Airtight Terminal
The airtight terminal design addresses cracking issues by using a metal-insulating ring configuration with matching thermal expansion coefficients and brazing, ensuring reliable airtightness under thermal stress.
Patent Information
- Application Number
- JP2021010641
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-01-26
- Publication Date
- 2024-11-14
- Estimated Expiration
- 2041-01-26
AI Technical Summary
Ceramic rings used in airtight terminals for high vacuum systems are prone to cracking when bonded to conductors due to stress, especially when the conductor is heavy, leading to reliability issues.
The airtight terminal design includes a columnar conductor with a metal ring, insulating ring, and fixing members made of specific metals with similar thermal expansion coefficients, separated by a distance, and bonded using brazing materials to reduce stress and prevent cracking.
The design minimizes stress on the insulating ring, reducing the likelihood of cracks and enhancing the airtightness and reliability of the terminal even under thermal cycling.
Smart Images

Figure 0007583625000001 
Figure 0007583625000002 
Figure 0007583625000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a hermetic terminal. [Background technology]
[0002] Conventionally, airtight terminals using ceramic rings that can be electrically insulated from power supply systems have been used in some high vacuum pumping systems used in particle accelerators, nuclear fusion devices, etc. For example, Patent Document 1 discloses such a ceramic ring. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Japanese Utility Model Application Publication No. 59-47916 Summary of the Invention [Problem to be solved by the invention]
[0004] When the ceramic ring is fixed to the conductor via a sleeve with a Kovar ring abutting on one side of the ceramic ring, if the ceramic ring and the sleeve are connected to the conductor and the sleeve using brazing material, cracks may occur in the ceramic ring or the sleeve after joining. The occurrence of cracks is particularly noticeable when the conductor is heavy. [Means for solving the problem]
[0005] The hermetic terminal according to the present disclosure includes a columnar conductor, a metal ring coaxially disposed with the conductor, an insulating ring coaxially disposed with the conductor, a flange disposed on the insulating ring and dividing the columnar conductor into two regions, a first fixing member for fixing the insulating ring to the conductor, and a second fixing member for fixing the insulating ring to the flange. The metal ring, the first fixing member, and the second fixing member are formed of carbon steel, low alloy steel, tool steel, stainless steel, iron, copper, copper alloy, titanium or titanium alloy, molybdenum or molybdenum alloy. The metal ring and the first fixing member are connected, and the insulating ring is fixed to the conductor at a distance from the metal ring. Effect of the Invention
[0006] In the hermetic terminal according to the present disclosure, even if the first fixing member and the second fixing member are respectively joined to the insulating ring with brazing material, the stress remaining in the surface layer of the insulating ring on the second fixing member side is reduced, and as a result, cracks are less likely to occur in the insulating ring, the first fixing member, and the second fixing member. [Brief description of the drawings]
[0007] [Figure 1] FIG. 1 is a perspective view showing a hermetic terminal according to an embodiment of the present disclosure. [Diagram 2] 2 is an explanatory diagram showing a cross section taken along line XX shown in FIG. 1. [Diagram 3] 11 shows a modified example of a second fixing member included in the hermetic terminal according to the embodiment of the present disclosure. [Figure 4] 1 is an explanatory diagram showing a metal ring included in an airtight terminal according to an embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] A hermetic terminal according to one embodiment of the present disclosure will be described with reference to Figures 1 and 2. The hermetic terminal 1 according to one embodiment shown in Figure 1 includes a conductor 11, a metal ring 12, an insulating ring 13, a flange 14, a first fixing member 15, a second fixing member 16, and a spacer 17.
