Laminate and manufacturing method thereof
By introducing acidic functional groups and forming a polydopamine layer on the base material, the laminate addresses adhesion issues in polymer electrolyte membranes, ensuring strong bonding for applications in fuel cells and water electrolyzers.
Patent Information
- Application Number
- JP2020034706
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-03-02
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2040-03-02
AI Technical Summary
Existing methods for immobilizing polymer electrolyte membranes on base materials face challenges such as the need for expensive elastomers, brittleness, and insufficient adhesion, especially when using difficult-to-bond materials like polyolefin or fluororesin, complicating the structure and increasing costs.
A laminate is formed by introducing acidic functional groups onto the surface of the base material, followed by forming a polydopamine layer, and then laminating a polymer electrolyte membrane using a polymer electrolyte solution, leveraging polyion complex formation for strong adhesion.
The laminate achieves firm adhesion between the polymer electrolyte membrane and the base material, suitable for applications in fuel cells and water electrolyzers, with improved mechanical properties and reduced complexity.
Smart Images

Figure 0007562958000001
Abstract
Description
[Technical field]
[0001] The present invention relates to a laminate in which a polymer electrolyte membrane and a substrate are laminated via an adhesive layer, and a method for producing the same. [Background technology]
[0002] Polymer electrolyte membranes, taking advantage of their excellent ion exchange and ion transport properties, are used in a wide range of fields, including pure water and ultrapure water production equipment, electrodialysis equipment, desalination equipment, salt production equipment, ion chromatography, and fuel cells. Among them, fuel cells are attracting attention because they are effective in suppressing global warming as a next-generation power generation system. Fuel cells include phosphoric acid fuel cells, molten carbonate fuel cells, solid oxide fuel cells, and solid polymer fuel cells. Among these, solid polymer fuel cells have the advantages of being able to start up from room temperature, being small in size, and having high output, and are therefore expected to be applied to automobiles and household power sources.
[0003] In these applications, it is necessary to fix the electrolyte membrane to various substrates, but there are problems with the fixing method. For example, when fixing the electrolyte membrane to the substrate using a gasket, it is necessary to use a special and expensive elastomer having heat resistance and acid resistance as the material of the gasket, the electrolyte membrane may become brittle due to contact with the gasket, and the structure becomes complicated, which makes assembly complicated, resulting in unavoidable cost increases. On the other hand, Patent Document 1 and Patent Document 2 disclose fixing the electrolyte membrane to the substrate using an adhesive, but there are cases where sufficient adhesion is not necessarily obtained when a poorly adhesive material such as polyolefin or fluororesin-based material is used as the substrate.
[0004] Meanwhile, Patent Document 3 discloses a method for bonding a polyacetal resin molded body using polydopamine as a method for bonding poorly adhesive materials, but makes no mention of bonding an electrolyte membrane. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2008-112639 A [Patent Document 2] JP 2010-205493 A [Patent Document 3] JP 2010-144155 A Summary of the Invention [Problem to be solved by the invention]
[0006] The present invention relates to a laminate comprising a polymer electrolyte membrane and a substrate, the laminate being bonded via an adhesive layer made of polydopamine, and a method for producing the same. The present invention can provide a laminate that is strongly bonded to the polymer electrolyte membrane even when various types of substrates are used. [Means for solving the problem]
[0007] As a result of intensive research aimed at solving the above problems, the inventors have found that by adhering a substrate having acidic functional groups introduced onto its surface to a polymer electrolyte membrane via polydopamine, a laminate can be produced in which the polymer electrolyte membrane is firmly adhered to the substrate, and have thus completed the present invention.
[0008] That is, the respective aspects of the present invention are [1] to [3] shown below. [1] A laminate comprising a polymer electrolyte membrane and a substrate, the laminate being laminated via an adhesive layer made of polydopamine. [2] The laminate according to the above [1], characterized in that an acidic functional group is introduced onto the surface of the substrate. [3] A method for producing the laminate according to the above [1] or [2], comprising the steps of:
[0009] Step 1: A step of introducing acidic functional groups onto the substrate surface.
