Optical fiber rollable ribbon with low Young's modulus bonding matrix material.
A low Young's modulus bonding matrix material in optical fiber ribbons addresses the issue of signal loss by reducing external stress, enhancing signal integrity and packing efficiency.
Patent Information
- Application Number
- JP2023562840
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-04-13
- Filing Date
- 2021-08-30
- Publication Date
- 2025-10-14
- Estimated Expiration
- 2041-08-30
AI Technical Summary
Conventional partially bonded optical fiber ribbons suffer from optical signal transmission loss due to the lack of a uniform bonding matrix material and the high Young's modulus of existing matrix materials, which induce external stresses on optical fibers.
The use of a bonding matrix material with a low Young's modulus, applied intermittently to optical fibers, reduces external stress and minimizes optical signal transmission loss.
The low Young's modulus matrix material effectively reduces optical signal transmission loss in partially bonded optical fiber ribbons, maintaining signal integrity and enabling more efficient packing of optical fibers in cables.
Smart Images

Figure 0007753386000001 
Figure 0007753386000002 
Figure 0007753386000003
Abstract
Description
[Technical Field]
[0001] [Reference to Related Application] This patent application claims priority under 35 U.S.C. §119(e) to U.S. Provisional Patent Application No. 63 / 174,125 (filed April 13, 2021), entitled "Low Modulus Matrix in Rollable Ribbon," the entire contents of which are incorporated herein by reference.
[0002] [Field of the Invention] The present invention relates to optical fiber rollable ribbons, and more particularly to optical fiber rollable ribbons having a low Young's modulus bonding matrix material. [Background technology]
[0003] A fiber optic ribbon contains two or more parallel optical fibers bonded together along their length. A material, commonly called a matrix or bonding matrix, bonds the fibers together. In "flat" or "encapsulated" fiber optic ribbons, the parallel optical fibers may be completely enclosed within the bonding matrix material.
[0004] In partially bonded optical fiber ribbons, also called rollable ribbons or rollable ribbon units, the optical fibers forming the optical fiber ribbon are not bonded with a matrix material along their entire length. Rather, the optical fibers are intermittently bonded with a matrix material, thus allowing the optical fiber ribbon to be folded or wound into a generally cylindrical shape, allowing for better packing of circular cables and resulting in more optical fibers being included in a given cable diameter compared to optical fiber cables having conventional fully bonded ribbon structures.
[0005] However, in conventional partially bonded optical fiber ribbons, the lack of a uniform bonding matrix material that completely covers the entire length of each optical fiber can make one or more of the optical fibers relatively susceptible to optical signal transmission loss. That is, conventional bonding matrix materials that are intermittently applied to the optical fibers in a rollable ribbon can induce external stresses on one or more of the optical fibers, causing undesirable optical signal transmission loss. Summary of the Invention
[0006] The present invention comprises an optical fiber ribbon having a bonding matrix material with a low Young's modulus. The optical fiber ribbon includes a plurality of optical fibers arranged adjacent to one another in a linear array. The optical fiber ribbon also includes a plurality of portions of bonding matrix material applied to at least a portion of the outer surfaces of at least two adjacent optical fibers. The bonding matrix material portions have a low Young's modulus. The plurality of portions of bonding matrix material are applied to at least a portion of the outer surfaces of at least two adjacent optical fibers such that the linear array of optical fibers forms a partially bonded optical fiber ribbon. [Brief explanation of the drawings]
[0007] [Figure 1] 1 is a perspective view of a partially bonded optical fiber ribbon or rollable ribbon according to an embodiment of the present invention. [Figure 2] FIG. 2 is a top view of another partially bonded optical fiber ribbon or rollable ribbon according to an embodiment of the present invention. [Figure 3A] 1 is a perspective view of a partially bonded optical fiber ribbon or rollable ribbon prior to being rolled, according to an embodiment of the present invention. [Figure 3B] 3B is a perspective view of the partially bonded optical fiber ribbon or rollable ribbon of FIG. 3A after being wound, according to an embodiment of the present invention. [Figure 4]1 is a graph of transmission loss on a ribbon spool for a partially bonded optical fiber ribbon having a relatively low Young's modulus bonding matrix material according to an embodiment of the present invention and a partially bonded optical fiber ribbon having a conventional relatively high Young's modulus bonding matrix material. [Figure 5] 1 is a graph