Run-flat tires

The tire design addresses the challenge of balancing rolling resistance and durability by using an inner layer rubber with a lower loss tangent and strategic placement to minimize inner liner presence, achieving reduced rolling resistance and improved run-flat durability.

JP7595506B2Active Publication Date: 2024-12-06BRIDGESTONE CORP
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2021062013
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-03-31
Publication Date
2024-12-06
Estimated Expiration
2041-03-31

AI Technical Summary

Technical Problem

Run-flat tires face challenges in balancing high durability under run-flat conditions while minimizing rolling resistance, which is exacerbated by the weight and high temperature/strain conditions experienced by the side reinforcing rubber.

Method used

The tire design incorporates an inner layer rubber with a lower loss tangent than the inner liner, arranged to overlap with the inner liner by a specific width, and positioned to reduce the amount of inner liner, along with a carcass structure and belt layers to support the side reinforcing rubber, ensuring adequate load support and durability.

Benefits of technology

The design effectively suppresses rolling resistance while maintaining run-flat durability by reducing the inner liner's presence and optimizing the inner layer's properties, enhancing peeling resistance and load support.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007595506000002
    Figure 0007595506000002
  • Figure 0007595506000001
    Figure 0007595506000001
Patent Text Reader

Abstract

To provide a run-flat tire that suppresses increase of rolling resistance while ensuring run-flat durability.SOLUTION: A run-flat tire according to the present invention includes a tread part, a sidewall part, a bead part, a side reinforcing rubber, a carcass, and a belt, and has an inner liner arranged on an inner surface of the tire, and an inner-layer rubber arranged between the side reinforcing rubber and the inner liner. An outer end part of the inner liner in a tire width direction and an outer end part of the inner-layer rubber in a tire radial direction are arranged to face each other, or the outer end part of the inner liner in the tire width direction and the outer end part of the inner-layer rubber in the tire radial direction overlap with each other, with an overlap width of 30 mm or less, satisfying W2≤W1≤W2+20(mm) in a reference state. A loss tangent tan δ1 of the inner-layer rubber is 80% or less of a loss tangent tan δ2 of the inner liner.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a run-flat tire. [Background technology]

[0002] Run-flat tires having a crescent-shaped cross-section of a side reinforcing rubber on the sidewall are known as pneumatic tires (see, for example, Patent Document 1). With such run-flat tires, even if the tire is punctured and the internal pressure drops, the side reinforcing rubber takes over the load, allowing the tire to travel a considerable distance. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2011-184000 A Summary of the Invention [Problem to be solved by the invention]

[0004] While run-flat tires are required to have high durability when driving with run-flat tires, the problem is that the weight of the tires increases due to the placement of side reinforcing rubber, which leads to increased rolling resistance.In particular, when driving with run-flat tires, the innermost part of the side reinforcing rubber is subject to high temperature and strain due to large deflection, which can cause cracks in the side reinforcing rubber and reduce run-flat durability.

[0005] SUMMARY OF THE PRESENT DISCLOSURE An object of the present invention is to provide a run-flat tire which ensures run-flat durability while suppressing an increase in rolling resistance. [Means for solving the problem]

[0006] The gist and configuration of the present invention are as follows. (1) a tread portion; A pair of sidewall portions connected to both sides of the tread portion; a bead portion connected to each of the sidewall portions; A side reinforcing rubber having a crescent-shaped cross section disposed on the sidewall portion; a carcass extending in a toroidal shape between the pair of bead portions; A run-flat tire comprising: a belt having one or more belt layers disposed on a radially outer side of a crown portion of the carcass, Inner liner on the inside of the tire and inner rubber is placed, before an outer end of the inner liner in the tire width direction and an outer end of the inner layer rubber in the tire radial direction are disposed to abut against each other, or an outer end of the inner liner in the tire width direction and an outer end of the inner layer rubber in the tire radial direction are overlapped with an overlap width of 30 mm or less, an outer end portion of the inner layer rubber in the tire radial direction is located closer to the inner surface of the tire than an outer end portion of the inner liner in the tire width direction; In a standard state in which the run-flat tire is mounted on an applicable rim, inflated to a specified internal pressure, and unloaded, the width of the inner liner in the tire width direction is W1 (mm) and the width of the innermost belt layer in the tire radial direction among the one or more belt layers in the tire width direction is W2 (mm), satisfying W2≦W1≦W2+20 (mm), A run-flat tire, wherein a loss tangent tan δ1 of the inner layer rubber is 80% or less of a loss tangent tan δ2 of the inner liner.

