2-blade ball end mill

The ball end mill with optimized rake and relief angles addresses cutting resistance and tool wear issues, enhancing machining accuracy and reducing burrs for high-hardness materials.

JP7569633B2Active Publication Date: 2024-10-18NISSHIN KOGU
View PDF 17 Cites 0 Cited by

Patent Information

Application Number
JP2020110088
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-06-26
Publication Date
2024-10-18
Estimated Expiration
2040-06-26

AI Technical Summary

Technical Problem

Existing two-flute ball end mills face issues with high cutting resistance, low machining accuracy, rapid tool wear, and burr formation due to negative rake angles and large cutting edge angles, particularly when cutting high-hardness materials.

Method used

The ball end mill is designed with a rake angle ranging from -5° to 10° and a relief angle of 15° to 25°, forming an acute cutting edge angle, which reduces cutting resistance and suppresses tool wear, while the clearance angle of 15° to 25° enhances machining accuracy and minimizes burr formation.

Benefits of technology

This configuration improves machining accuracy, extends tool life, and reduces burr formation, ensuring high precision in both rough and finishing machining of high-hardness materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007569633000001
    Figure 0007569633000001
  • Figure 0007569633000002
    Figure 0007569633000002
  • Figure 0007569633000003
    Figure 0007569633000003
Patent Text Reader

Abstract

To provide a two-blade ball end mill that improves processing accuracy and restrains tool wear by reducing cutting resistance.SOLUTION: A two-blade ball end mill 1 has a substantially semispherical cutting edge part 3 on a tip side of a tool body which is rotatable around a central axis O. A tip surface of the cutting edge part 3 is provided with a two bottom blades 5 formed in a substantially 1 / 4 circular arc shape, a gash groove 4 formed on a front side in a rotation direction of the bottom blade 5 and having a rake face 7 of the bottom blade 5, and a flank 6 formed on a rear side in the rotation direction of the bottom blade 5. The two bottom blades are arranged at a position that is opposite the central axis O by substantially 180 degrees, with a chisel edge 10 passing through the central axis O being arranged at its inside end part. A rake angle of the rake face 7 of the bottom blade 5 is set in a range of -5° to 10°. A clearance angle of the flank 6 of the bottom blade 5 is set in a range of 15° to 25°.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a two-blade ball end mill having two bottom cutting edges disposed on a cutting edge portion at the tip of a tool body. [Background technology]

[0002] In the field of precision machining, ball end mills and the like are generally used to cut high-hardness materials such as dies, precision parts, etc. Furthermore, cutting of high-hardness workpieces requires high-precision cutting that can form a stable machined surface for a long period of time.

[0003] For example, in the two-blade ball end mill described in Patent Document 1, two approximately arc-shaped bottom blades are formed at equal intervals in the circumferential direction on the tip surface of the approximately hemispherical cutting blade part of the tool body. The rake angle of each bottom blade is set in the range of -15° to -35° near the 90° outer periphery of the bottom blade, and in the range of -20° to -40° at the center of rotation. The relief angle of each bottom blade is set in the range of 12° to 20° near the 90° outer periphery of the bottom blade, and in the range of 15° to 30° at the center of rotation of 0°. This ensures cutting edge strength and clearance, and reduces wear and chipping even during 3D machining.

[0004] Moreover, the two-blade ball end mill described in Patent Document 2 is a small-diameter ball end mill with an outer diameter of 3 mm or less, and when viewed in a cross section in the normal direction of the tip, the cutting tool angle (cutting edge angle) between the normal reference line and the first relief surface is set to 85° to 90°, and the relief angle is set in the range of 0.5° to 5.0°. This ensures the cutting edge angle and suppresses wear of the bottom cutting edge, particularly the wear of the chisel blade. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] Japanese Patent Application Publication No. 6-218612 [Patent Document 2] JP 2005-342835 A Summary of the Invention [Problem to be solved by the invention]

[0006] However, the ball end mill described in Patent Document 1 has a negative rake angle on the bottom cutting edge, which results in a large cutting edge angle, resulting in high cutting resistance, low machining accuracy, and the tendency to produce burrs. The ball end mill described in Patent Document 2 has a large cutting edge angle and a small relief angle, which results in the problem that the cutting surface is easily scraped, wear progresses quickly, burrs are easily produced, and uncut areas are easily produced.

