Flow baffles for molten carbonate fuel cells

Baffles in fuel cell stacks manage gas flow to achieve one-dimensional current and thermal gradients, addressing non-uniformity issues and enhancing mechanical stability and performance.

JP7595183B2Active Publication Date: 2024-12-05EXXONMOBIL TECHNOLOGY & ENGINEERING CO
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023548610
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-02-11
Filing Date
2021-03-04
Publication Date
2024-12-05
Estimated Expiration
2041-03-04

AI Technical Summary

Technical Problem

Conventional fuel cell stacks experience non-uniform current and thermal distribution due to vertical or cross-flow configurations, leading to differential thermal expansion and mechanical issues such as stack distortion, tilting, and contact losses.

Method used

Implementing baffles within the fuel cell stack to manage gas flow, allowing for parallel or countercurrent flow configurations that achieve one-dimensional current and thermal gradients, using apertures to control pressure drop and uniform gas distribution across the anode and cathode active regions.

Benefits of technology

This approach maintains the planarity of fuel cells within the stack, ensuring better contact and predictable compression, reducing mechanical challenges and improving uniformity of current density and temperature distribution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007595183000001
    Figure 0007595183000001
  • Figure 0007595183000002
    Figure 0007595183000002
  • Figure 0007595183000003
    Figure 0007595183000003
Patent Text Reader

Abstract

A molten carbonate fuel cell configuration is provided that allows for the introduction of an anode input gas flow to the side of the fuel cell adjacent to the inlet side of the cathode input gas flow while allowing the anode and cathode to operate under co-flow and / or counter-flow conditions. Improved flow characteristics are achieved during co-flow or counter-flow operation by diverting the input flow for the anode or cathode to an extended edge seal area adjacent to the active area of ​​the anode or cathode, and then using a baffle to provide a sufficient pressure drop for even flow distribution across the anode or cathode. A second baffle can be used to create a pressure drop when the output flow exits the active area to a second extended edge seal area before leaving the fuel cell.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] Baffle structures for molten carbonate fuel cells are provided along with methods for operating such fuel cells. [Background technology]

[0002] A conventional fuel cell stack assembly may be formed of a plurality of fuel cells, each having an anode layer and a cathode layer separated by an electrolyte layer. The plurality of fuel cells may be arranged to form a stack of fuel cells. Each anode layer includes an anode inlet (i.e., on one side of the stack of fuel cells) and an opposing anode outlet (i.e., on the opposite side of the stack), and an anode supply gas passes through the anode layer in a first direction from the anode inlet to the anode outlet. Similarly, each cathode layer includes a cathode inlet (i.e., on the other side of the stack) and an opposing cathode outlet (i.e., on the opposite side of the stack), and a cathode supply gas passes through the cathode layer in a second direction perpendicular to the first direction from the cathode inlet to the cathode outlet. The perpendicular flow of the anode supply gas and the cathode supply gas generates a two-dimensional distribution of electrical current within the fuel cell. For example, the current may be greatest at the corners adjacent to both the anode inlet and cathode inlet (due to increased gas concentration) and least at the corners adjacent to the anode outlet and cathode outlet (due to reduced electrochemical activity). The two-dimensional distribution of the current then changes in both the first and second directions, making it difficult to optimize the flows of anode and cathode feed gases to reduce the distribution of current across each fuel cell.

[0003] Standard perpendicular or cross flow configurations generate two-dimensional currents across the cell surface, which then induces a two-dimensional thermal gradient. This thermal gradient, where one corner is cooler than the average temperature of the flow field and another corner is hotter than the average temperature of the flow field, is problematic when many cells are stacked due to differential thermal expansion. Because the cell is no longer planar, the hot corner / side grows larger than the cold corner / side, causing distortion, tilt, and bending of the stack. This distortion can also induce contact loss and vary the amount of local compression in different areas of the cell. The higher the stack height, the more this effect operates. It would be advantageous to provide a fuel cell assembly that provides anode and cathode supply gases that flow in parallel directions to provide a one-dimensional distribution of current and therefore a one-dimensional temperature gradient. If achieved, the cells in the stack remain substantially planar, which allows for better contact, more predictable movement, and fewer challenges in maintaining uniform stack compression.

[0004] U.S. Patent No. 6,509,113 describes a baffle for use in an electrode of a solid oxide fuel cell that is said to reduce the amount of fuel that can access the anode when the fuel concentration is at a maximum, while allowing maximum exposure of the fuel to the anode when the fuel concentration is at a minimum.

[0005] U.S. Patent Application Publication No. 2020 / 0176787 describes a flow field baffle for a cathode in a molten carbonate fuel cell. Summary of the Invention

[0006] In various embodiments, an element in a molten carbonate fuel cell stack including a baffle is provided. The fuel cell stack element includes a gas flow inlet. The fuel cell stack element further includes a first volume in fluid communication with the gas flow inlet. The fuel cell stack element further includes a second volume, the second volume including at least a portion of an anode active area of ​​the fuel cell anode, at least a portion of a cathode active area of ​​the fuel cell cathode, or a reforming catalyst. The second volume may be in fluid communication with the gas flow inlet through the first volume. The fuel cell stack element further includes an inlet baffle including a plurality of inlet baffle apertures at an inlet boundary between the first volume and the second volume. At least a portion of the fluid communication between the first volume and the second volume may correspond to a fluid flow through the plurality of inlet baffle apertures. The length of the inlet baffle may be at least 60% of the length of the inlet boundary. The average height of the inlet baffle may be 100% or more of the average height along the inlet boundary. A combined cross-sectional area of ​​the multiple inlet baffle apertures can be between 0.5% and 6.0% of a total cross-sectional area at the inlet boundary. Additionally, the fuel cell stack element can include a gas flow outlet in fluid communication with the second volume.

[0007] In some embodiments, the fuel cell stack element may correspond to an anode or a cathode of a molten carbonate fuel cell. In such embodiments, the first volume may correspond to at least a portion of the volume within the extended edge wet seal chamber. In such embodiments, the second volume may correspond to at least a portion of the anode active area and associated anode flow field, or at least a portion of the cathode active area and associated flow field. In some embodiments, the fuel cell stack element may correspond to a reforming element, and the second volume includes a reforming catalyst.

[0008] A method for operating a fuel cell stack including such fuel cell stack components is also provided. [Brief description of the drawings]

[0009] [Figure 1] FIG. 1 is a schematic diagram of a fuel cell. [Diagram 2] FIG. 1 is a perspective view of a fuel cell stack configured for cross-flow operation. [Diagram 3] 1 is a perspective view of a fuel cell stack according to an exemplary embodiment; [Figure 4A] FIG. 2 is a top view of a fuel cell assembly according to an exemplary embodiment. [Figure 4B] FIG. 2 is a plan view of a fuel cell assembly according to another exemplary embodiment. [Figure 4C] FIG. 4B is a cathode level plan view of the fuel cell assembly shown in FIG. 4A. [Figure 4D] FIG. 4B is an anode level plan view of the fuel cell assembly shown in FIG. 4A. [Diagram 5] 1 illustrates a side view of an example baffle structure. [Figure 6] 1 shows a side view of another example of a baffle structure. [Figure 7] 1 shows a perspective view of an example baffle structure. [Figure 8] 1 shows a top view of a fuel cell with an extended wet seal and a desired flow pattern for anode gas flow. [Figure 9] 1 illustrates the anode gas flow direction within the anode with the use of a baffle structure. [Figure 10] 1 shows anode gas flow direction within an anode having a comparative baffle configuration. [Figure 11] 1 illustrates anode gas flow direction within an anode having another comparative baffle configuration. [Figure 12] 1 shows a comparative baffle structure. [Figure 13] FIG. 13 shows the pressure drop variation when the comparative baffle structure of FIG. 12 is used. [Figure 14] 1 shows another comparative baffle structure. [Figure 15] The pressure drop variation when the comparative baffle structure of FIG. 14 is used is shown. [Figure 16] 1 shows a top view of an example of a reformer unit as an element in a fuel cell stack. [Figure 17] 4 shows an example of a baffle aperture pattern. [Figure 18] 1 shows an example of a baffle configuration. [Figure 19] 4 shows another example of a baffle configuration. [Figure 20] 4 shows the average temperature profile of the cathode in the fuel cell stack. [Figure 21] 19 shows the average temperature profile of the cathode in a fuel cell stack including a reformer unit using a baffle configuration according to FIG. 18. [Figure 22] 22 shows the temperature profile of the cathode from FIG. 21 along the centerline of the cathode. [Diagram 23] 20 shows the average temperature profile of the cathode in a fuel cell stack including a reformer unit using a baffle configuration according to FIG. 19. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] In various aspects, a molten carbonate fuel cell configuration is provided that allows for the introduction of an anode input gas flow to the side of the fuel cell adjacent to the inlet side of the cathode input gas flow while allowing the anode and cathode to operate under co-current flow and / or counter-current flow conditions. It has been found that improved flow characteristics can be achieved in the anode during co-current flow or counter-current flow operation by diverting the anode input flow to an extended edge seal area (in an extended edge seal chamber) adjacent to the active area of ​​the anode, and then using a baffle to provide a sufficient pressure drop for even flow distribution of the anode input flow across the anode. A second baffle can be used to create a pressure drop when the anode output flow leaves the active area to a second extended edge seal area (in a second extended edge seal chamber) before the anode output flow leaves the fuel cell. Similar arrangements could be used to manage the cathode input flow and the cathode output flow, if desired.

[0011] Additionally, when using baffles to manage the pressure drop between the extended edge seal volume, it has further been found to be beneficial to use a solid baffle that substantially blocks the entire flow field but includes apertures or perforations that allow gas to flow across the baffle. This is in contrast to conventional baffle configurations where the pressure drop may be controlled based on the gap between the baffle and the top or bottom of the flow field. Due to the sensitivity of the pressure drop to minute manufacturing tolerance variations, it has been found that improved control over the pressure drop may be achieved by using apertures rather than relying on the gap between the surfaces. Optionally, for the input flow, an increased amount of available flow field may be provided at the end of the baffle that is furthest from where the anode input gas flow enters the input extended edge seal volume. This increased amount of available flow field may be based on using larger apertures near the far end of the baffle and / or by using a baffle that does not extend the entire length of the flow field (such as a baffle with a length up to 5% shorter than the length of the flow field). Optionally, for output flow, an increased amount of the available flow field can be provided at the end of the baffle furthest from where the anode output gas flow exits the output extended edge seal volume.

[0012] In another further embodiment, the baffles may also be used to manage flow to an integrated reforming unit as an element in a fuel cell stack. In such an embodiment, the reforming unit may be integrated as a stack element in a fuel cell stack periodically, such as having one reforming unit for every three or more fuel cells, or one reforming unit for every five or more fuel cells, for example, up to one reforming unit for every twenty fuel cells, or even less in some cases. The integration of the reforming unit in the fuel cell stack may at least partially consume excess heat generated during operation of the fuel cell by performing reforming in adjacent and / or nearby elements in the fuel cell stack. In such an embodiment, the baffles may be used to adjust the flow pattern in the reforming unit so that the heat consumption pattern in the reforming unit is relatively similar to the heat production pattern in adjacent and / or nearby fuel cell elements in the stack.

