CURING MOLD ASSEMBLY FOR NON-PNEUMATIC TIRE AND METHOD FOR MANUFACTURING SAME - Patent application
The mold assembly with a radially offset curing bladder system effectively cures non-pneumatic tires by applying pressure and heat, addressing the limitations of conventional methods and enabling the production of structurally sound non-pneumatic tires.
Patent Information
- Application Number
- JP2023577499
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-06-18
- Filing Date
- 2022-06-14
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2042-06-14
AI Technical Summary
Conventional tire mold assemblies and manufacturing methods are unable to produce non-pneumatic tires effectively, limiting their manufacture and applicability.
A mold assembly with a first curing bladder assembly supported radially offset to the mold axis, using elastomeric material to cure non-pneumatic tires by applying pressure and heat through a stiffening bladder system.
Enables the complete curing of non-pneumatic tires by transitioning uncured elastomeric materials to a fully cured state, facilitating the production of non-pneumatic tires with structural integrity.
Smart Images

Figure 0007559268000001 
Figure 0007559268000002 
Figure 0007559268000003
Abstract
Description
[Technical field]
[0001] The subject matter of this disclosure relates broadly to vehicle tire manufacturing techniques and, more particularly, to mold assemblies for curing non-pneumatic tires and methods of manufacturing non-pneumatic tires using such mold assemblies. [Background technology]
[0002] The subject matter of the present disclosure may find particular application and use in conjunction with components for vehicles, and is shown and described herein with reference thereto, however, it should be understood that the subject matter of the present disclosure is also suitable for use in other applications and environments, and the particular uses shown and described herein are merely exemplary.
[0003] A conventional pneumatic tire includes a tire casing having a tread formed on or along its exterior configured to engage a roadway or other ground. The tire casing includes an annular body formed from a plurality of layers or plies (e.g., radial plies, belt plies) and having opposed sidewalls extending radially inwardly from shoulder portions of the annular body therealong to beads that form the radially inward extents of the sidewalls. The inner surface of the annular body and the opposed sidewalls are covered by an inner liner that defines the tire chamber of the pneumatic tire.
[0004] In a conventional tire manufacturing process, an uncured tire carcass and tread assembly is loaded into a mold assembly on a tire curing press. The mold assembly includes a plurality of die segments having an inner surface portion that includes a section of the tread pattern. The mold assembly is closed by a tire curing press, which positions the die segments into abutting engagement with the tread material of the uncured tire assembly. The tire curing press also includes a curing bladder that is positioned inside the mold assembly such that in its uninflated state, the uncured tire assembly is spaced outboard of the curing bladder. During the curing process, the curing bladder is inflated such that it extends into the tire chamber of the uncured tire assembly into abutting engagement with the inner liner. While under pressure from the mold assembly and the inflated curing bladder, the tire curing press introduces heat into the uncured tire assembly which vulcanizes or otherwise crosslinks the uncured tire material to form a finished tire. Summary of the Invention [Problem to be solved by the invention]
[0005] Despite the widespread use and overall success of known types and varieties of tire mold assemblies and manufacturing methods, it has been recognized that certain disadvantages exist in the known processes that may limit their applicability and / or use with respect to the manufacture of tire assemblies having other structural arrangements, such as, for example, so-called non-pneumatic tires. As such, it would be desirable to develop mold assemblies and manufacturing methods that may help overcome the aforementioned and / or other problems of the known technology and / or that may otherwise advance the manufacture of non-pneumatic tires.
[0006] An example of a method of manufacturing a non-pneumatic tire assembly according to the subject matter of the present disclosure can include providing a first mold section including a longitudinally extending mold axis. The method can also include supporting a first curing bladder assembly on the first mold section radially offset relative to the mold axis. The first curing bladder assembly can include a first bladder wall at least partially formed from an elastomeric material. The first bladder wall can at least partially define a first bladder chamber and can include a first end wall portion disposed along the first mold section and a second end wall portion spaced longitudinally from the first end wall portion. The first bladder wall can also include a first edge wall portion extending longitudinally between the first end wall portion and the second end wall portion and a second edge wall portion extending longitudinally between the first end wall portion and the second end wall portion spaced apart relative to the first edge wall portion. The first bladder wall may further include a first sidewall portion and a second sidewall portion extending longitudinally between the first endwall portion and the second endwall portion and extending laterally between the first edgewall portion and the second edgewall portion. The first sidewall portion may include a first outer surface portion having a concave cross-sectional profile. The second sidewall portion may include a second outer surface portion having a convex cross-sectional profile. The method may also include providing an uncured, non-pneumatic tire assembly including a plurality of support structures disposed in a circumferentially spaced relationship to one another and a plurality of spaces disposed in a circumferentially spaced relationship to one another, one of the plurality of spaces being between adjacent support structures of the plurality of support structures. The method may further include positioning the uncured, non-pneumatic tire assembly along the first mold section such that the first curing bladder assembly is disposed in one of the plurality of spaces and axially coextensive with at least a portion of the uncured, non-pneumatic tire assembly.The method may also include inflating the first curing bladder assembly, thereby displacing at least the first and second edge wall portions outwardly into engagement with and applying pressure to the uncured non-pneumatic tire assembly. The method may further include curing the non-pneumatic tire assembly.