[0010] Step 2: A step of forming a polydopamine layer on the surface of the substrate.
[0011] Step 3: A step of applying a polymer electrolyte solution to at least one of the substrate surface and the polymer electrolyte membrane surface, and then laminating the two together.
[0012] The details will be explained below.
[0013] The laminate according to one embodiment of the present invention is a laminate comprising a polymer electrolyte membrane and a substrate, and the laminate is laminated via an adhesive layer made of polydopamine.
[0014] The polymer electrolyte membrane may be any polymer electrolyte membrane having proton conductivity, and examples thereof include hydrocarbon-based electrolyte membranes such as polystyrene sulfonate / divinylbenzene copolymer, sulfonated poly(4-phenoxybenzoyl-1,4-phenylene), sulfonated poly(4-phenoxybenzoyl-1,4-phenylene) / polycyanophenyl ether copolymer, sulfonated polyether ether ketone, sulfonated polysulfone, sulfonated polyether sulfone, sulfonated polybenzimidazole, sulfonated polyimide sulfonated polyphosphazene, etc., partially fluorinated electrolyte membranes such as poly-α-fluorostyrene sulfonate / divinylbenzene copolymer, and fluorine-based electrolyte membranes such as tetrafluoroethylene / perfluoro[2-(hydroxysulfonylethoxy)propyl vinyl ether] copolymer, tetrafluoroethylene / perfluoro(2-hydroxysulfonylethyl vinyl ether) copolymer, tetrafluoroethylene / perfluoro(4-hydroxysulfonylbutyl vinyl ether) copolymer, etc. Of these electrolyte membranes, sulfonated poly(4-phenoxybenzoyl-1,4-phenylene) / polycyanophenyl ether copolymers, sulfonated polybenzimidazole, poly-α-fluorostyrenesulfonic acid / divinylbenzene copolymers, tetrafluoroethylene / perfluoro[2-(hydroxysulfonylethoxy)propyl vinyl ether] copolymers, tetrafluoroethylene / perfluoro(2-hydroxysulfonylethyl vinyl ether) copolymers, and tetrafluoroethylene / perfluoro(4-hydroxysulfonylbutyl vinyl ether) copolymers are preferably used, as they have excellent mechanical properties, high heat resistance, high oxidation resistance, and excellent proton conductivity.
[0015] As the substrate, various materials such as metals, ceramics, and polymers can be used, but polymers are preferably used because of their corrosion resistance and the ease of introducing functional groups onto the substrate surface. Examples of the polymers used include polyolefins such as polyethylene, polypropylene, ethylene / propylene copolymers, ethylene / butene copolymers, ethylene / vinyl acetate copolymers, ethylene / vinyl alcohol copolymers, polymethylpentene, and cycloolefin polymers; halogen-containing polymers such as polyvinyl chloride, polyvinylidene chloride, polyvinylidene fluoride, and polytetrafluoroethylene; styrene-based polymers such as polystyrene, styrene / acrylonitrile copolymers, styrene / butadiene / acrylonitrile copolymers, styrene / butadiene copolymers, and styrene / maleic anhydride copolymers; acrylic resins such as polymethyl methacrylate and methyl methacrylate / styrene copolymers; polyesters such as polyethylene terephthalate, polybutylene terephthalate, polyethylene naphthalate, polylactic acid, and unsaturated polyesters; polyamides such as nylon 6, nylon 66, nylon 46, nylon 12, and nylon 6T; polyvinyl alcohol, polyurethane, polycarbonate, polyphenylene sulfide, polyethersulfone, polyetheretherketone, polyimide, polyamideimide, epoxy resins, phenolic resins, and silicone resins. In order to enhance the adhesion of the adhesive layer to the polydopamine, it is preferable to introduce an acidic functional group into the surface of the substrate. Examples of the acidic functional group include a carboxyl group, a sulfonic acid group, a sulfate group, a phosphoric acid group, and a phenolic hydroxyl group. There is no particular restriction on the amount of acidic functional group introduced. For example, when the substrate is a polyolefin, the amount of the acidic functional group introduced is 1450 cm -1 1700cm normalized by CH bending absorption -1 The relative absorbance ratio of the C=O stretching of the carboxyl group is preferably 0.1 to 0.7. The shape of the substrate is not limited, and substrates in the shape of a block, plate, sheet, film, porous, net, woven fabric, nonwoven fabric, etc. can be used.
