Ammonia as a processing aid for atomized solid dispersions
Using ammonia to form ammonium salts and carefully removing residual ammonia, the method addresses low solubility issues in forming sprayed solid dispersions, enhancing solubility and stability of active agents while maintaining high manufacturing efficiency.
Patent Information
- Application Number
- JP2022509012
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-08-15
- Filing Date
- 2020-08-11
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2040-08-11
AI Technical Summary
Existing methods for forming sprayed solid dispersions face challenges due to low solubility of active agents in volatile organic solvents, leading to unacceptably low manufacturing throughput, degraded particle properties, and thermal/chemical degradation, particularly for weakly acidic agents with low solubility in common organic solvents.
The use of ammonia as a processing aid to form ammonium salts of active agents, increasing solubility, followed by careful removal of residual ammonia to regenerate the active agent in its free acid form, using controlled temperature, humidity, and sweep gas to achieve a final product with minimal ammonia content.
This approach enhances solubility of active agents by several times, allows for higher concentrations in the spray solution, and results in a final product with at least 90% of the active agent in free acid form and minimal ammonia content, improving manufacturing efficiency and product stability.
Smart Images

Figure 0007590409000002 
Figure 0007590409000003 
Figure 0007590409000001
Abstract
Description
[Technical field]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims priority to the earlier filing date of U.S. Provisional Application No. 62 / 887,471, filed August 15, 2019, which is incorporated by reference in its entirety.
[0002] The present disclosure relates to methods for using ammonia as a processing aid when forming an atomized solid dispersion and subsequently removing the ammonia from the atomized solid dispersion. The atomized solid dispersion formed by the disclosed methods is also included in the present disclosure. Summary of the Invention
[0003] Disclosed are embodiments of a method for using ammonia as a processing aid in forming a sprayed solid dispersion, as well as embodiments of the sprayed solid dispersion formed by the method. In some embodiments, the method for preparing the sprayed solid dispersion includes: (i) mixing an active agent, a dispersion polymer, an amount of ammonia, and a solvent to form a spray solution; (ii) spraying the spray solution to form a sprayed solid dispersion comprising the active agent, the dispersion polymer, and ammonia; and (iii) removing residual ammonia from the sprayed solid dispersion to form a product comprising a solid dispersion of the active agent and the dispersion polymer, the product comprising 500 ppm or less of ammonia. In any of the above embodiments, at least 90% by weight of the active agent in the product may be in free acid form.
[0004] In some embodiments, the solvent comprises a C1-C3 alkanol, the active agent in free acid form has a pKa of 7 or less and a solubility of 40 mg / mL or less in the solvent, and the amount of ammonia is sufficient to dissolve the active agent in the solvent. The solvent may comprise a C1-C3 alkanol and a co-solvent.
[0005] In any of the above embodiments, the amount of ammonia can be at least 0.95 molar equivalents relative to the total of the acid groups of the active agent and any acid groups of the dispersion polymer, for example, 0.95 to 10 molar equivalents relative to the total of the acid groups of the active agent and all acid groups of the dispersion polymer and other excipients (if present). In some embodiments, the amount of ammonia is 0.95 to 4 molar equivalents relative to the total of the acid groups of the active agent and all acid groups of the dispersion polymer and other excipients (if present). In some embodiments, the amount of ammonia is at least 0.95 molar equivalents relative to the total of all acid groups of the dispersion polymer and an amount of acid groups of the active agent that exceeds the solubility of the free acid form of the active agent in the solvent.
[0006] In any of the foregoing embodiments, the active agent can have a solubility in the spray solution that is at least two times higher than the solubility of the free acid form of the active agent in the ammonia-free solvent. In any of the foregoing embodiments, the spray solution can have a dissolved solids content in the range of 2-40% by weight, where 0.5-95% by weight of the dissolved solids is the active agent. In some embodiments, the spray solution comprises 0.5-20% by weight of the active agent.
[0007] In any of the foregoing embodiments, removing residual ammonia may include heating the atomized solid dispersion at a temperature in the range of 30-70° C. and a relative humidity (RH) in the range of 10-75% for a time sufficient to form a product containing 500 ppm or less of ammonia. In some embodiments, (i) the time is 2-60 hours, or (ii) the temperature is in the range of 40-60° C., or (iii) the RH is in the range of 15-50%, or (iv) any combination of (i), (ii), and (iii). In any of the foregoing embodiments, removing residual ammonia may further include blowing a sweep gas over the atomized solid dispersion while heating the atomized solid dispersion at the temperature and RH.
[0008] Embodiments of the atomized solid dispersions prepared by the disclosed methods include at least 0.5% by weight of active agent and 500 ppm or less of ammonia. In some embodiments, the atomized solid dispersions include 0.5-95% by weight of active agent, where at least 90% by weight of the active agent is amorphous and the dispersion polymer, and 50 ppm or less of ammonia.
[0009] The above and other objects, features and advantages of the present invention will become more apparent from the following detailed description which proceeds with reference to the accompanying drawings. [Brief description of the drawings]
[0010] [Figure 1] PXRD spectra of spray dried dispersions (SDD) of piroxicam and PVP-VA64 after drying at 50° C. and 30% relative humidity for 48 hours. [Diagram 2] PXRD spectra of SDD of piroxicam and HPMCAS after drying at 50° C. and 30% relative humidity for 48 hours. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Methods for forming sprayed solid dispersions (e.g., spray-dried dispersions, spray-layered dispersions) comprising an active agent and a dispersion polymer generally involve spraying a solution comprising the active agent, the dispersion polymer, and a solvent. A problem that frequently arises during spray drying of active agents, e.g., active pharmaceutical ingredients (APIs), is that low solubility of the active agent in preferred volatile organic spray solvents, e.g., acetone and methanol, can adversely affect manufacturability and product quality. Specifically, low dissolved solids concentrations in the spray solution can lead to unacceptably low manufacturing throughput and poor particle properties. In some cases, solubility in the spray solvent is so low that commercial production of spray-dried intermediates, e.g., spray-dried dispersions (SDDs) or spray-layered dispersions (SLDs), is not economically feasible and / or cannot be carried out without special measures, e.g., high temperatures and / or long spray times using dilute solutions. However, elevated temperatures can lead to thermal and / or chemical degradation of some active agents. Prolonged spraying of dilute solutions can tie up equipment for long periods of time, reducing throughput and profits, and adversely affect particle properties. Poorly soluble actives often have a strong tendency to crystallize and a high melting point, contributing to their poor solubility in organic solvents. In addition, many of these actives exist in various polymorphs and tend to recrystallize in the spray solvent or turn to the lowest energy (least soluble) polymorph. If the low-solubility active is a weak acid (pKa 3-7), one solution to the low organic solubility of the active is to ionize the active with a base to increase the solubility of the active in polar volatile organic solvents, e.g., methanol. Processes have been described previously in which such bases include non-volatile counterions that are not removed from the spray-dried material and become part of the product as a salt of the acid, e.g., potassium salt (U.S. Patent No. 8,372,836). Two important drawbacks of this method are that 1) the addition of non-volatile counterions reduces the efficacy of the formulation, and 2) the presence of non-volatile counterions can adversely affect the physical stability of the product compared to the free acid form, e.g., by increasing the hygroscopicity of the salt form of the active.
[0012] The disclosed process embodiments alleviate one or more of these problems. As disclosed herein, ammonia, a volatile base, is used to form an ammonium salt with a weak acid active agent, resulting in a several-fold higher concentration of the active agent dissolved in a volatile solvent. This ammonium salt of the active agent can be prepared in the presence of a dispersion polymer and other excipients and sprayed (e.g., spray-dried or spray-layered) to form a sprayed dispersion (SD). During the spraying process, some of the ammonia is removed and some of the free acid form of the active agent is regenerated. During secondary drying of the SD to remove the solvent, another ammonia is removed, but not to the extent desired. In some embodiments, near complete removal of the ammonia, and thus near complete regeneration of the active agent in its free acid form, typically utilizes extended processing times and / or more aggressive drying conditions (e.g., relative saturation of the solvent using solvent-assisted drying, relative humidity, and / or elevated temperatures) than are typically used when no base is added. In some cases, elevated temperature and humidity, with or without extended processing times, removes nearly all of the ammonia and regenerates nearly all of the active agent as a free acid. The time, temperature, and / or humidity conditions used to remove substantially all of the ammonia may depend, at least in part, on the pKa of the active agent, the type of dispersion polymer and other excipients used, the mass ratio of these materials, and / or potentially, the particle morphology.
