Magnetic nanowire memory

The magnetic thin wire memory achieves high-density magnetic domain formation with reduced power consumption by incorporating recessed and convex portions to lower coercive force and current magnetic field requirements.

JP7594975B2Active Publication Date: 2024-12-05NIPPON HOSO KYOKAI
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2021086273
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-05-21
Publication Date
2024-12-05
Estimated Expiration
2041-05-21

AI Technical Summary

Technical Problem

Conventional magnetic thin wire memories face challenges in forming magnetic domains at high density due to the difficulty in reducing the coercive force and current magnetic field required for magnetization reversal.

Method used

The magnetic thin wire memory incorporates recessed and convex portions in the magnetic thin wire structure, which reduces the coercive force and current magnetic field needed for magnetization reversal, allowing for higher density magnetic domain formation.

Benefits of technology

The proposed structure enables the formation of stable-shaped magnetic domains at higher densities with reduced power consumption by minimizing the current required for magnetization reversal.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007594975000001
    Figure 0007594975000001
  • Figure 0007594975000002
    Figure 0007594975000002
  • Figure 0007594975000003
    Figure 0007594975000003
Patent Text Reader

Abstract

To provide a magnetic wire memory capable of forming a magnetic domain in a magnetic wire at high density.SOLUTION: A magnetic wire memory 1 includes at least one magnetic wire 2 made of a thin magnetic material, and a recording element 4 made of a conductor through which a recording current flows and arranged so as to intersect the magnetic wire 2 with an interlayer insulating film 3 interposed in the film thickness direction of the magnetic wire 2, the magnetic wire 2 has a concave portion 6 locally formed with a film thickness smaller than that in other regions in the longitudinal direction of the magnetic wire 2, and the concave portion 6 is arranged in a region 21 of a first predetermined length located adjacent to the recording element 4.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a magnetic nanowire memory, and more particularly to a magnetic nanowire memory that records information by locally reversing magnetization. [Background technology]

[0002] Research is being conducted into magnetic nanowire memory as a magnetic recording device that can record and reproduce binary information at high speed on a medium made of magnetic material formed into a nanowire shape. Magnetic nanowire memory has a nanowire-shaped conductor (hereafter referred to as the recording element) arranged orthogonally above the magnetic nanowire, and records information by locally reversing the magnetization in the magnetic nanowire using the current magnetic field generated by applying a current to the recording element. By arranging and stacking such magnetic nanowire memories in parallel, ultra-high speed operation by parallel synchronous control is possible, and high operational reliability can be ensured because the operating principle does not require any mechanical moving parts.

[0003] The racetrack memory described in Non-Patent Document 1 is a memory with a U-shaped three-dimensional structure in which a magnetic nanowire is stretched perpendicular to a substrate. In the racetrack memory, a recording head arranged perpendicular to the magnetic nanowire forms magnetic domains in the magnetic nanowire, and a pulse current is applied to the magnetic nanowire to move the position of the magnetic domains to record and store data. A magnetic field generated by applying a current to the recording head forms magnetic domains in the magnetic nanowire, and data is recorded. In addition, in order to enable random access, the racetrack memory applies a pulse current to the magnetic nanowire during playback to move the magnetic domain so that the magnetic domain is located directly under the playback head arranged on the magnetic nanowire.

[0004] Non-Patent Document 2 describes a Hall bar type domain wall motion device in which two Ti / Au electrodes (one for recording and one for reproducing) are provided perpendicularly on a magnetic nanowire in which Co / Ni is laminated as a material exhibiting perpendicular magnetization, with a gap of 12 μm between them. The area between the two electrodes is a storage area for data recorded in the magnetic nanowire. One electrode functions as a recording head, and the other electrode functions as a reproducing head. In this device, a magnetic domain is recorded in the magnetic nanowire by using a current magnetic field generated by passing a current through one electrode (recording head). Then, a current pulse is passed through the magnetic nanowire in which the magnetic domain is recorded, via the electrodes, to move the magnetic domain within the magnetic nanowire. Non-Patent Document 2 discloses that the magnetic domain length (distance between magnetic domain walls) shifted by the current pulse is 5.1±0.9 μm or 3.2±0.6 μm. [Prior art documents] [Non-patent literature]

[0005] [Non-Patent Document 1] Parkin Stuart SP et al., “Magnetic Domain-Wall Racetrack Memory”, Science, 11 Apr 2008, Vol. 320, Issue 5873, pp. 190-194 [Non-Patent Document 2] Chiba D., et al., “Control of Multiple Magnetic Domain Walls by Current in a Co / Ni Nano-Wire”, Applied Physics Express, June 2010, 073004 Summary of the Invention [Problem to be solved by the invention]

[0006] However, in conventional devices, it was difficult to form magnetic domains equivalent to recording bits at high density in a magnetic nanowire.

[0007] The present invention has been made in consideration of the above problems, and an object of the present invention is to provide a magnetic nano-wire memory capable of forming magnetic domains in a magnetic nano-wire at a high density. [Means for solving the problem]

[0008] In order to solve the above problems, a magnetic nanowire memory according to a first aspect of the present invention comprises at least one magnetic nanowire made of a thin-film magnetic material, and a recording element made of a conductor for passing a recording current and arranged so as to cross the magnetic nanowire via an interlayer insulating film in the film thickness direction of the magnetic nanowire, the magnetic nanowire having a recess formed so that the film thickness is locally smaller in the longitudinal direction of the magnetic nanowire than in other regions, the recess being arranged in a region within a first predetermined length located adjacent to the recording element. the recess is formed across the width direction perpendicular to the longitudinal direction of the magnetic nanowire, the recording element is disposed adjacent to one upper edge of the recess on the upstream side, the magnetic nanowire further includes a protrusion protruding in the film thickness direction of the magnetic nanowire, the protrusion being made of a magnetic material and disposed in a region located downstream adjacent to the other upper edge of the recess in the longitudinal direction of the magnetic nanowire. It was decided that there would be

[0010] In addition, the present invention 2 The magnetic nanowire memory according to the above aspect includes at least one magnetic nanowire made of a thin-film magnetic material, and two recording elements made of a conductor for passing a recording current and arranged at a first predetermined length apart so as to cross the magnetic nanowire in the film thickness direction of the magnetic nanowire via an interlayer insulating film, the magnetic nanowire includes a recess formed in a region in the longitudinal direction of the magnetic nanowire that is locally thinner than the film thickness in other regions, and the recess is arranged in a region within the first predetermined length between one recording element and the other recording element. the recess is formed across the width direction perpendicular to the longitudinal direction of the magnetic thin wire, one recording element is disposed upstream adjacent to one upper edge of the recess, and the other recording element is disposed downstream adjacent to the other upper edge of the recess, the magnetic thin wire further includes a protrusion protruding in the film thickness direction of the magnetic thin wire, the protrusion being made of a magnetic material and disposed in a region located downstream adjacent to the other upper edge of the recess in the longitudinal direction of the magnetic thin wire. It was decided that there would be Effect of the Invention

[0012] The present invention provides the following excellent effects. The magnetic nanowire memories according to the first and third aspects of the present invention include a recess, which reduces the local magnetization and coercivity of the magnetic nanowire medium. This reduces the magnitude of the current magnetic field required for magnetization reversal, and therefore reduces the current value to be applied to the recording element, thereby realizing power saving. As a result, by reducing the recording current, magnetic domains can be formed in the magnetic nanowire at a higher density than before when compared with the same recording current. The magnetic nanowire memories according to the second and fourth aspects of the present invention include a convex portion, and therefore, even if the magnetic domain length is made shorter than in the past, the magnetic domains can be formed. As a result, the magnetic domains can be formed at high density in the magnetic nanowire by increasing the linear recording density. The magnetic nanowire memories according to the third and fourth aspects of the present invention include two recording elements, and therefore magnetic domains with stable shapes can be formed at high density in the magnetic nanowire. [Brief description of the drawings]