showing the transmission loss after cable formation of a partially bonded optical fiber ribbon having a bonding matrix material with a relatively low Young's modulus according to an embodiment of the present invention and the transmission loss after cable formation of a partially bonded optical fiber ribbon having a conventional bonding matrix material with a relatively high Young's modulus. [Figure 6A] FIG. 1 is a perspective view of an optical fiber cable or loose tube cable structure including a plurality of partially bonded optical fiber ribbons, in which the intermittently applied bonding matrix material portions of the partially bonded optical fiber ribbons are a low Young's modulus bonding matrix material, according to an embodiment of the present invention. [Figure 6B] FIG. 6B is a cross-sectional view of the optical fiber cable or loose tube cable structure of FIG. 6A including a plurality of partially bonded optical fiber ribbons, wherein the intermittently applied bonding matrix material portions of the partially bonded optical fiber ribbons are a low Young's modulus bonding matrix material, according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE INVENTION
[0008] In the following description, like reference numerals refer to like components to enhance understanding of the present invention through the description of the drawings. Also, while specific features, configurations, and arrangements are discussed below, it should be understood that such is done for illustrative purposes only. Those skilled in the art will recognize that other steps, configurations, and arrangements are useful without departing from the spirit and scope of the present invention.
[0009] FIG. 1 is a perspective view of a four-fiber partially bonded optical fiber ribbon or rollable ribbon 30. The optical fiber ribbon 30 includes a plurality of optical fibers 32 arranged linearly in a ribbon configuration, each having a glass portion 34 and a coating portion 36. In the optical fiber ribbon 30, the optical fibers 32 are intermittently covered with bonding or ribbon matrix material portions 38. As shown, the matrix material portions 38 are applied (uniformly or non-uniformly) along various portions of the outer surfaces of the optical fibers 32 between adjacent optical fibers 32 and bonded thereto. The matrix material portions 38 are applied across portions of adjacent optical fibers in a manner such that the bonding matrix material is sufficiently dense to allow the resulting partially bonded optical fiber ribbon to lie substantially flat, but sparsely enough to allow the resulting partially bonded optical fiber ribbon to be wound into a substantially circular shape.
[0010] 2 is a top view of an eight-fiber bonded optical fiber ribbon or rollable ribbon 40. The optical fiber ribbon 40 includes a plurality of optical fibers 42 arranged linearly in a ribbon configuration, each optical fiber 42 having a fiber portion and a coating portion surrounding the fiber portion. The optical fiber ribbon 40 also includes a plurality of bonding or ribbon matrix material portions 44 applied in a suitable manner to bond various portions between adjacent optical fibers 42. As shown, the matrix material portions 44 may be applied in a staggered uniform pattern across the optical fibers 42; however, the matrix material portions 44 may be applied to the optical fibers 42 in a manner that allows adjacent optical fibers 42 to remain connected to each other, thus remaining an optical fiber ribbon, but that allows the optical fiber ribbon 40 to be wound and / or folded into one of a plurality of more closely packed unit shapes.
[0011] The matrix material portions 44 may be applied in a repeating pattern along adjacent optical fibers 42. According to an embodiment of the present invention, each matrix material portion 44 is about 5 millimeters (mm) to about 20 millimeters (mm) in length. Also according to an embodiment of the present invention, the distance, or pitch, between the matrix material portions 44 along the same adjacent optical fiber 42 is about 20 millimeters (mm) to about 100 millimeters (mm). For example, according to an embodiment of the present invention, the distance, or pitch, between the matrix material portions 44 along the same adjacent optical fiber 42 is about 40 millimeters (mm).
[0012] According to an embodiment of the present invention, the amount of matrix material used in a partially bonded optical fiber ribbon is about 0.010 kilograms (kg) to about 0.030 kilograms (kg) per kilometer (km) of optical fiber ribbon. The amount of matrix material used in a partially bonded optical fiber ribbon depends on the distance (pitch) between the matrix material portions 44 and the length of each of the matrix material portions 44. According to an embodiment of the present invention, for a partially bonded optical fiber ribbon having matrix material portions 44 that are 5 to 20 mm in length and spaced about 40 mm apart, the amount of matrix material used in the partially bonded optical fiber ribbon is about 0.024 kg per km of optical fiber ribbon.