[0013] In the case of a fuel cell stack, one option for managing the gas flows into and out of the stack is to use manifolds. Based on practical considerations, it may be beneficial to physically separate the manifolds for the anode input and anode output flows from the manifolds for the cathode input and cathode input flows. In the case of a fuel cell stack with an approximately rectangular or square geometry, a convenient way to physically separate the manifolds may be to place the manifolds for the anode input and anode output flows on a different side of the fuel cell stack than the manifold for the cathode input flow (and the manifold for the cathode output flow, if present). This type of configuration may reduce or minimize the geometric difficulties in connecting the manifolds to the fuel cell stack, but it may result in the direction of flow in the anode being approximately perpendicular to the direction of flow in the cathode or in cross-flow. Unfortunately, under some operating conditions, operating the fuel cell in a cross-flow configuration may result in non-uniformity of the reaction conditions in the fuel cell. This may potentially present mechanical problems and / or fuel cell lifetime difficulties.

[0014] To avoid the drawbacks of the cross-flow configuration while maintaining the benefits of maintaining a physical separation of the anode and cathode manifolds, it has been found that the direction of flow within the anode can be changed to achieve co-current or counter-current flow within the fuel cell while still achieving a substantially uniform altered flow pattern within the anode. However, it has been found that in order to achieve a substantially uniform altered flow pattern, a relatively even distribution of the anode input flow must occur across the entire width of the anode in a direction perpendicular to the desired flow direction within the anode. Otherwise, flow pattern drawbacks similar to those associated with the cross-flow configuration will remain because an uneven distribution of gas will exist within the anode.

[0015] In this discussion, modifying fuel cell operation to have co-current or counter-current flow is described based on changing the direction of flow in the anode. Changing the anode flow is described for ease of explanation of the variations. It is understood that the direction of flow in the cathode can be changed instead.

[0016] It has been found that a substantially uniform distribution of gas across the entire width of the anode can be achieved in part by using multiple baffles. First, the anode input flow can enter the fuel cell stack and can be diverted into the (input) extended edge seal chamber by a blocker. A first baffle can then be used to create a pressure drop for the anode input flow after it enters the extended edge seal chamber but before it enters the active area of ​​the anode. A second baffle can be used to create a second pressure drop for the anode output flow before it leaves the active area of ​​the anode and enters the second (output) extended edge seal chamber. It has been found that a sufficient pressure drop on either side of the active area of ​​the anode can enable uniform flow distribution within the active area of ​​the anode. Additionally, it has been found that positioning the baffles approximately at the boundaries of the active area of ​​the anode can reduce or minimize non-uniform operation within the active area of ​​the fuel cell.

[0017] It has further been found that the type of baffle used can affect operation to achieve the desired substantially uniform distribution of gas while reducing or minimizing non-uniform operation. To achieve a relatively uniform distribution of gas, the pressure drop between the extended edge seal area and the active area of ​​the anode can be between 0.1 kPa and 1.0 kPa. Achieving this level of pressure drop can require reducing the cross-sectional area of ​​the flow field available for fluid flow to about 0.5% to 6.0%, or 0.5% to 4.0%, or 0.5% to 2.5% of the total cross-sectional area of ​​the flow field at the baffle location. In some embodiments where a relatively uniform pattern of apertures is used along the entire length of the baffle, the available cross-sectional fluid flow area at the baffle location can be between 0.5% to 2.5% of the total cross-sectional area of ​​the flow field at the baffle location. In embodiments where there is additional available cross-sectional area at the end of the baffle furthest from the gas inlet / outlet location, the available cross-sectional area at the baffle location may be 0.5% to 4.0% or 0.5% to 6.0% of the total cross-sectional area of ​​the flow field at the baffle location. In this discussion, the available cross-sectional fluid flow area at the baffle location is defined as the percentage of the total cross-sectional flow field area that remains open for fluid flow at the baffle location after the baffle is placed in the flow field. As explained in more detail below, the total cross-sectional flow field area may depend on the configuration of the fuel cell. In some embodiments, the total flow field cross-sectional area at the baffle location may correspond to the area between the plate-like surface of the anode collector (or cathode collector) and the opposing separator plate that is compressed against the anode collector (or cathode collector) during construction of the fuel cell.

[0018] When determining the available cross-sectional flow field area provided by the apertures in a baffle, it should be noted that for a V-shaped baffle, the size and / or number of apertures may be different on the two sides of the V. In such embodiments, the available cross-sectional flow field area for a V-shaped baffle is defined as the available cross-sectional flow field area for the side of the baffle having the lower cross-sectional flow field area. More generally, for any type of baffle shape in which gas flow must pass through two or more apertures to completely traverse the baffle, the available cross-sectional flow field area is defined as the cross-sectional area for the set of apertures that corresponds to the lowest cross-sectional area.

[0019] Due in part to the relatively small amount of cross-sectional area available for fluid flow, it has been found that the pressure drop between the extended edge seal chamber and the anode has a relatively high sensitivity to variations in cross-sectional area. Due to this relatively high sensitivity, it has been found that a solid baffle having apertures that otherwise occupy or fill the entire flow field (i.e., gas flow path) along the boundary or line between the extended edge seal chamber and the anode can provide improved operation. This improved operation is associated with a configuration in which the baffle has a height that is less than the height of the flow field at the boundary, such that the baffle occupies or fills most, but not all, of the cross-sectional area of ​​the flow field along the boundary between the extended edge seal chamber and the anode. This improved operation may be achieved in part based on an improved ability to control the manufacturing tolerances of the apertures in the baffle as opposed to the manufacturing tolerances of the overall size and shape of the baffle.

[0020] It should be noted that the location of the baffle defines the boundary between the first volume and the second volume. In aspects where the length of the baffle is less than the full length of the fuel cell at the baffle location, the boundary is defined to extend beyond the baffle, so that the boundary extends the full length of the fuel cell at that location. Thus, the boundary can be longer than the baffle that defines it. It should be further noted that the boundary defined by the baffle does not have to be the same as the boundary between the extended edge seal chamber and the anode (or cathode). For example, the baffle can be located within the extended edge seal chamber. For input flow, this would mean that after passing the baffle, the gas flow may still have a distance to travel before reaching the portion of the anode flow field associated with the active area of ​​the anode. It is less preferred to place the baffle over a portion of the anode active area, as this means that the anode gas flow may interact with the anode active area before achieving the improved gas flow distribution provided by the pressure drop across the baffle. In other words, a baffle over a portion of the anode active area would mean that the anode input gas flow may enter the anode flow field associated with the anode active area before encountering the baffle.

[0021] In some embodiments, the baffle may correspond to a conforming baffle that initially has a height slightly greater than the height of the flow field. In such embodiments, the conforming baffle may deform under the pressures used in assembly of the fuel cell. This may reduce or minimize the difficulty of controlling tolerances on the baffle height while still allowing the baffle to completely block the flow field at the baffle location, except for the apertures in the baffle.

[0022] A variety of options are available for how to use the baffles to provide a desired amount of available cross-sectional area for the flow field. For example, the apertures within the baffle may be uniform (i.e., substantially the same size), or the size of the apertures may vary within the baffle. Optionally, the variation in aperture size may follow a pattern such as alternating larger and smaller sized apertures, or increasing aperture size along the length of the baffle, or another convenient pattern. More generally, any convenient method for selecting aperture sizes to achieve a desired amount of available flow field cross-sectional area may be used.

[0023] In various embodiments, for a V-shaped baffle, the apertures on one side of the "V" may be offset from the apertures on the second side of the V. By using offset apertures on the two sides of the V, any gas entering through an aperture on the first side of the V-shaped baffle must move laterally within the baffle before exiting through an aperture on the second side. If the apertures on the two sides of the V are aligned, "channeling" of gas flow may occur, where gas may pass through the aligned apertures without lateral movement. Such channeling may reduce the pressure drop across the baffle and / or reduce the benefits provided by the baffle to generate a more desirable flow pattern. Although the apertures on different sides of the baffle are preferably offset, in some embodiments the size and / or pattern of the apertures may otherwise be the same for the two sides of the baffle. In other embodiments, at least one of the aperture size and the aperture pattern may vary between the two sides of the V-shaped baffle.

[0024] In some embodiments, additional available cross-sectional flow field area can be provided at the end of the baffle furthest from the location where the anode gas flow enters / exits the extended edge seal volume. For example, in the case of an input extended edge seal volume, the anode input flow enters at a first end of the input extended edge seal volume. In such an example, a baffle between the input extended edge seal volume and the anode active area (optionally located at the anode inlet corresponding to the beginning of the anode active area) can allow additional available cross-sectional flow field area at the baffle location at the second end of the input extended edge seal volume (i.e., the portion of the inlet baffle location furthest from the gas input flow into the extended edge seal volume). This additional available cross-sectional flow field area can correspond to 25% or more, or 50% or more of the total available cross-sectional flow field area. Additionally or alternatively, the amount of available cross-sectional flow field area located at the furthest end section of the baffle can correspond to 0.1% to 5.0%, or 0.1% to 3.0% of the total cross-sectional flow field area. In embodiments where there is additional available cross-sectional flow field area at the furthest end of the baffle, the remainder of the baffle may have an available cross-sectional flow field area corresponding to between 0.4% and 2.5% of the total cross-sectional area of ​​the flow field at the baffle location.

[0025] There are several options for providing additional available cross-sectional flow field area. One option may be to have a relatively large aperture in the portion of the baffle corresponding to 3.0%-20% (or 3.0%-15%, or 3.0%-10%) of the length of the baffle and / or the length of the baffle location furthest from the entry point of the anode input gas flow into the input extended edge seal volume. Similarly, for the output extended edge seal volume, a relatively large aperture may be included in the portion of the baffle furthest from the exit point of the anode output gas flow from the output extended edge seal volume. By way of example, in some embodiments, the length of the flow field (corresponding to the internal length of the fuel cell) may be about 30 inches to 40 inches (about 750 mm to 1000 mm). Baffles for such flow fields may have similar lengths. In an embodiment in which the baffle and / or baffle location has a length of 30 inches (about 750 mm), the last 1.0 inch (about 25 mm) of the baffle and / or baffle location would correspond to about 3.3% of the length of the baffle and / or baffle location, while the last 6.0 inches (about 150 mm) would correspond to about 20% of the length of the flow field at the baffle location.

[0026] Another option may be to use a baffle that is less than the full length of the flow field at the baffle location. In such an option, the baffle may be 0.05% to 5.0%, or 0.05% to 3.0%, or 0.05% to 1.0%, or 1.0% to 5.0% shorter than the full length of the flow field. In such an option, the gap created by the difference between the baffle length and the length of the flow field may be placed at the end of the extended edge seal volume furthest from the anode gas flow input / outlet location. As an example, in an embodiment where the length of the flow field is about 750 mm, a baffle that is 0.05% shorter than the flow field would correspond to a baffle having a length of 749.6 mm. A baffle that is 5.0% shorter than the flow field would correspond to a baffle having a length of 712.5 mm. It is noted that for a baffle that is a percentage shorter than the full length of the flow field, the amount of additional available cross-sectional flow field area resulting from the open gap is roughly the same as the difference in length between the baffle and the flow field. Thus, a baffle that is 1.0% shorter than the flow field provides 1.0% additional available cross-sectional flow field area.

[0027] Yet another option may be to have an initial portion of the baffle (i.e., the portion closest to the flow input / output) with a reduced or minimized amount of cross-sectional flow field area. For example, the first 5.0%-25% of the baffle may comprise less than 0.1% of the available cross-sectional flow field area. Optionally, this may correspond to the first 5.0%-25% of the baffle having no apertures.

[0028] In some embodiments, the baffles for the input extended edge seal volume may be different from the baffles for the output extended edge seal volume. In such embodiments, any convenient type of difference may exist between the baffles. This may include, but is not limited to, having different available cross-sectional flow field areas for the baffles, having different aperture sizes for the baffles, having different patterns of apertures for the baffles, and / or having differences in the amount of available cross-sectional flow field area at the ends of the baffles. In some embodiments, the difference in available cross-sectional flow field area between the input and output baffles may be between 0.1% and 1.0%. In some embodiments, the difference in available cross-sectional flow field area between the input and output baffles may be between 1.1% and 5.0%.

