Magnetoresistance element and manufacturing method
By using a multilayer structure of ferromagnetic materials with negligible AMR effects and non-magnetic layers, the free layer in GMR elements achieves robust shape anisotropy and minimizes AMR interference, improving the accuracy of magnetic multiturn sensors.
Patent Information
- Application Number
- JP2021087703
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-05-11
- Filing Date
- 2021-05-25
- Publication Date
- 2024-10-08
- Estimated Expiration
- 2041-05-25
AI Technical Summary
Magnetic multiturn sensors using giant magnetoresistive (GMR) elements face issues due to strong anisotropic magnetoresistive (AMR) effects in the free layer, which distort the sensor output by making electrical resistance dependent on the angle between current flow and magnetization, especially when the free layer is thick for shape anisotropy.
The free layer is composed of multiple alternating layers of ferromagnetic materials with negligible AMR effects and layers of materials that do not interfere with the GMR effect, ensuring sufficient thickness for shape anisotropy without significant AMR effects, using materials like CoFeB, CoZrTa, and NiFe for the ferromagnetic layers and non-magnetic materials like Ta or Ru.
This configuration provides strong shape anisotropy while minimizing AMR effects, resulting in accurate resistance changes due to GMR effects, enhancing the sensor's output reliability.
Smart Images

Figure 0007564058000001 
Figure 0007564058000002 
Figure 0007564058000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to magnetic sensors, and more particularly to giant magnetoresistance elements for use in magnetic multi-turn sensors. [Background technology]
[0002] Magnetic multi-turn sensors are commonly used in applications where it is necessary to monitor the number of times a device has been turned. One example is a vehicle steering wheel. Magnetic multi-turn sensors typically contain a giant magnetoresistance (GMR) element that is sensitive to an applied external magnetic field. The resistance of the GMR element can be changed by rotating a magnetic field within the vicinity of the sensor. The variation in the resistance of the GMR element can be tracked to determine the number of turns in the magnetic field, which can be translated into the number of turns in the device being monitored.
[0003] GMR elements are often based on GMR spin-valve stacks using artificial antiferromagnetic (AAF) materials, such as stack 1 shown in FIG. 1. Stack 1 includes a substrate 100 at the base, followed by a seed layer 102 to facilitate the growth of subsequent layers by providing a smooth surface and favorable crystal structure to be grown thereon. The next layer is the AAF multilayer 104, which includes a sequence of layers consisting of a natural antiferromagnetic layer (such as platinum manganese (PtMn) or iridium manganese (IrMn)), a ferromagnetic layer (typically cobalt iron (CoFe)), a non-magnetic spacer (ruthenium (Ru)), and another ferromagnetic layer (CoFe), also referred to as the "pinned" layer. The main purpose of the AAF layer 104 is to align and maintain the magnetization of the pinned layer in an orientation that was established by an annealing process during fabrication.
[0004] A non-magnetic spacer layer 106 (typically copper (Cu)) is provided directly on the pinned layer of the AAF layer 104, followed by the so-called free layer 108. The free layer 108 is a ferromagnetic layer that is free to align its magnetization with an external magnetic field. The free layer 108 is typically formed of two ferromagnetic layers, typically a CoFe layer followed by a Nickel Iron (NiFe) layer. The GMR effect is observed as a change in film resistance associated with the relative angle between the magnetization of the free layer 108 and the magnetization of the pinned layer of the AAF layer 104. When the magnetizations are parallel, a low resistance is observed, and when they are antiparallel, a high resistance is observed. The purpose of the non-magnetic layer 106 is therefore to create a distance between the free layer 108 and the pinned layer, and the thickness of this spacer layer 106 is selected such that the magnetic coupling between the pinned layer and the free layer 108 is minimized.
[0005] The stack 1 is then typically covered with a capping layer 110, typically a non-magnetic metal layer, which protects the stack 1 and reduces diffusion when connecting the stack 1 to other metal layers (such as aluminum, copper, or gold) to provide interconnects for connecting the stack 1 to other components of the magnetic sensor. Summary of the Invention [Means for solving the problem]
[0006] The present disclosure provides a giant magnetoresistance (GMR) element for use in a magnetic multi-turn sensor, where the free layer, i.e., the layer that changes its magnetization direction in response to an external magnetic field to produce a resistance change, is thick enough to provide good shape anisotropy without exhibiting the AMR effect. To achieve this, at least a portion of the free layer includes layers of at least two different conductive materials, specifically layers of at least a first material that is ferromagnetic, and layers of at least a second material that is known not to exhibit the AMR effect and that does not interfere with the GMR effect of the layers of ferromagnetic material.
