Manufacturing method of a cup-shaped container
The method improves sealing and sterilization capabilities of cup-shaped containers by using laminates with metal foil and heat-fusible resin layers, addressing the limitations of paper and plastic cups for long-term storage and sterilization.
Patent Information
- Application Number
- JP2020210060
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-12-25
- Filing Date
- 2020-12-18
- Publication Date
- 2024-10-10
- Estimated Expiration
- 2040-12-18
AI Technical Summary
Existing paper cups for food products like ice cream and yogurt have low barrier properties, leading to water ingress and inability for long-term storage, while plastic containers are costly and unsuitable for long-term storage, and both types face issues with sealing performance and sterilization methods.
A manufacturing method involving laminates with a metal foil layer and heat-fusible resin layers on both surfaces, using high-frequency sealing to join edges and integrate the body and bottom body, ensuring reliable sealing and aseptic or retort sterilization capabilities.
The method enhances sealing performance, prevents deformation, and allows for cost-effective production using paper cup equipment, ensuring long-term storage stability and hygiene, suitable for aseptic and retort sterilization.
Smart Images

Figure 0007565208000001 
Figure 0007565208000002 
Figure 0007565208000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a cup-shaped container for containing food or beverages such as ice cream or yogurt. [Background technology]
[0002] 2. Description of the Related Art Paper cup-shaped containers, that is, paper cups, are commonly used as containers for filling and packaging semi-solid dairy products such as ice cream and yogurt. A paper cup is usually formed by joining together a body and a bottom, each of which is made of a paper blank cut to a predetermined shape. More specifically, the body is formed into a cylindrical shape by overlapping and joining both end edges of a substantially sector-shaped body blank, with a folded-back portion folded inward at the bottom opening edge and a flange portion curled outward at the top opening edge. The bottom has a substantially inverted U-shaped cross section, formed by skirt-molding a substantially circular bottom blank so that a hanging portion is formed on its outer periphery. The hanging portion of the bottom is wrapped around and joined to the folded-back portion of the body, thereby integrating the body and the bottom. Each blank for the body and bottom body is made of a laminate having, for example, a paper layer made of general base paper, acid-resistant paper, coated paper, etc., and a polyethylene (PE) layer laminated on one or both sides of the paper layer (see, for example, Patent Document 1 below).
[0003] Also known is a paper cup that uses a laminate formed by laminating a barrier layer made of aluminum foil or the like in addition to a paper layer and a polyethylene (PE) layer as the material for each of the above blanks (see, for example, Patent Document 2 below).
[0004] Additionally, containers for ice cream, yogurt, etc., made of plastic molded bodies such as polypropylene (PP) are also known (see, for example, Patent Document 3 below). [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Japanese Patent Application Publication No. 58-30955 [Patent Document 2] JP 2007-210639 A [Patent Document 3] JP 2007-176505 A Summary of the Invention [Problem to be solved by the invention]
[0006] However, while paper cups have excellent productivity and can be manufactured at low cost, they have poor barrier properties and are not suitable for long-term storage of contents. Paper cups with a barrier layer such as aluminum foil improve the long-term storage of the contents, but water easily penetrates through the edges of the paper layer, making retort sterilization impossible. In addition, plastic containers are expensive to manufacture and are not suitable for long-term storage of the contents.
[0007] In order to solve the above problems, the present inventor previously proposed a cup-shaped container using a laminate consisting of a metal foil layer and a heat-fusible resin layer laminated on at least one of its two sides as the material for each of the body blank and the bottom blank (Patent Application No. 2019-106125). The above-mentioned cup-shaped container can be produced inexpensively using paper cup manufacturing equipment, has excellent long-term storage properties for the contents, and can also be subjected to aseptic sterilization or retort sterilization.
[0008] In the case of the above-mentioned cup-shaped container, if the joining of both end edges of the body blank or the joining of the body and the bottom body is insufficient, the sealing ability of the container will decrease, and there is a risk of the contents leaking, etc. On the other hand, if the sealing conditions are made stricter in order to increase the joint strength, there is a risk that deformation or the like will occur at the joint, damaging the appearance of the container. The object of the present invention is to provide a manufacturing method for a cup-shaped container that can be produced inexpensively using paper cup manufacturing equipment, has excellent long-term storage properties for the contents, and can be aseptically or retort sterilized, by more reliably joining both end edges of a body blank and joining the body and bottom without causing appearance defects such as deformation of the container, thereby improving the sealing properties of the container. [Means for solving the problem]
[0009] In order to achieve the above object, the present invention comprises the following aspects.
[0010] 1) forming a body blank by punching out a laminate including a metal foil layer and a heat-sealable resin layer laminated on at least one of both surfaces of the metal foil layer that will become the inside of the body; A step of punching out a laminate including a metal foil layer and a heat-sealable resin layer laminated on at least one of both surfaces of the metal foil layer that will be the upper surface of the bottom body to form a bottom body blank; forming a bottom body having a generally inverted U-shaped cross section by drawing a bottom body blank so as to form a bottom and a hanging portion extending downward from an outer peripheral edge of the bottom body; forming a cylindrical body by overlapping both end edge portions of the body blank and heat-sealing the heat-sealable resin layers constituting the overlapping surfaces of the body blank; and overlapping the inner surface of the lower end of the body and the outer surface of the hanging portion of the bottom body, and heat-sealing the heat-sealable resin layers constituting these surfaces together to integrate the body and the bottom body. A method for manufacturing a cup-shaped container, in which, in the process of forming a cylindrical body, the heat-sealable resin layers at both end edges of a body blank are heat-sealed twice, with the second heat-sealing being performed by high-frequency sealing.
[0011] 2) In the process of forming a blank for a fuselage, a laminate in which a heat-sealable resin layer is laminated on both sides of a metal foil layer is used, A method for manufacturing a cup-shaped container as described above in 1), in which, in the process of forming a cylindrical body, both end edges of a body blank are overlapped in a folded shape and the heat-fusible resin layers constituting the overlapping surfaces are joined together by a first heat fusion to form a cylindrical body having a folded portion, and then the folded portion is folded to one side and placed over the outer surface of the body, and a second heat fusion is performed by high-frequency sealing to join the folded portion to the outer surface of the body.
