Piezoelectric film device

The piezoelectric film utilization device with a recessed peripheral edge upper electrode design addresses the challenge of maintaining electric field uniformity and increasing membrane displacement, enhancing the performance of inkjet print heads by reducing thickness-related issues.

JP7573519B2Active Publication Date: 2024-10-25ROHM CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2021515854
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-04-24
Filing Date
2020-03-05
Publication Date
2024-10-25
Estimated Expiration
2040-03-05

AI Technical Summary

Technical Problem

The existing inkjet print head designs face challenges in increasing the displacement of the movable membrane while maintaining a uniform electric field application, as reducing the thickness of the upper electrode leads to increased electrical resistance and potential voltage drop, causing fatigue and reduced response.

Method used

A piezoelectric film utilization device with a recessed peripheral edge upper electrode, featuring a thick central portion and a thin peripheral portion with a tapered design, allows for uniform electric field application and reduced average thickness, enhancing membrane displacement.

Benefits of technology

This configuration enables increased displacement of the movable membrane by maintaining a normal electric field distribution, even with a reduced average thickness, thus improving the performance of the inkjet print head.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007573519000001
    Figure 0007573519000001
  • Figure 0007573519000002
    Figure 0007573519000002
  • Figure 0007573519000003
    Figure 0007573519000003
Patent Text Reader

Abstract

In the present invention, an inkjet print head 1 includes: a pressure chamber 5; a movable film forming layer 10 containing a movable film 10A which defines the top surface section of the pressure chamber 5; and a piezoelectric element 6 that is formed so as to be in contact with the surface of the movable film 10A on the side thereof opposite the pressure chamber 5, and that has a peripheral edge that is recessed from the movable film 10A inward with respect to the pressure chamber 5, in plan view. The piezoelectric element 6 includes: a lower electrode 7 formed on the surface of the movable film forming layer 10 on the side thereof opposite the pressure chamber 5; an upper electrode 9 disposed on the lower electrode 7 on the side thereof opposite the movable film forming layer 10; and a piezoelectric film 8 provided between the upper electrode 9 and the lower electrode 7. The upper electrode 9 includes a thin section 92 at least at a portion of the peripheral edge part of the upper electrode.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a piezoelectric film-utilizing device such as an actuator or a sensor using a piezoelectric film. [Background technology]

[0002] Inkjet printheads are known as actuators using a piezoelectric film. One example of such an inkjet printhead is disclosed in Patent Document 1. The inkjet printhead disclosed in Patent Document 1 includes a nozzle substrate, a pressure chamber substrate, a movable membrane (vibration membrane), and a piezoelectric element bonded to the movable membrane. A pressure chamber into which ink is introduced is formed in the pressure chamber substrate, and the movable membrane faces this pressure chamber. The piezoelectric element is configured by laminating a lower electrode, a piezoelectric film, and an upper electrode from the movable membrane side. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2013-215930 A Summary of the Invention [Problem to be solved by the invention]

[0004] In the configuration described in Patent Document 1, the upper electrode is formed with a uniform thickness. To increase the amount of displacement of the movable film, it is preferable that the thickness of the upper electrode is thin. However, if the thickness of the upper electrode is made thin, the electrical resistance increases, and there is a risk that the electric field will not be applied uniformly to the piezoelectric film. Therefore, if the applied voltage is increased, the amount of displacement of the piezoelectric film may decrease and the response may become slow, which may cause the piezoelectric film to enter a so-called fatigue state.

[0005] An object of the present invention is to provide a piezoelectric film utilizing device capable of applying a normal electric field to a piezoelectric film and increasing the amount of displacement of a movable film. [Means for solving the problem]

[0006] The piezoelectric film utilization device of the present invention includes a cavity, a movable film forming layer including a movable film arranged on the cavity and defining the top surface of the cavity, and a piezoelectric element formed in contact with the surface of the movable film opposite the cavity and having a periphery that is recessed further inward into the cavity than the movable film in a planar view, wherein the piezoelectric element includes a lower electrode formed on the surface of the movable film forming layer opposite the cavity, an upper electrode arranged on the opposite side of the movable film forming layer from the lower electrode, and a piezoelectric film provided between the upper electrode and the lower electrode, and the upper electrode has a thin-walled portion in at least a part of its periphery.

[0007] In this configuration, the central portion of the upper electrode other than the peripheral portion and the portion of the peripheral portion other than the thin portion are the thick portion. The thick portion has a smaller electrical resistance than the thin portion, so that electric charges can be injected into the piezoelectric film without causing a large voltage drop. On the other hand, the thin portion has a larger electrical resistance than the thick portion, but the distance to the peripheral portion of the upper electrode is short, and the distance that the electric charges travel is short, so the amount of current flowing to the peripheral portion is small. Therefore, a large voltage drop does not occur even in the thin portion.