[0013] I. Definitions and Abbreviations The following explanations of terms and abbreviations are provided to better describe the present disclosure and guide those skilled in the art in practicing the present disclosure. As used herein, "comprising" means "including," and the singular form "a" or "an" or "the" includes plural references unless the context clearly dictates otherwise. Thus, the indefinite article "a" or "an" generally means "at least one." The term "or" refers to a single element or a combination of two or more elements of stated alternative elements, unless the context clearly dictates otherwise.
[0014] Unless otherwise stated, all technical and scientific terms used herein have the same meaning as commonly understood by those skilled in the art to which this disclosure belongs.Methods and materials similar or equivalent to those described herein can be used to carry out or test this disclosure, but suitable methods and materials are described below.The materials, methods, and examples are illustrative only and are not intended to be limiting.Other features of the present disclosure will be apparent from the following detailed description and claims.
[0015] The disclosure of a numerical range should be understood as referring to each discrete point within the range, including the endpoints, unless otherwise indicated. Unless otherwise indicated, all numbers expressing amounts, molecular weights, proportions of ingredients, temperatures, times, etc. used in the specification or claims should be understood as modified by the term "about". The term "about" used in the disclosure of a numerical range indicates that deviations from the stated value are acceptable within the range in which the deviations are the result of measurement variability and / or products of the same or similar properties are obtained. Thus, unless otherwise implicitly or explicitly indicated, or unless the skilled artisan properly understands the situation and provides a more clear explanation, the numerical parameters described are approximations that may depend on the desired properties sought and / or detection limits under standard testing conditions / methods known to those skilled in the art. When directly and explicitly distinguishing the embodiments from the prior art described, the numerical values of the embodiments are not approximations unless the word "about" is recited.
[0016] The existence of alternatives for the various components, parameters, operating conditions, etc. described herein does not imply that the alternatives are necessarily equivalent and / or will function equally well, nor does it imply that the alternatives are listed in order of preference, unless otherwise stated.
[0017] Definitions of common chemical terms can be found in "Hawley's Condensed Chemical Dictionary," edited by Richard J. Lewis, Sr., published by John Wiley & Sons, Inc. in 2016 (ISBN 978-1-118-13515-0).
[0018] Active Agent: As used herein, the term "active agent" refers to an ingredient that exerts a desired physiological effect on a mammal, including but not limited to a human. Synonyms include "active ingredient," "active substance," "active ingredient," "active pharmaceutical ingredient," and "drug."
[0019] Amorphous: Substantially non-crystalline (e.g., at least 95% amorphous). Amorphous solids lack a definite crystal structure and a sharp, well-defined melting point; instead, amorphous solids melt gradually over a wide range of temperatures.
[0020] Dispersion: a system in which particles are distributed in a continuous phase of different composition. A solid dispersion is a system in which at least one solid component is dispersed in another solid component.
[0021] Excipient: A physiologically inactive substance used as an additive in a pharmaceutical composition. As used herein, an excipient may be incorporated within or physically mixed with a particle of a pharmaceutical composition. For example, an excipient may be used to dilute an active agent and / or to change the properties of a pharmaceutical composition. Examples of excipients include, but are not limited to, binders, fillers, diluents, disintegrants, lubricants, surfactants, coating agents, colorants, flavorings, and combinations thereof. The term "excipient" does not include the dispersion polymers disclosed herein.
[0022] Glass transition temperature, T g : The temperature at which an amorphous solid, such as a glass or polymer, becomes brittle or tough when cooled, or soft or pliable when heated. T gcan be measured, for example, by differential scanning calorimetry (DSC). DSC measures the difference in the amount of heat required to raise the temperature of a sample and a reference as a function of temperature. During a phase transition, for example, during the change from an amorphous state to a crystalline state, the amount of heat required changes. For solids with no crystalline components, a single glass transition temperature indicates that the solid is homogeneous or a molecular dispersion. Generally, when glasses are tested by raising the temperature of a sample at a constant rate, usually 1-10 °C / min, the T g A relatively rapid increase in heat capacity is observed near T g can also be measured by dynamic mechanical analyzer (DMA), dilatometer, or dielectric constant measurement. g The values may vary, but are usually within 10-30°C of each other. For example, the T measured by DMA is g is often measured by DSC. g The dry glass transition temperature is the temperature measured when the solid is in equilibrium at a relative humidity of 5% or less. g Refers to...
[0023] Relative Humidity (RH): A measurement of the amount of water in the air compared to the amount of water the air can hold at a particular temperature.
[0024] SD: nebulized solid dispersion.
[0025] SDD: Spray-dried dispersion.
[0026] SLD: sprayed layered dispersion.
[0027] Solubilize: To dissolve or increase solubility.
[0028] Solution: A homogeneous mixture of two or more substances. The solute (minor component) is dissolved in the solvent (major component). In contrast to a suspension, light passes through a solution without being scattered from the solute particles.
[0029] Spray solution: As used herein, the term "spray solution" refers to a fluid formed by dissolving an active agent and a dispersion polymer in a solvent and a quantity of ammonia. In the case of an active agent, the term "dissolved" has its conventional meaning, indicating that the active agent is in solution when mixed with a solvent and a quantity of ammonia. In the case of a dispersion polymer, the term "dissolved" can take a broader definition. In the case of some dispersion polymers, the term "dissolved" can mean that the dispersion polymer is in solution and dissolved in the conventional sense, or that the dispersion polymer is dispersed or highly swollen with the solvent so that it acts as if it is in solution, or that some of the dispersed polymer molecules are in solution and the remaining dispersed polymer molecules are dispersed or highly swollen with the solvent. Any suitable technique can be used to determine whether the active agent and the dispersion polymer are dissolved. Examples include dynamic or static light scattering analysis, turbidity analysis, and visual observation.
[0030] Volatile organic solvent: an organic solvent having a boiling point of 150° C. or less. Volatile organic solvents include, but are not limited to, methanol, ethanol, propanol isomers, butanol isomers, 1-pentanol, 2-methyl-1-propanol, acetic acid, formic acid, certain ketones (e.g., acetone, methyl ethyl ketone), certain esters (e.g., methyl acetate, ethyl formate, ethyl acetate), C4 to C7 alkanes, and the like.
[0031] II. Spraying process Ideally, the spray solution has a dissolved solids content (e.g., active agent and dispersion polymer) of 10-15% by weight at ambient temperature. Often it is advantageous to prepare a sprayed solid dispersion (SD) containing active agent and dispersion polymer, the SD having a high loading of active agent, e.g., at least 25% by weight active agent content.
[0032] In some embodiments, the active agent is a weakly acidic active agent (e.g., an active agent having a pKa in the range of 3-7 in its free acid form). Many weakly acidic active agents are poorly soluble in common organic spray solvents, including volatile organic solvents, such as C1-C5 alkanols, e.g., methanol, ethanol, n-propanol, isopropanol, and the like. As used herein, "poorly soluble" means that the active agent in the free acid form has a solubility of 40 mg / mL or less in one or more C1-C5 alkanols, e.g., a solubility of 30 mg / mL or less, 20 mg / mL or less, or 10 mg / mL or less in one or more C1-C5 alkanols. In some embodiments, the active agent in the free acid form has a solubility of 40 mg / mL or less in one or more C1-C3 alkanols, e.g., a solubility of 30 mg / mL or less, 20 mg / mL or less, or 10 mg / mL or less in one or more C1-C3 alkanols. For example, the active agent can have a solubility of 40 mg / mL or less in methanol, ethanol, n-propanol, and / or isopropanol at ambient or room temperature, where the ambient temperature is within the range of 20-25° C. In some examples, the active agent has a solubility of 10 mg / mL or less in methanol, ethanol, n-propanol, and / or isopropanol at ambient temperature.
[0033] The solubility of the active agent can be increased by forming an ammonium salt of the active agent in the spray solution. In some embodiments, the weakly acidic active agent is dissolved in a C1-C5 alkanol by converting the active agent to an ammonium salt of the active agent. In some embodiments, the C1-C5 alkanol is a C1-C3 alkanol or a combination of C1-C3 alkanols. Exemplary alkanols include methanol, ethanol, n-propanol, isopropanol, or any combination thereof. However, the presence of ammonia in the final product is often undesirable. Ammonia can impart an unpleasant odor to the product. In some cases, ammonia present in the product can degrade the active agent and / or the dispersion polymer over time.
