Additive for isocyanate-based electrolyte containing sulfonamide structural group and use thereof

The isocyanate-based electrolyte additive with a sulfonamide group addresses the issues of oxidative decomposition and high impedance in lithium secondary batteries by forming a stable interfacial film, enhancing cycle performance and high-temperature stability.

JP7559253B2Active Publication Date: 2024-10-01VALIANT CO LTD

Patent Information

Application Number
JP2023546182
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-11-24
Filing Date
2022-03-02
Publication Date
2024-10-01
Estimated Expiration
2042-03-02

AI Technical Summary

Technical Problem

Conventional lithium secondary batteries face issues with oxidative decomposition of the electrolyte, metal ion elution, and high interfacial film impedance, leading to performance deterioration, especially at high temperatures, due to the limitations of existing film-forming additives like 1,3-propane sultone and ethylene sulfate.

Method used

An isocyanate-based electrolyte additive containing a sulfonamide structural group is introduced, which forms a stable interfacial film with high thermal stability, reducing impedance and acting as an electrolyte stabilizer, effectively suppressing acid value and color changes in the electrolyte.

Benefits of technology

The additive enhances the cycle performance and high-temperature stability of lithium-ion batteries by forming a stable interfacial film, reducing impedance, and preventing discoloration and acidity increases, thereby improving battery performance under extreme conditions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007559253000001
    Figure 0007559253000001
  • Figure 0007559253000002
    Figure 0007559253000002
  • Figure 0007559253000003
    Figure 0007559253000003
Patent Text Reader

Abstract

The present invention relates to an isocyanate-based electrolyte additive containing a sulfonamide structural group, the structural formula of which is as shown in Formula I. JPEG2024514997000012.jpg62144, where R1 and R2 are the same or different, R1 and R2 are independently selected from methyl, ethyl, butyl, methoxy, methanesulfonyl, ethanesulfonyl, fluorosulfonyl, trifluoromethanesulfonyl, perfluoroethylsulfonyl, benzenesulfonyl, alkyl-containing benzenesulfonyl, cyanide-containing / fluorine-containing benzenesulfonyl, and alkoxy-containing benzenesulfonyl, and R1 and R2 can be linked to form a five-membered or six-membered ring. The electrolyte additive organically bonds the sulfonyl group and the isocyanate structural group together, has good thermal stability, and acts as an electrolyte stabilizer to prevent high-temperature discoloration and increase in acid value of the electrolyte. The electrolyte containing the novel additive provided by the present invention is used in a battery to improve high-temperature cycleability and high-temperature storage stability, and shows low impedance.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an isocyanate-based electrolyte additive containing a sulfonamide structure group and its use, and belongs to the technical field of additives for non-aqueous electrolytes of lithium batteries. [Background technology]

[0002] Since being commercialized, lithium secondary batteries have been widely used in the fields of digital, energy storage, power, military space flight and communication devices due to their high specific energy and high cycle performance. Compared with other secondary batteries, lithium secondary batteries have the advantages of high operating voltage, long cycle life, low self-discharge rate, environmental friendliness, no memory effect, etc.

[0003] In lithium-ion batteries, the oxidative decomposition of the electrolyte deteriorates the battery performance, and is always accompanied by the dissolution of metal ions during cycles and high-temperature storage, resulting in a serious decline in battery performance. With the continuous increase in the demand for lithium-ion batteries in the market, higher requirements are put forward for the overall performance of the battery, and the use of additives is one of the effective ways to improve the overall performance of lithium-ion batteries. There are many types of additives, which can be divided into film-forming additives, overcharge protection additives, conductive additives, flame retardant additives, electrolyte stabilizers, etc. according to the different roles that the additives play in the electrolyte. Regardless of which additives they are, they take up a very small proportion in the electrolyte, but they have prominent functions and are therefore widely researched and developed.

[0004] Conventional lithium secondary batteries use carbonate-based electrolytes, and the interfacial film formed on the surfaces of the positive and negative electrodes is unfavorable to the transmission of lithium ions, leading to high impedance of the interfacial film and causing the attenuation of the electrochemical properties of the battery. Film-forming additives can be an effective means of improving the properties of the interfacial film of the positive and negative electrodes, where impedance is considered to be an important property of the interfacial film, and it is expected to develop a film-forming additive that can reduce the impedance of the interfacial film of the positive and negative electrodes of lithium secondary batteries.

