Electrochemical cell, electrochemical cell device, module, and module accommodation device
Patent Information
- Application Number
- JP2024508287
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Priority Date
- 2023-03-17
- Filing Date
- 2023-03-17
- Publication Date
- 2024-11-26
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Current fuel cell stack devices face limitations in power generation performance due to chromium release from metal bodies into oxidizing atmospheres during high-temperature operation, leading to decreased efficiency and durability.
An electrochemical cell with a chromium-containing metal body coated with a conductive oxide film that reduces chromium release, combined with a cell stack device and module housing configuration to enhance power generation performance.
The oxide coating improves power generation performance by preventing chromium release, enhancing oxidation resistance and durability, and the modular design optimizes fuel cell performance and operation.
Abstract
Description
Electrochemical cell, electrochemical cell device, module, and module housing device
[0001] The present disclosure relates to electrochemical cells, electrochemical cell devices, modules and module housing devices.
[0002] In recent years, various fuel cell stack devices having multiple fuel cell units have been proposed as next-generation energy sources. A fuel cell unit is a type of electrochemical cell that can generate electric power using a fuel gas such as a hydrogen-containing gas and an oxygen-containing gas such as air.
[0003] JP 2015-162357 A
[0004] An electrochemical cell according to one aspect of the embodiment includes an element unit, a metal body, and an oxide coating material. The metal body contains chromium and is electrically connected to the element unit. The oxide coating material coats the metal body and is exposed to an oxidizing atmosphere. The oxide coating material suppresses the release of chromium into the oxidizing atmosphere. The oxide coating material includes at least a conductive first coating material.
[0005] The electrochemical cell device of the present disclosure also includes a cell stack including the electrochemical cell described above.
[0006] The module of the present disclosure includes the electrochemical cell device described above and a container that houses the electrochemical cell device.
[0007] The module housing device of the present disclosure includes the module described above, an auxiliary device for operating the module, and an exterior case for housing the module and the auxiliary device.
[0008] FIG. 1A is a cross-sectional view showing an example of an electrochemical cell according to the first embodiment. FIG. 1B is a side view of an example of an electrochemical cell according to the first embodiment, viewed from the air electrode side. FIG. 2A is a perspective view showing an example of a cell stack device according to the first embodiment. FIG. 2B is a cross-sectional view taken along line X-X shown in FIG. 2A. FIG. 2C is a top view showing an example of a cell stack device according to the first embodiment. FIG. 3 is an external perspective view showing an example of a module according to the first embodiment. FIG. 4 is an exploded perspective view schematically showing an example of a module housing device according to the first embodiment. FIG. 5 is a cross-sectional view showing an example of an electrochemical cell according to the second embodiment. FIG. 6 is a cross-sectional view showing an example of an electrochemical cell according to the third embodiment. FIG. 7 is a cross-sectional view showing an example of an electrochemical cell according to the fourth embodiment. FIG. 8 is a cross-sectional view showing an example of an electrochemical cell according to the fifth embodiment. FIG. 9 is a cross-sectional view showing an example of an electrochemical cell according to the sixth embodiment.
[0009] The above-described fuel cell stack device has room for improvement in terms of power generation performance.
[0010] Therefore, it is desired to provide an electrochemical cell, an electrochemical cell device, a module, and a module housing device that can improve performance.
[0011] Hereinafter, embodiments of an electrochemical cell, an electrochemical cell device, a module, and a module housing device disclosed in the present application will be described in detail with reference to the accompanying drawings. However, the present invention is not limited to the embodiments described below.
[0012] It should also be noted that the drawings are schematic and that the dimensional relationships and ratios of elements may differ from reality. Furthermore, the drawings may contain parts whose dimensional relationships and ratios differ from one another.
[0013] First Embodiment Cell Configuration First, an electrochemical cell according to a first embodiment will be described using a solid oxide fuel cell as an example, with reference to Figures 1A and 1B. The electrochemical cell device may include a cell stack having a plurality of electrochemical cells. An electrochemical cell device having a plurality of electrochemical cells will be simply referred to as a cell stack device.