[0008] As a result, it is possible to apply a normal electric field to the piezoelectric film even if the average thickness is reduced, compared to when the entire upper electrode has the same thickness as the thick portion. Since the average thickness can be reduced compared to when the entire upper electrode has the same thickness as the thick portion, the amount of displacement of the movable film can be increased.

[0009] In one embodiment of the present invention, the upper electrode has a thin portion over the entire periphery.

[0010] In one embodiment of the present invention, the upper electrode has a rectangular shape that is long in one direction in a plan view, and the upper electrode has thin portions on both sides.

[0011] In one embodiment of the present invention, the upper electrode also has thin portions at both ends.

[0012] In one embodiment of the present invention, the thin portion has a tapered upper surface whose distance from the upper surface of the piezoelectric film gradually decreases outward.

[0013] In one embodiment of the present invention, the thin portion has a length in an inner / outer direction of 0.5 μm or more in a plan view.

[0014] In one embodiment of the present invention, the inclination angle of the tapered upper surface with respect to the upper surface of the piezoelectric film is equal to or greater than 1 degree and equal to or less than 8 degrees.

[0015] In one embodiment of the present invention, the outer edge of the tapered upper surface is formed into an outwardly convex curved surface.

[0016] In one embodiment of the present invention, the upper electrode is composed of a laminated film of an IrO2 film formed on the upper surface of the piezoelectric film and an Ir film laminated on the IrO2 film, and the Ir film is present on the IrO2 film at the outer edge of the thin portion.

[0017] In one embodiment of the present invention, the upper electrode is composed of a laminated film of an IrO2 film formed on the upper surface of the piezoelectric film and an Ir film laminated on the IrO2 film, and at the outer edge of the thin portion, the Ir film is not present on the IrO2 film.

[0018] In one embodiment of the present invention, the upper electrode is made of a laminated film of an IrO2 film formed on the upper surface of the piezoelectric film, and an Ir film laminated on the IrO2 film.

[0019] In one embodiment of the present invention, the piezoelectric film is made of a material containing PZT as a main component.

[0020] In one embodiment of the present invention, the lower electrode is made of a material containing Pt as a main component.

[0021] In one embodiment of the present invention, the thin portion has a constant thickness and has an upper surface parallel to an upper surface of the piezoelectric film.

[0022] In one embodiment of the present invention, the thin portion has a length in an inner / outer direction of 0.5 μm or more in a plan view.

[0023] The above and other objects, features and advantages of the present invention will become apparent from the following detailed description of the embodiments with reference to the accompanying drawings. [Brief description of the drawings]

[0024] [Figure 1] FIG. 1 is a schematic plan view of an inkjet print head to which a piezoelectric film utilization device according to an embodiment of the present invention is applied. [Diagram 2] FIG. 2 is a schematic enlarged cross-sectional view taken along line II-II in FIG. [Diagram 3] FIG. 3 is a schematic enlarged cross-sectional view taken along line III-III in FIG. [Figure 4A] FIG. 4A is a partially enlarged view mainly showing the actual shape of the peripheral portion of the upper electrode in FIG. [Figure 4B] FIG. 4B is a partial enlarged view showing a modified example of the shape of the peripheral edge of the upper electrode. [Figure 5A] FIG. 5A is a cross-sectional view showing an example of a manufacturing process of the inkjet printhead. [Figure 5B] FIG. 5B is a cross-sectional view showing a step subsequent to that of FIG. 5A. [Figure 5C] FIG. 5C is a cross-sectional view showing a step subsequent to that of FIG. 5B. [Figure 5D] FIG. 5D is a cross-sectional view showing the next step after FIG. 5C. [Figure 5E] FIG. 5E is a cross-sectional view showing the next step of FIG. 5D. [Figure 5F] FIG. 5F is a cross-sectional view showing the step following FIG. 5E. [Figure 5G] FIG. 5G is a cross-sectional view showing the step following FIG. 5F. [Figure 5H] FIG. 5H is a cross-sectional view showing the step following FIG. 5G. [Figure 5I] FIG. 5I is a cross-sectional view showing the step following FIG. 5H. [Figure 5J] FIG. 5J is a cross-sectional view showing a step subsequent to that of FIG. 5I. [Figure 5K] FIG. 5K is a cross-sectional view showing the step following that of FIG. 5J. [Figure 5L] FIG. 5L is a cross-sectional view showing the step following FIG. 5K. [Figure 5M] FIG. 5M is a cross-sectional view showing the next step of FIG. 5K. [Figure 6] FIG. 6 is a cross-sectional view illustrating the configuration of an ink-jet printhead according to another embodiment of the present invention, and corresponds to FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0025] Fig. 1 is a schematic plan view of an inkjet print head to which a piezoelectric film utilization device according to an embodiment of the present invention is applied. Fig. 2 is a schematic enlarged cross-sectional view taken along line II-II in Fig. 1. Fig. 3 is a schematic enlarged cross-sectional view taken along line III-III in Fig. 1. Fig. 4A is a partial enlarged view mainly showing the actual shape of the periphery of the upper electrode in Fig. 2. However, in Figs. 1 and 4A, the hydrogen barrier film and insulating film indicated by reference numerals 11 and 12 in Figs. 2 and 3 are omitted.

