Testing method for crystallinity in amorphous pharmaceutical compositions

UV/visible spectroscopy with a predictive model and in-line testing apparatus addresses the challenge of determining crystallinity in amorphous pharmaceutical compositions, enhancing manufacturing efficiency and quality control.

JP7557473B2Active Publication Date: 2024-09-27コルビステック アクチェンゲゼルシャフト
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2021545977
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-02-05
Filing Date
2020-01-29
Publication Date
2024-09-27
Estimated Expiration
2040-01-29

AI Technical Summary

Technical Problem

Existing methods for determining the crystallinity of amorphous pharmaceutical compositions are time-consuming and not suitable for real-time monitoring in manufacturing processes, posing challenges in ensuring compliance with regulatory standards and product quality.

Method used

A method using UV/visible spectroscopy to create a predictive model for crystallinity detection, involving the measurement of reflectance and/or transmission spectra to quantify the amount of crystallinity in amorphous solid dispersions, combined with an apparatus for in-line testing and adjustment of manufacturing parameters.

Benefits of technology

Enables rapid, cost-effective detection of crystallinity in amorphous pharmaceutical compositions, improving manufacturing efficiency and ensuring high-quality products meet regulatory standards by allowing real-time adjustments in the production process.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007557473000005
    Figure 0007557473000005
  • Figure 0007557473000013
    Figure 0007557473000013
  • Figure 0007557473000011
    Figure 0007557473000011
Patent Text Reader

Abstract

A method is provided for testing a pharmaceutical composition for the presence or absence of crystallinity of an active pharmaceutical ingredient (API) in an amorphous solid dispersion or solid-state solution using a UV / Vis spectrometer. The testing can be performed alone or during the manufacture of the pharmaceutical composition. A predictive model provides a quantitative analysis of the amount of crystalline API based on the UV / Vis data of a corresponding reference sample. An apparatus for manufacturing the pharmaceutical composition is also provided.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001]

[0001] This application claims priority from GB1901579.1, filed on February 5, 2019, the content and elements of which are incorporated herein by reference for all purposes.

[0002] Field of Disclosure

[0003] The present invention relates to the presence of crystallinity in normally amorphous pharmaceutical compositions. In particular, the present invention relates to a method for detecting and optionally quantifying the degree of crystallinity in normally amorphous pharmaceutical compositions. [Background technology]

[0002]

[0004] background

[0005] Products manufactured in the pharmaceutical industry are required to meet very strict quality standards. This is because the adverse effects of substandard pharmaceuticals pose a widespread threat to public safety. In the past, the incidence of substandard pharmaceutical compositions reaching the market was high. In an attempt to reduce the incidence of substandard pharmaceutical compositions reaching the market, the pharmaceutical industry is aware of widespread and ever-increasing regulatory demands.

[0003]

[0006] Pharmaceutical companies often have dedicated quality control departments to ensure that their pharmaceutical compositions meet relevant regulatory standards. Meeting regulatory standards entails a large financial burden due to the time, personnel, and equipment required. It would be desirable to reduce the amount of time and money required to meet regulatory standards without compromising quality.

[0004]

[0007] Process Analytical Technology (PAT) is used to effectively design and control pharmaceutical manufacturing processes by monitoring specific quality indicators and parameters. The pharmaceutical industry is evolving and there is regulatory pressure to switch from batch-based manufacturing to continuous manufacturing. PAT is particularly relevant to the emerging continuous manufacturing methods.

[0005]

[0008] There are several factors that are evaluated in the quality control of pharmaceutical compositions. One of these factors is the physical form. Active pharmaceutical ingredients (APIs) can exist in a variety of different solid forms, including polymorphs, solvates, hydrates, salts, cocrystals, and amorphous solids. Each form exhibits unique physicochemical properties that can significantly affect bioavailability, manufacturability, purification, stability, and other characteristics.

[0006]

[0009] Crystallinity, especially crystalline polymorphism, can have a significant impact on the solubility, bioavailability, and stability of many APIs. By co-formulating small molecule APIs with water-soluble polymers, significant enhancement of drug absorption kinetics and overall bioavailability is observed.

[0007]

[0010] Therefore, there is great interest in producing "amorphous solid dispersions" of APIs, whereby crystalline material is "dissolved", i.e., molecularly dispersed, by incorporation into a molten polymer phase and is no longer crystalline, and therefore becomes amorphous.

[0008]

[0011] Efficient mixing and sufficient mechanical energy are necessary to produce a properly dispersed amorphous product, however, it is not easy to determine the degree of dissolution / dispersion, especially in an on-line situation.

[0009]

[0012] Typically, to determine the level of residual crystalline material present in a solid sample, it is necessary to first mill the solid into a homogenous powder and then analyze it with a powder X-ray diffractometer. Powder XRD is not a rapid process, it is performed offline and typically takes 15 minutes to an hour to produce results.

[0010]

[0013] It is also possible to use Raman spectroscopy to measure the level of crystallinity in such solid samples. See, for example, Thiel et al., Manufacturing Amorphous Solid Dispersions with a Tailored Amount of Crystallized API for Biopharmaceutical Testing, Mol. Pharmaceutics, 2018, 15(5), pp. 1870-1877, which reports a study of crystal growth over time in fenofibrate tablets. However, Raman spectroscopy is difficult to use in in-line manufacturing conditions due to the complexities associated with laser light, laser safety, and the typically long integration times required to obtain a useful spectrum.

[0011]

[0014] In view of the above, there is a need for improved methods and apparatus for monitoring and producing high quality amorphous pharmaceutical compositions.

[0015] WO2016 / 118633 A1 describes the quantification and preparation of pharmaceutical grade cantharidin. US2008 / 0165354 A1 describes a method and apparatus for dissolving solid substances in liquids.

[0012]

[0016] The use of in-line UV / Vis spectroscopy as a high-throughput Process Analytical Technology (PAT) in the early stages of product development using hot melt extrusion is known. See Pharmaceutics 2018, 10, 166.