[0034] The solid dispersion to be sprayed can be prepared by (i) mixing an active agent, a dispersion polymer, an amount of ammonia, and a solvent to form a spray solution, (ii) spray drying the spray solution to form a SD comprising the active agent, the dispersion polymer, and ammonia, and (iii) removing residual ammonia from the SD to form a product comprising a solid dispersion of the active agent and the dispersion polymer, the product comprising 500 ppm or less of ammonia, e.g., 300 ppm or less, 200 ppm or less, 100 ppm or less, or 50 ppm or less of ammonia. Unless otherwise specified, "ppm" as used herein refers to parts per million by weight. In some embodiments, the product comprises 1 to 500 ppm, e.g., 1 to 300 ppm, 1 to 200 ppm, 1 to 100 ppm, 1 to 50 ppm, or 1 to 25 ppm of ammonia. The ammonia content can be determined by any suitable method, e.g., by use of an ammonia ion-selective electrode. In some embodiments, the solid dispersion is a solid amorphous dispersion.
[0035] In some embodiments, the solvent comprises a C1-C3 alkanol or a combination of C1-C3 alkanols, e.g., the solvent comprises methanol, ethanol, n-propanol, isopropanol, or any combination thereof. In some embodiments, the solvent further comprises a co-solvent. Exemplary co-solvents include, but are not limited to, water, tetrahydrofuran, ethyl acetate, methyl acetate, 1,3-dioxolane, acetone, methyl ethyl ketone, or any combination thereof. The co-solvent can facilitate dissolution of the active agent, the dispersion polymer, or both, provided that the amount of C1-C3 alkanol in the mixed solvent is sufficient to form a salt of the active agent using ammonia. In some embodiments, the solvent comprises 50% or less by weight of one or more co-solvents, e.g., 40% or less by weight, 30% or less by weight, 20% or less by weight, or 15% or less by weight of one or more co-solvents, with the remainder being one or more C1-C3 alkanols. For example, the solvent can include 0.01-50% by weight of the co-solvent, e.g., 0.1-40% by weight, 1-30% by weight, 2-20% by weight, or 5-15% by weight of one or more co-solvents. In some embodiments, the co-solvent is water, e.g., 30% by weight or less water, 20% by weight or less water, or 15% by weight or less water, the remainder being one or more C1-C3 alkanols. In some embodiments, the solvent includes 0.01-30% by weight water, 0.1-30% by weight water, 1-30% by weight water, 10-30% by weight water, or 10-20% by weight water. In some examples, water is included when the dispersion polymer includes hydroxypropyl methylcellulose (HPMC). In some embodiments, the co-solvent is tetrahydrofuran (THF), e.g., 30% by weight or less THF, 20% by weight or less THF, or 15% by weight or less THF, the remainder being one or more C1-C3 alkanols. In some examples, THF is included when the dispersion polymer comprises cellulose acetate phthalate (CAP), hi some embodiments, the solvent comprises 0.01-30 wt% THF, 0.1-30 wt% THF, 1-30 wt% THF, 10-30 wt% THF, or 20-30 wt% THF.For example, when the dispersion polymer includes CAP, the solvent may include methanol and THF in a weight ratio of 8:2 or 7:3.
[0036] The active agent in crystalline or free acid form has a pKa of 7 or less and a solubility of 40 mg / mL or less in the solvent, e.g., 30 mg / mL or less, 20 mg / mL or less, or 10 mg / mL or less. In some embodiments, the free acid form of the active agent has a pKa in the range of 3 to 7. The active agent may have a solubility of the free acid form in the solvent in the range of 0.0001 mg / mL to 40 mg / mL, e.g., a solubility of the free acid form in the solvent in the range of 0.001 to 40 mg / mL, 0.001 to 30 mg / mL, 0.001 to 20 mg / mL, 0.001 to 10 mg / mL, 0.01 to 10 mg / mL, 0.01 to 5 mg / mL, 0.01 to 2.5 mg / mL, or 0.01 to 1 mg / mL.
[0037] The amount of ammonia is sufficient to dissolve the activator in the solvent, i.e., to form a solution of the activator in the solvent. However, excess ammonia may degrade certain activators and / or dispersion polymers. Thus, the amount of ammonia is not so great as to degrade either the activator or the dispersion polymer. In some embodiments, the activator and the solvent are mixed to form a suspension or slurry, and sufficient ammonia is added to dissolve the activator. In one independent embodiment, the ammonia and the solvent are mixed, followed by the activator to form a solution. In some embodiments, the amount of ammonia is at least 0.95 molar equivalents relative to the total number of acid groups of the activator. However, the amount of ammonia may be significantly greater and is essentially unlimited, provided that the additional ammonia does not degrade either the activator or the dispersion polymer. For example, in some examples, the amount of ammonia may be up to 10 molar equivalents relative to the total number of acid groups of the activator. In some embodiments, the amount of ammonia in the spray solution is 0.95 to 10 molar equivalents relative to the total acid groups of the activator, e.g., 0.95 to 5, 0.95 to 4, 0.95 to 3, 0.95 to 2, 0.95 to 1.5, or 0.95 to 1.1 molar equivalents relative to the total acid groups of the activator.
[0038] The mass of ammonia added used to form the salt of the activator is a function of the molecular weight of the activator. For example, when forming a dispersion to be sprayed containing 100 g of an activator with a molecular weight of 250 g / mole, one equivalent of ammonia will be 6.8 g. However, when forming a dispersion to be sprayed containing 100 g of an activator with a molecular weight of 500 g / mole, one equivalent of ammonia will be only 3.4 g.
[0039] Advantageously, in some embodiments, the addition of ammonia increases the solubility of the active agent in the solvent by at least a factor of 2. In some embodiments, ammonia increases the solubility of the active agent by at least a factor of 3, at least a factor of 4, at least a factor of 5, at least a factor of 10, at least a factor of 20, at least a factor of 30, or at least a factor of 40, as compared to the crystalline (free acid form) solubility of the active agent in the solvent without ammonia.
[0040] However, in some embodiments, it may be beneficial or desirable to limit the amount of excess ammonia. Excess ammonia may be limited, for example, if the excess ammonia degrades the active agent and / or the dispersion polymer. In such cases, the amount of active agent that does not dissolve can be determined or calculated, and the amount of ammonia added may be 0.95 to 1.1 molar equivalents relative to the amount of active agent that exceeds the solubility of the free acid form of the active agent in the solvent, i.e., the sum of the acid groups of the amount of active agent that does not dissolve. For example, active agent X may have a solubility of the free acid form of 5.0 mg / mL in methanol, and a concentration of 20.0 mg / mL may be desired for spray drying. Since 25% of active agent X has dissolved in methanol, the amount of ammonia to dissolve the remaining active agent X may be 75% of the amount calculated based on the total concentration of active agent X (20 mg / mL). Thus, the amount of ammonia may be about 0.75 molar equivalents per 20 mg / mL of total acid groups of activator X, or 0.95-1.1 molar equivalents per 15 mg / mL of total acid groups of activator X.
[0041] The dispersion polymer is added to the solution to form a spray solution. In some embodiments, the dispersion polymer is dissolved in the solvent and is in solution. In some embodiments, the dispersion polymer is dispersed or highly swollen with the solvent and behaves as if it were in solution. In some cases, some of the dispersed polymer molecules are in solution and the remaining dispersed polymer molecules are dispersed or highly swollen with the solvent. The dispersed polymer has a dry glass transition temperature T greater than 60° C. g The dispersion polymer may have a solubility of 0.95 to 1.0001%. The dispersion polymer may be added before or after the addition of ammonia. In some cases, two or more dispersion polymers are added to the solution to form a spray solution. Some dispersion polymers contain one or more acid groups. In such cases, the amount of ammonia added may be at least 0.95 molar equivalents relative to the total of the acid groups of the active agent and all of the acid groups of the dispersion polymer or polymers to ensure that there is enough ammonia to completely dissolve the active agent. Excess ammonia may be utilized as long as the amount of ammonia is not sufficient to decompose the active agent and / or the dispersion polymer. In some embodiments, the amount of ammonia is 0.95 to 10 molar equivalents relative to the total of the acid groups of the active agent and all of the acid groups of the dispersion polymer, for example, 0.95 to 5, 0.95 to 4, 0.95 to 3, 0.95 to 2, 0.95 to 1.5, or 0.95 to 1.1 molar equivalents relative to the total of the acid groups of the active agent and all of the acid groups of the dispersion polymer. Alternatively, if it is beneficial or desirable to limit the amount of excess ammonia, the amount of ammonia added may be 0.95 to 1.1 molar equivalents based on the total amount of acid groups on the undissolved activator and all of the acid groups on the dispersion polymer.