[0013] [Figure 1] 1 is a perspective view showing a schematic diagram of a magnetic nanowire memory according to a first embodiment of the present invention. [Diagram 2] FIG. 1 is a perspective view showing a typical example of a conventional magnetic nanowire memory. [Diagram 3] 1A to 1C are cross-sectional views illustrating a first manufacturing method of a magnetic nanowire memory. [Figure 4] 11A to 11C are cross-sectional views illustrating a second manufacturing method of the magnetic nanowire memory. [Diagram 5] 13A to 13C are cross-sectional views (part 1) that diagrammatically show a third manufacturing method of a magnetic nanowire memory. [Figure 6] 13 is a cross-sectional view (part 2) that diagrammatically illustrates the third manufacturing method of the magnetic nanowire memory. [Figure 7] 1A and 1B are schematic diagrams of a magnetic nanowire memory according to a first embodiment of the present invention, in which (a) is a plan view and (b) is a side view. [Figure 8] 4A and 4B are examples of current pulse waveforms applied to a recording element. [Figure 9] FIG. 8 is a diagram showing a simulation result of the magnetic nanowire memory of FIG. [Figure 10] 5A and 5B are schematic diagrams of a magnetic nanowire memory according to a second embodiment of the present invention, in which (a) is a plan view and (b) is a side view. [Figure 11] FIG. 11 is a diagram showing a simulation result of a magnetic nanowire memory according to a comparative example. [Figure 12] FIG. 11 is a diagram showing a simulation result of the magnetic nanowire memory of FIG. [Figure 13]1A and 1B are schematic diagrams showing changes in energy consumption due to protrusions in a magnetic nanowire memory. [Figure 14] 11A and 11B are schematic diagrams of a magnetic nanowire memory according to a third embodiment of the present invention, in which (a) is a plan view and (b) is a side view. [Figure 15] FIG. 15 is a diagram showing a simulation result of the magnetic nanowire memory of FIG. [Figure 16] 10A and 10B are schematic diagrams of a magnetic nanowire memory according to a fourth embodiment of the present invention, in which (a) is a plan view and (b) is a side view. [Figure 17] 11A and 11B are schematic diagrams of a magnetic nanowire memory according to a fifth embodiment of the present invention, in which (a) is a plan view and (b) is a side view. [Figure 18] FIG. 13 is a schematic diagram of a magnetic nanowire memory according to a modified example of an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] (First embodiment) The magnetic nanowire memory according to the first embodiment will be described with reference to Fig. 1. Note that the sizes and positional relationships of the members shown in each drawing may be exaggerated for clarity of explanation. The magnetic nanowire memory 1 includes a magnetic nanowire 2 made of a thin-film magnetic material, an interlayer insulating film 3, and a recording element 4. The recording element 4 is made of a conductor that passes a recording current and is disposed so as to cross the magnetic nanowire 2 via the interlayer insulating film 3 in the film thickness direction of the magnetic nanowire 2. The magnetic nanowire 2 includes a recess 6 formed in a local area in the longitudinal direction of the magnetic nanowire 2 such that the film thickness is smaller than that of other areas. The recess 6 is disposed in a region 21 of the magnetic nanowire 2. The region 21 of the magnetic nanowire 2 is a region within a first predetermined length located in the vicinity (close to) adjacent to the recording element 4. Here, the first predetermined length is assumed to be smaller than the magnetic domain length in microns disclosed in Non-Patent Document 2.

[0015] Fig. 1 shows a schematic diagram of the structure near the recording element 4 of the magnetic nano-wire memory 1 and the recording method. Fig. 1 shows a state in which the magnetization direction of the magnetic nano-wire 2 is, for example, upward before recording (initial state), and the entire region of the magnetic nano-wire 2 is an upward magnetic domain region (region indicated by an upward arrow in magnetic domain region 13 in Fig. 1), but changes after recording. After recording, region 21 of the magnetic nano-wire 2 changes to a downward magnetic domain region (region indicated by a downward arrow in magnetic domain region 14 in Fig. 1), and the nano-wire region other than this region 21 remains as the upward magnetic domain region 13.

[0016] The magnetic nanowire 2 is a magnetic nanowire medium that functions as a magnetic recording medium. Here, it is assumed that the upstream side (left side in FIG. 1) and downstream side (right side in FIG. 1) are predefined in the longitudinal direction of the magnetic nanowire 2. The downstream side is the side that drives the magnetic domains formed in the magnetic nanowire 2, and the opposite side is the upstream side. A recess 6 is formed in region 21 of the magnetic nanowire 2.

[0017] The magnetic nanowire 2 is made of a magnetic material with a large coercive force and anisotropic magnetic field (large anisotropic energy) so that the magnetization state recorded inside the magnetic nanowire medium is not affected by external disturbances, etc. Therefore, in order to reverse the magnetization state of a specific magnetic domain, a large magnetic field that exceeds these energetically is required. Examples of materials for the magnetic nanowire 2 include materials (multilayer films or alloys) that exhibit perpendicular magnetization, such as Co / Tb, Co / Pt, Co / Ni, and Co / Pd. The magnetic nanowire 2 is formed on a substrate 10. The substrate 10 can be formed using various commonly used materials, such as surface thermally oxidized silicon, sapphire, magnesium oxide, and glass (including quartz).

[0018] The interlayer insulating film 3 is formed on the magnetic nanowire 2. The insulator forming the interlayer insulating film 3 is made of a general insulating material. Examples of such materials include oxide films such as SiO2 and Al2O3, silicon nitride (Si3N4), MgF2, etc. The shape of the interlayer insulating film 3 is not limited to the shape shown in the figure as long as it is stably supported on the substrate 10. The interlayer insulating film 3 may also be an insulating coating in which an insulating material is spread around the recording element 4.

[0019] The recording element 4 records magnetic domains corresponding to recording bits in the magnetic nanowire 2. The method for recording the magnetic domains is to apply a recording current from the outside to the recording element 4, generate a magnetic field due to the current flowing through the recording element 4, and locally reverse the magnetization in the magnetic nanowire 2 due to this current magnetic field. This area where the magnetization is locally reversed is recorded as a magnetic domain. The recording element 4 is provided on the interlayer insulating film 3. The recording element 4 is provided upstream of the center in the longitudinal direction of the magnetic nanowire 2 (on the left side in FIG. 1).

[0020] One end of the recording element 4 is connected to a conductor wiring 11, and the other end of the recording element 4 is connected to a conductor wiring 12. A current (recording current I) is applied to the recording element 4 via the conductor wirings 11 and 12 from an external power supply (pulse current source) not shown. The material of the recording element 4 may be a metal material with high conductivity, such as Ag, Au, Cu, or Al, which is commonly used in semiconductor integrated devices.

[0021] The structure of the magnetic fine wire 2 of the magnetic fine wire memory 1 shown in FIG. 1 is different from the structure of the magnetic fine wire 102 of the conventional magnetic fine wire memory 101 shown in FIG. 2. The magnetic fine wire 102 of the conventional magnetic fine wire memory 101 is a flat magnetic fine wire without a recess. In other words, the magnetic fine wire 102 has a uniform film thickness and a flat upper surface. In contrast, the magnetic fine wire 2 of the magnetic fine wire memory 1 of this embodiment has a recess 6. The recess 6 is formed in the longitudinal direction of the magnetic fine wire 2 on the side that receives the current magnetic field generated by the recording element 4 (the side that moves the magnetic domain).

[0022] The recess 6 is restricted in the longitudinal direction of the magnetic fine wire 2 and is formed in a groove shape with a recess in the film thickness direction. The recess 6 is formed across the width direction perpendicular to the longitudinal direction of the magnetic fine wire 2. That is, the recess 6 is a groove that penetrates continuously in the width direction of the magnetic fine wire 2. The size of the recess 6 in the top view is approximately the same as the size of the magnetic domain in the top view. Here, the size of the recess 6 in the longitudinal direction of the magnetic fine wire 2 is called the length of the recess, the size of the recess 6 in the width direction of the magnetic fine wire 2 is called the width of the recess, and the size of the recess 6 in the thickness direction of the magnetic fine wire 2 is called the depth of the recess. The length of the recess is equal to or smaller than the first predetermined length. In the following description, the shape of the recess 6 in the side view is assumed to be rectangular.

[0023] The process of forming magnetic domains in the magnetic nanowire 2 is as follows. First, a current (recording current I) is applied to the recording element 4 in the direction from the conductor wiring 11 to the conductor wiring 12. According to Ampere's law, a current magnetic field H rotating clockwise with respect to the current application direction is formed in the space around the recording element 4. When the current magnetic field H exceeds the coercive force of the magnetic nanowire 2, the magnetization direction of the magnetic nanowire 2 near the recording element 4 is reversed (downward in the figure) in line with the direction of the current magnetic field H, and a downward magnetic domain is formed. A magnetic domain wall 15 is formed at the boundary between the upward magnetic domain region 13 and the downward magnetic domain region 14. Although FIG. 1 shows the magnetic domain regions and magnetic domain walls as viewed from the side of the magnetic nanowire, they can also be shown as viewed from another surface, such as the top surface. Furthermore, the magnetic domains formed on the magnetic nanowire 2 can be moved downstream (to the right in Figure 1) by applying a current (driving current) in the longitudinal direction of the magnetic nanowire 2, and by repeating magnetic domain recording, information can be sequentially stored on the downstream side.