[0013]

[0017] The present disclosure has been devised in light of the above considerations. [Prior art documents] [Patent documents]

[0014] [Patent Document 1] WO2016 / 118633 A1 [Patent Document 2] US2008 / 0165354 A1 [Non-patent literature]

[0015] [Non-Patent Document 1] Mol. Pharmaceutics, 2018, 15(5), pp. 1870-1877 [Non-Patent Document 2] Pharmaceutics 2018, 10, 166 Summary of the Invention

[0016]

[0018] Disclosure Summary

[0019] In a first aspect of the present invention, there is provided a method of generating a predictive model for determining the amount of crystallinity of an API in an amorphous solid dispersion or solid-state solution, the method comprising the steps of: (i) subjecting a plurality of reference samples of the dispersion or solution spanning a range of amounts of crystallinity of the API to UV / Vis spectroscopy; (ii) measuring the reflectance and / or transmittance spectra of each reference sample; and (iii) processing the spectra collected in step (ii) to generate a predictive crystallinity model.

[0017]

[0020] References herein to "dispersions" and "solutions" mean "amorphous solid dispersions" and "solid state solutions", respectively.

[0021] By developing a predictive model in this manner, it is possible to determine a quantitative amount of crystallinity of an API in a dispersion or solution, such as in the method provided in the first aspect of the invention.

[0018]

[0022] In some cases, the number of reference samples is 5 or more.

[0023] Optionally, the spectrum is pre-processed prior to step (iii) to normalize and / or smooth the spectrum.

[0019]

[0024] In some cases, the spectra of reference samples are processed to derive features that correlate with crystallinity over at least a portion of said range of crystallinity.

[0025] Optionally, the features include at least a first principal component derived from a principal component analysis (PCA) of the spectra, where the variance of the first principal component with crystallinity may be substantially linear over the range of crystallinity of the plurality of dispersions or solutions; or a lightness value L in CIELAB color space derived from the spectra. * ;includes.

[0020]

[0026] In a second aspect of the present invention, there is provided a method of testing a pharmaceutical composition comprising an API in an amorphous solid dispersion or solid state solution for crystallinity of the API, comprising the steps of: (i) subjecting the dispersion or solution to UV / Visible spectroscopy; (ii) measuring the reflectance and / or transmittance spectrum; and (iii) determining the presence or absence of crystallinity of the API by comparing the measured reflectance and / or transmittance spectrum to that expected for a completely amorphous sample.

[0021]

[0027] The transmittance / absorbance and reflectance of amorphous solid dispersions or solid state solutions have been found to correlate with the crystallinity of the API. As applied herein, UV / Vis spectroscopy does not rely on the transition of electrons between orbitals. Without wishing to be bound by theory, the present invention relies on the scattering of light by API crystals present in an otherwise amorphous pharmaceutical composition. The advantage is that the detection of API crystallinity in an otherwise amorphous dispersion or solution is fast and inexpensive.

[0022]

[0028] In some cases, if crystalline API is found to be present, there is a step of determining the amount of crystallinity in the dispersion or solution by comparing the observed spectrum to a predictive model, such as a standard curve.

[0023]

[0029] Optionally, the predictive model is according to the first aspect of the invention.

[0030] In some cases, comparing the observed spectrum to the predictive model includes processing the observed spectrum in the same manner as spectra of said plurality of reference samples.

[0024]

[0031] In some cases, the amount of crystallinity in the dispersion or solution is measured at 50% by weight or less, such as 25% by weight or less, or 20% by weight or less, or 15% by weight or less.

[0032] In some cases, the amount of crystallinity in the dispersion or solution is measured as 1 weight percent or more, such as 2 weight percent or more, or 3 weight percent or more, or 5 weight percent or more.

[0025]

[0033] In a third aspect of the invention, there is provided a method for preparing a pharmaceutical composition comprising the steps of: (i) forming an API into an amorphous solid dispersion or solid state solution; (ii) testing the dispersion or solution one or more times for crystallinity of the API according to the second aspect of the invention; and (iii) if the dispersion or solution has an amount of crystallinity within an acceptable range, processing the composition into a final pharmaceutical product.

[0026]

[0034] Advantageously, testing a dispersion or solution for API crystallinity at one or more times allows for improved reliability and consistency in the manufacture of high quality pharmaceutical compositions that meet required regulatory standards, and reduces wastage of time, money, and resources due to increased manufacturing efficiency.

[0027]

[0035] In some cases, forming the API into a dispersion or solution form is performed by extrusion, ball milling, or spray drying; and / or one or more tests for the presence or absence of crystallinity of the dispersion or solution are performed in-line.

[0028]

[0036] In some cases, forming is performed by extrusion and testing is performed at one or more of the point of API injection, upstream of the point of extrusion, and at the point of extrusion.

[0037] In some cases, forming is performed by ball milling in a ball mill having one or more clearing points, and testing is performed through one or more clearing points substantially perpendicular to the axis of motion.

[0029]

[0038] In some cases, formation is performed by spray drying and testing is performed at one or more of the following: the point of API input, the point of atomization in the drying chamber, or the point of settling after atomization.

[0039] In some cases, the acceptable range of crystallinity is 1% or less by weight. The acceptable range of crystallinity may be 0.25% or less by weight, 0.5% or less by weight, 2% or less by weight, or 3% or less by weight.

[0030]

[0040] In some cases, the API input to a screw extruder, ball mill, or spray dryer is automatically adjusted, if necessary, to ensure that the crystallinity is within an acceptable range.

[0031]

[0041] In some cases, the speed of a screw extruder, ball mill, or spray dryer is automatically adjusted, if necessary, to ensure that the crystallinity is within an acceptable range.

[0032]

[0042] Optionally, the temperature of the extruder barrel or spray dryer is automatically adjusted, if necessary, to ensure that the crystallinity is within an acceptable range.

[0043] In some cases, the UV / Visible reflectance and / or transmittance is measured continuously, such as 7 times per second, 5 times per second, or 2 times per second.

[0033]

[0044] Optionally, the reflectance and / or transmittance spectrum is measured at wavelengths from 210 to 800 nm, for example from 300 to 700 nm, preferably from 315 nm to 400 nm (UVA).

[0034]

[0045] In some cases, only the reflectance spectrum is measured.

[0046] In some cases, only the transmission spectrum is measured.

[0047] In some cases, the particle size of the dispersion or solution is measured before being subjected to UV / Vis spectroscopy. Known methods for sizing a dispersion or solution include sieve analysis, direct imaging and laser diffraction. In this disclosure, a Mastersizer (Malvern Instruments) laser diffractometer was used.