[0007] One embodiment of a mold assembly according to the disclosed subject matter can include a first mold section having a mold axis and sized to receive an associated, uncured, non-pneumatic tire assembly. The mold assembly can include a first curing bladder assembly supported on the first mold section radially offset relative to the mold axis. The first curing bladder assembly can include a first bladder wall at least partially formed from an elastomeric material. The first bladder wall can at least partially define a first bladder chamber. The first bladder wall can include a first end wall portion disposed along the first mold section and a second end wall portion spaced longitudinally from the first end wall portion. The first bladder wall can also include a first edge wall portion extending longitudinally between the first end wall portion and the second end wall portion and a second edge wall portion extending longitudinally between the first end wall portion and the second end wall portion spaced apart relative to the first edge wall portion. The first bladder wall can further include first and second sidewall portions extending longitudinally between the first and second end wall portions and extending laterally between the first and second edge wall portions. The first sidewall portion can include a first outer surface portion having a concave cross-sectional profile. The second sidewall portion can include a second outer surface portion having a convex cross-sectional profile. [Brief description of the drawings]
[0008] [Figure 1] FIG. 1 is an exploded top perspective view of the components of an exemplary uncured, non-pneumatic tire, shown prior to assembly. [Diagram 2]FIG. 2 is a perspective bottom view of an exemplary uncured non-pneumatic tire in an assembled condition and ready for curing. [Diagram 3] FIG. 3 is a front view of the tire curing press showing the mold assembly in an open position and loaded with an exemplary fully uncured, non-pneumatic tire. [Figure 4] FIG. 4 is a front view of the tire curing press of FIG. 3 with the mold assembly in a closed position and an exemplary uncured, non-pneumatic tire loaded for curing. [Diagram 5] FIG. 5 is a cross-sectional top view of the mold assembly and exemplary uncured non-pneumatic tire taken along line 5-5 of FIG. [Figure 6] FIG. 6 is an enlarged view of a portion of the mold assembly and exemplary uncured non-pneumatic tire identified as Detail 6 in FIG. [Figure 7] 7 is a cross-sectional side view of the mold assembly of FIGS. 1-6 and an illustrative uncured non-pneumatic tire taken along line 7-7 of FIG. [Figure 8] 8 is a cross-sectional side view of the mold assembly of FIGS. 1-7 and an illustrative uncured non-pneumatic tire taken along line 8-8 of FIG. 6. FIG. [Figure 9] FIG. 9 is an enlarged view of a portion of the mold assembly and exemplary uncured non-pneumatic tire identified as Detail 9 in FIG. [Figure 10] FIG. 10 is an enlarged view of a portion of the mold assembly and exemplary uncured non-pneumatic tire identified as detail 10 in FIG. [Figure 11] FIG. 11 is an exploded top perspective view of one embodiment of a stiffening bladder assembly in accordance with the subject matter of the present disclosure, for example as shown in FIGS. 6-10. [Figure 12] FIG. 12 is a graphical representation of one embodiment of a manufacturing method according to the subject matter of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] Referring now to the drawings, it should be understood that the drawings are presented for purposes of illustrating embodiments of the subject matter of the present disclosure, and that such embodiments are not intended to be limiting. In addition, it will be appreciated that the drawings are not to scale, and that portions of certain features and / or elements may be exaggerated for clarity and ease of understanding.
[0010] 1 and 2 illustrate one embodiment of an uncured, non-pneumatic tire sized and / or otherwise configured for curing in a mold assembly according to the subject matter of the present disclosure and / or through a manufacturing method according to the subject matter of the present disclosure. It will be appreciated that various types, varieties, and / or constructions of non-pneumatic tires have been developed and / or are used in different applications and / or environments. As one non-limiting example, an uncured, non-pneumatic tire (or tire assembly) 100 is shown in FIGS. 1-5 as having a longitudinal axis AX and may extend axially from an end 102 to an end 104 opposite the end 102. The uncured, non-pneumatic tire 100 may include an annular ring 106 extending circumferentially about the axis AX and a structure 108 disposed outside at least a portion of the annular ring 106 and also extending circumferentially about the axis AX. The uncured, non-pneumatic tire 100 may also include an annular ring 110 extending circumferentially about the axis AX, with at least a portion of the annular ring 110 disposed outside the annular ring 106 and / or the structure 108. The uncured, non-pneumatic tire 100 may further include a tread body 112 extending circumferentially about the axis AX, with at least a portion of the tread body 112 disposed outside the annular ring 110.
[0011] It will be appreciated that the mold assemblies and manufacturing methods according to the presently disclosed subject matter may be used to transition a non-pneumatic tire having one or more portions formed from an elastomeric material that is not fully cured into a non-pneumatic tire in which all or substantially all of the portions are substantially entirely crosslinked, vulcanized, and / or otherwise cured. Thus, it will be appreciated and understood that any one or more of the aforementioned components of non-pneumatic tire 100 may include an elastomeric material that is transitioned from a fully uncured state to at least a substantially entirely cured state, and that the configurations of non-pneumatic tire 100 shown and described herein are merely exemplary and are not intended to be limiting.
[0012] It will be appreciated that the annular ring 106 may be of any suitable size, shape, and / or configuration, and may include any suitable number of one or more walls and / or wall portions. As one non-limiting example, the annular ring may be a part of, or otherwise at least partially form, an outer wall or outer wall portion of a vehicle wheel or rim, as represented in FIGS. 1 and 2 by reference character VRM. In such an exemplary arrangement, the annular ring 106 may include a ring wall (or ring wall portion) 114 extending circumferentially around the longitudinal axis AX. Optionally, the annular ring 106 may include a hub wall (or hub wall portion) HUB disposed inside the ring wall portion 114. If included, the hub wall portion HUB may be operably connected to the ring wall portion 114. Additionally, if included, the hub wall portion HUB may optionally be dimensioned and / or otherwise adapted for mounting in a conventional manner on or along an associated component or device, such as an associated vehicle axle through bolt hole BHL.
[0013] The ring wall portion 114 of the annular ring 106 may extend axially between a ring edge 116 disposed toward the end 102 and a ring edge 118 disposed axially spaced apart from the ring edge 116 toward the end 104. The ring wall portion 114 may include an outer surface portion 120 that faces radially outward and extends circumferentially about the longitudinal axis AX and axially between the ends 102, 104. In some cases, the ring wall portion 114 may optionally include an inner surface portion 122 that extends circumferentially about the longitudinal axis AX and faces axially radially inward along and / or between the ends 102 and / or 104.
[0014] The structure 108 may include an inner wrap or layer 124 and an outer wrap or layer 126 disposed radially outward of the inner layer 124. The inner layer 124 and the outer layer 126 extend axially between ends 102 and 104, the inner layer 124 extends axially between edges 132 and 134, and the outer layer 126 extends axially between edges 128 and 130. In some cases, the inner layer 124 and the outer layer 126 may be substantially coextensive with one another such that edges 128 and 132 are at least approximately aligned with one another along end 102, and edges 130 and 134 are at least approximately aligned with one another along end 104. The inner layer 124 may at least partially define an inner surface portion 136 of the structure 108 that extends circumferentially about the longitudinal axis AX and axially between ends 102 and 104. The outer layer 126 may at least partially define an outer surface portion 138 of the structure 108 that extends circumferentially about the longitudinal axis AX and axially between the ends 102 and 104 .