[0007] A first aspect of the disclosure provides a giant magnetoresistance (GMR) element for a magnetic multi-turn sensor according to the first aspect, the giant magnetoresistance element comprising a reference layer, a non-magnetic layer adjacent to the reference layer, and a free layer of ferromagnetic material, the free layer comprising a multi-layer arrangement including at least a first layer of ferromagnetic material adjacent to the non-magnetic layer, and multiple layers of a first material and multiple layers of a second material, the first material being ferromagnetic.
[0008] Preferably, the second material is a material that has negligible or nearly negligible anisotropic magnetoresistance (AMR) effect.The layers of the first material and the layers of the second material may then be arranged in an alternating configuration.
[0009] Thus, by having layers of two different materials, where one of the materials is ferromagnetic and the other exhibits negligible or nearly negligible AMR effect, the free layer is thick enough to provide good shape anisotropy while exhibiting no AMR effect or very little AMR effect relative to the amount of GMR effect exhibited. In this regard, the layer of material exhibiting negligible AMR effect will dampen any AMR effect that may be present in the layer of ferromagnetic material.
[0010] In some arrangements, the first material may be one of NiFe and CoFe, and the second material may be one of CoFeB, CoZrTa, CoZrTaB, CoZrNb, and CoZrO.
[0011] In some arrangements, the thicknesses and / or compositions of the first and second materials may be configured such that the free layer is magnetostrictive-free, i.e., such that the free layer is free of mechanical strain or deformation as the magnetization changes.
[0012] Each of the layers of the first material and the layers of the second material may have a thickness of about 0.5 nm to about 8 nm, and it will be appreciated that any suitable number of layers may be used depending on the desired thickness of the free layer and the thickness of the individual layers.
[0013] It will be appreciated that the free layer is so referred to in that at least a first layer of ferromagnetic material has a magnetization that is free to align with an externally applied magnetic field, which may be CoFe, or any other suitable ferromagnetic material that has strong GMR properties.
[0014] It will also be understood that the reference layer is so named in that at least a portion of the reference layer has a magnetization that is in a fixed direction. The portion of the reference layer that has a fixed magnetization direction may be referred to as a "pinned" layer, the pinned layer being a layer of ferromagnetic material. The GMR effect is observed as a change in film resistance associated with the relative angle between the magnetization of the free layer and the magnetization of the pinned layer. The reference layer may include a series of layers that define an artificial antiferromagnetic material, the layer of artificial antiferromagnetic material having a magnetization in a fixed direction. The artificial antiferromagnetic material may include a natural antiferromagnetic layer, a first ferromagnetic layer, a non-magnetic spacer, and a second ferromagnetic layer, the second ferromagnetic layer being the pinned layer.
[0015] In other arrangements disclosed herein, the second material may be a non-magnetic material. As before, the ferromagnetic material may be one of NiFe and CoFe, while the non-magnetic material may be one of Ta, Ru, and Cu.
[0016] In such cases, each of the multiple layers of ferromagnetic material and the multiple layers of non-magnetic material may have a thickness of about 0.2 nm to about 0.4 nm.
[0017] Another arrangement described herein provides a magnetoresistive element for a magnetic multi-turn sensor, the magnetoresistive element comprising a reference layer of antiferromagnetic material, a non-magnetic layer adjacent to the reference layer, and a free layer of ferromagnetic material, the free layer comprising a first layer of ferromagnetic material adjacent to the non-magnetic layer, and a second layer of amorphous ferromagnetic material.
[0018] The amorphous ferromagnetic material may be one of CoFeB, CoZrTa, CoZrTaB, CoZrNb, and CoZrO, while the first layer may include a crystalline ferromagnetic material. For example, the first layer of ferromagnetic material may be CoFe.
[0019] A further aspect of the present disclosure provides a magnetic multi-turn sensor comprising one or more giant magnetoresistance elements, each giant magnetoresistance element comprising a reference layer, a non-magnetic layer adjacent to the reference layer, and a free layer of ferromagnetic material, the free layer comprising a multi-layer arrangement including at least a first layer of ferromagnetic material adjacent to the non-magnetic layer, as well as multiple layers of the first material and multiple layers of a second material, where the first material is ferromagnetic.
[0020] As noted above, the second material is preferably a material having negligible or nearly negligible anisotropic magnetoresistance (AMR) effect. In some arrangements, the first material may be one of NiFe and CoFe. The second material may be one of CoFeB, CoZrTa, CoZrTaB, CoZrNb, and CoZrO.
