Sensor and manufacturing method thereof

A strain sensor using a flexible MLD layer between ALD layers addresses the challenge of monitoring implant strain, ensuring mechanical integrity and safe recovery by detecting distortions and strains on medical implants.

JP7565161B2Active Publication Date: 2024-10-10PICOSUN OY
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2020056917
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-03-29
Filing Date
2020-03-27
Publication Date
2024-10-10
Estimated Expiration
2040-03-27

AI Technical Summary

Technical Problem

Existing medical implants, such as stents and orthopedic screws, face challenges in maintaining mechanical integrity and monitoring strain to prevent restenosis and bone union failure due to inflammatory responses and excessive strain, necessitating a means to monitor distortion and ensure proper biomechanical loading during recovery.

Method used

A strain sensor device comprising a flexible Molecular Layer Deposition (MLD) layer sandwiched between two conductive Atomic Layer Deposition (ALD) layers, forming a deformable capacitor that detects strain through capacitance changes, which can be read externally using an RF signal, allowing monitoring of mechanical forces applied to the implant.

Benefits of technology

Enables continuous monitoring of strain on implants, preventing failure by detecting anomalies early and ensuring safe recovery by providing real-time feedback on mechanical loading.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007565161000001
    Figure 0007565161000001
  • Figure 0007565161000002
    Figure 0007565161000002
  • Figure 0007565161000003
    Figure 0007565161000003
Patent Text Reader

Abstract

To provide a strain sensor for acquiring strain information from a human body.SOLUTION: A strain sensor structure 100 comprises a first atomic layer deposition layer 101 provided on a substrate 110, a flexible molecular layer deposition layer 102 provided on top of the first atomic layer deposition layer 101, and a second atomic layer deposition layer 103 provided on top of the flexible molecular layer deposition layer 102.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates generally to sensors and methods for making the same.

[0002] This section provides useful background information, but is not an admission that any of the technology described herein is prior art.

[0003] Obtaining strain information from the human body is useful in medical applications to obtain the performance of implanted devices without expensive imaging. An example of such an application is a tubular mesh stent, which may or may not be covered with a fabric to maintain flow in the tube and also to maintain fluid leakage from the tube. Further examples include artificial valves for the treatment of cardiovascular disease, screws and nails used in urology and gastroenterology, fixing plates for fracture treatment, or fixation of bone structures (osteosynthesis) in other indications. The greatest challenge is to keep the stent open after insertion to allow unobstructed flow for as long as possible. However, the insertion of a stent can cause an inflammatory response, which can cause restenosis due to the tissue repair response, ultimately resulting in occlusion of the stented area. The most common factor leading to restenosis is twisting or excessive strain of the stent or the stented area. This stresses the stent wall and ultimately causes the mechanical integrity of the stent to be lost. A means of monitoring the strain on the stent allows the integrity of the stent to be monitored, abnormalities to be detected, and action taken before stent failure occurs. For orthopedic screws and nails, it is necessary to be able to monitor the biomechanical loading as the patient heals. Premature loading can lead to poor bone integration and costly revision surgery. The bone integration must be allowed to solidify until the bone has fully healed. A means of monitoring the strain of orthopedic screws and nails allows proper mechanical loading of the repair area to be monitored and patient recovery controlled with maximum safety. Abstract

[0004] Certain embodiments of the present invention are directed to obtaining strain information from the human body.

[0005] According to a first exemplary aspect of the present invention, there is provided a strain sensor device as defined in claim 1 attached hereto.

[0006] Variations of the first aspect are defined in the dependent claims.

[0007] According to a second exemplary aspect of the present invention, there is provided a method for manufacturing a strain sensor device as defined in claim 10 attached hereto.

[0008] According to a further exemplary aspect of the present invention, there is provided a strain sensor comprising: The first layer, a flexible or compressible molecular layer deposition (MLD) layer on the first layer; and a second layer on the MLD layer; Equipped with.

[0009] Embodiments of the present invention may be used, for example, in implantable and biodegradable components.

[0010] In certain embodiments, the first and second layers are electrically conductive or are conductors (or form electrodes).

[0011] In a particular embodiment, the flexible MLD layer is electrically insulating.

[0012] In a particular embodiment, the first and second layers are atomic layer deposition (ALD) layers. Instead of ALD, the first and second layers may be fabricated using other methods.

[0013] In certain embodiments, all three layers at least partially overlap such that deformation of the flexible layer forms an area that affects the capacitance measured between conductive layers (electrodes) that may be formed by ALD.