[0029] Typical molten carbonate fuel cell structure FIG. 1 shows a typical example of a portion of a molten carbonate fuel cell stack. The portion of the stack shown in FIG. 1 corresponds to a fuel cell 401. The fuel cell includes separator plates 410 and 411 to separate the fuel cell from adjacent fuel cells in the stack and / or other elements in the stack. In FIG. 1, the fuel cell 401 includes an anode 430 and a cathode 450 separated by an electrolyte matrix 440 that includes an electrolyte 442. In various embodiments, the cathode 450 may correspond to a bi-layer (or multi-layer) cathode. The anode collector 420 provides electrical contact between the anode 430 and other anodes in the stack, while the cathode collector 460 provides similar electrical contact between the cathode 450 and other cathodes in the fuel cell stack. Additionally, the anode collector 420 allows for the introduction and exhaust of gases from the anode 430, while the cathode collector 460 allows for the introduction and exhaust of gases from the cathode 450. The shape of the anode collector 420 in Figure 1 is intended to represent the concept that curved structures (such as curved protrusions from a plate-like surface) may be used to provide contact between the anode collector 420 and either the anode 430 or the separator plate 410. For example, such curved structures may reside above gaps in the anode collector 420 to allow fluid to pass into or out of the anode 430. Other convenient shapes may be used, including having at least one surface corresponding to a plate-like surface with openings that allow gas to pass through the plate-like surface. The cathode collector 460 is similarly represented by a curved surface, with the understanding that other convenient shapes may also be used.

[0030] In operation, CO 2 O 2 The CO is passed through the cathode collector 460. 2 and / or O 2 CO may come from any convenient source, such as air or flue gas from a combustion device. 2 and O 2CO diffuses into the porous cathode 450 and migrates to the cathode interface region near the interface of the cathode 450 and the electrolyte matrix 440. At the cathode interface region, some of the electrolyte 442 may reside within the pores of the cathode 450. 2 and O 2 is the concentration of carbonate ions (CO 3 2- ), which can then be transported across the electrolyte 442 (and thus across the electrolyte matrix 440) to facilitate the generation of an electric current. In embodiments where alternative ion transport is occurring, O 2 A portion of the carbonate ions may be converted to substitute ions, such as hydroxide or peroxide ions, for transport into the electrolyte 442. After transporting across the electrolyte 442, the carbonate ions (or substitute ions) may reach the anode interfacial region near the boundary of the electrolyte matrix 440 and the anode 430. The carbonate ions are converted to H 2 In the presence of CO 2 and H 2 O to release electrons that are used to form the electrical current generated by the fuel cell. This can occur, for example, when the electrolyte 442 is present within the pores of the electrolyte matrix 440. 2 , and / or H 2 A hydrocarbon suitable for forming the anode 430 is introduced to the anode 430 via the anode collector 420 .

[0031] 2, a conventional fuel cell stack 10 includes a plurality of fuel cells 11 (such as fuel cell 401 shown in FIG. 1), each having an anode layer 12 (including an anode electrode and an anode flow chamber / current collector, not shown) and a cathode layer 14 (including a cathode electrode and a cathode flow chamber / current collector, not shown), stacked one on top of the other. The fuel cell stack 10 includes an anode inlet side (or stack face) 16 configured to receive an anode feed gas, and an opposing anode outlet side (or stack face) 18 configured to output an anode exhaust gas after passing through the anode layer 12. The anode feed gas may be provided via an external manifold (anode inlet manifold 116) adjacent to and sealed to the anode inlet stack face 16. For reference purposes, the external manifold shown in FIG. 2 has been removed from the fuel cell stack 10. For clarity, during operation, an external manifold (e.g., anode inlet manifold 116) will be sealed against the corresponding fuel stack face. Anode exhaust may be received by another external manifold (anode outlet manifold 118) adjacent to and sealed against the anode outlet stack face 18. The fuel cell stack 10 further includes a cathode inlet side (or stack face) 20 configured to receive a cathode supply gas and an opposite cathode outlet side (or stack face) 22 configured to output the cathode exhaust after passing through the cathode layers 14. Cathode supply gas may be provided via an external manifold adjacent to and sealed against the cathode inlet stack face 20 (cathode inlet manifold 120). Cathode exhaust may be received by another external manifold (cathode outlet manifold 122) sealed against the cathode outlet stack face 22. In some embodiments, at least three of the four stack faces may have external manifolds sealed against their respective stack faces. For example, the stack may be contained in a sealed housing (eg, a module) and the anode inlet side, anode outlet side, and cathode inlet side may be sealed with external manifolds.The cathode outlet side in this example may be open to the sealed housing.

[0032] In a conventional fuel cell stack 10 shown in Figure 2, anode supply gas flows through each anode layer 12 in a substantially linear direction from an anode inlet stack face 16 to an anode outlet stack face 18. (As referred to herein, "substantially linear" means a majority of the volume of gas flow in a particular direction.) Similarly, cathode supply gas flows through cathode layers 14 in a substantially linear direction from a cathode inlet stack face 20 to a cathode outlet stack face 22. The anode supply gas and cathode supply gas flow substantially perpendicular to one another when they are in the stack (i.e., a majority of the volume of the anode supply gas flows in a first direction and a majority of the volume of the cathode supply gas flows in a second direction that is substantially perpendicular to the first direction) (also known as "cross flow"). Thus, current density may be highest at the corners of the fuel cell stack 10 proximate where the anode inlet side 16 meets the cathode inlet side 20 (Region I), and varies non-linearly with the direction of each of the anode and cathode supply gas flows through the fuel cell assembly 11. It may therefore be advantageous to redirect the flows of anode and cathode supply gases relative to one another within the stack, such that the anode and cathode flows pass through the fuel cell stack 10 in a substantially parallel configuration (also known as "parallel flow," "concurrent flow," or "counter flow").

[0033] The present invention allows for substantially parallel flow of two process gas mixtures in a four-sided fuel cell stack, where the two process gas mixtures are supplied and removed from the stack in directions substantially perpendicular to one another. In other words, the present invention allows for substantially parallel flow within the fuel cell stack without significantly modifying the process gas delivery between the fuel cell stacks (i.e., using external manifolds), as described in connection with FIG.

[0034] 3, a fuel cell stack 200 illustrates how the anode supply gas is redirected through a corner of the fuel cell stack 200 substantially parallel to the cathode supply gas, and the anode exhaust is redirected again to be output substantially perpendicular to the cathode exhaust. (For ease of reference, the arrows labeled "A" represent the flow path of the anode process gas, and the arrows labeled "C" represent the flow path of the cathode process gas.) The fuel cell stack 200 includes multiple fuel cell assemblies 211, each having an anode layer 208 and a cathode layer 210, the fuel cells stacked on top of each other and separated from each other by steel separator sheets (e.g., bipolar plates). Note that the top surface of the top fuel cell assembly 211 has been removed to show the flow paths within that fuel cell assembly. Except for the porous active area (anode active area) 213 of the anode electrode, the anode layer 208 of each fuel cell assembly 211 will be understood to be otherwise a sealed chamber with a single inlet (partial anode inlet 216, described below) and a single outlet (partial anode outlet 218, described below). As used herein, an "active area" is an area on a fuel cell layer (anode, cathode) that is configured to allow selective diffusion of molecules in a process gas thereto, i.e., the feed gas undergoes electrochemical reaction within the active area. Stated differently, the front and rear edges of both the anode and cathode of the fuel cell have narrow non-active areas corresponding to the wet seals between the adjacent cells above and below the fuel cell. The feed gas passes through the wet seals without undergoing electrochemical reaction. The remaining area of ​​the fuel cell, which overlaps and is common to both the anode and cathode layers, undergoes electrochemical activity and is known as the "active area." Similarly, aside from the porous active cathode electrode (not shown), the cathode layer 210 of each fuel cell assembly 211 is otherwise a sealed chamber having a cathode inlet 226 and a cathode outlet 228 .It is further noted that a portion of the sidewall of the fuel cell assembly 211 has been removed to show the flow paths through the cathode layer of the top fuel cell assembly 211 (and the flow paths of the anode and cathode layers of the fuel cell assembly 211 immediately below the top fuel cell assembly 211). It is further noted that reference may be made to enumerated features corresponding to the top fuel cell assembly 211, but such enumerated features may be applicable to the other fuel cell assemblies 211 included in the fuel cell stack 200.

[0035] It should be noted that the fuel cell assembly 211 described herein includes an anode layer 208 and a cathode layer 210 separated by an electrolyte matrix layer, with steel separator sheets forming the top and bottom surfaces of the fuel cell assembly. However, in other embodiments, a first fuel cell assembly may include an anode layer 208 and a cathode layer 210 separated by a steel separator sheet, with the anode electrode forming the first surface (e.g., the top surface) and the cathode electrode forming the second surface (e.g., the bottom surface). A single functional fuel cell unit is formed when a second fuel cell assembly (having the same components as the first fuel cell assembly) is stacked on top or bottom of the first fuel cell assembly, with the two fuel cell assemblies separated by an electrolyte matrix layer. In other words, a single fuel cell unit is formed when the cathode of the first fuel cell assembly is in communication with an electrolyte matrix that is in communication with the anode of the second fuel cell assembly.

[0036] 3 shows three fuel cell assemblies 211, the invention is not so limited and a fuel cell stack may include more or fewer fuel cell assemblies. Each fuel cell assembly 211 includes two extended edge seal chambers 236, 246: a first extended edge seal chamber 236 (e.g., an upstream extended edge seal chamber) on a first side of the fuel cell assembly and a second extended edge seal chamber 246 (e.g., a downstream extended edge seal chamber) on an opposite side of the fuel cell assembly. As shown in FIG. 3, the extended edge seal chambers cantilever outward from the stack face beyond the two opposite active areas of the fuel cells.

[0037] Similar to the fuel cell stack 10 shown in FIG. 2, the fuel cell stack 200 (of FIG. 3) includes an anode inlet side (or stack face) 212 and an opposing anode outlet side (or stack face) 214 that is substantially parallel to the anode inlet side 212. However, unlike the anode inlet stack face 16 of the fuel cell stack 10, which includes a substantially open face / inlet for anode feed gas to enter each fuel cell, the anode inlet stack face 212 is less open, and each fuel cell assembly 211 includes a first partial seal 212a and a partial anode inlet 216. In an exemplary embodiment, an external manifold is sealed against the anode inlet stack face 212 (not shown), and anode feed gas provided to the external manifold (not shown) enters the anode section of the fuel cell via the partial anode inlet 216. Thus, the external manifold and the partial anode inlet 216 are adjacent to the anode inlet stack face 212. Similarly, unlike the anode outlet stack face 18 of fuel cell stack 10, which includes a substantially open face / outlet (not shown) for the anode exhaust to leave each fuel cell, the anode outlet stack face 214 is not so open, and each fuel cell assembly 211 includes a second partial seal 214a and a partial anode outlet 218. Thus, the partial anode outlet 218 is adjacent to the anode outlet stack face 214.

