8b.
[0037] Fig. 5 shows in more detail the electrical connection of the positive electrode 9a and the negative electrode 9b shown in Fig. 4. In Fig. 5, the electrical connection is made of the same metal member containing iron (for example, an iron material), and of the metal members, the negative electrode 9b is covered with a conductive film 10. That is, of the metal member, the part not covered with the conductive film 10 functions as the positive electrode 9a, and the part of the metal member covered with the conductive film 10 functions as the negative electrode 9b.
[0038] When the electrically connected positive electrode 9a and negative electrode 9b are immersed in water in the above-mentioned configuration, the iron corrosion reaction shown in the following reaction formula (6) proceeds in the positive electrode 9a. Here, for example, when the water is neutral and contains dissolved oxygen, the following reaction formula (7) corresponding to the following reaction formula (6) occurs. That is, a local battery may be formed in the positive electrode 9a, but the iron corrosion reaction is difficult to occur in the negative electrode 9b because it is covered with the conductive film 10, and the above reaction formula (7) occurs preferentially in the negative electrode 9b. That is, most of the electrons generated in the anode reaction of the positive electrode 9a move to the negative electrode 9b. Note that, when dissolved oxygen is not contained in the water, it is considered that some of the electrons generated in the anode reaction of the positive electrode 9a are consumed in the reaction shown in the following reaction formula (8). In the positive electrode 9a, hydroxide ions (OH - ) and the iron ions (Fe 2+ ) reacts with iron hydroxide (II) (Fe(OH)2) to produce iron hydroxide (II) (Fe(OH)2) as shown in the following reaction formula (9). Then, the iron hydroxide (II) (Fe(OH2) undergoes an oxidation reaction with dissolved oxygen as shown in the following reaction formula (10), and the iron hydroxide (II) (Fe(OH)2) reacts directly with water as shown in the following reaction formula (11), to produce iron hydroxide (III) (Fe(OH)3) and hydrogen ions (H + As a result of this series of reactions, hydrogen ions (H + ) concentration increases, the water on the positive electrode 9a side turns into acidic water, and the iron ions (Fe 2+In addition, the negative electrode 9b contains hydroxide ions (OH - ) concentration increases, and the water on the negative electrode 9b side turns into reduced water. In addition, as water molecules are released from the iron hydroxide (III) (Fe(OH)3) generated on the positive electrode 9a side, iron oxide (Fe2O3) is generated as shown in the following reaction formula (12). 2Fe → 2Fe 2+ +4e - (6) O2+2H2O+4e - →4OH - (7) 2H2O+2e - →2OH - +H2(8) Fe 2+ +2OH - →Fe(OH)2(9) 4Fe(OH)2+2H2O+O2→4Fe(OH)3(10) Fe(OH)2+H2O→Fe(OH)3+H + +e - (11) 2Fe(OH)3 → Fe2O3 + 3H2O (12)
[0039] Metallic members containing iron can be used for the negative electrode and the positive electrode, and one side of a long metallic member can be used as the negative electrode and the other side as the positive electrode. The purity of iron in the metallic member is not particularly limited. From the viewpoint of the reaction rate at the positive electrode and the total amount of electrons moving to the negative electrode, the purity of iron in the metallic member is preferably 10.0 to 100.0 mass%, more preferably 15.0 to 100.0 mass%, further preferably 20.0 to 100.0 mass%, particularly preferably 50.0 to 100.0 mass%, extremely preferably 80.0 to 100.0 mass%, and very preferably 90.0 to 100.0 mass%. The metallic member may be pure iron. The purity of iron in the metallic member may be less than 100.0 mass%. The higher the purity of iron in the metallic member, the easier the corrosion reaction as a positive electrode progresses, and the iron-containing solution is effectively produced.
[0040] The metal member may include an iron alloy, such as an Fe-C alloy, an Fe-Au alloy, an Fe-Al alloy, an Fe-B alloy, an Fe-Ce alloy, an Fe-Cr alloy, an Fe-Cr-Ni alloy, an Fe-Cr-Mo alloy, an Fe-Cr-Al alloy, an Fe-Cr-Cu alloy, an Fe-Cr-Ti alloy, an Fe-Cr-Ni-Mn alloy, an Fe-Cu alloy, an Fe-Ga alloy, an Fe-Ge alloy, an Fe-Mg alloy, an Fe-Mn alloy, an Fe-Mo alloy, an Fe-N alloy, an Fe-Nb alloy, an Fe-Ni alloy, an Fe-P alloy, an Fe-S alloy, an Fe-Si alloy, an Fe-Si-Ag alloy, an Fe-Si-Mg alloy, an Fe-Ti alloy, an Fe-U alloy, an Fe-V alloy, an Fe-W alloy, or an Fe-Zn alloy.
[0041] From the viewpoint of corrosion reaction efficiency in the positive electrode, the iron content in the iron alloy is preferably 10.0 to 99.9 mass %, more preferably 15.0 to 99.8 mass %, and even more preferably 20.0 to 99.5 mass %.
[0042] The metal member may further contain other atoms that are inevitably mixed in. The content of the other atoms that are inevitably mixed in may be, for example, 3.0 mass% or less based on the total mass of the metal member. From the viewpoint of corrosion reaction efficiency at the positive electrode, the content of the above atoms contained in the metal member is preferably 1.0 mass% or less, more preferably 0.8 mass% or less, even more preferably 0.5 mass% or less, and particularly preferably 0.2 mass% or less.