[0024] The information recording method in the magnetic nanowire memory 1 shown in FIG. 1 is similar to the information recording method in the magnetic nanowire memory 101 shown in FIG. However, a recess 6 is provided in the region 21 of the magnetic fine wire 2 of the magnetic fine wire memory 1, while no recess is provided in the magnetic fine wire 102 of the magnetic fine wire memory 101. A magnetic moment m exists in a minute volume in a magnetic material such as a magnetic fine wire, and the magnetization M is expressed as M = Σm as the sum of the magnetic moments m per unit volume. When the film thickness of the magnetic fine wire is thin, the magnetization M1 is smaller than the magnetization M2 when the film thickness of the magnetic fine wire is thick, i.e., M1 < M2. The magnetic fine wire 2 is in a state where the local magnetic anisotropy is weakened compared to the magnetic fine wire 102.

[0025] Also, in the magnetic fine wire memory, by applying a recording current I to the recording element 4, the magnitude of the current magnetic field H generated at a position at a distance r from the recording element 4 is represented by H ∝ I / r. 2 Therefore, when the distance from the recording element 4 is the same, a large current needs to be applied to generate a large current magnetic field. When the recording current applied to the recording element 4 is increased, the generated current magnetic field also increases, and the power consumption as a recording device increases. In addition, when the current density in the recording element 4 becomes excessive, the recording element 4 may be damaged, and there is also a limit to the increase in the current applied to the recording element 4. Therefore, it is required to achieve power-saving recording within a current range that does not exceed the limit current density.

[0026] In the magnetic fine wire memory 1 according to this embodiment, for the magnetic fine wire 2, by making the film thickness in the range where the magnetic fine wire 2 receives the current magnetic field from the recording element 4 thinner than the film thickness in other ranges, the local magnetization and coercive force of the magnetic fine wire 2 are reduced. As a result, the magnitude of the current magnetic field required for magnetization reversal becomes smaller, so the current value to be applied to the recording element 4 also becomes smaller, and magnetization reversal can be realized with low power.

[0027] Specifically, in the magnetic nanowire memory 1, when the region 21 of the magnetic nanowire 2 in which the recess 6 is formed is focused on, the film thickness of the region 21 is thinner than the surroundings, so that the external magnetic field required for magnetization reversal of the magnetic nanowire 2 is smaller than the external magnetic field required for magnetization reversal of the magnetic nanowire 102. That is, the magnetic field strength required for aligning the magnetization state of the magnetic nanowire 2 with the recess 6 in the direction of the current magnetic field H is smaller than the magnetic field strength required in the absence of the recess 6. In other words, the amount of the recording current applied to the recording element 4 can be reduced compared to the conventional case. That is, even when a small recording current that does not cause magnetization reversal is applied in the absence of the recess 6, the magnetization state of the region 21 of the magnetic nanowire 2 is aligned in the direction of the current magnetic field, magnetization reversal is performed, and downward magnetic domains can be formed in the magnetic nanowire. Therefore, according to the magnetic nanowire memory 1, by reducing the recording current, magnetic domains can be formed in the magnetic nanowire at a higher density than in the conventional case when compared with the same recording current. In addition, according to the magnetic nanowire memory 1, power saving in writing and recording can be realized.

[0028] [Method of manufacturing magnetic nanowire memory] Next, a method for manufacturing the magnetic nanowire memory 1 of this embodiment will be described with reference to FIG. 1 and the like. First, the magnetic nanowire 2 is formed on the substrate 10. The magnetic nanowire 2 is structured to have a recess 6 by a method to be described later. An interlayer insulating film 3 is formed on the magnetic nanowire 2, and a recording element 4 is provided on the interlayer insulating film 3. This series of manufacturing steps is similar to that of the conventional magnetic nanowire memory 101, which employs a procedure for forming layers of the magnetic nanowire 2 and the recording element 4 in this order on the substrate 10 using a sputtering method, so a description thereof will be omitted. Below, a method for forming the recess 6 of the magnetic nanowire 2 will be described.

[0029] The recess 6 can be manufactured by a general semiconductor device manufacturing process. Examples include a manufacturing method in which a part of the magnetic nanowire is cut out by Ga ions using a focused ion beam (FIB), a manufacturing method in which a part of the magnetic nanowire is cut into a desired shape by ion milling or reactive ion etching using a photomask or the like, and a manufacturing method in which the magnetic nanowire is divided into two layers and formed by a lift-off method. Below, an outline of the FIB method and the manufacturing method in which the magnetic nanowire is formed by the lift-off method from two different viewpoints will be described with reference to the drawings.

[0030] <First manufacturing method> The first manufacturing method is a method of forming the recesses 6 by cutting out the magnetic nanowire. In this first manufacturing method, first, as shown in FIG. 3(a), a magnetic material 52 is deposited on a substrate 10 by sputtering 51. Next, as shown in FIG. 3(b), a mask 53 is placed to expose only the area corresponding to the recesses of the magnetic nanowire, and an ion beam 54 is irradiated by FIB. As a result, as shown in FIG. 3(c), the magnetic material 52 in the area irradiated with the ion beam 54 is cut out, and the recesses 6 are formed in the magnetic nanowire. According to this first manufacturing method, the depth of the recesses 6 can be controlled by adjusting the time for irradiating the ion beam.

[0031] <Second manufacturing method> The second manufacturing method is a method of forming the recesses 6 by performing multi-stage sputtering, in which the thin film portions of the magnetic nanowire (areas where the recesses are to be located) are formed after the thick film portions. In this second manufacturing method, first, as shown in Fig. 4(a), resist 55 is uniformly applied onto the substrate 10, and then a pattern is drawn using a laser or electron beam 56, etc., except for the areas corresponding to the recesses of the magnetic nanowire. This leaves the resist 55 only in the areas corresponding to the recesses of the magnetic nanowire, as shown in Fig. 4(b).

[0032] Next, as shown in Fig. 4(c), a magnetic material 52 is deposited as a first layer by sputtering 51. Next, the remaining portion of the resist 55 is lifted off as shown in Fig. 4(d), leaving only the magnetic material 52 corresponding to the region where the magnetic nanowire is thick. Next, as shown in Fig. 4(e), a magnetic material 52 is deposited as a second layer by sputtering 51, thereby producing a magnetic nanowire memory having a recess 6 as shown in Fig. 4(f). According to the second manufacturing method, the depth of the recess 6 can be controlled by adjusting the film thickness of the sputtering deposition in the first stage.

[0033] <Third manufacturing method> The third manufacturing method is a method of forming the recesses 6 by performing multi-stage sputtering, in which the thin film portions of the magnetic nanowire (areas where the recesses are to be located) are formed before the thick film portions. In this third manufacturing method, first, as shown in Fig. 5(a), resist 55 is uniformly applied onto the substrate 10, and then a pattern is drawn only in the areas corresponding to the recesses of the magnetic nanowire using a laser or electron beam 56. This leaves the resist 55 provided in the areas corresponding to the thick film portions of the magnetic nanowire, as shown in Fig. 5(b). Next, as shown in Fig. 5(c), a magnetic material 52 is deposited by sputtering 51. Next, the remaining portion of the resist 55 is lifted off as shown in Fig. 5(d), leaving only the magnetic material 52 formed in the region corresponding to the recess of the magnetic nanowire.

[0034] Next, as shown in FIG. 6(a), a resist 55 is uniformly applied onto the substrate 10 and the remaining magnetic material 52, and then a laser or electron beam 56 is used to draw a pattern only in the areas corresponding to the thicker portions of the magnetic nanowire, resulting in the layered state shown in FIG. 6(b). Next, a magnetic material 52 is deposited by sputtering 51 in Fig. 6(b) as shown in Fig. 6(c). Next, resist 55 remaining in the portion corresponding to the recess of the magnetic nanowire is lifted off to manufacture a magnetic nanowire memory having a recess 6 as shown in Fig. 6(d).

[0035] The shape of the recess 6 in cross section or side view is not limited to a rectangle, and may be any other shape as long as it locally narrows the magnetic nanowire 2 in the film thickness direction. Examples of shapes that locally narrow the magnetic nanowire 2 in the film thickness direction include a semi-ellipse and a V-groove shape. Even in such cases, the same effect as in this embodiment can be obtained.