[0007] The present invention has been made in consideration of the above-mentioned circumstances, and aims to provide a two-blade ball end mill that improves machining accuracy, reduces cutting resistance, and suppresses tool wear. [Means for solving the problem]

[0008] The two-blade ball end mill according to the present invention is a ball end mill having a cutting edge portion at the tip side of a tool body rotatable around a central axis, and is characterized in that it is equipped with two bottom blades having arc-shaped portions formed on the tip surface of the cutting edge portion, a gash groove formed on the front side in the direction of rotation of the bottom blades and having a rake face of the bottom blade, and a clearance face formed on the rear side in the direction of rotation of the bottom blade, and the rake angle of the bottom blades is set in the range of -5° to 10° and the clearance angle of the bottom blades is set in the range of 15° to 25°. According to the present invention, the rake angle of the bottom cutting edge is set to -5° to 10°, and the clearance angle is set to 15° to 25°, so that the cutting edge angle is set to an acute angle, and even if the workpiece is a high-hardness material, the cutting performance is good, the cutting resistance can be reduced, and tool wear can be suppressed. Therefore, in rough machining, the cutting performance is good and the tool life can be improved, and in finish machining, machining errors can be suppressed, the machined surface can be finished with high precision, and the amount of burrs generated can be suppressed.

[0009] It is also preferable that the cutting edge angle of the bottom cutting edge is set to an acute angle. If the bottom cutting edge is set at an acute angle, the machining accuracy of the workpiece is improved. The bottom cutting edge may also be provided with a coating film for cutting high-hardness materials. This ensures the strength of the end cutting edge, which has an acute cutting edge angle, even when the workpiece is a high-hardness material, thereby improving machining precision and the life of the cutting edge. Effect of the Invention

[0010] According to the two-blade ball end mill of the present invention, the rake angle of the bottom cutting edge is set in the range of -5° to 10°, and the clearance angle is set in the range of 15° to 25°, so that the cutting edge angle is acute and the clearance angle is strong, which improves the machining accuracy and reduces the cutting resistance, suppresses tool wear, and improves the tool life. Moreover, because the clearance angle is set strong, scraping of the machined surface is suppressed, preventing the generation of burrs. [Brief description of the drawings]

[0011] [Figure 1] FIG. 2 is a side view showing a cutting edge portion of a ball end mill according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a view of a tip surface of a cutting edge portion of the ball end mill shown in FIG. [Diagram 3] FIG. 2A is a cross-sectional view showing the cutting edge angle of the bottom cutting edge according to an embodiment, and FIG. 2B is a cross-sectional view showing the cutting edge angle of the bottom cutting edge according to a conventional technology. [Figure 4] Table 1 shows the rake angle, clearance angle, and cutting edge angle of the cutting edge shape of Conventional Examples 1 and 2 and the embodiment, as well as the machining error, burr amount, and machined surface of the finish machining. [Diagram 5] FIG. 2 is a perspective view showing a machined shape of a workpiece. [Figure 6] 6 is a graph showing the state of Conventional Examples 1 and 2 and the embodiment 1 hour and 3 hours after machining, where (a) is a graph showing the amount of machining error, and (b) is a graph showing the amount of burrs. [Figure 7] FIG. 1 is a diagram showing the roughness of the machined surface and the pattern of the cut surface after machining for three hours for Conventional Examples 1 and 2 and the Example. [Figure 8] FIG. 2 is a diagram showing the wear state after cutting with each bottom cutting edge of Conventional Examples 1 and 2 and the embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS A ball end mill according to an embodiment of the present invention will now be described with reference to the accompanying drawings. 1 to 3 show a two-blade ball end mill 1 according to an embodiment of the present invention. In Fig. 1 to 3, the ball end mill 1 according to this embodiment includes a tool body 2 formed in a substantially cylindrical shape and rotated about a central axis line O, and a cutting blade portion 3 brazed to or integrally formed with the tip of the tool body 2. Carbide alloy, cBN, PCD (sintered diamond), etc. can be appropriately used for the cutting edge portion 3. The ball end mill 1 according to the present embodiment is used for a small-diameter ball end mill 1 having a maximum outer diameter D of the substantially hemispherical cutting edge portion 3 of, for example, 6.0 mm or less.

[0013] This ball end mill 1 is used for cutting high-hardness materials such as small precision machine parts and dies, non-ferrous metals, general steel materials, etc. In this specification, the side of the cutting edge portion 3 along the central axis O of the tool body 2 is referred to as the tip side or tip, and the opposite side connected to the spindle is referred to as the base side or base.