[0021] A still further aspect provides a method for manufacturing a giant magnetoresistive element, comprising forming a reference layer, forming a nonmagnetic layer adjacent to the reference layer, and forming a free layer of ferromagnetic material, the free layer comprising a multi-layer arrangement including at least a first layer of ferromagnetic material adjacent to the nonmagnetic layer, as well as multiple layers of the first ferromagnetic material and multiple layers of a second material, the first material being ferromagnetic.
[0022] The method may include forming multiple layers of a first material and multiple layers of a second material in an alternating sequence to provide a multi-layer arrangement of the free layer.
[0023] For example, a method may include forming a first layer of a first material, forming a first layer of a second material on the first layer of the first material, forming a second layer of the first material on the first layer of the second material, and forming a second layer of the second material on the second layer of the first material, It will of course be understood that this process may be continued for as many layers as necessary.
[0024] Again, the second material is preferably a material that has negligible or nearly negligible anisotropic magnetoresistance (AMR) effect when alternating with a layer of ferromagnetic material, such that any AMR effect present in the layer of ferromagnetic material is attenuated.
[0025] Forming the reference layer may include forming a plurality of layers to provide an artificial antiferromagnetic material. The artificial antiferromagnetic material may include a natural antiferromagnetic layer, a first ferromagnetic layer, a non-magnetic spacer, and a second ferromagnetic layer, the second ferromagnetic layer being a layer having a magnetization in a fixed direction.
[0026] The method may further include providing a substrate and forming an antiferromagnetic material or free layer on the substrate such that a GMR stack is formed with the reference layer disposed at the bottom or top of the stack.
[0027] It will also be understood that the stack may include other layers, such as a seed layer formed on the substrate to facilitate the growth of subsequent layers, and a capping layer to protect the stack and provide interconnections to other components of the magnetic multi-turn sensor.
[0028] Any of the above-mentioned layers may be formed using any suitable fabrication process, such as sputtering or ion beam deposition.
[0029] The present disclosure will now be described, by way of example only, with reference to the accompanying drawings. [Brief description of the drawings]
[0030] [Figure 1] FIG. 1 is a schematic side view of a GMR stack according to the prior art. [Diagram 2] FIG. 2 is a schematic side view of a GMR stack according to an embodiment of the present disclosure. [Diagram 3] FIG. 13 is a schematic side view of a GMR stack according to a further embodiment of the present disclosure. [Figure 4] 1 is an example of a magnetic multi-turn system including a GMR element according to an embodiment of the present disclosure. [Figure 5A] 1A-1C are schematic side views illustrating a method of manufacturing a GMR stack according to an embodiment of the present disclosure. [Figure 5B] 1A-1C are schematic side views illustrating a method of manufacturing a GMR stack according to an embodiment of the present disclosure. [Figure 5C] 1A-1C are schematic side views illustrating a method of manufacturing a GMR stack according to an embodiment of the present disclosure. [Figure 5D] 1A-1C are schematic side views illustrating a method of manufacturing a GMR stack according to an embodiment of the present disclosure. [Figure 5E] 1A-1C are schematic side views illustrating a method of manufacturing a GMR stack according to an embodiment of the present disclosure. [Figure 5F] 1A-1C are schematic side views illustrating a method of manufacturing a GMR stack according to an embodiment of the present disclosure. [Figure 5G] 1A-1C are schematic side views illustrating a method of manufacturing a GMR stack according to an embodiment of the present disclosure. [Figure 5H] 1A-1C are schematic side views illustrating a method of manufacturing a GMR stack according to an embodiment of the present disclosure. [Figure 5I] 1A-1C are schematic side views illustrating a method of manufacturing a GMR stack according to an embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0031] Magnetic multi-turn sensors can be used to monitor the turn count of a rotating shaft. To do this, a magnet is typically attached to the end of the rotating shaft, and the multi-turn sensor senses the rotation of the magnetic field as the magnet rotates with the shaft. Such magnetic sensing can be applied to a variety of different applications, such as automotive applications, medical applications, industrial control applications, consumer applications, and a host of other applications that require information about the position of a rotating component.
[0032] Magnetic multi-turn sensors typically include a giant magnetoresistance (GMR) element that is sensitive to an applied external magnetic field. GMR elements are often based on a GMR spin-valve stack that includes a free layer of ferromagnetic material that is free to align its magnetization with the external magnetic field. In a typical GMR stack, the thickness of the free layer is usually less than 5 nm. However, to create strong shape anisotropy in long, narrow traces of the film, the free layer must be very thick (>30 nm). This thickness results in a strong anisotropic magnetoresistance (AMR) effect being exhibited in the free layer, which makes the electrical resistance more dependent on the angle between the direction of the current and the direction of the magnetization. In general, a higher resistance is observed when the current is parallel to the magnetization, and a lower resistance is observed when the current is perpendicular to the magnetization. This results in an undesired resistance change superimposed on the desired resistance change due to the GMR effect, thereby distorting the sensor output.