[0014] In a particular embodiment, the deformable dielectric of the capacitor is provided formed by molecular layer deposition.

[0015] In certain embodiments, the first atomic layer deposition layer is deposited on or attached to a biodegradable substrate, such as a biodegradable screw (e.g., a bone screw) or nail. In other embodiments, the substrate is not biodegradable.

[0016] In certain embodiments, the MLD layer is biodegradable. In other embodiments, the MLD layer is not biodegradable. In certain embodiments, the first layer and the second layer are each biodegradable. In other embodiments, the first layer and the second layer are each not biodegradable.

[0017] In certain embodiments, the strain sensor includes circuitry that provides information indicative of strain, which may indicate compression or force in a given direction or any other direction.

[0018] According to another embodiment of the invention, there is provided a substrate comprising a strain sensor according to any of the aspects of the strain sensor described above or any embodiment thereof.

[0019] According to another aspect of the present invention there is provided a sensor comprising: a molecular layer deposition (MLD) layer between two conductive layers; At least one of the conductive layers has at least one hole through which material can be forced through and absorbed into the MLD layer.

[0020] In certain embodiments, materials adsorbed on the MLD layer change the capacitance or any other electrical property of the capacitor structure.

[0021] According to another aspect of the present invention, there is provided a method of manufacturing a strain sensor, the method comprising the steps of: depositing a capacitor structure comprising conductive layers on either side of the MLD layer; providing a circuit comprising the capacitor structure configured to provide information indicative of distortion; Includes.

[0022] According to another aspect of the invention, there is provided the use of a molecular layer deposition (MLD) layer as a deformable capacitor layer in detection circuitry.

[0023] According to yet another aspect of the present invention, there is provided a method of manufacturing a strain sensor, the method comprising the steps of: depositing a first atomic layer deposition layer on a substrate; depositing a flexible molecular layer deposition layer on the first atomic layer deposition layer; depositing a second atomic layer deposition layer on the molecular layer deposition layer; attaching circuitry to the formed structure configured to provide information indicative of the distortion; Includes.

[0024] In a particular embodiment, the formed structure is a capacitor structure.

[0025] In a particular embodiment, the formed structure is at least in part a resistor structure.

[0026] According to yet another aspect of the invention, there is provided the use of a Molecular Layer Deposition (MLD) layer as a deformable capacitor layer in detection circuitry.

[0027] Various exemplary aspects and embodiments have been illustrated so far, which do not limit the present invention. The above and following embodiments are only used to describe selected aspects or steps that may be utilized in implementing the present invention. It should be understood that the corresponding embodiments can also be applied to other exemplary aspects. These embodiments may be combined in any and appropriate manner. [Brief description of the drawings]

[0028] The invention will now be described, by way of example only, with reference to the accompanying drawings. [Figure 1] FIG. 1 illustrates a strain sensor structure according to a particular embodiment. [Diagram 2] FIG. 2 shows a schematic perspective view of the sensor structure of FIG. [Diagram 3] FIG. 3 shows a detection circuit according to a particular embodiment. [Figure 4] FIG. 4 shows another sensor structure according to a further embodiment. Detailed explanation

[0029] The fundamentals of the growth mechanism of atomic layer deposition (ALD) are known to those skilled in the art. ALD is a specialized chemical deposition method based on the sequential introduction of at least two reactive precursor species to at least one substrate. However, it should be understood that one of these reactive precursors can be replaced with energy, for example when using photon-enhanced ALD or plasma-assisted ALD (e.g., Plasma Enhanced Atomic Layer Deposition (PEALD)), resulting in a single precursor ALD process. For example, for the deposition of a pure element such as a metal, only one precursor is required. Binary compounds such as oxides can also be produced with a single precursor chemical, provided that the precursor chemical contains elements of both materials to be deposited. Thin films grown by ALD are dense, pinhole-free, and have a uniform thickness.

[0030] Thereby, at least one substrate is typically exposed to time-separated precursor pulses in a reaction vessel to deposit material on the substrate surface by sequential self-saturating surface reactions. In the context of this application, the term ALD encompasses all applicable ALD techniques and any equivalent or closely related techniques. Examples include subtypes of ALD such as plasma-assisted ALD (e.g., PEALD), photon-enhanced atomic layer deposition (also known as photo-ALD or flash-enhanced ALD), etc.