[0042] A determined amount of ammonia is added to the solvent or to a slurry or suspension containing the solvent and the activator. The dispersion polymer can be added before or after the addition of the ammonia. In some embodiments, the ammonia is added to a solution of ammonia in an alcohol, for example, a solution of ammonia in methanol, ethanol, or propanol. In one separate embodiment, an aqueous solution of ammonia dissolved in water (i.e., ammonium hydroxide) is added. In another separate embodiment, ammonia gas is added.
[0043] In some embodiments, the spray solution further comprises one or more excipients. As used herein, the term "excipient" does not include dispersion polymers. Advantageously, any excipient is soluble in the spray solution. The excipients can be added before or after the addition of ammonia. In some embodiments, up to 25% by weight, up to 50% by weight, up to 75% by weight, up to 90% by weight, or up to 95% by weight of the dissolved solids is provided by one or more excipients. For example, the dissolved solids may comprise 0.01-95% by weight, 0.5-95% by weight, 1-95% by weight, 10-95% by weight, 25-95% by weight, 50-95% by weight, 75-95% by weight, 0.5-90% by weight, 0.5-75% by weight, 0.5-50% by weight, or 0.5-25% by weight of the excipients. In some embodiments, the amount of ammonia is 0.95 to 4 molar equivalents relative to the total of the acid groups of the active agent, all of the acid groups of the dispersion polymer, and all of the acid groups of the one or more excipients, such as 0.95 to 3, 0.95 to 2, 0.95 to 1.5, or 0.95 to 1.1 molar equivalents relative to the total of the acid groups of the active agent, all of the acid groups of the dispersion polymer, and all of the acid groups of the excipients. Alternatively, if it is beneficial or desirable to limit the amount of excess ammonia, the amount of ammonia added may be 0.95 to 1.1 molar equivalents relative to the total of the acid groups of the amount of undissolved active agent, all of the acid groups of the dispersion polymer, and all of the acid groups of the one or more excipients.
[0044] In some embodiments, the spray solution has a dissolved solids content of 2-40% by weight at ambient temperature (e.g., at a temperature of 20-25° C.), e.g., a solids content of 2-30%, 2-25%, 2-20%, 2-15%, 5-15%, or 10-15% by weight at ambient temperature, with 0.5-95% by weight of the dissolved solids being active agent. Thus, the spray solution may have a combined active agent and dispersion polymer content of 2-40%, 2-30%, 2-25%, 2-20%, 5-20%, 5-15%, or 10-15% by weight. Alternatively, the spray solution may have a combined active agent, dispersion polymer, and excipient content of 2-40%, 2-30%, 2-25%, 2-20%, 2-15%, 5-15%, or 10-15% by weight. It is often desirable for the active agent content in the sprayed solid dispersion to be at least 25% by weight, e.g., 25-95% by weight, with the remainder comprising dispersion polymer and optional excipients. In some embodiments, the spray solution comprises 0.5-20% by weight active agent and a total solids (active agent, dispersion polymer, and any optional excipients) content of 2-40% by weight. In some embodiments, the spray solution comprises 2.5-15% by weight active agent and a total solids content of 10-20% by weight. In some embodiments, the spray solution comprises at least 5 mg / mL active agent, e.g., 5-167 mg / mL or 5-125 mg / mL active agent.
[0045] The spray solution is sprayed to form a sprayed solid dispersion comprising the active agent, the dispersion polymer, and the ammonia. If an excipient is present in the spray solution, the SD further comprises the excipient. The SD may also include residual solvent. Since the presence of ammonia in the sprayed solid dispersion may be undesirable, the ammonia is then removed to form a product comprising a dispersion of the active agent and the dispersion polymer. If residual solvent is present, it may also be removed. In some embodiments, the residual solvent and the ammonia are removed simultaneously in a single process.
[0046] In some embodiments, the SD is formed by spray drying and is a spray-dried dispersion (SDD). The term "spray drying" is used conventionally and broadly refers to a process that involves breaking a liquid mixture into small droplets (atomization) and rapidly removing the solvent from the mixture in a container (drying chamber) where there is a strong driving force to evaporate the solvent from the droplets. Typically, an active agent, a dispersion polymer, and ammonia are added to a solvent to form a spray solution. The spray solution is then sprayed into a spray-drying chamber by an atomizer. The droplets are contacted with a heated drying gas, such as dry nitrogen, in the spray-drying chamber. The droplets are rapidly dried to form particles that include a solid dispersion or SDD, which includes the active agent and the dispersion polymer. The particles exit the spray dryer and are collected. Subsequent processes are used to remove ammonia and residual solvent from the particles.
[0047] Exemplary apparatus and procedures for forming SDDs are also described in U.S. Pat. Nos. 8,263,128, 9,084,944, 9,248,584, 9,724,664, and PCT Publication WO 2010 / 132827, each of which is incorporated herein by reference.
[0048] In some embodiments, the sprayed solid dispersion is a sprayed layered dispersion (SLD) sprayed onto a core, and a coating is formed comprising a dispersion of active agent and a dispersion polymer. For example, a spray solution can be sprayed onto the core by an atomizer to form a coating on the core comprising a dispersion of active agent and a dispersion polymer. Exemplary cores include, but are not limited to, melt-congealed cores (e.g., as described in US Published Application No. 2010 / 0068276), nonpareil or sugar-based cores, or tablets.
[0049] III. Solvent and Ammonia Removal The sprayed solid dispersion made by the process as disclosed herein includes an active agent, a dispersion polymer, and ammonia. The SD can further include one or more excipients. In many products that include SD, the presence of large amounts of ammonia (e.g., greater than 500 ppm) is undesirable. Thus, in some embodiments, the process further includes removal of residual ammonia from the SD to form a product containing 500 ppm or less of ammonia, e.g., 400 ppm or less, 300 ppm or less, 200 ppm or less, 100 ppm or less, or 50 ppm or less of ammonia. In some embodiments, the product contains 0-500 ppm, e.g., 1-500 ppm, 1-400 ppm, 1-300 ppm, 1-200 ppm, 1-100 ppm, 1-50 ppm, or 1-25 ppm of ammonia. Once the ammonia is removed, the ammonia salt of the active agent reverts to the free acid form in the SD. In some embodiments, when ammonia is removed from the sprayed solid dispersion, at least 90%, at least 95%, at least 97%, at least 98%, or at least 99% by weight of the active agent reverts to the free acid form. In some embodiments, when ammonia is removed, 90-100%, 95-100%, 97-100%, 98-100%, or 99-100% by weight of the active agent reverts to the free acid form. If the dispersion polymer contains acid groups, those groups can also revert to the acid form.
[0050] There is a correlation between the amount of ammonia remaining in the product and the molecular weight of the activator. For example, if enough ammonia is removed to convert 95% by weight of the activator to the free acid form, a SD containing a given mass of low molecular weight activator will retain a higher ppm level of ammonia than an SD containing the same mass of high molecular weight activator. If an SD contains 100 g of activator with a molecular weight of 250 g / mol and 5% by weight remains as the ammonium salt, the SD will retain 0.02 mol of ammonia. If an SD contains 100 g of activator with a molecular weight of 500 g / mol and 5% by weight remains as the ammonium salt, the SD will retain 0.01 mol of ammonia.
[0051] In some embodiments, the SD further comprises residual solvent. Including residual solvent may be undesirable. Separate processes may be used to remove the residual solvent and the ammonia. Alternatively, the residual solvent and at least a portion of the ammonia may be removed in a single process. In some embodiments, the removal of the solvent occurs much more quickly than the removal of ammonia under the same conditions. In some embodiments, all or substantially all (e.g., at least 95%) of the residual solvent is removed with ammonia. For example, the methanol content may be reduced to less than 0.3 wt.% in less than 30 minutes at temperature and relative humidity conditions that require 4 to 48 hours or more to reduce the ammonia to a concentration of 500 ppm or less. Thus, a single process may be performed at conditions selected to achieve the desired concentration of ammonia within a reasonable period of time.
[0052] In some embodiments, residual ammonia is removed by heating the SD at a temperature in the range of 30-70° C. for a sufficient time to form a product containing 500 ppm or less ammonia. Advantageously, the temperature is selected such that no significant thermal degradation of the activator occurs during the ammonia removal process. Once the ammonia is removed, the residual solvent may be removed. In some embodiments, the temperature is in the range of 40-60° C. In some embodiments, the SD is maintained at 10-75% relative humidity (RH) during the ammonia and solvent removal process. In some embodiments, the SD is maintained at 10-60% RH, 10-50% RH, 15-50% RH, or 15-30% RH.