[0007] In this specification, the term "applicable rim" refers to the standard rim (Measuring Rim in the ETRTO STANDARDS MANUAL, Design Rim in the TRA YEAR BOOK) for the applicable size which is an industrial standard valid in the region where the tire is produced and used, and which is described or will be described in the future in the JATMA YEAR BOOK of JATMA (Japan Automobile Tire Manufacturers Association), in Japan, the STANDARDS MANUAL of ETRTO (The European Tyre and Rim Technical Organisation), in Europe, and the YEAR BOOK of TRA (The Tire and Rim Association, Inc.) in the United States (i.e., the above "rim" includes not only current sizes but also sizes which may be included in the above industrial standards in the future. An example of "sizes to be described in the future" is the size described as "FUTURE DEVELOPMENTS" in the 2013 edition of ETRTO.), however, in the case of a size not described in the above industrial standards, it refers to a rim with a width corresponding to the bead width of the tire. In addition, "prescribed internal pressure" refers to the air pressure (maximum air pressure) that corresponds to the maximum load capacity of a single wheel for the applicable size and ply rating as stated in the above JATMA etc., and in the case of sizes not stated in the above industry standards, "prescribed internal pressure" refers to the air pressure (maximum air pressure) that corresponds to the maximum load capacity specified for each vehicle on which the tire is fitted. In addition, "loss tangent" refers to the ratio (E" / E') of the dynamic loss modulus E" to the dynamic storage modulus E' obtained using a dynamic tensile viscoelasticity measuring instrument on a test piece of vulcanized rubber with a thickness of 2 mm, width of 5 mm, and length of 20 mm under conditions of a temperature of 60°C, a frequency of 52 Hz, an initial strain of 2%, and a dynamic strain of 1%.

[0008] (2) The run-flat tire according to the above (1), wherein the number of repetitions until the test piece breaks is at least twice as long as that of the side reinforcing rubber when the inner layer rubber is subjected to repeated tension at a frequency of 10 Hz under conditions of 150°C using a test piece prepared by cutting out 1 mm of the center of a No. 8 dumbbell perpendicular to the direction of repeated tension of the test piece in accordance with JIS K6270:2001, and the applied tensile strain is in the range of 10% to 30%.

[0009] (3) The run-flat tire according to the above-mentioned (2), wherein in the reference state, a ratio T2 / T1 of a thickness T2 of the inner layer rubber measured in a perpendicular direction to a maximum thickness T1 at which the thickness of the side reinforcing rubber is at its maximum when measured in the perpendicular direction from the carcass to the inner surface of the tire is 0.05 to 0.30.

[0010] (4) The run-flat tire according to any one of the above (1) to (3), wherein a ratio of the elastic modulus of the inner layer rubber to the elastic modulus of the side reinforcing rubber is 0.75 or less. Here, "elastic modulus" refers to the tensile modulus of elasticity at 25% elongation at 25°C (JIS K 6251:2017) measured by processing vulcanized rubber into a dumbbell-shaped No. 8 test piece and measuring the tensile modulus at 25% elongation at a measurement temperature of 25°C. Effect of the Invention

[0011] According to the present invention, it is possible to provide a run-flat tire in which an increase in rolling resistance is suppressed while ensuring run-flat durability. [Brief description of the drawings]

[0012] [Figure 1] 1 is a partial cross-sectional view in the tire width direction of a run-flat tire according to one embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] Fig. 1 is a partial cross-sectional view in the tire width direction of a run-flat tire according to one embodiment of the present invention, Fig. 1 shows a cross-section in the tire width direction of a run-flat tire in the above-mentioned reference state.