[0043] The shape of the metal member is not particularly limited. Examples of the shape of the metal member include a plate shape, a block shape, a round wire shape, a sheet shape, and a combination of these shapes. The shape of the metal member is preferably a plate shape, a block shape, or a sheet shape from the viewpoints of the specific surface area as a reaction field for the anode reaction and the cathode reaction, the volume resistance as a metal member, and the workability of immersing in water.
[0044] When a metal member containing iron is used for the negative electrode and the positive electrode, the metal member can be partially made conductive, and the conductive part can be treated as the negative electrode. For example, the metal member can be partially covered with a conductive film, and the part can be treated as the negative electrode. By covering the surface of the negative electrode with a conductive film, contact between iron and water in water is suppressed, and the corrosion reaction shown in the above reaction formula (6) is less likely to proceed, and the cathodic reaction shown in the above reaction formula (7), for example, is promoted.
[0045] The conductive film may have conductivity. The conductive film may contain a conductivity imparting agent. As the conductivity imparting agent, conductive particles made of metal, carbon material (carbon), etc. may be used.
[0046] The method for producing an iron-containing solution may include a conductive film forming step of covering the negative electrode with a conductive film. In the conductive film forming step, the conductive film can be formed by applying a composition containing a conductive agent to the surface of the negative electrode, followed by drying, curing or sintering. Examples of the composition containing the conductive agent include inks and pastes obtained by dispersing the conductive agent in a liquid (such as an organic solvent). For example, a conductive film can be formed by applying an oil-based marking pen to the surface of a metal member and then drying it, and the part coated with the oil-based marking pen can be used as the negative electrode.
[0047] The conductive film may contain a metal having a higher standard electrode potential than iron. This causes galvanic corrosion when the metal member is immersed in water, reduces the corrosion rate at the negative electrode portion, and promotes the cathodic reaction shown in the above reaction formula (7). Examples of metals having a higher standard electrode potential than iron include nickel, tin, tungsten, bismuth, copper, and silver.
[0048] The method for forming a conductive film from a metal having a higher standard electrode potential than iron is not particularly limited, and may be, for example, a sputtering method, a vacuum deposition method, a pulse laser deposition (PLD), or the like. Alternatively, the conductive film may be formed by applying a paste containing a metal having a high standard electrode potential to the surface of a metal member by screen printing, inkjet, or the like, and then drying, curing, or sintering the paste by heating or the like. In this case, the film formation conditions can be appropriately selected so that the metal member is not dissolved, corroded, or peeled off by a chemical solution, or the metal member is not excessively oxidized by heat treatment, or the like.
[0049] The material and dimensions of the partition separating the positive electrode water and the negative electrode water are not particularly limited. The material of the partition may be the same as the material of the container, or may be different. It is preferable that the dimensions of the partition are the same as the inner dimensions of the container, so that the first water and the second water are separated and do not mix. Examples of the material of the partition include glass, quartz glass, polyethylene, polystyrene, polyamide, polyester, cellulose resin, silicon resin, fluorine-based resin, acrylic resin, phenolic resin, polyolefin, cellophane, craft paper, vinylon-mixed paper, synthetic pulp-mixed paper, polyolefin nonwoven fabric, cupra nonwoven fabric, polyamide nonwoven fabric, glass fiber nonwoven fabric, alumina, silicon carbide, aluminum nitride, boron nitride, and sialon.
[0050] A membrane that does not allow water molecules to pass through but allows specific ions to pass through (specifically, an ion-conductive polymer membrane, an ion-conductive solid electrolyte membrane, a polyolefin porous membrane, a cellulose porous membrane, etc.) can also be used as the partition material. Examples of ion-conductive polymer membranes include cation exchange membranes and anion exchange membranes. More specific examples include Selemion APS (registered trademark) (AGC), Nafion (registered trademark) (DuPont), and Neocepta (registered trademark) (Astrom). As a cation exchange membrane, a fluorine-based ion exchange membrane (for example, manufactured by DuPont, product name: Nafion117) can be used.
[0051] The positive electrode 9a and the negative electrode 9b are immersed in the first water 8a and the second water 8b contained in the container 6 and separated by the partition material 7, and are held in this state, whereby the above reaction proceeds, and the second water 8b in contact with the positive electrode can be collected as an iron-containing solution. This holding time may be a time during which the reaction proceeds sufficiently, and is not particularly limited, and may be 10 minutes to 72 hours. The holding temperature may be room temperature, for example, 10 to 50°C. The positive electrode 9a and the negative electrode 9b may be at least partially immersed in the first water 8a and the second water 8b, respectively, or may be entirely immersed.
[0052] <Method of manufacturing the radiation detecting liquid> The method for producing a radiation detecting liquid of this embodiment includes dissolving metallic tungsten in an aqueous hydrogen peroxide solution to prepare a tungsten-containing solution, preparing an iron-containing solution containing iron ions, mixing the tungsten-containing solution and the iron-containing solution, and irradiating the resulting mixed liquid with light. The tungsten-containing solution and the iron-containing solution may each be the same as those described above. This makes it possible to obtain a radiation detecting liquid that is colorless and transparent and has a clear degree of coloring in response to radiation. The mechanism by which the radiation detecting liquid is generated by mixing the tungsten-containing solution and the iron-containing solution and irradiating the resulting mixed liquid with light will be described below. Note that the mechanism by which the radiation detecting liquid is generated is not limited to the following mechanism.