[0026] 2 and 3, the inkjet print head 1 includes a silicon substrate 2 and a nozzle substrate 3 having an ejection port 31a for ejecting ink. A movable film formation layer 10 is laminated on the silicon substrate 2. A pressure chamber (cavity) 5 serving as an ink flow path (ink reservoir) is formed in the laminate of the silicon substrate 2 and the movable film formation layer 10.

[0027] The nozzle substrate 3 is made of, for example, a silicon plate, and is bonded to the rear surface of the silicon substrate 2. Together with the silicon substrate 2 and the movable film formation layer 10, the nozzle substrate 3 defines the pressure chamber 5. An ink ejection passage 31 is formed in the nozzle substrate 3. The ink ejection passage 31 penetrates the nozzle substrate 3, and has an ejection port 31a on the opposite side to the pressure chamber 5. Therefore, when a change in the volume of the pressure chamber 5 occurs, the ink stored in the pressure chamber 5 passes through the ink ejection passage 31 and is ejected from the ejection port 31a.

[0028] The pressure chambers 5 are formed by digging into the silicon substrate 2 (or the silicon substrate 2 and the movable film formation layer 10) from the back side of the silicon substrate 2. The silicon substrate 2 (or the silicon substrate 2 and the movable film formation layer 10) is further formed with ink supply paths 4 (see also Figures 1 and 3) that communicate with the pressure chambers 5. The ink supply paths 4 communicate with the pressure chambers 5, and are formed so as to guide ink from an ink tank (e.g., an ink cartridge), which is an ink supply source, to the pressure chambers 5.

[0029] The pressure chamber 5 is formed to extend long along the ink flow direction 21, which is the left-right direction in FIG. 3. The ceiling wall portion of the pressure chamber 5 in the movable film formation layer 10 constitutes the movable film 10A. The movable film 10A (movable film formation layer 10) is made of, for example, a silicon oxide (SiO2) film formed on a silicon substrate 2. The movable film 10A (movable film formation layer 10) may be made of, for example, a laminate of a silicon (Si) layer formed on the silicon substrate 2, a silicon oxide (SiO2) layer formed on the silicon layer, and a silicon nitride (SiN) layer formed on the silicon oxide layer. In this specification, the movable film 10A means the ceiling wall portion of the movable film formation layer 10 that defines the pressure chamber 5. Therefore, the portion of the movable film formation layer 10 other than the ceiling wall portion of the pressure chamber 5 does not constitute the movable film 10A.

[0030] The thickness of the movable film 10A is, for example, about 0.4 μm to 3 μm In this embodiment, the thickness of the movable film 10A is about 2 μm.

[0031] The pressure chamber 5 is defined by the movable film 10A, the silicon substrate 2, and the nozzle substrate 3, and in this embodiment, is formed in a substantially rectangular parallelepiped shape. The pressure chamber 5 has a length of, for example, about 600 μm, a width of, for example, about 100 μm, and a depth of, for example, about 100 μm. The ink supply path 4 is formed so as to communicate with one end of the pressure chamber 5 in the longitudinal direction (the end located opposite the ejection port 31a in this embodiment). In this embodiment, the ejection port 31a of the nozzle substrate 3 is disposed near the other end of the pressure chamber 5 in the longitudinal direction.

[0032] Since the pressure chamber 5 is rectangular, the movable film 10A is, in a plan view, rectangular in shape that is long in the ink flow direction 21. The length of the movable film 10A in the longitudinal direction is about 600 μm, and the length of the movable film 10A in the lateral direction is about 100 μm.