[0016] The adhesive layer is made of polydopamine. The adhesive layer made of polydopamine is formed by oxidative polymerization of dopamine, and its thickness is preferably 1 to 100 nm. Since polydopamine has many amino groups in its molecule, it forms a polyion complex with the sulfonic acid group on the surface of the polymer electrolyte membrane or the acidic functional group on the surface of the substrate, and firmly bonds the polymer electrolyte membrane and the substrate. On the other hand, when the amount of acidic functional groups on the substrate surface is small, the hydrophobic part of polydopamine exhibits adhesiveness due to hydrophobic interaction with the hydrophobic part of the substrate surface, or the hydroxyl group of polydopamine forms a hydrogen bond with the polar group on the substrate surface, and adhesiveness may be expressed, so introduction of acidic functional groups to the substrate surface is not necessarily essential.
[0017] Next, a method for producing the laminate according to one embodiment of the present invention will be described.
[0018] The laminate according to one embodiment of the present invention can be produced through at least the following three steps.
[0019] Step 1: A step of introducing acidic functional groups onto the substrate surface.
[0020] Step 2: A step of forming a polydopamine layer on the surface of the substrate.
[0021] Step 3: A step of applying a polymer electrolyte solution to at least one of the substrate surface and the polymer electrolyte membrane surface, and then laminating the two together.
[0022] Step 1 is a step of introducing an acidic functional group to the surface of the substrate. The method of introducing the acidic functional group is not particularly limited, and examples thereof include a method of graft polymerization of an acidic functional group-containing monomer, a method of introducing an acidic functional group to the surface of the substrate by corona treatment or plasma treatment, and a method of contacting an oxygen-containing gas or a mixed gas of sulfur dioxide gas and fluorine gas with the substrate and then hydrolyzing the mixture to introduce a carboxyl group or a sulfonic acid group. Among these methods, the method of contacting an oxygen-containing gas or a mixed gas of sulfur dioxide gas and fluorine gas with the substrate and then hydrolyzing the mixture is preferably used because it is possible to introduce an acidic functional group to the surface regardless of the shape of the substrate, and the amount of introduction can be easily controlled by changing the gas composition.
[0023] Step 2 is a step of forming a polydopamine layer on the surface of the substrate to which the acidic functional group has been introduced in step 1. A polydopamine layer may also be formed on the surface of the polymer electrolyte membrane. The formation of a polydopamine layer on the surface of the substrate or the surface of the polymer electrolyte membrane is carried out by contacting a dopamine solution with the substrate or the surface of the polymer electrolyte membrane, and oxidatively polymerizing dopamine, thereby forming a polydopamine thin film that spontaneously deposits on the substrate surface or the surface of the polymer electrolyte membrane. The dopamine solution used is a solution in which dopamine is dissolved in a solvent such as water, and the concentration is not particularly limited and can be appropriately set within the range of 0.1 to 10 mg / mL. Since the polymerization of dopamine is easily promoted in a weak alkaline environment, it is preferable to adjust the pH to 8 to 10 with tris(hydroxymethyl)aminomethane hydrochloride or the like. Since the polymerization of dopamine proceeds by oxidative polymerization, an oxidizing agent is required to promote the polymerization. As the oxidizing agent, oxygen, hydrogen peroxide, ozone, and organic peroxide can be used. The thickness of the polydopamine layer can be controlled by appropriately selecting the polymerization temperature, time, and the type and amount of the oxidizing agent, and is preferably in the range of 1 to 100 nm. The polydopamine layer can be formed on the surface of a substrate or a polymer electrolyte membrane, but since a polymer electrolyte membrane is generally thin and easily swells in water, it may be difficult to form a polydopamine layer on the surface of the substrate. Therefore, it is easier to handle the polydopamine layer when it is formed on the surface of a substrate.