[0038] During operation of the fuel cell stack 200, each anode layer 208 is configured to receive an anode feed gas from an anode feed gas supply (i.e., a source) at an anode inlet side 212 of the fuel cell stack 200, e.g., via an external manifold (not shown), and to output an anode exhaust at an anode outlet side 214 of the fuel cell stack 200, e.g., via another external manifold (not shown), after the anode feed gas is reacted with a cathode feed gas within the fuel cell stack 200. Specifically, each anode layer 208 includes a partial anode inlet 216 (i.e., an anode inlet opening) formed in only a portion of the anode inlet side 212 at an upstream portion of the anode layer 208. Each anode layer 208 further includes a partial anode outlet 218 (i.e., an anode outlet opening) formed in only a portion of the anode outlet side 214 at a downstream portion of the anode layer 208.

[0039] The fuel cell stack 200 further includes a cathode inlet side (or stack face) 222 and an opposing cathode outlet side (or stack face) 224 that is substantially parallel to the cathode inlet side 222. In some embodiments, the cathode layer 210 is similar in structure and operates similarly to the cathode layer 14 of the fuel cell stack 10 shown in FIG. 2. In other words, in some embodiments, the cathode feed gas may flow through the cathode layer 210 in a substantially linear direction from the cathode inlet stack face 222 to the cathode outlet stack face 224. As shown in FIG. 3, it will be appreciated that the first extended edge seal chamber 236 (in the anode layer 208) is cantilevered above the cathode inlet 226. Furthermore, the plurality of first extended edge seal chambers 236 form a series of cantilevered protrusions along the cathode inlet stack face 222. These cantilevered first extended edge seal chambers are adjacent to the anode 208 on the cathode inlet stack face 222. Similarly, a plurality of second extended edge seal chambers 246 form a series of cantilevered projections along the cathode outlet stack face 224. These cantilevered second extended edge seal chambers are adjacent to the anode 208 on the cathode outlet stack face 224.

[0040] During operation of the fuel cell stack 200, each cathode layer 210 is configured to receive a cathode feed gas from a cathode feed gas supply (i.e., a source) at a cathode inlet side 222 of the fuel cell stack 200, e.g., via an external manifold (not shown), and to output a cathode exhaust at a cathode outlet side 224 of the fuel cell stack 200, e.g., via an external manifold (not shown), after the cathode feed gas is reacted with the cathode feed gas within the fuel cell stack 200. Specifically, each cathode layer 210 includes a cathode inlet 226 (i.e., a cathode inlet opening) formed at the cathode inlet side 222 at an upstream portion of the cathode layer 210. Each cathode layer 210 further includes a cathode outlet 228 (i.e., a cathode outlet opening) formed at the cathode outlet side 224 at a downstream portion of the cathode layer 210. According to exemplary embodiments, the cathode inlet 226 and the cathode outlet 228 may extend substantially along the entire width of the cathode layer 210, while according to other exemplary embodiments, the cathode inlet 226 and / or the cathode outlet 228 may extend along only a portion of the width of the cathode layer 210.

[0041] 3, anode supply gas is supplied to the anode layer 208 and anode exhaust is output from the anode layer 208 along substantially parallel flow paths through the fuel cells and fuel cell stack. For example, anode supply gas is supplied to the anode layer 208 from an anode inlet manifold (not shown) along flow lines substantially perpendicular to the anode inlet stack face 212. Anode supply gas supplied through the partial anode inlet 216 is redirected at the anode inlet diverter (blocker or diversion face) 252 through the first extended edge seal chamber 236 and returns to the anode active area 213 of the fuel cell assembly 211, flowing substantially parallel to the flow of the cathode supply gas, then enters the second extended edge seal chamber 246 and then outputs through the partial anode outlet 218. It will be understood that a portion of the anode gas moving through the active anode section may be redirected at a first side of the anode output diverter (another blocker or bypass surface) 266 to the second extended edge seal chamber 246, and the anode gas moving through the second extended edge seal chamber 246 may be redirected at a second side of the anode output diverter 266 through the partial anode output 218.

[0042] In the previous configuration, the anode exhaust is diverted into flow lines that flow substantially perpendicular to the anode outlet stack face 214 of the fuel cell stack 200. As further shown in FIG. 3, the cathode inlet stack face 222 and the cathode outlet stack face 224 are substantially perpendicular to the anode inlet stack face 212 and the anode outlet stack face 214 of the fuel cell stack 200. In this configuration, the cathode supply gas is supplied to the cathode layer 210 and the cathode exhaust is output from the cathode layer 210 along flow paths that are substantially parallel to each other. For example, the cathode supply gas flows along flow lines that are substantially perpendicular to the cathode inlet stack face 222 and the cathode exhaust gas flows along flow lines that are substantially perpendicular to the cathode outlet stack face 224. According to an exemplary embodiment, the flow of the cathode supply gas through the cathode layer 210, once reacted and converted to cathode exhaust, flows along a substantially linear line between the cathode inlet 226 and the cathode outlet 228.

[0043] 3 have a trapezoidal footprint extending away from the anode active area bounded by one long sidewall, two shorter sidewalls, a top surface, and a bottom surface, it will be understood that the invention is not so limited. The first extended edge seal chamber 236 may have any dimension or shape that encloses a chamber that can receive anode process gas supplied via the partial anode inlet 216 and redirected by the anode inlet diverter 252, and provide that anode process gas through the anode active area inlet 272 to the anode active area 213. Similarly, the second extended edge seal chamber 246 may have any dimension or shape that encloses a chamber that can receive anode process gas supplied via the anode active area outlet 274, and provide that anode process gas through the partial anode outlet 218 (through redirection by the anode output diverter 266).

[0044] As shown in FIG. 3, the anode inlet diverter 252 extends at a non-perpendicular angle to each of the anode inlet side 212 and the cathode inlet side 222 of the fuel cell stack 200. Also shown in FIG. 3, the anode inlet diverter 252 extends in a straight linear fashion from the anode inlet side 212 toward the cathode inlet side 222. However, the anode inlet diverter 252 may be curved (concave or convex) or of other shape, so long as it redirects the anode process gas supplied through the partial anode inlet 216 to the first extended edge seal chamber 236. The anode inlet diverter 252 extends vertically along substantially the entire height of the anode layer 208. This can reduce, minimize, or even potentially eliminate the passage of anode feed gas above and / or below the anode inlet diverter 252. However, because it is difficult to form a seal between incompressible metal surfaces, in some embodiments, a small portion of the anode supply gas may still pass above and / or below the anode inlet diverter 252 into the anode layer 208.

[0045] Similarly, the anode outlet diverter 266 extends at a non-perpendicular angle to each of the anode outlet side 214 and the cathode outlet side 224 of the fuel cell stack 200. Although the anode inlet diverter 252 shown in FIG. 3 extends in a straight linear fashion from the anode outlet side 214 to the cathode outlet side 224, the anode inlet diverter 252 may be curved (concave or convex) or of other shape so long as it redirects the anode process gas provided through the partial anode outlet 218 and through the second extended edge seal chamber 236. The anode outlet diverter 266 extends vertically along substantially the entire height of the anode layer 208. Similar to the anode inlet diverter 252, the anode outlet diverter reduces or minimizes the passage of anode outlet gas above and / or below the anode outlet diverter 266. However, because it is difficult to form a seal between incompressible surfaces, in some embodiments there may be some flow of anode exit gas above and / or below the anode exit diverter 266.

[0046] Referring back to FIG. 2, it will be understood that as a process gas flows through a fuel cell, the composition of that gas changes as it travels through the fuel cell and reacts with other process gases within the fuel cell. Thus, the composition of the anode process gas flowing through the fuel cell stack 10 (of FIG. 2) changes as it travels from the anode inlet side 16 to the anode outlet side 18 of the stack. However, the composition of the cathode process gas entering the fuel cell stack 10 is uniformly distributed along the width of the cathode layer 14 (measured from the anode inlet side 16 to the anode outlet side 18 of the fuel cell stack 10). In contrast, during operation of the embodiment shown in FIG. 3, the anode process gas enters the anode active area 213 through the active anode inlet 272, rather than through an opening across the anode inlet side 212 of the fuel cell stack 200 (as shown in FIG. 2). Similar to the fuel cell stack 10 (of FIG. 2), the cathode process gas enters the fuel cell stack 200 (at the cathode inlet side 222) with a substantially uniform flow distribution along the entire width of the cathode layer 210 (measured from the anode inlet side 212 to the anode outlet side 214 of the fuel cell stack 200). Thus, the composition of the anode process gas entering the anode active area 213 and the composition of the cathode process gas entering the cathode layer 210 are substantially uniform across the width of the fuel cell stack 200 (measured from the anode inlet side 212 to the anode outlet side 214 of the fuel cell stack 200). As discussed below, the uniform composition distribution of the process gas entering the stack substantially parallel (along the width of the cathode inlet) allows for a more uniform distribution of current density across the cathode inlet area, instead of higher current density proximate the anode inlet side 16 and cathode inlet side 20 of the stack 10 (region I of FIG. 2) and lower current density away from the inlets.

[0047] 4A is a plan view of a fuel cell stack 200 with the top surface of the anode layer 208 (of the top fuel cell assembly 211) removed to show (a) the anode supply gas entering the anode active area 213 from the first extended edge seal chamber 236, and (b) the anode exhaust from the anode active area 213 entering the second extended edge seal chamber 246. The flow of anode process gas (entering as anode supply gas and exiting as anode exhaust) across the anode active area in a substantially linear manner parallel to the flow of cathode process gas through the cathode layer 210 of the fuel cell assembly 211. As discussed above, this flow arrangement may be described as parallel flow.

[0048] FIG. 4B shows the anode process gas flow through the fuel cell assemblies in a reverse flow direction. FIG. 4B is a plan view of the fuel cell stack 300 with the top surface of the anode layer 308 (of the top fuel cell assembly 311) removed. Similar to the fuel cell stack 200 and fuel cell assembly 211, the anode process gas enters the fuel cell stack 300 / fuel cell assembly 311 from the anode inlet side perpendicular to the side where the cathode process gas enters, the anode process gas exits on the opposite side to the anode inlet side, and the cathode process gas exits on the opposite side to the cathode inlet side. The anode process gas enters the anode inlet side of the fuel cell assembly 311 through a partial anode inlet 316, similar to the partial anode inlet 216 (of the fuel cell assembly 211). However, the partial anode inlet 316 is closer to the stack corner between the anode inlet side and the cathode outlet side of the fuel cell stack 300. Meanwhile, the partial anode inlet 216 (of the fuel cell assembly 211) is proximate to the stack corner between the anode inlet side and the cathode inlet side of the fuel cell stack 200. After entering the fuel cell assembly 311, the anode process gas is diverted (by the anode inlet diverter 352) into the first extended edge seal chamber 326 (located on the cathode outlet side of the fuel cell assembly 311) and further diverted towards the anode active area 313. The reacted anode process gas exits the anode active area 313 and enters the second extended edge seal chamber 346, where it is diverted towards the anode output diverter 366 and the anode partial outlet 318. In this configuration, the anode process gas traverses the anode active area 313 in a direction substantially parallel to but opposite to the cathode process gas traversing through the cathode layer of the fuel cell assembly 311.

[0049] In either flow configuration (parallel flow or counter flow), the distribution of each of the anode supply gas and cathode supply gas is substantially laterally uniform across the fuel cell stack in the direction from the anode inlet side to the anode outlet side, providing a one-dimensional distribution of current density across the fuel cell stack (measured from the cathode inlet to the cathode outlet).

[0050] It will be understood that the parallel flow configuration shown in Figure 4A and the counter flow configuration shown in Figure 4B can utilize the same external manifold arrangements as described herein with respect to fuel cell stack 10 (shown in Figure 2). Alternatively, the counter flow configuration can be achieved in the embodiment of Figure 4A by re-directing the anode process gas through the fuel cell stack (e.g., switching the anode inlet manifold with the anode outlet manifold) or by re-directing the cathode process gas through the fuel cell stack (e.g., switching the cathode inlet manifold with the cathode outlet manifold).