[0005] In general, sulfur-based additives have a certain effect of reducing battery impedance and further improve the high-temperature and low-temperature performance of the battery. 1,3-propane sultone (PS) and ethylene sulfate (DTD) are representative additives containing sulfur element, and are film-forming additives that have the effect of reducing battery impedance. However, 1,3-propane sultone (PS) is subject to restrictions in the European Union, and ethylene sulfate (DTD) has low thermal stability and, if a stabilizer is not present, causes deterioration of the acid value and color of the electrolyte, which adversely affects the high-temperature performance of the battery.

[0006] Therefore, it is important to develop new film-forming additives and electrolyte stabilizers. Summary of the Invention [Problem to be solved by the invention]

[0007] The present invention overcomes the shortcomings of the prior art by providing an isocyanate-based electrolyte additive with high thermal stability, which has an excellent impedance reducing effect and can form a stable interfacial film on the electrode surface, thereby achieving the objective of improving the interfacial properties. [Means for solving the problem]

[0008] The technical solution of the present invention to solve the above technical problems is an isocyanate-based electrolyte additive containing a sulfonamide structural group, the structural formula of which is as shown in Formula I: JPEG0007559253000001.jpg62144

[0009] (In the formula, R 1 and R 2 are the same or different, and R 1 and R 2are each independently selected from a methyl group, an ethyl group, a butyl group, a methoxy group, a methanesulfonyl group, an ethanesulfonyl group, a fluorosulfonyl group, a trifluoromethanesulfonyl group, a perfluoroethylsulfonyl group, a benzenesulfonyl group, an alkyl-containing benzenesulfonyl group, a cyanide-containing / fluorine-containing benzenesulfonyl group, and an alkoxy-containing benzenesulfonyl group; R 1 and R 2 can be linked to form a five- or six-membered ring.

[0010] Regarding the compound mechanism of the isocyanate-based electrolyte additive containing the above-mentioned sulfonamide structural group, there are documents reporting the preparation method thereof, and references such as J. Org. Chem. 1994, 59, 3540-3542., CN1039417, CN1033807, Phosphorus, Sulfur, and Silicon, 1992, 70, 91-97 all introduce this type of material.

[0011] Furthermore, the electrolyte additive is any one or a mixture selected from two or more of the following structural formulas: JPEG0007559253000002.jpg254170JPEG0007559253000003.jpg255146

[0012] The isocyanate-based additive containing a sulfonamide structural group provided by the present invention has high thermal stability, and when a non-aqueous electrolyte solution for a lithium ion battery is prepared using it and stored at a high temperature of 45° C. for 30 days, the acid value and color of the electrolyte solution are stable. When the novel additive provided by the present invention is mixed with diethyl ether dithiocarbamate (DTD) or methylene disulfonate (MMDS) to prepare an electrolyte solution, it acts as a DTD or MMDS stabilizer, effectively inhibiting the increase in acidity and color of the electrolyte solution, thereby improving the relevant performance of the battery.

[0013] The present invention further discloses the use of an isocyanate-based electrolyte additive containing a sulfonamide structural group, which is used in a lithium ion battery comprising a negative electrode, a positive electrode, a separator disposed between the negative electrode and the positive electrode, and an electrolyte.

[0014] The negative electrode is a single material selected from the group consisting of a carbon-based active material, a silicon-based active material, a metal-based active material, or a lithium-containing nitride, or a mixture of two or more of them.

[0015] Furthermore, the electrolyte solution contains a solvent, an electrolyte lithium salt, and an additive, and the additive contains at least the isocyanate-based electrolyte solution additive containing the sulfonamide structural group.

[0016] Furthermore, the content of the isocyanate-based electrolyte additive containing a sulfonamide structural group is 0.01 to 5%, preferably 0.05 to 1%, based on the total mass of the electrolyte.

[0017] Furthermore, the electrolyte lithium salt is LiPF 6 , LiClO 4 , LiBF 4 , LiBOB, LiODFB, LiTDI, LiTFSI and LiFSI, and the content of the electrolyte lithium salt is 10 to 20 wt % based on the total mass of the electrolyte.

