Biosensor with a porous core layer
The integration of a porous wicking layer with enzymes in OTFT sensors addresses the inefficiencies in liquid sample detection, enabling rapid and accurate glucose sensing in saliva, paving the way for non-invasive blood sugar monitoring.
Patent Information
- Application Number
- JP2020564669
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2018-05-15
- Filing Date
- 2019-05-15
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2039-05-15
AI Technical Summary
Existing organic thin film transistor (OTFT) sensors face challenges in efficiently detecting analytes in liquid samples, particularly glucose in saliva, due to limitations in liquid uptake and analyte exposure within the device, which affects detection speed and accuracy.
Incorporating a porous wicking layer containing enzymes into the OTFT sensor, which enhances liquid uptake through capillary action and ensures efficient exposure of analytes to enzymes, promoting the generation of charge carriers for rapid detection.
The porous layer improves liquid sample incorporation and analyte exposure, resulting in rapid and accurate detection of glucose in saliva by generating charge carriers efficiently, enabling a commercially viable glucose sensor for non-invasive blood sugar level monitoring.
Smart Images

Figure 0007570679000002 
Figure 0007570679000003 
Figure 0007570679000004
Abstract
Description
[Technical field]
[0001] The present invention relates to organic thin film sensors and their preparation and use in sensing applications, particularly glucose (dextrose) sensing applications. [Background technology]
[0002] The development of organic thin film transistor (OTFT) sensors has grown rapidly in recent years, primarily motivated by the unique physical properties of polymer devices, such as their flexibility and ability to be fabricated using low-cost solution-based techniques. Development efforts of OTFTs for new and existing applications have focused on two main areas. First, systematic improvements in materials and fabrication processes have led to improvements in traditional performance parameters of organic devices, making them comparable to inorganic devices. Second, improvements in the film morphology of the organic semiconductor layer have been made with the goal of eliminating electron and / or hole traps and enhancing free carrier transport in polymer semiconductor materials. Progress has also been made in the development of high capacitance organic dielectric layers, with significant improvements in OTFT performance reported. The inherent compatibility of organic materials with biomolecules makes OTFTs suitable for use in biosensing applications.
[0003] The inventors have successfully fabricated an OTFT device that can detect analyte levels over a wide range of concentrations, and is simple and relatively inexpensive to manufacture. This device may pave the way for commercially viable glucose sensors that can estimate blood glucose concentrations by detecting glucose levels in saliva as opposed to blood. Such a device could eliminate the need for diabetic patients to obtain blood samples to determine their blood glucose levels. The device may also pave the way for sensing of other analytes in a similar manner.
[0004] A reference to prior art in the specification is not an admission or suggestion that this prior art forms part of the common general knowledge in any jurisdiction, or that this prior art could reasonably be expected to be understood, considered relevant, and / or incorporated with other pieces of prior art by a person skilled in the art. Summary of the Invention [Means for solving the problem]
[0005] According to a first aspect of the present invention there is provided an organic thin film transistor based sensor for detecting the presence of an analyte in a liquid sample, the sensor comprising: A porous wicking layer having a first surface and a second surface, the first surface being configured to receive a liquid sample. An enzyme disposed on or within the porous layer, the enzyme facilitating the generation of charge carriers from the analyte. a polymer gate layer in contact with the second surface of the porous layer, the polymer gate layer being configured to be connected to an ohmic conductor for applying a gate voltage to the polymer gate layer, the polymer gate layer being conductive to charge carriers. An organic semiconductor layer configured to be connected to a source electrode and a drain electrode.
[0006] In one embodiment, the sensor further includes an ohmic conductor in contact with the polymer layer configured to apply a gate voltage to the polymer gate layer.
[0007] In one embodiment, the organic semiconductor layer is connected between a source electrode and a drain electrode.
[0008] In one embodiment, the porous layer has a thickness of about 50 nm to about 500 μm. Preferably, the thickness is at most 200 μm. More preferably, the thickness is at most 100 μm. Even more preferably, the thickness is at most 80 μm. Most preferably, the thickness is at most 60 μm. Alternatively or additionally, the thickness is from 500 nm. More preferably, the thickness is from 1 μm. Even more preferably, the thickness is from 20 μm. Most preferably, the thickness is from 40 μm. In a preferred form, the thickness is about 50 μm.
[0009] In one embodiment, the porous layer is formed of a material such that the contact angle of a liquid, preferably a biological fluid, more preferably diluted saliva, or undiluted or untreated saliva ("neat saliva"), at the first surface of the porous layer is 60° or less. Preferably, the contact angle is 50° or less. More preferably, the contact angle is 45° or less. Even more preferably, the contact angle is 40° or less. Most preferably, the contact angle is 38° or less.