[0014] Fig. 1A is a cross-sectional view showing an example of an electrochemical cell according to the first embodiment. Fig. 1B is a side view of the example of the electrochemical cell according to the first embodiment, seen from the air electrode side. Note that Figs. 1A and 1B show enlarged views of parts of each component of the cell 1. Hereinafter, the electrochemical cell may also be simply referred to as a cell.
[0015] 1A, the cell 1 includes a metal body 2, an element section 4, and a sealing material 8. The element section 4 includes a fuel electrode 5, a solid electrolyte layer 6, and a cathode 7.
[0016] The metal body 2 has a first surface 201 and a second surface 202 that face each other in the thickness direction T, and a third surface 203 and a fourth surface 204 that connect the first surface 201 and the second surface 202 together.
[0017] The metal body 2 also has a gas flow path 2a and an opening 2b. The gas flow path 2a is located between the first surface 201 and the second surface 202 and is a space extending in the longitudinal direction L. The opening 2b is a through-hole having a first end opening to the first surface 201 and a second end communicating with the gas flow path 2a. The fuel gas flowing through the gas flow path 2a is supplied to the anode 5 of the element section 4 through the opening 2b. The diameter of the opening 2b may be, for example, 0.1 mm to 0.5 mm, particularly 0.3 mm to 0.4 mm. The aperture ratio in the region where the opening 2b is formed may be, for example, 10% or more.
[0018] The metal body 2 is a member made of a metal containing chromium. The metal body 2 is electrically conductive. The metal body 2 may be, for example, a stainless steel such as a ferritic stainless steel or an austenitic stainless steel having high heat resistance. The metal body 2 may be, for example, a nickel-chromium alloy or an iron-chromium alloy. The metal body 2 may contain, for example, a metal oxide. The metal body 2 may have a structure in which a plurality of plate materials, such as a plate material having a first surface 201 and a plate material having a second surface 202, are stacked and the ends are welded.
[0019] The element portion 4 is located on the first surface 201 side of the metal body 2. The element portion 4 is located so as to face the first surface 201. The element portion 4 is fixed to the metal body 2 via an adhesive 3 and is supported by the metal body 2.
[0020] The element section 4 has an anode 5, a solid electrolyte layer 6, and an air electrode 7. A generally known material can be used for the anode 5. The anode 5 is made of a porous conductive ceramic, such as calcium oxide, magnesium oxide, or ZrO in which a rare earth element oxide is solid-solved. 2 and Ni and / or NiO may be used. The rare earth element oxide may contain, for example, a plurality of rare earth elements selected from Sc, Y, La, Nd, Sm, Gd, Dy, and Yb. Calcium oxide, magnesium oxide, or ZrO in which a rare earth element oxide is solid-solved may be used. 2 is sometimes referred to as stabilized zirconia. The stabilized zirconia may include partially stabilized zirconia. The fuel electrode 5 includes metal particles. The electrode including the metal particles may also be referred to as a first electrode.
[0021] The solid electrolyte layer 6 is an electrolyte and transfers ions between the fuel electrode 5 and the air electrode 7. At the same time, the solid electrolyte layer 6 has gas barrier properties and makes it difficult for leakage of fuel gas and oxygen-containing gas to occur.
[0022] The material of the solid electrolyte layer 6 is, for example, ZrO in which 3 mol % to 15 mol % of rare earth element oxide is dissolved. 2The rare earth element oxide may contain, for example, one or more rare earth elements selected from Sc, Y, La, Nd, Sm, Gd, Dy, and Yb. The solid electrolyte layer 6 may be, for example, ZrO in which Yb, Sc, or Gd is solid-solved. 2 and CeO in which La, Nd or Yb is solid-solved. 2 and BaZrO in which Sc or Yb is solid-solved. 3 and BaCeO in which Sc or Yb is solid-solved. 3 may include:
[0023] The air electrode 7 is gas permeable. The open porosity of the air electrode 7 may be, for example, in the range of 20% to 50%, particularly 30% to 50%. The open porosity of the air electrode 7 may also be referred to as the porosity of the air electrode 7.