[0036] (simulation) In order to confirm the performance of the magnetic nanowire memory 1 of this embodiment, the inventors of the present application conducted verification of magnetization reversal and magnetic domain formation of the magnetic nanowire 2 of this embodiment having a recess by micromagnetic simulation using the Landau-Lifshitz-Gilbert equation. In the simulation, a structure was used in which an air layer that functions in the same manner as the interlayer insulating film 3 was provided between the recording element 4 and the magnetic nanowire 2 . Hereinafter, the simulation according to this embodiment will also be referred to as "Experiment 1." First, the conditions of the simulation will be described with reference to Figures 7(a) and 7(b) (and other figures as appropriate). As shown in the figures, the longitudinal direction of the magnetic nanowire 2 is the x-direction, the width direction of the magnetic nanowire 2 is the y-direction, and the film thickness direction of the magnetic nanowire 2 is the z-direction. Note that the x-direction corresponds to the width direction of the recording element, the y-direction corresponds to the longitudinal direction of the recording element 4, and the z-direction corresponds to the film thickness direction of the recording element 4. 7(b), the position of one upper edge (left end) 6a of the recess 6 provided in the magnetic nanowire 2 corresponds to the right end 4R of the recording element 4. The upper edge is shown as the position where the plane of the magnetic nanowire 2 intersects with the vertical plane that forms the recess 6.

[0037] [Global Simulation Settings] The overall settings for the simulation were as follows: In the simulation, the magnetic nanowire 2 was divided into a 4[nm]×4[nm]×4[nm] mesh, and the recording element 4 was divided into a 40[nm]×40[nm]×40[nm] mesh to perform calculations. The behavior of the magnetic moment in each mesh of the magnetic nanowire 2 was then verified. In the initial state before application of a recording current to the recording element 4, the directions of the magnetic moments of the magnetic nanowires 2 were all set to be upward. In the simulation, a current (recording current I) was also applied to the recording element 4 in the direction from the conductor wiring 11 to the conductor wiring 12 as shown in FIG.

[0038] [Experiment 1] The simulation conditions for each part of the magnetic nanowire memory 1 were as follows: The magnetic nanowire memory 1 for which the following simulation conditions are set is hereinafter referred to as Example 1. <Recording element 4> Material and shape of the recording element: Wire-shaped made of uniform metal material (Cu) Length of recording element (L4, see Figure 7(a)): L4 = 2000 [nm] Width of recording element (W4, see Fig. 7(a)): W4 = 120 [nm] Thickness of the recording element (T4, see FIG. 7(b)): T4 = 120 [nm] <Magnetic thin wire 2> Magnetic nanowire material: Co / Tb Saturation magnetization: 0.15[T] Length of magnetic nanowire (L2, see Fig. 7(b)): L2 = 1600 [nm] Width of the magnetic nanowire (W2, see Fig. 7(a)): W2 = 120 [nm] Thickness of the magnetic nanowire (T2, see Fig. 7(b)): T2 = 12 [nm] <Recess 6> Length of recess (L6, see Figure 7(b)): L6 = 480 [nm] Width of recess (W6, see Fig. 7(a)): W6 = 120 [nm] Depth of recess (T6, see Fig. 7(b)): T6 = 4 [nm] Shape of the recess in the xz plane: Rectangular <Interlayer insulating film 3> In the simulation, a structure was used in which an air layer that functions in the same way as the interlayer insulating film 3 was provided. Thickness of the air layer (T0, see Fig. 7(b)): T0 = 10 [nm]

[0039] In experiment 1, under the overall settings of the simulation and the simulation conditions of each part described above, the current applied to the recording element 4 of the magnetic nanowire memory 1 was a pulse current having the waveform shown in FIG. 8(a). The maximum current value of this pulse current is 100 [mA] (current density 7 × 10 10 [A / cm 2 ]) and the pulse width is 2 [ns]. The calculation step is set to 10 [ps] (picoseconds), and the calculation is performed from the start of application of the recording current until 2 [ns] (nanoseconds). As Comparative Example 1 for comparison with Example 1, a simulation was performed for a conventional flat magnetic nanowire 102 (see FIG. 2) that does not have a recess.

[0040] The simulation conditions for each part of Comparative Example 1 were as follows. <Recording element 4> The material, shape, length, width and thickness are the same as those of the recording element 4 in the first embodiment. <Magnetic thin wire 102> The material, length, width and thickness of the flat magnetic nanowire 102 are the same as those of the magnetic nanowire 2 in the first embodiment. <Interlayer insulating film 3> As in Example 1, an air layer of the same thickness was provided.

[0041] [Results of Experiment 1] <Comparative Example 1> In the simulation, as shown in Figures 1 and 2, when a current (recording current I) is applied to the recording element 4 in the direction from conductor wiring 11 to conductor wiring 12, a downward current magnetic field is generated to the right of the recording element 4 due to the current flowing through the recording element 4. However, in the case of Comparative Example 1 relating to the flat magnetic nanowire 102 without a recess, 2 nanoseconds after the start of application of a current to the recording element 4, all parts of the magnetic nanowire 102 were still magnetized in the upward direction. Therefore, the magnetic moment in the film thickness direction inside the magnetic nanowire 102 remained upward before and after the application of the recording current, and did not change. That is, in the case of Comparative Example 1, it was found that magnetization reversal could not be achieved with a recording current with a maximum current value of 100 [mA], and a larger current must be applied to the recording element 4 to reverse the magnetization.

[0042] <Example 1> FIG. 9 shows a schematic representation of the magnetization state of the recording element 4 and the magnetic nanowire on its right side after 2 nanoseconds from the start of application of a pulse current in Example 1. In FIG. 9, the direction of the magnetic moment in the film thickness direction inside the magnetic nanowire is indicated by shading. The lighter the shading, the greater the degree to which the magnetic moment is directed upward. Also, the darker the shading, the greater the degree to which the magnetic moment is directed downward. The initial state of the experiment is shown as pure white. Note that in FIGS. 11, 12, and 15, the direction of the magnetic moment in the film thickness direction inside the magnetic nanowire is indicated by shading.

[0043] In Example 1, when a recording current is applied, a downward current magnetic field is generated on the right side of the recording element 4. As shown typically in FIG. 9, a darker region (region with downward magnetization) is formed in region 21 (region where recess 6 is formed) of the magnetic nanowire 2 extending from directly below to the right side of the recording element 4. This indicates that the magnetic moment of the magnetic nanowire 2 has changed locally to a downward direction. Therefore, it was confirmed that magnetization reversal in region 21 of the magnetic nanowire 2 can be achieved by providing recess 6 in this region 21.

[0044] These simulation results show that even if the recording current is low enough that magnetization reversal does not occur when there is no recess in the magnetic nanowire, by providing a recess locally in the magnetic nanowire, magnetization reversal is possible with the same recording current. Specifically, in the magnetic nanowire memory 101 according to Comparative Example 1, a recording current of 100 [mA] (current density 7×10 10 [A / cm 2 ]), a current magnetic field of sufficient magnitude could not be generated, and magnetic domains could not be formed in the magnetic nanowire 102. On the other hand, in the magnetic nanowire memory 1 according to the first embodiment, it was found that by providing a local recess 6 in the magnetic nanowire 2 at a position downstream (right side) of the recording element 4, magnetic domains can be sufficiently formed even with the same recording current of 100 [mA]. ​​Therefore, it was found that the recording current can be reduced by providing a recess in the magnetic nanowire, demonstrating the effectiveness of this effect.

[0045] Second embodiment Next, the magnetic nanowire memory according to the second embodiment will be described with reference to Fig. 10(a) and Fig. 10(b) (and Fig. 1 as appropriate). Fig. 10(a) and Fig. 10(b) show the structure of the magnetic nanowire memory according to the second embodiment used in the simulation, in which an air layer that functions in the same way as the interlayer insulating film 3 is provided between the recording element 4 and the magnetic nanowire 2B. The coordinate system is the same as Fig. 7(a) and Fig. 7(b). In the following, the same components as those in the magnetic fine wire memory 1 according to the first embodiment are denoted by the same reference numerals, and the description thereof will be omitted as appropriate. The magnetic fine wire memory 1B shown in Fig. 10(a) and Fig. 10(b) differs from the first embodiment in the structure of the magnetic fine wire 2B.

[0046] The magnetic nano-wire memory 1B includes a magnetic nano-wire 2B made of a magnetic material, an interlayer insulating film 3 (see FIG. 1), and a recording element 4. The magnetic nano-wire 2B includes a recess 6. The recording element 4 is disposed on the upstream side adjacent to one upper edge 6a of the recess 6. The magnetic nano-wire 2B includes a protrusion 8 protruding in the film thickness direction of the magnetic nano-wire 2B. The protrusion 8 is made of a magnetic material and disposed in a region 22 of the magnetic nano-wire 2B. The region 22 of the magnetic nano-wire 2B is a region located on the downstream side adjacent to the other upper edge 6b of the recess 6 in the longitudinal direction of the magnetic nano-wire 2B.