[0014] As shown in FIG. 1, this run-flat tire (hereinafter also simply referred to as tire) 10 has a tread portion 1 made of tread rubber, a sidewall portion 2 made of a pair of sidewall rubbers continuing on both sides of the tread portion 1, and a bead portion 3 continuing to each sidewall portion 2.

[0015] 1, a bead core 3a is embedded in each bead portion 3. In this example, a bead filler 3b is disposed on the outer side of the bead core 3a in the tire radial direction.

[0016] The tire 1 further includes a carcass 4 consisting of one or more carcass plies that span a pair of bead portions 3 in a toroidal shape. In this example, the carcass ply is made of organic fiber cords. The carcass 4 consists of a carcass main body portion 4a that is engaged with the bead core, and a carcass folded-up portion 4b that extends from the carcass main body portion 4a and is folded back around the bead core 3a. In the illustrated example, the carcass folded-up portion 4b extends to a position on the inner side in the tire width direction than the belt end and terminates, forming a so-called envelope structure, but is not limited to this example, and the end of the carcass folded-up portion 4b may be located, for example, on the inner side in the tire radial direction than the maximum tire width position.

[0017] A belt 5 consisting of one or more belt layers 5a, 5b (two layers in the illustrated example) is disposed on the radially outer side of the crown portion of the carcass 4. The belt cords of the two belt layers extend so as to cross each other between the layers, and the belt cords can extend at an inclination angle of 30 to 60° with respect to the tire circumferential direction, for example. The belt cords are steel cords in this example.

[0018] In addition, this tire 1 is provided with a side reinforcing rubber 6 having a crescent-shaped cross section on the sidewall portion 2. By providing such a side reinforcing rubber 6, the side reinforcing rubber 6, which contributes to supporting the vehicle weight, enables the vehicle to travel safely for a certain distance even in a state where the internal pressure of the tire is reduced due to a puncture or the like. In the illustrated example, the side reinforcing rubber 6 has a shape in which the thickness in the tire width direction gradually decreases from near the tire radial center position of the side reinforcing rubber 6 toward the tire radial inner and outer sides in the tire width direction in the tire width direction cross section, and protrudes convexly outward in the tire width direction.

[0019] As shown in FIG. 1, the tire 1 of this embodiment includes an inner liner 7 on the inner surface of the tire. In this example, the inner liner 7 is made of butyl rubber. In this tire 1, On the inside of the tire , the inner rubber layer 8 is disposed . Inside In accordance with JIS K6270:2001, a test piece is prepared by cutting out 1 mm from the center of a No. 8 dumbbell perpendicular to the direction of repeated tension of the test piece, and when tension is repeatedly applied at a frequency of 10 Hz under conditions of 150°C, the number of repetitions until the test piece breaks is at least twice (preferably at least 10 times) that of the side reinforcing rubber 6, in the range of applied tensile strain of 10% to 30%. As for the material, the inner layer rubber 8 is made of a rubber that does not contain a copolymer of isobutylene and isoprene (for example, a rubber blended with butadiene rubber and natural rubber).

[0020] In addition, in the above-mentioned standard state, the ratio T2 / T1 of the thickness T2 of the inner layer rubber when measured in the direction of a perpendicular line extending from the carcass 4 down to the inner surface of the tire to the maximum thickness T1 at which the thickness of the side reinforcing rubber 6 is at its maximum when measured in the direction of the perpendicular line is 0.05 to 0.30.