[0033] Thus, the present disclosure provides a giant magnetoresistance (GMR) element for use in a magnetic multi-turn sensor, where the free layer, i.e., the layer that changes its magnetization direction in response to an external magnetic field to produce a resistance change, is thick enough to provide good shape anisotropy while exhibiting no AMR effect or a very small AMR effect relative to the amount of GMR effect exhibited (less than 10%). To achieve this, at least a portion of the free layer includes layers of at least two different materials, specifically layers of at least a first material that is ferromagnetic and layers of at least a second material that are known not to exhibit the AMR effect and that do not interfere with the GMR effect of the layers of ferromagnetic material.
[0034] One embodiment according to the present disclosure is shown in Figure 2. As described with reference to Figure 1, the GMR element is configured as a spin valve stack 2 including a substrate 200, a seed layer 202, an AAF layer 204, and a non-magnetic spacer layer 206. The free layer, designated 208, includes a first ferromagnetic layer 212, preferably a crystalline ferromagnetic material with low AMR effect such as CoFe, followed by a multi-layer arrangement 214. As described above, the GMR effect is observed at the interface of the pinned layer of the AAF layer 204, the non-magnetic spacer layer 206, and the first ferromagnetic layer 212. The multi-layer arrangement 214 includes multiple layers of both crystalline ferromagnetic material 216 and amorphous ferromagnetic material 218 arranged in alternating layers. The crystalline ferromagnetic layer 216 is formed of a crystalline ferromagnetic material such as NiFe, while the amorphous ferromagnetic layer 218 may be formed of any suitable amorphous ferromagnetic material such as cobalt iron boron (CoFeB), cobalt zirconium tantalum (CoZrTa), cobalt zirconium tantalum boron (CoZrTaB), cobalt zirconium niobium (CoZrNb), or cobalt zirconium oxide (CoZrO). Because the magnetization of the amorphous ferromagnetic layer 218 also aligns with the externally applied magnetic field, the multilayer arrangement 214 functions as a single ferromagnetic layer that aligns with the external magnetic field, thus providing good shape anisotropy. However, in amorphous ferromagnetic materials, there is little effect on the current as a result of the change in magnetization direction, and the layers of crystalline ferromagnetic material 216 are individually too thin to exhibit any AMR effect, or at least exhibit a negligible or very small amount of AMR effect, so no AMR effect or a very small AMR effect is observed. Thus, by interspersing layers of crystalline ferromagnetic material 216 with layers of amorphous ferromagnetic material 218, a ferromagnetic multilayer arrangement 214 is provided that is thick enough to provide the desired shape anisotropy without inducing any undesirable AMR effect. In fact, one skilled in the art will appreciate that the ferromagnetic multilayer arrangement 214 may include layers of any two ferromagnetic materials, at least one of which exhibits a negligible or nearly negligible amount of the AMR effect, thereby damping any ARM effect exhibited by the other ferromagnetic material.
[0035] The individual layers 216, 218 of the multi-layer arrangement 214 may be from about 0.5 nm to about 8 nm, with the total thickness of the free layer 208 being approximately 10 nm to 50 nm.
[0036] The resulting magnetostriction experienced by the multi-layer arrangement 214 may also need to be considered when selecting the thicknesses, as well as compositions, of the layers 216, 218. Magnetostriction is the relationship between mechanical stress and magnetization of a material. This relationship works in both directions, in that a change in magnetization results in mechanical strain or deformation, and a mechanical deformation results in a magnetization change. Magnetostriction measurements may have a positive or negative sign, depending on whether the material expands or contracts when magnetized in a particular direction.
[0037] For sensor applications, very low or ideally zero magnetostriction is required. Some crystalline ferromagnetic materials, such as NiFe, have very low magnetostriction. For example, NiFe with a Ni:Fe ratio of 81:19 has no magnetostriction. Therefore, such materials are typically preferred for providing a free layer in a GMR sensor. On the other hand, other crystalline ferromagnetic materials, such as CoFe, and amorphous ferromagnetic materials, such as CoFeB, have significant magnetostriction. Therefore, for a multilayer arrangement 214 including an amorphous ferromagnetic material 218 with positive magnetostriction, the thickness and composition of the layer of crystalline ferromagnetic material 216 needs to be adapted to have negative magnetostriction to compensate for the positive magnetostriction of the other layers, which may result in an entirely magnetostriction-free free layer 208.