[0047] The magnetic wire 2B differs from the magnetic wire 2 of the first embodiment in that it includes a convex portion 8. The convex portion 8 is formed in the longitudinal direction of the magnetic nanowire 2B on the side that receives the current magnetic field generated by the recording element 4 (the side that moves the magnetic domain). In this embodiment, the convex portion 8 is provided on the downstream side (the right side in FIG. 10(b)) of the concave portion 6. The convex portion 8 is also disposed adjacent to the right end of the concave portion 6 (the upper edge portion 6b on the right side).

[0048] The protrusions 8 are restricted in the longitudinal direction of the magnetic fine wire 2B, and are formed in stripes in the width direction, protruding in the film thickness direction. The protrusions 8 are formed across the width direction perpendicular to the longitudinal direction of the magnetic fine wire 2B. Here, the size of the protrusions 8 in the longitudinal direction of the magnetic fine wire 2 is called the length of the protrusions, the size of the protrusions 8 in the width direction of the magnetic fine wire 2 is called the width of the protrusions, and the size of the protrusions 8 in the thickness direction of the magnetic fine wire 2 is called the thickness of the protrusions. The length of the protrusions is smaller than the length of the recesses. In FIG. 14(b), the shape of the protrusions 8 in a side view is rectangular. The protrusions 8 are made of, for example, the same material as the magnetic fine wire.

[0049] (simulation) In order to confirm the performance of the magnetic nanowire memory 1B having the recesses 6 and the protrusions 8, the inventors of the present application carried out a micromagnetic simulation using the Landau-Lifshitz-Gilbert equation as described below. Hereinafter, the simulation according to this embodiment is also referred to as Experiment 2. In Experiment 2, the overall settings of the simulation were the same as those of Experiment 1 described above.

[0050] [Experiment 2] The simulation conditions for each part of the magnetic nanowire memory 1B were as follows: The magnetic nanowire memory 1B for which the following simulation conditions are set is hereinafter referred to as Example 2. <Recording element 4> The material, shape, length, width, and thickness were the same as those of the recording element 4 in Experiment 1. <Magnetic thin wire 2B> The main body of the magnetic fine wire 2B was provided with protrusions in addition to recesses, but the material, length, width and thickness of the main body of the magnetic fine wire 2B were the same as those of the magnetic fine wire 2 in the first experiment. <Recess 6> Compared to Experiment 1, the length of the recess was shortened as described below, but the width and depth of the recess were the same as those of recess 6 in Experiment 1. Length of the recess (L6, see FIG. 10(b)): L6 = 60 [nm] Width of recess (W6, see Fig. 10(a)): W6 = 120 [nm] Depth of recess (T6, see Fig. 10(b)): T6 = 4 [nm] <Interlayer insulating film 3> As in Example 1, an air layer of the same thickness was provided. <Protruding part 8> Length of the protrusion (L8, see Figure 10(a)): L8 = 30 [nm] Width of the protrusion (W8, see Fig. 10(a)): W8 = 120 [nm] Thickness of the protrusion (T8, see Fig. 10(b)): T8 = 4 [nm]

[0051] In experiment 2, under the overall simulation settings and simulation conditions for each part described above, the current applied to the recording element 4 of the magnetic nanowire memory 1B was a pulse current (maximum current value 100 mA) having the waveform shown in Figure 8(a), as in experiment 1. In Experiment 2, the calculation was performed from the start of application of the write current until 2 ns had elapsed. The calculation step was 10 ps, ​​the same as in Experiment 1. As a comparative example 2 to be compared with the second embodiment, a simulation was carried out for a magnetic nanowire 2 (see FIG. 1) that does not have a protrusion.

[0052] The simulation conditions for each part of Comparative Example 2 were as follows. <Recording element 4> The material, shape, length, width, and thickness are the same as those of the recording element 4 in the second embodiment. <Magnetic thin wire 2> The material, length, width and thickness of the magnetic wire 2 having no protrusions are the same as those of the magnetic wire 2B in the second embodiment. <Recess 6> The length, width and thickness are the same as in the second embodiment. <Interlayer insulating film 3> As in Example 2, an air layer of the same thickness was provided.

[0053] [Results of Experiment 2] <Comparative Example 2> FIG. 11 shows a schematic representation of the magnetization state of the recording element 4 and the magnetic nanowire on its right side after 2 nanoseconds have elapsed since the start of application of a pulse current in Comparative Example 2. In FIG. In Comparative Example 2, which has a structure having only recesses 6 without protrusions 8, when a recording current is applied, a downward current magnetic field is generated on the right side of the recording element 4. As shown typically in FIG. 11, in region 21 (region where recesses 6 are formed) of the magnetic nanowire 2 extending from directly below the recording element 4 to the right side, a dark region (region in a downward magnetized state) is formed in a semicircular shape, and the dark region occupies only a part of the width of the magnetic nanowire. Furthermore, the shape of the magnetic wall, which is the boundary between the magnetic domains, is disturbed. This shows that although the magnetic nanowire according to Comparative Example 2 has succeeded in partial magnetization reversal, it has not been able to form normal magnetic domains as recording bits. In Example 1 in Experiment 1 described above, the length L6 of the recesses 6 was set to 480 [nm], and the energy of the current magnetic field created by the recording current (100 [mA]) was able to reverse the magnetization of the entire recesses 6 (the entire region 21 of the magnetic nanowire 2). In contrast, in Comparative Example 2 in Experiment 2, the energy of the current magnetic field created by the same recording current (100 [mA]) did not reverse the magnetization of the entire recesses 6, which is believed to be because the length L6 of the recesses 6 was set to an extremely small 60 nm.

[0054] <Example 2> FIG. 12 shows a schematic representation of the magnetization state of the recording element 4 and the magnetic nanowire on its right side after 2 nanoseconds have elapsed since the start of application of a pulse current in Example 2. In FIG. In the second embodiment having the structure with the recessed portion 6 and the protruding portion 8, when a recording current is applied, a downward current magnetic field is generated on the right side of the recording element 4. As shown in FIG. 12, a dark area (a downward magnetized area) is formed in the area 21 (the area where the recessed portion 6 is formed) of the magnetic nanowire 2 immediately below the recording element 4 to the right side. This indicates that the magnetic moment of the magnetic nanowire 2B has changed locally to the downward direction. Also, as shown in FIG. 12, the magnetic domain wall, which is the boundary of the magnetic domain, is formed on a straight line in the full width direction of the magnetic nanowire, and the shape of the magnetic domain wall is stable. Therefore, it was confirmed that the magnetic nanowire 2B has the protruding portion 8, thereby realizing magnetization reversal in the recessed portion 6 adjacent to the upstream side of the protruding portion 8. From this, it is understood that the magnetic nanowire 2B according to the second embodiment can form a normal magnetic domain as a recording bit.

[0055] Here, the effect of the convex portion 8 of Example 2 will be described with reference to Fig. 13 (and other drawings as appropriate). A graph is arranged at the top of Fig. 13. The horizontal axis of this graph represents the distance x from the recording element 4 in the x direction, and the vertical axis of the graph represents the energy of the current magnetic field generated at the position of the distance x. As shown in the graph, the energy of the current magnetic field decreases by 1 / x as the distance x from the recording element 4 in the x direction increases. 2The energy attenuates at a rate of 0.01 V. The lower part of FIG. 13 shows a part of an enlarged view of FIG. 10(b). The imaginary line V1 shows a schematic representation of the origin of the graph being the center of the recording element 4. The imaginary line V2 shows a schematic representation of the correspondence between the position of the convex portion 8 of the magnetic wire 2b in the x direction (the position of the upper edge (right end) 6b of the concave portion 6 in the x direction) and the position on the horizontal axis of the graph. The region V3 surrounded by the imaginary line shows a schematic representation of the energy of the current magnetic field that would be used for magnetization reversal in the region downstream (to the right) of the position of the convex portion 8 of the magnetic wire 2b in the x direction if there was no convex portion.