[0015] The structure 108 also includes a plurality of support structures 140 extending between and operably interconnecting the inner layer 124 and the outer layer 126. It will be appreciated that the support structures 140 may be of any suitable shape, configuration, and / or arrangement and may be operably connected to the inner layer 124 and the outer layer 126 in any suitable manner. As one non-limiting example, the support structure 140 may extend axially from an edge 142 disposed toward the end 102 to an edge 144 disposed toward the end 104. The support structure 140 may also include an end 146 disposed toward the inner layer 124 and an end 148 disposed toward the outer layer 126 in a spaced relationship relative to the end 146. The support structure 140 is illustrated and described herein as having a curved or otherwise non-linear profile along a plane transverse to the longitudinal axis AX. Support structure 140 is shown and described as having one circumferentially facing concave portion 150 about longitudinal axis AX and an opposite circumferentially facing convex portion 152. However, it will be recognized that such configuration is merely exemplary and that support structures having other shapes and / or profiles may alternatively be used without departing from the subject matter of the present disclosure.
[0016] The support structures 140 are arranged circumferentially spaced apart from one another about the longitudinal axis AX such that the spaces 154 are also arranged circumferentially spaced apart from one another about the longitudinal axis, with one of the spaces 154 disposed between adjacent ones of the support structures 140. In such an arrangement, the spaces 154 may have an arcuate, curved, or otherwise generally crescent-shaped cross-sectional profile or configuration, with the concave portion 150 of one support structure 140 and the convex portion 152 of the adjacent support structure 140 at least partially defining the circumferentially spaced sides of the spaces 154. In some cases, the support structures 140 may extend into or otherwise be at least partially embedded in the inner layer 124 and / or the outer layer 126. In such cases, a portion 156 of the inner layer 124 may at least partially define an end portion 158 of the spaces 154 such that the portions 156 of the inner layer 124 may have a curved or otherwise non-linear cross-sectional shape and / or configuration. Additionally or alternatively, a portion 160 of the outer layer 126 may at least partially define an end portion 162 of the space 154 such that the portion 160 may have a curved or otherwise non-linear cross-sectional shape and / or configuration.
[0017] It will be understood that the annular ring 110 may be of any suitable size, shape, and / or configuration, and may include any suitable number of one or more walls and / or wall portions. As one non-limiting example, the annular ring 110 may include a ring wall (or ring wall portion) 164 extending circumferentially about the longitudinal axis AX. The ring wall portion 164 may extend axially between a ring edge 166 disposed toward the end 102 and a ring edge 168 disposed axially spaced apart from the ring edge 166 toward the end 104. The ring wall portion 164 may include an inner surface portion 170 that faces radially inward and extends circumferentially about the longitudinal axis AX and axially along and / or between the ends 102 and 104. The ring wall portion 164 may also include an outer surface portion 172 that extends circumferentially about the longitudinal axis AX and faces axially radially outward along and / or between the ends 102 and / or 104.
[0018] The tread body 112 may extend axially between the ends 102 and 104, with a tread edge 174 disposed along the end 102 and a tread edge 176 disposed along the end 104. The tread body 112 may also include an inner surface portion 178 facing radially inward and an outer surface portion 180 facing radially outward. One or more tread structures 182 (e.g., grooves, ribs, lugs, sipes) may optionally be preformed on or otherwise extend into the tread body 112 from and along the outer surface portion 180 of the fully uncured non-pneumatic tire 100, such tread structures adapted to at least partially define a ground-engaging tread (or tread pattern) on the cured non-pneumatic tire during the curing process.
[0019] As discussed above, one or more walls and / or wall portions of the non-pneumatic tire 100 can be formed from an elastomeric material that is in a not fully cured state such that at least those walls and / or wall portions are curable using the mold assembly and / or manufacturing method according to the subject matter of the present disclosure. For example, the tread body 112 can be at least partially formed from an elastomeric material that is not fully cured. Additionally or alternatively, one or more of the inner layer 124 and / or the outer layer 126 of the structure 108 can be at least partially formed from an elastomeric material that is not fully cured. As a further example and / or another alternative, the support structure 140 can optionally include one or more layers of an elastomeric material that is not fully cured. As a non-limiting example of such a structure, the support structure 140 can be at least partially formed from a sheet of a relatively rigid material (e.g., metal, fiber reinforced composite), the ends 146 and 148 of which can be at least partially embedded or otherwise disposed within the inner layer 124 and the outer layer 126 of the structure 108, respectively. Additionally or alternatively, a layer of not fully cured elastomeric material can extend along and / or at least partially define concave portion 150 and / or convex portion 152. As another non-limiting example, support structure 140 can be formed at least in part from a plurality of relatively stiff wires and / or filaments disposed adjacent one another and at least partially embedded with an amount of not fully cured elastomeric material that at least partially forms a sheet-like structure.
[0020] It will be appreciated that the not fully cured non-pneumatic tire 100 may include any suitable elastomeric material or combination of elastomeric materials, such as, for example, natural rubber, synthetic rubber, and / or thermoplastic elastomers. In addition, it will be recognized and appreciated that in some cases, the various components may be formed from a common not fully cured elastomeric material. In other cases, however, two or more compositions, compounds, and / or grades of not fully cured elastomeric materials may be used. Terms such as "not fully cured" as used herein refer to elastomeric materials that have polymer chains that are crosslinked or otherwise bonded with "fully cured" or "substantially fully cured" elastomeric materials when exposed to heat, pressure, and / or chemical compounds, and that exhibit substantially different material and / or mechanical properties than the "not fully cured" elastomeric materials. One non-limiting example of a suitable curing process includes the vulcanization of natural and synthetic rubber elastomers.