[0024] There are no particular limitations on the material of the air electrode 7 as long as it is a material generally used for air electrodes. 3 Conductive ceramics such as perovskite oxides may also be used.
[0025] The material of the air electrode 7 may be, for example, a composite oxide in which Sr (strontium) and La (lanthanum) coexist at the A site. Examples of such composite oxides include La x Sr 1-x Co y Fe 1-y O 3 , La x Sr 1-x MnO 3 , La x Sr 1-x FeO 3 , La x Sr 1-x CoO 3 Here, x is 0<x<1, and y is 0<y<1. The air electrode 7 may be referred to as a second electrode in contrast to a first electrode containing metal particles.
[0026] The element section 4 may also have an intermediate layer located between the solid electrolyte layer 6 and the air electrode 7. When the element section 4 has an intermediate layer, the intermediate layer functions, for example, as a diffusion suppression layer. When Sr (strontium) contained in the air electrode 7 diffuses into the solid electrolyte layer 6, SrZrO 3 The intermediate layer makes it difficult for Sr to diffuse, resulting in a resistive layer of SrZrO 3 This makes it difficult for
[0027] The material of the intermediate layer is not particularly limited as long as it generally prevents diffusion of elements between the air electrode 7 and the solid electrolyte layer 6. The material of the intermediate layer is, for example, cerium oxide (CeO) in which rare earth elements other than Ce (cerium) are dissolved. 2 ) may be included. Examples of such rare earth elements include Gd (gadolinium) and Sm (samarium).
[0028] The sealant 8 is located on the end surface of the anode 5. The sealant 8 has gas barrier properties and is located so as to cover the periphery of the anode 5, thereby sealing off the flow of fuel gas between the anode 5 and the outside. The sealant 8 may have a porosity of, for example, 5% or less. When the sealant 8 has a porosity of 5% or less, the flow of fuel gas between the anode 5 and the outside becomes difficult. The porosity of the sealant 8 may be, for example, the average value of the porosities in at least three arbitrary cross sections of the sealant 8. As shown in FIGS. 1A and 1B , the sealant 8 may be located on the end surfaces of the anode 5 and the solid electrolyte layer 6.
[0029] The sealing material 8 has electrical insulation properties. Hereinafter, electrical insulation may be simply referred to as insulation. For example, oxides with low electrical conductivity, such as glass, may be used as the sealing material 8. Herein, "having insulation properties" or "low electrical conductivity" means that the electrical conductivity is 1 / 10 or less of that of the solid electrolyte layer 6. The electrical conductivity of the sealing material 8 may be, for example, 0.2 S / m or less, particularly 0.002 S / m or less at room temperature (25°C). The material of the sealing material 8 may be, for example, amorphous glass or crystallized glass. Crystallized glass, for example, is SiO 2 -CaO system, MgO-B 2 O3 System, La 2 O 3 -B 2 O 3 -MgO-based, La 2 O 3 -B 2 O 3 -ZnO-based, SiO 2 -CaO-ZnO system materials, etc., may be used, and in particular SiO 2 - MgO-based materials may also be used.
[0030] The cell 1 may also have an adhesive 3 located between the metal body 2 and the element section 4. The adhesive 3 is located between the first surface 201 of the metal body 2 and the fuel electrode 5, and bonds the metal body 2 and the element section 4. The adhesive 3 has, for example, electrical conductivity. The adhesive 3 may have, for example, gas permeability. The cell 1 may have, for example, chromium oxide (Cr 2 O 3 ) may be further positioned.
[0031] The adhesive 3 is made of, for example, conductive particles such as Ni and TiO 2 , rare earth element oxides (Y 2 O 3 , CeO 2 etc.), transition metal oxides (Fe 2 O 3 , CuO, etc.) The adhesive 3 may be located so as to be in contact with the first surface 201 where the opening 2 b is not located. The anode 5 may be fixed to the metal body 2 without the adhesive 3.
[0032] Of the first surface 201 to the fourth surface 204 located on the surface of the metal body 2, the portions that are not in contact with the adhesive 3 or the element portion 4 are exposed to the external space. This external space is the space where the air electrode 7 of the cell 1 is exposed, and is filled with an oxygen-containing gas. In other words, the external space is an oxidizing atmosphere.