[0018] Furthermore, the solvent is one or a combination of two or more selected from ethylene carbonate, propylene carbonate, butylene carbonate, fluoroethylene carbonate, dimethyl carbonate, diethyl carbonate, dipropyl carbonate, ethyl methyl carbonate, methyl propyl carbonate, ethyl propyl carbonate, methyl propynyl carbonate, 1,4-butyrolactone, methyl propionate, methyl butyrate, ethyl acetate, ethyl propionate, propyl propionate, and ethyl butyrate. Effect of the Invention

[0019] The beneficial effects of the present invention are the following (1), (2) and (3).

[0020] (1) The present invention provides an isocyanate-based additive containing a sulfonamide structural group, in which the isocyanate group has a high electrophilic activity and reacts with the water in the electrolyte system and the active hydrogen contained in the positive and negative electrodes to generate LiPF due to the active hydrogen. 6 The decomposition of can be reduced.

[0021] (2) The novel additive provided by the present invention has a sulfonyl group that has high film-forming properties. When added to an electrolyte, it can form a stable interfacial film on the electrode surface. The sulfonyl structural group introduces S element into the SEI film, improving the ionic conductivity, and thus effectively improving the cycle performance of the lithium-ion battery. Specifically, the battery has high cycle performance and at the same time exhibits low internal resistance.

[0022] (3) The novel additive provided by the present invention organically bonds a sulfonyl group and an isocyanate structural group together, has high thermal stability, and acts as an electrolyte stabilizer, preventing high-temperature discoloration and an increase in acid value of the electrolyte. Even when the novel additive provided by the present invention is used in an electrolyte system containing diethyl ether dithiocarbamate (DTD) or methylene disulfonate (MMDS), which are prone to causing an increase in the acid value and color of the electrolyte, it acts as a good electrolyte stabilizer and effectively suppresses discoloration and an increase in acid value of the electrolyte. When an electrolyte containing the novel additive provided by the present invention is used in a battery, it improves high-temperature cycle performance and high-temperature storage stability, and shows low impedance. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0023] In order to make the above objects, features and advantages of the present invention more clear, the following is a detailed description of specific embodiments of the present invention. In the following description, many specific details are described in order to make the present invention easy to fully understand. However, the present invention can be implemented in many other ways different from this description, and those skilled in the art can make similar improvements without departing from the content of the present invention, so the present invention is not limited to the specific examples disclosed below.

[0024] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which the present invention pertains. The terms used in the present specification are only for describing specific embodiments and are not intended to limit the present invention. Battery Example

[0025] The components of the nonaqueous electrolyte solutions of the lithium ion batteries of Battery Examples 1 to 8 and Comparative Examples 1 to 5 are as shown in Table 1. Table 1. Components of the non-aqueous electrolyte of the lithium ion batteries of battery examples 1 to 8 and comparative examples 1 to 5 JPEG0007559253000004.jpg233170JPEG0007559253000005.jpg104170

[0026] The methods for producing lithium ion type coin batteries using the nonaqueous electrolytes of the lithium ion batteries of Battery Examples 1 to 8 and Comparative Examples 1 to 5 are (1), (2), (3), and (4) below. (1) Manufacturing of positive electrode sheets

[0027] Positive electrode LiNi 0.8 Co 0.1 Mn 0.1 O 2 The powder, carbon black (particle size is 1000 nm), polyvinylidene fluoride (PVDF) and N,N-dimethylpyrrolidone (NMP) were mixed to prepare a uniform slurry, and the slurry was uniformly applied to an aluminum foil (15 μm) current collector, then dried and rolled to obtain the LiNi 0.8Co 0.1 Mn 0.1 O 2 The positive electrode material was obtained. It was dried at 120°C for 12 hours, and the LiNi 0.8 Co 0.1 Mn 0.1 O 2 The carbon black accounted for 2% of the total coating, while the adhesive accounted for 4%. The resulting electrode sheet was then sheared into 8 mm diameter wafers to form the positive electrodes. (2) Manufacturing of negative electrode sheets

[0028] For example, artificial graphite anode material is prepared by mixing artificial graphite, polyvinylidene fluoride (PVDF) and N-methylpyrrolidone (NMP) to prepare a uniform slurry, which is then uniformly coated on a copper foil (15μm) current collector, then dried and rolled to obtain a carbon anode material. After drying at 120℃ for 12 hours, the graphite accounts for 96.4% of the total coating mass and the adhesive accounts for 3.6% of the total coating mass in the dried electrode sheet. The electrode sheet is then sheared into wafers with a diameter of 8mm to prepare the anode. (3) Preparation of electrolyte