[0038] The stack 2 is then typically covered with a capping layer 210, typically a non-magnetic metal layer such as tantalum (Ta) or titanium tungsten (TiW), which protects the stack 2 and reduces diffusion when connecting the stack 2 to other metal layers (e.g., aluminum, copper, or gold) to provide interconnects for connecting the stack 2 to other components of the magnetic sensor.
[0039] A further embodiment according to the present disclosure is also shown in FIG. 3. As before, the GMR element is configured as a spin valve stack 3 including a substrate 300, a seed layer 302, an AAF layer 304, and a non-magnetic spacer layer 306. The free layer, generally designated 308, includes a first ferromagnetic layer 312, preferably a crystalline ferromagnetic material with a low AMR effect such as CoFe, followed by another multi-layer arrangement 314. In this embodiment, the multi-layer arrangement 314 is formed of a number of ferromagnetic layers 316, again formed of a soft magnetic material such as NiFe, and a number of non-magnetic layers 318, again arranged as alternating layers. The non-magnetic material layers 318 may be any suitable material, for example Ta, Ru, or Cu. The non-magnetic layers 318 do not add any magnetic moment to the free layer 308 and therefore do not exhibit any AMR effect, while the ferromagnetic 316 layers are individually too thin to exhibit any AMR effect, or at least exhibit negligible or very small amounts. Thus, interspersed with layers of ferromagnetic material 316 and layers of non-magnetic material 318 provides a ferromagnetic multi-layer arrangement 314 that is thick enough to provide the desired shape anisotropy without inducing any undesirable AMR effects.
[0040] In such an arrangement, it is important that the ferromagnetic layers 316 are thin enough so as not to produce any AMR effects, and the non-magnetic layers 318 are thin enough to ensure strong ferromagnetic coupling between the ferromagnetic layers, i.e., so that the shape anisotropy exhibited by the multi-layer arrangement 314 corresponds to the sum of the ferromagnetic layers 316 as opposed to each individual ferromagnetic layer 316. For example, the thickness of both sets of layers 316, 318 may be about 0.2 nm to 0.4 nm.
[0041] Additionally, as mentioned above, the ferromagnetic layers 316 may be formed from soft magnetic materials that have very low or zero magnetostriction, such as NiFe. These ferromagnetic materials 316 are interspersed with non-magnetic layers 318, so that the free layer 308 is an entirely soft magnet with no magnetostriction.
[0042] The stack 3 is then typically covered with a capping layer 210, typically a non-magnetic metal layer, which protects the stack 3 and reduces diffusion when connecting the stack 3 to other metal layers (e.g., aluminum, copper, or gold) to provide interconnects for connecting the stack 3 to other components of the magnetic sensor.
[0043] In any of the above described embodiments, it will be understood that any number of layers (and layer thicknesses) may be used in the multi-layer arrangement 214, 314 depending on the thickness and shape anisotropy required. For example, there may be a total of four layers, or there may be as many as a total of 20 layers.
[0044] In addition, it will be appreciated that in any of the above-described embodiments, a natural antiferromagnetic layer, such as platinum manganese (PtMn), may be used in place of the AAF layer 204, 304 where a measurable GMR effect is also observed.
[0045] FIG. 4 illustrates an example of a magnetic strip layout representation of a magnetic multi-turn sensor 4 comprising multiple GMR elements 400 according to an embodiment of the present disclosure. In the example of FIG. 4, the magnetic strip 400 is a giant magnetoresistance track physically laid down in a spiral configuration. Thus, the magnetic strip 400 has multiple segments formed from magnetoresistance elements 402 arranged in series with one another. The magnetoresistance elements 402 function as variable resistors that change resistance depending on the magnetic alignment state. One end of the magnetic strip 400 is coupled to a domain wall generator (DWG) 404. In this regard, it will be understood that the DWG 404 may be coupled to either end of the magnetic strip 400. The DWG 404 generates domain walls in response to rotation in an external magnetic field or application of some other strong external magnetic field beyond the operating magnetic window of the sensor 4. These domain walls can then be injected into the magnetic strip 400. As the magnetic domain position changes, the resistance of the GMR element 402 also changes due to the resulting change in magnetic alignment.
[0046] To measure the resistance of the GMR element 402, which changes as the domain walls are created, the magnetic piece 400 is electrically connected to a supply voltage VDD 406 and ground GND 408 to apply a voltage between a pair of opposing corners. At the corner midway between the voltage supplies, an electrical connection 410 is provided to provide a half-bridge output. Thus, the multi-turn sensor 4 comprises multiple Wheatstone bridge circuits, with each half-bridge 410 corresponding to one half-turn or 180° rotation of the external magnetic field. Measurements of the voltage at the electrical connections 410 can then be used to measure the change in resistance of the GMR element 402, which is indicative of a change in the magnetic alignment of the free layer.