[0033] A piezoelectric element 6 is disposed on the surface of the movable film 10A. The piezoelectric element 6 includes a lower electrode 7 formed on the movable film formation layer 10, a piezoelectric film 8 formed on the lower electrode 7, and an upper electrode 9 formed on the piezoelectric film 8. In other words, the piezoelectric element 6 is configured by sandwiching the piezoelectric film 8 between the upper electrode 9 and the lower electrode 7 from above and below.

[0034] The lower electrode 7 is composed of a single film of, for example, a Pt (platinum) layer. Alternatively, the lower electrode 7 may be formed of a single film of, for example, an Au (gold) film, a Cr (chromium) layer, or a Ni (nickel) layer. The lower electrode 7 may also be formed of a laminated film in which a Ti (titanium) layer and a Pt (platinum) layer are laminated in this order from the movable film 10A side. The film thickness of the lower electrode 7 is, for example, about 200 nm.

[0035] The lower electrode 7 is disposed on the movable film 10A and has a rectangular portion 71 having approximately the same shape and size as the movable film 10A, an extraction electrode portion 72 drawn out from one end side of the rectangular portion 71, and a common connection portion 73 that commonly connects the lower electrodes 7 of the multiple piezoelectric elements 6. Of the rectangular portion 71, the portion in contact with the lower surface of the piezoelectric film 8 is a main electrode portion 71A that constitutes the piezoelectric element 6.

[0036] 3 and 1, the extracted electrode portion 7B is extracted downstream from the width center portion of the downstream end of the rectangular portion 71 in the ink flow direction 21. The common connection portion 73 extends in a direction perpendicular to the ink flow direction 21, downstream of the rectangular portion 71. The downstream ends of the multiple extracted electrode portions 72 are connected to the common connection portion 73.

[0037] 2 and 3, the piezoelectric film 8 is, for example, a PZT (PbZr x Ti 1-x O3: lead zirconate titanate film can be applied. Such a piezoelectric film 8 is made of a sintered body of metal oxide crystal. The thickness of the piezoelectric film 8 is preferably about 1 μm to 5 μm. In this embodiment, the thickness of the piezoelectric film 8 is about 2 μm. The overall thickness of the movable film 10A is preferably about the same as the thickness of the piezoelectric film 8 or about 2 / 3 of the thickness of the piezoelectric film.

[0038] The piezoelectric film 8 has a rectangular shape that is long in the ink flow direction 21 in a plan view. The side surface of the piezoelectric film 8 is formed into an inclined surface that widens outward as it goes downward. The longitudinal length of the piezoelectric film 8 is formed to be shorter than the longitudinal length of the movable film 10A (pressure chamber 5), and both end edges are disposed inward with a predetermined first interval from the corresponding end edges of the movable film 10A. The longitudinal length of the upper surface of the piezoelectric film 8 is approximately 500 μm.

[0039] The length of the piezoelectric film 8 in the short side direction is shorter than the length of the movable film 10A (pressure chamber 5) in the short side direction, and both side edges thereof are disposed inside the corresponding both side edges of the movable film 10A with a predetermined second gap therebetween. The length of the short side direction of the upper surface of the piezoelectric film 8 is about 33 μm.

[0040] The upper electrode 9 is formed in a pattern substantially similar to that of the upper surface of the piezoelectric film 8. That is, the upper electrode 9 is a rectangle that is long in the ink flow direction 21. As shown in Fig. 4A, the upper electrode 9 has a two-layer structure in which, for example, an IrO2 (iridium oxide) film 9A and an Ir (iridium) film 9B are laminated in this order from the piezoelectric film 8 side.

[0041] The upper electrode 9, in a plan view, is composed of a thick central portion 91 and a thin peripheral portion 92 outside the central portion 91. In a plan view, the central portion 91 has a rectangular shape that is long in the ink flow direction 21. The film thickness of the central portion 91 is constant, and the upper surface of the central portion 91 is formed into a flat surface that is approximately parallel to the upper surface of the piezoelectric film 8.

[0042] The peripheral portion 92 has a rectangular ring shape in a plan view. In this embodiment, the peripheral portion 92 is formed as a tapered thin portion whose film thickness gradually decreases toward the outside (outer periphery). In other words, the peripheral portion 92 has a tapered upper surface 92a whose distance from the upper surface of the piezoelectric film 8 gradually decreases toward the outside.