[0053] The removal of ammonia is carried out for a time sufficient to reduce the ammonia content to 500 ppm or less. The ammonia content can be determined by any suitable method, such as by use of an ammonia ion selective electrode (ISE). In some embodiments, the ammonia is measured by dissolving a known amount of the SD in a dilute aqueous base solution (e.g., 0.1 M NaOH) and taking millivolt readings with the ISE. The readings are compared to a standard curve made from solutions of known ammonia concentrations to determine the amount of ammonia remaining in the SD. In some embodiments, the time is between 2 and 60 hours, such as between 4 and 60 hours or between 4 and 48 hours.
[0054] In some embodiments, removing residual ammonia further comprises blowing a sweep gas over the SD for at least a period of time. Desirably, the sweep gas is inert to the SD. Suitable sweep gases include, but are not limited to, nitrogen, argon, carbon dioxide, air, and combinations thereof.
[0055] In some embodiments, the sweep gas further comprises water vapor (e.g., sufficient water to provide 10-50% RH during the ammonia and solvent removal process) and / or a volatile organic solvent vapor (e.g., methanol vapor). Without wishing to be bound by any theory or mechanism of action, the inclusion of water vapor or a volatile organic solvent vapor in the sweep gas may lower the glass transition temperature of the particles of SD, thereby increasing the diffusion rate of residual ammonia and / or residual solvent within the particles. As a result, mass transfer of ammonia and / or residual solvent from the particles may increase, such that the ammonia and / or residual solvent are removed more quickly.
[0056] In some embodiments, the drying parameters (time, temperature, relative humidity, and / or sweep gas composition) depend, at least in part, on the active agent pKa, dispersion polymer composition, properties of any excipients, mass ratios of components, and / or particle morphology (e.g., particle size). For example, larger particle sizes may require longer times. Furthermore, for at least some SDs, the dispersion polymer influences the time. For example, it has been found that a longer time is required to remove ammonia from an SD containing PVP-VA than from a comparable SD containing HPMCAS. Increasing the temperature and / or RH may reduce the time to remove the desired amount of ammonia.
[0057] The removal of ammonia (and solvent) can be carried out using any suitable equipment, such as tray dryers, mechanically agitated drying chambers, drum dryers, fluidized beds, drying equipment with conveyor belts passing through the equipment, etc. The above list is not intended to indicate that all embodiments are equally and / or equally suitable. In some embodiments, a tray dryer or a mechanically agitated drying chamber is utilized. When a mechanically agitated drying chamber is utilized, the particles of SD are introduced into a drying chamber having an outer wall. A sweep gas flows through the drying chamber and the particles are circulated within the drying chamber by a mechanical agitator independent of the wall.
[0058] IV. Activators Embodiments of the disclosed processes are used to form sprayed solid dispersions (SDs) containing an active agent. By "active agent" is meant a drug, agent, pharmaceutical, therapeutic, dietary supplement, pesticide, fertilizer, agricultural chemical, herbicide, nutrient, or other compound that may be desired to be formulated as an SD. An active agent may be a "small molecule" having a molecular weight of approximately 2000 Daltons or less. In some embodiments, SDs made by some of the disclosed processes contain two or more active agents.
[0059] Embodiments of the disclosed process are particularly suitable for acidic active agents having a crystalline or free acid form with a pKa of less than or equal to 7. In some embodiments, the free acid form of the active agent has a pKa in the range of 3-7.
[0060] The active agent may be a crystalline drug having a solubility of the free acid form of 40 mg / mL or less in one or more C1-C3 alkanols at ambient temperature (e.g., 20-25° C.). The term "crystalline" refers to a solid material in which atoms or molecules are arranged in a well-defined pattern that is regularly repeated in three dimensions. In some embodiments, the active agent has a solubility of the free acid form of 30 mg / mL or less, 20 mg / mL or less, 10 mg / mL or less, 5 mg / mL or less, 2.5 mg / mL or less, or 1 mg / mL or less in one or more C1-C5 alkanols at ambient temperature. In some embodiments, the active agent has a solubility of the free acid form in one or more C1-C3 alkanols at ambient temperature (e.g., a temperature of 20-25° C.) within the range of 0.0001-40 mg / mL, 0.001-40 mg / mL, 0.001-30 mg / mL, 0.001-20 mg / mL, 0.001-10 mg / mL, 0.01-10 mg / mL, 0.1-10 mg / mL, 0.01-5 mg / mL, 0.01-2.5 mg / mL, or 0.01-1 mg / mL.
[0061] V. Dispersion Polymers Embodiments of the disclosed processes are used to form an SD that includes a dispersion polymer. In some embodiments, the SD includes multiple dispersion polymers. Dispersion polymers suitable for use in SDs formed by the disclosed methods should be inert, in the sense that they do not chemically react with the active agent in an adverse manner.
[0062] Suitable dispersion polymers include, but are not limited to, hydroxypropyl methylcellulose acetate succinate (HPMCAS), hydroxypropyl methylcellulose phthalate (HPMCP), hydroxypropyl methylcellulose (HPMC), hydroxypropyl cellulose (HPC), cellulose acetate phthalate (CAP), carboxymethylethylcellulose (CMEC), polyvinylpyrrolidone (PVP), poly(vinylpyrrolidone-co-vinyl acetate) (PVP-VA), poly(methacrylic acid-co-methyl methacrylate) (PMMAMA), poly(methacrylic acid-co-ethyl acrylate), or any combination thereof. Suitable PMMAMA polymers include, but are not limited to, poly(methacrylic acid-co-methyl methacrylate) 1:1 (Eudragit® L100 polymer, Evonik Industries AG), and poly(methacrylic acid-co-methyl methacrylate) 1:2 (Eudragit® S100 polymer). In some embodiments, the poly(methacrylic acid-co-ethyl acrylate) is poly(methacrylic acid-co-ethyl acrylate) 1:1. The above list is not intended to indicate that all embodiments are equally and / or equally suitable. In some embodiments, the dispersion polymer comprises HPMCAS or PVP-VA.
[0063] VI. Excipients In some embodiments, the SD further comprises one or more excipients in addition to the active agent and the dispersion polymer. Suitable excipients include, but are not limited to, binders, fillers, diluents, disintegrants, lubricants, surfactants, coating agents, colorants, flavorings, and combinations thereof.
[0064] Exemplary surfactants include fatty acids, alkyl sulfonates, and commercially available surfactants, such as those sold under trade names, such as benzethonium chloride (Hyamine® 1622, available from Lonza, Inc., Fairlawn, NJ), docusate sodium (available from Mallinckrodt Spec. Chem., St. Louis, MO), and polyoxyethylene sorbitan fatty acid esters (Tween® surfactants, available from ICI Americas Inc., Wilmington, DE; Liposorb® P-20, available from Lipochem Inc., Patterson, NJ; and Abitec Examples of binders include Capmul® POE-0 available from Sigma-Aldrich Corp., Janesville, WI), sorbitan esters (e.g., Span® 20 (sorbitan monolaurate), 40 (sorbitan monopalmitate), 60 (sorbitan monostearate), 65 (sorbitan tristearate), 80 (sorbitan monooleate), and 85 (sorbitan trioleate) nonionic surfactants available from Sigma-Aldrich, St. Louis, MO), and natural surfactants such as sodium taurocholate, 1-palmitoyl-2-oleoyl-sn-glycero-3-phosphocholine, lecithin, other phospholipids, and mono- and diglycerides. Examples of binders include methylcellulose, microcrystalline cellulose, starch, and gums such as guar gum, and tragacanth. Examples of lubricants include talc, colloidal silica, magnesium stearate and calcium stearate. Examples of disintegrants include sodium starch glycolate, sodium alginate, sodium carboxymethylcellulose, methylcellulose, and croscarmellose sodium.Examples of other matrix materials, fillers, or diluents include lactose, mannitol, xylitol, microcrystalline cellulose, calcium diphosphate, calcium silicate, hydrated aluminum silicate, bentonite, hectorite, montmorillonite, magnesium trisilicate, magnesium oxide, and starch.
[0065] VII. Atomized Solid Dispersions The atomized solid dispersions made by the disclosed method embodiments include an active agent, a dispersion polymer, and 500 ppm or less of ammonia. In some embodiments, the SD includes 400 ppm or less, 300 ppm or less, 200 ppm or less, 100 ppm or less, or 50 ppm or less of ammonia.
