Injection molding mold and injection molding method using the same

The injection mold with frame-shaped temperature control flow paths and opposing directions stabilizes temperature control, addressing uneven cooling issues to achieve high-precision and defect-free eyeglass frame molding.

JP7595866B2Active Publication Date: 2024-12-09MAEZAWA MOLD CO LTD +1
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2021088731
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-05-26
Publication Date
2024-12-09
Estimated Expiration
2041-05-26

AI Technical Summary

Technical Problem

Existing injection molding methods for eyeglass frame members suffer from uneven cooling due to temperature changes in the cooling and temperature control media, leading to deformation and reduced precision in the molding process.

Method used

The injection mold features frame-shaped temperature control flow paths in the cavity and core molds, with opposing flow directions to stabilize temperature control, and includes gas venting sections made of porous material to manage gas efficiently.

Benefits of technology

This configuration ensures uniform and stable temperature control, resulting in high-precision molding of eyeglass frame members with reduced defects and improved productivity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007595866000001
    Figure 0007595866000001
  • Figure 0007595866000002
    Figure 0007595866000002
  • Figure 0007595866000003
    Figure 0007595866000003
Patent Text Reader

Abstract

To provide an injection molding mold and an injection molding method using the same capable of performing efficient and stable molding treatment in molding an eyeglass frame member.SOLUTION: In an injection molding mold, a cavity mold 1 and a core mold 2 are set in a manner that molding directions match in a case of manufacturing by a metal powder sintering method; inside of the cavity mold, frame-shaped cavity side temperature controlling channels 11 and 12 are formed so as to overlap each other with a prescribed interval in the molding direction with respect to frame-shaped areas C1 and C2 of a molding gap part C; and inside of the core mold, frame-shaped core side temperature controlling channels 21 and 22 are formed so as to overlap each other with a prescribed interval in the molding direction with respect to the frame-shaped areas.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an injection molding die used for injection molding in which heated and melted material is injected into a mold and then cooled and solidified, and an injection molding method using the same, and in particular to an injection molding die suitable for molding eyeglass frame members and an injection molding method using the same. [Background technology]

[0002] Conventionally, the injection molding method has been widely used to manufacture molded products by injecting molten resin material into a mold and cooling and solidifying it. By forming a highly accurate molding cavity in the mold, it is possible to manufacture molded products with high precision and complex shapes.

[0003] In such an injection molding method, a mold that is processed to a high degree of accuracy in accordance with the complex shape of the molded product is used, and a cooling passage for circulating a cooling fluid is formed in the mold in order to solidify the filled molten resin in a short time. For example, Patent Document 1 describes an injection molding mold that is molded by rapid prototyping and has a cooling passage formed with a uniform thickness from the cavity surface. Patent Document 2 describes that a temperature control circuit is simultaneously formed inside the mold when the mold is molded by sintering metal powder using a laser beam. Patent Document 3 describes that a mold that includes a fixed side mold and a movable side mold, in which resin is injected into a cavity formed in the contact area between the mold and the movable side mold, is provided with a temperature control section that includes a flow channel through which a temperature control medium flows and a plurality of channel support columns that support a load in the flow channel, in at least one of the fixed side mold or the movable side mold. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Patent No. 4544398 [Patent Document 2] Japanese Patent Application Publication No. 11-348045 [Patent Document 3] Patent No. 6191356 Summary of the Invention [Problem to be solved by the invention]

[0005] In Patent Document 1, a cooling passage is formed with a uniform thickness from the cavity surface of the injection molding die, but one cooling passage is formed to surround the side surface of the three-dimensional shape formed by the cavity surface. Therefore, the temperature of the cooling fluid flowing through the cooling passage changes while flowing, and uneven cooling cannot be avoided.