[0021] In this tire 10, the outer end of the inner liner 7 in the tire width direction and the outer end of the inner layer rubber 8 in the tire radial direction are disposed to abut against each other, or as shown in the figure, the outer end of the inner liner 7 in the tire width direction and the outer end of the inner layer rubber 8 in the tire radial direction overlap with an overlap width of 30 mm or less. Note that in the example shown, the inner liner 7 overlaps so as to be positioned outside the inner layer rubber 8 in the tire radial direction, but this is not limited to this case, and the inner liner 7 may overlap so as to be positioned inside the inner layer rubber 8 in the tire radial direction. Furthermore, in the above-mentioned reference state, when the width in the tire width direction of the inner liner 7 is W1 (mm) and the width in the tire width direction of the innermost belt layer 5a in the tire radial direction among the one or more belt layers is W2 (mm), W2≦W1≦W2+20 (mm) is satisfied.

[0022] Moreover, the loss tangent tan δ1 of the inner layer rubber 8 is 80% or less of the loss tangent tan δ2 of the inner liner 7, preferably 70% or less, and more preferably 60% or less. The effects of the run-flat tire of this embodiment will be described below.

[0023] The inventors of the present invention noticed that in run-flat tires, the side reinforcing rubber 6 arranged on the sidewall suppresses air permeation, and therefore the inner liner 7 does not necessarily have to be arranged, and came up with the idea that the rolling resistance can be reduced by removing the inner liner with a large loss tangent from the sidewall. On the other hand, if the side reinforcing rubber 6 is exposed on the innermost surface of the tire, the run-flat durability may decrease, and the inventors found that by arranging an inner layer rubber with a loss tangent smaller than that of the inner liner, the decrease in run-flat durability can be suppressed without significantly losing the above-mentioned effect of reducing rolling resistance. Specifically, in the tire of this embodiment, the outer end of the inner liner 7 in the tire width direction and the outer end of the inner layer rubber 8 in the tire radial direction are arranged to butt against each other, or as shown in the illustrated example, the outer end of the inner liner 7 in the tire width direction and the outer end of the inner layer rubber 8 in the tire radial direction overlap with an overlap width of 30 mm or less. In addition, in the above-mentioned reference state, when the width of the inner liner 7 in the tire width direction is W1 (mm) and the width of the innermost belt layer 5a in the tire radial direction among one or more belt layers is W2 (mm), W2≦W1≦W2+20 (mm) is satisfied. In this way, the rolling resistance can be reduced by reducing the amount of the inner liner 7 arranged. That is, if the overlap width is more than 30 mm, the effect of reducing the rolling resistance cannot be sufficiently obtained. Also, even if W1>W2+20 (mm), the effect of reducing the rolling resistance cannot be sufficiently obtained. Note that, if W2>W1, the occurrence of failure near the belt end due to air getting in near the belt end cannot be sufficiently suppressed. In addition, since the inner liner 7 itself is a heat source, by reducing the amount of the inner liner 7 disposed as described above, it is also possible to improve run-flat durability. Furthermore, in this embodiment, the side reinforcing rubber 6 of Inner Liner 7 The inner surface not covered by By disposing the inner layer rubber 8 on the inner lining 7, it is possible to suppress a decrease in run-flat durability compared to a case where the side reinforcing rubber 6 is exposed on the innermost surface of the tire. Furthermore, since the loss tangent tanδ1 of such inner layer rubber 8 is 80% or less of the loss tangent tanδ2 of the inner liner 7, it is possible to reduce rolling resistance compared to a case where the inner liner 7 is disposed over the entire inner surface of the tire. As described above, according to the run-flat tire of the present embodiment, it is possible to suppress an increase in rolling resistance while ensuring run-flat durability.