[0056] In the magnetic fine wire 2B according to the second embodiment, the coercive force in the fine wire region with the recess 6 is lower than that in the region without the recess. In other words, the coercive force of the fine wire region (flat magnetic fine wire region without recess processing) located to the right of the upper edge (right end) 6b of the recess 6 is relatively higher than that of the fine wire region with the recess 6. And the protrusion 8 provided at the upper edge (right end) 6b of the recess 6 in the magnetic fine wire 2B acts as a barrier for the energy of the current magnetic field generated by the current flowing through the recording element 4. In other words, a part of the energy of the current magnetic field by the recording element 4 is not used for the magnetization reversal of the region to the right of the protrusion 8, but is instead additionally consumed in the fine wire region upstream (left side) of the barrier (protrusion 8). Thus, in the second embodiment, it is considered that the energy contributing to the formation of the magnetic domain to the left of the protrusion 8 formed the magnetic domain uniform in the width direction of the magnetic fine wire 2B.

[0057] As shown in Figure 13, the convex portion 8 of the magnetic wire 2B functions as a guard band that protects the energy of the current magnetic field that would normally be consumed in the area downstream (to the right) of the position of the convex portion 8 at the position of the convex portion 8, thereby locally strengthening the magnetization of the magnetic wire 2B upstream (to the left). The magnetic domain length of the magnetic domain formed in the magnetic nanowire 2B corresponds to the recording bit length. By making the magnetic domain length as narrow as possible, the linear recording density can be improved. However, even if the magnetic domain length is narrow, if uniform magnetization reversal cannot be achieved in the width direction of the magnetic nanowire in a local region in the nanowire direction as in Comparative Example 2, the magnetic domain state is not suitable for a recording bit.

[0058] According to these simulation results, when the length L6 of the recess 6 is narrowed to about 60 nm, as in Comparative Example 2 in which no protrusion is provided, the area (L6×T6) of the recess 6 is reduced, narrowing the range having a weak coercive force. Therefore, the magnetization cannot be reversed uniformly in the width direction (y direction) of the magnetic nanowire. In contrast, even in a magnetic nanowire structure with a narrow recess 6, as in Example 2 with the protrusion 8, magnetic domains that can reverse magnetization uniformly in the width direction of the magnetic nanowire can be formed in the magnetic nanowire 2B under conditions of applying a current of 100 mA to the recording element 4. Therefore, even in a structure with a narrow area of ​​the recess 6, magnetic domains can be formed at a low current by providing the protrusion 8. Moreover, Example 2 allows magnetic domains suitable as recording bits to be formed in the magnetic nanowire at a high density.

[0059] According to the magnetic nano-wire memory 1B of this embodiment, the effect of assisting magnetic domain formation by current application is enhanced by providing a combination of a region 21 on the magnetic nano-wire 2B in which the coercive force is locally reduced by the recess 6 and a local region 22 immediately downstream (right end) of the region 21 in which the film thickness is greater than that of a flat magnetic nano-wire. Also, according to the magnetic nano-wire memory 1B, by combining the protrusion 8 and the recess 6, the length of the magnetic domain in which uniform magnetization reversal can be achieved in the width direction of the magnetic nano-wire can be reduced even with the same recording current.

[0060] [Method of manufacturing magnetic nanowire memory] Next, the manufacturing method of the magnetic fine wire memory 1B of this embodiment will be described with respect to the differences from the manufacturing method of the magnetic fine wire memory 1 of the first embodiment. In this embodiment, the magnetic fine wire 2B has a structure having a recess 6 and a protrusion 8. The protrusion 8 can be manufactured by a general semiconductor device manufacturing process. For example, there is a method of dividing the magnetic fine wire into two or three layers and stacking them sequentially by a lift-off method, a method of preparing a magnetic fine wire that has been formed in advance to the height of the protrusion and forming the part other than the region where the protrusion is to be formed by cutting with an FIB, and a manufacturing method of cutting the magnetic fine wire other than the region where the protrusion is to be formed by ion milling or reactive ion etching using a photomask or the like.

[0061] Third embodiment Next, the magnetic nanowire memory according to the third embodiment will be described with reference to Figs. 14(a) and 14(b) (and Figs. 1, 10(a) and 10(b) as appropriate). Figs. 14(a) and 14(b) show the structure of the magnetic nanowire memory according to the third embodiment used in the simulation, in which an air layer that functions in the same way as the interlayer insulating film 3 is provided between the recording element 4 and the magnetic nanowire 2C. The coordinate system is the same as that in Figs. 10(a) and 10(b). In the following, the same components as those in the magnetic fine-wire memory 1B according to the second embodiment are denoted by the same reference numerals, and the description thereof will be omitted as appropriate. The magnetic fine-wire memory 1C shown in Fig. 14(a) and Fig. 14(b) differs from the second embodiment in the structure of the magnetic fine wire 2C. In this third embodiment, the convex portion provided on the magnetic fine wire described in the second embodiment exerts the effect of forming high-density magnetic domains by itself without being combined with the concave portion, as will be described in detail below.

[0062] The magnetic nanowire memory 1C includes a magnetic nanowire 2C made of a thin-film magnetic material, an interlayer insulating film 3 (see FIG. 1), and a recording element 4. The recording element 4 is made of a conductor that passes a recording current and is disposed so as to intersect with the magnetic nanowire 2C via the interlayer insulating film 3 in the film thickness direction of the magnetic nanowire 2C. The magnetic nanowire 2C includes a convex portion 8 formed so that the film thickness is locally larger than the film thickness in other regions in the longitudinal direction of the magnetic nanowire 2C. The recording element 4 is disposed on a predetermined upstream side (left side in FIG. 14(b)) in the longitudinal direction of the magnetic nanowire 2C. The convex portion 8 is disposed in a region 22 of the magnetic nanowire 2C. The region 22 of the magnetic nanowire 2C is a region on the downstream side (right side in FIG. 14(b)) separated from the recording element 4 by a region 21 having a first predetermined length. Here, the first predetermined length is assumed to be a length smaller than the magnetic domain length in microns disclosed in Non-Patent Document 2.

[0063] The magnetic nanowire 2C differs from the magnetic nanowire 2B of the second embodiment in that it has a convex portion 8 but no concave portion. The magnetic nanowire 2C has no concave portion in a first predetermined length region 21 between the recording element 4 and the convex portion 8, but the magnetization is reversed in this region 21 to form a magnetic domain.

[0064] (simulation) In order to confirm the performance of the magnetic nanowire memory 1C having the convex portion 8 on the flat magnetic nanowire, the inventors of the present application carried out a micromagnetic simulation using the Landau-Lifshitz-Gilbert equation as described below. Hereinafter, the simulation according to this embodiment is also referred to as Experiment 3. In Experiment 3, the overall settings of the simulation were the same as those in Experiment 2 described above.

[0065] [Experiment 3] The simulation conditions for each part of the magnetic nanowire memory 1C were as follows: The magnetic nanowire memory 1C for which the following simulation conditions are set is hereinafter referred to as Example 3. <Recording element 4> The conditions are the same as those of recording element 4 in Experiment 2. <Magnetic thin wire 2C> The conditions are the same as those for the magnetic nanowire 2B in Experiment 2, except that no recess is provided. <Interlayer insulating film 3> As in Example 2, an air layer of the same thickness was provided. <Protruding part 8> The conditions, including the position of the protrusion, are the same as those of protrusion 8 in Experiment 2.

[0066] In experiment 3, under the overall simulation settings and simulation conditions for each part described above, the current applied to the recording element 4 of the magnetic nanowire memory 1C was changed from the conditions in experiment 2 to a pulse current having the waveform shown in Figure 8(b). The maximum current value of this pulse current is 130 mA (current density 9 × 10 10 [A / cm 2 ]) and the pulse width is 2 [ns]. As in Experiment 2, the calculation was performed from the start of application of the write current until 2 ns had elapsed, and the calculation step was set to 10 ps.

[0067] [Results of Experiment 3] FIG. 15 shows a schematic diagram of the magnetization state of the recording element 4 and the magnetic nanowire on the right side thereof 2 nanoseconds after the start of application of a pulse current in Example 3. In FIG. In Example 3 having the convex portion 8 on the flat magnetic nanowire, when a recording current is applied, a downward current magnetic field is generated on the right side of the recording element 4. As shown in FIG. 15, a dark area (a downward magnetized area) is formed in the area 21 of the magnetic nanowire 2 from directly below the recording element 4 to the right side. This indicates that the magnetic moment of the magnetic nanowire 2C has changed locally to the downward direction. Therefore, by providing the convex portion 8 at a position away from the recording element 4 by a first predetermined length, the magnetic nanowire 2C can realize magnetization reversal in the area adjacent to the upstream side of the convex portion 8, and can form a normal magnetic domain as a recording bit. This is considered to be because, as described with reference to FIG. 13, part of the energy of the current magnetic field by the recording element 4 is not used for magnetization reversal in the area to the right of the convex portion 8, but is instead consumed in the nanowire area to the left of the barrier (convex portion 8), and a magnetic domain uniform in the width direction of the magnetic nanowire 2C is formed. It is clear that the third embodiment having the convex portion 8 on the flat magnetic nanowire can form magnetic domains even if the magnetic domain length is made shorter than in the past. Therefore, the third embodiment can form magnetic domains at high density on the magnetic nanowire by increasing the linear recording density.