[0006] In Patent Document 2, it is possible to form a desired temperature control circuit in a molded mold, but the temperature control circuit is formed in a spiral shape around the cavity, which creates the problem of uneven cooling caused by temperature changes in the cooling medium flowing through the temperature control circuit.In Patent Document 3, flow channels through which the temperature control medium flows are formed in the fixed side mold and the movable side mold, but there is a problem of uneven cooling caused by temperature changes while the temperature control medium flows through the flow channels.

[0007] When injection molding eyeglass frame components using resin material, the molding process is carried out with temperature control circuits placed on both sides of the molding gap formed in the injection mold. However, uneven cooling of the eyeglass frame components causes deformation, which inevitably reduces accuracy, making it necessary to make fine adjustments when attaching the eyeglass lenses.

[0008] Therefore, an object of the present invention is to provide an injection molding mold and an injection molding method using the same that can perform efficient and stable molding processing by forming a frame-shaped temperature control flow path in a frame-shaped region of a molding gap portion corresponding to an eyeglass frame member formed in the injection molding mold. [Means for solving the problem]

[0009] The injection molding mold of the present invention is an injection molding mold comprising a cavity mold and a core mold formed by stacking and sintering metal powder material, and into which molten resin is injected into a molding gap portion formed in the abutment area of ​​the cavity mold and the core mold, the molding directions of which are aligned and the core mold are set to abut, and inside the cavity mold, frame-shaped cavity side temperature control flow passages are formed so as to overlap with a predetermined distance in the molding direction relative to the frame-shaped area of ​​the molding gap portion, and inside the core mold, frame-shaped core side temperature control flow passages are formed so as to overlap with a predetermined distance in the molding direction relative to the frame-shaped area. Furthermore, the cavity-side temperature control flow path is formed with a pair of cavity-side connection paths along the molding direction on the side opposite to the frame-shaped region through which the temperature control fluid flows in and out, and the core-side temperature control flow path is formed with a pair of core-side connection paths along the molding direction on the side opposite to the frame-shaped region through which the temperature control fluid flows in and out, and the cavity-side connection paths and the core-side connection paths are arranged to face each other. Furthermore, an injection path communicating with the molding gap is formed between the pair of frame-shaped regions, and a gas vent portion communicating with the molding gap is formed on the side opposite to the injection path of the frame-shaped region. Furthermore, the gas vent portion is formed of a porous material through which gas can flow.

[0010] The injection molding method of the present invention is an injection molding method in which molten resin is injected into the molding void portion formed in the above-mentioned injection molding mold to form a mold, and a temperature control fluid is circulated in opposite directions through the cavity side temperature control flow path and the core side temperature control flow path. Effect of the Invention

[0011] By having the above-mentioned configuration, the present invention forms temperature-control flow paths inside the cavity mold and the core mold, respectively, so that they overlap with the frame-shaped region corresponding to the frame portion of the eyeglass frame member, making it possible to efficiently control the temperature of the entire frame-shaped region from both sides, thereby producing molded products of stable quality.

[0012] The frame portion of the eyeglass frame component is where the eyeglass lens is fitted, so it needs to be molded with high precision to match the three-dimensional shape of the peripheral portion of the eyeglass lens. However, as described above, by adjusting the temperature of the frame-shaped region corresponding to the frame portion from both sides, it is possible to carry out the preheating and cooling processes around the frame-shaped region at a stable temperature, allowing the molding process to be carried out accurately and efficiently.

[0013] In addition, a pair of connecting paths through which the temperature control fluid flows in and out are formed on the opposite side of the frame-shaped region, so that the effect of the temperature control fluid flowing through the connecting paths on the temperature state of the frame-shaped region can be suppressed, and the temperature state due to the temperature control fluid flowing through the temperature control flow path can be maintained stably.

[0014] In addition, since the gas vent section is formed of a porous material through which gas can flow, gas generated during processing can be smoothly exhausted, thereby preventing the influence of gas generation on the molding process.