[0031] A basic ALD deposition cycle has four steps, Pulse A, Purge A, Pulse B, and Purge B, performed sequentially. Pulse A consists of a first precursor vapor, and Pulse B consists of another precursor vapor. An inert gas and a vacuum pump are typically used to purge gaseous reaction by-products and residual reactant molecules from the reaction space during Purge A and Purge B. A deposition sequence includes at least one deposition cycle. The deposition cycles are repeated until the deposition sequence produces a thin film or coating of the desired thickness. However, deposition cycles can be simpler or more complex. For example, the cycles can include three or more reactant vapor pulses, with intervening purge steps, or certain purge steps can be omitted. On the other hand, light-enhanced ALD has a variety of options, such as only one active precursor, and a variety of purge options. All of these deposition cycles form a timed deposition sequence controlled by a logic unit or microprocessor.

[0032] Molecular layer deposition (MLD) is a deposition technique in which materials are deposited on a substrate surface by sequential self-saturating surface reactions (similar to ALD), except that in MLD, multiple atomic layers of, e.g., polymer chains (e.g., organic polymer chains) are deposited in one cycle.

[0033] 1 shows a strain sensor structure 100 fabricated on a substrate 110. The structure comprises a first ALD layer 101 deposited by ALD on the substrate 110, a flexible MLD layer 102 deposited by MLD on the first ALD layer 101, and a second ALD layer 103 deposited by ALD on the MLD layer 102.

[0034] The first ALD layer 101 and the second ALD layer 103 are electrical conductors (Al2O3, In2O3, ZnO doped with Ru, Pt and / or combinations thereof). The flexible MLD layer 102 is made of a dielectric material, i.e. an electrically insulating material (such as alucone film, titanicone, or zincone). Thus, the structure 100 is a capacitor, i.e. an ALD-MLD-ALD capacitor. In a particular embodiment, it is a capacitor with a (variable) resistance that is or can be affected by mechanical forces or chemical absorption, i.e. an ALD-MLD-ALD capacitor. Another example of a dielectric material is Nb2O5.

[0035] In a particular embodiment, each of the layers 101-103 and the substrate 110 are biodegradable (but in other embodiments they are not, or at least some of them are not). The flexible MLD layer 102 contracts (compresses) when pressure is applied and expands when pressure is released. The capacitance of the capacitor structure changes, and this change is detectable by an external radio frequency signal. For example, an LC or RLC circuit may be formed that can be read externally (or the reflected power is measured). The change in capacitance changes the response of the circuit configuration. Based on the change in capacitance, for example, the strain (or compression) of a (coated) substrate, such as a bone screw, nail, or stent, can be known. This change in capacitance can be caused by various means specific to the capacitor dielectric material(s).

[0036] Figure 2 shows a schematic perspective view of the sensor structure of Figure 1. Figure 2 shows a flexible MLD layer between two conductive layers (Conductor 1 and Conductor 2), which are formed by ALD or another method. All three layers overlap at least partially, forming an area where deformation of the flexible layer affects the capacitance measured between the electrodes (conductive layers). The conductive layers may be provided with electrical conductors (wires or other electrical paths), which are shown by arrows in Figure 2.

[0037] Fig. 3 shows a detection circuit according to a particular embodiment. The detection circuit comprises a capacitor structure (conductor 1 + MLD layer + conductor 2) with an attached resistor (attached to conductor 1) and an antenna (attached to conductor 2 and resistor). In this way, a detection circuit is provided. The antenna may be an inductive element (e.g. an inductor), in which case the circuit is an RLC circuit. The circuit is read externally (or the reflected power is measured). Based on the change in capacitance, the strain of the (coated) substrate, such as a bone screw, nail or stent, can be known. The resistor may be formed by ALD.

[0038] Figure 4 shows another sensor structure according to a further embodiment. The structure shown in Figure 4 corresponds to that of Figure 2, except that one of the conductive layers has hole(s) or opening(s) through which molecules or ions can penetrate and be absorbed into the MLD layer, thereby changing the capacitance of the capacitor, its electrical properties such as its conductivity, etc. (In another embodiment, said one of the conductive layers is porous with a similar effect). In this way the structure can be used, for example, as an ion detector. An RLC circuit can be formed, for example, similar to that of Figure 3.

[0039] To summarize the specific embodiments, these provide an MLD layer for use as a dielectric layer in a (variable) capacitor or variable resistor. The flexibility of the MLD layer allows the capacitor (and / or resistive properties) to be tuned by strain, such as pressure or compression, induced or applied to the layer. In a specific embodiment, the MLD layer is biodegradable. The MLD layer may be made of MLD materials such as, but not limited to, Alcone, Titanicone, and Zincone. The performance and properties of the MLD layer can be modified by doping with other ALD layers and MLD layers or ALD pulses.