[0010] In one embodiment, the porous layer comprises a plurality of pores having a pore size of 50 nm to 2000 nm. Preferably, the pore size is up to 1600 nm. More preferably, the pore size is up to 1200 nm. Most preferably, the pore size is up to 1000 nm. Alternatively or additionally, the pore size is from 80 nm. More preferably, the pore size is from 100 nm. Most preferably, the pore size is from 150 nm.
[0011] In one embodiment, the porous layer has a void ratio of about 30% to about 95%. Preferably, the void ratio is up to about 90%. Alternatively or additionally, the void ratio is from about 35%. Preferably, the void ratio is from about 40%. More preferably, the void ratio is from about 45%. Most preferably, the void ratio is from about 50%.
[0012] It will be appreciated that a range of different porous materials may be used to form the porous layer, for example porous ceramic materials, porous metals, porous layers formed from protein fibers, or porous polymer layers. In a preferred form of the invention, the porous layer is a porous polymer layer. The porous polymer layer may be a layer of a homopolymer, copolymer, or polymer blend.
[0013] In certain embodiments, the porous polymer layer comprises, consists of, or consists essentially of a porous polymer, an enzyme, and optionally one or more additives selected from the group consisting of an elastomer, a stabilizer, or a surfactant.
[0014] In those aspects of the invention in which the porous layer is a porous polymer layer, it is preferred that the polymer layer be formed from a polymer having a glass transition temperature of at least 50° C. More preferably, the glass transition temperature is at least 70° C. Even more preferably, the glass transition temperature is at least 80° C. Even more preferably, the glass transition temperature is at least 90° C. Most preferably, the glass transition temperature is about 95° C.
[0015] In those aspects of the invention in which the porous layer is a porous polymer layer, the porous polymer layer is preferably formed from a polymer that is soluble in an organic solvent. Preferably, the polymer is soluble in a polar aprotic solvent, such as, for example, dimethylsulfoxide.
[0016] In the embodiment of the present invention in which the porous layer is a porous polymer layer, the porous polymer layer is preferably formed from a polymer formed from one or more repeating monomer units, and the one or more repeating monomer units do not contain halide atoms.Preferably, the one or more repeating monomer units are composed of C atoms, N atoms, O atoms and H atoms.More preferably, the one or more repeating monomer units are composed of C atoms, N atoms and H atoms.
[0017] In one embodiment, the porous core layer is a porous polyacrylonitrile (PAN) layer.
[0018] In one or more embodiments, the porous wicking layer is layered directly onto the surface of the polymeric gate layer.
[0019] In one or more embodiments, the polymer gating layer is layered directly on the surface of the organic semiconductor layer.
[0020] In one or more embodiments, the sensor also includes a substrate layer. Preferably, at least the source electrode and the drain electrode are disposed on the substrate. In at least one embodiment, the source electrode, the drain electrode, and the organic semiconductor are each in contact with the substrate. The substrate may be glass or any other suitable substrate known to those skilled in the art, such as paper or low-cost plastic, such as polyethylene terephthalate (PET).
[0021] In a preferred form of the invention, the analyte is glucose and the enzyme is glucose oxidase.
[0022] In a second aspect of the invention, there is provided a method of forming an organic thin film transistor-based sensor as defined according to the first aspect of the invention, the method comprising forming a porous core layer by phase inversion.
[0023] In one embodiment, the porous layer is formed in situ on the surface of the polymer gate layer, in an alternative embodiment, the porous layer is first formed on a substrate separate from the organic thin film transistor based sensor and subsequently removed from the substrate and applied to the surface of the polymer gate layer.
[0024] In a third aspect of the invention, there is provided a method of forming an organic thin film transistor-based sensor for detecting the presence of an analyte in a liquid sample, the method comprising the steps of: Providing a layered structure including at least an organic semiconductor layer configured to be connected to a source electrode and a drain electrode, and a polymer gate layer. A porous core layer is disposed on the surface of the polymer gate layer. Here, the porous core layer contains, or is treated to contain, an enzyme to promote generation of charge carriers from the analyte.
[0025] In one embodiment, the step of disposing the porous wicking layer on the surface of the polymeric gate layer comprises forming the porous wicking layer on the surface of the polymeric gate layer by a phase inversion process.