[0009] The conductor 11 included in the airtight terminal 1 according to an embodiment has a columnar shape, and the size and shape are not limited as long as the conductor 11 is columnar. As shown in FIG. 1, the conductor 11 may have a shape in which a cylindrical portion and a rectangular columnar (plate-shaped) portion are present. The size of the conductor 11 may be appropriately set according to the device including the airtight terminal 1. When the conductor 11 has a shape in which the cylindrical portion and the rectangular columnar (plate-shaped) portion are connected in the axial direction, the length (total length) is, for example, about 200 mm to 300 mm, the outer diameter of the cylindrical portion is about 90 mm to 110 mm, and the width of the rectangular columnar (plate-shaped) portion is about 80 mm to 88 mm. The conductor 11 is formed of, for example, copper or a copper alloy such as oxygen-free copper, tough pitch copper, or phosphorus deoxidized copper.
[0010] The metal ring 12 included in the airtight terminal 1 according to one embodiment is provided so as to be positioned coaxially with the conductor 11. The metal ring 12 is formed of carbon steel, low alloy steel, tool steel, stainless steel, iron, copper, copper alloy, titanium, titanium alloy, molybdenum, or molybdenum alloy. These metals forming the metal ring 12 have an average linear expansion coefficient at 30°C to 400°C that is equivalent to or lower than the average linear expansion coefficient of copper, copper alloy, etc., which constitute the conductor 11. Therefore, when the metal ring 12 is thermally joined to the conductor 11 by a brazing material described later, a gap is not generated between the metal ring 12 and the conductor 11, and the reliability of airtightness can be improved.
[0011] Carbon steel is an alloy of Fe and 0.02 to 2.14 mass% C, and contains Si, Mn, P, and S in addition to C. Examples of such carbon steel include S10C, S12C, S15C, S17C, S20C, S22C, S25C, S28C, S30C, S33C, S35C, S38C, S40C, S43C, S45C, S48C, S50C, S53C, S55C, S58C, S60C, S65C, S70C, and S75C, as specified in JIS G4051:2016. Low alloy steel refers to carbon steel that contains at least one of Al, B, Co, Cr, Cu, La, Mo, Nb, Ni, Pb, Se, Te, Ti, V, W, and Zr, and the total content of these elements is 5 mass% or less. Tool steel refers to carbon tool steel as specified in JIS G 4401:2009 and alloy tool steel as specified in JIS G 4404:2006. Stainless steel is an alloy of Fe and 10.5 mass% or more of Cr, with a C content of 1.2% or less. Other components are specified, for example, in ISO 15510:2014. When insulating ring 13 is made of ceramics, ceramics have the lowest average linear expansion coefficient at 30°C to 400°C compared to the above metals. When insulating ring 13 made of ceramics is thermally joined to first fixing member 15 and second fixing member 16, it is preferable to use titanium or a titanium alloy for metal ring 1, since this has the lowest risk of causing cracks in the ceramics. This is because the average linear expansion coefficient of titanium or a titanium alloy is close to that of ceramics. The metal ring 12 is attached to the outer circumferential surface of the conductor 11 by, for example, a silver brazing material (Bag-8, Bag-9, etc.).
[0012] 2, the metal ring 12 is also connected to the first fixing member 15. When the metal ring 12 is connected to the first fixing member 15, the joint between the conductor 11 and the first fixing member 15 can be reinforced. The metal ring 12 and the first fixing member 15 may be connected by brazing, for example, or may simply be in contact with each other.
[0013] The size of the metal ring 12 is not limited as long as it is large enough to insert the conductor 11. For example, the outer diameter of the metal ring 12 is 1.1 to 1.4 times the outer diameter of the conductor 11. The thickness of the metal ring 12 is also not limited, and is, for example, about 2 mm to 4 mm.