[0068] (Fourth embodiment) Next, a magnetic fine wire memory according to a fourth embodiment will be described with reference to Figs. 16(a) and 16(b) (and Fig. 1 as appropriate). The magnetic fine wire memory 1D shown in Figs. 16(a) and 16(b) has two recording elements 4. In the following, the same components as those in the magnetic fine wire memory 1B according to the second embodiment (Figs. 10(a) and 10(b)) are denoted by the same reference numerals and will not be described as appropriate. When distinguishing between the recording elements 4, they will be represented as recording elements 4a and 4b. Note that in Figs. 16(a) and 16(b), the interlayer insulating film 3 (see Fig. 1) between the recording element 4 and the magnetic fine wire 2B is not shown.

[0069] The magnetic nano-wire memory 1D includes a magnetic nano-wire 2B made of a thin-film magnetic material, an interlayer insulating film 3 (see FIG. 1), and two recording elements 4. The two recording elements 4 are made of a conductor that passes a recording current, and are disposed at a first predetermined length apart so as to intersect with the magnetic nano-wire 2B via the interlayer insulating film 3 in the film thickness direction of the magnetic nano-wire 2B. The magnetic nanowire 2B has a recess 6. The recess 6 is disposed in a region 21 of the magnetic nanowire 2B. In this magnetic nanowire memory 1D, the region 21 of the magnetic nanowire 2B is a region in a range of a first predetermined length between one recording element 4a and the other recording element 4b. Here, the first predetermined length is set to be a length smaller than the magnetic domain length in microns disclosed in Non-Patent Document 2.

[0070] 16(b), in the magnetic fine wire memory 1D, one (left) recording element 4a is disposed on the upstream side adjacent to one (left) upper edge 6a of the recess 6. The other (right) recording element 4b is disposed on the downstream side adjacent to the other (right) upper edge 6b of the recess 6. The magnetic fine wire 2B has a protrusion 8 protruding in the film thickness direction of the magnetic fine wire 2B. The protrusion 8 is made of a magnetic material and is disposed at least in a region 22 of the magnetic fine wire 2B. As shown in Fig. 16(b), the region 22 of the magnetic fine wire 2B is a region located adjacent to and downstream of the other (right) upper edge 6b of the recess 6 in the longitudinal direction of the magnetic fine wire 2B.

[0071] In this embodiment, the distance between the two recording elements 4 and the length of the recess 6 are both set to a first predetermined length. Therefore, as shown in FIG. 16(b), the right end of the recording element 4a is located at a position corresponding to the left end 6a of the recess 6. Also, the left end of the recording element 4b is located at a position corresponding to the right end 6b of the recess 6.

[0072] The area between the two recording elements 4 of the magnetic nanowire memory 1D corresponds to a magnetic domain formation area designed to form a magnetic domain in the magnetic nanowire 2B. The two recording elements 4 record the magnetic domains using a composite current magnetic field generated by currents flowing in opposite directions. Specifically, for example, a recording current I a At the same time, a write current I b In the region 21 of the magnetic nanowire 2B sandwiched between the two recording elements 4, a recording current I a The direction of the current magnetic field generated by the recording current I b The direction of the current magnetic field generated by is also downward. By using these combined current magnetic fields, the upward magnetization of the region 21 of the magnetic nanowire 2B can be reversed to form a downward magnetic domain. The recording current I a and recording current I b Alternatively, the directions of the magnetization directions may be interchanged to invert the downward magnetization of the region 21 of the magnetic nanowire 2B to form an upward magnetic domain.

[0073] By using two recording elements 4 as in this embodiment, one magnetic wall can be formed in the magnetic nanowire directly below the recording element 4a, and the other magnetic wall can be formed directly below the recording element 4b. At this time, each magnetic wall is formed in a straight line in the full width direction of the magnetic nanowire. Therefore, when forming minute magnetic domains in the magnetic nanowire to increase the density of the magnetic domains, the shapes of the magnetic walls arranged directly below each recording element can be made stable without any disturbance. In addition, according to this embodiment, it is possible to control the spread of the magnetic domains and sequentially form minute magnetic domains of a constant length, and the magnetic domains can be formed in the magnetic nanowire at a high density.

[0074] In this embodiment, the magnetic nanowire 2B is provided with a convex portion 8 adjacent to the concave portion 6 in the driving direction (downstream side) of the magnetic domain. This makes the convex portion 8 a barrier to the combined current magnetic field created by the two recording elements 4, and the boundary of the magnetic domain formed in the magnetic nanowire 2B does not extend beyond the boundary of the initially designed magnetic domain formation region, making it possible to control the magnetic domain length more accurately than in the case where there is no convex portion 8. Note that, in the magnetic nanowire memory 1D according to this embodiment, both the concave portion 6 and the convex portion 8 are formed in the magnetic nanowire, but a magnetic nanowire having only either the concave portion 6 or the convex portion 8 may be used.

[0075] (First modified example of the fourth embodiment) The first modified example of the magnetic fine-wire memory 1D uses a magnetic fine-wire 2 (see FIG. 7(a) and FIG. 7(b)) in which there is no convex portion 8 and only a concave portion 6 is formed, instead of the magnetic fine-wire 2B. In detail, the first modified example of the magnetic fine-wire memory 1D includes a magnetic fine-wire 2 made of a magnetic material, an interlayer insulating film 3 (see FIG. 1), and two recording elements 4a, 4b (see FIG. 16(a) and FIG. 16(b)). The two recording elements 4a, 4b are made of a conductor that passes a recording current, and are arranged at a first predetermined length so as to intersect with the magnetic fine-wire 2 via the interlayer insulating film 3 in the film thickness direction of the magnetic fine-wire 2. The magnetic fine-wire 2 includes a concave portion 6. The concave portion 6 is arranged in a region 21 of the magnetic fine-wire 2. The region 21 of the magnetic fine-wire 2 is a region within a first predetermined length between one recording element 4a and the other recording element 4b. In the first modified example of the magnetic nanowire memory 1D, it is also possible to control the spread of the magnetic domains and form magnetic domains of a constant length, and the magnetic domains can be formed at a high density in the magnetic nanowire.

[0076] (Second modified example of the fourth embodiment) The second modified example of the magnetic fine-wire memory 1D uses a magnetic fine-wire 2C (see FIG. 14(a) and FIG. 14(b)) in which the recess 6 does not exist and only the protrusion 8 is formed, instead of the magnetic fine-wire 2B. In detail, the second modified example of the magnetic fine-wire memory 1D includes a magnetic fine-wire 2C made of a magnetic material, an interlayer insulating film 3 (see FIG. 1), and two recording elements 4a, 4b (see FIG. 16(a) and FIG. 16(b)). The two recording elements 4a, 4b are made of a conductor that passes a recording current, and are arranged at a first predetermined length so as to intersect with the magnetic fine-wire 2C via the interlayer insulating film 3 in the film thickness direction of the magnetic fine-wire 2C. The magnetic fine-wire 2C includes a protrusion 8. One recording element 4a is arranged on a predetermined upstream side in the longitudinal direction of the magnetic fine-wire 2C, and the other recording element 4b is arranged on a downstream side. The protrusion 8 is arranged in the region 22 of the magnetic fine-wire 2C. The region 22 of the magnetic wire 2C is a region on the downstream side separated by a first predetermined length from one recording element 4a in the longitudinal direction of the magnetic wire 2C. In the second modified example of the magnetic nanowire memory 1D, it is also possible to control the spread of the magnetic domains and form magnetic domains of a constant length, and the magnetic domains can be formed at a high density in the magnetic nanowire.

[0077] Fifth embodiment Next, a magnetic fine wire memory according to a fifth embodiment will be described with reference to Figs. 17(a) and 17(b) (and Fig. 1 as appropriate). The magnetic fine wire memory 1E shown in Figs. 17(a) and 17(b) has two recording elements 4 and has two convex portions 8 on the magnetic fine wire. In the following, the same components as those in the magnetic fine wire memory 1D according to the fourth embodiment (Figs. 16(a) and 16(b)) are denoted by the same reference numerals and will not be described as appropriate. Note that the interlayer insulating film 3 between the recording element 4 and the magnetic fine wire 2E is not shown.