[0014] 1 and 2, the cutting edge portion 3 of the ball end mill 1 has a tip surface formed in an approximately hemispherical shape, and a plurality of, for example, two gash grooves 4 are formed in a concave shape facing each other from the base end side to the tip end side at intervals of approximately 180 degrees in the circumferential direction. A clearance surface 6 is formed on the rear side of each gash groove 4 of the cutting edge portion 3 in the rotation direction centered on the central axis O, and a bottom cutting edge 5 in the shape of an approximately quarter arc is formed at the intersection ridge of the gash groove 4 and the clearance surface 6. Each bottom cutting edge 5 is formed with the center raised. The surface of each gash groove 4 facing the front side in the rotation direction of the tool body 2 forms the rake surface 7 of the bottom cutting edge 5.

[0015] In the conventional ball end mill, the rake angle of the rake face 7 of the bottom cutting edge 5 is set to a negative angle, but in this embodiment, the rake angle α is set in the range of -5° to +10°. By setting the rake angle α to a stronger positive angle than in the past, cutting performance can be improved and cutting resistance can be reduced. Moreover, since the bottom cutting edge 5 is formed with the center raised, chipping resistance and wear resistance can be improved. On the other hand, if the rake angle α is less than -5°, the negative angle becomes too large and the above effect cannot be achieved, and if it exceeds +10°, the cutting edge angle becomes too small and the cutting edge becomes easily chipped.

[0016] The clearance angle β of the clearance face 6 formed on the rear side of the bottom cutting edge 5 in the rotation direction is set to a positive angle in the range of 15° to 25°. By setting the clearance angle β larger than that of the conventional product, the cutting ability of the bottom cutting edge 5 can be improved, the cutting resistance can be reduced, and the thrust force can be made smaller. Also, if the clearance angle is less than 15°, there is a drawback in that the cutting ability of the bottom cutting edge 5 is reduced and the cutting resistance increases. Therefore, due to the relationship between the rake angle α and clearance angle β of the bottom cutting edge 5, the cutting edge angle (cutting edge angle) is set to an acute angle in the range of 55° to 80°. Therefore, the bottom cutting edge 5 has good cutting properties and can reduce cutting resistance.

[0017] The rake angle α of the bottom cutting edge 5 may gradually change from the outer periphery (90° side) toward the central axis O (0° side) within the range of -5° to +10° toward the negative angle side or the positive angle side, or may be maintained at the same angle. Similarly, the clearance angle β may gradually change from the outer periphery (90° side) toward the central axis O (0° side) within the range of 15° to 25° so as to become larger or smaller, or may be maintained at the same angle. The gash groove 4 having the rake face 7 of the bottom cutting edge 5 in the cutting edge portion 3 is connected to the flute groove 9 at its base end, and the flute groove 9 is twisted backward in the rotation direction by the same twist angle as the gash groove 4 or by a twist angle larger than that of the gash groove 4. Therefore, the chips flow from the rake face 7 through the gash groove 4 to the outside, or flow smoothly from the gash groove 4 to the flute groove 9 and are discharged to the outside.

[0018] The two bottom blades 5 are disposed facing each other with approximately 180° rotational symmetry about the central axis O. Moreover, in Fig. 2, the two bottom blades 5 are connected via a chisel blade 10 passing through the central axis O at the end on the central axis O side. The flank 6 of each bottom blade 5 has a first flank 6a and a second flank 6b successively facing rearward in the rotational direction, with the first flank 6a having a clearance angle β in the range of 15° to 25°, and the second flank 6b continuing from the first flank 6a having a positive clearance angle even larger than the clearance angle β.

[0019] 2, a chisel blade 10 including a central axis O is provided between the inner ends of the two bottom blades 5. The chisel blade 10 is formed in a straight line, but may be formed in a concave curve or a convex curve. The chisel blades 10 are formed along a substantially hemispherical path drawn by the rotation of the arc-shaped bottom blade 5 about the central axis O. The chisel blades 10 following each bottom blade 5 are formed so that their inner ends join on the central axis O, but the chisel blades 10 do not need to intersect on the central axis O and may be offset from each other.

[0020] Next, a cutting method for a workpiece using the ball end mill 1 according to this embodiment will be described. While rotating the ball end mill 1 around the central axis O, a vertical wall is machined perpendicular to the workpiece by the contour machining method. When cutting, the bottom cutting edge 5 of the cutting edge portion 3 cuts the workpiece, and the generated chips travel along the rake face 7 of the gash groove 4, flow toward the base end, and are discharged to the outside. In this case, the bottom cutting edge 5 formed on the outer peripheral surface of the cutting portion 3 has a rake angle in the range of -5° to +10° and a clearance angle in the range of 15° to 25°, so that even in rough machining with high cutting resistance, the bottom cutting edge 5 has high cutting ability, reduces cutting resistance, and also improves chipping resistance and wear resistance.