[0043] In this embodiment, the length of the central portion 91 in the longitudinal direction is about 497 μm, and the length of the central portion 91 in the lateral direction is about 30 μm. In addition, in a plan view, the length of the peripheral portion 92 in the inner and outer directions (the width of the peripheral portion) is about 1.5 μm. The length of the peripheral portion 92 in the inner and outer directions is preferably 0.5 μm or more. In this embodiment, the inclination angle of the tapered upper surface 92a with respect to the upper surface of the piezoelectric film 8 is about 4 degrees. The inclination angle of the tapered upper surface 92a with respect to the upper surface of the piezoelectric film 8 is preferably 1 degree or more and 8 degrees or less.

[0044] As shown in Fig. 4A, an outer edge 92b of a tapered upper surface 92a of the peripheral portion 92 is formed into an outwardly convex curved surface. In Fig. 4A, an Ir film 9B is present on an IrO2 film 9A at the outer edge 92b of the peripheral portion 92. However, as shown in Fig. 4B, an Ir film 9B does not have to be present on an IrO2 film 9A at the outer edge 92b of the peripheral portion 92.

[0045] The surface of the movable film formation layer 10, the surface of the piezoelectric element 6, and the surface of the lower electrode 7 other than the main electrode portion 71A are covered with a hydrogen barrier film 11. The hydrogen barrier film 11 is made of, for example, Al2O3 (alumina). This makes it possible to prevent the characteristics of the piezoelectric film 8 from deteriorating due to hydrogen reduction. The thickness of the hydrogen barrier film 11 is about 100 nm.

[0046] An insulating film 12 is laminated on the hydrogen barrier film 11. The insulating film 12 is made of, for example, SiO2. A wiring 13 is formed on the insulating film 12. The wiring 13 is made of a metal material containing Al (aluminum).

[0047] One end of the wiring 13 is disposed above one end of the upper electrode 9. A through hole 14 is formed between the wiring 13 and the upper electrode 9, continuously penetrating the hydrogen barrier film 11 and the insulating film 12. One end of the wiring 13 enters the through hole 14 and is connected to the upper electrode 9 within the through hole 14. The hydrogen barrier film 11 and the insulating film 12 have a cutout portion 15 at a position corresponding to a region surrounded by the periphery of the central portion 91 on the surface of the upper electrode 9. The cutout portion 15 is a portion where the hydrogen barrier film 11 and the insulating film 12 are cut out.

[0048] Although not shown, an opening that penetrates continuously through the hydrogen barrier film 11 and the insulating film 12 is formed at a position corresponding to a predetermined region on the common connection portion 73 of the lower electrode 7, and the surface of the common connection portion 73 is exposed through the opening. This exposed portion constitutes a pad portion for connecting the lower electrode 7 to the outside.

[0049] The piezoelectric element 6 is formed at a position facing the pressure chamber 5 across the movable film 10A. That is, the piezoelectric element 6 is formed so as to contact the surface of the movable film 10A opposite to the pressure chamber 5. The pressure chamber 5 is filled with ink supplied from an ink tank (not shown) through an ink supply path 4. The movable film 10A defines the top surface of the pressure chamber 5 and faces the pressure chamber 5. The movable film 10A is supported by the surrounding portion of the pressure chamber 5 in the laminate of the movable film formation layer 10 and the silicon substrate 2, and has flexibility that allows it to deform in the direction facing the pressure chamber 5 (in other words, the thickness direction of the movable film 10A).

[0050] The common connection portion 73 of the wiring 13 and the lower electrode 7 is connected to a drive circuit 20. The drive circuit 20 may be formed in a region of the silicon substrate 2 separate from the pressure chamber 5, or may be formed outside the silicon substrate 2. When a drive voltage is applied from the drive circuit 20 to the piezoelectric element 6, the piezoelectric film 8 is deformed by the inverse piezoelectric effect. This causes the piezoelectric element 6 and the movable film 10A to deform, which changes the volume of the pressure chamber 5 and pressurizes the ink in the pressure chamber 5. The pressurized ink passes through the ink ejection passage 31 and is ejected as minute droplets from the ejection port 31a.

[0051] 1 to 3, a plurality of pressure chambers 5 are formed in a stripe pattern extending parallel to each other in a silicon substrate 2 (or a laminate of the silicon substrate 2 and the movable film formation layer 10). The pressure chambers 5 are formed at equal intervals in their width direction with small intervals (for example, about 30 μm to 350 μm) between them.

[0052] In a plan view, each pressure chamber 5 has an elongated rectangular shape that extends along the ink flow direction 21 from the ink supply path 4 toward the ejection path 33. That is, the top surface of the pressure chamber 5 has two side edges 5c, 5d that extend along the ink flow direction 21 and two end edges 5a, 5b that extend along a direction perpendicular to the ink flow direction 21.