[0066] In some embodiments, the active agent is an acid agent having a pKa of 7 or less and a solubility of the free acid form of 10 mg / mL or less in methanol, ethanol, n-propanol, isopropanol, or any combination thereof. In some embodiments, the SD comprises at least 0.5% active agent by weight, e.g., at least 1%, at least 5%, at least 10%, at least 25%, or at least 50% active agent by weight. In some embodiments, the SD comprises 0.5-95% active agent by weight, e.g., 1-95%, 5-95%, 10-95%, or 25-95% active agent by weight.
[0067] In some embodiments, at least 90% by weight of the active agent in the SD is in the free acid form. In some embodiments, at least 95%, at least 97%, at least 98%, or at least 99% by weight of the active agent is in its free acid form. For example, 90-100%, 95-100%, 97-100%, 98-100%, or 99-100% by weight of the active agent can be in the free acid form in the sprayed dispersion.
[0068] The SD further comprises a dispersion polymer. In some embodiments, the dispersion polymer comprises hydroxypropyl methylcellulose acetate succinate (HPMCAS), hydroxypropyl methylcellulose phthalate (HPMCP), hydroxypropyl methylcellulose (HPMC), hydroxypropyl cellulose (HPC), cellulose acetate phthalate (CAP), carboxymethyl ethyl cellulose (CMEC), polyvinylpyrrolidone (PVP), poly(vinylpyrrolidone-co-vinyl acetate) (PVP-VA), poly(methacrylic acid-co-methyl methacrylate) 1:1, poly(methacrylic acid-co-methyl methacrylate) 1:2, poly(methacrylic acid-co-ethyl acrylate) 1:1, or any combination thereof. In some embodiments, the SD comprises two or more dispersion polymers. The SD may further comprise one or more excipients.
[0069] In some embodiments, the SD comprises, consists essentially of, or consists of an active agent, a dispersion polymer, 500 ppm or less ammonia, and a trace amount (50 ppm or less) of a solvent. By "consists essentially" it is meant that the SD does not contain any components that would substantially affect the properties of the SD. Thus, the SD does not contain, for example, any polymer other than the dispersion polymer, or any active agent with a pKa greater than 7. However, the SD may contain trace amounts (e.g., less than 500 ppm) of other components that do not substantially affect the properties of the SD, such as small amounts of impurities present in the materials used to make the SD. In some embodiments, the SD comprises, consists essentially of, or consists of an active agent, a dispersion polymer, 50 ppm or less ammonia, and 5 ppm or less of a solvent. In some embodiments, the SD comprises, consists essentially of, or consists of an active agent, a dispersion polymer, one or more excipients, 500 ppm or less ammonia, and a trace amount (50 ppm or less) of a solvent. In another independent embodiment, the SD comprises, consists essentially of, or consists of an active agent, a dispersion polymer, one or more excipients, 50 ppm or less ammonia, and 5 ppm or less solvent.
[0070] The active agent in the SD can be crystalline, amorphous, or any state in between. In some embodiments, the active agent in the SD is amorphous or substantially (i.e., at least 90% by weight) amorphous. In one embodiment, the active agent is molecularly dispersed throughout the SD. In a separate embodiment, the SD is a spray-dried dispersion comprising a plurality of particles, at least a portion of the particles comprising an active agent domain. The active agent domain may comprise an amorphous active agent, a crystalline active agent, or a combination of amorphous and crystalline active agents. In some embodiments, at least 90% by weight, e.g., 90-100%, 90-99.9%, or 90-99.5% by weight, of the active agent in the active agent domain is amorphous.
[0071] In some embodiments, SDs prepared by the disclosed methods have advantages over SDs prepared by other methods, such as SDs containing a salt of the active agent prepared with a non-volatile counterion, e.g., Na+ or K+, or SDs prepared by spraying the free acid form of the active agent. For example, SD embodiments disclosed herein can have higher potency and / or higher physical stability (e.g., reduced hygroscopicity) compared to SDs containing a salt of the active agent. In some embodiments, SD embodiments contain a higher percentage of the active agent compared to SDs prepared from the free acid form of the active agent, where solubility constraints limit the concentration of the active agent in the spray solution and subsequent solid dispersion.
[0072] VII. Representative Embodiments Some representative embodiments are described in the following paragraphs.
[0073] 1. A method for preparing a sprayed solid dispersion comprising: mixing an active agent, a dispersion polymer, an amount of ammonia, and a solvent to form a spray solution, wherein the solvent comprises a C1-C3 alkanol, wherein the active agent in free acid form has a pKa of 7 or less and a solubility of 40 mg / mL or less in the solvent, and wherein the amount of ammonia is sufficient to dissolve the active agent in the solvent; spraying the spray solution to form a sprayed solid dispersion comprising the active agent, the dispersion polymer, and ammonia; and removing residual ammonia from the sprayed solid dispersion to form a product comprising a solid dispersion of the active agent and the dispersion polymer, wherein the product comprises 500 ppm or less of ammonia.
[0074] The method of the preceding paragraph, wherein the amount of ammonia is at least 0.95 molar equivalents relative to the total acid groups of the activator equivalents relative to the total acid groups of the activator.
[0075] The method of paragraph 1, wherein the amount of ammonia is at least 0.95 molar equivalents relative to the total acid groups of the activator and all acid groups of the dispersion polymer.
[0076] The method according to the preceding paragraph, wherein the amount of ammonia is 0.95 to 4 molar equivalents relative to the total acid groups of the activator and all acid groups of the dispersion polymer.
[0077] The method of paragraph 1, wherein the amount of ammonia is at least 0.95 molar equivalents relative to the amount of acid groups on the active agent that exceeds the solubility of the free acid form of the active agent in the solvent and the total of all acid groups on the dispersion polymer.
[0078] The method of any one of the preceding paragraphs, wherein at least 90% by weight of the active agent in the product is in the free acid form.
[0079] The method of any one of the preceding paragraphs, wherein the C1 to C3 alkanol comprises methanol, ethanol, n-propanol, isopropanol, or any combination thereof.
[0080] The method of any one of the preceding paragraphs, wherein the solvent comprises a C1-C3 alkanol and a co-solvent.
[0081] The method of the preceding paragraph, wherein the co-solvent comprises water, tetrahydrofuran, ethyl acetate, methyl acetate, 1,3-dioxolane, acetone, methyl ethyl ketone, or any combination thereof.
[0082] The method of any one of the preceding paragraphs, wherein the solvent comprises 0.01 to 30% by weight water, the remainder being a C1 to C3 alkanol.
[0083] The method of any one of the preceding paragraphs, wherein the active agent has a solubility in the spray solution that is at least two times greater than the solubility of the free acid form of the active agent in the ammonia-free solvent.
[0084] The method of any one of the preceding paragraphs, wherein the spray solution has a dissolved solids content in the range of 2 to 40% by weight, with 0.5 to 95% by weight of the dissolved solids being active agent.
[0085] The method of any one of the preceding paragraphs, wherein the spray solution comprises 0.5 to 20% by weight of an active agent.
[0086] The method of any one of the preceding paragraphs, wherein removing the residual ammonia comprises heating the atomized solid dispersion at a temperature in the range of 30-70° C. and a relative humidity (RH) in the range of 10-75% for a time sufficient to form a product containing 500 ppm or less of ammonia.
[0087] The method according to the preceding paragraph, wherein (i) the time is from 2 to 60 hours, or (ii) the temperature is in the range of 40 to 60° C., or (iii) the RH is in the range of 15 to 50%, or (iv) any combination of (i), (ii), and (iii).
[0088] The method of any one of the preceding paragraphs, wherein removing residual ammonia further comprises blowing a sweep gas over the atomized solid dispersion while heating the atomized solid dispersion at temperature and RH.
[0089] The method of the preceding paragraph, wherein the sweep gas comprises nitrogen, argon, carbon dioxide, air, or any combination thereof.
[0090] The method of the preceding paragraph, wherein the sweep gas further comprises water vapor or a volatile organic solvent vapor.
[0091] The method of the preceding paragraph, wherein the sweep gas further comprises a volatile organic solvent vapor, and the volatile organic solvent is methanol.
[0092] The method of any one of the preceding paragraphs, wherein the removal of residual ammonia is carried out in a tray dryer or a mechanically agitated drying chamber.
[0093] The method of any one of the preceding paragraphs, wherein at least a portion of the residual solvent is removed simultaneously with removing residual ammonia from the atomized solid dispersion.