[0024] Step 3 is a step of laminating a polymer electrolyte membrane, in which a polymer electrolyte solution is applied to at least one of the substrate surface and the polymer electrolyte membrane surface, and then the two are laminated together.
[0025] Since the adhesion mechanism of the laminate of the present invention is the formation of a polyion complex, no adhesion is generated even if the polymer electrolyte membrane and the substrate having a polydopamine layer formed on the surface are brought into contact in a dry state. In order to adhere the polymer electrolyte membrane and the substrate having a polydopamine layer formed on the surface, it is necessary that the polymer chains on the polydopamine layer and the polymer electrolyte membrane surface have mobility in a wet state. The adhesion can be achieved by applying a polymer electrolyte solution to the substrate or polymer electrolyte membrane on which the polydopamine layer is formed, and then laminating the two in a wet state. The type of polymer electrolyte in the polymer electrolyte solution used in this process is preferably the same type as the polymer electrolyte membrane to be laminated, but it does not necessarily have to be the same. The solvent used in the polymer electrolyte solution is not particularly limited as long as it is a solvent that can dissolve the polymer electrolyte, and water, a water / alcohol mixed solvent, etc. are selected according to the type of polymer electrolyte. There is also no limitation on the concentration of the polymer electrolyte solution, and it can be selected in the range of 5 to 30%. Effect of the Invention
[0026] According to the present invention, it is possible to provide a laminate in which a polymer electrolyte membrane and a substrate are firmly bonded. The laminate of the present invention is applicable to a membrane-catalyst layer composite, a membrane-subgasket composite, and a membrane-electrode assembly of a fuel cell or a water electrolysis device, and is applicable to a wide range of fields requiring the immobilization of an electrolyte membrane. EXAMPLES
[0027] The present invention will be described in more detail below based on examples, but the present invention is not limited to these examples.
[0028] Example 1 Introduction of carboxyl groups onto the substrate surface A 1 mm thick polypropylene (hereinafter abbreviated as PP) sheet was cut to 50 mm x 50 mm and placed in a pressure vessel. Oxygen gas at 82 kPa and fluorine gas at 8 kPa were introduced into the pressure vessel and held for 1 hour. The vessel was then purged with nitrogen gas, and the PP sheet was removed and immersed in water at room temperature for 30 minutes to introduce carboxyl groups onto the PP sheet surface. The amount of carboxyl groups introduced (relative value) was measured by attenuated total reflection (ATR), an infrared spectroscopy (IR) measurement, at 1710 cm -1 The carbonyl absorption (absorption of the introduced carboxyl group) was measured at 1460cm -1 The absorbance ratio of the carbonyl obtained was 0.6, and it was confirmed that many carboxyl groups were introduced onto the surface of the PP sheet.
[0029] Formation of polydopamine layer The PP sheet with carboxyl groups introduced obtained above was cut into strips of 10 mm x 50 mm and immersed in an aqueous dopamine solution (dopamine concentration 1.6 mg / ml, pH adjusted to 8 with Tris-HCl). After immersion for 24 hours at room temperature with the top of the container open and the aqueous dopamine solution in free contact with air, the PP sheet was removed, washed with water, and then dried. The PP sheet was colored blackish brown, confirming the formation of a polydopamine layer.