[0026] In one or more embodiments, the phase inversion method includes the following steps. Forming a wet film of a polymer solution on the surface of the substrate, the polymer solution comprising at least a polymer dissolved in a solvent. A non-solvent is applied to the wet film. The non-solvent is miscible with the solvent, forms a porous polymer membrane, and dissolves the solvent through the pores of the porous polymer membrane.
[0027] In one form, the substrate is a surface of the polymer gate layer. In an alternative form, the substrate is an inert layer separate from the organic thin film transistor based sensor, and the method further comprises removing the porous wick layer from the substrate prior to disposing the porous wick layer on the surface of the polymer gate layer.
[0028] Further aspects of the invention and further embodiments of the aspects described in the preceding paragraphs will become apparent from the following description, given by way of example only, with reference to the accompanying drawings, in which: [Brief description of the drawings]
[0029] [Figure 1] 1 is a schematic diagram showing the structure of a device according to one embodiment of the present invention; [Diagram 2] 1 is a schematic diagram showing the structure of a device according to one embodiment of the present invention; [Diagram 3]Scanning electron micrographs (SEM) of poly(acrylonitrile) (PAN) porous membranes. Scale bar in Figure 3(a) is 100 μm, and scale bar in Figure 3(b) is 1 μm. [Figure 4] Photographs showing the contact angle of water on a glucose sensor, Fig. 4(a) with poly(acrylonitrile) (PAN) and Fig. 4(b) without PAN. [Diagram 5] Figure 5(a) shows an XPS survey scan of a pristine Nafion film. Figure 5(b) shows XPS area scans of a pristine PAN film (solid line), a Nafion / PAN bilayer (dashed line), and a Nafion / PAN bilayer (dotted line) exposed to an analyte solution. [Figure 6] Schematic showing the sensor device architecture incorporating a porous poly(acrylonitrile) membrane. Figure 6(a) shows layer 1, electrode, ITO. Figure 6(b) shows layer 2, polymer semiconductor, P3HT. Figure 6(c) shows layer 3, gate electrode, Nafion. Figure 6(d) shows layer 4, porous membrane, PAN. Figure 6(e) shows layer 5, enzyme, GOX. Each substrate photographed contains two sensors. [Figure 7] Figure 7(a) is a photograph of the sensors placed on the platen of an inkjet printer after printing of the GOX layer. The sensor on the left contains a PAN porous membrane, while the sensor on the right does not. Figure 7(b) shows the sensor response to a 10 mM glucose solution added at t = 180 s to the device with (solid line) and without (dashed line) a PAN membrane. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0030] According to a first aspect of the present invention there is provided an organic thin film transistor based sensor for detecting the presence of an analyte in a liquid sample, the sensor comprising: A porous wicking layer having a first surface and a second surface, the first surface being configured to receive a liquid sample. An enzyme disposed on or within the porous layer, the enzyme facilitating the generation of charge carriers from the analyte. a polymer gate layer in contact with the second surface of the porous layer, the polymer gate layer being configured such that an ohmic conductor can be connected to the polymer gate layer for applying a gate voltage to the polymer gate layer, the polymer gate layer being conductive to charge carriers. An organic semiconductor layer configured to be connected to a source electrode and a drain electrode.
[0031] An exemplary organic thin film transistor-based sensor 100 according to an embodiment of the present invention is shown in FIG. 1, which provides a conceptual representation of the structure of the sensor 100. The sensor 100 includes a drain electrode 102 and a source electrode 104 disposed on a surface of a substrate 106. The sensor includes a three-layer film structure including a porous core layer 108, a polymer gate layer 120, and an organic semiconductor layer 122. The organic semiconductor layer 122 covers a portion of the drain electrode and the source electrode, and the organic semiconductor layer 108 contacts and extends between the drain electrode 102 and the source electrode 104. The polymer gate layer 120 is disposed on a surface of the organic semiconductor layer 122. An ohmic conductor 132 contacts the polymer gate layer 120 so that a gate voltage can be applied to the polymer gate layer 120. The porous core layer 108 is disposed on a surface of the polymer gate layer 120. The surface of the porous core layer 108 is exposed to receive a fluid sample. An enzyme is disposed within and / or on the surface of the porous core layer 108. The porous core layer 100 is not disposed between the gate and drain electrodes. The porous core layer 100 is not configured to allow an ohmic conductor to be connected to the porous core layer.