[0033] When a cell 1 is used in such an environment, the chromium (Cr) contained in the metal body 2 may be desorbed into the oxidizing atmosphere and adhere to the element portion 4 during high-temperature operation, which may result in a decrease in power generation performance.
[0034] Therefore, the cell 1 according to this embodiment further includes an oxide coating 9. The oxide coating 9 covers the metal body 2 and is exposed to an oxidizing atmosphere. The oxide coating 9 suppresses the release of chromium from the metal body 2 into the oxidizing atmosphere, thereby improving the power generation performance of the cell 1. Furthermore, the oxide coating 9 makes it difficult for chromium to be released from the metal body 2 into the oxidizing atmosphere, thereby improving the oxidation resistance and durability of the metal body 2. The oxide coating 9 is formed by covering the chromium (II) oxide (Cr 2 O 3 ) may be difficult to grow a coating containing the same.
[0035] The oxide coating 9 may have, for example, a conductive first coating 31. The first coating 31 is an example of a first coating material. The first coating 31 may have a conductivity of 0.005 S / cm or more. The first coating 31 may contain a transition metal oxide, for example, manganese (Mn). The first coating 31 may contain, for example, a composite oxide containing Mn. The composite oxide containing Mn may have a spinel structure. The first coating 31 may be, for example, CoMn 2 O 4 , MnCo 2 O 4 , Mn 1.5 Co 1.5 O 4 , ZnMnCoO 4 In such a spinel-type composite oxide containing Mn and Co and / or Zn, the composition ratio of Mn to Co and / or Zn can be selected arbitrarily. This reduces the internal resistance of the element part 4 compared to a case where the first coating 31 is not provided, thereby improving the power generation performance of the cell 1. Note that the first coating 31 may contain, for example, a small amount of Cr 2 O 3 , Al 2 O 3 , ZrO 2 The Mn-containing composite oxide may further contain Al, Zr, etc.
[0036] Such a cell 1 can be obtained as follows. For example, a laminate formed by stacking and firing a molded sheet of the anode 5 and a molded sheet of the solid electrolyte layer 6 is prepared. A metal body 2 having the first coating 31 (or a molded film of the first coating 31) is also prepared. The anode 5 surface of the laminate is bonded to the first surface 201 of the metal body 2, which has the opening 2b, via an adhesive 3. An intermediate layer and a cathode 7 are then formed on the solid electrolyte layer 6, and a sealant 8 is further provided on the side surface of the element unit 4, thereby obtaining the cell 1. The sealant 8 may be located only on the side surface of the anode 5 of the element unit 4. The sealant 8 may be located on at least a portion of the side surface of the solid electrolyte layer 6 and at least a portion of the surface of the solid electrolyte layer 6. The sealant 8 may be located on the adhesive 3 or on at least a portion of the first coating 31. The first coating 31 does not have to be located on the first surface 201 of the metal body 2, which has the opening 2b.
[0037] The laminate of the anode 5 and the solid electrolyte layer 6 may be fabricated, for example, as follows: A mixture of Ni or NiO powder, stabilized zirconia powder, an organic solvent, and a binder is formed into a sheet to obtain a sheet compact of the anode 5. A mixture of stabilized zirconia powder, an organic solvent, and a binder is formed into a sheet on the sheet compact of the anode 5 to obtain a laminate compact. The obtained laminate compact is fired to obtain a laminate of the anode 5 and the solid electrolyte layer 6.
[0038] The first coating 31 may be formed as follows. For example, a paste containing a mixture of a Mn-containing composite oxide powder, a solvent, and a binder is applied to the surface of the metal body 2 that does not have the opening 2b and dried to form a molded film of the first coating 31. The surface of the fuel electrode 5 of the laminate is then bonded to the surface of the metal body 2 that has the opening 2b using an adhesive 3, and the resulting composite is fired at, for example, 900°C to 1200°C to obtain a bonded body of the metal body 2 and the laminate having the first coating 31. A molded body for the intermediate layer is then formed on the surface of the solid electrolyte layer 6 of the bonded body, and fired at, for example, 1000°C to 1200°C to form the intermediate layer. The air electrode 7 is then formed on the intermediate layer, and fired at, for example, 1000°C to 1200°C to form the air electrode 7, thereby obtaining the cell 1.