[0053] As mentioned above, the tungsten-containing solution contains tungstate ions (WO4) generated by the above reaction formula (5). 2+ The iron-containing solution may contain iron ions (Fe 2+ When a tungsten-containing solution and an iron-containing solution are mixed and irradiated with light, the hydroxyl radical OH is generated by the hydrogen peroxide decomposition reaction (Fenton reaction) in the tungsten-containing solution, as shown in the following reaction formula (13). Then, as shown in the following reaction formula (14), tungstate ions WO4 2+ , hydroxyl radical OH and iron ion Fe 2+The reaction produces tungsten oxide carrying iron ions, WO3 (Fe 2+ ) is generated. H2O2+hν→2·OH (13) 2WO4 2+ +2·OH+2Fe 2+ →2WO3(Fe 2+ ) + O2 + 2OH - (14)
[0054] The iron ion-loaded tungsten oxide WO3(Fe 2+ ) is dispersed as fine particles in the radiation detecting liquid and exhibits chromicity to radiation in substantially the same manner as tungsten oxide (WO3).
[0055] The mixing ratio of the tungsten-containing solution and the iron-containing solution when preparing the radiation detecting liquid is not particularly limited. The content of the tungsten-containing solution when the total amount of the tungsten-containing solution and the iron-containing solution is taken as 100.0 mass %, is the ratio of the iron ion-supported tungsten oxide WO3 (Fe 2+ From the viewpoint of dispersibility of the component (I) and colorability upon irradiation with radiation, the content is preferably 1.0 to 50.0 mass%, more preferably 2.0 to 40.0 mass%, and even more preferably 3.0 to 30.0 mass%, and from the viewpoint of colorability, the content is still more preferably 20.0 to 30.0 mass%.
[0056] The light used in the light irradiation step after mixing the tungsten-containing solution and the iron-containing solution preferably has a wavelength of less than 400 nm at which the intensity in the spectrum is maximum. The spectrum of light may be rephrased as the spectral radiant distribution of light, and the intensity may be rephrased as the spectral irradiance or spectral irradiance. The unit of the spectral irradiance (intensity) of light is, for example, W·m -2 nm -1 By adjusting the wavelength of light irradiated onto the mixed solution of the tungsten-containing solution and the iron-containing solution in the wavelength region of less than 400 nm, the Fenton reaction shown in the above reaction formula (13) is promoted. The light used in the light irradiation step has a wavelength at which the intensity is maximum preferably less than 400 nm, and more preferably 380 nm or less. The light has a wavelength at which the intensity is maximum preferably 200 nm or more, and more preferably 300 nm or more. The light preferably has a wavelength at which the intensity is maximum in the ultraviolet region. The light used in the light irradiation process has an intensity of 10 to 500 W·m at a position 20 cm away from the light source. -2 nm -1 is preferable, and 100 to 300 W m -2 nm -1 is more preferred.
[0057] The light source for irradiating the mixed solution of the tungsten-containing solution and the iron-containing solution is not particularly limited as long as it can irradiate the above-mentioned light. The light source may be, for example, the sun, an LED, a xenon lamp, a mercury lamp, a fluorescent lamp, a UV lamp, etc.
[0058] The time for which the mixed solution of the tungsten-containing solution and the iron-containing solution is irradiated with light is not particularly limited, and can be appropriately adjusted depending on the volume of the radiation detecting liquid to be prepared, the content of the tungsten solution, etc. The time for which the mixed solution of the tungsten-containing solution and the iron-containing solution is irradiated with light may be, for example, 30 minutes to 100 hours.
[0059] The particle diameter of the tungsten oxide particles in the radiation detecting liquid is preferably 1.0 μm or less when the accumulated volume of the tungsten oxide particles in the radiation detecting liquid is 50.0%. When the particle diameter of the tungsten oxide particles is within the above range, the dispersibility of the tungsten oxide particles in the radiation detecting liquid is improved. Furthermore, the transparency of the radiation detecting liquid is improved, so that the color change upon irradiation with radiation can be clearly grasped. The particle size of the tungsten oxide particles in the radiation detecting liquid when the accumulated volume thereof is 50.0% is preferably 0.02 to 1.0 μm, and more preferably 0.05 to 0.5 μm.
[0060] The particle size when the accumulated volume of the tungsten oxide particles is 50.0% can be measured by a laser diffraction particle size distribution analyzer. The particle size of the tungsten oxide particles can be measured by using a radiation detection liquid containing tungsten oxide particles as a sample. For example, the laser diffraction particle size distribution analyzer can be the "LS 13 320 type laser scattering diffraction particle size distribution analyzer" (product name) manufactured by Beckman Coulter.
[0061] The tungsten oxide particles preferably have an average particle size of 0.02 to 1.0 μm, more preferably 0.05 to 0.5 μm, as determined by image observation. The average particle size from image observation can be calculated by measuring the maximum diameter of all particles observed in a measurement area of about 2 μm x 2 μm and taking the average value. A transmission electron microscope can be used for image observation. The sample can be prepared by applying a radiation-detecting liquid containing tungsten oxide particles to a mesh dedicated to the transmission electron microscope and drying it.
[0062] The shape of the tungsten oxide particles is not particularly limited, and may be substantially spherical, flat, block-like, plate-like, scale-like, etc. From the viewpoint of dispersibility of the tungsten oxide particles in the radiation detecting liquid, substantially spherical, flat, or plate-like is preferred.