[0032] The inventors have found it advantageous to incorporate a porous wicking layer containing an enzyme into an organic thin film transistor. There are two main reasons for this. First, when a liquid sample is deposited on the surface of the porous wicking layer, the porous wicking layer exhibits a wicking (capillary action) effect that improves the uptake of the liquid sample into the device, and this wicking effect may ensure the delivery of a standard amount of liquid sample inside the device. Second, the wicking effect leads to excellent wettability of the internal porous structure of the porous wicking layer, resulting in high exposure of the analyte in the liquid sample to the enzyme held in the porous wicking layer. This is beneficial as it leads to efficient generation of charge carriers in the device, resulting in rapid detection of the analyte if it is present in the liquid sample.
[0033] Those skilled in the art will appreciate that the porous wicking layer 108 can be formed from a variety of different materials, including porous ceramics, porous metals, porous protein fibers, or porous polymers. However, porous polymers are generally preferred for ease of sensor fabrication. Suitable polymers include, but are not limited to, polyacrylonitrile, polysulfone, polyethersulfone, polystyrene, polybutadiene, polyisoprene, polyimide, polyamide, and fluoropolymers. Typically, the porous wicking layer is formed from a material that is not the same as the material from which the polymeric gate layer is formed. If the polymeric gate layer is formed from Nafion, the porous wicking layer is not formed from Nafion. Preferably, the porous wicking layer is not formed from Nafion.
[0034] Ideally, the porous wick layer 108 is formed from a material that has a low contact angle with the liquid of the liquid sample so that the liquid sample is rapidly taken up into the porous wick layer 108 and good wetting of the pore surfaces of the porous wick layer 108 is ensured.
[0035] Preferably, the porous core layer is in the form of a layer that allows for the rapid formation of droplets, preferably aqueous droplets, more preferably biofluid droplets, more preferably saliva droplets, such as neat saliva droplets and treated or diluted saliva droplets, which have a low contact angle with the porous core layer on the porous core layer.
[0036] Preferably, the porous wick layer is formed from a layer that is highly wettable by water droplets, more preferably by biofluid droplets, more preferably by saliva droplets, more preferably by neat saliva droplets or treated or diluted saliva droplets.
[0037] Notwithstanding the above, it is preferred that the porous core layer 108 is a porous poly(acrylonitrile) (PAN) layer. PAN has physical properties that make it particularly useful as the porous core layer 108. PAN has a glass transition temperature (T g ) and melting temperature (Tm) (>300°C), making it thermally stable. From this perspective, PAN exhibits good thermal stability, which is desirable for sensors, as it is unlikely to exceed its Tg during typical use; if the Tg is exceeded, the porous structure may collapse. PAN also has high strength, a high elastic modulus, and low density. Furthermore, from a manufacturing standpoint, PAN is soluble in dimethylsulfoxide (DMSO) and can be used to prepare porous polymeric membranes via a phase inversion method - immersion precipitation.
[0038] In a preferred embodiment, the porous wicking layer has a surface energy low enough to allow bodily fluids, preferably saliva, preferably undiluted or otherwise untreated saliva, or treated saliva, to rapidly wet and penetrate the porous wicking layer.
[0039] As described above, the porous core layer 108 includes an enzyme. The enzyme may be disposed on a surface of the porous core layer 108 and / or may be disposed throughout the porous core layer 108 such that the enzyme is exposed on the interior pore surfaces of the porous core layer 108.
[0040] The enzyme is selected to promote the generation of charge carriers when an analyte contacts the device. Charge carriers are typically electrons, anions, or cations (e.g., hydrogen ions / protons). The generation of charge carriers can be further promoted by the presence of an electric field. As described below, these generated charge carriers can participate in electrical current flow through the device. It will be appreciated that for any particular analyte, a range of enzymes may be used. Moreover, given the diversity of enzymes available, devices can be adapted or developed for the detection of a range of analytes by following the disclosure herein.
[0041] A particularly preferred class of enzymes is the oxidoreductases. The oxidoreductases used in the device can act on any one of the following donor functionalities: CH-OH donor groups (alcohol oxidoreductases), aldehyde donor groups or oxo donor groups, CH-CH donor groups (CH-CH oxidoreductases), CH-NH2 donor groups (amino acid oxidoreductases, monoamine oxidases), CH-NH donor groups, NADH or NADPH, other nitrogen compounds as donors, sulfur donor groups, heme donor groups, diphenols and related substances as donors, peroxides (peroxidases) as acceptors, hydrogen as donors, single donors incorporating molecular oxygen (oxygenases), paired donors incorporating molecular oxygen, superoxide radicals as acceptors, CH or CH2 groups, iron-sulfur proteins as donors, reduced flavodoxins as donors, phosphorus or arsenic in the donor, XH and YH to form XY bonds, or oxidoreductases to oxidize metal ions.