[0012] 3) A method for manufacturing a cup-shaped container as described in 1) or 2) above, in which, in the process of integrating the body and the bottom body, the heat-sealing resin layers at the lower end of the body and the hanging portion of the bottom body are heat-sealed twice, and the second heat-sealing is performed by high-frequency sealing.
[0013] 4) forming a body blank by punching out a laminate including a metal foil layer and a heat-sealable resin layer laminated on at least one of both surfaces of the metal foil layer that will become the inside of the body; A step of punching out a laminate including a metal foil layer and a heat-sealable resin layer laminated on at least one of both surfaces of the metal foil layer that will be the upper surface of the bottom body to form a bottom body blank; forming a bottom body having a generally inverted U-shaped cross section by drawing a bottom body blank so as to form a bottom and a hanging portion extending downward from an outer peripheral edge of the bottom body; forming a cylindrical body by overlapping both end edge portions of the body blank and heat-sealing the heat-sealable resin layers constituting the overlapping surfaces of the body blank; and a step of integrating the body and the bottom body by heat-sealing the heat-sealable resin layers constituting the inner surface of the lower end of the body and the outer surface of the hanging portion of the bottom body, A method for manufacturing a cup-shaped container, in which, in a process of integrating a body and a bottom body, the heat-sealing resin layers at the lower end of the body and the hanging portion of the bottom body are heat-sealed twice, with the second heat-sealing being performed by high-frequency sealing.
[0014] 5) In the step of forming a bottom blank, a laminate in which a heat-sealable resin layer is laminated on both sides of a metal foil layer is used, A method for manufacturing a cup-shaped container as described in 3) or 4) above, in which, in the step of integrating the body and the bottom body, the body is folded inward from its lower end opening edge so as to enclose the hanging portion of the bottom body to form a folded portion, and the heat-sealable resin layers constituting the overlapping surfaces of the lower end of the body and the folded portion and the hanging portion of the bottom body are heat-sealed to each other to integrate the body and the bottom body, and the heat-sealing resin layers of the lower end and folded portion of the body and the hanging portion of the bottom body are heat-sealed twice, and the second heat-sealing is performed by high-frequency sealing. Effect of the Invention
[0015] According to the manufacturing method for a cup-shaped container described above in 1), the heat-sealable resin layers at both end edges of the body blank are also heat-sealed by being heated by the metal foil layer which has been heated by the induction heating of the high-frequency seal, so that both end edges of the body blank are more securely joined together, and since a resin pool is easily formed at the joint due to the heat sealing, the sealing performance of the container can be improved and the occurrence of appearance defects such as deformation of the container due to the heat sealing can be effectively suppressed.
[0016] According to the manufacturing method for cup-shaped containers described above in 2), the occurrence of delamination and the like is suppressed since both end faces of the body blank do not come into contact with the contents, and since the surface that comes into contact with the contents is made of a single type of resin, hygienic containers that are easy to sterilize can be easily manufactured. Furthermore, according to the manufacturing method of a cup-shaped container described above in 2), the process of joining the joint portion of the body to the outer surface of the body can be carried out by heating from the metal foil layer using ultrasonic sealing. Therefore, the heat for heat fusion is transmitted evenly to each heat-sealable resin layer, making it possible to more reliably join the two, which is advantageous in terms of manufacturing efficiency.
[0017] According to the manufacturing methods of cup-shaped containers 3) and 4) above, the lower end of the body and the hanging portion of the base are more securely joined by high-frequency sealing, and a resin pool is likely to form at the joint due to heat fusion, thereby improving the sealing performance of the container and effectively suppressing the occurrence of appearance defects such as deformation due to heat fusion.
[0018] According to the method for manufacturing a cup-shaped container as described above in 5), the sealing performance of the joint between the body and the bottom, including the inside of the folded portion, is further improved. [Brief description of the drawings]
[0019] [Figure 1] 1 is a perspective view of a cup-shaped container according to a first embodiment of the present invention. [Diagram 2] This is a vertical cross-sectional view taken along line II-II in FIG. 1, in which the portion surrounded by dashed dotted line A is an enlarged view of the portion surrounded by dashed dotted line a, and the portion surrounded by dashed dotted line B is an enlarged view of the portion surrounded by dashed dotted line b. [Diagram 3] 1A is an enlarged cross-sectional view showing the layer structure of a laminate used as the material for the body blank, and FIG. 1B is an enlarged cross-sectional view showing the layer structure of a laminate used as the material for the bottom blank. [Figure 4] 3 is a horizontal cross-sectional view showing an enlarged overlapping portion of the body of the cup-shaped container. FIG. [Diagram 5] FIG. 2(a) is a plan view of a fuselage blank, and FIG. 2(b) is a perspective view of a fuselage formed from the fuselage blank. [Figure 6] 1A is a plan view of a bottom body blank, and FIG. 1B is a perspective view of a bottom body formed from the bottom body blank. [Figure 7] 5A to 5C are vertical cross-sectional views showing a part of the manufacturing process of the cup-shaped container. [Figure 8] 10 is a partially enlarged vertical cross-sectional view showing a modified example of the connecting structure between the body and the bottom body of the cup-shaped container. FIG. [Figure 9]5 is an enlarged horizontal cross-sectional view showing an overlapping portion of a body of a cup-shaped container according to a second embodiment of the present invention. FIG. [Figure 10] 3A to 3C are horizontal cross-sectional views sequentially showing a part of the manufacturing process for the body of the cup-shaped container. [Figure 11] FIG. 11 is a horizontal cross-sectional view of a cup-shaped container according to a third embodiment of the present invention, in which the portion surrounded by the dashed dotted line C is an enlarged view of the portion surrounded by the dashed dotted line c. [Figure 12] 5A to 5C are horizontal cross-sectional views showing a part of a manufacturing process for the body of the cup-shaped container. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0020] Hereinafter, an embodiment of the present invention will be described with reference to FIGS. In the following explanation, "upper and lower" refers to the upper and lower sides of the cup-shaped container, body and bottom body (e.g., the upper and lower sides in Figures 2, 7 and 8), "inner" refers to the side closer to the center of the cup-shaped container, body and bottom body (e.g., the upper side in Figures 4, 9 and 10, and the right side in Figures 7 and 8), and "outer" refers to the side farther from the center of the cup-shaped container, body and bottom body (e.g., the lower side in Figures 4, 9 and 10, and the left side in Figures 7 and 8).