[0040] If the implant is conductive, the implant itself will function and can be connected as an antenna.

[0041] In a particular embodiment, the MLD layer is coated with a conductive material to form a capacitor. The conductive materials on both sides of the MLD layer can be formed by known processes, such as conductive biodegradable materials, e.g. Al2O3+ZnO. The resistance value can be adjusted by the ratio between the materials. In addition, a variety of other materials and deposition processes can be used to create the conductor. However, a thin film is preferred to minimize the thickness and the impact on the environment in which it is used.

[0042] Additionally, the MLD layer may be coated with an electrically insulating layer, such as Al2O3, deposited by ALD, having a selected thickness.

[0043] Capacitors can be used as part of well-known RC or RLC circuits in various wireless communication solutions.

[0044] Resistors in RC or RLC circuits can be formed using biodegradable materials by ALD.

[0045] If an antenna with an RC or RLC circuit configuration is present, the antenna can be formed using biodegradable materials by ALD.

[0046] The circuit (or circuitry) is read by an external means, such as an antenna, which generates sufficient RF excitation to generate an internal current in the RC circuitry. This current depends on the change in capacitance C of the capacitor formed by the MLD, which is deformed by the external load, such as by compression, reducing its thickness. The change in behavior of the circuitry may then be measured by external means to obtain a value indicative of, for example, an applied force.

[0047] In some embodiments, the completed assembly can be at least partially coated with a non-biodegradable layer (such as a SiO / HfO stack) formed by ALD or similar methods, or with a layer that takes significantly longer to biodegrade than the sensor structure.

[0048] In certain embodiments, the capacitance and / or resistance changes with the degree of absorption of molecules or ions into the MLD layer. This absorption is enabled by a surrounding (or adjacent) layer. The surrounding layer (which may be formed by ALD) may be a permeable detectable material or may be patterned with holes that allow the material to permeate as described above. This permeation may be by ion exchange. The openings described above may be further coated with a material that influences the permeation of the absorbing species.

[0049] Advantages of certain embodiments include that the shape of the bioimplant used can be used to measure the forces induced therein, and in some cases, for example the bioimplant screw can be degradable, and it would be advantageous if the implanted sensor were also degradable.

[0050] Without limiting the scope or interpretation of the claims in any way, the technical effects of one or more exemplary embodiments disclosed herein are listed below: One technical effect includes obtaining strain information from a human body.

[0051] The foregoing description provides a complete and informative description of the best ways currently contemplated by the inventors for carrying out the present invention as non-limiting examples of specific implementations and embodiments of the present invention, but those skilled in the art will appreciate that the present invention is not limited to the details of the above-described embodiments, and that equivalent means may be used in other embodiments without departing from the characteristics of the present invention.

[0052] Moreover, some of the features of the above-described embodiments of the invention may be used to advantage without the corresponding use of other features. Thus, the foregoing description should be taken as merely illustrative, rather than in limitation of the principles of the invention. The scope of the invention is therefore limited only by the appended claims.

Claims

1. a first conductive atomic layer deposition (ALD) layer applied or deposited on a substrate; a flexible or compressible electrically insulating Molecular Layer Deposition (MLD) layer on the first ALD layer; a second conductive ALD layer on the MLD layer; and forming a circuit that provides information indicative of strain.

2. The device of claim 1 which is an implantable device.

3. 3. A device as claimed in claim 1 or 2, comprising an antenna for providing information indicative of said distortion.

4. The device of claim 1 , wherein the substrate is biodegradable.

5. 5. The device of claim 1 which is biodegradable.

6. The device of claim 1 , wherein the substrate is a biodegradable screw or nail.

7. A device as claimed in any preceding claim, comprising an RC or RLD circuit for providing information indicative of said distortion.

8. 8. A device according to claim 1, wherein the device is arranged to provide externally readable information indicative of the distortion by radio frequency.

9. A method for manufacturing a strain sensor device, comprising: Providing an implantable substrate; depositing a capacitor structure comprising a conductive layer on either side of a Molecular Layer Deposition (MLD) layer; providing a circuit comprising the capacitor structure configured to provide information indicative of distortion; wherein both the MLD layer and the device are biodegradable.

Citation Information

Patent Citations

  • Pressure-sensitive display touch unit, touch screen, and manufacturing method thereof

    EP3082022A1

  • Biodegradable bone nail

    US20160235456A1

  • Novel Methods of Preparing Nanodevices

    US20160304341A1

  • Wireless strain sensing device

    US20160354174A1