[0035]

[0048] Optionally, the dispersion or solution is sized to compare to the size of one or more reference samples of known crystallinity, which compare to the API and carrier of the dispersion or solution.

[0036]

[0049] In some cases, the API is a compound with a molecular weight of 2000 g / mol or less, e.g., a small molecule drug with a molecular weight of 1000 g / mol or less. In some cases, the API is a compound with a molecular weight of 100 g / mol or more, e.g., 200 g / mol or more.

[0037]

[0050] Optionally, the API is at least 95% pure, such as at least 97% pure or at least 99% pure, prior to incorporation into said dispersion or solution.

[0051] In some cases, the API comprises 5 wt% or less water. Preferably, the API comprises 3 wt% or less water, such as 1 wt% or less water.

[0038]

[0052] Optionally, the API is a non-nucleoside reverse transcriptase inhibitor (NNRTI), preferably etravirine (ETR), or a non-steroidal anti-inflammatory drug (NSAID), preferably piroxicam (PRX). The API can be any class of orally available drug having at least one crystalline form.

[0039]

[0053] In some cases, the carrier of the dispersion or solution comprises an amorphous polymer. Of course, an amorphous solid dispersion or solid state solution comprises a carrier in which other components are dispersed or "dissolved."

[0040]

[0054] Optionally, the amorphous polymer is one or more of a cellulose polymer, a vinyl polymer, a polymethacrylate polymer, and a polyalkylene glycol polymer.

[0055] In some cases, the amorphous polymer is one or more of ethyl cellulose, hydroxyethyl cellulose, hydroxypropyl cellulose, hydroxypropyl methylcellulose (HPMC), HPMC acetate succinate (HPMCAS); polyvinyl acetate phthalate; polymethacrylate; polyalkylene glycols, such as polyethylene glycol (PEG), copolymers of PEG, polypropylene glycol (PPG), poloxamers (triblock polymers having a central hydrophobic PPG block flanked by two hydrophilic PEG blocks), soluplus (PEG-polyvinyl acetate-polyvinyl caprolactam graft copolymer (PVAc-PVCap-PEG)); polyvinylpyrrolidone (povidone), copovidone, vinylpyrrolidone-vinyl acetate copolymer, and linear random copolymers of N-vinyl-2-pyrrolidone and vinyl acetate (e.g., 60:40).

[0041]

[0056] Optionally, the amorphous spray polymer is one or more of Kollidon® VA 64, Soluplus®, Kollidon® 12 PF, Kollidon® 17 PF, Kollidon® 30, Kollidon® 90 F, Kollidon® SR, Kollicoat® MAE 100P, Kollicoat® IR, Kollicoat® Protect, Kolliphor® P407, Kolliphor® P407 micro, Kolliphor® P188, Kolliphor® P188 micro, Kolliphor® PEG grades, Kolliphor® RH 40, and Kolliphor® TPGS provided by BASF.

[0042]

[0057] In some cases, the carrier of the dispersion or solution contains 5% or less water by weight. Preferably, the dispersion or solution contains 3% or less water by weight, such as 1% or less water by weight.

[0058] Optionally, the dispersion or solution contains 5% or less water by weight. Preferably, the dispersion or solution contains 3% or less water by weight, such as 1% or less water by weight.

[0043]

[0059] In a fourth aspect of the present invention, there is provided an apparatus for forming a pharmaceutical composition as an amorphous solid dispersion or a solid state solution, said apparatus comprising a quality control system for testing the amount of crystallinity of an API in the composition by one or more UV / Visible spectrometers configured to measure reflectance and / or transmittance intensity.

[0044]

[0060] By having such an instrument, the amount of crystalline API in an amorphous solid dispersion can be determined quickly and inexpensively without the need for a separate instrument, and therefore quality control is integral to the instrument rather than a separate off-line entity.

[0045]

[0061] Optionally, the apparatus comprises a screw extruder, ball mill, or spray dryer, and the or each UV / Vis spectrometer is positioned at an in-line measurement point to measure the reflectance and / or transmittance of the dispersion or solution. By positioning the UV / Vis spectrometer in-line, the results of the reflectance and / or transmittance measurements can be used immediately to modify the extrusion parameters as needed.

[0046]

[0062] In some cases, the apparatus includes a screw extruder, and the or at least one UV / Vis spectrometer is configured to measure reflectance and / or intensity at one or more of the API injection point, upstream of the extrusion point, and at the extrusion point.

[0047]

[0063] Optionally, the apparatus includes a ball mill having one or more clearing points, and the or at least one UV / Vis spectrometer is configured to measure reflectance and / or transmittance through the one or more clearing points and is substantially perpendicular to the axis of motion.

[0048]

[0064] In some cases, the apparatus includes a spray dryer, and the or at least one UV / Vis spectrometer is configured to measure reflectance and / or transmittance at one or more of the API input point, the point of atomization within the drying chamber, and the point of settling after atomization.

[0049]

[0065] Optionally, the or each UV / Vis spectrometer is photonically connected to a probe at the or each measurement point by an optical fiber. The tip of each probe may include a sapphire window. Preferably, each optical fiber is 20m or less in length. The UV / Vis spectrometer may include a xenon flash lamp for illuminating via the optical fiber.

[0050]

[0066] In a reflection polymer melt probe (RPMP), each optical fiber can have six circumferentially positioned illumination glass fibers and a centrally positioned reflectance glass fiber. Light travels through the circumferentially positioned glass fibers to the measurement point and returns through the centrally positioned reflectance glass fiber.

[0051]

[0067] In a transmission polymer melt probe (TPMP), there are two separate units placed at a distance across the path of the solution or dispersion. One unit provides illumination while the other unit collects the light transmitted through the solution or dispersion across the path. The distance between the two units can be varied to optimize the measurement for the dispersion or solution in the path.

[0052]

[0068] Optionally, the apparatus is configured to automatically adjust API input to the screw extruder, ball mill, or spray dryer, as needed, in response to in-line measurements from the or each UV / Vis spectrometer.

[0053]

[0069] Optionally, the apparatus is configured to automatically adjust the speed of a screw extruder, ball mill, or spray dryer, if necessary, in response to in-line measurements from the or each UV / Vis spectrometer.