[0014] The insulating ring 13 included in the airtight terminal 1 according to the embodiment is provided so as to be positioned coaxially with the conductor 11. The flatness of the main surfaces 13a and 13b on both sides of the insulating ring 13 is preferably 50 μm or less. If the flatness of the main surface 13a is 50 μm or less, when a metallized layer (not shown) is formed on the main surface 13a and the first fixing member 15 and the insulating ring 13 are joined with a brazing material, a gap is unlikely to occur between the main surface 13a and the metallized layer, and the joining reliability between the first fixing member 15 and the insulating ring 13 is improved. Similarly, if the flatness of the main surface 13b is 50 μm or less, when a metallized layer (not shown) is formed on the main surface 13b and the second fixing member 16 and the insulating ring 13 are joined with a brazing material, a gap is unlikely to occur between the main surface 13b and the metallized layer, and the joining reliability between the second fixing member 16 and the insulating ring 13 is improved. The metallized layer contains, for example, 10% to 30% by mass of manganese, with the remainder being molybdenum. The parallelism of principal surface 13a to principal surface 13b is preferably 0.1 mm or less. If the parallelism is 0.1 mm or less, when conductor 11 is inserted and fixed in the inner space of insulating ring 13, the risk of the inner surface of insulating ring 13 coming into contact with the outer surface of conductor 11 and damaging this outer surface is reduced. The insulating ring 13 is made of an insulating material, for example, a material having a volume resistivity of 10 12 There are no limitations as long as the material has a resistance of Ω·m or more. Examples of such insulating materials include ceramics containing aluminum oxide, silicon carbide, or silicon nitride as the main component. Among these materials, it is preferable to use ceramics containing aluminum oxide as the main component, since the primary raw material is inexpensive and processing is easy.
[0015] The aluminum oxide crystals preferably have an average particle size of 5 μm to 20 μm. In the present invention, the main component refers to a component that accounts for 80 mass% or more of the total 100 mass% of the components that make up the ceramic. Each component contained in the ceramic is identified by an X-ray diffraction device using CuKα rays, and the content of each component can be determined, for example, by an ICP (Inductively Coupled Plasma) emission spectroscopic analyzer or a fluorescent X-ray analyzer.
[0016] When the average grain size of the aluminum oxide crystals is 5 μm or more, the area occupied by the grain boundary phase per unit area is smaller than when the average grain size is less than 5 μm, improving thermal conductivity. On the other hand, when the average grain size is 20 μm or less, the area occupied by the grain boundary phase per unit area is larger than when the average grain size is more than 20 μm, so the anchor effect of the components that make up the brazing material increases adhesion, improving reliability and increasing mechanical strength.
[0017] The grain size of the aluminum oxide crystals can be obtained as follows. First, the surface of the insulating ring 13 is polished on a copper plate using diamond abrasive grains with an average grain size D50 of 3 μm to a depth of 0.6 mm in the thickness direction. Then, the surface is polished on a tin plate using diamond abrasive grains with an average grain size D50 of 0.5 μm. The polished surface obtained by these polishing steps is heat-treated at 1480° C. until the crystal grains and the grain boundary layer become distinguishable, and is used as the observation surface. The heat treatment is performed for, for example, about 30 minutes.
[0018] The observation surface is observed with an optical microscope, and an image is taken at a magnification of, for example, 400 times. The area of the image taken is set as the measurement range, which is 4.8747 × 102 μm. By analyzing this measurement range using image analysis software (for example, WinROOF, manufactured by Mitani Shoji Co., Ltd.), the grain size of each crystal and the average grain size from this grain size can be calculated.
[0019] Furthermore, in terms of suppressing a decrease in local mechanical strength, it is preferable that the grain size of the aluminum oxide crystals has a kurtosis of 0 or more, and may be 1 to 8. When the grain size of the aluminum oxide crystals has a kurtosis of 0 or more, the variation in grain size is suppressed. As a result, the aggregation of pores is reduced, and the shedding occurring from the outline and inside of the pores can be reduced, and it is particularly preferable that the kurtosis is 1 or more. On the other hand, when the grain size of the aluminum oxide crystals has a kurtosis of 8 or less, large grain crystals and small grain crystals are present in an appropriate ratio, and a structure is formed in which the small grain crystals fill the triple points, thereby improving the thermal conductivity.
[0020] Here, kurtosis is an index (statistic) that indicates how much the peak and tail of a distribution differ from a normal distribution, and when kurtosis is greater than 0, the distribution has a sharp peak, when kurtosis is 0, the distribution is normal, and when kurtosis is less than 0, the distribution has a rounded peak. The kurtosis of the grain size of aluminum oxide crystals can be found using the function Kurt provided in Excel (registered trademark, Microsoft Corporation).