[0063] The elemental concentration of tungsten in the radiation detecting liquid is preferably higher than the elemental concentration of iron. This improves the effect of supporting iron ions on the tungsten oxide particles, and a radiation detecting liquid having excellent dispersibility and radiation detection ability is obtained. When the total amount of the elemental concentrations of tungsten and iron in the radiation detecting liquid is taken as 100.0 mass%, the content of the elemental iron is preferably 0.1 to 20.0 mass%, more preferably 0.3 to 15.0 mass%, and even more preferably 0.5 to 10.0 mass%. From the viewpoint of coloring upon irradiation with radiation, the content of the elemental iron is preferably 5.0 mass% or less, and more preferably 2.0 mass% or less.
[0064] The elemental concentration of tungsten in the radiation detecting liquid may be, for example, 1 to 1000 ppm, 10 to 500 ppm, or 100 to 200 ppm. From the viewpoint of coloring upon irradiation with radiation, the elemental concentration of tungsten is preferably 200 ppm or more. The iron element concentration in the radiation detecting liquid may be, for example, 0.1 to 50 ppm, 0.5 to 10 ppm, or 1 to 5 ppm. Within this range, the tungsten oxide particles can be finely dispersed by the light irradiation step, and the coloring property upon radiation irradiation can be further improved.
[0065] The elemental concentrations of tungsten and iron in the radiation detecting liquid can be measured, for example, by inductively coupled plasma-atomic emission spectrometry (ICP-AES).
[0066] The method for producing a radiation detecting liquid may further include storing the radiation detecting liquid in a dark place after the light irradiation step. By passing through this step, a more colorless and transparent radiation detecting liquid can be obtained. The time for storing in a dark place is not particularly limited, but may be from 10 minutes to 72 hours.
[0067] <Other ingredients> The radiation detecting liquid may further contain other components in addition to the components mentioned above, such as a solvent other than water, a resin, a plasticizer, a dispersant, a surfactant, a thickener, a gelling agent, an inorganic binder, etc.
[0068] <How to detect radiation> The radiation detection method of the present embodiment includes preparing a radiation detecting liquid containing tungsten oxide particles and iron ions, and detecting radiation based on a color change of the radiation detecting liquid when the radiation detecting liquid is irradiated with radiation. The details of the radiation detecting liquid that can be used are as described above, and the radiation detecting liquid can be produced by the method described above. According to this radiation detection method, a container containing a radiation detecting liquid is placed at a detection position, and radiation can be detected by a color change of the radiation detecting liquid. The radiation detecting liquid is colorless and transparent when not irradiated with radiation, and changes color when irradiated with radiation. Furthermore, when irradiation of radiation is stopped after irradiation, the radiation detecting liquid changes color to colorless and transparent. This makes it possible to detect the presence or absence of radiation at the detection position. When irradiated with radiation, the radiation detecting liquid changes color from light blue to dark blue due to the coloring of the tungsten oxide particles. The intensity of the color changes depending on the composition of the radiation detecting liquid and the intensity of the irradiated radiation, etc.
[0069] The radiation detection method can be carried out using a radiation detection device including a container and a radiation detecting liquid contained in the container. One embodiment of the radiation detection device is shown in FIG. The radiation detecting device shown in Fig. 1 includes a container 2 and a radiation detecting liquid 1 contained in the container 2. As shown in Fig. 1, the radiation detecting device may include an openable and closable lid 3, allowing the inside of the container 2 to be open to the atmosphere. In a radiation detecting method, this radiation detecting device is placed at a detection position, and when radiation E is irradiated, the radiation detecting liquid 1 is irradiated with the radiation E through a side wall of the container 2, and the radiation detecting liquid 1 changes color, for example to deep blue, due to the action of tungsten oxide particles and iron ions contained in the radiation detecting liquid 1, making it possible to detect the presence or absence of radiation E.
[0070] The radiation detection method of the present embodiment can detect ionizing radiation, and can detect ultraviolet radiation from among non-ionizing radiation. Examples of ionizing radiation include α-rays, β-rays, neutron rays, X-rays, and γ-rays. The radiation detection method can detect at least one type of radiation selected from the group consisting of X-rays, γ-rays, α-rays, β-rays, and ultraviolet radiation. The radiation detection method is suitable for detecting radiation whose intensity is maximum at a wavelength of less than 400 nm in the light spectrum. Examples of radiation whose intensity is maximum at a wavelength of less than 400 nm in the light spectrum include electromagnetic waves such as ultraviolet rays, X-rays, and γ-rays. Although ultraviolet rays, X-rays, and γ-rays have a weaker ionizing effect than α-rays and β-rays, they have a long transmission distance and cannot be observed by the naked eye, so it is desired to detect them easily in a wide range. Note that ultraviolet rays are light in the wavelength range of 1 to 400 nm, but they exhibit ionizing effects at shorter wavelengths, so they are sometimes treated as equivalent to ionizing radiation. The radiation detection method of the present embodiment is capable of detecting radiation whose intensity is maximum at a wavelength of less than 400 nm, and therefore can selectively detect light exhibiting these ionizing actions. The radiation detection method of the present embodiment is capable of detecting a single type of radiation, and is also capable of detecting a combination of multiple types of radiation.