[0054]

[0070] In some cases, the apparatus is configured to automatically adjust the temperature of a screw extruder, ball mill, or spray dryer, if necessary, in response to in-line measurements from the or each UV / Vis spectrometer.

[0055]

[0071] In some cases, the spectrometer is configured to measure reflectance and / or transmittance intensity over a range of 210-800 nm, such as 300-700 nm or 315 nm-400 nm (UVA).

[0056]

[0072] In some cases, the or each UV / Vis spectrometer is configured to measure reflectance and / or transmittance continuously, for example, at least once per second, at least twice per second, at least five times per second, or at least seven times per second.

[0057]

[0073] Optionally, the apparatus is for use with a method according to the third aspect of the invention.

[0074] Drawing Overview

[0075] So that the invention may be understood and further aspects and features thereof may be appreciated, embodiments illustrating the principles of the invention will now be described in more detail with reference to the accompanying drawings. [Brief description of the drawings]

[0058] [Figure 1]

[0076] Figure 1 shows the UV / Visible transmission spectra of five samples of 15, 18, 20, 23, and 25 wt% PRX from 230 to 810 nm. An increase in overall absorbance is seen with increasing amounts of PRX, with a particularly large increase in overall absorbance being observed from 23% to 25% PRX. [Diagram 2]

[0077] Figure 2 shows five XRD spectra of pure solid PRX, Kollidon VA64, and 20, 25, and 30 wt% PRX mixtures obtained on a Bruker instrument. Traces of the XRD fingerprint of crystalline PRX are first observed in the 30% PRX spectrum. [Diagram 3]

[0078] FIG. 3 shows overlaid UV / Vis spectra for polymer blends of HMPC-E5 (VIVAPHARM® hydroxypropyl methylcellulose) and sodium stearoyl fumarate (SSF) with 20, 10, 5, 2.5, 1.25, and 0.625 wt % crystalline etravirine. [Figure 4]

[0079] FIG. 4 shows overlaid UV / Vis reflectance spectra for ETR dispersed in hydroxypropyl methylcellulose (HMPC-E5) with a total amount of ETR of 20 or 25 wt %. [Diagram 5]

[0080] Figure 5 shows a good correlation between L* values ​​and crystallinity for 13 unmilled ETR samples, each with a different degree of crystallinity previously determined by Raman spectroscopy obtained on a Kaiser instrument. The total amount of ETR in each sample was 25 wt%, including both amorphous and crystalline content. The unmilled samples are the direct solid monolithic form resulting from solidification after extrusion. [Figure 6]

[0081] FIG. 6 shows the reflectance UV / visible transmission spectra from 220 to 800 nm for the same 13 ETR samples as in FIG. [Figure 7]

[0082] FIG. 7 shows XRD spectra obtained on a Rigaku instrument for the same 13 ETR samples as in FIG. [Figure 8]

[0083] Figure 8 shows the UV reflectance spectra for five of the 13 ETR samples from Figure 5 that have virtually no crystallinity (<1% as measured by Raman spectroscopy). Good reliability and reproducibility of the overall spectral shape and amount of reflectance is observed between these very similar samples. [Figure 9]

[0084] Figure 9 shows a plot of the loadings (y-axis) contributing to Factor 1, the first principal component resulting from a PCA on the reflectance spectra of ETR-containing samples as described in Method 3, versus wavelength (x-axis) from 290 to 400 nm. As shown, Factor 1 provides the first eigenvector explaining the variance in the data set. [Figure 10]

[0085] FIG. 10 shows a plot of variance (y-axis) against factors (x-axis) in the PCA, showing that factors 1 and 2 explain approximately 98% and 2% of the variance in the dataset, respectively. [Figure 11]

[0086] Figure 11 shows a scatter plot of factor 1 (x-axis) versus factor 2 (y-axis) derived from the PCA analysis in method 3. As can be seen, the samples cluster according to crystallinity (i.e., samples with 2.5% crystallinity (squares), 5% crystallinity (circles), 10% crystallinity (triangles), and 20% crystallinity (diamonds)). [Figure 12]

[0087] Figure 12 shows a plot of the known (reference) crystallinity levels of the samples (x-axis) versus the predicted crystallinity by factor 1 (y-axis). The inset shows the linearity of the correlation. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0059]

[0088] Detailed Description

[0089] The features disclosed in the foregoing description, or in the following claims, or in the accompanying drawings, whether expressed in a specific form or in terms of means for performing a disclosed function, or a method or process for obtaining a disclosed result, can be utilized, as appropriate, separately or in any combination of such features to realize the invention in diverse forms thereof.

[0060]

[0090] While the present invention has been described in connection with the exemplary embodiments above, many equivalent modifications and variations will become apparent to those skilled in the art given this disclosure. Accordingly, the exemplary embodiments of the present invention described above are considered to be illustrative and not limiting. Various changes may be made to the described embodiments without departing from the scope of the present invention.

[0061]

[0091] For the avoidance of any doubt, any theoretical explanations provided herein are provided for the purpose of improving the understanding of the reader, and the inventors do not wish to be bound by any of these theoretical explanations.

[0062]

[0092] Any section headings used herein are for organizational purposes only and are not to be construed as limiting the subject matter described.

[0093] Throughout this specification, including the claims which follow, unless otherwise required by context, the words "have," "include," and "comprise," as well as variations such as "having," "include (singular)," "including," and "comprising," should be understood to mean the inclusion of a stated integer or step or group of integers or steps, but not the exclusion of any other integer or step or group of integers or steps.

[0063]

[0094] It should be noted that, as used in this specification and the appended claims, the singular forms "a," "an," and "the" include plural referents unless the context clearly dictates otherwise. Ranges can be expressed herein as from one particular value preceded by "about" and / or to another particular value preceded by "about." When such a range is expressed, another embodiment includes from the one particular value and / or to the other particular value. Similarly, when values ​​are expressed as approximations, it will be understood that the particular value forms another embodiment by using the antecedent "about." The term "about" with respect to numerical values ​​is optional and means, for example, ±10%.