[0021] The insulating ring 13 is fixed to the conductor 11 via the first fixing member 15. The first fixing member 15 is made of carbon steel, low alloy steel, tool steel, stainless steel, iron, copper, copper alloy, titanium, titanium alloy, molybdenum, or molybdenum alloy. The average linear expansion coefficient of these metals forming the first fixing member 15 at 30°C to 400°C is equal to or lower than the average linear expansion coefficient of copper, copper alloy, etc., which constitute the conductor 11. In addition, when the insulating ring 13 is made of ceramics, even if the first fixing member 15 is thermally joined to the conductor 11 and the insulating ring 13 with a brazing material, no gap is generated between the first fixing member 15 and the conductor 11, and between the first fixing member 15 and the insulating ring 13, and the reliability of airtightness can be improved. Among these metals, titanium or a titanium alloy is preferably used for the first fixing member 11 because it has the lowest average linear expansion coefficient at 30°C to 400°C and is therefore least likely to cause cracks in the ceramics when the insulating ring 13 made of ceramics is heat-bonded.
[0022] The size of the insulating ring 13 is not limited as long as the conductor 11 can be inserted therein. For example, the outer diameter of the insulating ring 13 is about 1.2 to 1.5 times larger than the outer diameter of the conductor 11. The thickness of the insulating ring 13 is also not limited, and is, for example, about 28 mm to 32 mm. The thickness of the insulating ring 13 is preferably 5 times or more the thickness of the metal ring 12 in order to reduce the stress remaining on the surface layer of the insulating ring 13 on the second fixing member 16 side, making it more difficult for cracks to occur. Furthermore, the thickness of the insulating ring 13 is preferably 15 times or less the thickness of the metal ring 12 in order to reduce material costs.
[0023] The insulating ring 13 is fixed to the conductor 11 at a distance from the metal ring 12. By providing the metal ring 12 and the insulating ring 13 at a distance, the stress remaining in the surface layer of the insulating ring 13 on the second fixing member 16 side is reduced, so that cracks are less likely to occur in the insulating ring 13, the first fixing member 15, and the second fixing member 16 even if heating and cooling are repeated. The distance between the metal ring 12 and the insulating ring 13 is not limited and is set appropriately depending on the size of the airtight terminal 1. The distance between the metal ring 12 and the insulating ring 13 is, for example, about 8 mm to 12 mm.
[0024] The flange 14 included in the hermetic terminal 1 according to one embodiment is placed on the insulating ring 13 and divides the conductor 11 into two regions. In the hermetic terminal 1 according to one embodiment, as shown in Fig. 1, the flange 14 divides the conductor 11 into a cylindrical portion and a rectangular prism-shaped (plate-shaped) portion.
[0025] The flange 14 is fixed to the insulating ring 13 via the second fixing member 16. The second fixing member 16 is made of carbon steel, low alloy steel, tool steel, stainless steel, iron, copper, copper alloy, titanium, titanium alloy, molybdenum, or molybdenum alloy. The average linear expansion coefficient of these metals forming the second fixing member 16 at 30°C to 400°C is equal to or lower than that of the copper or copper alloy constituting the conductor 11. In addition, when the insulating ring 13 is made of ceramics, even if the second fixing member 16 is heat-bonded to the conductor 11 and the insulating ring 13 with a brazing material, no gap is generated between the second fixing member 16 and the conductor 11, or between the second fixing member 16 and the insulating ring 13, and the reliability of airtightness can be improved. Among these metals, titanium or a titanium alloy is preferably used because it has the lowest average linear expansion coefficient at 30°C to 400°C and is least likely to cause cracks in the ceramics when the insulating ring 13 made of ceramics is heat-bonded. When at least one of the metal ring 12, the first fixing member 15 and the second fixing member 16 is made of stainless steel, the stainless steel is, for example, SUS304, SUS304L, SUS304ULC, SUS310ULC or SUSXM15J1.