[0021] [First embodiment] Figures 1 and 2 show the overall structure of a cup-shaped container (1) according to a first embodiment of the present invention. The container (1) is formed by joining together a body (2) formed from a body blank (20A) and a bottom body (3) formed from a bottom body blank (30A). The body (2) is a tapered cylinder, and is formed by overlapping and joining both end edges of a sector-shaped body blank (20A) as shown in Fig. 5. Therefore, the body (2) has an overlap portion (21) that extends along its height direction. The body (2) has a folded-back portion (22) folded inward at the edge of the lower opening. The body 2 has an outwardly bent flange 23 at the upper opening edge. The flange 23 is folded downward and formed into a substantially horizontal flat shape. The flange may have a shape other than that shown in the figure, for example, it may be curled downward and formed into a substantially arc-shaped cross section. The bottom body (3) has a generally inverted U-shaped cross section, with a circular, horizontal bottom portion (31) and a hanging portion (32) extending downward from the outer peripheral edge of the bottom portion (31), and is formed by drawing a circular bottom body blank (30A) as shown in Figure 6. The outer surface of the hanging portion (32) of the bottom body (3) is joined to the inner surface of the lower end portion (2a) of the body (2), and the folded portion (22) of the body (2) is joined to the inner surface of the hanging portion (32), thereby integrating the body (2) and the bottom body (3) (see Figures 2 and 7). 8, the body (2) and the bottom body (3) can be integrated by a connecting structure in which the outer surface of the hanging portion (32) of the bottom body (3) is joined to the inner surface of the lower end (2a) of the body (2) without forming a folded portion (22) at the edge of the lower end opening of the body (2). With this configuration, even if some wrinkles are generated in the hanging portion (32) when the bottom body (3) is molded, the lower end (2a) of the body (2) and the hanging portion (32) of the bottom body (3) can be reliably sealed without mixing in air or the like.
[0022] As shown in FIG. 3(a), the body blank (20A) is formed from a laminate (20) comprising a metal foil layer (201), a heat-sealable resin layer (202) laminated on one of both sides of the metal foil layer (201) that will be the inside of the body (2), and an outer heat-sealable resin layer (203) laminated on one of both sides of the metal foil layer (201) that will be the outside of the body (2), and does not have a paper layer. As shown in Fig. 3(b), the bottom blank (30A) is also formed of a laminate (30) consisting of a metal foil layer (301), an upper heat-sealable resin layer (302) laminated on the upper side of the metal foil layer (301) that is the upper side of the bottom body (3), and a lower heat-sealable resin layer (303) laminated on the lower side of the metal foil layer (301) that is the lower side of the bottom body (3), and does not have a paper layer. Note that if the folded portion (22) is not formed at the edge of the lower opening of the body (2) and the connection structure is such that the outer surface of the hanging portion (32) of the bottom body (3) is only joined to the inner surface of the lower end (2a) of the body (2) (see Fig. 8), the lower heat-sealable resin layer (303) of the bottom blank (30A) can be omitted. The thickness of each laminate (20)(30) is preferably less than 250 μm, and more preferably less than 200 μm. By setting the thickness of each laminate (20)(30) within the above range, as in the case of a paper cup using a laminate with a thickness of about 250 to 400 μm as the blank material, the step of the part of the flange portion (23) of the body (2) formed by the overlap portion (21) becomes too large, and the lower end portion (2a) and the folded portion (22) of the body (2) and the hanging portion of the bottom body (3) become too large. (32) This reliably avoids problems such as unstable bonding with the
[0023] The metal foil layers (201) (301) function as a barrier layer to protect the contents from gas, water vapor, light, etc. The metal foil constituting the metal foil layer (201) (301) may be aluminum foil, iron foil, stainless steel foil, copper foil, etc., but aluminum foil is preferably used. In the case of aluminum foil, either pure aluminum foil or aluminum alloy foil may be used, and either soft or hard. For example, annealed soft material (O material) of A8000 series (particularly A8079H or A8021H) classified by JIS H4160 is preferably used because it has excellent formability. In addition, when a hard material (H material) is used as the aluminum foil constituting the metal foil layer (201) (particularly the metal foil layer (201) of the body blank (20A)), the strength of the flange portion (23) is increased, deformation of the flange portion (23) due to unexpected impact is suppressed, and the shape retention of the cup-shaped container (1) as a whole is improved. Both sides of the aluminum foil constituting the metal foil layers (201) and (301) are subjected to a base treatment such as a chemical conversion treatment, if necessary. Specifically, for example, the surface of the aluminum foil that has been degreased is 1) Phosphoric acid, Chromic acid, and at least one compound selected from the group consisting of metal salts of fluorides and nonmetal salts of fluorides. 2) phosphoric acid; At least one resin selected from the group consisting of acrylic resins, chitosan derivative resins, and phenolic resins; and at least one compound selected from the group consisting of chromic acid and chromium (III) salts. 3) phosphoric acid; At least one resin selected from the group consisting of acrylic resins, chitosan derivative resins, and phenolic resins; At least one compound selected from the group consisting of chromic acid and chromium (III) salts; and at least one compound selected from the group consisting of metal salts of fluorides and nonmetal salts of fluorides. A coating is formed by applying an aqueous solution of any one of the above 1) to 3) and then drying the applied solution to perform a chemical conversion treatment. The coating formed on the surface of the metal foil layer (201) (301) by the above chemical conversion treatment has a chromium deposition amount (per side) of 0.1 mg / m 2 ~50mg / m 2 It is preferable to use a concentration of 2 mg / m 2 ~20mg / m 2 It is preferable to set the above. When a soft material is used as the aluminum foil, it is not always necessary to carry out a degreasing treatment as a pretreatment for the chemical conversion treatment. The thickness of the metal foil layer (201)(301) is preferably 40 to 200 μm, more preferably 80 to 160 μm. By setting the thickness of the metal foil layer (201)(301) within the above range, sufficient barrier properties and moldability can be obtained.