[0039] The anode 5, solid electrolyte layer 6, intermediate layer, and cathode 7 may be formed in this order directly on the first surface 201 having the opening 2b of the metal body 2 having the first coating 31 or a formed film of the first coating 31. Alternatively, a laminated sheet to become the element portion 4 may be prepared in advance, and the laminated sheet may be bonded to the first surface 201 having the opening 2b of the metal body 2, and then fired.
[0040] The sealing material 8 can be formed by applying a paste of the above-mentioned glass powder to a predetermined portion, drying it, and then heat treating it at a temperature of 800 to 900°C, for example.
[0041] <Configuration of Cell Stack Device> Next, a cell stack device according to this embodiment using the above-described cell 1 will be described with reference to Figures 2A to 2C. Figure 2A is a perspective view showing an example of a cell stack device according to the first embodiment, Figure 2B is a cross-sectional view taken along line X-X shown in Figure 2A, and Figure 2C is a top view showing an example of a cell stack device according to the first embodiment.
[0042] As shown in FIG. 2A, the cell stack device 10 includes a cell stack 11 having a plurality of cells 1 arranged (stacked) in the thickness direction T of the cells 1 (see FIG. 1A), and a fixing member 12.
[0043] The fixing member 12 has a fixing material 13 and a support member 14. The support member 14 supports the cell 1. The fixing material 13 fixes the cell 1 to the support member 14. The support member 14 also has a support 15 and a gas tank 16. The support 15 and the gas tank 16, which are the support member 14, are made of metal and are electrically conductive.
[0044] 2B, the support body 15 has insertion holes 15a into which the lower ends of the plurality of cells 1 are inserted. The lower ends of the plurality of cells 1 and the inner wall of the insertion holes 15a are joined with fixing material 13.
[0045] The gas tank 16 has an opening for supplying a reaction gas to the cells 1 through the insertion holes 15a, and a recessed groove 16a located around the opening. The outer peripheral edge of the support 15 is joined to the gas tank 16 by a bonding material 21 filled in the recessed groove 16a of the gas tank 16.
[0046] In the example shown in Fig. 2A, fuel gas is stored in an internal space 22 formed by a support 15, which is the support member 14, and a gas tank 16. A gas circulation pipe 20 is connected to the gas tank 16. The fuel gas is supplied to the gas tank 16 through this gas circulation pipe 20, and is supplied from the gas tank 16 to a gas flow path 2a (see Fig. 1A) inside the cell 1. The fuel gas supplied to the gas tank 16 is generated in a reformer 102 (see Fig. 3), which will be described later.
[0047] The hydrogen-rich fuel gas can be produced by steam reforming the raw fuel, etc. When the fuel gas is produced by steam reforming, the fuel gas contains water vapor.
[0048] The example shown in Fig. 2A includes two rows of cell stacks 11, two supports 15, and a gas tank 16. Each of the two rows of cell stacks 11 has a plurality of cells 1. Each cell stack 11 is fixed to a corresponding support 15. The gas tank 16 has two through-holes on its top surface. A support 15 is disposed in each through-hole. An internal space 22 is formed by the one gas tank 16 and the two supports 15.
[0049] The shape of the insertion hole 15a is, for example, an oval shape when viewed from above. For example, the length of the insertion hole 15a in the arrangement direction of the cells 1, i.e., the thickness direction T, is greater than the distance between the two end current collecting members 17 located at both ends of the cell stack 11. For example, the width of the insertion hole 15a is greater than the length of the cell 1 in the width direction W (see FIG. 1A ).
[0050] 2B , the joints between the inner walls of the insertion holes 15a and the lower ends of the cells 1 are filled with and solidified with fixing material 13. This bonds and fixes the inner walls of the insertion holes 15a to the lower ends of the multiple cells 1, respectively, and also bonds and fixes the lower ends of the cells 1 to each other. The gas flow paths 2a of each cell 1 communicate with the internal space 22 of the support member 14 at their lower ends.