[0021] It will be appreciated that any combination of one or more not fully cured elastomeric materials may be used or otherwise included in a not fully cured non-pneumatic tire (e.g., non-pneumatic tire 100). As one non-limiting example, a not fully cured non-pneumatic tire 100 may include one or more amounts of elastomeric materials, substantially all or each of which are in a "green" or substantially entirely uncured condition. As another non-limiting example, a not fully cured non-pneumatic tire 100 may include one or more amounts of elastomeric materials that are in a "green" or substantially entirely uncured condition and one or more amounts of elastomeric materials that are in an at least partially cured condition. As a further non-limiting example, a not fully cured non-pneumatic tire 100 may include one or more amounts of elastomeric materials that are in a partially, but not entirely, cured condition. As such, it is appreciated and recognized that an uncured non-pneumatic tire 100 may include, without limitation, one or more amounts of "green" or substantially entirely uncured elastomeric material, or one or more amounts of partially but not fully cured elastomeric material, or both one or more amounts of "green" or substantially entirely uncured elastomeric material and one or more amounts of partially but not fully cured elastomeric material.
[0022] 3 and 4 illustrate, in a schematic manner, another conventional tire curing press TCP, including a press base PRB having a base mounting surface BMS. The tire curing press TCP also includes a press head PRH having a head mounting surface HMS. The press head PRH is movable relative to the press base PRB in a conventional manner, for example along linear guide rods LGR. The press head PRH is shown in FIG. 3 as being located in a first or raised position and is movable to a second or lowered position shown in FIG. 4, the movement of which is represented in FIG. 3 by the arrow MVT. The tire curing press TCP may include one or more pressurized fluid sources, one or more heated fluid sources, and / or one or more vacuum sources, as diagrammatically represented in FIG. 3 and FIG. 4 by dashed boxes PFS, HFS, and VCS, respectively, and may be included on, along, or otherwise operatively associated with the press base PRB and / or the press head PRH, as is well known in the art.
[0023] A mold assembly 200 according to the disclosed subject matter is shown in Figures 2-10 as being operably supported within or otherwise on or along a tire curing press TCP. The mold assembly 200 includes a mold section 202 supported on or along a base mounting surface BSM of the press base PRB, and a mold section 204 supported on or along a head mounting surface HMS of the press head PRH. The mold section 202 may be operably connected in fluid communication with a pressurized fluid source PFS, a heated fluid source HFS, and / or a vacuum source VCS of the press base PRB in any manner suitable for transporting pressurized and / or heated fluid to and / or from the mold sections, such as, for example, via one or more conduits or passages 206. Additionally or alternatively, the mold section 204 may be operably connected in fluid communication with a pressurized fluid source PFS, a heated fluid source HFS, and / or a vacuum source VCS of the press head PRH in any manner suitable for transporting pressurized and / or heated fluid to and / or from the mold section, such as via one or more conduits or passages 208.
[0024] The mold assembly 200 includes a mold axis MAX extending in the direction of or otherwise along the movement MVT of the tire curing press TCP. Thus, the mold sections 202 and 204 are axially displaceable relative to one another during operation of the tire curing press, with the mold sections 202 and 204 shown spaced apart in FIG. 3 representing an open state of the mold assembly, and the mold sections 202 and 204 shown engaged with one another over the same extent in FIG. 4 representing a closed state of the mold assembly. The mold section 202 includes a gap curing system 210 and a plurality of tread die segments 212 circumferentially disposed around the gap curing system 210 to at least partially define a mold cavity 214 within the mold section 202. The mold section 204 includes a surface portion 216 that at least partially defines a mold cavity 218 within the mold section. The mold cavity 218 is dimensioned to receive at least a portion of the mold section 202 in the closed state of the mold assembly. In some cases, the exterior surface portion 220 of the tread die segment 212 may abut and engage the surface portion 216 of the mold section 204 as the mold sections move toward the closed configuration.
[0025] For example, as represented by arrow LOA in Figure 3 and shown in Figures 4 and 5, with an uncured, non-pneumatic tire 100 at least partially loaded or otherwise positioned within the mold cavity 214, the tread die segments 212 are displaced radially inward to engage the tread body 112 of the uncured, non-pneumatic tire 100. Such radial compression urges the inner surface portion 178 of the tread body 112 into engagement with the outer surface portion 172 of the annular ring 110. In addition, such radial compression urges the inner surface portion 170 of the annular ring 110 into engagement with the outer surface portion 138 of the structure 108. In some cases, such radial compression may also urge the inner surface portion 136 of the structure 108 into engagement with the outer surface portion 120 of the annular ring 106. Additionally, the tread die segment 212 includes features formed therealong generally opposite the surface portion 220 that, under such radial compression, extend from and along the outer surface portion 180 of the tread body 112 in engagement with the tread body 112 to at least partially define a ground-engaging tread pattern (e.g., grooves, ribs, lugs, sipes) on or along the non-pneumatic tire 100.
[0026] As shown in Figures 2-4, in some cases, a support plate 222 can be disposed along the end 102 of the not fully cured non-pneumatic tire 100. Additionally or alternatively, a support plate 224 can be disposed along the end 104 of the not fully cured non-pneumatic tire 100. The support plates 222 and / or 224, if included, can assist in maintaining the annular ring 106, the structure 108, the annular ring 110, and / or the tread body 112 in a desired axial position (e.g., in approximate axial alignment) relative to one another during loading and / or unloading of the non-pneumatic tire 100 into and / or from the mold assembly 200 (or mold section thereof), for example, during transport to a tire curing press TCP, and / or for rotatably indexing or otherwise positioning the support structure 140 and / or the space 154 about the longitudinal axis AX relative to the gap cure system 210 and / or other features of the mold assembly 200. The support plates 222 and / or 224, when included, may each include a plurality of openings 226 and 228 having a shape, configuration, and / or arrangement (e.g., radially offset from the axis AX and disposed at a common circumferential interval) that are complementary to the support structure 140 and / or space 154 of the non-fully cured non-pneumatic tire 100. In this manner, the support plates 222 and / or 224, when included, may be positioned within the mold cavity 214 together with the non-pneumatic tire 100 and / or may be operatively engaged over the same extent as the gap curing system 210. The support plates 222 and 224 also include a peripheral edge 230, in a preferred arrangement, having an outer cross-sectional dimension that is equal to or less than approximately the outermost cross-sectional dimension of the non-pneumatic tire 100 (e.g., diametrically across the tread body 112). Additionally, in some cases, the support plates 222 and 224 may optionally include an inner peripheral edge 232.Further, in some cases, the support plates 222 and 224 may optionally include an alignment ridge 234 that is dimensioned to operably engage a portion of the non-fully cured non-pneumatic tire 100 (e.g., the inner surface portion 122 of the annular ring 106) such that the alignment ridge 234 axially coexists with a portion of the non-pneumatic tire.