[0024] From the viewpoint of minimizing the amount of inner liner 7 placed and obtaining the above-mentioned effect of reducing rolling resistance and improving run-flat durability by reducing heat generation, it is preferable for the overlap width to be small, and it is more preferable for the tire widthwise outer end of the inner liner and the tire radially outer end of the inner layer rubber to be arranged abutting each other. From the same viewpoint, it is more preferable to satisfy W1≦W2+10 (mm). From the viewpoint of suppressing air leakage, it is preferable that there is no gap between the outer end of the inner liner in the tire width direction and the outer end of the inner layer rubber in the tire radial direction.

[0025] From the viewpoint of suppressing an increase in rolling resistance, the loss tangent tan δ1 of the inner layer rubber 8 is preferably 70% or less of the loss tangent tan δ2 of the inner liner 7, and more preferably 60% or less.

[0026] During run-flat driving, the innermost part of the sidewall reinforcement rubber is exposed to high temperatures and high strain due to large deflections. Therefore, the sidewall reinforcement rubber is required to have the function of supporting the load in the run-flat state, as well as the function of being resistant to fracture under high temperatures and high strain. Therefore, the inner layer rubber 8 is preferably, in accordance with JIS K6270:2001, a test piece obtained by cutting out the center of a No. 8 dumbbell by 1 mm perpendicular to the direction of repeated pulling of the test piece, and when tension is repeatedly applied at a frequency of 10 Hz under conditions of 150°C, the number of repetitions until the test piece breaks is at least twice (more preferably at least 10 times) that of the side reinforcing rubber 6 in the range of applied tensile strain of 10% to 30%. Such rubber has high peeling resistance. As a result, the side reinforcing rubber 6 can be made to bear the load, while the inner layer rubber 8 can be made to suppress destruction from the inner surface side of the tire, and run-flat durability can be further improved. In addition, the inner layer rubber 8 is preferably, in accordance with JIS K6270:2001, a test piece obtained by cutting out the center of a No. 8 dumbbell by 1 mm perpendicular to the direction of repeated pulling of the test piece, and when tension is repeatedly applied at a frequency of 10 Hz under conditions of 150°C, with a strain of 30%, the number of repetitions until the test piece breaks is at least 70,000. By using such an inner layer rubber 8, it is possible to further increase the peeling resistance and further improve the run-flat durability.

[0027] When using an inner layer rubber 8 having high peel resistance as described above, in the above-mentioned standard state, the ratio T2 / T1 of the thickness T2 of the inner layer rubber 8 measured in the direction of a perpendicular line extending from the carcass to the inner surface of the tire to the maximum thickness T1 at which the thickness of the side reinforcing rubber 6 is at its maximum when measured in the direction of the perpendicular line is preferably 0.05 to 0.30. This can further improve run-flat durability. That is, by making the ratio T2 / T1 0.30 or less, the volume of the side reinforcing rubber 6 can be secured, and the load support capacity can be made even more sufficient. On the other hand, by making the ratio T2 / T1 0.05 or more, the volume of the inner layer rubber 8, which has high peel resistance, can be secured, and the fracture resistance under high temperature and high strain conditions can be secured sufficiently.

[0028] Here, the ratio of the elastic modulus of the inner layer rubber 8 to the elastic modulus of the side reinforcing rubber 6 is preferably 0.75 or less (preferably 0.6 or less), because this makes it possible to suppress a decrease in ride comfort. EXAMPLES

[0029] In order to confirm the effect of the present invention, Example 1 of the invention for tire size PSR 235 / 60F18 was Tires according to the above No. 1, No. 2 and a comparative example were produced as prototypes, and tests were carried out to evaluate the tire performance. Comparative Example: The side reinforcing rubber was made of one type of rubber. Example 1: The inner layer rubber has an elastic modulus of 35% compared to the side reinforcing rubber, and is arranged so that the gauge ratio of the inner layer rubber / the side reinforcing rubber is 0.09 at the thickest part of the side reinforcing rubber gauge. In addition, at the overlapping part between the inner liner and the inner layer rubber, the inner layer rubber is closer to the side reinforcing rubber than the inner liner. The other configurations are the same as those of the comparative example. Invention Example 2: The inner layer rubber having an elastic modulus of 31% compared to the side reinforcing rubber was arranged so that the gauge ratio of the inner layer rubber / the side reinforcing rubber was 0.09 at the thickest part of the side reinforcing rubber gauge. In addition, at the overlapping part between the inner liner and the inner layer rubber, the inner liner was positioned closer to the side reinforcing rubber than the inner layer rubber. The other configurations were the same as those of the comparative example.