[0051] 4C is a plan view of the cathode layer 210 (of the fuel cell assembly 211) with the cathode electrode removed to show the cathode active area 2113. During operation, a cathode process gas traverses the cathode active area 2113 in a substantially linear path from the cathode inlet side to the cathode outlet side. A first cathode edge seal 2115 prevents the cathode process gas from entering the anode inlet side of the fuel cell assembly 211, e.g., the anode inlet manifold (not shown). A second cathode edge seal 2117 prevents the cathode process gas from entering the anode outlet side of the fuel cell assembly 211, e.g., the anode outlet manifold (not shown).

[0052] 4D is a plan view of the anode layer 208 (of the fuel cell assembly 211), with a major portion of the top surface covering the anode active area 313 and the extended edge seal chambers 236, 246. In operation, as described in detail above, the anode process gas enters the first extended edge seal chamber 236 and traverses the anode active area 313 in a substantially linear path from the cathode inlet side to the cathode outlet side (of the fuel cell assembly 211). The first anode edge seal 3115 prevents the anode process gas from entering the cathode inlet side of the fuel cell assembly 211, e.g., the cathode inlet manifold (not shown), as the anode process gas travels from the partial anode inlet 216 to the first extended edge seal chamber 236 and the anode active area 313. The second anode edge seal 3117 prevents the anode process gas from entering the cathode outlet side of the fuel cell assembly 211, e.g., the cathode outlet manifold (not shown), as the anode process gas travels from the anode active area 313 to the second extended edge seal chamber 246 and the anode portion outlet 218.

[0053] It should be appreciated that according to yet another exemplary embodiment, the cathode layer 210 may be configured in substantially the same manner as, and instead of, the anode layer 208, such that an extended edge seal chamber associated with the cathode inlet (e.g., a "cathode inlet chamber" or first extended edge seal chamber 236) is disposed on a side of the stack adjacent to (and perpendicular to) the cathode inlet side 222 and configured to cooperate with an inlet diverter in the cathode layer 210 to redirect the cathode supply gas therein substantially parallel to the anode supply gas received directly at the anode inlet side 212 of the stack. Similarly, an extended edge seal chamber associated with the cathode outlet (e.g., a "cathode outlet chamber" or second extended edge seal chamber 246) may be disposed on a side of the stack opposite the cathode inlet chamber and configured to cooperate with an outlet diverter in the cathode layer to redirect the cathode exhaust from the fuel cell stack 200.

[0054] In this discussion, fluid communication between elements refers to the ability of a fluid (gas and / or liquid) to flow between two elements. Direct fluid communication refers to a fluid that can pass between two elements without passing through another intervening element. Indirect fluid communication refers to a fluid that moves from a first element to a second element by passing through an intervening element. For example, in FIG. 3, partial anode inlet 216 is in direct fluid communication with extended edge seal chamber 236. Partial anode inlet 216 is in indirect fluid communication with anode layer 208 through extended edge seal chamber 236. Note that if a baffle structure is present at the interface between the extended edge seal chamber and the anode, the extended edge seal chamber may be in indirect fluid communication with the anode through the baffle. Alternatively, if the baffle is located entirely within the extended edge seal chamber, a portion of the extended edge seal chamber may be in direct fluid communication with the anode.

[0055] Baffle construction and manufacturing tolerances One method for forming a molten carbonate fuel cell, such as the fuel cell shown in any of Figures 1-4, is to build the fuel cell in layers and then compress the layers together to seal the fuel cell and form the desired electrical contacts. However, the manufacturing tolerances involved in this type of layered structure can present challenges when attempting to add baffles to the anode (or cathode) flow field to achieve a desired pressure drop.

[0056] In molten carbonate fuel cells, the height of the anode flow field can typically be 1.0 mm to 4.0 mm, or 1.0 mm to 3.0 mm, or 1.3 mm to 4.0 mm, or 1.3 mm to 3.0 mm. The height of the flow field can be selected based on the design of the anode collector (or cathode collector). For example, in some embodiments, the anode collector can correspond to a plate-like structure with protrusions that provide gaps that allow gas to pass through the anode collector to the pores of the anode. A separator plate is then compressed onto the anode collector. In such embodiments, the height of the flow field can roughly correspond to the height of the protrusions, or alternatively, depending on the configuration, can correspond to the thickness of the plate-like structure in addition to the height of the protrusions. In some embodiments, baffles can be present on the plate-like structure in the gaps between the protrusions. In such embodiments, the height of the flow field at the location of the baffles can correspond to the height of the protrusions.

[0057] Due to limitations in the nature of how sheet metal can be processed to form the various fuel cell layers, the height of the anode flow field can vary by + / - 0.025 mm. When forming a solid cylinder (or other shape) for use as a baffle, the size of the baffle can also vary by + / - 0.025 mm. Thus, when attempting to insert a baffle while providing the desired gap in the flow field, the combination of the two tolerances means that the size of the gap can vary by as much as 0.05 mm.

[0058] In various embodiments, improved uniformity in the anode flow may be achieved by using baffles to generate a pressure drop of 0.1 kPa to 1.0 kPa between the extended edge seal volume and the anode. To achieve this level of pressure drop, the baffle must block 94% or more of the cross-sectional area of ​​the flow field such that the available cross-sectional area for fluid flow is 0.5% to 6.0%, or 0.5% to 4.0%, or 0.5% to 2.5% of the original flow field cross-sectional area. In embodiments where there is additional available cross-sectional area at the end of the baffle furthest from the gas inlet / outlet location, the available cross-sectional area may be 0.5% to 2.5%, or 0.5% to 4.0%, or 0.5% to 6.0% of the total cross-sectional area of ​​the flow field. In other embodiments, it may be desirable to have the baffle restrict flow along the entire length of the baffle. In such other embodiments, it may be desirable to block 97.5% or more of the cross-sectional area of ​​the flow field. In other such embodiments, the available cross-sectional fluid flow area may be between 0.5% and 2.5% of the total cross-sectional area of ​​the flow field at the baffle location.

[0059] In various aspects, it has been found that the flow patterns and / or general operation of a molten carbonate fuel cell may be improved by including an improved baffle structure in the anode and / or cathode flow fields. The improved baffle structure may occupy the full height of the flow field, so that the pressure drop is managed based on apertures (such as perforations) in the baffle. This is in contrast to traditional baffle designs, where the pressure drop across the baffle may be determined based on the baffle height, which is less than the height of the flow field and therefore gas may flow above / below the baffle.

[0060] The baffle may be formed from any convenient material that does not degrade in the presence of the anode input flow, such as stainless steel. The apertures may be formed in the baffle by a technique with low size variability, such as photochemical etching, which has a size variability tolerance of 0.001 inch (0.025 mm). The apertures may correspond to holes, slots, or other convenient shapes having the desired cross-sectional area. After the apertures are formed, conventional methods, such as using a press brake and tooling dies, may be used to form the sheet metal into the desired baffle shape.

[0061] The baffle may be formed in any convenient shape that allows for the formation of apertures that allow gas flow while blocking the entire height of the flow field. An example of a suitable shape for the baffle may be a V-shaped baffle oriented such that the bottom of the "V" is closest to the anode during assembly. In the case of a rigid or incompressible baffle, the baffle may have the same height as the flow field, so that when the fuel cell is assembled, substantially all of the flow field (except for the apertures) is blocked by the baffle. In the case of a compressible baffle, the baffle may have a height of about 0.1 mm to 0.2 mm greater than the height of the flow field. When the fuel cell is assembled, the baffle may be compressed such that the compressed baffle substantially matches the height of the flow field. In such an embodiment, the top of the baffle structure may include a tab or flange that serves as an initial contact point with the layer above the baffle during assembly of the fuel cell. For example, in the case of a V-shaped baffle, an additional tab or flange may be present at the top of each arm of the baffle. It should also be noted that the compressible nature of the baffle can be beneficial to any small changes in flow field height that may occur during operation of the fuel cell, such as changes in flow field height due to differential thermal expansion of various elements.

[0062] Figure 5 shows an example of a baffle that may include multiple apertures to manage the flow of gas through the baffle. In Figure 5, the baffle 510 is in the gap between the curved protrusions 520 of the anode collector structure 501. The baffle 510 is shown as a V-shaped baffle, although other convenient shapes that allow for the formation of apertures to allow gas flow may be used.

[0063] In some embodiments, the location of the baffle (i.e., the gap between the curved protrusions 520 of the anode collector structure 501) may be substantially aligned with the interface between the extended edge seal volume and the active area of ​​the anode. In other embodiments, the baffle location may be completely within the extended edge seal volume. Using either positioning, the baffle may provide a flow restriction (i.e., a pressure drop) so that the anode input flow gas is substantially uniformly distributed throughout the extended edge seal volume before passing through the baffle and entering the anode. By substantially aligning the baffle with the interface between the extended edge seal volume and the active area of ​​the anode, or by positioning the baffle completely within the extended edge seal volume, current density variations may be reduced or minimized. If the baffle is placed such that the anode input flow can contact a substantial portion of the anode active area before passing through the baffle, the contacted portion of the anode active area will be exposed to the anode input flow at an increased pressure compared to the remainder of the anode active area. This will contribute to non-uniformity in current density. Note that positioning the baffle such that the anode input flow is still within the extended edge seal volume after it has passed the baffle can potentially reduce the available volume within the extended edge seal volume to hold the anode input flow before it passes through the baffle. In aspects in which a baffle is located within an extended edge seal chamber, the portions of the chamber volume on either side of the baffle can be referred to as separate chamber volumes.

[0064] In the example shown in FIG. 5, the bottom of the baffle 510 rests on the plate-like bottom surface of the anode collector structure 501. The top of the baffle 510 includes a top surface 512 that corresponds to a flange or tab extending from the side wall 540. The top surface 512 of the baffle 510 is slightly higher than the curved protrusions 520 that are used to contact the separator plate (not shown). For example, the top surface 512 of the baffle 510 can be higher than the top surfaces of the curved protrusions 520 by a compressed height 514 of about 0.002 inches to 0.01 inches (about 0.04 mm to 0.25 mm). The top surface 512 of the baffle 510 can be compressed such that the baffle has the same height as the curved protrusions 520 when the fuel cell is assembled. This means that the baffle can also have the same height as the total height of the flow field 530 of the anode input flow. The use of compressible baffles can reduce or minimize problems associated with manufacturing tolerances because variations in height of the top surface of the compressible baffle, such as 0.025 mm (about 0.001 inches), do not substantially change the operation of the compressible baffle. Instead, such variations in height primarily change the amount of compression of the baffle in the fuel cell assembly.

[0065] Alternatively, incompressible baffles may also be used. FIG. 6 shows an example of an incompressible baffle 610. The incompressible baffle of FIG. 6 may be placed in the gap between the curved projections 520, similar to FIG. 5. However, the height of the sidewalls 640 of the incompressible baffle 610 may be substantially the same as the height of the flow field, such that substantially the entire flow field is blocked, except for the apertures in the baffle. Thus, the height of the incompressible baffle 610 may correspond to the flow field height defined by the distance from the bottom surface 660 of the anode collector (or cathode collector) and the surface of the adjacent separator plate 670. Again, any convenient shape may be used for the incompressible baffle 610, so long as apertures can be formed in the baffle to provide the desired cross-sectional area for fluid flow. It is noted that for the incompressible baffle, baffles having a single wall shape or a solid shape may be suitable, so long as apertures can be formed.