[0053] The ink supply path 4 is formed at one end of the pressure chamber 5 by dividing it into two paths, which communicate with a common ink path 22. The common ink path 22 communicates with the ink supply paths 4 corresponding to the multiple pressure chambers 5, and is formed so as to supply ink from an ink tank to those ink supply paths 4.

[0054] The wiring 13 is composed of a lead-out portion 13A, one end of which is connected to one end of the upper electrode 9 on the upstream side in the ink flow direction 21 and extends in the opposite direction to the ink flow direction 21, and a pad portion 13B, which is integrated with the lead-out portion 13A and has a rectangular shape in a plan view and is connected to the tip of the lead-out portion 13A. The lead-out portion 13A is formed on the surface of the insulating film 12 that covers one end of the upper surface of the piezoelectric element 6, the end face of the piezoelectric element 6 connected to it, and the surface of the movable film formation layer 10, except for the portion connected to the upper electrode 9. The pad portion 13B is formed on the insulating film 12 that covers the surface of the movable film formation layer 10.

[0055] The annular region of the movable film 10A between the periphery of the movable film 10A and the periphery of the piezoelectric element 6 (in this embodiment, a rectangular annular region long in the ink flow direction 21) is an area that is not constrained by the piezoelectric element 6 or the surrounding wall of the pressure chamber 5, and is an area where large deformation occurs. In other words, the peripheral portion of the movable film 10A is an area where large deformation occurs. For this reason, when the piezoelectric element 6 is driven, the peripheral portion of the movable film 10A bends so that the inner edge side of the peripheral portion of the movable film 10A is displaced in the thickness direction of the pressure chamber 5 (downward in this embodiment), and as a result, the entire central portion surrounded by the peripheral portion of the movable film 10A is displaced in the thickness direction of the pressure chamber 5 (downward in this embodiment).

[0056] A method for manufacturing the inkjet printhead 1 will now be described in detail.

[0057] 5A to 5M are cross-sectional views showing the manufacturing process of the inkjet printhead 1, and correspond to the cross section of FIG.

[0058] First, a silicon substrate 2 is prepared as shown in Fig. 5A. However, the silicon substrate 2 to be used has a thickness greater than the final thickness of the silicon substrate 2.

[0059] 5B, a movable film formation layer 10 is formed on the surface of the silicon substrate 2. Specifically, a silicon oxide film (e.g., 2 μm thick) is formed on the surface of the silicon substrate 2. When the movable film formation layer 10 is composed of a laminated film of a silicon film, a silicon oxide film, and a silicon nitride film, a silicon film (e.g., 0.6 μm thick) is formed on the surface of the silicon substrate 2, a silicon oxide film (e.g., 0.6 μm thick) is formed on the silicon film, and a silicon nitride film (e.g., 0.6 μm thick) is formed on the silicon oxide film.

[0060] 5C, a lower electrode film 107, which is a material layer of the lower electrode 7, is formed on the movable film formation layer 10. The lower electrode film 107 is made of, for example, a Pt film (for example, 200 nm thick). Such a lower electrode film 107 is formed, for example, by a sputtering method.

[0061] 5D, a piezoelectric material film 108, which is the material of the piezoelectric film 8, is formed on the entire surface of the lower electrode film 107. Specifically, the piezoelectric material film 108 is formed to a thickness of, for example, 2 μm by a sol-gel method. Such a piezoelectric material film 108 is made of a sintered body of metal oxide crystal grains.

[0062] Next, as shown in Fig. 5E, an upper electrode film 109, which is the material of the upper electrode 9, is formed on the entire surface of the piezoelectric material film 108. The upper electrode film 109 is made of, for example, an IrO2 / Ir laminated film having an IrO2 film (e.g., 50 nm thick) as a lower layer and an Ir film (e.g., 50 nm thick) as an upper layer. Such an upper electrode film 109 is formed by, for example, a sputtering method.

[0063] 5F, a resist mask 111 having a pattern for the upper electrode 9 is formed by photolithography. Each side surface 111a of the resist mask 111 is formed into an inclined surface that widens outward as it goes downward.

[0064] Next, as shown in FIG. 5G and FIG. 5H, the upper electrode film 109 is etched using the resist mask 111 as a mask, thereby forming the upper electrode 9 in a predetermined pattern. In this etching process, as shown in FIG. 5H, the surface and the inclined side surface 111a of the resist mask 111 are gradually etched, so that the amount of etching increases toward the outside in the peripheral portion of the upper surface of the upper electrode 9. As a result, the upper electrode 9 is obtained, which is composed of a central portion (thick portion) 91 having a constant film thickness and a peripheral portion (thin portion) 92 having a film thickness that gradually decreases toward the outside. The peripheral portion 92 has a tapered upper surface 92a in which the distance from the upper surface of the piezoelectric film 8 gradually decreases toward the outside. The outer edge portion 92b of the peripheral portion 92 is formed in an outwardly convex curved shape.