[0024] The heat-sealable resin layers (202), (203), (302), (303) constitute the inner and outer surfaces of the container (1), and serve to protect the metal foil layers (201), (301) and to impart formability to the laminates (20), (30). They also function as heat-sealing layers when joining both end edges of the body blank (20A) and when joining the lower end (2a) and folded portion (22) of the body (2) to the hanging portion (32) of the bottom body (3). The heat-sealable resin layers (202)(203)(302)(303) are usually made of a versatile polyolefin film such as a heat-sealable polypropylene (PP) film or a polyethylene (PE) film, or a composite film made by bonding these together, but a non-oriented polypropylene film (CPP), which has excellent heat resistance and draw formability, is particularly suitable. The heat-sealable resin layers (202)(203)(302)(303) may be formed of a coating layer of maleic acid-modified polyethylene, maleic acid-modified polypropylene, ethylene-vinyl acetate, epoxy resin, shellac resin, or the like, instead of the above-mentioned films. The thickness of the heat-sealable resin layers (202), (203), (302), (303) is preferably 5 to 80 μm, and more preferably 10 to 60 μm. By setting the thickness of the heat-sealable resin layers (202), (203), (302), (303) within the above range, sufficient adhesive strength can be obtained at the joint between both end edges of the body blank (20A) and at the joint between the lower end (2a) and the folded-back portion (22) of the body (2) and the hanging portion (32) of the bottom body (3), and the step formed by the overlap (21) on the upper surface of the flange portion (23) of the body (2) can be made gentle, resulting in good sealing performance when sealed with a lid.
[0025] The aluminum foil constituting the metal foil layer (201) (301) and the film constituting the heat-fusible resin layer (202) (203) (302) (303) are laminated, for example, by a dry lamination method via an adhesive layer (not shown). For the adhesive layer, for example, a two-component curing polyester-polyurethane adhesive or a polyether-polyurethane adhesive is used. Due to the presence of the adhesive layer, even if the heat-sealable resin layers (202) and (203) at both end edges of the body blank (20A) in the overlapping portion (21) of the body (2) are thinned by heat fusion, the metal foil layers (201) are prevented from coming into contact with each other, so that the sealing performance is maintained. Furthermore, with the adhesive layer, even if the container (1) is filled with contents that permeate the heat-sealable resin layers (202) and (203) and (302) and (303), it is possible to prevent the metal foil layers (201) and (301) from corroding and causing the contents to leak out.
[0026] The laminate (20) constituting the body blank (20A) and the laminate (30) constituting the bottom blank (30A) are usually the same, but may be made of different materials and / or thicknesses.
[0027] Next, a method for manufacturing the cup-shaped container (1) according to the first embodiment will be described. The manufacturing method comprises the following steps 1 to 6. The order of the steps may be changed as appropriate.
[0028] (First step) The first step is to form a body blank (20A) by punching out a laminate (20) consisting of a metal foil layer (201) and an inner heat-sealable resin layer (202) and an outer heat-sealable resin layer (203) laminated on both sides of the metal foil layer (201) into a sector shape of a predetermined size (see Figure 5(a)).
[0029] (Second step) The second step is to punch out a laminate (30) consisting of a metal foil layer (301) and an upper heat-sealable resin layer (302) and a lower heat-sealable resin layer (303) laminated on both sides of the metal foil layer (301) into a circle of a predetermined size to form a bottom body blank (30A) (see Figure 6(a)).
[0030] (Third step) The third step is to form the bottom body blank (30A) by drawing using a mold (not shown) to form the bottom body (3) having an approximately inverted U-shaped cross section and consisting of a bottom portion (31) and a hanging portion (32) (see Figure 6(b)). The bottom body (3) thus obtained is free of wrinkles, and the corners between the bottom portion (31) and the hanging portion (32) on the outer surface of the bottom body (3) are rounded.
[0031] (Fourth step) The fourth step is to form a cylindrical body (2) by overlapping both end edges of the body blank (20A) and heat-sealing the inner heat-sealable resin layer (202) and the outer heat-sealable resin layer (203) which constitute the overlapping surfaces (see Figures 4 and 5(b)). This process is usually carried out by setting the bottom body (3) on the top surface of a roughly truncated cone-shaped mold (not shown) so that the upper surface of its bottom part (31) is overlapped, wrapping the body blank (20A) around the outer peripheral surface of the mold so that both end edges are overlapped, and then heat-sealing the inner heat-sealable resin layer (202) and the outer heat-sealable resin layer (203), which form the overlapping surfaces of both end edges. In this fourth step, both end edges of the body blank (20A) are heat-sealed a total of two times. The first heat-sealing is usually performed by heat sealing using a hot plate or the like, but may also be performed by high-frequency sealing, ultrasonic sealing, or the like. The second heat-sealing is performed by high-frequency sealing. By performing the above two-stage heat-sealing, both end edges of the body blank (20A) are more reliably joined, and resin pools are more likely to form at the joint due to the heat-sealing (see Figure 4), and deformation due to the heat-sealing is suppressed. Here, when the inner heat-sealable resin layer (202) and the outer heat-sealable resin layer (203) are made of a non-oriented polypropylene film (CPP), the heat sealing is preferably performed under the conditions of a sealing temperature of 160 to 220°C, a load (sealing pressure) of 80 to 200 kgf, and a sealing time of 1 to 5 seconds. When the inner heat-sealable resin layer (202) and the outer heat-sealable resin layer (203) are made of a polyethylene film (PE), the heat sealing is preferably performed under the conditions of a sealing temperature of 140 to 220°C, a load of 80 to 200 kgf, and a sealing time of 1 to 5 seconds. In other words, in the case of heat sealing, it is preferable to heat both ends of the overlapped body blank (20A) at a temperature 20 to 40°C higher than the melting point of the resin constituting the heat-sealable resin layers (202) and (203) from both sides. Moreover, the high frequency sealing is preferably performed under the conditions of, for example, output: 0.5 to 1.5 kW, sealing time: 3 to 5 seconds, distance from the coil: 0.5 to 15 mm, and load: 100 to 200 kgf.