[0029] In an argon atmosphere glove box with a moisture content of <1 ppm, the lithium salt was dissolved in a solvent, and then the novel phosphine-containing isocyanate system was added and mixed homogeneously to obtain the electrolyte. (4) Manufacture of lithium-ion batteries

[0030] The materials described in steps (1) and (2) above were used as the working electrode, and Celgard 2400 membrane (Tianjin) was used as the separator to assemble a CR2430-type coin battery. The assembly order was from the negative electrode to the positive electrode, and was the negative electrode case, elastic sheet, gasket, negative electrode sheet, electrolyte, separator, positive electrode sheet, and positive electrode case, and then sealed with a sealing machine. All of these operations were completed in a pure argon gas glove box, and after leaving it to stand for 6 hours, it was taken out and subjected to electrochemical property testing. Lithium-ion battery performance testing

[0031] Test 1, electrolyte stability test: The lithium ion battery electrolytes prepared in the above Examples 1 to 8 and Comparative Examples 1 to 5 were placed in sealed aluminum bottles, and the aluminum bottles were vacuumed and sealed with an aluminum plastic film. The electrolyte samples were simultaneously stored in an incubator with a set temperature of 45°C, and samples were taken in a glove box before and after 30 days of storage to detect the acidity and color value of the electrolyte, and the acidity was tested with a potentiometric titrator. The acidity value was converted to HF and the unit was ppm, and the color was measured by platinum-cobalt colorimetry and the color unit was Hazen. The test results are shown in Table 2. Table 2. Effect of additives on the acid value and color of electrolyte JPEG0007559253000006.jpg88170

[0032] As can be seen from Table 2, the electrolytes of Examples 1 to 8 had lower acidity and color than the comparative examples after storage at a high temperature of 45° C. for 30 days, i.e., when the novel additive provided by the present invention was added to the electrolyte system of diethyl ether sulfate (DTD) or methylene disulfonate (MMDS), the acid value and color of the electrolyte were effectively suppressed. Thus, the novel additive provided by the present invention effectively suppresses the increase in acidity and color of the electrolyte and improves the stability of the electrolyte under high temperature conditions. Test 2: High temperature cycle performance test and high temperature storage test

[0033] The following tests were carried out on the manufactured batteries.

[0034] (1) At 45°C, the battery is charged at a constant current of 0.1C up to 4.3V, and then discharged at a constant current of the corresponding rate up to 2.7V, which is the first cycle.

[0035] (2) After the first cycle was completed, the batteries were charged at a constant current of 1.0C up to 4.3V, and then discharged at a constant current of 2.7V at the corresponding charging rate. Tests were performed for 100 and 500 cycles according to these cycle conditions, and the capacity retention after 100 and 500 battery cycles was calculated. The capacity retention after cycling was calculated according to the following formula. The relevant test data obtained for each battery are shown in Table 2. Capacity retention after cycling = (discharge capacity after the corresponding number of cycles / discharge capacity of the first cycle) × 100%.

[0036] Test of rate of change in internal resistance due to high temperature storage: The batteries obtained in Examples 1 to 8 and Comparative Examples 1 to 5 were subjected to five charge / discharge cycle tests at room temperature with a charge / discharge rate of 1C, and finally charged to a fully charged state at a rate of 1C. The internal resistance T of the battery was recorded. The fully charged battery was stored at 60°C for 15 days, the internal resistance T0 of the battery was recorded, and experimental data such as the rate of change in internal resistance of the battery were calculated. The recorded results are shown in Table 3 (the battery numbers of Examples 1 to 8 are Battery 1 to Battery 8, respectively, and the battery numbers of Comparative Examples 1 to 5 are Battery 1# to Battery 5#, respectively). Internal resistance change rate = (T-T0) / T×100%. Table 3. Test results of Examples and Comparative Examples JPEG0007559253000007.jpg172170

[0037] As can be seen from Table 3, the use of the novel additive of the present invention can obviously improve the high temperature cycle performance and high temperature impedance of the lithium secondary battery. This shows that the novel additive of the present invention can improve the negative electrode / electrolyte interface properties, thereby reducing the irreversible capacity at the first charge / discharge of the lithium secondary battery, lowering the interface impedance, and maintaining the interface stability at the same time, which is helpful in improving the high temperature cycle stability of the lithium secondary battery.