[0042] The polymer gate layer 120 is disposed between the porous core layer 108 and the organic semiconductor layer 122. The function of the polymer gate layer 120 is to facilitate the transport of charge carriers generated in the porous core layer 108 from the analyte upon application of a gate voltage. Depending on the nature of the analyte, enzyme and / or charge carrier, a range of different polymers can be used to form the polymer gate layer 120. In a preferred form, the charge carriers are protons (e.g. hydrogen ions) and the polymer gate layer 120 is proton conductive. Preferably, the polymer layer has a conductivity for protons that is greater than the conductivity for protons of the organic semiconductor layer 122. The conductivity may be due to the permeability of the polymer gate layer 120 to the charge carriers, e.g., conduction may occur due to migration of the charge carriers or may occur due to other mechanisms, e.g., the Grotthuss mechanism. When the charge carriers are protons or electrons, the polymer gate layer may be proton conductive or electron conductive.
[0043] In a preferred embodiment of the invention, the polymeric gate layer 120 comprises, consists of, or consists essentially of a sulfonated tetrafluoroethylene-based fluoropolymer-copolymer, such as a copolymer comprising a tetrafluoroethylene backbone and perfluoroalkyl ether groups terminated with sulfonic acid groups. More preferably, the sulfonated tetrafluoroethylene-based fluoropolymer-copolymer is a copolymer of tetrafluoroethylene and perfluoro-3,6-dioxa-4-methyl-7-octene-sulfonic acid. An example of a suitable polymer is tetrafluoroethylene-perfluoro-3,6-dioxa-4-methyl-7-octene-sulfonic acid copolymer (commonly referred to as Nafion).
[0044] In a preferred embodiment of the invention, the polymer gate layer has a thickness in the range of about 50 nm to about 5 μm, preferably about 200 to about 800 nm.
[0045] The organic semiconductor layer 122 is configured to allow the flow of electrical current between the source and drain electrodes as a result of the generation of these charge carriers.
[0046] The organic semiconductor layer 122 comprises one or more organic compounds. Any organic compound having semiconducting properties is suitable for use. However, the one or more organic compounds are preferably selected from the group consisting of polyacetylenes, porphyrins, phthalocyanines, fullerenes, polyparaphenylenes, polyphenylenevinylenes, polyfluorenes, polythiophenes, polypyrroles, polypyridines, polycarbazoles, polypyridinevinylenes, polyarylvinylenes, poly(p-phenylmethylvinylenes), including derivatives and copolymers thereof, and combinations thereof. More preferably, the one or more organic compounds are selected from the group consisting of poly(9,9-dioctylfluorene-2,7-diyl-co-bis-N, N-(4-butylphenyl)-bis-N, N-phenyl-1,4-phenylenediamine), poly(9,9-dioctylfluorene-2,7-diyl-co-benzothiadiazole), poly(3-hexylthiophene), (6,6)-phenyl-C 61 -butyric acid methyl ester, poly(2-methoxy-5-(2'-ethyl-hexyloxy)-1,4-phenylenevinylene), and combinations thereof. Most preferably, the semiconducting layer comprises, consists of, or consists essentially of P3HT.
[0047] In a preferred embodiment of the invention, the organic semiconductor layer has a layer thickness of from 20 nm to 500 nm. Preferably, the layer thickness is at most 350 nm. More preferably, the layer thickness is at most 200 nm. Most preferably, the layer thickness is at most 150 nm. Alternatively or additionally, the layer thickness is from 40 nm. More preferably, the layer thickness is from 60 nm. Most preferably, the layer thickness is from 70 nm.
[0048] The use of sensor 100 is described below in connection with one preferred embodiment, in which sensor 100 is for detecting the presence of glucose in a saliva sample.
[0049] When using, the gate voltage V G and the drain voltage V D is applied to the sensor 100 (the voltage is referenced to the source electrode 104 as shown in FIG. 1), and a liquid sample containing glucose, e.g., a bodily fluid such as saliva, is brought into contact with the porous wick layer 108. The liquid sample is wicked into the internal porous structure of the porous wick layer where glucose in the liquid sample comes into contact with the glucose oxidase enzyme (GOX) present within the porous wick layer. Glucose is decomposed by the enzymatic reaction with GOX to produce H2O2. The gate voltage V G and the drain voltage V D is H2O2 to H + The gate and drain voltages applied are typically between about 0V and -2V, e.g., about -1V.