[0071] The container containing the radiation detecting liquid is preferably placed at a location where it is desired to detect the presence or absence of radiation. For example, it may be a location near a facility, device, etc. that uses radiation and where there is a possibility of radiation exposure. When the location where radiation is irradiated is more or less fixed, the distance from the radiation source (light source in the case of ultraviolet radiation) to the container is not particularly limited and may be adjusted as appropriate depending on the type of radiation, the purpose of measurement, etc.
[0072] There is no limitation on the material of the container as long as it does not prevent the radiation to be detected from being inserted into the radiation detecting liquid. The material of the container can be selected from, for example, borosilicate glass, quartz glass, polyethylene, Teflon (registered trademark), etc. Also, a shielding material may be placed around the container depending on the type of radiation to be measured. For example, when it is desired to detect X-rays, gamma rays, and neutrons as radiation, it is possible to prevent alpha rays and beta rays from being irradiated to the radiation detecting liquid by placing a sheet or plate containing a light metal such as aluminum around the container. Also, when it is desired to detect radiation while excluding the influence of ultraviolet rays as radiation, it is possible to selectively detect radiation other than ultraviolet rays by using a container coated with an ultraviolet ray shielding agent, a container made of ultraviolet ray cut glass, etc.
[0073] As described above, when the radiation detection liquid becomes colored by irradiation, the tungsten ion quotient changes as shown in reaction formula (4) above, and the liquid returns to colorless and transparent when the irradiation is stopped. The oxygen in reaction formula (4) above is either dissolved oxygen in the radiation detection liquid or oxygen supplied from the outside. When the dissolved oxygen level in the radiation detection liquid is low, as shown in Figure 1, opening and closing the lid 3 provided on the container 2 allows outside air to be introduced into the container 2, making it possible to supply oxygen from the outside.
[0074] <Other methods of detecting radiation> A radiation detection method according to another aspect of this embodiment includes preparing a support to which a radiation detecting liquid containing tungsten oxide particles and iron ions has been applied, and detecting radiation based on a color change of the support when the support is irradiated with radiation. The details of the radiation detecting liquid that can be used are as described above, and the radiation detecting liquid can be produced by the method described above. According to this radiation detection method, a support to which a radiation detecting liquid has been applied is placed at a detection position, and radiation can be detected by a color change of the support. When not irradiated with radiation, the support has the color of the support itself, and when irradiated with radiation, the color changes to dark blue. Furthermore, when irradiation with radiation is stopped after irradiation, the radiation detecting liquid changes color from dark blue to the color of the support itself. This makes it possible to detect the presence or absence of radiation at the detection position. The intensity of the color change of the support varies depending on the composition of the radiation detecting liquid, the intensity of the irradiated radiation, the type of support, etc., and is observed to be, for example, light blue to dark blue.
[0075] The color of the support is not particularly limited, but from the viewpoint of detecting the degree of deep blue color of the radiation detecting liquid, it is preferably colorless, transparent, or white.
[0076] The material of the support is not particularly limited and may be appropriately adjusted depending on the type of radiation, the purpose of the measurement, etc. The material of the support may be a porous material, a dense body, etc., and can be selected from, for example, fibrous materials such as cloth and paper, plastics, glass, ceramics, metals, etc.
[0077] There is no particular limitation on the method for applying the radiation detecting liquid to the support. For example, the radiation detecting liquid may be impregnated into a porous material such as cloth or paper, or the radiation detecting liquid may be made into a paste form and applied or printed onto a dense body such as plastic or glass. Alternatively, a structure in which the radiation detecting liquid is sandwiched between transparent plates such as glass and then bonded together may be used.
[0078] This radiation detection method can be carried out using a radiation detection device comprising a support to which a radiation detecting liquid has been applied. One example of a radiation detection device can comprise a support, and tungsten oxide and iron ions supported on the support. When a porous material is used as the support, it is preferable that tungsten oxide and iron ions are supported on the pore surfaces of the porous material. Tungsten oxide and iron ions may be supported on a dense support. The tungsten oxide and iron ions supported on this support preferably have a hydrate structure. This can further improve the responsiveness of the support to return to its original color when radiation irradiation is stopped due to dissolved oxygen or oxygen taken in from the outside. Another example of the radiation detection device may include a support and a radiation detection layer formed on the support and containing tungsten oxide particles and iron ions. When a dense body is used as the support, the radiation detection layer is preferably coated or printed on the support. This radiation detection layer preferably contains water together with tungsten oxide and iron ions. This radiation detection layer may contain a material having water retention properties such as agar in order to retain water. In addition, this radiation detection layer may contain a binder resin or the like to further increase adhesion to the support. This allows the radiation detection layer to contain dissolved oxygen, and the responsiveness of the support returning to its original color when radiation irradiation is stopped can be further increased. In the above-mentioned radiation detection device, it is preferable that the surface of the support to which the radiation detection liquid is applied is exposed to the surface to be irradiated with radiation. This allows the surface to be directly irradiated with radiation, thereby further enhancing the coloring reactivity of the tungsten oxide particles. In this configuration, radiation with low transmittance, such as α-rays and β-rays, can be detected with high sensitivity. A support may be further formed on the application surface to which the radiation detecting liquid has been applied. This makes it possible to hold the radiation detecting liquid between the pair of supports, and the state in which the radiation detecting liquid has been applied to the support can be maintained even when the support has a high moisture content. This configuration is useful for applications in which the responsiveness of the support to return to its original color when radiation irradiation is stopped and the color change occurs is improved.