[0013] 3A is a perspective view of a partially bonded or rollable optical fiber ribbon 50 prior to being rolled, in accordance with an embodiment of the present invention. The optical fiber ribbon 50 includes a plurality of optical fibers 52, e.g., optical fibers 52A-D, for a four-fiber rollable optical fiber ribbon. Prior to being rolled, the optical fibers 52A-D within the optical fiber ribbon 50 exist as a linear array of partially bonded optical fibers. The optical fiber ribbon 50 also includes a plurality of bond or ribbon matrix material portions 54, e.g., matrix material portions 54A-B, which are applied in a suitable manner and bonded at various locations between adjacent optical fibers 52.
[0014] 3B is a perspective view of the optical fiber ribbon 50 of FIG. 3A after being wound, in accordance with an embodiment of the present invention. As shown, the optical fibers 52A-D are wound and / or folded into a more densely organized unit shape, for example, a generally circular shape as shown. As mentioned above, due to the particular structure of the rollable optical fiber ribbon 50, for example, being an optical fiber ribbon having a partially bonded optical fiber ribbon or other suitable structure, the rollable optical fiber ribbon 50 can be wound and / or folded into a more densely organized unit shape.
[0015] Conventionally, the material used for the bonding or ribbon matrix portion can be any suitable material for bonding the linear array of optical fibers together into an optical fiber ribbon, including the properties described above. For example, the bonding matrix material can be any suitable UV-curable resin, thermosetting resin, thermoplastic resin, or other suitable bonding matrix material. Also, conventionally, bonding matrix materials typically have a Young's modulus in the range of about 40 to 600 megapascals (MPa) or Newtons per millimeter squared (N / mm squared).
[0016] As discussed above, in conventional partially bonded or rollable optical fiber ribbons, the lack of a uniform bond or ribbon matrix material that completely covers all portions of each optical fiber can make one or more of the optical fibers relatively sensitive to optical signal transmission loss. Additionally, the relatively high Young's modulus of the bond or ribbon matrix material further contributes to optical signal transmission loss.
[0017] According to an embodiment of the present invention, a partially bonded or rollable optical fiber ribbon includes a bond or ribbon matrix material portion having a relatively low Young's modulus, for example, a Young's modulus of about 0.2 MPa. The partially bonded or rollable optical fiber ribbon includes two or more optical fibers arranged adjacent to one another in a linear array and a bond or ribbon matrix material applied to at least a portion of the outer surface of at least two adjacent optical fibers, the bond or ribbon matrix material having a relatively low Young's modulus. According to an embodiment of the present invention, the matrix material portion with a relatively low Young's modulus induces less external stress on the optical fibers to which it is bonded, thus reducing the effect of the matrix material on optical signal transmission loss of the optical fibers.
[0018] According to embodiments of the present invention, the bond or ribbon matrix material can be any suitable material for bonding a linear array of optical fibers into an optical fiber ribbon and having a relatively low Young's modulus, for example, a Young's modulus in the range of about 0.1 to 30 megapascals (MPa) or Newtons per millimeter (N / mm). For example, the bond or ribbon matrix material can be any suitable ultraviolet curable resin, thermosetting resin, thermoplastic resin, epoxy resin, or other suitable bond or ribbon matrix material having a relatively low Young's modulus, for example, in the range of about 0.1 to 30 MPa.
[0019] The bonding or ribbon matrix material typically consists of four components: (1) an oligomer (about 50-70% of the total volume) to control Young's modulus and optionally viscosity, (2) a monomer (about 15-40% of the total volume) to control viscosity and optionally Young's modulus, (3) a release or slip agent (about 1-10% of the total volume) to facilitate release or prevent sticking, and (4) a photoinitiator (about 1-6% of the total volume) to promote curing and / or allow all components to react and / or mix with one another. In accordance with embodiments of the present invention, an oligomer is used that provides a bonding or ribbon matrix material with a lower Young's modulus compared to that of conventional bonding or ribbon matrix materials.