[0050] H + Ions are conducted from the porous core layer 108 through the polymer gate layer 120 (e.g., Nafion) to the organic semiconductor layer. This causes doping of the semiconductor, which results in a current flow between the drain and source electrodes. While not wishing to be bound by theory, the inventors believe that the gate potential controls the doping and dedoping of the semiconductor compound by ion migration from the ion generation site to the active channel in the organic semiconductor. Thus, H + An increase in ions results in an increase in the drain current, so that a relationship is established between the amount of glucose present in the sample and the magnitude of the drain current, which is then measured to provide an indication of the presence and concentration of glucose in the saliva sample.
[0051] Gate voltage V G and the drain voltage V D is H +The electrical field provided is strong enough to liberate H2O2 from the H2O2, but not so strong as to cause electrolysis of water, which may result in a decrease in the signal-to-noise ratio of the sensor. In at least one embodiment, the gate and drain voltages applied are between about 0V and -2V, e.g., about -1V.
[0052] In an alternative form of the invention, as shown in FIG. 2, a sensor 200 is similar to the sensor 100 of FIG. 1, but further includes a dielectric layer 234 between and in contact with the polymer gate layer 220 and the organic semiconductor layer 222.
[0053] The dielectric layer 234 comprises, consists of, or consists essentially of an organic dielectric material. Preferably, the organic dielectric material has a conductivity for protons greater than the conductivity of the organic semiconductor layer 222. Preferably, the organic dielectric material is a hygroscopic insulator, such as polyvinylphenol. In particular, the dielectric layer may comprise, consist of, or consist essentially of poly(4-vinylphenol).
[0054] Alternative dielectric materials that can be used in the device will be readily apparent to those skilled in the art. Non-limiting examples include polyimide and poly(methyl methacrylate (PMMA). In alternative embodiments, the dielectric layer may comprise a doped dielectric material, for example poly(4-vinylpyridine) doped with lithium perchlorate.
[0055] (e.g. device manufacturing) Pre-patterned ITO-on-glass substrate (15Ω□ -1 ITO (XinYan Technology Co., Ltd.) was used as the substrate and electrodes for the devices. Poly-3-hexylthiophene (P3HT) (MW ~ 20000) was dissolved in CHCl3 (Sigma-Aldrich Co., Ltd.) at various concentrations and sonicated for approximately 1 h or until the material was completely dissolved. Poly-4-vinylphenol (PVP) (Sigma-Aldrich Co., Ltd.) was dissolved in ethanol (Sigma-Aldrich Co., Ltd.) at 80 mg mL -1and sonicated for approximately 1 h or until the material was completely dissolved. Nafion solution (5 wt % in lower aliphatic alcohol and water, Sigma-Aldrich) was used as received.
[0056] The prepatterned ITO-on-glass substrate was washed with methanol and purified water. A solution of P3HT in CHCl3 was spin-coated onto the substrate at 2000 rpm for 60 s. 5 mg mL -1 , 10mg mL -1 , 15 mg mL -1 , 20mg mL -1 , and 40 mg mL -1 P3HT solutions were prepared and the average thicknesses of films spun from these P3HT concentrations were 22 nm, 36 nm, 74 nm, 108 nm, and 390 nm, respectively. The P3HT layers were patterned and left to dry at 40 °C for 15 min. The Nafion solution was first spin-coated at 500 rpm for 120 s.
[0057] The devices exemplified here do not include a dielectric layer, but may include one. A preferred dielectric layer is a PVP layer. For devices that include a PVP layer, a PVP solution is spun onto the P3HT layer at 2000 rpm for 60 seconds to form a film approximately 400 nm thick, which can be patterned and dried. For devices that include PVP, Nafion can be drop cast onto the source-drain channel regions, connected to the ITO gate pads of the substrate, and allowed to dry for approximately 30 minutes.
[0058] Porous polymer membranes can be fabricated using the phase inversion method (immersion precipitation). First, a viscous solution of polyacrylonitrile (PAN) polymer in DMSO solvent is coated onto a flat, rigid substrate, such as glass, to form a uniform "wet" film. The "wet" film can be coated by spin coating, drop casting, or printing techniques, such as slot die coating. The "wet" film is not a solid dry film, but a composite film, containing a polymer network with liquid solvent molecules present in the voids between the polymer chains. Then, when the "wet" film on the rigid substrate is submerged in water (non-solvent), the DMSO solvent diffuses out of the polymer network into the surrounding water bath, and the water diffuses into the polymer network, a porous polymer membrane is formed. It is this solvent exchange with the non-solvent that induces the precipitation of the polymer. The choice of solvent and non-solvent is highly dependent on the selected polymer, the solvent must be capable of dissolving the polymer, while the non-solvent is one in which the polymer is insoluble. The solvent and non-solvent combination must be miscible, otherwise the solvent will not diffuse into the non-solvent and a porous polymer membrane will not form, remaining instead as a "wet" solvent-containing film. Fabrication is a two-step process, with the "wet" film converting to a solid film in the second step. Once the solid film is formed, it is processed into individual layers of the desired size and thickness and applied to the device as the porous core layer.