[0079] An example of a radiation detection device according to another embodiment is shown in FIG. The radiation detecting device shown in Fig. 2 comprises a plate-shaped support 4 and a radiation detecting liquid applicator 5 formed on at least one surface of the support 4. The radiation detecting liquid applicator 5 is a portion to which the radiation detecting liquid is applied. In a radiation detection method, this radiation detecting device is placed at a detection position, and when radiation E is applied, the radiation detecting liquid applicator 5 of the support 4 is irradiated with radiation E, and the radiation detecting liquid applicator 5 changes color to, for example, deep blue due to the action of tungsten oxide particles and iron ions contained in the radiation detecting liquid applicator 5, making it possible to detect the presence or absence of radiation E.
[0080] The support to which radiation has been applied is preferably in a dry state, for example, the support to which radiation has been applied is preferably in a state in which moisture has been removed by drying. The reason why coloring due to radiation exposure and decolorization due to the cessation of irradiation occur even in a state in which moisture has been removed from the support can be considered as follows. That is, the iron ion-supported tungsten oxide WO3 (Fe 2+ ) is partially hydrated, and WO3(Fe 2+ )·nH2O, and the valence state of the tungsten ion can be reversibly changed by utilizing the water in the hydrate.
[0081] The method for producing a support to which radiation has been applied can include preparing a radiation detecting liquid as described above, applying the radiation detecting liquid to a support, and drying the support to remove moisture. The method for applying the radiation detecting liquid to a support is as described above. By drying the support in the drying step, the support can contain water in the form of a hydrate together with tungsten oxide particles and iron ions. The drying conditions for the support may be set according to the material and shape of the support, and are not particularly limited, but may be, for example, at 30 to 100°C for 10 minutes to 10 hours. Preferably, the drying is performed at 40 to 60°C for 10 to 60 minutes. EXAMPLES
[0082] The contents of the present disclosure will be described in more detail below using examples and comparative examples, but the present disclosure is not limited to the following examples. Unless otherwise specified, the same components and measuring devices are used throughout the examples.
[0083] <Example 1> (a) Preparation of radiation detection liquid 50 ml of 10.0 mass % hydrogen peroxide solution was placed in a glass container, to which 1.0 g of metallic tungsten particles (manufactured by FUJIFILM Wako Pure Chemical Industries, Ltd., particle size 0.7 μm, purity 99.95%) was added, and the mixture was stirred at 25° C. for 24 hours to dissolve the tungsten, producing a colorless, transparent tungsten-containing solution. A plate of 40 mm x 10 mm x 0.5 mm was cut out from iron with a purity of 99.5% by mass, and as shown in FIG. 5, the entire surface of the iron plate from the center to the half side was painted with an oil-based marking pen and then dried at room temperature to form a conductive film, which was used as a positive electrode / negative electrode electrical connector. The part on which the conductive film was formed became the negative electrode, and the part on which the conductive film was not formed became the positive electrode. Next, pure water was placed in a glass container, and the positive electrode / negative electrode electrical connector was immersed in the pure water. Then, as shown in FIG. 4, the water on the positive electrode side and the water on the negative electrode side were separated by an acrylic plate processed so that the positive electrode / negative electrode electrical connector could be penetrated. The dimensions of the acrylic plate were the same as the inner dimensions of the container. In this state, it was left to stand for 48 hours, and the water that had been in contact with the positive electrode was collected and used as an iron-containing solution. 18 ml of the iron-containing solution was placed in a glass container, and 2 ml of the tungsten-containing solution was added thereto. The entire glass container was then irradiated with ultraviolet light for 72 hours while stirring at a temperature of 25°C. In the light irradiation process, a UV lamp (manufactured by UVP, "B-100AP" (product name)) was used as the light source. The light output was 100 W. The light spectrum was measured with a spectroradiometer (manufactured by Gentec-EO, "SOLO 2" (product name)). As a result, the wavelength with the maximum intensity in the spectrum of the light emitted from the UV lamp was approximately 365 nm. The light intensity at the light irradiation position 20 cm away from the light source was 100 W / m 2After the 72-hour light irradiation step, the light irradiation was stopped and the solution was allowed to stand in a dark place for 12 hours to obtain a colorless and transparent radiation detection liquid. The elemental concentrations of tungsten and iron in the radiation detection liquid were measured by inductively coupled plasma atomic emission spectrometry (ICP-AES). Thermo Fisher Scientific's "iCAP 6300 Duo" (product name) was used for the ICP-AES analysis. The elemental concentrations of tungsten and iron in the radiation detection liquid were 100 ppm and 2.5 ppm, respectively, and the elemental concentration of tungsten was higher than the elemental concentration of iron.
[0084] (b) Radiation exposure experiment The radiation detection liquid obtained above was irradiated with gamma rays, and the color change of the radiation detection liquid was investigated. Specifically, 10 ml of the radiation detection liquid was placed in a transparent quartz cell and sealed, and cobalt 60 ( 60 The cell was irradiated with gamma rays from a γ-ray source of 10000 Cr (Co) for 2 hours. The distance between the radiation source and the quartz cell was 5 cm. After gamma irradiation, the radiation detection liquid was found to have turned deep blue. 60 minutes after gamma irradiation was stopped, the color of the radiation detection liquid returned to colorless and transparent.