[0027] As shown in Figures 5-11, the gap curing system 210 includes a plurality of curing bladder assemblies 236, represented by dashed lines in Figure 5, positioned or otherwise disposed radially offset from the mold axis MAX and circumferentially spaced apart relative to one another about the mold axis. In a preferred arrangement, the curing bladder assemblies 236 are disposed such that when an uncured non-pneumatic tire 100 is positioned within the mold cavity 214, one or more of the curing bladder assemblies are disposed within one of the spaces 154. In such an arrangement, the curing bladder assemblies 236 can be selectively activated or deactivated such that the curing bladder assemblies correspondingly engage and disengage one or more walls and / or wall portions of the structure 108. In an engaged state, the curing bladder assemblies can apply surface pressure and / or transfer heat to the structure 108, and can be operable, for example, to transition one or more walls and / or wall portions of the structure formed from an uncured elastomeric material to a substantially cured elastomeric material.
[0028] That is, in the actuated state, the stiffening bladder assemblies 236 abuttingly engage the inner layer 124 of the structure 108, thereby applying pressure thereto and / or transferring heat thereto. In such an arrangement, application of pressure by the stiffening bladder assemblies urges the inner layer toward the annular ring 106. Additionally or alternatively, in the actuated state, the stiffening bladder assemblies 236 abuttingly engage the outer layer 126 of the structure 108, thereby applying pressure thereto and / or transferring heat thereto. In such an arrangement, application of pressure by the stiffening bladder assemblies 236 urges the outer layer toward the annular ring 110. Additionally and / or as another alternative, in the actuated state, the stiffening bladder assemblies 236 abuttingly engage the support structures 140, thereby applying pressure thereto and / or transferring heat thereto, by adjacent stiffening bladder assemblies 236 applying pressure to and / or transferring heat to the support structures disposed therebetween. In some cases, the stiffening bladder assembly 236 can apply pressure and / or heat on or along the ends 146 and / or 148 of the support structure, thereby ensuring that the ends 146 and / or 148 are embedded and engaged with the inner layer 124 and outer layer 126, respectively.
[0029] It will be appreciated that stiffening bladder assemblies according to the presently disclosed subject matter may be of any suitable type, variety, and / or configuration and may be operably connected on and / or along mold sections 202 and / or 204 in any suitable manner. As one non-limiting example of a suitable configuration, stiffening bladder assembly 236 may include a bladder 238 supported on one of mold sections 202 and 204 and extending toward the other of the mold sections. In some cases, each of stiffening bladder assemblies 236 and its bladder 238 may be supported on or along mold section 202. In other cases, each of stiffening bladder assemblies 236 and its bladder 238 may be supported on or along mold section 204. In yet other cases, one or more of the stiffening bladder assemblies 236 and their bladders 238 may be supported on or along the mold section 202, and the remainder of the stiffening bladder assemblies 236 and their bladders 238 are supported on or along the mold section 204, such as in an alternating or interleaved arrangement.
[0030] In the arrangement shown in FIGS. 6-11 , the bladder 238 includes a bladder wall 240 that at least partially defines a bladder chamber 242. The bladder wall 240 is at least partially formed from an elastomeric material, such as fully cured (e.g., vulcanized) natural and / or synthetic rubber. The bladder wall 240 includes an end wall portion 244 and an end wall portion 246 that is axially spaced apart from the end wall portion 244. As discussed above, each one of the end wall portions 244 and 246 of the bladder 238 can be secured on or along the mold section 204 or on or along the mold section 202. As a non-limiting example, the mold section 202 can include a base wall portion 248 that can at least partially contain and / or otherwise be disposed in fluid communication with the conduit 206, such as by two or more manifold walls or wall portions assembled together as represented by dashed line 248M in FIGS. 7 and 9 . End wall portion 244 is secured on or along base wall portion 248 by end wall portion 246 supported by base wall portion 244 in an axially spaced relationship such that bladder chamber 242 is at least partially disposed between end wall portion 244 and end wall portion 246.
[0031] The stiffening bladder assembly 236 includes a clamp plate 250 disposed within the bladder chamber 242 positioned along the end wall portion 244. The clamp plate 250 is secured to the base wall portion 248 such that one or more portions 244P of the end wall portion 244 are captured between the clamp plate 250 and the base wall portion 248. The stiffening bladder assembly 236 also includes a clamp plate 252 disposed within the bladder chamber 242 and positioned along the end wall portion 246. A clamp plate 254 is positioned and secured outside the bladder chamber opposite the clamp plate 252 along the end wall portion 246 such that one or more portions 246P of the end wall portion 246 are captured between the clamp plate 252 and the clamp plate 254.
[0032] It will be appreciated that end wall portions 244 and 246 may be supported in spaced relation to one another on or along the base wall portion in any suitable manner. For example, an elongated connecting member 256 may be operably secured between base wall portion 248 and clamp plate 254. An elongated connecting member 258 may be disposed between clamp plate 250 and clamp plate 252 to establish and maintain a predetermined distance therebetween. In some cases, connecting members 256 and 258 may be axially coextensive and / or coaxial with one another, as shown, for example, in FIGS. 6, 8, 10, and 11. In some cases, connecting member 256 may extend axially between ends 260 and 262 disposed toward base wall portion 248 and clamp plate 254, respectively. Clamp plates 250, 252, and 254 may include one or more fastening holes extending therethrough, as identified by reference numerals 264, 266, and 268, respectively. In addition, base wall portion 248 may include a fastening hole 270 extending therethrough. Clamp plates 250, 252, and 254 are positioned by fastening holes 270 such that fastening holes 264, 266, and 268 are at least approximately coaxially aligned with one another, and such that end 260 of connecting member 256 extends through at least holes 264 and 270, and end 262 extends through at least holes 266 and 268. In some cases, either or both of ends 260 and / or 262 may include one or more helical threads. A fastening device 272, such as, for example, a threaded nut, may then be operably secured to end 260 and / or end 262.