[0064]

[0095] As used herein, the words "preferred" and "preferably" refer to aspects of the invention that may provide certain benefits, under some circumstances. It should be understood, however, that other aspects may also be preferred, under the same or different circumstances. Thus, the recitation of one or more preferred aspects does not mean or imply that other aspects are not useful, and is not intended to exclude other aspects from the scope of the disclosure or from the claims. The present invention includes the following inventions. [Item 1] A method for generating a predictive model for determining the amount of crystallinity of an active pharmaceutical ingredient (API) in an amorphous solid dispersion or solid-state solution, comprising: (i) subjecting a plurality of reference samples of a dispersion or solution spanning a range of API crystallinity to UV / Vis spectroscopy; (ii) measuring the reflectance and / or transmission spectrum of each reference sample; and (iii) processing the spectra collected in step (ii) to generate a predicted crystallinity model; The method comprising: [Item 2] The method according to Item 1, wherein the number of reference samples is 5 or more. [Item 3] The method according to any one of items 1 to 2, wherein the spectrum is pre-processed prior to step (iii) to normalize and / or smooth the spectrum. [Item 4] The method according to any one of items 1 to 3, further comprising processing a spectrum of a reference sample to derive features that correlate with crystallinity over at least a portion of the range of crystallinity. [Item 5] The above-mentioned features are At least a first principal component derived from a principal component analysis (PCA) of the spectra, where the variance of said first principal component with crystallinity may be substantially linear across the range of crystallinity of said plurality of dispersions or solutions; or Lightness value L in the CIELAB color space derived from the spectrum * ; The method according to item 4, comprising: [Item 6] A method for testing a pharmaceutical composition containing an API in an amorphous solid dispersion or solid-state solution for crystallinity of the API, comprising: (i) subjecting the dispersion or solution to UV / Vis spectroscopy; (ii) measuring the reflectance and / or transmittance spectrum, and (iii) determining the presence or absence of crystallinity of the API by comparing the measured reflectance and / or transmittance spectra with that expected for a completely amorphous sample; The method comprising: [Item 7] Furthermore, (iv) if crystalline API is found to be present, determining the amount of crystallinity in the dispersion or solution by comparing the observed spectrum to a predictive model; The method according to item 6, comprising: [Item 8] The method according to Item 7, wherein the predictive model is created according to any one of Items 1 to 5. [Item 9] The method according to item 7 or 8, wherein comparing the observed spectrum with the predictive model comprises processing the observed spectrum in the same manner as the spectra of the multiple reference samples described in any one of items 1 to 5. [Item 10] The method according to any one of Items 6 to 9, wherein the amount of crystallinity in the dispersion or solution is measured at 50% by weight or less. [Item 11] The method according to any one of Items 6 to 10, wherein the amount of crystallinity in the dispersion or solution is measured to be 1% by weight or more. [Item 12] (i) forming the API into an amorphous solid dispersion or solid-state solution; (ii) testing the dispersion or solution for crystallinity of the API one or more times by the method according to any one of items 6 to 10; and (iii) if the dispersion or solution has an acceptable amount of crystallinity, processing the composition into a final drug product; A method for producing a pharmaceutical composition comprising the steps of: [Item 13] Forming the API into a dispersion or solution is carried out by extrusion, ball milling, or spray drying; and / or One or more tests regarding the presence or absence of crystallinity of the dispersion or solution are carried out in-line; Item 13. The method according to item 12. [Item 14] The method of item 13, wherein forming is performed by extrusion and testing is performed at one or more of the API injection points, upstream of the extrusion point, and at the extrusion point. [Item 15] The method of item 13, wherein forming is performed by ball milling in a ball mill having one or more clearing points, and testing is performed through one or more clearing points substantially perpendicular to the axis of motion. [Item 16] The method according to item 13, wherein the forming is carried out by spray drying and the testing is carried out at one or more of the API injection points, the atomization point in the drying chamber, or the settling point after atomization. [Item 17] The method according to any one of Items 12 to 16, wherein the allowable range of crystallinity is 1% by weight or less. [Item 18] The method according to any one of Items 13 to 17, wherein the API input to the screw extruder, ball mill, or spray dryer is automatically adjusted, if necessary, to ensure that the crystallinity is within an acceptable range. [Item 19] The method according to any one of Items 13 to 18, wherein the speed of the screw extruder, ball mill, or spray dryer is automatically adjusted, if necessary, to ensure that the crystallinity is within an acceptable range. [Item 20] The method according to any one of Items 13 to 19, wherein the temperature of the extruder barrel, ball mirror, or spray dryer is automatically adjusted, if necessary, to ensure that the crystallinity is within an acceptable range. [Item 21] The method according to any one of Items 12 to 20, wherein the ultraviolet / visible reflectance and / or transmittance is measured continuously. [Item 22] The method according to any one of Items 1 to 21, wherein the reflectance and / or transmittance spectrum is measured at a wavelength of 210 to 800 nm. [Item 23] The method according to any one of Items 1 to 22, wherein only the reflectance spectrum is measured. [Item 24] The method according to any one of Items 13 to 22, wherein only the transmission spectrum is measured. [Item 25] The method according to any one of Items 1 to 24, wherein the particle size of the dispersion or solution is measured before subjecting it to UV / Vis spectroscopy. [Item 26] The method of item 25, wherein the dispersion or solution is sized to compare with the size of one or more reference samples having known crystallinity, the reference samples being comparable to the API and carrier of the dispersion or solution. [Item 27] ​​The method according to any one of Items 1 to 26, wherein the API is a compound having a molecular weight of 2000 g / mol or less. [Item 28] The method according to any one of items 1 to 27, wherein the API is at least 95% pure prior to incorporation into the dispersion or solution. [Item 29] The method according to any one of Items 1 to 28, wherein the API contains 5 wt% or less of water. [Item 30] The method according to any one of items 1 to 29, wherein the API is a non-nucleoside reverse transcriptase inhibitor (NNRTI), preferably etravirine (ETR), or a non-steroidal anti-inflammatory drug (NSAID), preferably piroxicam (PRX). [Item 31] The method according to any one of Items 1 to 30, wherein the carrier of the dispersion or solution comprises an amorphous polymer. [Item 32] The method according to Item 31, wherein the amorphous polymer is one or more of a cellulose polymer, a vinyl polymer, a polymethacrylate polymer, and a polyalkylene glycol polymer. [Item 33] The method of item 32, wherein the amorphous polymer is one or more of ethyl cellulose, hydroxyethyl cellulose, hydroxypropyl cellulose, hydroxypropyl methylcellulose (HPMC), HPMC acetate succinate (HPMCAS); polyvinyl acetate phthalate; polymethacrylate; polyalkylene glycol, e.g., polyethylene glycol (PEG), copolymers of PEG and polypropylene glycol (PPG), poloxamer (a triblock polymer having a central hydrophobic PPG block flanked by two hydrophilic PEG blocks), Soluplus (PEG-polyvinyl acetate-polyvinyl caprolactam graft copolymer (PVAc-PVCap-PEG)); polyvinylpyrrolidone (povidone), copovidone, vinylpyrrolidone-vinyl acetate copolymer, and linear random copolymers of N-vinyl-2-pyrrolidone and vinyl acetate (e.g., 60:40). [Item 34] The method according to any one of Items 1 to 33, wherein the carrier of the dispersion or solution contains 5% by weight or less of water. 35. An apparatus for producing a pharmaceutical composition as an amorphous solid dispersion or solid-state solution, comprising a quality control system for testing the amount of crystallinity of an API in the composition by one or more UV / Vis spectrometers configured to measure reflectance and / or transmittance intensity. 36. The apparatus of claim 35, comprising a screw extruder, a ball mill, or a spray dryer, wherein the or each UV / Vis spectrometer is positioned at an in-line measurement point to measure the reflectance and / or transmittance of a dispersion or solution. [Item 37] The apparatus described in Item 36, comprising a screw extruder, wherein the or at least one UV / Vis spectrometer is configured to measure reflectance and / or intensity at one or more of the API injection point, upstream of the extrusion point, and the extrusion point. [Item 38] The apparatus described in Item 36, comprising a ball mill having one or more clearing points, wherein the or at least one UV / Vis spectrometer is configured to measure reflectance and / or transmittance through the one or more clearing points and is substantially perpendicular to the axis of motion. 39. The apparatus of claim 36, further comprising a spray dryer, wherein the or at least one UV / Vis spectrometer is configured to measure reflectance and / or transmittance at one or more of the API input point, the atomization point in the drying chamber, and the settling point after atomization. [Item 40] An apparatus according to any one of items 35 to 39, wherein the or each UV / Vis spectrometer is photonically connected to the or each measurement point by an optical fiber. [Item 41] The apparatus of any one of items 36 to 40, wherein the apparatus is configured to automatically adjust the API input to the screw extruder, ball mill, or spray dryer, if necessary, in response to in-line measurements of the or each UV / Vis spectrometer. [Item 42] The apparatus of any one of items 36 to 41, wherein the apparatus is configured to automatically adjust the speed of a screw extruder, ball mill, or spray dryer, if necessary, in response to in-line measurements of the or each UV / Vis spectrometer. [Item 43] The apparatus of any one of items 36 to 42, wherein the apparatus is configured to automatically adjust the temperature of the screw extruder, ball mill, or spray dryer, if necessary, in response to in-line measurements of the or each UV / Vis spectrometer. [Item 44] An apparatus described in any one of items 35 to 43, wherein the or each UV / Vis spectrometer is configured to measure reflectance and / or transmittance intensity over the range 210 to 800 nm. [Item 45] An apparatus according to any one of items 35 to 44, wherein the or each UV / Vis spectrometer is configured to continuously measure reflectance and / or transmittance. [Item 46] The apparatus according to any one of Items 35 to 45, for producing a pharmaceutical composition as an amorphous solid dispersion or a solid-state solution according to any one of Items 12 to 32. EXAMPLES