[0021] At the tip of the cutting portion 3, a chisel blade 10 is connected to the inner end of the bottom blade 5. The chisel blade 10 is rotated at a low speed, but the bottom blade 5 is formed with a sharp cutting edge with a large rake angle α on the positive side, and the chisel blade 10 is a small area, so the cutting performance and rigidity of the entire bottom blade 5 are ensured. During finishing, the cutting depth is small and the cutting resistance is small, so that the wear of the chisel blade 10 in the center is reduced, resulting in a finished surface with small surface roughness. Furthermore, if the flank 6 scrapes the machined surface of the workpiece during cutting, burrs are likely to occur, but since the clearance angle β is set large, within the range of 15° to 25°, the flank does not scrape the machined surface, and therefore burrs are unlikely to occur on the machined surface of the workpiece.

[0022] As described above, in the two-blade ball end mill 1 of this embodiment, the rake angle of the bottom cutting edge 5 is set on the positive side of -5° to 10°, and the clearance angle is set strong at 15° to 25°, so that even if the workpiece is of high hardness, good machining accuracy is achieved, cutting resistance is reduced, tool wear is suppressed, and tool life is improved. In addition, the ball end mill 1 according to this embodiment can perform high-precision machining not only in rough machining but also in finish machining. Moreover, since the rake angle α is on the positive side, the clearance angle β is large, and the cutting edge angle is formed as an acute angle, the cutting performance is good and the amount of burrs generated on the machined surface of the workpiece can be suppressed.

[0023] Next, cutting tests carried out on the example of the ball end mill 1 according to the embodiment and the conventional example will be described with reference to FIGS. In this test example, the example uses a two-blade ball end mill 1 according to the embodiment, the conventional example 1 is a two-blade ball end mill corresponding to the invention of the above-mentioned Patent Document 1, and the conventional example 2 is a two-blade ball end mill corresponding to the invention of Patent Document 2. The work material was HAP40 (HAP is a registered trademark, and the common name is SKH. 64HRC). Using the ball end mills of the embodiment, conventional example 1, and conventional example 2, rough machining and finish machining (contour machining) were performed by mounting them on a machine tool. The results are shown in Table 1 in Figure 4. In addition, in the cutting performance shown in Table 1, ◯ is good, △ is slightly poor, and × is poor.

[0024] The embodiment, conventional example 1, and conventional example 2 each have the end cutting edge shapes shown in Table 1 of FIG. 4, and rough machining and finish machining were performed on these. Table 1 shows a comparison of the lifespan of the bottom cutting edge 5 and the machining accuracy of the machined surface after rough cutting and finish cutting of the work material HAP40 (64HRC) in the embodiment, conventional example 1, and conventional example 2. In addition, in the cutting performance shown in Table 1, the lifespan of the bottom cutting edge 5 in rough cutting is shown as the time until it is significantly damaged, and in finish cutting, the amount of machining error, the amount of burrs generated on the machined surface of the work material, and the finished shape of the machined surface were observed. In the results in Table 1, ◯ is good, △ is slightly poor, and × is poor. From the results shown in Table 1, Conventional Example 1 was △ (slightly poor) in both rough cutting and finish cutting, and Conventional Example 2 was slightly poor in rough cutting life and burr amount in finish cutting. In contrast, the working examples were good in both rough cutting and finish cutting and had a long life.

[0025] Next, the embodiment, conventional example 1, and conventional example 2 were subjected to a performance test in finishing. The work material was HAP40 (64HRC). The rotation speed n of the embodiment, conventional example 1, and conventional example 2 was 18000 min -1 The table feed rate Vf was 1000 mm / min, the single blade feed rate fz was 0.028 mm / tooth, the finishing allowance was 0.03, and the movement amount pf of the machining tool was 0.03 mm. Oil mist was used as the coolant, and the machining time was 3 hours. The workpiece was machined into a shape that would form a recess with an inclined surface by performing rough machining and finishing, as shown in Figure 5. The machined surface of the recess had a vertical 90-degree side, a 45-degree incline, and a horizontal bottom, and the machined size was 43.7 mm x 23.0 mm in length and width, and 12.0 mm in depth. One workpiece was machined per hour, and three pieces were machined in three hours. The machined surface roughness of the 90-degree side, 45-degree incline, and horizontal bottom of the recess after machining of the workpiece was measured.