[0026] The size of the flange 14 is not limited as long as the conductor 11 can be inserted therein. For example, the outer diameter of the flange 14 is 1.5 to 2.5 times the outer diameter of the insulating ring 13. The thickness of the flange 14 is not limited and is, for example, about 8 mm to 16 mm. A plurality of holes are formed in the flange 14. These holes are screw holes used to fix the airtight terminal 1 to a device.
[0027] The spacer 17 included in the hermetic terminal 1 according to one embodiment is provided between the metal ring 12 and the first fixing member 15. By providing the spacer 17, the holding force at the outer periphery of the insulating ring 13 is increased, and the reliability of the obtained hermetic terminal 1 is further improved. The spacer 17 is formed of stainless steel such as SUS304, SUS304L, SUS304ULC, SUS310ULC, and SUSXM15J1. The thickness of the spacer 17 is not limited and is, for example, about 6 mm to 14 mm.
[0028] A plurality of spacers 17 are provided along the circumferential direction (the circumferential direction in the case of a cylindrical conductor 11). It is preferable that the spacers 17 are provided at equal intervals, since the outer periphery of the insulating ring 13 can be held relatively uniformly. As a result, the reliability of the obtained airtight terminal 1 is further improved. Furthermore, at least one of the spacers 17 may have a first groove formed on the outer periphery of the spacer 17. By forming the first groove, the thermal stress is alleviated by the first groove even if heating and cooling are repeated, so that the stress applied to the insulating ring 13 can be further reduced. The first groove is formed along the circumferential direction, for example, and has a V-groove shape, a U-groove shape, or the like. Similarly, as shown in Fig. 4, the metal ring 12 may have a plurality of second groove portions 12a formed on its inner circumferential surface. By forming the second groove portions 12a, even if heating and cooling are repeated, the thermal stress is alleviated by the second groove portions 12a, so that the stress applied to the metal ring 12 can be further reduced. In particular, the second groove portions 12a are preferably positioned at equal intervals along the inner circumferential surface, and the number of the second groove portions is, for example, 3 to 20. The shape of the second groove portion 12a is, for example, rectangular as shown in FIG. 4(a) or semicircular as shown in FIG. 4(b).
[0029] The airtight terminal according to the present disclosure is not limited to the above-mentioned embodiment. For example, the above-mentioned airtight terminal 1 includes the spacer 17. However, the airtight terminal according to the present disclosure does not need to include the spacer 17. The spacer 17 is a member used to further improve the effect of the airtight terminal according to the present disclosure.
[0030] In the airtight terminal according to the present disclosure, at least one of the first fixing member 15 and the second fixing member 16 may be a sleeve having a bent portion. With such a configuration, the stress around the bent portion of the first fixing member 15 and the second fixing member 16 is further reduced, making it more difficult for cracks to occur. The inner radius of the bent portion is not limited, and in consideration of a better stress reduction effect, it is preferably 2 mm or more, and may be 4 mm or less. In particular, it is preferable that first fixing member 15 is made of a sleeve having three bent portions, as shown in Fig. 2. With this configuration, first fixing member 15 can have the main surface of insulating ring 13 on the metal ring 12 side and the outer circumferential surface of conductor 11 as bonding surfaces. If these are bonding surfaces, it becomes easy to increase the bonding area, and the reliability of airtightness can be further improved. 2, the second fixing member 16 may be made of a sleeve having a bent portion, and a part of the sleeve may be disposed between the main surface of the insulating ring 13 on the flange 14 side and the main surface of the flange 14 on the insulating ring 13 side. With this configuration, the second fixing member 16 may use the main surface of the insulating ring 13 on the flange 14 side and the main surface of the flange 14 on the insulating ring 13 side as bonding surfaces. If these are bonding surfaces, it becomes easy to increase the bonding area, and the reliability of the airtightness can be further improved. Furthermore, even if high pressure is applied to the flange 14 from the opposite side of the insulating ring 13, durability can be sufficiently maintained.