[0085] <Example 2> In Example 2, a radiation detecting liquid was prepared in the same manner as in Example 1. Next, an irradiation experiment was carried out using X-rays as radiation. Specifically, 10 ml of the radiation detecting liquid was placed in a transparent quartz cell, which was then sealed, and X-rays using aluminum-magnesium as the radiation source were irradiated for one hour. The distance from the radiation source to the quartz cell was 10 cm. After the X-ray irradiation, the radiation detecting liquid was found to have turned dark blue. In addition, 30 minutes after the X-ray irradiation was stopped, the color of the radiation detecting liquid returned to colorless and transparent.
[0086] <Example 3> In Example 3, a radiation detecting liquid was prepared in the same manner as in Example 1. Next, an irradiation experiment was carried out using α-rays as radiation. Specifically, 10 ml of the radiation detecting liquid was placed in a quartz cell and sealed, and α-rays (He + ) to 3.0×10 13 ions / cm 2The quartz cell was irradiated with α-rays at a distance of 10 cm from the radiation source. After the α-ray irradiation, the radiation detection liquid was found to have turned deep blue. After 60 minutes from the end of the α-ray irradiation, the color of the radiation detection liquid returned to colorless and transparent.
[0087] <Example 4> In Example 4, a radiation detecting liquid was prepared in the same manner as in Example 1. Next, an irradiation experiment was carried out using β-rays as radiation. Specifically, 10 ml of the radiation detecting liquid was placed in a quartz cell, which was then sealed, and β-rays were irradiated for 5 minutes using an electron gun. The distance from the radiation source to the quartz cell was set to 5 cm. After the β-ray irradiation, the radiation detecting liquid was found to have turned dark blue. In addition, 60 minutes after the β-ray irradiation was stopped, the color of the radiation detecting liquid returned to colorless and transparent.
[0088] <Example 5> In Example 5, a radiation detecting liquid was prepared in the same manner as in Example 1. Next, an irradiation experiment was carried out using ultraviolet light as radiation. Specifically, 10 ml of the radiation detecting liquid was placed in a glass container, and the container was not sealed. The container was irradiated with ultraviolet light for 30 minutes using the UV lamp used in Example 1. That is, in the spectrum of light emitted from the UV lamp, the wavelength at which the intensity is maximum is approximately 365 nm, and the light intensity at the light irradiation position 20 cm away from the light source is 100 W / m 2 The distance between the UV lamp (light source) and the glass container was 10 cm. The radiation detection liquid turned blue within 10 minutes of being irradiated with UV light, and turned dark blue after 30 minutes. In addition, 60 minutes after the UV irradiation was stopped, the color of the radiation detection liquid returned to colorless and transparent.
[0089] <Example 6> In Example 6, a radiation detecting liquid was prepared in the same manner as in Example 5, except for the following points, and a radiation irradiation experiment was carried out. In Example 6, a monochrome filter was installed on the UV lamp (light source) in the irradiation experiment, and the wavelength of the ultraviolet light was changed. Specifically, the wavelength at which the intensity was maximum in the spectrum of the light emitted from the UV lamp was changed to about 400 nm. The radiation detecting liquid turned light blue within 10 minutes of ultraviolet light irradiation, and turned blue after 30 minutes. The degree of coloration was lower than in Example 5. In addition, 60 minutes after ultraviolet light irradiation was stopped, the color of the radiation detecting liquid returned to colorless and transparent.
[0090] <Example 7> In Example 7, a radiation detecting liquid was prepared in the same manner as in Example 5, except for the following points, and a radiation irradiation experiment was performed. In Example 7, the volume of the iron-containing solution was changed from 18 ml to 16 ml, and the volume of the tungsten-containing solution was changed from 2 ml to 4 ml. The elemental concentrations of tungsten and iron in the radiation detecting liquid measured by ICP-AES analysis were 200 ppm and 2.2 ppm, respectively, and the elemental concentration of tungsten was higher than the elemental concentration of iron. The radiation detecting liquid turned dark blue within 10 minutes of ultraviolet irradiation, and further turned dark blue after 30 minutes. The degree of coloring was higher than that of Example 5. In addition, 60 minutes after the ultraviolet irradiation was stopped, the color of the radiation detecting liquid returned to colorless and transparent.
[0091] <Example 8> In Example 8, a radiation detecting liquid was prepared in the same manner as in Example 5, except for the following points, and a radiation irradiation experiment was performed. In Example 8, agar was added to the radiation detecting liquid. Specifically, 8 ml of the same radiation detecting liquid as in Example 1 was placed in a glass container, 0.3 g of agar was added thereto, and dissolved while stirring. Thereafter, the agar-containing radiation detecting liquid was sandwiched and fixed using two transparent glass plates (glass size: 40 mm x 20 mm x 1 mm). When the radiation detecting liquid was irradiated with ultraviolet light under the same conditions as in Example 5, it turned blue within 10 minutes, and turned dark blue after 30 minutes. This was equivalent to Example 5. In addition, 10 minutes after the ultraviolet light irradiation was stopped, the color of the radiation detecting liquid returned to colorless and transparent. From this, it was found that the dissolving of the colored radiation detecting liquid proceeded due to the oxygen dissolved in the radiation detecting liquid, even without supplying oxygen from the outside.