[0032] (5th step) The fifth step is a step of folding the body (2) inward from its lower end opening edge so as to wrap around the hanging portion (32) of the bottom body (3) to form a folded portion (22), and heat-sealing the inner heat-sealable resin layer (202), as well as the upper heat-sealable resin layer (302) and the lower heat-sealable resin layer (303), which form the overlapping surfaces of the lower end portion (2a) of the body (2) and the folded portion (22) with the hanging portion (32) of the bottom body (3), thereby integrating the body (2) and the bottom body (3) (see Figures 2 and 7). This process typically involves folding the lower opening edge of the body (2) inward and pressing the folded portion (22) against the hanging portion (32) of the bottom body (3) with a disk-shaped rotating die (not shown), and then heat-sealing the inner heat-sealable resin layer (202) to the upper heat-sealable resin layer (302) and the lower heat-sealable resin layer (303), which form the overlapping surfaces of the lower end (2a) and folded portion (22) of the body (2) and the hanging portion (32) of the bottom body (3). In this fifth step, the heat-sealable resin layers (202), (302), (303) of the lower end (2a) and folded portion (22) of the body (2) and the hanging portion (32) of the bottom body (3) are heat-sealed twice in total. The first heat-sealing is usually performed by heat sealing using a hot plate or the like, but may also be performed by high-frequency sealing, ultrasonic sealing, or the like. The second heat-sealing is performed by high-frequency sealing. In the case of high-frequency sealing, the metal foil layer is heated to a high temperature by induction heating, and the heat emitted from this metal foil layer promotes heat-sealing between the heat-sealable resin layers. The above two-stage heat-sealing more reliably joins the lower end (2a) and folded portion (22) of the body (2) to the hanging portion (32) of the bottom body (3), and the heat-sealing makes it easier for resin pools to form at the joints, and furthermore, the occurrence of deformation and the like due to the heat-sealing is suppressed. The suitable conditions for heat sealing and high frequency sealing are the same as those in the fourth step.
[0033] In addition, as shown in FIG. 8, in the case of a container in which no folded portion (22) is formed at the lower opening edge of the body (2) and the outer surface of the hanging portion (32) of the bottom body (3) is joined to the inner surface of the lower end (2a) of the body (2), a process substantially similar to the fifth process described above can be carried out, i.e., the inner surface of the lower end (2a) of the body (2) and the outer surface of the hanging portion (32) of the bottom body (3) are overlapped, and the inner heat-sealable resin layer (202) and the upper heat-sealable resin layer (302) constituting these surfaces are heat-sealed twice, with the second heat-sealing being performed by high-frequency sealing, thereby integrating the body (2) and the bottom body (3).
[0034] (Sixth step) The sixth step is to form the flange portion (23) by curling the upper opening edge of the body (2) outward using a specified curl forming die (not shown) and pressing it vertically to form it into a flat shape (see FIG. 7). Depending on the shape of the flange portion, the flange portion may be formed by means or steps different from those described above.
[0035] Referring to Fig. 4, in the overlap portion (21) of the body (2) of the cup-shaped container (1), the total thickness (T1) of the inner heat-sealable resin layer (202) and the outer heat-sealable resin layer (203) heat-sealed to each other at both end edges of the body blank (20A) is preferably 8 to 150 µm, more preferably 16 to 80 µm. If the total thickness (T1) is less than 8 µm, the sealing property of the overlap portion (21) may be insufficient. On the other hand, if the total thickness (T1) exceeds 150 µm, the barrier property of the overlap portion (21) may be impaired. In the overlapping portion (21) of the body (2), the overlapping width (W1) between the metal foil layers (201) (201) at both ends of the body blank (20A) as viewed in the thickness direction is preferably 2 to 10 mm, more preferably 4 to 8 mm. If the overlapping width (W1) is less than 2 mm, the barrier properties of the overlapping portion (21) may be impaired, and the seal width may be too small, resulting in insufficient sealability. On the other hand, if the overlapping width (W1) exceeds 10 mm, the width of the overlapping portion (21) becomes larger than necessary, leading to increased costs, and furthermore, due to the difference in stress applied to the inner portion (one end edge of the body blank (20A)) and the outer portion (the other end edge of the body blank (20A)) of the overlapping portion (21), there is a risk of wrinkles or other defects in appearance occurring in the inner portion of the overlapping portion (21).
[0036] Furthermore, as shown in Fig. 4, it is preferable that the inner end surface of the body blank (20A) located on the inner side of the body (2) is covered with an inner resin reservoir (R1) formed when the inner heat-sealable resin layer (202) and the outer heat-sealable resin layer (203) constituting the mutually overlapping surfaces of both end edges of the body blank (20A) are heat-sealed. Also, although not shown in the figure, the outer end surface of the body blank (20A) located on the outer side of the body (2) is preferably covered with an inner resin reservoir (R1) formed when the inner heat-sealable resin layer (202) and the outer heat-sealable resin layer (203) constituting the mutually overlapping surfaces of both end edges of the body blank (20A). It may be covered by an outer resin reservoir portion formed when the inner heat-sealable resin layer (202) and the outer heat-sealable resin layer (203) constituting the overlapping surfaces are heat-sealed. The inner resin reservoir (R1) and the outer resin reservoir (R2) are formed when the overlapped end edges of the body blank (20A) are heat-sealed together, and the inner heat-sealable resin layer (202) and the outer heat-sealable resin layer (203) constituting the overlapping surfaces melt in part, and the molten resin is pushed out in the width direction of the overlapping portion (21) by the pressure applied during heat fusion. FaceThe inner heat-sealable resin layer (202) and the outer heat-sealable resin layer (203) that constitute the inner end On the surface The adjacent inner heat-sealable resin layer (202) is also formed by a part of the molten resin, and the outer resin pool portion is formed at the outer end of the body blank (20A). Face The inner heat-sealable resin layer (202) and the outer heat-sealable resin layer (203) that constitute the outer end On the surface It is believed that a portion of the adjacent outer heat-sealable resin layer (203) is also formed by the molten resin. These resin reservoirs (R1) can be formed, for example, by controlling the sealing conditions during heat fusion (sealing temperature, pressure, sealing time, sealing range, etc.) or by appropriately setting the configuration of the body blank (20A), etc. In particular, in the case of this embodiment, since heat fusion is performed in two stages in the above-mentioned fourth step, the desired resin reservoirs (R1) are reliably formed.