[0065]

[0096] Working Example

[0097] Method 1: In-line crystallinity detection of piroxicam in Kollidon VA64

[0098] A twin-screw extruder was used to evaluate the maximum solubility of mixtures of the nonsteroidal anti-inflammatory drug (NSAID) piroxicam (PRX) and the carrier polymer Kollidon VA64. Using an in-line UV / Vis spectrometer system, the mixture was continuously analyzed while moving laterally through the extruder screws, and the dosage of PRX was adjusted until crystallinity was first detected.

[0066] [ka]

[0067]

[0099] Samples were analyzed by UV / Vis spectrometer in transmission mode (Figure 1) and XRD spectra of the same samples were also obtained for comparison and validation (Figure 2). While XRD samples required offline milling and analysis, UV / Vis has the advantage that it can be performed quickly in-line without milling.

[0068]

[0100] UV / visible transmission spectra were obtained for 15, 18, 20, 23, and 25 wt% PRX samples. There is a clear overall increase in absorbance for the 23-25 ​​wt% PRX samples. This correlates with the observation that the mixture appears amorphous, homogeneous, and transparent at PRX loadings below 25 wt%. However, at 25 wt% PRX, initial microcrystalline domains are observed, resulting in increased scattering and decreased transmitted light (i.e., increased absorbance).

[0069]

[0101] XRD spectra were obtained separately on a Bruker instrument for each of the pure solid PRX, Kollidon VA64, and the 20, 25, and 30 wt% PRX blends. In comparison, XRD does not detect the presence of crystallinity in the 25 wt% PRX blend. Only at 30 wt% PRX loading, well above the maximum solubility, does the XRD spectrum show peaks that correlate with the XRD spectrum of pure PRX for the first time, where substantially higher crystallinity is present. The Kollidon VA64 spectrum indicates that the polymeric component of the blend is amorphous.

[0070]

[0102] This experiment demonstrates that UV / Vis can have a higher sensitivity to low amounts of crystallinity compared to XRD.

[0071]

[0103] Method 2: UV / Vis calibration using a milled crystalline ETR dilution series

[0104] Etravirine (0.82271 g), sodium stearoyl fumarate (0.03291 g), and HMPC-E5 (2.444 g) were added to a small sealable plastic bag to give a 25% by weight ETR mixture. The ETR was 100% crystalline. HMPC-E5 was cryomilled for 20 minutes and dried before use.

[0072] [ka]

[0073]

[0105] The particle size distribution of the ingredients was measured using a Mastersizer and is shown in the table below.