[0015] Furthermore, since the temperature control fluid is caused to flow in opposite directions through the temperature control flow paths formed on both sides of the frame-shaped region, the entire frame-shaped region can be set to a more uniform and stable temperature state. [Brief description of the drawings]

[0016] [Figure 1] FIG. 1 is an explanatory view showing a schematic configuration of an injection molding die according to the present invention, illustrating the internal structure in a see-through manner. [Diagram 2] FIG. [Diagram 3] 3 is a cross-sectional view taken along the line AA in FIG. 2, and is an explanatory view showing the internal structure in a see-through manner. [Figure 4] FIG. [Diagram 5] 5 is a cross-sectional view taken along the line B-B of FIG. 4, and is an explanatory view showing the internal structure in a see-through manner. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] Hereinafter, the embodiments of the present invention will be described in detail. Note that the embodiments described below are preferred examples for carrying out the present invention, and therefore various technical limitations are imposed thereon, but the present invention is not limited to these embodiments unless otherwise specified in the following description to limit the invention.

[0018] 1 is an explanatory diagram showing a schematic configuration of an injection molding die according to the present invention, and is drawn to allow a view of the internal structure. The injection molding die for molding an eyeglass frame member includes a cavity die 1 and a core die 2 (each shown by a dashed line), and in this example, the front part of the eyeglass frame member that holds the eyeglass lens is molded from a resin material. Therefore, when the cavity die 1 and the core die 2 are in contact with each other, a molding gap part C (shown by a thin line) corresponding to the front part is formed in the contact area, and a pair of frame-shaped areas C1 and C2 are formed in the molding gap part C corresponding to the rim part into which the eyeglass lens is fitted.

[0019] An injection passage 40 communicating with the molding gap C is connected between the pair of frame-shaped regions C1 and C2, and gas vents 30a and 30b communicating with the molding gap C are formed on the opposite sides of the injection passage 40 of the frame-shaped regions C1 and C2. The injection passage 40 is connected to a region corresponding to the bridge of the front part, and molten resin material is injected from a supply device (not shown). The gas vent 30a extends from the end of the frame-shaped region C1 corresponding to the end piece toward the side of the injection mold, and is formed porous to allow gas to flow through. Therefore, gas generated when molten resin is injected into the molding gap C to perform injection molding is discharged to the outside, and the molten resin filled in the molding gap C is prevented from leaking. The gas vent 30b extends from the end of the frame-shaped region C2 corresponding to the end piece toward the side of the injection mold, and is formed porous to allow gas to flow through, similar to the frame-shaped region C1. Therefore, the generated gas can be discharged without causing the molten resin filled in the molding cavity C to leak out.

[0020] The cavity mold 1 is integrally formed with the base plate 10 as indicated by the dashed line, and frame-shaped cavity-side temperature control flow paths 11 and 12 (indicated by thin lines) are formed inside. The cavity-side temperature control flow paths 11 and 12 are composed of pipes for circulating a temperature control fluid such as water adjusted to a predetermined temperature. The cavity-side temperature control flow path 11 is formed at a predetermined interval so as to overlap with the frame-shaped region C1 in a plan view, and the cavity-side temperature control flow path 12 is formed at a predetermined interval so as to overlap with the frame-shaped region C2 in a plan view.

[0021] A pair of cavity side connection paths 13a and 13b through which the temperature control fluid flows in and out are formed in the cavity side temperature control flow path 11 on the opposite side to the frame-shaped region C1, and the cavity side connection paths 13a and 13b are each configured to communicate with a pair of flow passages 15a and 15b formed in the base plate 10.

[0022] A pair of cavity side connection paths 14a and 14b through which temperature control fluid flows in and out are formed in the cavity side temperature control flow path 12 on the opposite side to the frame-shaped region C2, and the cavity side connection paths 14a and 14b are each configured to communicate with a pair of flow passages 16a and 16b formed in the base plate 10.