[0051] A material with low conductivity, such as glass, can be used for the fixing material 13 and the bonding material 21. Specific materials for the fixing material 13 and the bonding material 21 include amorphous glass, and in particular, crystallized glass.
[0052] Examples of the crystallized glass include SiO 2 -CaO system, MgO-B 2 O 3 System, La 2 O 3 -B 2 O 3 -MgO-based, La 2 O 3 -B 2 O 3 -ZnO-based, SiO 2 -CaO-ZnO system materials, etc., may be used, and in particular SiO 2 - MgO-based materials may also be used.
[0053] 2B , a conductive member 18 is interposed between adjacent cells 1 among the plurality of cells 1. The conductive member 18 electrically connects one adjacent cell 1 to the other adjacent cell 1 in series. More specifically, the conductive member 18 connects the fuel electrode 5 of one cell 1 to the air electrode 7 of the other cell 1.
[0054] 2B, an end current collecting member 17 is electrically connected to the cell 1 positioned outermost in the arrangement direction of the multiple cells 1. The end current collecting member 17 is connected to a conductive portion 19 that protrudes outside the cell stack 11. The conductive portion 19 collects electricity generated by power generation in the cells 1 and extracts it to the outside. Note that the end current collecting member 17 is not shown in FIG. 2A.
[0055] 2C, the cell stack device 10 may be a single battery in which two cell stacks 11A, 11B are connected in series. In such a case, the conductive portion 19 of the cell stack device 10 may have a positive terminal 19A, a negative terminal 19B, and a connection terminal 19C.
[0056] The positive terminal 19A is a positive electrode when the power generated by the cell stack 11 is output to the outside, and is electrically connected to the positive-side end current collecting member 17 of the cell stack 11A. The negative terminal 19B is a negative electrode when the power generated by the cell stack 11 is output to the outside, and is electrically connected to the negative-side end current collecting member 17 of the cell stack 11B.
[0057] The connection terminal 19C electrically connects the end current collecting member 17 on the negative electrode side of the cell stack 11A to the end current collecting member 17 on the positive electrode side of the cell stack 11B.
[0058] <Module> Next, a module according to an embodiment of the present disclosure using the above-described cell stack device 10 will be described with reference to Fig. 3. Fig. 3 is an external perspective view showing the module according to the first embodiment. Fig. 3 shows a state in which the front and rear surfaces, which are part of the storage container 101, have been removed and the cell stack device 10 of the fuel cell stored inside has been pulled out to the rear.
[0059] 3, the module 100 includes a storage container 101 and a cell stack device 10 housed in the storage container 101. A reformer 102 is disposed above the cell stack device 10.
[0060] The reformer 102 reforms raw fuel such as natural gas or kerosene to generate fuel gas, which is then supplied to the cell 1. The raw fuel is supplied to the reformer 102 through a raw fuel supply pipe 103. The reformer 102 may include a vaporizer 102a that vaporizes water, and a reformer 102b. The reformer 102b includes a reforming catalyst (not shown) and reforms the raw fuel into fuel gas. Such a reformer 102 can perform steam reforming, a highly efficient reforming reaction.
[0061] The fuel gas produced in the reformer 102 is supplied to the gas flow channel 2 a of the cell 1 (see FIG. 1A) through the gas distribution pipe 20 , the gas tank 16 , and the support member 14 .
[0062] Furthermore, in the module 100 having the above-described configuration, the temperature inside the module 100 during normal power generation reaches approximately 500°C to 1000°C due to the combustion of gas and the power generation of the cells 1.
[0063] In such a module 100, as described above, the module 100 can be configured to house a cell stack device 10 having cells 1 that improve power generation performance, thereby making it possible to create a module 100 with improved power generation performance.
[0064] <Module Enclosure Device> Fig. 4 is an exploded perspective view showing an example of a module enclosure device according to the first embodiment. The module enclosure device 110 according to this embodiment includes an outer case 111, the module 100 shown in Fig. 3, and auxiliary equipment (not shown). The auxiliary equipment operates the module 100. The module 100 and the auxiliary equipment are housed in the outer case 111. Note that some components are omitted in Fig. 4.