[0020] Depending on which type of oligomer is used in the bond or ribbon matrix material, adjusting the amount of a particular oligomer as a percentage of the total volume of the bond or ribbon matrix material can increase or decrease the Young's modulus of the bond or ribbon matrix material. For example, for oligomers that have a relatively low Young's modulus value compared to other oligomers, increasing the amount of the relatively low Young's modulus oligomer as a percentage of the total volume of the bond or ribbon matrix material will decrease the overall Young's modulus of the bond or ribbon matrix material. According to embodiments of the present invention, the relatively low Young's modulus oligomer is used in a suitable amount as a percentage of the total volume of the bonding or ribbon matrix material that results in a lower Young's modulus of the bonding or ribbon matrix material compared to that of conventional bonding or ribbon matrix materials.
[0021] Additionally, the amount of curing of the bond or ribbon matrix material can affect the Young's modulus of the bond or ribbon matrix material. Typically, more curing (e.g., higher curing force and / or longer curing time) results in a higher Young's modulus of the bond or ribbon matrix material. According to one embodiment of the present invention, the bond or ribbon matrix material is cured in a manner that results in a lower Young's modulus of the bond or ribbon matrix material compared to the Young's modulus of conventional bond or ribbon matrix materials.
[0022] 4 is a graph 60 of transmission loss on a ribbon spool for a partially bonded or rollable optical fiber ribbon having a relatively low Young's modulus matrix material in accordance with an embodiment of the present invention and a partially bonded or rollable optical fiber ribbon having a conventional relatively high Young's modulus matrix material. The transmission loss of the partially bonded or rollable optical fiber ribbon having a relatively low Young's modulus matrix material in accordance with an embodiment of the present invention is generally shown as loss 62. The transmission loss of the partially bonded or rollable optical fiber ribbon having a conventional relatively high Young's modulus matrix material is generally shown as loss 64. The transmission loss of each optical fiber ribbon is measured in decibels per kilometer of fiber (dB / km) for optical transmission at 1300 nanometers (nm).
[0023] As shown in graph 60, the loss 62 of the partially bonded or rollable optical fiber ribbon having a relatively low Young's modulus matrix material is about 0.78 dB / km to about 0.96 dB / km. In comparison, the loss 64 of the partially bonded or rollable optical fiber ribbon having a conventional relatively high Young's modulus matrix material is about 0.85 dB / km to about 1.24 dB / km. Thus, for partially bonded or rollable optical fiber ribbons fabricated on ribbon spools, the use of a relatively low Young's modulus matrix material to partially bond the optical fiber ribbons results in lower optical transmission loss than the use of a relatively high Young's modulus matrix material to partially bond the optical fiber ribbons.
[0024] 5 is a graph 70 of the cabled transmission loss of a partially bonded or rollable optical fiber ribbon having a relatively low Young's modulus matrix material according to an embodiment of the present invention and a conventional partially bonded or rollable optical fiber ribbon having a relatively high Young's modulus matrix material. The loss is shown for various temperatures, e.g., 23° C., −40° C., and 70° C. The loss of each optical fiber ribbon is measured in decibels per kilometer of fiber (dB / km) for 1300 nanometer (nm) optical transmission.
[0025] The losses of partially bonded or rollable optical fiber ribbons having a relatively low Young's modulus matrix material according to embodiments of the present invention are generally shown as loss 72 (at 23° C.), losses 76 and 86 (at −40° C.), and losses 82 and 92 (at 70° C.). The losses of partially bonded or rollable optical fiber ribbons having a conventional relatively high Young's modulus matrix material are generally shown as loss 74 (at 23° C.), losses 78 and 88 (at −40° C.), and losses 84 and 94 (at 70° C.).
[0026] As shown in graph 70, the loss 72 of the partially bonded or rollable optical fiber ribbon having a relatively low Young's modulus matrix material at 23° C. is about 0.51 dB / km to about 0.65 dB / km. In comparison, the ribbon loss 74 of the conventional partially bonded or rollable optical fiber ribbon having a relatively high Young's modulus matrix material at 23° C. is about 0.61 dB / km to about 0.81 dB / km.
[0027] At −40° C., the losses 76, 86 of the partially bonded or rollable optical fiber ribbons having a relatively low Young's modulus matrix material are about 0.59 dB / km to about 0.74 dB / km (first measurement) and about 0.62 dB / km to about 0.74 dB / km (second measurement). In comparison, at −40° C., the losses 78, 88 of the conventional partially bonded or rollable optical fiber ribbons having a relatively high Young's modulus matrix material are about 0.67 dB / km to about 0.99 dB / km (first measurement) and about 0.69 dB / km to about 0.98 dB / km (second measurement).