[0066] To allow gas to pass through a baffle such as the baffles shown in Figures 5 or 6, apertures (not shown) can be drilled, etched, or otherwise formed in sidewall 540 of baffle 510 or sidewall 640 of baffle 610. The apertures can be seen in Figure 7, which shows a perspective view of baffle 510. As shown in Figure 7, apertures 750 correspond to openings that are substantially uniformly distributed along the length of baffle 510. Although the apertures in Figure 7 are shown as being located at an elevation approximately midway between the top and bottom of the flow field, other convenient heights and / or patterns for varying heights may be used.

[0067] In embodiments in which the baffle may be compressed, the sheet metal used to form the baffle shape may have a thickness of about 0.25 mm to 0.40 mm. The thickness of the sheet metal may be selected such that the baffle will be compressed during the fuel cell fabrication process to conform to the height of the flow field. Because the fuel cell fabrication process may typically include pressing fuel cell layers together under pressures of 100 kPa to 200 kPa, the thickness of the sheet metal may be selected to be thin enough to be compressed under pressures of 100 kPa to 200 kPa.

[0068] The apertures of the baffle may have a total cross-sectional area corresponding to 0.5% to 2.0% of the area of ​​the flow field. The area of ​​an individual aperture may vary depending on the number of apertures relative to the length of the baffle. This is one of the advantages of using apertures because the size of the apertures can be selected to reduce or minimize the effects of manufacturing variability. As the size of the apertures increases, a desired reduction in the available cross-sectional area for the flow field can be maintained by decreasing the number of apertures. In contrast, when using solid baffles, the size of the gap between the baffle and the surface above the baffle is dictated by the desired cross-sectional area, so there is little or no ability to adjust the solid baffle configuration to mitigate problems due to manufacturing variability.

[0069] Based on manufacturing tolerances, it may be beneficial to have apertures with a characteristic dimension of 0.25 mm or more, or 0.5 mm or more, or 0.7 or more, for example up to 1.5 mm (or possibly larger), so that manufacturing variations do not substantially affect the area of ​​the individual apertures. For substantially round apertures, the characteristic dimension may correspond to the diameter. For apertures with an elliptical, rectangular, or rectangular shape, the characteristic dimension may correspond to the shortest axis or shortest side. As mentioned above, techniques such as photochemical etching can create features with variations of 0.025 mm or less. By using a characteristic dimension of 0.25 mm or more (or 0.5 mm or more, or 0.7 mm or more) for the apertures, any manufacturing variations in the apertures will result in a variation of less than + / - 10% in the characteristic dimension. In the limiting case of round apertures, a variation of + / - 10% in the characteristic dimension corresponds to a variation of approximately + / - 20% in the area. This is in contrast to the situation with solid baffles, where the combination of variations in the manufacture of the baffle (+ / - 0.025 mm) and variations in the flow field height of the assembled fuel cell (+ / - 0.025 mm) can correspond to up to 60% or more of the desired gap between the baffle and the separator plate above it. For example, for an anode flow field having a height of 4.0 mm, a gap corresponding to 2% of the flow field height would correspond to 0.08 mm. The total tolerance variation of the flow field height and the baffle height is 0.05 mm, which means that the gap formed between the baffle and the separator plate above it can vary by as much as + / - 60%.

[0070] Figure 17 shows examples of four different types of aperture patterns for a baffle. In Figure 17, a top-down view of four different V-shaped baffles is shown. Generally, the apertures on the two sides of the "V" are not aligned, so that any gas flow passing through an aperture on one side of the baffle must travel laterally within the baffle before exiting the aperture on the other side. In other embodiments, one or more apertures on the two sides of the "V" can be aligned, which can result in channeling of the gas flow.

[0071] Baffle 1710 corresponds to a V-shaped baffle where the aperture pattern is different on the two sides of the V. Baffle 1710 represents a baffle where apertures 1712 and 1714 are 0.032 inches (0.81 mm) in diameter. Apertures 1714 are spaced apart by 0.233 inches (5.9 mm), while apertures 1712 are spaced apart by 0.466 inches (11.8 mm).

[0072] Baffle 1720 corresponds to a V-shaped baffle where the size and aperture pattern is the same on both sides of the V, but the apertures are still offset between the two sides of the V. Baffle 1720 represents a baffle where apertures 1722 are 0.032 inches (0.81 mm) in diameter. 1722 are spaced apart from each other by 0.466 inches (11.9 mm).

[0073] Baffle 1730 corresponds to a V-shaped baffle where the aperture pattern is different on the two sides of the V. Baffle 1730 represents a baffle where apertures 1732 and 1734 are 0.030 inches (0.76 mm) in diameter. Apertures 1734 are spaced apart 0.233 inches (5.9 mm) from each other, while apertures 1732 are spaced apart 0.698 inches (17.7 mm) from each other.

[0074] Baffle 1740 corresponds to a V-shaped baffle where the size and aperture pattern is the same on both sides of the V, but the apertures are still offset between the two sides of the V. Baffle 1740 represents a baffle where the apertures 1742 are 0.030 inches (0.76 mm) in diameter. The apertures 1742 are spaced apart from each other by 0.233 inches (5.9 mm).

[0075] In terms of the relative resistance to gas flow of the baffle configurations shown in FIG. 17, baffle 1740 provides the lowest gas flow resistance (i.e., lowest pressure drop) because baffle 1740 has the greatest amount of cross-sectional area available for gas to pass on both sides of the baffle. Baffles 1710 and 1720 provide a similar level of resistance based on the lowest cross-sectional area side where the area of ​​the apertures in both baffles is roughly the same. Note that baffle 1710 presents slightly less resistance to gas flow based on the greater number of baffles on one of the sides of the V. Baffle 1730 represents the baffle with the highest resistance to gas flow.

[0076] Baffles for integrated reforming units In some embodiments, the baffles described herein may also be used to manage flow patterns in a reforming unit integrated into a molten carbonate fuel cell stack. The baffles described herein may be used to allow co-current or counter-current flow within the fuel cells in the fuel cell stack while providing improved flow uniformity and / or reaction rate uniformity across the fuel cells. During such co-current or counter-current operation, the pattern of heat generated within the fuel cells differs from the pattern of heat generated within the fuel cells during cross-flow operation. It may be desirable to develop flow patterns within the integrated reforming unit that allow heat consumption within the reforming unit to take advantage of heat generation patterns within adjacent and / or nearby fuel cells. The baffles described herein, in combination with appropriate selection of reforming catalyst patterns, may assist in developing such flow patterns within the reforming unit.

[0077] When a fuel cell is operated with co-current or counter-current flow in the anode and cathode, the corresponding pattern of heat generation in the fuel cell can be approximately aligned with an axis corresponding to the direction of the co-current or counter-current flow. The use of baffles to separate the extended edge wet seal volume from the anode or cathode can further help reduce or minimize the tendency of gas to flow directly from the gas inlet to the gas outlet in the anode and / or cathode. As a result, the use of baffles can further align the heat generation pattern in a fuel cell operating in a co-current or counter-current flow mode with an axis corresponding to the direction of the co-current or counter-current flow.

[0078] Based on aligning the heat production patterns in the fuel cell with the axis of co-current or counter-current flow, it may be beneficial for any integrated reforming unit in the fuel cell stack to have a heat consumption pattern that is increased in alignment with the axis of flow in the fuel cell. One approach to accomplish this may be to introduce the hydrocarbons for reforming along the same inlet face of the fuel cell stack as the inlet face for either the cathode or anode flow.

[0079] In some embodiments, the baffles described herein may then be used in a reforming unit in a manner similar to how the baffles are positioned in the anode or cathode. In other words, the baffles may be used to define an inlet volume into which the hydrocarbons for reforming enter and are distributed along the length of the volume before contacting any reforming catalyst. The hydrocarbons may then flow across the reforming catalyst through apertures in or around the ends of the baffle. After reforming, the reformed products may pass through or around a second baffle before exiting the reforming unit. Note that the reforming unit does not include an extended volume. Instead, the inlet and outlet volumes in the reforming unit are within the footprint of the fuel cell stack.

[0080] By using baffles to modify the flow pattern within the reforming unit, various corresponding reforming catalyst patterns may be suitable within the reforming unit. In some embodiments, a relatively constant density of reforming catalyst may be used in the region between the baffles. In other embodiments, a gradient of catalyst density may be used such that the density of reforming catalyst is lower near the input baffle and gradually increases until it reaches a maximum near the output baffle. Still other options for the reforming catalyst pattern may also be suitable. The catalyst pattern may be achieved in any convenient manner. For example, a desired uniform catalyst density, or a gradient of catalyst density, may be achieved by depositing small particles of catalyst in a desired pattern on the bottom and / or top surface of the reforming unit. In various embodiments, any convenient type of reforming catalyst may be used.

[0081] Flow Pattern Example FIG. 8 illustrates an example of the desired operation of a fuel cell when the anode flow input is redirected to allow for co-flow or counter-flow operation. In FIG. 8, a top cross-sectional view of the fuel cell is shown with the anode flow field corresponding to the top layer. In FIG. 8, the anode input flow 801 is introduced into an inlet volume 805. The inlet volume 805 includes a blocker 810 that redirects the anode input flow 801 into an extended edge seal area 820. The dashed line 830 indicates the location of the baffle that creates a sufficient pressure drop to allow the anode input flow 801 to distribute across the extended edge seal area 820 before passing through the baffle. The dotted line 832 represents the active area of ​​the anode. As shown in FIG. 8, the baffle location 830 is selected such that the anode input flow 801 passes through the baffle before reaching the active area of ​​the anode. The anode input flow 801 is substantially evenly distributed over the entire length of the anode as the gas flow passes through the active area of ​​the anode. Dashed line 840 indicates the location of a second baffle that provides a second pressure drop to further assist in maintaining an even distribution of gas flow across the active area of ​​the anode. Blocker 850 reduces, minimizes, or prevents direct passage of gas flow from the anode active area to the anode outlet volume 860. Instead, anode output flow 861 is formed by gas passing through the second baffle (located at position 840) and into the extended edge seal area 870.

[0082] A series of tests were performed in which air was passed through various anode flow field configurations to test the gas flow patterns within the active area of ​​the anodes of various configurations. During the tests, the flow patterns through the cell were determined by passing two types of air flows through the cell with diazo paper on the bottom surface of the anode flow field. The flow field had a total height (plate thickness + projection height) of about 2.3 mm. However, the plate thickness was not included for the flow field height at the baffle position, since the baffle was on the bottom plate of the anode collector at the baffle position. Thus, at the baffle position, the flow field height was about 2.0 mm. A first air flow, corresponding to air without further additives, was passed through the cell under controlled conditions and vented to atmosphere at the cell's outlet. This first air flow had a sufficient volume to establish the flow patterns within the cell. A second air flow, saturated with ammonium hydroxide, was introduced at a series of ports machined into the flow test fixture. Trace air enriched with ammonium hydroxide turned the diazo paper blue, indicating the direction in which the air was flowing. This microflow was less than 1% of the flow and therefore did not affect the flow direction. The ammonium hydroxide was consumed by reaction with the diazo paper, so by introducing a microflow through a series of ports, the flow patterns could be traced at multiple points within the cell. The concentration of ammonium hydroxide across the paper affected how dark the flow streams appeared. If there was more air flow in a particular area of ​​the cell, the concentration of ammonium hydroxide was lower and the flow streams appeared lighter and lighter. If there was less air flow, the higher the concentration of ammonium hydroxide, the darker and darker the flow streams appeared. This technique was used to evaluate a series of baffle designs and a CFD (computational fluid dynamics) model was calibrated using the results of the flow tests to find the optimized baffle configuration.