[0065] 5I, the piezoelectric material film 108 is etched to form a predetermined pattern of the piezoelectric film 8. Thereafter, the resist mask 111 is peeled off.

[0066] Next, as shown in FIG. 5J, a resist mask 112 having a pattern of the lower electrode 7 is formed by photolithography.

[0067] 5K, the lower electrode film 107 is etched using the resist mask 112 as a mask to form the lower electrode 7 including the rectangular portion 71 including the main electrode portion 71A, the extraction electrode portion 72, and the common connection portion 73. Thereafter, the resist mask 112 is peeled off.

[0068] Next, a hydrogen barrier film 11 is formed to cover the entire surface. After that, an insulating film 12 is formed on the entire surface of the hydrogen barrier film 11. Next, the insulating film 12 and the hydrogen barrier film 11 are continuously etched to form a through hole 14. A wiring film constituting the wiring 13 is formed by a sputtering method on the insulating film 12 including the inside of the through hole 14. After that, the wiring film is patterned by photolithography and etching to form the wiring 13. After that, as shown in FIG. 5L, the insulating film 12 and the hydrogen barrier film 11 are continuously etched to form a cutout portion 15.

[0069] Next, as shown in Fig. 5M, back grinding is performed to thin the silicon substrate 2. The silicon substrate 2 is thinned by polishing the back surface. For example, the silicon substrate 2, which is about 670 µm thick in the initial state, is thinned to about 100 µm thick. Thereafter, the common ink passage 22, the ink supply passage 4, and the pressure chamber 5 are formed in the silicon substrate 2 by photolithography and etching.

[0070] Finally, the nozzle substrate 3 is attached to the rear surface of the silicon substrate 2, thereby obtaining the inkjet printhead 1 as shown in FIGS. 1 to 4A.

[0071] In the above embodiment, the upper electrode 9 is composed of a thick central portion 91 and a thin peripheral portion 92 outside the central portion 91. The thickness of the central portion 91 is constant. The peripheral portion 92 is formed as a tapered thin portion whose thickness gradually decreases outward. In other words, the peripheral portion 92 has a tapered upper surface 92a whose distance from the upper surface of the piezoelectric film 8 gradually decreases outward.

[0072] The central portion (thick portion) 91 has a smaller electrical resistance than the peripheral portion (thin portion) 92, so that electric charges can be injected into the piezoelectric film 8 without causing a large voltage drop. On the other hand, the peripheral portion 92 has a larger electrical resistance than the central portion 91, but the distance to the peripheral portion of the upper electrode 9 is short, and therefore the distance that the electric charges travel is short, so that the amount of current flowing through the peripheral portion 92 is small. Therefore, no large voltage drop occurs in the peripheral portion 92 either.

[0073] As a result, even if the average thickness is reduced, a normal electric field can be applied to the piezoelectric film 8, compared to when the entire upper electrode 9 has the same thickness as the central portion 91. Since the average thickness can be reduced, compared to when the entire upper electrode 9 has the same thickness as the central portion 91, the amount of displacement of the movable film 10A can be increased.

[0074] In the above embodiment, the entire periphery of the upper electrode 9 is formed into a tapered thin portion, but only a part of the periphery of the upper electrode 9 may be formed into a tapered thin portion. For example, of both side portions and both end portions of the upper electrode 9, only both side portions may be formed into a tapered thin portion.

[0075] Furthermore, in the above embodiment, the upper electrode 9 has a rectangular shape in a plan view, but the planar shape of the upper electrode 9 may be any shape, such as a circle or an ellipse.

[0076] In the above embodiment, the peripheral portion 92 of the upper electrode 9 is formed as a tapered thin portion, but as in the inkjet printhead 1A shown in FIG. 6, the peripheral portion 92 of the upper electrode 9 may be formed as a thin portion that is thinner than the central portion 91 and has a constant thickness. FIG. 6 is a cross-sectional view corresponding to FIG. 2. Even in this case, the length of the peripheral portion 92 in the inner and outer directions is preferably 0.5 μm or more in plan view. In the example of FIG. 6, the length of the peripheral portion 92 in the inner and outer directions is about 1.5 μm.