[0047] The example shown by FIG. 4 comprises eight half bridges 410 with four spiral windings, and is therefore configured to count four turns of an external magnetic field. However, it will be understood that a multi-turn sensor may have any number of spiral windings depending on the number of GMR elements. In general, a multi-turn sensor can count the same number of turns as there are spiral windings. It will also be understood that the GMR elements 402 may be electrically connected in any suitable manner to provide a sensor output representative of a change in magnetic alignment state. For example, the GMR elements 402 may be connected in a matrix arrangement as described in US2017 / 0261345, the entirety of which is incorporated by reference herein. As a further alternative, each magnetoresistance segment may be individually connected, rather than in a bridge arrangement.
[0048] In this example, the magnetic multi-turn sensor 4 comprises an integrated circuit 412 in which the magnetic strips 400 are disposed, which may include processing circuitry (not shown) for processing the sensor output.
[0049] 5A to 5I, a method of fabricating the GMR stack 2 will now be described, however, it will be understood that the GMR stack 3 may be similarly fabricated.
[0050] FIG. 5A shows the first step of the fabrication process. A silicon wafer is used as the substrate 200. Below, the process of forming one device is described, but hundreds of devices may be formed in parallel on the same wafer. The substrate 200 is used for mechanical support and can be replaced with another type of material such as glass or sapphire. Typically, the silicon wafer is oxidized to isolate subsequent layers from the bare silicon, or an isolator such as aluminum oxide may be used. In some arrangements, the substrate 200 may comprise electronic circuitry.
[0051] Next, as shown in Figure 5B, a seed layer 202 is deposited on the substrate 200. The seed layer 202 provides a smooth surface and a favorable crystal structure to promote the growth of subsequent layers. The seed layer 202 may be a layer of tantalum, ruthenium, or tantalum nitride (TaN), or may include additional layers of other compounds.
[0052] FIG. 5C illustrates the formation of an AAF layer 204 deposited on the seed layer 202. The AAF layer 204 is formed by first depositing a natural antiferromagnetic layer on the seed layer 202. A ferromagnetic layer is then deposited on the antiferromagnetic layer, followed by a nonmagnetic spacer layer. Finally, a second ferromagnetic layer is deposited on the nonmagnetic layer. This second ferromagnetic layer is the so-called "pinned" or "reference" layer. The antiferromagnetic material used in the AAF layer 204 may be PtMn, IrMn, NiMn, or some other suitable antiferromagnetic material, and the ferromagnetic material may be CoFe or some other suitable ferromagnetic material, where the nonmagnetic material is typically ruthenium.
[0053] As shown in Figure 5D, a non-magnetic spacer layer 206 is formed on the pinner layer of the AAF layer 204. It acts as a spacer between the pinned layer and the subsequent free layer to reduce any magnetic coupling.
[0054] FIG. 5E shows the beginning of the free layer formed by first depositing the first ferromagnetic layer 212 .
[0055] The multi-layer arrangement is then built up on the first ferromagnetic layer by depositing a layer of crystalline ferromagnetic material 216 as shown in Figure 5F, followed by a layer of amorphous ferromagnetic material 218 as shown in Figure 5G. This process is repeated as many times as necessary until the entire multi-layer arrangement 214 is formed, as shown in Figure 5H.
[0056] Finally, a capping layer 210 is placed over the stack 2, as shown in Figure 5I. As mentioned above, the capping layer 210 typically consists of a non-magnetic metal layer that protects the stack 2 and reduces diffusion when connecting the stack 2 to other metal layers to provide interconnects.
[0057] Once deposited, the GMR film can then be annealed in a magnetic field and patterned using standard photolithography techniques and subsequent ion milling to remove excess material and form the required resistor shape.
[0058] It will be appreciated that in the embodiment of FIG. 3, stack 3 may be processed in substantially the same manner, with ferromagnetic layer 316 and non-magnetic layer 318 of multi-layer arrangement 314 formed in substantially the same manner as shown in FIGS. 5F-5H.
[0059] It will be appreciated that each of the layers in the stacks 2, 3 described above may be formed using any suitable physical vapor deposition method, such as sputtering. Similarly, the deposition of each stack 2, 3 may be performed in one vacuum step, such that there is no exposure to the ambient atmosphere between the individual steps, thereby avoiding contamination or oxidation of the various layers. For example, the entire stack 2, 3, from the seed layer 202, 302 to the capping layer 210, 310, is deposited by either sputtering or ion beam deposition in one tool, without breaking the vacuum between the different layers to prevent surface contamination or changes due to exposure to atmospheric gases.