[0083] FIG. 9 shows results from a configuration using a blocker to divert the input flow to an extended edge seal area and a baffle containing apertures to achieve a pressure drop of 0.1 kPa or more. In FIG. 9, the input flow 901 is diverted by a blocker 910 to an extended edge seal area 920. Baffles containing apertures to accommodate the full height of the flow field but to allow fluid flow were placed at positions 930 and 940. The apertures provided an available cross-sectional area corresponding to 2.5% or less of the original flow field such that the pressure drop across the baffle was 0.1 kPa or more. As shown in FIG. 9, this resulted in a gas flow pattern that may be substantially parallel to the cathode gas flow during operation. Based on the measured flow patterns, CFD simulations were performed to model the operation of the fuel cell. The CFD simulations showed improved uniformity of the current density across the fuel cell.

[0084] Note that in Figure 9, some flow occurred across blocker 910. This is due to the difficulty in forming a complete seal of a fixed height blocker when assembling the fuel cell. As shown in Figure 9, this was a relatively low volumetric flow and therefore did not pose a problem for improving the uniformity of the current density during the CFD simulation. A similar low volumetric flow across blocker 950 was also observed.

[0085] A series of comparative configurations were also investigated to illustrate the advantages of configurations such as that of FIG. 9. FIG. 10 shows the results of flow testing for the first comparative configuration. In FIG. 10, no blockers were used to redirect the input flow to the extended edge wet seal area. Instead, the input flow 1001 was allowed to enter above the anode active area. A solid (cylindrical) baffle was used to block a portion of the flow field. The height of the baffle was about 1.6 mm. Compared to the flow field height of 2.0 mm at the baffle location, this corresponds to blocking about 80% of the total cross-sectional area of ​​the flow field. The locations used for the baffles are indicated by dashed lines 1030 and 1040. As shown in FIG. 10, the baffle locations 1030 and 1040 are within the anode active area. Additionally, in the example shown in FIG. 10, the baffles blocked no more than 80% of the flow field such that the pressure drop across each baffle was less than 0.1 kPa. As shown in FIG. 10, because there was not enough pressure drop across the baffle, the flow pattern clearly shows corner-to-corner flow within the anode rather than side-to-side flow (which may be parallel to the cathode flow during operation).

[0086] FIG. 11 shows the results of flow testing for a second comparative configuration. In FIG. 11, a larger solid cylindrical baffle was used, reducing the available cross-sectional area of ​​the flow field to 2.0% of the original cross-sectional area. Again, no blockers were used and the baffles were placed at locations 1130 and 1140, which are above the active area of ​​the anode during operation. As shown in FIG. 11, a pressure drop of more than 0.1 kPa was achieved by reducing the available cross-sectional area for fluid flow to 2.0% or less. This resulted in the flow pattern shown in FIG. 11, which may be substantially parallel to the cathode flow during operation. However, as shown in FIG. 11, the baffle locations 1130 and 1140 were above what may be the active area of ​​the anode during operation. CFD modeling of fuel cell performance using the configuration shown in FIG. 11 showed poor uniformity in current density. This was partially due to the input flow being retained before passing through the first baffle while still above the active area. Similar non-uniformity was observed on one side of the second baffle.

[0087] Based on CFD modeling performed using the flow results shown in Figures 9-11, substantial improvements in current density could be achieved in fuel cells by using a blocker to divert the input flow to the extended edge seal area and using a baffle to provide a pressure drop of 0.1 kPa or more for gas passing from the extended edge seal area to the anode active area (or from the anode active area to the second extended edge seal area).

[0088] During flow testing, an additional difficulty in using baffles to achieve the desired pressure drop was also discovered. Based on limitations in manufacturing technology, the height of the anode flow field of a molten carbonate fuel cell has a tolerance of + / - 0.025 mm. For solid baffles, the height of the baffle has a similar tolerance of + / - 0.025 mm. Because this variation was similar in magnitude to the desired gap between the baffle and the separator plate, it was discovered that the accumulation of manufacturing tolerances could cause substantial variation in the pressure drop across the baffle during fuel cell operation.

[0089] Figure 12 shows an example of a solid cylindrical baffle placed in the flow field of the anode input flow of a flow battery. While Figure 12 is not necessarily to scale, the figure illustrates the problems associated with trying to control the formation of gaps on the order of 0.1 mm in height using baffles on the order of 1-10 mm in height.

[0090] To further investigate this difficulty, a series of tests were performed to determine how much the pressure drop changed as a function of gap height. FIG. 13 shows the results from these tests. As shown in FIG. 13, for a 2.0 mm flow field, the desired pressure drop was about 0.1 kPa (or about 0.4 inches of water) when the gap height between the baffle and the separator plate was 0.1 mm (about 0.004 inches). However, due to manufacturing variability as described above, building a fuel cell to have a desired gap height of 0.1 mm may result in an actual gap of 0.05 mm to 0.15 mm (about 0.002 inches to 0.006 inches). As shown in FIG. 13, this means that the pressure drop across the baffle during operation may range from about 0.06 kPa to 0.24 kPa. This would mean that the flow rate could vary by as much as a factor of four between different fuel cells. This substantial variability would result in poor and / or unpredictable performance of fuel cells manufactured using solid baffles.

[0091] In an effort to mitigate the effects of manufacturing variability, different baffle shapes were tested. FIG. 14 shows an example of a trapezoidal shaped baffle, with the long side of the trapezoid at the top. For a round baffle, the flow constriction occurs at a single point corresponding to the top of the cylinder. In contrast, the trapezoidal shaped baffle provides flow restriction along the entire width of the top surface. Based on the longer path length of the constricted flow, the trapezoidal shaped baffle was able to generate the same desired pressure drop of 0.1 kPa with a gap height between the baffle and the separator plate of about 0.23 mm, or more than twice the gap height of the cylindrical baffle. However, even with the larger gap height, variations due to manufacturing tolerances still resulted in a potential variation in pressure drop between different fuel cells of nearly 100%. This is shown in FIG. 15.

[0092] As noted above, forming apertures with a characteristic dimension of 0.25 mm or more (or 0.5 mm or more, or 0.7 mm or more) results in a size variation of 20% or less. Additionally, the magnitude of this size variation can be further reduced by using larger aperture sizes, such as with a variation of 10% or less for apertures with a characteristic dimension of 0.5 mm or more. In contrast, even with trapezoidal baffles, the gap height variation due to manufacturing tolerances was greater than 20%. Thus, by using apertures to control the available cross-sectional area for fluid flow, a substantial reduction in manufacturing variability can be achieved such that fuel cell performance can be maintained more consistently from cell to cell.

[0093] Example of a reforming unit FIG. 16 shows an example of a baffle configuration for use in a reforming unit. In FIG. 16, the hydrocarbon input 1610 for the reforming unit enters the fuel cell stack on the same side as the reforming outlet 1620. When the hydrocarbon input for reforming enters the reforming unit via the hydrocarbon input 1610, the hydrocarbon is first passed through the inlet volume 1630. Preferably, the inlet volume does not contain any reforming catalyst. This allows the hydrocarbon to distribute along the length of the inlet volume 1630 before undergoing any reaction with the reforming catalyst. The hydrocarbon can then enter the main volume 1640 of the reforming unit where the reforming catalyst 1645 is located. The hydrocarbon can enter the main volume by either passing through an aperture in the baffle 1650 or by passing around the end of the baffle 1650 if the length of the baffle 1650 is less than the length of the inlet volume 1630. In some embodiments, the baffle 1650 can have a length substantially the same as the length of the inlet volume 1630. In other embodiments, the length of the baffle 1650 may be 0.05% or more, or 0.5% or more, or 5% or more, or 10% or more, or 20% or more, such as up to 50% less, or even in some cases even less than the length of the inlet volume 1630. Expressed as a ratio, this corresponds to a baffle having a length of 0.9995 times or less, or 0.995 times or less, or 0.95 times or less, or 0.90 times or less, or 0.80 times or less, such as up to 0.5 times the length of the inlet volume. For example, the input baffle 1650 shown in FIG. 16 has a length of about 60% of the length of the inlet volume 1630. This results in a gap or region 1651 where there is no baffle. Note that the outlet baffle 1660 may independently have a length similar to the length of the outlet volume 1670, or a length shorter than the length of the outlet volume 1670 by any of the values ​​above.

[0094] After entering the main volume 1640, the hydrocarbons undergo reforming on the catalyst 1645 to form H 216. The reformed product is at least partially reformed by forming a reformed product such as . The reformed product may then pass through apertures in and / or around the outlet baffle 1660 (if the length of the outlet baffle 1660 is less than the length of the outlet volume 1670). The reformed product may then exit the outlet volume 1670 via the reformed outlet 1620. Note that an output blocker structure 1680 is shown in FIG. 16. The blocker structure provides another structure to directly reduce, minimize, or eliminate flow from the main volume 1640 to the reformed outlet 1620.

[0095] FIG. 18 shows an example of a baffle configuration. In the example shown in FIG. 18, the baffle configuration is used as a baffle for a reformer stack element. In FIG. 18, an initial portion 1850 of the inlet baffle corresponds to a solid blocker (still V-shaped) that does not include an aperture. A second portion 1840 of the inlet baffle corresponds to a baffle having the aperture size and pattern used in baffle 1740 of FIG. 17. The initial portion 1850 and the second portion 1840 meet at location 1801. Note that the initial portion 1850 and the second portion 1840 may correspond to a single baffle piece with different hole patterns etched in the initial portion 1850 and the second portion 1840. Alternatively, two or more pieces may be used to form the baffle. The outlet baffle 1841 corresponds to the aperture size and pattern used in baffle 1740 of FIG. 17. A solid blocker 1855 is used to prevent direct flow from the reforming active area to the outlet for the reforming element.

[0096] FIG. 19 shows another example of a baffle configuration. In FIG. 19, there is variation in the aperture size and pattern of both the inlet and outlet baffles. In the example shown in FIG. 19, the initial portion 1950 of the inlet baffle corresponds to a solid blocker that does not include apertures. The second portion 1930 (starting at position 1903) corresponds to the aperture size and pattern of the baffle 1730 from FIG. 17. The third portion 1940 (starting at position 1904) corresponds to the aperture size and pattern of the baffle 1740 from FIG. 17. For the outlet baffle, the first portion 1931 corresponds to the aperture size and pattern of the baffle 1730 from FIG. 17. The second portion 1921 (starting at position 1912) corresponds to the aperture size and pattern of the baffle 1720 from FIG. 17. A third portion 1941 (starting at location 1914) corresponds to the aperture size and pattern of baffle 1740 from FIG.

[0097] Figures 20 and 21 show temperature profiles from operation of two fuel cell stacks. In Figure 20, the average cathode temperature profile is shown for the cathode in a fuel cell stack that did not include any reforming units as an element in the stack. The fuel cell stack of Figure 20 was run at 130 mA / cm 2 current density, 50% fuel utilization, and 70% CO 2 The cathode input flow was operated at 100% CO 2 The concentration of was 8.4% by volume. The fuel cells were operated in countercurrent flow mode. For FIG. 21, a similar fuel cell stack was used, but a reformer unit was inserted every 6 fuel cells. The baffle shape shown in FIG. 18 was used in the reformer unit. The operating conditions were the same as for FIG. 20, except that the fuel utilization in FIG. 21 was 55% instead of 50%. However, based on having the same current density, it is believed that FIG. 20 and FIG. 21 provide a good comparison of the effect of including a reformer unit on the average cathode temperature profile. Note that the flow direction for the reformer unit in the stack corresponding to FIG. 21 was co-current with the anode flow direction.