[0065] An exterior case 111 of a module accommodating device 110 shown in Fig. 4 has support columns 112 and an exterior plate 113. A partition plate 114 divides the interior of the exterior case 111 into upper and lower sections. The space above the partition plate 114 in the exterior case 111 is a module accommodating chamber 115 that accommodates the module 100, and the space below the partition plate 114 in the exterior case 111 is an auxiliary equipment accommodating chamber 116 that accommodates auxiliary equipment for operating the module 100. Note that in Fig. 4, the auxiliary equipment accommodated in the auxiliary equipment accommodating chamber 116 is not shown.
[0066] The partition plate 114 also has an air flow port 117 for allowing air from the auxiliary equipment housing chamber 116 to flow toward the module housing chamber 115. The exterior plate 113 that constitutes the module housing chamber 115 has an exhaust port 118 for exhausting air from within the module housing chamber 115.
[0067] In such a module accommodating device 110, as described above, by providing the module 100 with improved power generation performance in the module accommodating chamber 115, the module accommodating device 110 can be made to have improved power generation performance.
[0068] 5 is a cross-sectional view showing an example of an electrochemical cell according to a second embodiment. The cell 1 according to this embodiment differs from the cell 1 according to the first embodiment in that the first coating 31 is located away from the adhesive 3. By locating the first coating 31 and the adhesive 3 at a distance, the gap between the first coating 31 and the adhesive 3 is reduced. 2- Since the so-called back diffusion, in which ions such as the above move, is less likely to occur, the power generation performance of the cell 1 is improved.
[0069] The cell 1 according to this embodiment is obtained as follows. For example, the surface of the anode 5 of the laminate described in the first embodiment above is bonded to the first surface 201 of the metal body 2, which has the opening 2b, via an adhesive 3. At this time, the laminate is arranged so that the first coating 31 formed on the metal body 2 is spaced apart from the anode 5 of the laminate. Thereafter, an intermediate layer and a cathode 7 are formed on the solid electrolyte layer 6, and a sealant 8 is further provided on the side surface of the element portion 4, thereby obtaining the cell 1 according to this embodiment.
[0070] A sealing material 8 may be positioned in the gap between the first coating 31 and the adhesive material 3. This can suppress the release of chromium from the first surface 201 of the metal body 2 exposed to an oxidizing atmosphere, for example, thereby improving the durability of the metal body 2. Such sealing material 8 is an example of a second coating material positioned between the metal body 2 and the element portion 4.
[0071] A second coating 32 may be disposed between the metal body 2 and the sealing material 8. The second coating 32 may be, for example, Cr 2 O 3 The second coating 32 is neither the first coating material nor the second coating material.
[0072] [Third Embodiment] Figure 6 is a cross-sectional view showing an example of an electrochemical cell according to a third embodiment. The cell 1 according to this embodiment differs from the cell 1 shown in Figure 5 in that it has a plug 28 instead of the plug 8. The plug 28 has gas barrier properties. The plug 28 may have a porosity of, for example, 5% or less. When the plug 28 has a porosity of 5% or less, fuel gas is less likely to flow between the anode 5 and the outside. The porosity of the plug 28 may be, for example, the average value of the porosities of at least three arbitrary cross sections of the plug 28.
[0073] The cell 1 according to this embodiment is obtained as follows. For example, the surface of the anode 5 of the laminate described in the first embodiment is bonded to the first surface 201 of the metal body 2, which has the opening 2b, via the adhesive 3. At this time, the laminate is arranged so that the first coating 31 formed on the metal body 2 and the anode 5 of the laminate are spaced apart. An intermediate layer is then formed on the solid electrolyte layer 6, and a sealant 28 is further provided on the side surface of the laminate. After the sealant 28 is provided, the air electrode 7 is formed on the intermediate layer, thereby obtaining the cell 1 according to this embodiment. The intermediate layer may be formed by a gas-phase method such as vacuum deposition.