[0031] Furthermore, in the airtight terminal according to the present disclosure, the distances L1 and L2 from the axial center of the conductor 11 to the tip surfaces 15a and 16a of the first fixing member 15 and the second fixing member 16 may be the same as shown in FIG. 2, or may be different as shown in FIG. 3. It is preferable that the distances L1 and L2 from the axial center of the conductor 11 to the tip surfaces 15a and 16a of the first fixing member 15 and the second fixing member 16 are different as shown in FIG. 3, in order to prevent cracks from occurring along the axial direction of the insulating ring 13. For example, even if the brazing material shrinks due to a drop in temperature during the brazing material joining process and the insulating ring 13 is pulled in the axial direction, the tensile stress can be suppressed. The difference δ between the distances L1 and L2 from the axial center of the conductor 11 to the tip surfaces 15a and 16a of the first fixing member 15 and the second fixing member 16 is, for example, 3 mm or more and 6 mm or less.
[0032] In the above-mentioned airtight terminal 1, the conductor 11 has a shape having a cylindrical portion and a rectangular prism (plate) portion. However, the shape of the conductor in the airtight terminal according to the present disclosure is not limited as long as it is columnar. The shape of the conductor may be appropriately designed depending on the device equipped with the airtight terminal. [Explanation of symbols]
[0033] 1 Airtight Terminal 11 Conductor 12 Metal Ring 13 Insulation ring 14 Flange 15 First fixing member 16 Second fixing member 17 Spacer
Claims
1. A cylindrical conductor; a metal ring positioned coaxially with the conductor; an insulating ring positioned coaxially with the conductor; a flange disposed on the insulating ring and dividing the columnar conductor into two regions; a first fixing member for fixing the insulating ring to the conductor; a second fixing member for fixing the insulating ring to the flange; Including, the metal ring, the first fixing member and the second fixing member are formed of carbon steel, low alloy steel, tool steel, stainless steel, iron, copper, copper alloy, titanium, titanium alloy, molybdenum or molybdenum alloy, the metal ring is connected to the conductor and is connected to or in contact with the first fixing member; The insulating ring is fixed to the conductor and spaced from the metal ring.
2. 2. The hermetic terminal according to claim 1, wherein the insulating ring has a thickness that is 5 to 15 times the thickness of the metal ring.
3. 3. The hermetic terminal according to claim 1, wherein at least one of the first fixing member and the second fixing member is a sleeve having a bent portion.
4. 4. The airtight terminal according to claim 1, wherein the first fixing member is a sleeve having three bent portions.
5. The airtight terminal according to any one of claims 1 to 4, wherein the second fixing member is a sleeve having a bent portion, and a portion of the sleeve is disposed between a main surface of the insulating ring on the flange side and a main surface of the flange on the insulating ring side.
6. 6. The hermetic terminal according to claim 1, wherein the distances from the axis of the conductor to the tip faces of the first fixing member and the second fixing member are different from each other.
7. 7. The hermetic terminal according to claim 1, further comprising a plurality of spacers provided along a circumferential direction between the metal ring and the first fixing member.
8. 8. The hermetic terminal according to claim 7, wherein the spacers are disposed at equal intervals.
9. 9. The hermetic terminal according to claim 7, wherein at least one of the spacers has a first groove formed on an outer circumferential surface thereof.
10. The airtight terminal according to any one of claims 1 to 9, wherein the metal ring has a plurality of second grooves formed on an inner peripheral surface thereof.
11. 11. The hermetic terminal according to claim 1, wherein the insulating ring contains ceramics containing aluminum oxide as a main component, and the aluminum oxide crystals have an average grain size of 5 μm or more and 20 μm or less.
12. 12. The hermetic terminal according to claim 11, wherein the grain size of the aluminum oxide crystals has a kurtosis of 0 or more.
Citation Information
Patent Citations
Ceramic insulating ring
JP1984047916U
Structure of brazing and airtight terminal
JP2006210172A
Airtight terminal
JP2007201335A
Hermetic terminal
WO2021015189A1