[0037] The cup-shaped container (1) and its manufacturing method of this embodiment provide the following advantages. a) The body blank (20A) and the bottom blank (30A) are each formed from a laminate (20) (30) consisting of a metal foil layer (201) (301) and heat-sealable resin layers (202) (203) (302) (303) laminated on both sides thereof, and therefore can be produced inexpensively using paper cup production equipment. b) The laminates (20) (30) from which the blanks (20A) (30A) are made have metal foil layers (201) (301), so that the contents can be stored for a long time. c) Since the thickness of the body blank (20A) is smaller than that of a paper cup, the step on the upper surface of the flange portion (23) of the body (2) formed by the overlap portion (21) can be made smaller, and therefore poor sealing is less likely to occur when sealing the lid to the upper surface of the flange portion (23) of the container (1). Also, when performing aseptic (sterile) filling, sterilizing liquid is less likely to remain in the step on the upper surface of the flange portion (23). d) Since the bottom body (3) is formed by drawing the bottom body blank (30A), wrinkles do not occur in the bottom body (3). Therefore, there is no risk of poor bonding between the hanging portion (32) of the bottom body (3) and the lower end portion (2a) and the folded portion (22) of the body (2) or of reduced barrier properties, as occurs with conventional paper cups. e) Since the thickness of the body blank (20A) and the bottom blank (30A) is smaller than that of a paper cup, the lower end (2a) and the folded portion (22) of the body (2) can be stably joined to the hanging portion (32) of the bottom body (3). f) Compared to a paper cup, the radius of curvature (R) of the corner portion between the bottom portion (31) and the hanging portion (32) on the outer surface of the base body (3) can be made smaller, so that when performing aseptic filling, sterilizing liquid is less likely to remain at the boundary between the upper surface of the bottom body (3) and the inner surface of the body (2) of the cup-shaped container (1). g) Since the laminates 20, 30 from which the blanks 20A, 30A are made do not have a paper layer, retort sterilization can be carried out without any problems. h) In the fourth step of forming the cylindrical body (2), the heat-sealing resin layers at both end edges of the body blank are heat-sealed twice in total, and the second heat-sealing is performed by high-frequency sealing that allows heating from the metal foil layer, so that both end edges of the body blank (20A) are more reliably joined together, and resin pools are more likely to form at the joints due to the heat sealing, improving the sealing performance of the container (1). Moreover, the occurrence of defects in appearance such as deformation of the container (1) can be effectively suppressed. i) In the fifth step of integrating the body and the bottom body, the heat-sealing resin layers (202), (302), (303) of the lower end (2a) and folded portion (22) of the body (2) and the hanging portion (32) of the bottom body (3) are heat-sealed twice in total, and the second heat-sealing is performed by high-frequency sealing, so that the lower end (2a) and folded portion (22) of the body (2) and the hanging portion (32) of the bottom body (3) are more reliably joined, and resin pools are easily formed at the joints due to the heat sealing, improving the sealing performance of the container (1). Moreover, the occurrence of defects in appearance such as deformation of the container (1) can be effectively suppressed. j) In the overlapping portion (21) of the body (2), when the inner end surface of the body blank (20A) located on the inside of the body (2) is covered by the inner resin reservoir (R1) formed when the heat-sealable resin layers (202) and (203) at both end edges of the body blank (2) are heat-sealed to each other, the inner end surface is not exposed to the contents, so that deterioration due to delamination and corrosion of the inner end surface is effectively suppressed, and this is also preferable from the viewpoint of hygiene. Also, in the overlapping portion (21) of the body (2), when the outer end surface of the body blank (20A) located on the outside of the body (2) is covered by the outer resin reservoir formed when the heat-sealable resin layers (202) and (203) at both end edges of the body blank (2) are heat-sealed to each other, deterioration due to delamination and corrosion of the outer end surface is effectively suppressed.
[0038] [Second embodiment] 9 and 10 show a cup-shaped container (1X) according to a second embodiment of the present invention and a method for manufacturing the same. This embodiment is substantially the same as the cup-shaped container (1) and the manufacturing method thereof of the first embodiment shown in Figs. 1 to 8, except for the following points. That is, as shown in Figures 9 and 10, in the cup-shaped container (1X) of this embodiment, of the two end edge portions of the body blank (20A), the edge portion (204) that faces the inside of the body (2) is folded over so as to overlap the surface of the body blank (20A) that faces the outside of the body (2) and is heat-sealed to that surface, and the folded over edge portion (204) and the other edge portion (205) are overlapped, and the inner heat-sealable resin layers (202) that form the overlapping surfaces of these edges (204) and (205) are heat-sealed to each other. According to the above-mentioned cup-shaped container (1X), at the overlap portion (21) of the body (2), both end faces of the body blank (20A) do not come into contact with the contents contained in the container (1X), thereby suppressing the occurrence of delamination, corrosion, and the like. Furthermore, since the surface that comes into contact with the contents can be made of a single type of resin, sterilization is easy, which is advantageous in terms of hygiene. In addition, the width of the folded edge (204) and the overlap width of both end edges (204) and (205) are substantially the same as shown in the figure. Each other It is also possible to make the number of times different.