[0060] In a further embodiment of the present disclosure, a GMR stack may be provided in which the free layer includes a first layer of a crystalline ferromagnetic material with a low AMR effect, such as CoFe, and a second layer of an amorphous ferromagnetic material, such as CoFeB. Such an arrangement precludes the use of any ferromagnetic material that exhibits a high AMR effect, but also experiences more magnetostriction.
[0061] Although the above arrangement shows the AAF layers 204, 304 at the bottom of the stacks 2, 3 (so-called "bottom pinned"), it will be understood that the stacks 2, 3 may alternatively be arranged such that the non-magnetic spacers 206, 306 and then the free layers 208, 308 are at the bottom and the AAF layers 204, 304 (so-called "top pinned") are at the top of the stacks 2, 3.
[0062] Similarly, while the above arrangement describes the use of an AAF layer 204, it will be appreciated that a simple antiferromagnetic layer may instead be used, including, for example, a layer of an antiferromagnetic material such as PtMn, IrMn, NiMn, etc., and a layer of a ferromagnetic material such as CoFe that acts as a "pinned" layer.
[0063] Purpose Any of the principles and advantages discussed herein may be applied to other systems, not just the system described above. Some embodiments may include a subset of the features and / or advantages described herein. Elements and acts of the various embodiments described above may be combined to provide further embodiments. The method actions discussed herein may be performed in any order, as appropriate. Furthermore, the method actions discussed herein may be performed sequentially or in parallel, as appropriate. Although circuits are shown in a particular arrangement, other equivalent arrangements are possible.
[0064] Any of the principles and advantages discussed herein may be implemented in connection with any other system, apparatus, or method that may benefit from any of the teachings herein. For example, any of the principles and advantages described herein may be implemented in connection with any device that has a need to correct rotational angular position data derived from a rotating magnetic field. Additionally, the device may include any magnetoresistance or Hall effect device that can sense a magnetic field.
[0065] Aspects of the present disclosure may be implemented in a variety of electronic devices or systems. For example, phase correction methods and sensors implemented according to any of the principles and advantages discussed herein may be included in a variety of electronic devices and / or applications. Examples of electronic devices and applications may include, but are not limited to, servos, robotics, aircraft, submarines, toothbrushes, biomedical sensing devices, and components of consumer electronic products such as semiconductor dies and / or packaged modules, electronic test equipment, etc. Additionally, electronic devices may include unfinished products, including those for industrial, automotive, and / or medical applications.
[0066] Unless the context clearly requires otherwise, words such as "comprises," "comprising," "includes," "including," and the like, throughout the description and claims, should be interpreted in an inclusive sense, i.e., "including, but not limited to," and not in an exclusive or exhaustive sense. As generally used herein, words such as "coupled" or "connected" refer to two or more elements that may be directly connected or connected through one or more intermediate elements. Thus, while the various schematic diagrams shown in the figures show example arrangements of elements and components, additional intervening elements, devices, features, or components may be present in an actual embodiment (assuming the functionality of the circuitry shown is not adversely affected). As used herein, words such as "based on" are generally intended to encompass "based only on" and "based at least in part on." Additionally, when used in this application, words such as "herein," "on," "under," and words of similar import refer to this application as a whole, and not to any particular portions of this application. Where the context permits, words in the Detailed Description using the singular or plural can also include the plural or singular, respectively. Words such as "or" referring to a list of two or more items are intended to cover all interpretations of the following word: any of the items in the list, all of the items in the list, and any combination of the items in the list. All numerical values or distances provided herein are intended to include similar values within measurement error.
[0067] Although specific embodiments have been described, these embodiments are presented by way of example only and are not intended to limit the scope of the disclosure. Indeed, the novel apparatus, systems, and methods described herein may be embodied in a variety of other forms. Furthermore, various omissions, substitutions, and changes in the form of the methods and systems described herein may be made without departing from the spirit of the disclosure. [Explanation of symbols]
[0068] 2, 3 Spin valve stack 200, 300 boards 202, 302 seed layer 204, 304 AAF layers 206, 306 Non-magnetic spacer layer 208, 308 free layer 210, 310 Capping layer 212, 312 First ferromagnetic layer 214, 314 multilayer arrangement 216 Layer of crystalline ferromagnetic material 218 Amorphous Ferromagnetic Material Layer 316 Multiple ferromagnetic layers 318 Multiple non-magnetic layers 4 Magnetic multi-turn sensors 400 GMR element, magnetic piece 402 Magnetoresistance element 404 Domain Wall Generator (DWG) 406 Supply voltage VDD 408 Ground GND410 Half bridge 410 Electrical connections 412 Integrated Circuits
Claims
1. A giant magnetoresistance (GMR) element for a magnetic multi-turn sensor according to a first aspect, comprising: A reference layer; a nonmagnetic layer adjacent to the reference layer; a free layer of ferromagnetic material, the free layer including a multi-layer arrangement including at least a first layer of ferromagnetic material adjacent the non-magnetic layer, and multiple layers of a first material, and multiple layers of a second material, the first material being ferromagnetic; A giant magnetoresistive element, wherein the layers of the first material have a first magnetostriction and the layers of the second material have a second magnetostriction that reduces the magnetostriction of the free layer.