[0028] At 70° C., the losses 82, 92 of the partially bonded or rollable optical fiber ribbons having a relatively low Young's modulus matrix material are about 0.52 dB / km to about 0.57 dB / km (first measurement) and about 0.50 dB / km to about 0.56 dB / km (second measurement). In comparison, the losses 84, 94 of the conventional partially bonded or rollable optical fiber ribbons having a relatively high Young's modulus matrix material at 70° C. are about 0.56 dB / km to about 0.67 dB / km (first measurement) and about 0.58 dB / km to about 0.65 dB / km (second measurement).
[0029] Thus, for cabled partially bonded or rollable optical fiber ribbons, the use of a relatively low Young's modulus matrix material to partially bond the optical fiber ribbons results in lower optical transmission loss than the use of a relatively high Young's modulus matrix material to partially bond the optical fiber ribbons. Furthermore, the lower optical transmission loss of partially bonded cabled or rollable optical fiber ribbons having a relatively low Young's modulus matrix material compared to partially bonded cabled or rollable optical fiber ribbons having a relatively high Young's modulus matrix material occurs consistently over several different temperatures.
[0030] 6 is a perspective view of a fiber optic cable or loose tube cable structure 100 incorporating partially bonded optical fiber ribbons in accordance with an embodiment of the present invention. In accordance with an embodiment of the present invention, the partially bonded optical fiber ribbons have a relatively low Young's modulus, for example, about 0.2 MPa or N / mm 2 The adhesive matrix material includes portions of intermittently applied adhesive matrix material having a thickness of 100 μm.
[0031] The cable structure 100 includes a plurality of multi-fiber unit tubes or loose tubes 102 disposed within a cable jacket 104. Each of the multi-fiber unit tubes 102 is substantially circular and sized to receive a plurality of partially spliced optical fiber ribbons 106 therein. The plurality of multi-fiber unit tubes 102 may be disposed around a central strength member 108. Alternatively, a second plurality of multi-fiber unit tubes (not shown) may be disposed around the first plurality of multi-fiber unit tubes 102.
[0032] The cable structure 100 may include a layer 112 of reinforcing strength yarns (e.g., aramid or glass fiber) between the cable jacket 104 and the multi-fiber unit tube 102. The cable structure 100 may also include a superabsorbent tape (not shown) between the cable jacket 104 and the multi-fiber unit tube 102.
[0033] The multi-core unit tube 102 can be made of any suitable material. For example, the multi-fiber unit tube 102 can be made of polypropylene, polybutylene terephthalate (PBT), polyethylene, nylon, polycarbonate, thermoplastic polyurethane (TPU), poly(vinyl chloride) (PVC), or other suitable material(s). Flame retardant additives can be incorporated into the multi-fiber tube 102 to help provide fire resistance. The multi-fiber unit tube 102 can be a homogenous tube or a multi-layer tube produced by coextrusion.
[0034] The jacket 104 can be made of any suitable material. For example, the jacket 104 can be made of polyethylene, thermoplastic polyurethane, nylon 12, or other suitable materials. Flame retardant additives can be incorporated into the jacket 104 to provide fire resistance.
[0035] 6, the plurality of multi-fiber unit tubes 102 may be arranged within the jacket 104 as a first (inner) plurality of multi-fiber unit tubes 102 generally disposed about a central strength member 108 to form a substantially circular cross-section. Alternatively, a second (outer) plurality of multi-fiber unit tubes (not shown) may be generally disposed about the first plurality of multi-fiber unit tubes 102 in a manner that also forms a substantially circular cross-section.
[0036] According to an embodiment of the present invention, the cable structure 100 can include a total of 72 to 3456 optical fibers. For example, a 72-fiber cable structure includes six multi-fiber unit tubes 102, each having a 12-fiber partially spliced optical fiber ribbon. According to an embodiment of the present invention, the cable structure 100 can include 144 optical fibers, i.e., 12 multi-fiber unit tubes 102, each having a 12-fiber partially spliced optical fiber ribbon therein.
[0037] It will be apparent to those skilled in the art that numerous modifications and substitutions can be made to the embodiments of the invention described herein without departing from the spirit and scope of the invention, as defined by the appended claims and their full range of equivalents.