[0059] To incorporate the GOX into the core layer, the GOX is cast onto the core layer, the porosity of which facilitates the dispersion of the GOX throughout the core layer.
[0060] (Testing the device) The porosity of the PAN membranes prepared by the phase inversion technique was investigated using scanning electron microscopy (SEM) (see Figure 3) on a Zeiss ZP FESEM operating at an accelerating voltage of 2 kV. DMSO was used as the solvent and water was used as the non-solvent in the membrane preparation process. SEM revealed that the pore size of the PAN membranes was in the size range of 200-800 nm.
[0061] To investigate the potential of PAN membranes as wicking materials, the contact angle of water on PAN was measured in comparison to water on Nafion. Figure 4 shows photographs of water droplets on Fig. 4(a) PAN and Fig. 4(b) Nafion from which the contact angles were extracted. The contact angle of water on PAN was measured to be about 35°, which increased to about 70° on Nafion. The reduced contact angle of water on PAN indicates that PAN is a more hydrophilic surface than Nafion. This reduced contact angle on PAN is beneficial for the wicking (capillary action) effect, which is an excellent result in the first testing of this material.
[0062] X-ray photoelectron spectroscopy (XPS) was performed to probe the potential redistribution of Nafion throughout the PAN porous membrane after the addition of analytes. XPS spectra were collected by irradiating the samples with a non-monochromatic X-ray source (Omnivac) using Al Kα (1486.6 eV) radiation, and photoemission was collected by an SES2002 analyzer (Scienta). The F1s peak was utilized as a marker for Nafion, since Nafion contains fluorine atoms bonded to carbon atoms in the polymer backbone, whereas PAN contains only the elements carbon, nitrogen, and hydrogen. The structures of (a) PAN and (b) Nafion are shown below.
[0063] [ka]
[0064] An XPS survey scan of the pristine Nafion film (Figure 5(a)) identified an F1s peak at a binding energy of 691 eV. Next, XPS area scans of the pristine PAN film, the Nafion / PAN bilayer, and the Nafion / PAN bilayer after exposure to the analyte solution were performed. The pristine PAN film does not have an F1s peak (Figure 5(b)). The Nafion / PAN bilayer XPS spectrum contains an F1s peak, and the Nafion / PAN bilayer after exposure to the analyte solution also contains an F1s peak, and this peak is fairly unchanged compared to the Nafion / PAN bilayer, indicating that the analyte solution does not cause solvation and redistribution of the underlying Nafion film. This is a positive result for the biosensor and indicates that the Nafion film is very robust.
[0065] Glucose sensors were fabricated with the architecture shown in Figure 6. Sensors with and without PAN were fabricated and the GOX layer was inkjet printed with a Dimatix DMP2831 inkjet printer equipped with a 10 pL nozzle printhead (Figure 7).
[0066] The sensor was exposed to a glucose analyte solution and the difference in response of the sensor with and without the PAN porous membrane was analyzed. Figure 7(b) shows a representative plot of the sensor with and without PAN after exposure to a 10 mM glucose solution. Here, we observe an improvement in the drain current (ID) response time and maximum current when using the porous PAN membrane. The increase in ID changes from 0.04 μA / s without PAN to 0.93 μA / s with PAN, and a more than three-fold improvement in the total ID can be observed for the sensor with PAN. The better response time suggests that glucose is oxidized at a faster rate and / or hydrogen peroxide can migrate to the Nafion layer more quickly.
[0067] It will be understood that the invention disclosed and defined herein extends to all alternative combinations of two or more of the individual features mentioned or apparent from the text or drawings, all of these various combinations constituting various alternative aspects of the invention.
Claims
1. An organic thin film transistor-based sensor for detecting the presence of an analyte in an aqueous liquid sample, comprising: a porous wick layer having a first surface and a second surface, the first surface configured to receive an aqueous liquid sample; an enzyme disposed on or within the porous core layer for promoting generation of charge carriers from an analyte; a polymer gate layer in contact with the second surface of the porous core layer, the polymer gate layer being configured to be connected to an ohmic conductor for applying a gate voltage to the polymer gate layer, the polymer gate layer being conductive to charge carriers; an organic semiconductor layer connected to and between the source and drain electrodes; the porous wicking layer is a porous polymer wicking layer and is a different material than the polymer gate layer; The sensor wherein the contact angle of an aqueous liquid sample on the first surface of the porous core layer is 60° or less.