2. The giant magnetoresistive element of claim 1 , wherein the second material is a material having negligible or nearly negligible anisotropic magnetoresistance (AMR) effect.
3. 2. The giant magnetoresistive element of claim 1, wherein said plurality of layers of said first material and said plurality of layers of said second material are arranged in an alternating configuration.
4. The giant magnetoresistive element of claim 1 , wherein the first material is one of NiFe and CoFe.
5. 2. The giant magnetoresistive element of claim 1, wherein the second material is one of CoFeB, CoZrTa, CoZrTaB, CoZrNb, and CoZrO.
6. The giant magnetoresistive element of claim 1 , wherein the thicknesses and / or compositions of the first and second materials are configured such that the free layer is magnetostriction-free.
7. The giant magnetoresistive element of claim 1 , wherein each of said layers of said first material and said layers of said second material has a thickness of about 0.5 nm to about 8 nm.
8. The giant magnetoresistive element of claim 1 , wherein the first layer of ferromagnetic material has a magnetization that is free to align with an externally applied magnetic field.
9. The giant magnetoresistive element of claim 1 wherein said first layer of ferromagnetic material is CoFe.
10. The giant magnetoresistive element of claim 1 , wherein at least a portion of the reference layer has a magnetization that is in a fixed direction.
11. The giant magnetoresistive element of claim 1 , wherein the reference layer includes a series of layers defining an artificial antiferromagnetic material, the layers of artificial antiferromagnetic material having a magnetization that is in a fixed direction.
12. 1. A magnetic multi-turn sensor comprising one or more giant magnetoresistance elements, each of which comprises: A reference layer; a nonmagnetic layer adjacent to the reference layer; a free layer of ferromagnetic material, the free layer including a multi-layer arrangement including at least a first layer of ferromagnetic material adjacent the non-magnetic layer, and multiple layers of a first material, and multiple layers of a second material, the first material being ferromagnetic; 11. A magnetic multi-turn sensor, wherein the layers of the first material have a first magnetostriction and the layers of the second material have a second magnetostriction that reduces the magnetostriction of the free layer.
13. The magnetic multi-turn sensor of claim 12 , wherein the second material is a material having negligible or nearly negligible anisotropic magnetoresistance (AMR) effect.
14. The magnetic multi-turn sensor of claim 12 , wherein the first material is one of NiFe and CoFe.
15. The magnetic multi-turn sensor of claim 12 , wherein the second material is one of CoFeB, CoZrTa, CoZrTaB, CoZrNb, and CoZrO.
16. A method for manufacturing a giant magnetoresistive element, comprising the steps of: forming a reference layer; forming a nonmagnetic layer adjacent to the reference layer; forming a free layer of ferromagnetic material, the free layer comprising a multi-layer arrangement including at least a first layer of ferromagnetic material adjacent the non-magnetic layer, and multiple layers of a first material, and multiple layers of a second material, the first material being ferromagnetic; The method of claim 1, wherein the layers of the first material have a first magnetostriction and the layers of the second material have a second magnetostriction that reduces the magnetostriction of the free layer.
17. 17. The method of claim 16, further comprising forming a plurality of layers of the first material and a plurality of layers of the second material in an alternating sequence to provide the multi-layer arrangement of the free layer.
18. The method of claim 17 , wherein the second material is a material having negligible or nearly negligible anisotropic magnetoresistance (AMR) effect.
19. The method of claim 16 , wherein forming the reference layer comprises forming a plurality of layers to provide an artificial antiferromagnetic material.
20. The method further comprising: Providing a substrate; 20. The method of claim 19, further comprising forming the artificial antiferromagnetic material or the free layer on the substrate.
Citation Information
Patent Citations
Magnetoresistance element
JP2002204010A
Arrangement and reading of multi-turn sensor
JP2017161524A
Magnetoresistive effect element and magnetic recording / reproducing device
WO2011064822A1