[0033] In some cases, end wall portion 244 can include one or more holes 274 extending axially therethrough through which end 260 of connecting member 256 can extend when the ends of the connecting member pass through through holes 264 and 270 in clamping plate 250 and base wall portion 248. Additionally or alternatively, end wall portion 246 can include one or more holes 276 extending axially therethrough through which end 262 of connecting member 256 can extend when the ends of the connecting member pass through through holes 266 and 268 in clamping plates 252 and 254. A seal 278 can be operably disposed between connecting member 258 and clamping plate 250 to fluidly isolate bladder chamber 242 from holes 264 in clamping plate 250 and / or holes 274 in end wall portion 244. Additionally or alternatively, a seal 280 can be operably disposed between the connecting member 258 and the clamp plate 252 to fluidly isolate the bladder chamber 242 from the hole 266 in the clamp plate 252 and / or the hole 276 in the end wall portion 246.
[0034] It will be appreciated and recognized that in the exemplary arrangement shown and described herein, the end wall portion 244 of the bladder wall 240 is positioned between the base wall portion 248 and the clamp plate 250 such that the end wall portion 244 is compressed between the base wall portion and the clamp plate when the clamp plate is secured to the base wall portion. Similarly, the end wall portion 246 of the bladder wall 240 is positioned between the clamp plate 252 and the clamp plate 254 such that the end wall portion is compressed between the clamp plates when the clamp plates are secured together. To create and maintain a desired compression of the end wall portion 244 and / or the end wall portion 246, the stiffening bladder assembly 236 can include one or more compression restrictors having a length that establishes an approximate amount or limit of compression of the associated end wall portion. As shown in Figures 8, 10, and 11, the stiffening bladder assembly 236 can include a compression restrictor 282 extending into the through hole 274 of the end wall portion 244 and positioned between the base wall portion 248 and the clamp plate 250. Additionally or alternatively, stiffening bladder assembly 236 may include a compression restrictor 284 extending into throughbore 276 in end wall portion 246 and disposed between clamp plate 252 and clamp plate 254 .
[0035] As discussed above, one or more portions 244P of the end wall portion 244 may be captured between the base wall portion 248 and the clamp plate 250, for example, to form a substantially fluid-tight seal therewith and / or to substantially inhibit lateral (i.e., transverse to the mold axis MAX) expansion and recovery of the end wall portion portion 244P. Additionally or alternatively, one or more portions 246P of the end wall portion 246 may be captured between the clamp plate 252 and the clamp plate 254, for example, to form a substantially fluid-tight seal therewith and / or to substantially inhibit lateral (i.e., transverse to the mold axis MAX) expansion and recovery of the end wall portion portion 246P. In some cases, the base wall portion 248 may include one or more protrusions 286 extending axially outwardly toward the clamp plate 250. In other cases, the clamp plate 250 may include one or more protrusions 288 extending axially outwardly therefrom in a direction toward the base wall portion 248. In some cases, both projections 286 and projections 288 can be used to capture or otherwise clamp a portion of end wall portion 244 between them and disposed in general alignment with one another. Additionally or alternatively, clamp plate 252 can optionally include one or more projections 290 extending axially outward therefrom in a direction toward clamp plate 254. In other cases, clamp plate 254 can include one or more projections 292 extending axially outward therefrom in a direction toward clamp plate 252. In some cases, both projections 290 and projections 292 can be used to capture or otherwise clamp a portion of end wall portion 246 between them and disposed in general alignment with one another.
[0036] It will be appreciated that the bladder 238 may be of any suitable size, shape, and / or configuration that is cooperative with the configuration and / or arrangement of the walls, wall portions, and spaces of the structure 108, such as the inner layer 124, the outer layer 126, the support structure 140, and / or the space 156. The bladder wall 240 may also include an edge wall portion 294 and an edge wall portion 296 that is offset radially outward from the edge wall portion 294. The edge wall portions 294 and 296 extend axially along the end wall portion 244 therefrom toward the end wall portion 246 and have a curved cross-sectional profile transverse to the mold axis MAX. The edge wall portion 294 includes an outer surface portion 298 having a convex shape and an inner surface portion 300 having a concave shape. The edge wall portion 296 includes an outer surface portion 302 having a convex shape and an inner surface portion 304 having a concave shape. Inner surface portions 300 and 304 at least partially define bladder chamber 242. In a preferred arrangement, edge wall portions 294 and 296 inflate or otherwise expand during operation to substantially conform to end portion 158 of inner layer portion 156 and end portion 162 of outer layer portion 160.
[0037] Bladder wall 240 may further include a sidewall portion 306 and a sidewall portion 308 laterally spaced from sidewall portion 306. Sidewall portions 306 and 308 extend axially along end wall portion 244 from there toward end wall portion 246. Sidewall portions 306 and 308 may also extend laterally between edge wall portion 294 and edge wall portion 296 and have a curved cross-sectional profile transverse to mold axis MAX. Sidewall portion 306 includes an outer surface portion 310 having a convex shape and an inner surface portion 312 having a concave shape that at least partially defines bladder chamber 242. Sidewall portion 308 includes an outer surface portion 314 having a concave shape and an inner surface portion 316 having a concave shape that at least partially defines bladder chamber 242. Thus, bladder 238 may, in some cases, have a crescent-shaped cross-sectional configuration transverse to mold axis MAX.
[0038] As discussed above, the stiffening bladder assembly 236 is actuated by introducing pressurized and / or heated fluid, such as from a pressurized fluid source PFS and / or a heated fluid source HFS, via, for example, conduit 206, into the bladder chamber 242 of the bladder 238. It will be appreciated that the mold assembly 200, the gap stiffening system 210, and / or the stiffening bladder assembly 236 may include any combination of features and / or components operable to facilitate the transfer of pressurized and / or heated fluid into and / or out of the bladder chamber 242. As a non-limiting example, the stiffening bladder assembly 236 may include a transfer tube 318 extending longitudinally from an end 320 secured to the base wall portion 248 and / or the clamp plate 250 to an end 322 disposed within the bladder chamber 242 toward the clamp plate 252. The transfer tube 318 can include a tube wall 324 that at least partially defines a tube passage 326 disposed in fluid communication with the conduit 206A along end 320 and the bladder chamber 242 along end 322. In some cases, the tube wall 324 can include a notch or other end relief feature 328 extending into the tube wall from an end face portion 330 thereof and can be suitable for ensuring fluid communication between the bladder chamber 242 and the tube passage 326 when the end face portion 330 is disposed near or in abutting engagement with the clamping plate 250, for example, as represented by arrow FCM in FIG.