[0026] The results of finish machining of a workpiece HAP40 (64HRC) as shown in Fig. 5 using each of the two-blade ball end mills of the Example, Conventional Example 1, and Conventional Example 2 are shown in Figs. 6 to 7. Figs. 6(a) and 6(b) show the results of measuring the amount of machining error and the amount of burrs one hour and three hours after machining for the Example, Conventional Example 1, and Conventional Example 2. Both the amount of machining error and the amount of burrs for the Example were smaller than those for Conventional Examples 1 and 2. 7 shows the machining marks (patterns) and surface roughness of the bottom cutting edge 5 generated after machining the cutting surface after 3 hours of machining for the embodiment, conventional example 1, and conventional example 2. The surface roughness of the embodiment was smaller than that of conventional example 1, and was about the same as that of conventional example 2. The difference in the patterns of the machining marks in the embodiment, conventional example 1, and conventional example 2 is due to the difference in the shape of the chisel blade 10.

[0027] Next, Fig. 8 is a photograph showing the shape of the end cutting edge 5 after rough cutting for 1.5 hours. The work material is HAP72 (69HRC). In Conventional Examples 1 and 2, the area around the central axis O of the bottom cutting edge 5 and the chisel blade 10 were significantly damaged, making further cutting difficult. On the other hand, in the Example, the area around the central axis O of the bottom cutting edge 5 and the chisel blade 10 were only slightly damaged and slightly worn. From the above test results, the embodiment had a longer tool life in rough machining than the conventional examples 1 and 2. In addition, the machining error and machining accuracy of the workpiece after finishing were good, and the amount of burrs was small. Therefore, it was confirmed that the embodiment has a smaller cutting resistance of the bottom cutting edge 5 than the conventional examples 1 and 2, and can suppress wear.

[0028] Although the ball end mill 1 according to the embodiment of the present invention has been described above, it goes without saying that the present invention is not limited to such an embodiment and that appropriate modifications and variations can be adopted within the scope of the present invention. All of these are included in the technical scope of the present invention. Modifications of the present invention will be described below, but the same reference numerals will be used to describe the same or similar parts as those in the above-described embodiment.

[0029] Instead of the two-blade ball end mill 1 according to the above-described embodiment, an appropriate coating layer may be formed on the surface of the cutting edge portion 3 having the bottom cutting edge 5. For example, the cutting edge portion 3 may be made of a material such as cemented carbide, cBN, cermet, ceramics, etc., and the surface of the cutting edge portion 3 may be coated with a coating for cutting high-hardness materials that appropriately contains nitrides or carbides of Ti, Si, Cr, etc. By forming a coating layer on the surface of the bottom blade 5, the bottom blade 5, which is prone to chipping due to the sharp cutting edge angle, can be strengthened by the coating layer, thereby suppressing damage and wear of the bottom blade 5 and further improving the tool life.

[0030] In the ball end mill 1 according to the embodiment described above, the cutting edge portion 3 is formed with two bottom blades 5, and the two bottom blades are arranged at equal intervals at positions that are 180 degrees apart, but the two bottom blades 5 may be arranged at unequal intervals. Arranging the two bottom blades 5 at unequal intervals can prevent resonance during cutting, suppress vibration, and ensure cutting balance. [Explanation of symbols]

[0031] 1, 20 Ball end mill 2 Tool body 3 Cutting edge 4 Gash groove 5 Bottom blade 6 Flank 7. Scooping surface 10 Chisel blade O center axis

Claims

[Claim 1] In a two-blade ball end mill having a cutting edge portion at the tip side of a tool body that can rotate around a central axis, Two bottom blades each having a substantially arcuate portion formed on a tip surface of the cutting blade portion; A gash groove is formed on a front side of the bottom cutting edge in a rotational direction and has a rake face of the bottom cutting edge; A flank surface formed on a rear side of the end cutting edge in a rotation direction; The bottom cutting edge is formed with an acute cutting edge having a rake angle in the range of 0° to 10° and a clearance angle of the bottom cutting edge in the range of 15° to 25°, The rake angle of the end cutting edge gradually changes from the outer periphery (90° side) to the center axis (0° side) within a range of 0° to 10°, This two-blade ball end mill is characterized in that the clearance angle of the bottom cutting edge is gradually increased or decreased in the range of 15° to 25° from the outer periphery (90° side) toward the central axis (0° side).

Citation Information

Patent Citations

  • End mill

    CN110508854A

  • Ball end mill

    JP1994218612A

  • ball end mill

    JP1995020211U

  • end mill

    JP1996507724A

  • Ball end mill

    JP1998263913A