[0030] Lamination of substrate and electrolyte membrane A 1 cm Nafion solution (DE2020, Nafion concentration 20%, DuPont) was applied to the edge of the PP sheet on which the polydopamine layer was formed. 2 Immediately after coating, a Nafion (registered trademark) membrane (NR212, thickness 51 μm, DuPont, cut into strips of 10 mm × 50 mm) which is a tetrafluoroethylene / perfluoro[2-(hydroxysulfonylethoxy)propyl vinyl ether] copolymer was laminated on the Nafion solution coating portion as a polymer electrolyte membrane, and the solution was held for 1 hour with a load of 1 kg applied. After 1 hour, the load was removed, and the solution was dried under nitrogen to obtain a laminate.
[0031] Adhesive strength measurement The tensile shear adhesive strength of the above laminate was measured. Measurements were performed with a chuck distance of 20 mm and a tensile speed of 1 mm / min, and the tensile shear adhesive strength and tensile breaking elongation were calculated from the average values of six specimens. The results are shown in Table 1. The tensile shear adhesive strength was 0.09 MPa, and the tensile breaking elongation was 99%, indicating that the PP sheet and the Nafion membrane were firmly bonded. In all six specimens, no peeling was observed at the adhesive interface of the laminate, and the failure was due to cohesive failure of the Nafion membrane.
[0032] Example 2 A laminate was prepared in the same manner as in Example 1, except that the partial pressure of fluorine gas introduction was changed to 5 kPa in the introduction of carboxyl groups to the substrate surface. The results are shown in Table 1. The adhesive shear strength was 0.10 MPa, the tensile breaking elongation was 97%, and the PP sheet and the Nafion membrane were firmly bonded. In all six specimens, no peeling was observed at the adhesive interface of the laminate, and the failure was a cohesive failure of the Nafion membrane.
[0033] Comparative Example 1 Except for not using fluorine gas in the introduction reaction of carboxyl groups onto the PP sheet surface and not forming a polydopamine layer, the PP sheet and the Nafion membrane were laminated in the same manner as in Example 1. The PP sheet and the Nafion membrane did not bond at all, and the adhesive strength could not be measured.
[0034] Comparative Example 2 Except for not using fluorine gas in the reaction for introducing carboxyl groups onto the surface of the PP sheet, lamination of the PP sheet and the Nafion membrane was carried out in the same manner as in Example 1. Although the Nafion membrane on the PP sheet maintained the laminated state under load, it peeled off during drying, and a laminate could not be obtained.
[0035] [Table 1] [Industrial Applicability]
[0036] The laminate of the present invention is a laminate in which a polymer electrolyte membrane and a substrate are firmly bonded, and can be applied to membrane-catalyst layer assemblies, membrane-subgasket assemblies, and membrane-electrode assemblies in fuel cells and water electrolysis devices, and can be applied in a wide range of fields where fixation of an electrolyte membrane is required.
Claims
1. A laminate in which a polymer electrolyte membrane and a substrate are laminated via an adhesive layer, the adhesive layer being made of polydopamine; A laminate comprising a substrate made of polyolefin, a substrate surface having a carboxyl group as an acidic functional group, and a relative absorbance ratio of the C=O stretching of the carboxyl group at 1700 cm -1 normalized by the absorption of the CH bending angle at 1450 cm -1 of 0.1 to 0.
7.
2. A method for producing a laminate, comprising at least the following steps 1 to 3: Step 1: A step of introducing acidic functional groups onto the substrate surface. Step 2: A step of forming a polydopamine layer on the surface of the substrate. Step 3: A step of applying a polymer electrolyte solution to at least one of the substrate surface and the polymer electrolyte membrane surface, and then laminating the two together.
Citation Information
Patent Citations
Adhesive for fuel cell
JP2008112639A
Method of adhesion of polyacetal resin molding, surface-modified polyacetal resin molding and complex molding
JP2010144155A
Adhesive for fuel cell and membrane electrode assembly using this
JP2010205493A
Surface-decorated base material and polymer-coated base material
JP2010261001A
Separation material and column
JP2018173306A