[0039] In manufacturing the above cup container (1X), the fifth step of forming the body (2) is carried out as follows. That is, of both end edges of the body blank (20A), the edge portion (204) that faces the inside of the body (2) is folded back so as to overlap the surface of the body blank (20A) that faces the outside of the body (2), and the folded back edge portion (204) is overlapped with the other edge portion (205). The inner heat-sealable resin layer (202) and the outer heat-sealable resin layer (203), which form the overlapping surfaces of these layers (204) and (205), are heat-sealed together a total of two times. The first heat fusion is usually performed by heat sealing using a hot plate or the like, but may also be performed by high-frequency sealing, ultrasonic sealing, etc. The second heat fusion is performed by high-frequency sealing. By performing the above two-stage heat fusion, both end edge portions of the body blank (20A) are more reliably joined together, resin pools are more likely to form at the joints due to the heat fusion, and deformation due to the heat fusion is suppressed.
[0040] [Third embodiment] 11 and 12 show a cup-shaped container according to a third embodiment of the present invention. (1Y) and The manufacturing method is shown. This embodiment is substantially the same as the cup-shaped container (1) and the manufacturing method thereof of the first embodiment shown in Figs. 1 to 8, except for the following points. That is, as shown in Figs. 11 and 12, in the cup-shaped container (1Y) of this embodiment, The body 2 is formed into a cylindrical shape by overlapping and joining both end edges of a body blank 20A in a palm-to-palm shape (see FIG. 12(a)). More specifically, both end edges of the body blank 20A overlapped in a palm-to-palm shape are joined by heat fusing their inner heat-fusible resin layers 202 together. Also, the joint portion (21Y) of the body (2) is bent to one side so as to overlap with the outer surface of the body (2) and is heat-sealed to the outer surface (see FIG. 12(b)). According to the above-mentioned cup-shaped container (1Y), both end faces of the body blank (20A) are connected to the joint portion (21Y) of the body (2). (1Y) Since the container (1Y) does not come into contact with the contents contained therein, the occurrence of delamination, corrosion, etc. is suppressed. In addition, according to the container (1Y), the surface that comes into contact with the contents can be made of one type of resin, which makes sterilization easy and is advantageous in terms of hygiene. In addition, according to the cup-shaped container (1Y), the joint portion (21Y) of the body (2) is bent to one side and heat-sealed to the outer surface of the body (2), improving the sealing and barrier properties of the same part. Moreover, according to the cup-shaped container (1Y), the joint portion (21Y) does not protrude outward, improving the appearance and making it easier to hold. The width (overlap) of the joint portion (21Y) of the body (2) is preferably 5 to 20 mm, and more preferably 10 to 18 mm. If the width is less than 5 mm, sealing the joint portion (21Y) may be difficult. On the other hand, if the width exceeds 20 mm, the width of the joint portion (21Y) becomes larger than necessary, which leads to increased costs. Furthermore, when the joint portion (21Y) is folded to one side so as to overlap with the outer surface of the body (2) and joined to the outer surface, wrinkles or other defects in appearance may occur in the joint portion (21Y).
[0041] In manufacturing the above cup container (1Y), the fifth step of forming the body (2) is carried out as follows. That is, both end edge portions of the body blank (20A) are overlapped in a palm-to-palm manner, and the inner heat-fusible resin layers (202) constituting the overlapping surfaces are joined together by a first heat fusion to form a cylindrical body (2) having a palm-to-palm portion (21Y). The first heat fusion is usually performed by heat sealing using a hot plate or the like, but may also be performed by high-frequency sealing, ultrasonic sealing, or the like. Next, the joint portion (12Y) is folded to one side and placed on the outer surface of the body (2), and in this state, a second heat fusion is performed by high frequency sealing. As a result, the inner heat fusion resin layers (202) constituting the overlapping surfaces of both end edges of the body blank (20A) are further heat fused to each other, and at the same time, the inner surface of the folded joint portion (21Y) and the outer heat fusion resin layers (203) constituting the overlapping outer surface of the body (2) are heat fused to each other, and the joint portion (21Y) is joined to the outer surface of the body (2). The above-described two-stage heat sealing process ensures that both end edges of the body blank (20A) are more reliably joined together, and the heat sealing makes it easier for resin pools to form at the joints, and furthermore, prevents deformation and other problems associated with heat sealing. The suitable conditions for carrying out the heat sealing and high frequency sealing are the same as those in the fourth step of the above-mentioned first embodiment. EXAMPLES
[0042] Next, specific examples of the present invention will be described, but the present invention is not limited to the following examples.
[0043] <Example 1> A two-component curing urethane adhesive was applied at approximately 3 g / m2 to both sides of a 100 μm thick aluminum foil (A8021H-O) that had been chemically treated. 2 The adhesive was applied and dry laminated to a 30 μm-thick non-oriented polypropylene film (CPP), and then a predetermined aging treatment was performed to harden the adhesive, thereby obtaining a laminate. Next, the obtained laminate was punched into a predetermined shape to form a body blank and a bottom blank (see Figs. 5 and 6). Then, using the body blank and the bottom blank, a cup-shaped container having the configuration shown in FIGS. 1 and 2 was produced by the same process as in the first embodiment described above. This was designated as Example 1. The cup-shaped container is made of 100 μm thick aluminum foil, so it has good barrier properties and is almost completely impermeable to oxygen and water vapor. The dimensions of the cup-shaped container were as follows: -Inner diameter of the opening at the top of the cup-shaped container: 65mm -Inner diameter of the bottom of the cup-shaped container: 50mm Flange width: 4mm Height of cup: 95mm Height of the cup-shaped container's legs (hanging part (32)): 6 mm -Width of fuselage overlap (overlap): 8mm In producing the cup-shaped container, the four steps of forming the body and the fifth step of integrating the body and the bottom were each performed under the following sealing conditions for the two-stage heat fusion. [First heat fusion] Equipment used: Heat sealer Sealing temperature: 180℃ Sealing time: 2sec Load capacity: 150kgf [Second heat fusion] Equipment used: High-frequency sealing device (manufactured by BME Co., Ltd., model BMD-1S) Power setting: 0.75kW Sealing time: 3.0sec Load capacity: 100kgf Coil distance: 5mm
[0044] <Comparative Example 1> In each of the fourth step of forming the body and the fifth step of integrating the body and the bottom body, heat sealing was performed only once under the same conditions as the first heat sealing in Example 1, and otherwise a cup-shaped container was produced in the same manner as Example 1, and this was designated Comparative Example 1.