[0077] In the above embodiment, the insulating film 12 is formed on the hydrogen barrier film 11, but the insulating film 12 does not necessarily have to be formed on the hydrogen barrier film 11.

[0078] In the above embodiment, the present invention is described as being applied to an inkjet printhead, but the present invention can also be applied to microphones, pressure sensors, acceleration sensors, angular velocity sensors, ultrasonic sensors, speakers, IR sensors (thermal sensors), etc. that use piezoelectric films.

[0079] Although the embodiments of the present invention have been described in detail, these are merely examples used to clarify the technical contents of the present invention, and the present invention should not be interpreted as being limited to these examples, and the scope of the present invention is limited only by the appended claims.

[0080] This application corresponds to Patent Application No. 2019-083070 filed with the Japan Patent Office on April 24, 2019, the entire disclosure of which is incorporated herein by reference. [Explanation of symbols]

[0081] 1,1A Inkjet Printhead 2. Silicon substrate 3 Nozzle Board 31 Ink ejection passage 31a Discharge port 4 Ink supply path 5 Pressure chamber (cavity) 6 Piezoelectric element 7 Lower electrode 71 Rectangular part 71A Main electrode section 72 Extraction electrode part 73 Common Connection 8 Piezoelectric film 9 Upper electrode 9A IrO2 membrane 9B Ir film 91 Central part 92 Periphery 92a Tapered top surface 92b Outer edge 10 Movable membrane forming layer 10A movable membrane 11 Hydrogen barrier film 12 Insulating film 13 Wiring 13A Pull-out section 13B Pad section 14 Through hole 15 Excision 20 Drive circuit 21 Ink flow direction 22 Common ink passage 107 Lower electrode film 108 Piezoelectric material film 109 Upper electrode film 111,112 Resist mask

Claims

1. Cavity and a movable film forming layer including a movable film disposed on the cavity and defining a top surface of the cavity; a piezoelectric element formed in contact with a surface of the movable film opposite to the cavity and having a periphery recessed inwardly of the cavity relative to the movable film in a plan view; The piezoelectric element includes a lower electrode formed on a surface of the movable film formation layer opposite to the cavity, and an upper electrode disposed on the opposite side of the movable film formation layer with respect to the lower electrode. a piezoelectric film provided between the upper electrode and the lower electrode, the upper electrode has a thin portion at least in a part of a peripheral edge thereof, the upper electrode includes a lower layer formed on the upper surface of the piezoelectric element, and an upper layer formed on the upper surface of the lower layer and made of a material different from that of the lower layer; the upper layer has an upper layer thin portion at least in a part of the entire peripheral portion, the thin-walled portion is formed by forming the upper-layer thin-walled portion on the upper layer, the upper thin portion has a tapered upper surface whose distance from the upper surface of the piezoelectric film gradually decreases outward; At an outer edge of the thin portion, the lower layer has a flat upper surface parallel to an upper surface of the piezoelectric film and a side surface perpendicular to the flat upper surface, A piezoelectric film utilization device, wherein there is an area on the flat upper surface where the upper layer is not present.

2. 2. The device utilizing a piezoelectric film according to claim 1, wherein said upper layer has said upper layer thin portion over its entire peripheral portion.

3. The upper layer has a rectangular shape that is long in one direction in a plan view, 2. The device utilizing a piezoelectric film according to claim 1, wherein said upper layer has said upper layer thin portions on both sides along each of two long sides of said upper layer.

4. 4. The device utilizing a piezoelectric film according to claim 3, wherein said upper layer also has said upper layer thin portions at both ends along each of the two short sides of said upper layer.

5. 5. The piezoelectric film utilization device according to claim 1, wherein an inclination angle of the tapered upper surface with respect to the upper surface of the piezoelectric film is 1 degree or more and 8 degrees or less.

6. The lower layer is IrO 2 6. The piezoelectric film utilization device according to claim 1, wherein the upper layer is an Ir film.

7. 7. The piezoelectric film utilization device according to claim 1, wherein the piezoelectric film is made of a material containing PZT as a main component.

8. The piezoelectric film utilization device according to any one of claims 1 to 7, wherein the lower electrode is made of a material containing Pt as a main component.

Citation Information

Patent Citations

  • Laminated piezoelectric element and method of manufacturing the same

    JP2004111939A

  • Piezoelectric thin film resonator with mass loading in perimeter

    JP2006109472A

  • Bulk acoustic wave resonator

    JP2007184816A

  • Ferroelectric element, ink jet recording head, and ink jet image forming apparatus

    JP2013016738A

  • Inkjet print head and fabrication method thereof

    JP2013215930A