[0074] [Table 1]

[0075]

[0106] Alternatively, the sealed bag was kneaded and shaken for a total of 2 minutes. The resulting powder was used in a serial dilution series to obtain mixtures with 20, 10, 5, 2.5, 1.25, 0.625, and 0.3125 wt% crystalline ETR. The diluent was a fully amorphous solid dispersion with the same ratios of ETF, SSF, and HPMC-E5 to maintain an ETR loading of 25%.

[0076]

[0107] Multiple UV / Vis reflectance spectra were obtained for each sample in the dilution series. The spectra for mixtures with 20, 10, 5, 2.5, 1.25, and 0.625 wt. % crystalline ETR are shown in FIG.

[0077]

[0108] The overall reflectance increases with the degree of crystallinity at all measured wavelengths. There is a clear correlation between the amount of crystalline ETR (20-0.6 wt%) and the reflectance observed in each UV / Vis spectrum. The amount of crystalline ETR was independently verified on the same samples using offline XRD and Raman spectroscopy.

[0078]

[0109] Additionally, Figure 4 shows overlaid UV / Vis spectra for another series of ETR preparations with different degrees of crystallinity. There is a similarly clear correlation between the amount of crystalline ETR (0-9.8 wt%) and the reflectance observed in each UV / Vis spectrum.

[0079]

[0110] Method 3: Predictive modelling of crystallinity

[0111] To generate a predictive model for determining crystallinity, each reflectance spectrum for each amount of crystalline ETR in Method 2 was first transformed to its second derivative and then processed by standard normal variate (SNV) analysis, and a Savitzky Golay analysis was performed to create a moving average over all data points in each spectrum. Following these data processing steps to normalize and smooth the spectral data, the data were subjected to principal component analysis (PCA) to obtain the first principal component (Factor 1) that was found to explain approximately 98% of the spectral variance (see Figures 9 and 10). A plot of Factor 1 (y-axis) against wavelength (x-axis) in the range of 290-400 nm is shown in Figure 9. This represents a simplified "spectrum" that best fits the entire data set of samples across the entire range of crystallinity tested.

[0080]

[0112] Factor 2 primarily explains the remaining 2% of variation in the data set (Figure 10). A scatter plot of factor 2 (y-axis) against factor 1 (x-axis) is shown in Figure 11. The samples were found to cluster according to their crystallinity (i.e., samples with 2.5% crystallinity (squares), 5% crystallinity (circles), 10% crystallinity (triangles), and 20% crystallinity (diamonds)). This indicates that by processing the UV / Vis spectral data to form a PCA model, the spectra are well resolved and samples can be differentiated by their crystallinity in the range of 2.5-20%.

[0081]

[0113] In Figure 12, the predicted crystallinity by factor 1 (y-axis) is plotted against the known (reference) crystallinity levels of the samples (x-axis). A high degree of correlation is observed (R 2 (values ​​are greater than 0.99). This example demonstrates that UV / Vis spectra, optionally after data normalization and / or smoothing, can be processed to generate a PCA model to facilitate the determination of the crystallinity of one or more samples by the methods of the present invention.

[0082]

[0114] Importantly, without wishing to be bound by any particular theory, the inventors believe that many other API / carrier combinations are amenable to such PCA modeling, since PCA is an adaptable analysis that can be used to reduce the complexity or dimensionality of spectral data without requiring understanding the cause of a particular spectral shape or pattern.

[0083]

[0115] In some cases, the data can be further processed by partial least squares regression (PLSR) to conveniently compare and predict the crystallinity of a sample(s) based on UV / Vis spectra, inter alia, by reference to a "standard curve" formed from values ​​obtained from multiple reference samples of known crystallinity and having the same API and carrier as the sample(s) of interest.

[0084]

[0116] Because the total reflectance and absorbance of a sample vary with crystallinity, another method for modeling UV / Vis spectral data is to compare the L of reference samples with known degrees of crystallinity. * The goal is to generate and plot values.

[0085]

[0117] L * is the L color space according to the "CIELAB color space" defined by the International Commission on Illumination (CIE). * a * b * The lightness value component of the darkest black is L * = 0, the brightest white is L * = 100. L for crystallinity * Such a plot of values ​​is shown in Figure 5. * A clear linear correlation is observed between the values, especially for crystallinity values ​​above 1%.

Claims

1. 1. A method for generating a predictive model for determining the level of crystallinity of an active pharmaceutical ingredient (API) in an amorphous solid dispersion, comprising: (i) subjecting a number of reference samples of dispersions spanning a range of API crystallinity to UV / Vis spectroscopy; (ii) measuring the reflectance and / or transmission spectrum of each reference sample; and (iii) processing the spectra collected in step (ii) to generate a predictive crystallinity model; The method comprising:

2. 2. The method of claim 1, wherein the number of reference samples is 5 or more; and / or the spectra are pre-processed prior to step (iii) to normalize and / or smooth the spectra.

3. 3. The method of claim 1 or 2, wherein the spectra of reference samples are processed to derive features that correlate with crystallinity over at least a portion of the range of crystallinity.

4. The features are: At least a first principal component derived from a principal component analysis (PCA) of the spectra, where the variance of said first principal component with crystallinity is substantially linear across the range of crystallinity of said plurality of dispersions; or The lightness value L in the CIELAB color space derived from the spectrum * ; Including, The method according to claim 3.

5. 1. A method for testing a pharmaceutical composition comprising an API in an amorphous solid dispersion for crystallinity of the API, comprising: (i) subjecting the dispersion to UV / Visible spectroscopy; (ii) measuring the reflectance and / or transmittance spectrum; and (iii) determining the presence or absence of crystallinity of the API by comparing the measured reflectance and / or transmittance spectra with those expected for a completely amorphous sample; The method comprising:

6. (iv) if crystalline API is found to be present, determining the level of crystallinity in the dispersion by comparing the observed spectra to a predictive model; The method of claim 5 further comprising:

7. The method according to claim 6, wherein the predictive model is generated according to any one of claims 1 to 4.

8. 8. The method of claim 6 or 7, wherein comparing the observed spectrum to the predictive model comprises processing the observed spectrum in the same manner as the spectra of the plurality of reference samples.

9. A method according to any one of claims 5 to 8, wherein the level of crystallinity in the dispersion is measured at 50% by weight or less.