[0045] <Verification of container sealability> Ten cup-shaped containers of each of Example 1 and Comparative Example 1 above were prepared, and each was filled with 50 cc of water colored with red ink and left for 120 minutes. After that, the presence or absence of coloring in these areas was visually checked to see if water was leaking from the overlapping part of the body or the seal part between the lower end of the body and the hanging part of the base. In the case of Example 1, no coloring was observed in the overlapping portion of the body or in the seal portion between the lower end of the body and the hanging portion of the bottom body in any of the containers. On the other hand, in Comparative Example 1, discoloration was observed in the overlapping portions of the bodies of two containers. [Industrial Applicability]
[0046] The present invention can be suitably used as a method for manufacturing a cup-shaped container for containing, for example, a liquid food or beverage. [Explanation of symbols]
[0047] (1)(1X)(1Y): Cup-shaped container (2): Torso (2a): Lower end of the fuselage (21): Overlap section (21Y): Gassho-bu (23): Flange (20A): Body blank (20): Laminate (201): Metal foil layer (202): Inner heat-sealable resin layer (203):Outer heat-fusible resin layer (3): Bottom body (31):Bottom (32): Drooping part (30A): Bottom blank (30): Laminate (301):Metal foil layer (302): Upper heat-sealable resin layer (303): Lower heat-fusible resin layer
Claims
1. a step of punching out a laminate including a metal foil layer and a heat-sealable resin layer laminated on at least one of both surfaces of the metal foil layer that will be the inner surface of the body, and no paper layer, to form a body blank; A step of forming a blank for a bottom body by punching out a laminate including a metal foil layer and a heat-sealable resin layer laminated on at least the upper surface of the bottom body out of both sides of the metal foil layer, and having no paper layer; A step of forming a bottom body having a cross section of a generally inverted U-shape by drawing a bottom body blank so as to form a bottom portion and a hanging portion extending downward from an outer peripheral edge portion of the bottom portion; forming a cylindrical body by overlapping both end edge portions of the body blank and heat-sealing the heat-sealable resin layers constituting the overlapping surfaces of the body blank; and overlapping the inner surface of the lower end of the body and the outer surface of the hanging portion of the bottom body, and heat-sealing the heat-sealable resin layers constituting these surfaces together to integrate the body and the bottom body. A method for manufacturing a cup-shaped container, in which, in a process for forming a cylindrical body, heat-sealable resin layers at both end edges of a body blank are heat-sealed twice, the first heat-sealing being by heat sealing and the second heat-sealing being by high-frequency sealing, and a resin pool is formed at the joint between the heat-sealable resin layers.
2. In the step of forming a body blank, a laminate in which a heat-fusible resin layer is laminated on both sides of a metal foil layer is used, 2. A method for manufacturing a cup-shaped container as claimed in claim 1, wherein in the process of forming the cylindrical body, both end edges of the body blank are overlapped in a folded shape, and the heat-fusible resin layers constituting the overlapping surfaces are joined together by a first heat fusion using heat sealing to form a cylindrical body having a folded portion, and then the folded portion is folded to one side and placed over the outer surface of the body, and a second heat fusion using high-frequency sealing is performed to join the folded portion to the outer surface of the body.
3. 3. A method for manufacturing a cup-shaped container as claimed in claim 1 or 2, wherein in the step of integrating the body and the bottom body, the heat-sealing resin layers at the lower end of the body and the hanging portion of the bottom body are heat-sealed twice, and the second heat-sealing is performed by high-frequency sealing.
4. a step of punching out a laminate including a metal foil layer and a heat-sealable resin layer laminated on at least one of both surfaces of the metal foil layer that will be the inner surface of the body, and no paper layer, to form a body blank; A step of forming a blank for a bottom body by punching out a laminate including a metal foil layer and a heat-sealable resin layer laminated on at least the upper surface of the bottom body out of both sides of the metal foil layer, and having no paper layer; A step of forming a bottom body having a cross section of a generally inverted U-shape by drawing a bottom body blank so as to form a bottom portion and a hanging portion extending downward from an outer peripheral edge portion of the bottom portion; forming a cylindrical body by overlapping both end edge portions of the body blank and heat-sealing the heat-sealable resin layers constituting the overlapping surfaces of the body blank; and a step of integrating the body and the bottom body by heat-sealing the heat-sealable resin layers constituting the inner surface of the lower end of the body and the outer surface of the hanging portion of the bottom body, A method for manufacturing a cup-shaped container, in which, in a process of integrating a body and a bottom body, the heat-sealable resin layers at the lower end of the body and the hanging portion of the bottom body are heat-sealed twice, the first heat-sealing being by heat sealing and the second heat-sealing being by high-frequency sealing, and a resin pool is formed at the joint between the heat-sealable resin layers.
5. In the step of forming a bottom blank, a laminate in which a heat-fusible resin layer is laminated on both sides of a metal foil layer is used, 5. A method for manufacturing a cup-shaped container as claimed in claim 3 or 4, wherein in the step of integrating the body and the bottom body, the body is folded inward from the edge of the lower opening of the body so as to enclose the hanging portion of the bottom body to form a folded portion, and the body and the bottom body are integrated by heat fusing together the heat-sealable resin layers constituting the overlapping surfaces of the lower end and folded portion of the body and the hanging portion of the bottom body, and the heat-sealing of the heat-sealable resin layers of the lower end and folded portion of the body and the hanging portion of the bottom body is performed twice, the first heat fusing being performed by heat sealing and the second heat fusing being performed by high-frequency sealing, and a resin pool is formed at the joint between the heat-sealable resin layers.
6. A method for manufacturing a cup-shaped container according to any one of claims 1 to 5, wherein the heat-sealable resin layers of the body blank and the bottom blank are composed of a single-layer or multi-layer polyolefin film.
Citation Information
Patent Citations
Vessel with sealing cover
JP1983030955A
Paper container having no cut edge of paper on inner surface of container
JP2001301739A
Synthetic resin cuplike container
JP2007176505A
Paper cup
JP2007210639A
Paper container
JP2012012039A