[0023] The core mold 2 is integrally formed with the base plate 20 as indicated by the dashed line, and frame-shaped core-side temperature control flow paths 21 and 22 (indicated by thin lines) are formed inside. The core-side temperature control flow paths 21 and 22 are composed of pipes for circulating a temperature control fluid such as water adjusted to a predetermined temperature. The core-side temperature control flow path 21 is formed at a predetermined interval so as to overlap with the frame-shaped region C1 in a plan view, and the core-side temperature control flow path 22 is formed at a predetermined interval so as to overlap with the frame-shaped region C2 in a plan view.

[0024] A pair of core side connection paths 23a and 23b through which temperature control fluid flows in and out are formed in the core side temperature control flow path 21 on the opposite side to the frame-shaped region C1, and the core side connection paths 23a and 23b are each configured to communicate with a pair of circulation paths 25a and 25b formed in the base plate 20.

[0025] The core side temperature control flow path 22 has a pair of core side connection paths 24a and 24b formed on the opposite side of the frame-shaped region C2, through which the temperature control fluid flows in and out, and the core side connection paths 24a and 24b are each configured to communicate with a pair of flow passages 26a and 26b formed in the base plate 20.

[0026] In the above example, the frame-shaped cavity-side temperature control flow path 11 and the core-side temperature control flow path 21 are arranged so as to overlap on both the upper and lower sides of the frame-shaped region C1, and the frame-shaped cavity-side temperature control flow path 12 and the core-side temperature control flow path 22 are arranged so as to overlap on both sides of the frame-shaped region C2. Therefore, by circulating the temperature control fluid through the temperature control flow paths arranged on both the upper and lower sides of the frame-shaped region, the frame-shaped region can be efficiently adjusted to a stable temperature state.

[0027] The temperature control fluid is passed through the cavity-side temperature control flow passage and the core-side temperature control flow passage arranged above and below the frame-shaped region in the opposite directions, so that the temperature state of the entire frame-shaped region can be made more uniform. As shown by the arrows in Fig. 1, in the frame-shaped region C1, the temperature control fluid passes through the cavity-side temperature control flow passage 11 in the flow path 15a → the cavity-side connection path 13a → the cavity-side temperature control flow passage 11 → the cavity-side connection path 13b → the flow path 15b, and in the core-side temperature control flow passage 21 in the flow path 25b → the core-side connection path 23b → the core-side temperature control flow passage 21 → the core-side connection path 23a → the flow path 25a, so that the flow directions are set in the opposite directions. Similarly, in the frame-shaped region C2, the flow directions are set in the cavity-side temperature control flow passage 12 and the core-type temperature control flow passage 22 in the flow path 22 in the flow path 25a.

[0028] The temperature control fluid changes in temperature while flowing through the pipeline. For example, when the injection mold is preheated before the injection of the molten resin, the temperature of the temperature control fluid decreases while flowing through the pipeline, and when the injection mold is cooled after the injection of the molten resin, the temperature of the temperature control fluid increases while flowing through the pipeline. Therefore, the temperature of the temperature control fluid changes between the inlet side connecting path and the outlet side connecting path of the temperature control flow path, so that the temperature state of the frame-shaped region becomes uneven. Therefore, by setting the inlet side and outlet side of the cavity side temperature control flow path and the core mold temperature control flow path to be in opposite directions, the temperature state of the frame-shaped region can be made more uniform, and the temperature states of both frame-shaped regions can be made almost the same. In addition, by performing such temperature adjustment, it is also easy to adjust the mold temperature by changing the temperature of the temperature control fluid.

[0029] The cavity mold and core mold used in such injection molding can be manufactured by a known metal powder sintering method. In the metal powder sintering method, first, slice data of a three-dimensional shape is created based on three-dimensional CAD data of the mold. Then, a high-energy laser beam is irradiated to metal powder laid at a predetermined thickness on a flat surface based on the slice data to melt and solidify the metal powder, thereby forming a cross-sectional shape. Such cross-sectional shapes can be stacked to form a three-dimensional shape. By manufacturing the mold in this way, the degree of freedom of the piping through which the temperature control fluid flows in the mold can be increased, and it becomes possible to form piping capable of adjusting the temperature state in the mold efficiently with high precision.