[0030] <Run-flat durability> Run-flat durability was evaluated under rim, internal pressure, and load conditions that conform to ISO standards. The results of the comparative example are expressed as an index, with a higher index indicating better performance. <Rolling resistance> Each tire was freely rotated on a drum at an air pressure of 210 kPa, a speed of 80 km / h, and a load of 6890 N to measure rolling resistance. The results of the comparative example were expressed as an index of 100, with a smaller index indicating better performance. <Vertical spring coefficient> The vertical spring coefficient was calculated when the tire was assembled on a JATMA-compliant rim, inflated with an internal pressure of 230 kPa, and subjected to a load of 6010 N. The results of the comparative example are expressed as an index of 100, with a smaller index indicating better performance. The evaluation results are shown in Table 1 below.

[0031] [Table 1] [Explanation of symbols]

[0032] 10: Run-flat tires, 1: tread part, 2: Sidewall part, 3: Bead part, 4: Carcass, 5: Belt, 6: Side reinforcement rubber, 7: Inner liner, 8: Inner rubber

Claims

1. A tread portion; A pair of sidewall portions connected to both sides of the tread portion; a bead portion connected to each of the sidewall portions; A side reinforcing rubber having a crescent-shaped cross section disposed on the sidewall portion; a carcass extending in a toroidal shape between the pair of bead portions; a belt consisting of one or more belt layers arranged on a radially outer side of a crown portion of the carcass, An inner liner and an inner rubber layer are arranged on the inner surface of the tire, an outer end of the inner liner in the tire width direction and an outer end of the inner layer rubber in the tire radial direction are disposed so as to abut against each other, or an outer end of the inner liner in the tire width direction and an outer end of the inner layer rubber in the tire radial direction overlap with an overlap width of 30 mm or less, and the outer end of the inner layer rubber in the tire radial direction is located closer to the inner surface of the tire than the outer end of the inner liner in the tire width direction, In a standard state in which the run-flat tire is mounted on an applicable rim, inflated to a specified internal pressure, and unloaded, the width of the inner liner in the tire width direction is W1 (mm) and the width of the innermost belt layer in the tire radial direction among the one or more belt layers is W2 (mm), satisfying W2≦W1≦W2+20 (mm), a loss tangent tanδ1 of the inner layer rubber is 80% or less of a loss tangent tanδ2 of the inner liner, The inner layer rubber 8 is a run-flat tire characterized in that, in accordance with JIS K6270:2001, a test specimen is prepared by cutting out the center of a No. 8 dumbbell by 1 mm perpendicular to the direction of repeated tension of the test specimen, and when repeated tension is applied at a frequency of 10 Hz under conditions of 150°C, the number of repetitions until the test specimen breaks is at least twice as long as that of the side reinforcing rubber, in the range of applied tensile strain of 10% to 30%.

2. 2. The run-flat tire according to claim 1, wherein a ratio T2 / T1 of a thickness T2 of the inner layer rubber measured in a perpendicular direction to a maximum thickness T1 at which the thickness of the side reinforcing rubber is maximum when measured in the perpendicular direction from the carcass to the inner surface of the tire in the reference state is 0.05 to 0.

30.

3. 3. The run-flat tire according to claim 1, wherein a ratio of an elastic modulus of said inner layer rubber to an elastic modulus of said side reinforcing rubber is 0.75 or less.

Citation Information

Patent Citations

  • Runflat tire

    JP2007069775A

  • Runflat tire

    JP2011088593A

  • Run-flat tire