[0039] Upon transitioning stiffening bladder assembly 236 to an operational state, pressurized and / or heated fluid 332 is transferred to bladder chamber 242, such as via conduit 206. To facilitate rapid and / or complete transfer of fluid 332 into the bladder chamber, existing fluid 334 (e.g., air, steam) contained within the bladder chamber, e.g., shown above fluid level FLV in FIG. 7, may be substantially simultaneously evacuated from bladder chamber 242, such as via conduit 206A, through tube passage 326, which may be disposed in fluid communication with a vacuum source VCS and / or another fluid transfer system.
[0040] As the pressurized and / or heated fluid 332 is transferred to the bladder chamber 242, the bladder 238 expands, causing the exterior surface portions 298, 302, 310, and 314 to apply pressure to the walls and / or wall portions of the structure 108, such as the inner layer 124, the outer layer 126, and / or the support structure 140. In such an actuated or otherwise pressurized state, represented by the dashed line ACT in Figures 7 and 8, heat may be transferred via the bladder walls 240 and / or other thermally conductive walls and / or wall portions of the mold sections 202 and / or 204 into at least the uncured elastomeric material of the structure 108 and / or tread body 112 for a predetermined period of time. At least some of the pressurized and / or heated fluid may be removed or otherwise withdrawn from the bladder chamber 242 once the predetermined cure time is reached and the uncured material of the non-pneumatic tire is fully or otherwise substantially entirely cured. In some cases, shutting down the stiffening bladder assembly 236 may include the pressurized fluid source PFS, the heated fluid source HFS, and / or the vacuum source VCS creating a reduced pressure condition in the bladder chamber 242, thereby allowing the bladder walls 240 to return to an uninflated or at least more fully uninflated state and / or to retract the bladder walls 240 to a contracted state, for example, as represented by the dashed lines DEA in FIGS. 7 and 8, and may facilitate loading and / or unloading the non-pneumatic tire 100.
[0041] It will be appreciated that the pressurized and / or heated fluid 332 may be transferred to the bladder chamber 242, and that the existing fluid 334 therefrom, the pressurized and / or heated fluid 332, and / or any condensate may be transferred from the bladder chamber 242 in any suitable manner. As one non-limiting example, the end wall portion 244 of the bladder wall 240 may include one or more passages 336 extending therethrough that are in fluid communication with the conduits 206 and / or 206A of the base wall portion 248 of the mold section 202. In such an arrangement, the clamp plate 250 may include one or more passages 338 extending therethrough that are in fluid communication with the passages 336 of the end wall portion of the bladder wall. In some cases, the passages 336 and / or 338 may be arranged in direct fluid communication with the bladder chamber 242. In other cases, the one or more passages 336 and / or 338 may be arranged in fluid communication with the tube passages 326. Thus, it will be appreciated that any suitable configuration and / or arrangement may be used without departing from the subject matter of the present disclosure.
[0042] As explained above, it will be appreciated that the remaining portions of end wall portions 244 and / or 246 of bladder wall 240 exterior to or otherwise spaced apart from portions 244P and / or 246P expand and recover upon actuation and deactivation of bladder 238. Thus, clamping plate 250 and / or clamping plate 252 may include one or more offset surface portions, identified by reference numerals 340 and / or 342 in Figures 8 and 10, respectively. Offset surface portion 340 may be disposed on or along clamping plate 250 facing end wall portion 244 such that an axial space or gap is formed between end wall portion 244 and offset surface portion 340, as represented by reference dimension GP1 in Figure 8. Additionally or alternatively, offset surface portion 342 can be disposed on or along clamping plate 252 facing end wall portion 246 such that an axial space or gap is formed between end wall portion 246 and offset surface portion 342, as represented by reference dimension GP2 in FIG. 10. Bladder wall 240 can also include an opening 344 along one of end wall portions 244 and 246 through which clamping plates 250 and / or 252 and other components of bladder assembly 236 can be inserted into bladder chamber 242.
[0043] A manufacturing method 400 according to the disclosed subject matter for manufacturing a non-pneumatic tire, as shown in FIG. 12, can include providing a mold section having a mold axis MAX, such as one of the mold sections 202 and 204, as represented by reference numeral 402 in FIG. 12. The method 400 can also include supporting one or more cure bladder assemblies, such as the cure bladder assembly 236, on the mold section in a radially offset relationship to the mold axis MAX, as represented by reference numeral 404 in FIG. 12. In a preferred arrangement, the cure bladder assemblies 236 are spaced apart from one another and disposed about the mold axis MAX to at least partially form the gap cure system 210. The method 400 can further include providing an uncured non-pneumatic tire 100 and positioning the uncured non-pneumatic tire on or along the mold section in an axially coextensive arrangement with the one or more cure bladder assemblies, as represented by reference numerals 406 and 408, respectively, in FIG. 12. The method 400 can include, for example, activating one or more curing bladder assemblies, as represented in FIG. 12 by reference numerals 410 and 412, respectively, and then curing the non-pneumatic tire.
[0044] When used herein in connection with certain features, elements, components, and / or structures, ordinal numbers (e.g., first, second, third, fourth, etc.) may be used to indicate multiple distinct singular numbers or otherwise identify certain features, elements, components, and / or structures, and do not imply any order or sequence unless specifically dictated by the claim terms. In addition, terms such as "transverse" should be interpreted broadly. Thus, terms such as "transverse" can include a wide range of relative angular orientations, including, but not limited to, approximately perpendicular angular orientations. Also, terms such as "circumferential", "circumferentially", etc. should be interpreted broadly and can include, but are not limited to, circular shapes and / or configurations. In this regard, terms such as "circumferential", "circumferentially", etc. can be synonymous with terms such as "peripheral", "circumferentially", etc.