10. A method according to any one of claims 5 to 9, wherein the level of crystallinity in the dispersion is measured at 1% by weight or greater.

11. (i) forming the API into an amorphous solid dispersion; (ii) testing the dispersion one or more times for crystallinity of the API by the method according to any one of claims 5 to 9; and (iii) if the dispersion has an acceptable level of crystallinity, processing the composition into a final pharmaceutical product; A method for producing a pharmaceutical composition comprising the steps of:

12. forming the API into a dispersion is carried out by extrusion, ball milling, or spray drying; and / or 12. The method of claim 11, wherein the one or more tests for the presence or absence of crystallinity in the dispersion are performed in-line.

13. Forming is performed by extrusion and testing is performed at one or more of the following: the point of API injection, upstream of the point of extrusion, and at the point of extrusion; or Forming is performed by ball milling in a ball mill having one or more clearing points and testing is performed through one or more clearing points substantially perpendicular to the axis of motion; or Formation is performed by spray drying and testing is performed at one or more of the following: the API injection point, the atomization point in the drying chamber, or the settling point after atomization; The method of claim 12.

14. The crystallinity tolerance is 1% by weight or less; and / or The API input to the screw extruder, ball mill, or spray dryer is automatically adjusted to ensure that the crystallinity is within an acceptable range; and / or The speed of the screw extruder, ball mill, or spray dryer is automatically adjusted to ensure that the crystallinity is within an acceptable range; and / or The temperature of the extruder barrel, ball mirror, or spray dryer is automatically adjusted to ensure that the crystallinity is within an acceptable range; and / or The UV / Vis reflectance and / or transmittance are continuously measured; The method according to any one of claims 11 to 13.

15. The method according to any one of the preceding claims, wherein the reflectance and / or transmittance spectrum is measured at wavelengths from 210 to 800 nm.

16. The method according to any one of claims 1 to 15, wherein only the reflectance spectrum or only the transmission spectrum is measured.

17. A method according to any one of claims 1 to 16, wherein the size of the particles in the dispersion is measured prior to subjecting them to UV / Vis spectroscopy.

18. 20. The method of claim 17, wherein the particles are sized to compare to the size of particles in one or more reference samples of known crystallinity, the reference samples being comparable to the API and carrier of the dispersion.

19. the API is a compound with a molecular weight of 2000 g / mol or less; and / or the API is at least 95% pure prior to incorporation into said dispersion; and / or The API contains 5% or less by weight of water; and / or The API is a non-nucleoside reverse transcriptase inhibitor (NNRTI), etravirine (ETR), a non-steroidal anti-inflammatory drug (NSAID), or piroxicam (PRX); and / or The carrier of the dispersion contains 5% by weight or less of water; The method according to any one of claims 1 to 18.

20. The method of any one of claims 1 to 19, wherein the carrier of the dispersion comprises an amorphous polymer.

21. 21. The method of claim 20, wherein the amorphous polymer is one or more of a cellulose polymer, a vinyl polymer, a polymethacrylate polymer, and a polyalkylene glycol polymer.

22. 22. The method of claim 21, wherein the amorphous polymer is one or more of ethyl cellulose, hydroxyethyl cellulose, hydroxypropyl cellulose, hydroxypropyl methylcellulose (HPMC), HPMC acetate succinate (HPMCAS); polyvinyl acetate phthalate; polymethacrylate; polyalkylene glycols selected from the group consisting of polyethylene glycol (PEG), copolymers of PEG, polypropylene glycol (PPG), poloxamer (a triblock polymer having a central hydrophobic PPG block flanked by two hydrophilic PEG blocks), and Soluplus (PEG-polyvinyl acetate-polyvinyl caprolactam graft copolymer (PVAc-PVCap-PEG)); polyvinylpyrrolidone (povidone), copovidone, vinylpyrrolidone-vinyl acetate copolymer, and linear random copolymers of N-vinyl-2-pyrrolidone and vinyl acetate.

23. 1. An apparatus for producing a pharmaceutical composition as an amorphous solid dispersion, comprising a screw extruder or a spray dryer, and a quality control system, said quality control system testing the level of crystallinity of an API in the composition by one or more UV / Vis spectrometers configured to measure reflectance and / or transmittance intensity.

24. The apparatus of claim 23, wherein the one or more UV / Vis spectrometers are positioned at in-line measurement points to measure the reflectance and / or transmittance of the dispersion.

25. 25. The apparatus of claim 24, wherein the apparatus comprises a screw extruder and the at least one UV / Vis spectrometer is configured to measure reflectance and / or intensity at one or more of the API injection point, upstream of the extrusion point, and at the extrusion point.

26. 25. The apparatus of claim 24, wherein the apparatus comprises a spray dryer and the at least one UV / Vis spectrometer is configured to measure reflectance and / or transmittance at one or more of the API input point, the point of atomization in the drying chamber, and the point of settling after atomization.

27. the one or more UV / Vis spectrometers are photonically coupled to the one or more measurement points by optical fibers; and / or the apparatus is configured to automatically adjust API dosage to the screw extruder or spray dryer in response to in-line measurements of the one or more UV / Vis spectrometers; and / or the apparatus is configured to automatically adjust the speed of a screw extruder or a spray dryer in response to in-line measurements of each of the one or more UV / Vis spectrometers; and / or the apparatus is configured to automatically adjust the temperature of a screw extruder or a spray dryer in response to in-line measurements of the one or more UV / Vis spectrometers; and / or the one or more UV / Vis spectrometers are configured to measure reflectance and / or transmittance intensity over the 210-800 nm region; and / or the one or more UV / Vis spectrometers are configured to continuously measure reflectance and / or transmittance; Apparatus according to any one of claims 23 to 26.

28. Apparatus according to any one of claims 23 to 27 for producing a pharmaceutical composition as an amorphous solid dispersion according to any one of claims 11 to 21.

Citation Information

Patent Citations

  • Method of quantifying crystal

    JP2005337776A

  • Medicine evaluation method and medicine evaluation device

    JP2013152159A

  • Method and Apparatus For Dissolving Solid Matter in Liquid

    US20080165354A1

  • Method and system for emitting light

    US20110174064A1

  • Quantification and preparation of pharmaceutical grade cantharidin

    WO2016118633A1