Claims
1. A partially spliced optical fiber ribbon, a plurality of optical fibers arranged adjacently in a linear array; a plurality of bonding matrix material portions applied to at least a portion of the outer surfaces of at least two adjacent said optical fibers; the plurality of bonding matrix material portions having a low Young's modulus; the plurality of bonding matrix material portions are applied to at least a portion of an outer surface of the at least two adjacent optical fibers such that the linear array of optical fibers forms a partially bonded optical fiber ribbon; The optical fiber ribbon, wherein the Young's modulus of the plurality of bonding matrix material portions is within a range of about 0.1 megapascals (MPa) to about 0.2 MPa.
2. 2. The optical fiber ribbon according to claim 1, wherein the bonding matrix material includes an oligomer for controlling the Young's modulus of the bonding matrix material.
3. 3. The optical fiber ribbon of claim 2, wherein the oligomer is in the range of about 50 percent to about 70 percent of the total volume of the bonding matrix material.
4. 2. The optical fiber ribbon according to claim 1, wherein the bonding matrix material includes a monomer for controlling the Young's modulus of the bonding matrix material.
5. 2. The optical fiber ribbon of claim 1, wherein said plurality of bonding matrix material portions are about 5 millimeters (mm) to about 20 millimeters (mm) in length.
6. 2. The optical fiber ribbon of claim 1, wherein the distance between the portions of the bonding matrix material along the two adjacent optical fibers is from about 20 millimeters (mm) to about 20 millimeters (mm).
7. 2. The optical fiber ribbon of claim 1, wherein the distance between the portions of the bonding matrix material along the two adjacent optical fibers is about 40 millimeters (mm).
8. 10. The optical fiber ribbon of claim 1, wherein said optical fiber ribbon has about 0.010 to about 0.030 kilograms (kg) of said bonding matrix material per kilometer (km) of said optical fiber ribbon.
9. 10. The optical fiber ribbon of claim 1, wherein said optical fiber ribbon has approximately 0.024 kilograms (kg) of said bonding matrix material per kilometer (km) of said optical fiber ribbon.
10. 2. The optical fiber ribbon according to claim 1, wherein the bonding matrix material is an ultraviolet curable resin, a thermosetting resin, a thermoplastic resin, or an epoxy resin.
11. a plurality of multi-fiber unit tubes each substantially circular and sized to receive a plurality of optical fibers; a plurality of partially spliced optical fiber ribbons disposed within at least one multi-fiber tube; a jacket surrounding the plurality of multi-fiber unit tubes; the plurality of partially bonded optical fiber ribbons are partially bonded using a plurality of portions of bonding matrix material applied to at least a portion of the outer surfaces of at least two adjacent optical fibers; the bonding matrix material portion has a low Young's modulus; The fiber optic cable, wherein the Young's modulus of the plurality of bonding matrix material portions is within a range of about 0.1 megapascals (MPa) to about 0.2 MPa.
12. 12. The fiber optic cable of claim 11, wherein the bond matrix material includes an oligomer for controlling the Young's modulus of the bond matrix material.
13. 13. The fiber optic cable of claim 12, wherein the oligomer is in the range of about 50 percent to about 70 percent of the total volume of the bonding matrix material.
14. 12. The fiber optic cable of claim 11, wherein the bond matrix material includes a monomer to control the Young's modulus of the bond matrix material.
15. 12. The fiber optic cable of claim 11, wherein the optical fiber ribbon has approximately 0.024 kilograms (kg) of the bonding matrix material per kilometer (km) of the optical fiber ribbon.
16. 12. The optical fiber cable of claim 11, wherein the plurality of multi-fiber unit tubes further includes 12 of the multi-fiber unit tubes, each of the 12 multi-fiber unit tubes including 12 partially joined optical fiber ribbons.
17. 12. The fiber optic cable of claim 11, wherein at least one of the partially bonded optical fiber ribbons is bonded such that the optical fiber ribbon is wound in a substantially circular configuration.
Citation Information
Patent Citations
Optical fiber ribbon, optical cable, and method for manufacturing optical fiber ribbon
CN111175887A
Coated optical fiber
JP2004054138A
A circular, small-diameter optical cable with a ribbon-shaped optical fiber structure.
JP2015517679A
Optical fiber ribbon
JP2017062431A
rollable fiber optic ribbon
JP2018526687A