[0045] Furthermore, phrases such as "flowable material joint" as used herein should be construed to include any joint or connection in which a liquid or other flowable material (e.g., molten metal or combination of molten metals) is deposited or otherwise present between adjacent components and functions to form a fixed, substantially fluid-tight connection between the adjacent components. Examples of processes that can be used to form such flowable material joints include, but are not limited to, welding, brazing, and soldering processes. In such cases, one or more metallic materials and / or alloys can be used to form such flowable material joints in addition to any materials from the components themselves. Another example of a process that can be used to form a flowable material joint includes applying, depositing, or otherwise presenting an adhesive between adjacent components that functions to form a fixed, substantially fluid-tight connection between the adjacent components. In such cases, it will be appreciated that any suitable adhesive material or combination of materials can be used, such as, for example, one-part and / or two-part epoxies.
[0046] It will be recognized that although a number of different features and / or components are presented in the embodiments shown and described herein, no embodiment has been specifically shown and described as including all such features and components. Thus, it should be understood that the subject matter of the present disclosure is intended to encompass any and all combinations of the different features and components shown and described herein, and that any suitable arrangement of features and components may be used, without limitation, in any combination. Thus, it should be clearly understood that claims directed to any such combination of features and / or components are intended to find basis in this disclosure, whether or not specifically expressed herein. In order to assist the Patent Office and the reader of this application and any resulting patent in interpreting the claims appended hereto, applicants do not intend that any of the appended claims or any claim elements invoke 35 U.S.C. 112(f) unless the words "means for" or "step for" are expressly used in a particular claim.
[0047] Although the subject matter of the present disclosure has been described with reference to the foregoing embodiments, and considerable emphasis has been placed on the structure of the disclosed embodiments and on the structural interrelationships between the components, it will be understood that other embodiments may be made and that numerous changes may be made to the illustrated and described embodiments without departing from the principles herein. Obviously, modifications and alterations to others will occur to those upon reading and understanding the foregoing Detailed Description of the Invention. It should therefore be clearly understood that the foregoing illustrative matter is to be construed as merely illustrative of the subject matter of the present disclosure, and not as limiting. It is therefore intended that the subject matter of the present disclosure be construed as including all such modifications and alterations.
Claims
1. 1. A method of manufacturing a non-pneumatic tire assembly, comprising: providing a first mold section including a longitudinally extending mold axis; supporting a first curing bladder assembly on the first mold section radially offset relative to the mold axis, the first curing bladder assembly including a first bladder wall formed at least in part from an elastomeric material, the first bladder wall at least in part defining a first bladder chamber, the first bladder wall comprising: a first end wall portion disposed along the first mold section and a second end wall portion spaced longitudinally from the first end wall portion; a first edge wall portion extending longitudinally between the first end wall portion and the second end wall portion, and a second edge wall portion extending longitudinally between the first end wall portion and the second end wall portion in a spaced relationship with the first edge wall portion; first and second sidewall portions extending longitudinally between the first end wall portion and the second end wall portion and extending laterally between the first edge wall portion and the second edge wall portion, the first sidewall portion including a first outer surface portion having a concave cross-sectional profile and the second sidewall portion including a second outer surface portion having a convex cross-sectional profile; providing a fully uncured non-pneumatic tire assembly including a plurality of support structures disposed in a circumferentially spaced relationship with respect to one another, and a plurality of spaces disposed in a circumferentially spaced relationship with respect to one another, one of the plurality of spaces being between adjacent ones of the plurality of support structures; positioning the uncured, non-pneumatic tire assembly along the first mold section such that the first cure bladder assembly is disposed within one of the plurality of spaces and axially coextensive with at least a portion of the uncured, non-pneumatic tire assembly; inflating the first curing bladder assembly, thereby displacing at least the first edge wall portion and the second edge wall portion outwardly into engagement with and pressure against the uncured, non-pneumatic tire assembly; and curing the non-pneumatic tire assembly.
2. supporting the first stiffening bladder assembly on the first mold section includes supporting a plurality of stiffening bladder assemblies on the first mold section in a circumferentially spaced relationship to one another about the mold axis; 2. The method of claim 1, wherein positioning the uncured, non-pneumatic tire assembly along the first mold section includes positioning the uncured, non-pneumatic tire assembly along the first mold section such that each of the plurality of curing bladder assemblies is disposed in a different one of the plurality of spaces.
3. 3. The method of claim 2, wherein inflating the first curing bladder assembly includes substantially simultaneously inflating the plurality of curing bladder assemblies such that the first sidewall portion of each of the plurality of curing bladder assemblies abuts and engages a different one of the plurality of support structures of the uncured, non-pneumatic tire assembly and the second sidewall portion of each of the plurality of curing bladder assemblies abuts and engages a different one of the plurality of support structures, thereby compressing each of the plurality of support structures between adjacent ones of the plurality of curing bladder assemblies.
4. 1. A mold assembly for curing a non-pneumatic tire, comprising: a first mold section having a mold axis and sized to receive an associated uncured, non-pneumatic tire assembly; a first curing bladder assembly supported on the first mold section radially offset relative to the mold axis, the first curing bladder assembly including a first bladder wall formed at least in part from an elastomeric material, the first bladder wall at least in part defining a first bladder chamber; and a first end wall portion disposed along the first mold section and a second end wall portion spaced longitudinally from the first end wall portion; a first edge wall portion extending longitudinally between the first end wall portion and the second end wall portion, and a second edge wall portion extending longitudinally between the first end wall portion and the second end wall portion in a spaced relationship to a first edge surface portion; and first and second sidewall portions extending longitudinally between the first end wall portion and the second end wall portion and extending laterally between the first edge wall portion and the second edge wall portion, the first sidewall portion including a first exterior surface portion having a concave cross-sectional profile and the second sidewall portion including a second exterior surface portion having a convex cross-sectional profile.
5. 5. The mold assembly of claim 4, wherein the first stiffening bladder assembly is one of a plurality of stiffening bladder assemblies secured on the first mold section and circumferentially spaced apart from one another about the mold axis.
Citation Information
Patent Citations
Manufacturing method for non-pneumatic tire
JP2021030542A
Systems and methods for forming non-pneumatic tires
US20140070448A1
Non-pneumatic tire and system for molding non-pneumatic tire
US20150027606A1
Reinforced non-pneumatic tire and system for molding reinforced non-pneumatic tire
US20150034225A1
Method of manufacturing a spoke for a non-pneumatic tire
US20210114312A1