[0038] As can be seen from the above, the novel additive of the present invention has high thermal stability and can act as an electrolyte stabilizer, preventing high-temperature discoloration and an increase in acid value of the electrolyte. Even when the novel additive provided by the present invention is used in an electrolyte system containing diethyl ether dithiocarbamate (DTD) or methylene disulfonate (MMDS), which are prone to causing an increase in acid value and color of the electrolyte, it still acts as a good electrolyte stabilizer and effectively inhibits discoloration and an increase in acid value of the electrolyte. When an electrolyte containing the novel additive provided by the present invention is used in a battery, it improves high-temperature cycle performance and shows low impedance, and has good future prospects for use.

[0039] The technical features of the above embodiments may be combined in any manner, and for the sake of brevity, not all possible combinations of the technical features in the above embodiments are described; however, as long as there is no contradiction in the combination of these technical features, any combination should be considered to be within the scope of the present specification.

[0040] The above examples only show some embodiments of the present invention, and the description is specific and detailed, but it should not be understood as limiting the scope of the invention patent. It should be noted that those skilled in the art can make some modifications and improvements without departing from the concept of the present invention, all of which are within the scope of protection of the present invention. Therefore, the scope of protection of the patent of the present invention should be based on the attached claims.

Claims

1. An isocyanate-based electrolyte additive containing a sulfonamide structural group, characterized in that the structural formula is as shown in Formula I. (In the formula, R 1 and R 2 are the same or different, R 1 and R 2 are each independently selected from a methyl group, an ethyl group, a butyl group, a methoxy group, a methanesulfonyl group, an ethanesulfonyl group, a fluorosulfonyl group, a trifluoromethanesulfonyl group, a perfluoroethylsulfonyl group, a benzenesulfonyl group, an alkyl-containing benzenesulfonyl group, a cyanide-containing / fluorine-containing benzenesulfonyl group, and an alkoxy-containing benzenesulfonyl group; R 1 and R 2 can be linked to form a five- or six-membered ring)

2. The isocyanate-based electrolyte additive containing a sulfonamide structural group according to claim 1, characterized in that it is any one or a mixture of two or more selected from the following structural formulas:

3. A lithium ion battery using the isocyanate-based electrolyte additive containing a sulfonamide structural group according to claim 1 or 2, characterized in that the electrolyte additive is used in a lithium ion battery including a negative electrode, a positive electrode, a separator disposed between the negative electrode and the positive electrode, and an electrolyte.

4. 4. The lithium ion battery using the isocyanate-based electrolyte additive containing a sulfonamide structural group according to claim 3, wherein the electrolyte comprises a solvent, an electrolyte lithium salt, and an additive, and the additive comprises at least the isocyanate-based electrolyte additive containing the sulfonamide structural group.

5. The content of the isocyanate-based electrolyte additive containing a sulfonamide structural group according to claim 4 is 0.01 to 5% by weight of the total weight of the electrolyte.

6. The electrolyte lithium salt is LiPF 6 , LiClO 4 , LiBF 4 5. The lithium ion battery using the isocyanate-based electrolyte additive having a sulfonamide structural group according to claim 4, wherein the electrolyte lithium salt is one or more selected from the group consisting of LiBOB, LiODFB, LiTDI, LiTFSI and LiFSI, and the content of the electrolyte lithium salt is 10 to 20 wt % based on the total mass of the electrolyte.

7. The solvent is selected from the group consisting of ethylene carbonate, propylene carbonate, butylene carbonate, fluoroethylene carbonate, dimethyl carbonate, diethyl carbonate, dipropyl carbonate, ethyl methyl carbonate, methyl propyl carbonate, ethyl propyl carbonate, methyl propynyl carbonate, 1,4-butyrolactone, methyl propionate, methyl butyrate, ethyl acetate, ethyl propionate, propyl propionate, and ethyl butyrate. A lithium ion battery using the isocyanate-based electrolyte additive containing a sulfonamide structural group according to claim 4.

Citation Information

Patent Citations

  • JP1974081320A

  • Fluorescent x-ray analysis apparatus

    JP1990045743A

  • Heterocyclic substituted sulfonyl ureas, their preparation and their use as herbicide or plant growth regulator

    JP1991068562A

  • Nonaqueous electrolyte, and battery comprising the same

    JP2013093242A

  • Lithium secondary battery including isocyanate compound

    US20200127321A1

Cited By

  • Non-aqueous secondary batteries

    JP2026181921A