[0078] The magnetic nanowire memory 1E includes a magnetic nanowire 2E made of a magnetic material, an interlayer insulating film 3 (see FIG. 1), and two recording elements 4a and 4b. The magnetic nanowire 2E has a recess 6 and a protrusion 8. The protrusion 8 is disposed in a region 23 located on the upstream side (left side) adjacent to an upper edge portion (left end) 6a of one of the recesses 6 (left side in FIG. 17(b)) in the longitudinal direction of the magnetic nanowire 2E, and in a region 22 located on the downstream side (right side) adjacent to an upper edge portion (right end) 6b of the other of the recesses 6 (right side in FIG. 17(b)).

[0079] In this embodiment, the distance of the area sandwiched between the two recording elements 4 and the length of the recess 6 are both set to a first predetermined length. In addition, the position of the right end of the convex portion 8 immediately below the recording element 4a corresponds to the upper edge (left end) 6a of the recess 6. In addition, the position of the left end of the convex portion 8 immediately below the recording element 4b corresponds to the upper edge (right end) 6b of the recess 6. Therefore, the distance of the area sandwiched between the convex portion 8 immediately below the recording element 4a and the convex portion 8 immediately below the recording element 4b is also the first predetermined length.

[0080] In this embodiment, too, by using two recording elements 4, it becomes possible to control the spread of the magnetic domains and form magnetic domains of a constant length, and the magnetic domains can be formed at a high density in the magnetic nanowire. In addition, in this embodiment, the magnetic nanowire 2E is provided with the convex portion 8 adjacent to the concave portion 6 not only on the downstream side but also on the upstream side. As a result, the two convex portions 8 each act as a barrier to the composite current magnetic field generated by the two recording elements 4, and both ends in the x direction of the magnetic domain formed in the magnetic nanowire 2E do not extend beyond both boundaries of the initially designed magnetic domain formation region, making it possible to control the magnetic domain length more accurately than in the case where there is no convex portion 8. Note that, in the magnetic nanowire memory 1E according to this embodiment, the magnetic nanowire has the concave portion 6 formed adjacent to the convex portion 8, but a magnetic nanowire without a concave portion may be used.

[0081] (Modification of the fifth embodiment) In the modified magnetic fine wire memory 1E, a magnetic fine wire having two convex parts 8 formed on a flat magnetic fine wire is used instead of the magnetic fine wire 2E. This magnetic fine wire having two convex parts 8 formed on a flat magnetic fine wire corresponds to a magnetic fine wire 2C (see FIG. 14(b)) having one convex part 8 to which another convex part 8 is provided, and is therefore referred to as a magnetic fine wire 2C below. The magnetic fine wire 2C having these two convex parts 8 corresponds to the magnetic fine wire 2E (see FIG. 16(b)) in a state in which a concave part 6 is not formed in the region 21. Therefore, in the magnetic fine wire 2C having two convex parts 8, the distance of the region sandwiched between the two convex parts 8 is the first predetermined length described above.

[0082] In detail, the modified magnetic nanowire memory 1E includes a magnetic nanowire 2C made of a magnetic material, an interlayer insulating film 3 (see FIG. 1), and two recording elements 4a and 4b. The two recording elements 4a and 4b are made of a conductor that passes a recording current, and are arranged at a first predetermined length apart so as to intersect with the magnetic nanowire 2C via the interlayer insulating film 3 in the film thickness direction of the magnetic nanowire 2C. The magnetic nanowire 2C includes a protruding portion 8. As shown in FIG. 17(b), the protruding portion 8 is arranged in a downstream region 22 and an upstream region 23, which are separated by the first predetermined length in the longitudinal direction of the magnetic nanowire 2C. This modified example of the magnetic nanowire memory 1E also makes it possible to control the spread of the magnetic domains and form magnetic domains of a constant length, and thus makes it possible to form the magnetic domains at a high density in the magnetic nanowire.

[0083] Although the magnetic nanowire memory according to the embodiment of the present invention has been described above, the gist of the present invention is not limited to these descriptions and should be broadly interpreted based on the claims. Furthermore, it goes without saying that various changes and modifications based on these descriptions are also included in the gist of the present invention.

[0084] For example, although the magnetic fine wire memory of each embodiment has one magnetic fine wire, the number of magnetic fine wires 2 may be more than one as shown in FIG. 18. The magnetic fine wire memory 1F shown in FIG. 18 is a magnetic fine wire memory according to a modified example of the magnetic fine wire memory 1 of the first embodiment shown in FIG. 7. Note that the substrate 10 (see FIG. 1) and the interlayer insulating film 3 (see FIG. 1) are omitted in FIG. 18. Also, although four magnetic fine wires 2 are illustrated as an example, the number is not limited to this and is arbitrary. In this magnetic fine wire memory 1F, a plurality of magnetic fine wires 2 are arranged in parallel at a predetermined interval in the width direction of the magnetic fine wires 2 on the substrate 10 (see FIG. 1). In this way, the storage capacity of the magnetic fine wire memory can be increased. Also, it is of course possible to provide a plurality of magnetic fine wires in the second to fifth embodiments and their modified examples. [Explanation of symbols]

[0085] 1,1B,1C,1D,1E,1F Magnetic nanowire memory 2,2B,2C,2E Magnetic wire 3. Interlayer insulating film 4, 4a, 4b Recording element 4R Right end of recording element 6 Recess 6a Left end of recess 6b Right end of recess 8 Convex 10 Substrate 11,12 Conductor wiring 13 Upward magnetic domain region 14 Downward magnetic domain region 15 Domain wall 21,22,23 area

Claims

1. At least one magnetic nanowire made of a thin-film magnetic material; a recording element made of a conductor for passing a recording current and disposed in a film thickness direction of the magnetic nanowire so as to intersect with the magnetic nanowire via an interlayer insulating film; the magnetic nanowire has a recess formed in a longitudinal direction of the magnetic nanowire such that the thickness of the recess is locally smaller than the thickness of the other region of the magnetic nanowire; the recess is disposed in a region within a range of a first predetermined length located adjacent to the recording element, The recess is formed across the width of the magnetic nanowire, the width being perpendicular to the longitudinal direction of the magnetic nanowire. the recording element is disposed upstream adjacent to one upper edge of the recess, The magnetic nanowire further includes a protrusion protruding in a thickness direction of the magnetic nanowire, The magnetic nanowire memory is characterized in that the convex portion is made of a magnetic material and is disposed in a region adjacent to and downstream from the other upper edge portion of the concave portion in the longitudinal direction of the magnetic nanowire.

2. At least one magnetic nanowire made of a thin-film magnetic material; two recording elements each made of a conductor for passing a recording current and disposed at a first predetermined distance from the magnetic nanowire so as to intersect the magnetic nanowire in a film thickness direction of the magnetic nanowire via an interlayer insulating film; the magnetic nanowire has a recess formed in a longitudinal direction of the magnetic nanowire such that the thickness of the recess is locally smaller than the thickness of the other region of the magnetic nanowire; the recess is disposed in a region within the range of the first predetermined length between one recording element and the other recording element, The recess is formed across the width of the magnetic nanowire, the width being perpendicular to the longitudinal direction of the magnetic nanowire. a recording element is disposed on the upstream side adjacent to one upper edge of the recess; the other recording element is disposed downstream adjacent to the other upper edge of the recess, The magnetic nanowire further includes a protrusion protruding in a thickness direction of the magnetic nanowire, The magnetic nanowire memory is characterized in that the convex portion is made of a magnetic material and is disposed in a region adjacent to and downstream from the other upper edge portion of the concave portion in the longitudinal direction of the magnetic nanowire.

3. The magnetic nanowire memory according to claim 2, characterized in that the convex portions are arranged in a region located downstream adjacent to the other upper edge portion of the concave portion in the longitudinal direction of the magnetic nanowire, and in a region located upstream adjacent to one upper edge portion of the concave portion.

4. 4. The magnetic nanowire memory according to claim 1, wherein the protrusion is formed across the width of the magnetic nanowire, the width being perpendicular to the longitudinal direction of the magnetic nanowire.

5. 5. The magnetic nanowire memory according to claim 1, wherein a plurality of the magnetic nanowires are arranged in parallel at predetermined intervals in a width direction of the magnetic nanowires on a substrate.

Citation Information

Patent Citations

  • Magnetic track, information storage device including magnetic track, and method of operating information storage device

    JP2010141340A

  • Domain wall displacement type device, data recording method thereof, and recording apparatus

    JP2020027805A

  • Spin transfer torque switching of a magnetic layer with volume uniaxial magnetic crystalline anistotropy

    US20200105999A1

  • Magnetic memory element, magnetic memory, and method for manufacturing the same