[0030] Fig. 2 is a perspective view of the cavity mold, and Fig. 3 is a cross-sectional view taken along line AA in Fig. 2, which is an explanatory diagram showing the internal structure. The contact surface of the cavity mold 1 is formed in a convex curved shape to match the shape of the front part, and the contact surface has a step portion formed in a three-dimensional shape corresponding to the molding gap portion C. Inside the cavity mold 1, a frame-shaped cavity-side temperature control flow path 11 is formed at a predetermined interval from the frame-shaped region C1, and a frame-shaped cavity-side temperature control flow path 12 is formed at a predetermined interval from the frame-shaped region C2.

[0031] When the cavity mold 1 is manufactured by the metal powder sintering method, metal powder is laid in a predetermined thickness on the upper surface of the base plate 10, and laser light is irradiated to stack them in the vertical direction to form the mold. Therefore, each cavity side temperature control flow passage can be accurately formed at a predetermined interval in the molding direction for each frame-shaped region, and it is possible to accurately form them so that they overlap when viewed from the molding direction. Furthermore, when forming a frame-shaped temperature control flow passage that intersects with the molding direction, the cross-sectional shapes 11a and 12a of the temperature control flow passages 11 and 12 can be formed into a stable shape by forming them into a substantially hexagonal shape having both sides along the molding direction and both ends of the upper side cut out in an oblique direction.

[0032] A pair of cavity-side connecting passages 13a and 13b arranged opposite to each other are formed downward in the cavity-side temperature control passage 11, and a pair of cavity-side connecting passages 14a and 14b arranged opposite to each other are formed downward in the cavity-side temperature control passage 12. A pair of flow passages 15a and 15b and a pair of flow passages 16a and 16b are formed in the base plate 10 from both side surfaces by a drill or the like, and the flow passages 15a and 15b are connected to the cavity-side connecting passages 13a and 13b, respectively, and the flow passages 16a and 16b are connected to the cavity-side connecting passages 14a and 14b, respectively.

[0033] When constructing such pipelines, each flow passage is formed in the base plate 10, and each cavity side connecting passage is then shaped to match the upper opening of each flow passage, thereby allowing the interconnected pipelines to be formed accurately.

[0034] Fig. 4 is a perspective view of the core mold, and Fig. 5 is a cross-sectional view taken along line BB of Fig. 4, which is an explanatory diagram drawn to see through the internal structure. The contact surface of the core mold 2 is formed in a concave curved shape in accordance with the three-dimensional shape of the front part, and the contact surface has a step portion formed in a three-dimensional shape corresponding to the molding gap C. A pair of frame-shaped regions C1 and C2 of the molding gap C are formed with band-shaped gas vents 30a and 30b extending to the outer side, respectively, and inside the core mold 2, a frame-shaped core-side temperature control flow path 21 is formed at a predetermined interval from the frame-shaped region C1, and a frame-shaped core-side temperature control flow path 22 is formed at a predetermined interval from the frame-shaped region C2.

[0035] When the core mold 2 is manufactured by the metal powder sintering method, similar to the cavity mold 1, metal powder is spread to a predetermined thickness on the upper surface of the base plate 20 and irradiated with laser light to stack and mold in the vertical direction. Therefore, each core side temperature control flow passage can be accurately molded at a predetermined interval in the molding direction for each frame-shaped region, and it is possible to accurately form them so that they overlap when viewed from the molding direction. Since the core mold 2 is molded by stacking in the vertical direction, similar to the cavity mold 1, the molding directions become the same when the two are abutted.

[0036] When forming a frame-shaped temperature control flow path that intersects with the forming direction, the cross-sectional shapes 21a and 22a of the temperature control flow paths 21 and 22 can be formed into a stable shape by forming them into an approximately hexagonal shape having both side sides along the forming direction and both ends of the upper side cut out diagonally.