2. 10. The sensor of claim 1, wherein the porous core layer has a thickness of from 50 nm to 500 μm.
3. 3. The sensor according to claim 1, wherein the contact angle is 50[deg.] or less.
4. 3. The sensor according to claim 1, wherein the contact angle is 40 degrees or less.
5. The sensor of any one of claims 1 to 4, wherein the porous core layer has a pore size of from 50 nm to 2000 nm.
6. The sensor of claim 5, wherein the pore size is from 100 nm to 1000 nm.
7. The sensor according to any one of claims 1 to 6, wherein the porous core layer has a porosity of from 30% to 95%.
8. The sensor of any one of claims 1 to 7, wherein the porous core layer is formed from a polymer having a glass transition temperature of at least 80°C.
9. 9. The sensor of claim 8, wherein the glass transition temperature is at least 90°C.
10. The sensor according to any one of claims 1 to 9, wherein the porous core layer is formed from a polymer that is soluble in dimethylsulfoxide.
11. The sensor of any one of claims 1 to 10, wherein the porous core layer is formed from a polymer formed from one or more repeating monomer units, the one or more repeating monomer units being free of halide atoms.
12. The sensor of claim 11 , wherein the one or more repeating monomer units consist of C, N and H atoms.
13. The sensor according to any one of claims 1 to 12, wherein the porous core layer is a porous polyacrylonitrile (PAN) layer.
14. The sensor according to any one of claims 1 to 13, wherein the enzyme is present within the porous core layer.
15. 15. The sensor according to claim 1, wherein the analyte is glucose and the enzyme is glucose oxidase.
16. The sensor according to any one of claims 1 to 15, wherein the polymeric gate layer is a fluoropolymer-copolymer based on sulfonated tetrafluoroethylene.
17. 17. The sensor of claim 16, wherein the polymer gate layer comprises a copolymer of tetrafluoroethylene and perfluoro-3,6-dioxa-4-methyl-7-octene-sulfonic acid.
18. 18. The sensor of any one of claims 1 to 17, wherein the organic semiconductor layer comprises one or more organic polymers selected from the group consisting of polyacetylene, porphyrin, phthalocyanine, fullerene, polyparaphenylene, polyphenylenevinylene, polyfluorene, polythiophene, polypyrrole, polypyridine, polycarbazole, polypyridinevinylene, polyarylvinylene, and poly(p-phenylmethylvinylene).
19. The sensor of any one of claims 1 to 18, wherein the organic semiconductor layer comprises poly(3-hexylthiophene).
20. A method for producing an organic thin film transistor-based sensor according to any one of claims 1 to 19, comprising the steps of: A method comprising forming a porous core layer by a phase inversion process.
21. A method of forming an organic thin film transistor based sensor for detecting the presence of an analyte in an aqueous liquid sample, comprising: providing a layered structure including at least an organic semiconductor layer configured to be connected to a source electrode and a drain electrode, and a polymer gate layer; disposing a porous wicking layer on a surface of the polymeric gate layer, the porous wicking layer being a porous polymeric wicking layer and being of a different material than the polymeric gate layer; the porous core layer contains, or is treated to contain, an enzyme for promoting generation of charge carriers from the analyte; The method wherein the contact angle of an aqueous liquid sample on the first surface of the porous core layer is 60° or less.
22. 22. The method of claim 21, wherein the step of disposing the porous wicking layer on the surface of the polymeric gate layer comprises forming the porous wicking layer on the surface of the polymeric gate layer by a phase inversion process.
23. The phase inversion method is forming a wet film of a polymer solution on a surface of a substrate, the polymer solution including at least a polymer dissolved in a solvent; - applying a non-solvent to the wet film, the non-solvent being miscible with the solvent to form a porous polymer membrane and dissolving the solvent from the pores of the porous polymer membrane.
24. A method for detecting the concentration of glucose in an aqueous liquid sample using a sensor according to any one of claims 1 to 19.
Citation Information
Patent Citations
Novel immobilizing material combined with biologically active substance* its preparation* device comprising it* method* and preparation of support
JP1980048392A
Biological electrochemical sensor and manufacture thereof
JP1982127841A
Enzyme sensor
JP1986155850A
Immobilizing material for biological activator and assay method using the same
JP2004105065A
Ink for manufacturing semiconductor device, and method for manufacturing semiconductor device by using the ink
JP2005328030A