Cathode active material, method for producing the same, and method for using the same
JP7872957B2Active Publication Date: 2026-06-11BASF SE +1
Patent Information
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- BASF SE
- Filing Date
- 2021-11-05
- Publication Date
- 2026-06-11
Smart Images

Figure 0007872957000003 
Figure 0007872957000004 
Figure 0007872957000005
Abstract
Formula x Li2Ni 1-y1-y2 Mn y1 M 1 y2 O3 (1-x) LiNi 1-z M 2 z O2 (In the formula, x is in the range of 0.01 to 0.5, and z is in the range of 0 to 0.5, M 1 is selected from Ti, Zr, Sn, Ge, Ta, Nb, Sb, W, Mo, and a combination of at least two of the above; M 2 is at least one of Co, Al, Mg, Fe, or Mn, or a combination of at least two of the above; 0.1≦y1≦0.75, 0≦y2≦0.05) A method for producing a complex oxide according to the present invention, The method comprises the steps of: (a) General formula x Ni 1-y1-y2 Mn y1 M 1 y (1-x)Ni 1-z M 2 z TM particulate hydroxide, oxide or oxyhydroxide, or M 1 and / or M 2 providing a corresponding species that does not contain (b) adding a lithium source; (c) heat treating the mixture obtained from step (b) in an oxygen-containing atmosphere in two steps: (c) heating the mixture obtained from step (b) to 680-800° C. in an atmosphere containing oxygen in the range of 10-100% by volume; and (e) heating the intermediate from step (c) to 450-580° C. in an atmosphere containing at least 90% by volume of oxygen; Includes.
Need to check novelty before this filing date? Find Prior Art