[0037] For the gas vents 30a and 30b, a porous member is formed by laminating and sintering metal powder at a low density separately from the core mold to match the shape of the gas vents. The formed core mold is then partially cut by cutting to match the position of the gas vents, and the porous member is fitted and embedded at the cut position to form the gas vents. By forming the gas vents in a porous material, it is possible to ensure air permeability between the molding gap C and the outside. In addition, for the connection parts between each gas vent and each frame-shaped region, the molding density is increased to a level that prevents the molten resin filled in the molding gap C from leaking out, making it possible to reliably perform injection molding.

[0038] A pair of core side connection paths 23a and 23b arranged opposite to each other are formed downward in the core side temperature control flow path 21, and a pair of core side connection paths 24a and 24b arranged opposite to each other are formed downward in the core side temperature control flow path 22. A pair of flow paths 25a and 25b and a pair of flow paths 26a and 26b are formed in the base plate 20 from both side surfaces by a drill or the like, and the flow paths 25a and 25b are connected to the core side connection paths 23a and 23b, respectively, and the flow paths 26a and 26b are connected to the core side connection paths 24a and 24b, respectively.

[0039] When constructing such pipelines, each flow passage is formed in the base plate 20, and each core side connection passage is then shaped to match the upper opening of each flow passage, thereby allowing the formation of a connected pipeline with precision. EXAMPLES

[0040] The cavity mold shown in Figure 2 was molded on a base plate (length 175 mm x width 225 mm x thickness 30 mm) made of steel using a metal powder sintering molding device (LUMEX Avance-25, manufactured by Matsuura Machine Works, Ltd.). Maraging steel (average particle size 45 μm, Matsuura Maraging II, manufactured by Matsuura Machine Works, Ltd.) was used as the metal powder. The molded cavity mold was formed to a size of length 100.3 mm x width 200.3 mm x thickness 19.4 mm, and then the contact surface including the molding gap portion C was precisely machined by cutting.

[0041] The core mold shown in Figure 4 was molded on a base plate (175 mm long x 225 mm wide x 20 mm thick) made of steel using the same metal powder sintering molding device as the cavity mold. The same maraging steel as the cavity mold was used as the metal powder. The molded core mold was formed to a size of 100.3 mm long x 200.3 mm wide x 20 mm thick, and the contact surface including the molding gap C was then precisely machined by cutting. For the gas vent, a porous member was prepared by molding the same metal powder as the cavity mold, and fine grooves corresponding to the gas vent were formed in the core mold by cutting, and the porous member was fitted into the fine grooves formed and fixed.

[0042] The obtained cavity mold and core mold were fixed together with their contact surfaces in close contact, and a preheating treatment was performed by circulating a temperature control fluid (water, 82°C) through the temperature control flow path. After 10 minutes of preheating, the mold surface temperatures in the frame-shaped regions were both stable at around 47°C with an almost uniform temperature distribution. The temperature control fluid circulated in the same direction through the temperature control flow paths arranged in parallel in each mold, while the temperature control fluid circulated in opposite directions in the cavity mold and the core mold, resulting in an almost uniform temperature distribution in both frame-shaped regions.

[0043] Next, polyamide resin (manufactured by Daicel-Evonik) was melted at high temperature (260°C-280°C) and injected through an injection port provided in the cavity mold to fill the molding gap. A temperature-control fluid was continuously circulated through the temperature-control flow path to perform a cooling process for 20 seconds. 60 seconds after the mold was opened, the mold surface temperature had dropped to 46°C-48°C, and the cooling process was performed almost uniformly over the entire frame-shaped area.

[0044] The eyeglass frame parts obtained by demolding after opening the mold had a nearly uniform shrinkage rate in the rim area and were molded with high precision, with no defects such as gas pockets. As a result, high-quality molded products could be obtained stably.

[0045] It was also confirmed that the preheating and cooling processes can be carried out efficiently, which is effective in shortening the processing time and improving productivity.