[0098] As shown in Figure 20, the fuel cell stack operating without an integrated reformer unit exhibited a substantial amount of temperature variation in the average cathode temperature profile. Specifically, in two separate regions, the average cathode temperature was above 660°C, with a peak temperature of 688°C. As shown in Figure 21, adding a reformer unit as an element in the fuel cell stack (one reformer unit for every six fuel cells) resulted in a reduction in the peak temperature from 688°C to 659°C, while maintaining roughly the same minimum temperature in the fuel cell at around 590°C. The temperature profile of Figure 21 can be seen more clearly in Figure 22, which shows the average cathode temperature along a line in the center of the fuel cell that is parallel to the axis of countercurrent flow.

[0099] Further improvements in the temperature profile were achieved using the baffle configuration from Figure 19. In another test run, a fuel cell stack was used with one reformer unit per six fuel cells, but the reformer unit included the baffle configuration shown in Figure 19. The resulting temperature profile in the cathode is shown in Figure 23. As shown in Figure 23, the minimum temperature is still near 590°C, but the maximum temperature is now 620°C-630°C.

[0100] Additional Embodiments Embodiment 1. An element in a molten carbonate fuel cell stack comprising: a gas flow inlet; a first volume in fluid communication with the gas flow inlet; a second volume comprising at least a portion of an anode active area of ​​a fuel cell anode, at least a portion of a cathode active area of ​​a fuel cell cathode, or a reforming catalyst, the second volume in fluid communication with the gas flow inlet through the first volume; an inlet baffle comprising a plurality of inlet baffle apertures at an inlet boundary between the first volume and the second volume, at least a portion of the fluid communication between the first volume and the second volume comprises fluid flow through the plurality of inlet baffle apertures, a length of the inlet baffle occupies at least 60% of a length of the inlet boundary, an average height of the inlet baffle occupies 100% or more of an average height along the inlet boundary, and a combined cross-sectional area of ​​the plurality of inlet baffle apertures occupies between 0.5% and 6.0% of a total cross-sectional area at the inlet boundary; and a gas flow outlet in fluid communication with the second volume.

[0101] Embodiment 2. A fuel cell stack element as described in embodiment 1, wherein at least one of the plurality of inlet baffle apertures has a characteristic dimension of 0.25 mm or more, or each of the plurality of inlet baffle apertures has a characteristic dimension of 0.25 mm or more.

[0102] Embodiment 3. A fuel cell stack element as described in any one of the previous embodiments, wherein the total cross-sectional area of ​​the multiple inlet baffle apertures is between 0.5% and 2.5% of the total cross-sectional area at the inlet boundary, or the length of the inlet baffle is between 0.05% and 5.0% of the length of the inlet boundary, or a combination thereof.

[0103] Embodiment 4. A fuel cell stack element as in any one of the previous embodiments, further comprising: a third volume in fluid communication with the gas flow outlet, the gas flow outlet indirectly in fluid communication with the second volume via the third volume; and an outlet baffle including a plurality of outlet baffle apertures at an outlet boundary between the first volume and the second volume, wherein at least a portion of the fluid communication between the first volume and the second volume includes fluid flow through the plurality of outlet baffle apertures, a length of the outlet baffle occupies at least 60% of a length of the outlet boundary, an average height of the outlet baffle occupies 100% or more of an average height along the outlet boundary, and a combined cross-sectional area of ​​the plurality of outlet baffle apertures occupies between 0.5% and 6.0% of a total cross-sectional area at the outlet boundary.

[0104] Embodiment 5. A fuel cell stack element as described in embodiment 4, wherein the total cross-sectional area of ​​the multiple inlet baffle apertures is different from the total cross-sectional area of ​​the multiple outlet baffle apertures, or one or more inlet baffle apertures include a different characteristic dimension than one or more outlet baffle apertures, or the length of the inlet baffle is different from the length of the outlet baffle, or a combination thereof.

[0105] Embodiment 6. A fuel cell stack element as described in any one of the previous embodiments, wherein the aperture of the portion of the inlet baffle furthest from the gas flow inlet occupies 25% or more of the total cross-sectional area of ​​the inlet baffle apertures, and the portion of the inlet baffle occupies between 5% and 20% of the length of the inlet boundary.

[0106] Embodiment 7. A fuel cell stack element as described in any one of embodiments 1 to 6, wherein the second volume contains a reforming catalyst, the gas flow inlet is adjacent to the first side of the fuel cell stack, and the gas flow outlet is optionally adjacent to the first side of the fuel cell stack.

[0107] Embodiment 8. A fuel cell stack element as described in any one of embodiments 1 to 6, wherein the second volume includes at least a portion of the anode active area and associated anode flow field, the first volume includes at least a portion of the extended edge seal input chamber, the extended edge seal input chamber adjacent to a first side of the fuel cell stack, and the gas flow inlet is adjacent to a second side of the fuel cell stack.

[0108] Embodiment 9. A fuel cell stack element as described in embodiment 8, wherein the gas flow inlet further comprises an inlet flow blocker, the inlet flow blocker being positioned at an oblique angle relative to the inlet baffle, or the second volume further comprises an outlet flow blocker, the outlet flow blocker being positioned at an oblique angle relative to the inlet baffle, or a combination thereof.

[0109] Embodiment 10. A fuel cell stack element as described in any one of embodiments 1 to 6, wherein the second volume includes at least a portion of the cathode active area and associated cathode flow field, the first volume includes at least a portion of the extended edge seal input chamber, the extended edge seal input chamber adjacent to a first side of the fuel cell stack, and the gas flow inlet is adjacent to a second side of the fuel cell stack.

[0110] Embodiment 11. A fuel cell stack element as described in embodiment 10, wherein the gas flow inlet further comprises an inlet flow blocker, the blocker being positioned at an oblique angle relative to the inlet baffle.

[0111] Embodiment 12. A fuel cell stack element as described in any one of embodiments 8 to 11, further comprising an extended edge seal output chamber adjacent a third side of the fuel cell stack, a gas flow outlet in fluid communication with a first output chamber volume of the extended edge seal output chamber, and an outlet baffle including a plurality of outlet baffle apertures at an outlet boundary of the first output chamber volume, wherein a cross-sectional area of ​​the plurality of outlet baffle apertures is between 0.5% and 6.0% of a total cross-sectional flow field area at the outlet boundary, and the first output chamber volume is in fluid communication with a second volume.

[0112] Embodiment 13. A fuel cell stack element according to any one of the previous embodiments, wherein the length of the inlet baffle includes the length of the inlet boundary.

[0113] Embodiment 14. A fuel cell stack element of any one of the previous embodiments, wherein the baffle includes a V-shaped baffle having a first side and a second side, and the apertures in the first side have at least one of a different aperture size and a different aperture pattern relative to the apertures in the second side.

[0114] Embodiment 15. Use of a fuel cell stack comprising a fuel cell stack element according to any one of the previous embodiments, wherein the pressure drop across the inlet baffle in use is optionally between 0.1 kPa and 1.0 kPa.

[0115] All numerical values ​​within the detailed description and claims herein are modified by the "about" or "approximate" value indicated to take into account experimental error and variations that can be expected by one of ordinary skill in the art.

[0116] Although the present invention has been described in terms of specific embodiments, it is not necessarily so limited. Suitable changes / modifications for operation under specific conditions should be apparent to those skilled in the art. It is therefore intended that the following claims be interpreted to encompass all such changes / modifications that fall within the true spirit / scope of the present invention.

Claims

1. A fuel cell stack, comprising: a cathode input manifold adjacent to a cathode input side of the fuel cell stack; and an anode input manifold adjacent to an anode input side of the fuel cell stack that is distinct from the cathode input side; a cathode output manifold adjacent a cathode output side of the fuel cell stack that is distinct from the cathode input side and the anode input side; 1. A fuel cell comprising: an anode located on the anode input side of the fuel cell stack, the anode including an anode inlet, an extended edge seal input chamber, and an anode active area; the anode inlet is in fluid communication with the anode input manifold, and the extended edge seal input chamber is located on the cathode input side or the cathode output side, the extended edge seal input chamber is in fluid communication with the anode input and the anode active area via an anode active area inlet, and the anode active area inlet is located on the cathode input side or the cathode output side; a cathode including a cathode inlet and a cathode active area; the cathode inlet is substantially parallel to the anode inlet; an electrolyte matrix layer separating the anode and the cathode; an inlet baffle positioned adjacent to the anode active area inlet; 13. A fuel cell stack comprising: an inlet baffle including a plurality of inlet baffle apertures at an inlet boundary between the extended edge seal input chamber and the anode inlet; at least a portion of fluid communication between the extended edge seal input chamber and the anode inlet includes fluid flow through the plurality of inlet baffle apertures; a length of the inlet baffle occupies at least 60% of a length of the inlet boundary; an average height of the inlet baffle occupies 100% or more of an average height along the inlet boundary; and a combined cross-sectional area of ​​the plurality of inlet baffle apertures occupies between 0.5% and 6.0% of a total cross-sectional area at the inlet boundary.

2. A fuel cell stack as described in claim 1, wherein at least one of the plurality of inlet baffle apertures has a characteristic dimension of 0.25 mm or greater, or each of the plurality of inlet baffle apertures has a characteristic dimension of 0.25 mm or greater.

3. 2. The fuel cell stack of claim 1, wherein the total cross-sectional area of ​​the multiple inlet baffle apertures is between 0.5% and 2.5% of the total cross-sectional area at the inlet boundary, or the length of the inlet baffle is between 0.05% and 5.0% of the length of the inlet boundary less than the length of the inlet boundary, or a combination thereof.

4. A fuel cell stack as described in claim 1, wherein the length of the inlet baffle includes the length of the inlet boundary.

5. An anode outlet in fluid communication with an anode outlet manifold, the anode outlet in fluid communication with an anode flow field; an outlet baffle including a plurality of outlet baffle apertures at an outlet boundary between the anode active area and the anode outlet manifold; at least a portion of the fluid communication between the anode active area and the anode outlet manifold includes fluid flow through the plurality of outlet baffle apertures; 2. The fuel cell stack of claim 1, wherein a length of the outlet baffle comprises at least 60% of a length of the outlet boundary, an average height of the outlet baffle comprises greater than or equal to 100% of an average height along the outlet boundary, and a combined cross-sectional area of ​​the multiple outlet baffle apertures comprises between 0.5% and 6.0% of a total cross-sectional area at the outlet boundary.

6. 6. The fuel cell stack of claim 5, wherein the total cross-sectional area of ​​the plurality of inlet baffle apertures is different from the total cross-sectional area of ​​the plurality of outlet baffle apertures, or one or more inlet baffle apertures have a different characteristic dimension than one or more outlet baffle apertures, or a length of the inlet baffle is different from a length of the outlet baffle, or a combination thereof.

7. A fuel cell stack as described in claim 1, wherein the aperture of a portion of the inlet baffle furthest from the anode inlet accounts for more than 25% of the total cross-sectional area of ​​the inlet baffle aperture, and said portion of the inlet baffle accounts for 5% to 20% of the length of the inlet boundary.

8. A fuel cell stack as described in claim 1, wherein the extended edge seal input chamber is configured to receive anode inlet gas provided to the fuel cell stack from an anode input manifold in a first direction relative to the fuel cell stack, and to output the anode inlet gas to the anode inlet in a second direction substantially perpendicular to the first direction.

Citation Information

Patent Citations

  • Fuel cell

    JP1987208557A

  • Fuel cell

    JP2006179233A

  • Fuel cell and fuel cell distribution plate

    JP2006202570A

  • Fuel cell

    JP2008027749A

  • Fuel cell plate construction with baffles in the wet seal area

    JP2009532832A