[0094] The dispersed polymer has a dry glass transition temperature T above 60°C as measured by differential scanning calorimetry. g The method of any one of the preceding paragraphs, comprising:
[0095] The method of any one of the preceding paragraphs, wherein the dispersion polymer comprises hydroxypropyl methylcellulose acetate succinate (HPMCAS), hydroxypropyl methylcellulose phthalate (HPMCP), hydroxypropyl methylcellulose (HPMC), hydroxypropyl cellulose (HPC), cellulose acetate phthalate (CAP), carboxymethyl ethyl cellulose (CMEC), polyvinylpyrrolidone (PVP), poly(vinylpyrrolidone-co-vinyl acetate) (PVP-VA), poly(methacrylic acid-co-methyl methacrylate), poly(methacrylic acid-co-ethyl acrylate), or any combination thereof.
[0096] The method of any one of the preceding paragraphs, wherein the spray solution comprises a plurality of dispersed polymers.
[0097] The method of any one of the preceding paragraphs, wherein the spray solution further comprises one or more excipients.
[0098] The method of the preceding paragraph, wherein the one or more excipients include one or more binders, fillers, diluents, disintegrants, lubricants, surfactants, coating agents, colorants, flavoring agents, or any combination thereof.
[0099] The method of any one of the preceding paragraphs, wherein the amount of ammonia is at least 0.95 molar equivalents relative to the total of the acid groups of the active agent, all of the acid groups of the dispersion polymer, and all of the acid groups of the one or more excipients.
[0100] The method of the preceding paragraph, wherein the amount of ammonia is 0.95 to 4 molar equivalents relative to the total of the acid groups of the active agent, all of the acid groups of the dispersion polymer, and all of the acid groups of the one or more excipients.
[0101] The sprayed solid dispersion prepared by the method of any one of the preceding paragraphs, wherein the sprayed solid dispersion comprises at least 0.5% by weight of an active agent and no more than 500 ppm ammonia.
[0102] The sprayed solid dispersion of the preceding paragraph, wherein at least 90% by weight of the active agent in the sprayed solid dispersion is in the free acid form.
[0103] 2. The sprayed solid dispersion of any one of the preceding paragraphs, comprising: 0.5-95% by weight of the active agent, wherein at least 90% by weight of the active agent is amorphous; a dispersion polymer; and up to 50 ppm of ammonia.
[0104] The method of any one of the preceding paragraphs, wherein the product contains 300 ppm or less ammonia, 100 ppm or less ammonia, or 50 ppm or less ammonia. EXAMPLES
[0105] VIII. Examples Characterization methods GC Analysis: Headspace gas chromatography (GC) was used to quantify the amount of residual methanol present in the test samples. GC samples were removed from the tray dryer at regular time intervals and samples of known mass, 10-60 mg, were sealed in 20 mL headspace vials. Samples were dissolved in 4 mL of N-N-dimethylacetamide injected through a PTFE / silicone septum. An Agilent® G7890GC (Agilent Technologies, Santa Clara, CA) equipped with an automatic headspace sampler was used with a DB-624 column (30 m x 0.32 mm ID x 1.8 μm) and a flame ionization detector. Residual solvents present in the samples are quantified using a six-point calibration curve of headspace samples with known solvent content.
[0106] PXRD: Powder X-ray diffraction (PXRD) was performed on a Rigaku® Miniflex® 600 X-ray diffractometer (Rigaku Corporation, Tokyo, Japan) equipped with a D / tex fast linear detector operating in theta / 2theta mode. Samples were spread on a 0.5 mm zero background holder. Analysis was performed with 600 W (40 kV and 15 mA) of Cu K-Falfa radiation, 1.25° dispersion slits on both incident and diffracted beams, 8.0 mm scattering slits, 5° Soller slits, and 15 micron Ni foil to eliminate the Cu K-beta diffracted beam. Samples were scanned at 2.5° / min from 3° to 40° 2θ in steps of 0.02° 2θ.
[0107] Ammonia quantification - ion selective electrode (ISE) method: Ammonia quantification of SDD samples was performed using an ammonia ion selective electrode, Orion® 9512HPBNWP (ThermoFisher Scientific), and a Beckman Coulter model PHI410 meter. The ISE was calibrated using an ammonium sulfate primary standard from Spectrum Chemical. Aqueous solutions of known ammonia concentrations in 0.1 M sodium hydroxide were measured in millivolts and used to generate a linear standard curve. A known mass of SDD sample was dissolved in 0.1 molar sodium hydroxide and analyzed using the ISE. Millivolt measurements were recorded and converted to concentration. Ammonia concentrations in SDD are reported as parts per million (ppm).
[0108] Example 1 Enhancement of sulfasalazine concentration in methanol containing ammonia A saturated solution of sulfasalazine (Spectrum Chemical) was prepared in methanol containing an excess of crystalline sulfasalazine. After centrifugation, analysis of the supernatant by thermogravimetry gave a crystalline solubility of approximately 1.0 mg / mL in methanol.
[0109] A second mixture of sulfasalazine in methanol was prepared by stirring 656.0 mg of sulfasalazine (1.65 mmol) in 14.00 mL of methanol. To this slurry, 0.825 mL (1.76 mmol) of a 2.14 M solution of ammonia in methanol was added with stirring, completely dissolving the sulfasalazine within 1 minute. The sulfasalazine concentration is greater than 43 mg / mL in methanol. The observed solubility enhancement of sulfasalazine in methanol in the presence of ammonia was approximately 43-fold.
[0110] Example 2 Enhancement of piroxicam concentration in methanol containing ammonia A saturated solution of piroxicam (Spectrum Chemical) was prepared in methanol containing an excess of crystalline piroxicam. After centrifugation, analysis of the supernatant by thermogravimetry gave a crystalline solubility of approximately 2.1 mg / mL in methanol.
[0111] A second mixture of piroxicam in methanol was prepared by stirring 661.8 mg of piroxicam (2.00 mmol) in 15.00 mL of methanol. To this slurry, 1.0 mL (2.14 mmol) of a 2.14 M solution of ammonia in methanol was added with stirring, and within 1 minute a clear yellow solution was obtained. The piroxicam concentration was greater than 41 mg / mL in methanol. The observed solubility enhancement of piroxicam in methanol in the presence of ammonia was greater than 19-fold.
[0112] Example 3 Piroxicam / PVP-VA65SDD with ammonia as processing aid A spray solution was prepared by dissolving 16.02 grams of Kollidon® VA-64 vinylpyrrolidone-vinyl acetate copolymer (BASF Corp.) in 475.07 grams of methanol. To 4.00 grams of this solution, 12.07 millimoles of piroxicam were added to obtain a suspension of piroxicam. To this suspension, 6.00 mL of a 2.14 M (12.84 millimoles) solution of ammonia in methanol (Aldrich Chemical) was added with stirring to obtain a clear yellow solution.
[0113] The solution was pumped into a laboratory-scale spray-drying chamber using a head pressure of 150 psi at the solution pot. The solution flow rate was estimated to be 30 g / min. The drug / polymer solution was atomized through a Schlick model 121 size 2.0 pressure swirl nozzle. Heated nitrogen gas was introduced into the 0.3 m diameter stainless steel chamber at a temperature of 139 °C and a flow rate of 500 g / min. The outlet temperature of the gas leaving the chamber was 45 °C. The solid dispersion was collected using a cyclone to separate the solid particles from the gas stream and stored in a sealed container at 2-8 °C.
[0114] Example 4 Piroxicam / HPMCAS SDD with ammonia as a processing aid A spray solution was prepared by dissolving 16.00 g of HPMCAS-M (Shin-Etsu AQOAT®) in 468.01 g of methanol. To 4.00 g of this solution, 12.07 mmol of piroxicam was added to obtain a suspension of the active agent. To this suspension, 14.82 mL of a 2.14 M (31.71 mmol) solution of ammonia in methanol (Aldrich Chemical) was added with stirring to obtain a slightly hazy yellow solution. This amount of ammonia was used to neutralize both the active agent and the polymer.
[0115] The solution was pumped into a laboratory-scale spray-drying chamber using a head pressure of 150 psi at the solution pot. The solution flow rate was estimated to be 30 g / min. The drug / polymer solution was atomized through a Schlick model 121 size 2.0 pressure swirl nozzle. Heated nitrogen gas was introduced into the 0.3 m diameter stainless steel chamber at a temperature of 139 °C and a flow rate of 500 g / min. The outlet temperature of the gas leaving the chamber was 45 °C. The solid dispersion was collected using a cyclone to separate the solid particles from the gas stream and stored in a sealed container at 2-8 °C.
[0116] Examples 5 to 10 Ammonia Removal Ammonia was removed from the spray-dried dispersions using an ES2000 environmental chamber from Environmental Specialties, Inc. at three different conditions. A constant temperature and relative humidity (RH) of the drying chamber was maintained for the three conditions tested: 40° C. and 15% RH, 50° C. and 30% RH, and 60° C. and 30% RH.