[0046] <Comparative Example> The cavity mold and the core mold were formed by cutting steel material. The contact surfaces of the cavity mold and the core mold were cut to form a molding gap portion similar to that of the examples, and a pair of temperature control flow paths were formed by drilling a straight pipe line through the lower side of the molding gap portion. The pipe line was configured so that the temperature control fluid was circulated through one temperature control flow path and then flowed into the other temperature control flow path.

[0047] The cavity mold and the core mold were fixed together with their contact surfaces in close contact, and a preheating treatment was performed by circulating a temperature control fluid (water, 82°C) through the temperature control flow path. During the preheating treatment, even after 20 minutes had passed, the mold surface temperature in the frame-shaped region was 43°C to 54°C, and there were unevenness in the temperature distribution, and the temperature was not uniform. This unevenness in the temperature distribution occurs because the temperature control fluid is circulated, so the temperature of the frame-shaped region closer to the inlet tends to be higher and the temperature of the frame-shaped region further away tends to be lower, resulting in temperature unevenness.

[0048] Next, similarly to the example, polyamide resin was melted at high temperature and injected from the injection port provided in the cavity mold to fill the molding gap. A temperature control fluid was continuously circulated through the temperature control flow path to perform a cooling process for 35 seconds. The mold surface temperature 60 seconds after the mold was opened was 50°C to 55°C, and the cooling process of the entire frame-shaped region was performed in an uneven state.

[0049] The eyeglass frame members obtained by demolding after opening the mold were found to have been molded with uneven shrinkage in the rim area, low precision, and had defects such as gas pockets. [Explanation of symbols]

[0050] C···Molding gap portion, C1, C2···Frame-shaped region, 1···Cavity mold, 10···Base plate, 11, 12···Cavity side temperature control flow path, 13a, 13b, 14a, 14b···Cavity side connecting path, 15a, 15b, 16a, 16b···Flow path, 2···Core mold, 20···Base plate, 21, 22···Cavity side temperature control flow path, 23a, 23b, 24a, 24b···Cavity side connecting path, 25a, 25b, 26a, 26b···Flow path, 30a, 30b···Gas vent portion, 40···Injection port

Claims

1. An injection molding mold comprising a cavity mold and a core mold formed by stacking and sintering metal powder material, and into which molten resin is injected into a molding gap portion formed in the abutment area of ​​the cavity mold and the core mold, the molding directions of which are aligned and the core mold are set to abut, and inside the cavity mold, frame-shaped cavity side temperature control flow passages are formed to overlap with a frame-shaped region of the molding gap portion at a predetermined interval in the molding direction, and inside the core mold, frame-shaped core side temperature control flow passages are formed to overlap with the frame-shaped region at a predetermined interval in the molding direction.

2. The injection molding die of claim 1, wherein the cavity side temperature control flow path has a pair of cavity side connection paths formed along the molding direction on the opposite side of the frame-shaped region, through which temperature control fluid flows in and out, and the core side temperature control flow path has a pair of core side connection paths formed along the molding direction on the opposite side of the frame-shaped region, through which temperature control fluid flows in and out, and the cavity side connection paths and the core side connection paths are arranged opposite each other.

3. 3. The injection molding die according to claim 1, wherein an injection passage communicating with the molding gap is formed between the pair of frame-shaped regions, and a gas vent portion communicating with the molding gap is formed on the opposite side of the frame-shaped region from the injection passage.

4. 4. The injection molding die according to claim 3, wherein the gas vent portion is formed of a porous material through which gas can flow.

5. 5. An injection molding method for injecting molten resin into the molding gap formed in the injection molding die according to claim 1, wherein a temperature control fluid is caused to flow in opposite directions through the cavity side temperature control flow path and the core side temperature control flow path.

Citation Information

Patent Citations

  • Controller for clamping of impact wrench

    JP1984053168A

  • Vacuum deposition device

    JP1986091356A

  • Metal mold

    JP1999348045A

  • Mold for molding rotary body equipped with tooth part and its manufacturing method

    JP2005335190A

  • Mold device

    JP2008179016A