[0092] <Example 9> In Example 9, a radiation detecting liquid was prepared in the same manner as in Example 5, except for the following points, and a radiation irradiation experiment was performed. In Example 9, as shown in FIG. 2, a radiation irradiation experiment was performed using a support to which a radiation detecting liquid was applied. 20 μl of the same radiation detecting liquid as in Example 1 was impregnated into an experimental filter paper having a diameter of 4 cm, and then the filter paper was dried at a temperature of 50° C. for 10 minutes to remove the moisture in the radiation detecting liquid by evaporation. The part of the filter paper as the support impregnated with the radiation detecting liquid turned light blue within 10 seconds when irradiated with ultraviolet light under the same conditions as in Example 5. The degree of coloring was the same as in Example 5. In addition, 24 hours after the ultraviolet light irradiation was stopped, the color of the filter paper returned to its original white color. From this, even when the filter paper was impregnated with the radiation detecting liquid and was in a dried state, the coloring and decolorization behavior of the radiation detecting liquid could be confirmed. On the other hand, it was found that the decolorization reaction rate decreased with a decrease in the moisture content.
[0093] <Comparative Example 1> In Comparative Example 1, a radiation detecting liquid was prepared in the same manner as in Example 5, except for the following points, and a radiation irradiation experiment was performed. In Comparative Example 1, a radiation detecting liquid was prepared by irradiating a tungsten-containing solution with ultraviolet light without using an iron-containing solution. Tungsten oxide particles of about 5 μm were dispersed in the radiation detecting liquid, and it was light brown in color. Furthermore, even when irradiated with ultraviolet light for 30 minutes or more in this state, it did not become colored. It is considered that the growth of tungsten oxide particles was promoted and the chromic reaction of tungsten oxide was inhibited because the radiation detecting liquid did not contain iron ions. [Explanation of symbols]
[0094] 1 Radiation detection liquid, 2 Container, 3 Lid, 4 Support, 5 Liquid application section, 6 Container, 7 Partition material, 8a First water, 8b Second water, 9a Positive electrode, 9b Negative electrode, 10 Conductive film, E Radiation
Claims
1. A method for detecting radiation, comprising: preparing a radiation detecting liquid containing tungsten oxide particles and iron ions; and detecting radiation based on a color change of the radiation detecting liquid when radiation is irradiated to the radiation detecting liquid.
2. A method for detecting radiation, comprising: preparing a support to which a radiation detecting liquid containing tungsten oxide particles and iron ions has been applied; and detecting radiation based on a color change of the support when radiation is irradiated to the support.
3. The method for detecting radiation according to claim 2 , wherein the support is dry.
4. 4. The radiation detection method according to claim 1, wherein the tungsten oxide particles have a particle diameter of 1.0 μm or less when their accumulated volume is 50.0%.
5. 5. The radiation detection method according to claim 1, wherein a concentration of tungsten in the radiation detecting liquid is higher than a concentration of iron in the radiation detecting liquid.
6. 6. The radiation detection method according to claim 1, wherein at least one type of radiation selected from the group consisting of X-rays, gamma rays, alpha rays, beta rays, and ultraviolet rays is detected.
7. 7. A method for producing a radiation detecting liquid used in the radiation detection method according to any one of claims 1 to 6, comprising: dissolving metallic tungsten in an aqueous hydrogen peroxide solution to prepare a tungsten-containing solution; preparing an iron-containing solution containing iron ions; mixing the tungsten-containing solution with the iron-containing solution; and irradiating the obtained mixed solution with light.
8. 8. The method for producing a radiation detecting liquid according to claim 7, wherein preparing the iron-containing solution includes extracting at least a portion of acidic water obtained by contacting the positive electrode in a configuration in which the first water and the second water are separated from each other and the iron-containing positive electrode and the iron-containing negative electrode are electrically connected to each other, with at least a portion of the positive electrode being immersed in the first water and at least a portion of the negative electrode being immersed in the second water.
9. 9. The method for producing a radiation detecting liquid according to claim 7 or 8, wherein the light irradiated to the mixed solution has a wavelength at which the intensity is maximum in the light spectrum of less than 400 nm.
10. 10. A method for producing a support used in the radiation detection method according to claim 2, comprising: preparing a radiation detecting liquid according to the method according to any one of claims 7 to 9; applying the radiation detecting liquid to a support; and drying the support to remove moisture.
11. A radiation detection device for use in the radiation detection method according to claim 1 , comprising: a container; and the radiation detecting liquid contained in the container.
12. The radiation detection device according to claim 11 , wherein the container further comprises an openable and closable lid.
13. 3. A radiation detection device for use in the radiation detection method according to claim 2, comprising a support on which the radiation detection liquid is applied.
14. The radiation sensing device of claim 13 , wherein the support is dry.
15. 3. A radiation detection device for use in the radiation detection method according to claim 2, comprising a support, and tungsten oxide particles and iron ions supported on the support.
16. 3. A radiation detection device for use in the radiation detection method according to claim 2, comprising: a support; and a radiation detection layer formed on the support and containing tungsten oxide particles and iron ions.
Citation Information
Patent Citations
Radiation dosimeter
JP1987293178A
X-ray image detection apparatus
JP1999352230A
Rapid determination of unknown absorbed radiation dose with high sensitivity using optically stimulated luminescence
JP2000503396A
METHOD FOR IMPROVING RADIATION RESPONSIBILITY OF RADIATION SENSING MATERIAL
JP2000503759A
Photovoltaic ultraviolet sensor
JP2007201393A