[0117] For each set of conditions, samples of the spray-dried dispersion were removed from the environmental chamber at time intervals of 0, 4, 8, 24, and 48 hours. The samples were stored in sealed vials for residual ammonia analysis using an ion-selective electrode as described above. The results are shown in Table 1. [Table 1]
[0118] Figure 1 is the PXRD spectrum of SDD from Example 7 after 48 hours at 50° C. and 30% RH. Figure 2 is the PXRD spectrum of SDD from Example 8 after 48 hours at 50° C. and 30% RH. The lack of sharp peaks in the spectrum indicates that the sample is amorphous.
[0119] Example 11 Solvent removal To demonstrate the large difference in time and conditions required to remove the solvent and ammonia from the SD, a second set of piroxicam SDDs containing either HPMCAS or PVPVA-64 polymer was prepared using the same procedure and amounts as in Examples 3 and 4. The wet SDDs were immediately transferred to an ES2000 environmental chamber set at 40°C / 15% RH. GC samples were taken at 0, 0.5, 1, 2, and 4 hours. The initial solvent content of the SDDs was approximately 1-2 wt% methanol. No methanol was detected in the samples at all time points above 0.5 hours. This indicates that methanol was removed well below the ICH (International Council for Harmonisation of Technical Requirements for Pharmaceuticals for Human Use) specification of 0.3 wt% within 30 minutes at these drying conditions.
[0120] Although the same equipment was used to remove residual solvent and residual ammonia from SDD, it is clear that there are significant differences in the conditions and processing times required to achieve acceptably low levels for each. For example, methanol removal from SDD prepared by the methods of Examples 3 and 4 was monitored, and in both cases, residual methanol was well below the ICH specification of 0.3 wt% after only 30 minutes in the dryer at 40°C / 15% RH. At these conditions, ammonia removal to the target of less than 500 ppm ammonia is more than 8 times slower than the time required to remove methanol from HPMCAS SDD (Table 1, Example 6). For PVP-VA 64 SDD, both longer times than 24 hours and higher temperature / humidity (50°C / 30% RH) conditions are required (Table 1, Example 7). This is more than 48 times slower than methanol removal at 40°C / 15% RH. To reach the more preferred target of less than 100 ppm ammonia in the SDD, the time required for the HPMCAS SDD approaches 24 hours at 40° C. / 15% RH (Table 1, Example 6), which is 48 times longer than methanol removal. For the PVP-VA SDD, much more than 48 hours of treatment is required to reach less than 100 ppm ammonia using 50° C. / 30% RH conditions (Table 1, Example 7), which is 98 times longer than methanol removal. To achieve a 24 hour treatment time for the PVP-VA SDD, the treatment conditions must be increased to 60° C. / 30% RH (Table 1, Example 9), which is much higher than the conditions required for methanol removal.
[0121] In view of the many possible embodiments to which the principles of the disclosed invention may be applied, it should be recognized that the illustrated embodiments are merely preferred examples of the invention and should not be construed as limiting the scope of the invention. Rather, the scope of the invention is defined by the following claims. We therefore claim as our invention all that comes within the scope and spirit of these claims.
Claims
1. 1. A method for preparing a nebulized solid dispersion comprising the steps of: mixing an active agent, a dispersion polymer, an amount of ammonia, and a solvent to form a spray solution; The solvent is C 1 ~C 3 Contains alkanols, the active agent in its free acid form has a pKa of 7 or less and a solubility of 40 mg / mL or less in the solvent; the amount of ammonia is sufficient to dissolve the activator in the solvent; Mixing and spraying the spray solution to form an atomized solid dispersion comprising the active agent, the dispersion polymer, and ammonia; removing residual ammonia from the atomized solid dispersion by heating the atomized solid dispersion at a temperature in the range of 30-70° C. and a relative humidity (RH) in the range of 10-75% for a time sufficient to form a product comprising a solid dispersion of the active agent and the dispersion polymer, the product containing 500 ppm or less of ammonia; A method comprising:
2. The amount of ammonia is at least 0.95 molar equivalents relative to the total acid groups of the activator; or at least 0.95 molar equivalents relative to the total acid groups of the active agent and all acid groups of the dispersion polymer; or 0.95 to 10 molar equivalents relative to the total acid groups of the activator and all acid groups of the dispersion polymer; or an amount of acid groups of the active agent that exceeds the solubility of the free acid form of the active agent in the solvent and is at least 0.95 molar equivalents relative to the total of all acid groups of the dispersion polymer; The method of claim 1.
3. 3. The method of claim 1 or 2, wherein at least 90% by weight of the active agent in the product is in the free acid form.
4. The solvent is C 1 ~C 3 The process of any one of claims 1 to 3, comprising an alkanol and a co-solvent.
5. The method of claim 4, wherein the co-solvent comprises water, tetrahydrofuran, ethyl acetate, methyl acetate, 1,3-dioxolane, acetone, methyl ethyl ketone, or any combination thereof.
6. The solvent contains 0.01 to 30% by weight of water, and the remainder is the C 1 ~C 3 The method according to claim 4 or 5, wherein the solvent is an alkanol.
7. 7. The method of any one of claims 1 to 6, wherein the activator has a solubility in the spray solution that is at least two times higher than the solubility of the free acid form of the activator in the ammonia-free solvent.
8. 8. The method of any one of claims 1 to 7, wherein the spray solution has a dissolved solids content in the range of 2 to 40% by weight, and 0.5 to 95% by weight of the dissolved solids is the active agent.
9. The method according to any one of claims 1 to 8, wherein the spray solution comprises 0.5 to 20% by weight of the active agent.
10. A method for preparing an atomized solid dispersion comprising the steps of: mixing an active agent, a dispersion polymer, an amount of ammonia, and a solvent to form a spray solution; the solvent comprises a C1-C3 alkanol; the active agent in its free acid form has a pKa of 7 or less and a solubility of 40 mg / mL or less in the solvent; the amount of ammonia is sufficient to dissolve the activator in the solvent; Mixing and spraying the spray solution to form an atomized solid dispersion comprising the active agent, the dispersion polymer, and ammonia; Including, The method of claim 1, wherein removing residual ammonia comprises heating the atomized solid dispersion at a temperature in the range of 30-70° C. and a relative humidity (RH) in the range of 10-75% for a time sufficient to form the product containing 500 ppm or less of ammonia, wherein the time is from 2 to 60 hours.
11. (i) the time period is between 4 and 48 hours; or (ii) the temperature is in the range of 40 to 60° C.; or (iii) RH is in the range of 15-50%, or (iv) any combination of (i), (ii), and (iii); The method according to claim 1 or 10.
12. 12. The method of claim 1 or 11, wherein removing residual ammonia further comprises blowing a sweep gas over the atomized solid dispersion while heating the atomized solid dispersion at the temperature and RH.
13. The method of claim 12 , wherein the sweep gas comprises nitrogen, argon, carbon dioxide, air, or any combination thereof.
14. 14. The method according to claim 13, wherein the sweep gas further comprises water vapor or a volatile organic solvent vapor. Method of posting.
15. 15. The method of any one of claims 1 to 14, wherein at least a portion of the residual solvent is removed simultaneously with removing residual ammonia from the atomized solid dispersion.
16. The dispersed polymer has a dry glass transition temperature T of greater than 60° C. as measured by differential scanning calorimetry. g The method according to any one of claims 1 to 15, comprising:
17. 17. The method of any one of claims 1 to 16, wherein the dispersion polymer comprises hydroxypropyl methylcellulose acetate succinate (HPMCAS), hydroxypropyl methylcellulose phthalate (HPMCP), hydroxypropyl methylcellulose (HPMC), hydroxypropyl cellulose (HPC), cellulose acetate phthalate (CAP), carboxymethyl ethyl cellulose (CMEC), polyvinylpyrrolidone (PVP), poly(vinylpyrrolidone-co-vinyl acetate) (PVP-VA), poly(methacrylic acid-co-methyl methacrylate), poly(methacrylic acid-co-ethyl acrylate), or any combination thereof.
18. The method of any one of claims 1 to 17, wherein the spray solution further comprises one or more excipients.
19. 20. The method of claim 18, wherein the amount of ammonia is at least 0.95 molar equivalents relative to the total of the acid groups of the active agent, all of the acid groups of the dispersion polymer, and all of the acid groups of the one or more excipients.
Citation Information
Patent Citations
Spray desiccant formulation
JP2008100997A
Pharmaceutical composition comprising amorphous selexipag
WO2018078383A1