[0074] The sealing material 28 may contain an insulating oxide, such as forsterite, that has higher heat resistance than the sealing material 8. As a result, the sealing material 28 suppresses the release of chromium from the first surface 201 of the metal body 2, not only during operation of the cell 1 but also during the manufacture of the cell 1, thereby further improving the power generation performance of the cell 1. Compared to the sealing material 8, the sealing material 28 is less likely to dissolve or evaporate components in high-temperature steam, and is therefore less likely to cause gas leaks or deterioration of electrode performance. In particular, forsterite has a thermal expansion coefficient close to that of the metal / alloy and / or element portion 4 that are the materials for the metal body 2, and can improve the thermal shock resistance of the cell 1. Furthermore, forsterite has a higher O content than glass, etc., used for the sealing material 8, even in high-temperature steam. 2- Forsterite has a low ionic conductivity of 1×10 at room temperature (25° C.), for example. 12 It has an electrical resistivity of Ω·m or more.
[0075] [Fourth Embodiment] Figure 7 is a cross-sectional view showing an example of an electrochemical cell according to a fourth embodiment. The cell 1 according to this embodiment differs from the cell 1 shown in Figure 1A in that the sealing material 8 is positioned around the third surface 203 and the fourth surface 204 of the metal body 2, from the first surface 211 to the second surface 212 where the oxide coating 9 is located. The metal body 2 is covered with the oxide coating 9 and the sealing material 8, which are exposed to an oxidizing atmosphere, and the metal body 2 itself is not exposed to the oxidizing atmosphere. This makes it difficult for chromium (Cr) contained in the metal body 2 to be released into the oxidizing atmosphere during high-temperature operation. Therefore, according to this embodiment, the power generation performance of the cell 1 can be improved. The oxide coating 9 according to this embodiment is, for example, the first coating 31. The cell 1 may also have, for example, a second coating 32 between the oxide coating 9 and the metal body 2.
[0076] Fifth and Sixth Embodiments Fig. 8 is a cross-sectional view showing an example of an electrochemical cell according to a fifth embodiment. Fig. 9 is a cross-sectional view showing an example of an electrochemical cell according to a sixth embodiment.
[0077] As shown in FIG. 8 , the cell 1 may have a substantially cylindrical metal body 2. Alternatively, as shown in FIG. 9 , the cell 1 may have a flat metal body 2. The flat metal body 2 is located between a first surface 211 and a second surface 212 facing each other in the thickness direction T, and has a gas flow path 2a extending in the longitudinal direction L (see FIG. 1B ). Regardless of the shape of the metal body 2, the power generation performance of the cell 1 can be improved by covering the portion exposed to an oxidizing atmosphere with the oxide coating 9 and the sealing material 8. The oxide coating 9 according to this embodiment is, for example, a first coating 31. Alternatively, the cell 1 may have, for example, a second coating 32 between the oxide coating 9 and the metal body 2.
[0078] Other Embodiments Although the cell 1 shown in FIGS. 7 to 9 is illustrated as having the sealing material 8, a sealing material 28 may be used instead of the sealing material 8.
[0079] Furthermore, in the above-described embodiments, a fuel cell, a fuel cell stack device, a fuel cell module, and a fuel cell device are shown as examples of an "electrochemical cell," "electrochemical cell device," "module," and "module housing device." However, other examples may be an electrolysis cell, an electrolysis cell stack device, an electrolysis module, and an electrolysis device, respectively. The electrolysis cell has a first electrode, a solid electrolyte layer, and a second electrode, and decomposes water vapor into hydrogen and oxygen, or decomposes carbon dioxide into carbon monoxide and oxygen, when supplied with electric power. Furthermore, in the above-described embodiments, an oxide ion conductor or a hydrogen ion conductor is shown as an example of the electrolyte material of the electrochemical cell, but a hydroxide ion conductor may also be used. Such an electrolysis cell, an electrolysis cell stack device, an electrolysis module, and an electrolysis device can improve electrolysis performance.
[0080] The present disclosure has been described in detail above, but the present disclosure is not limited to the above-described embodiments, and various modifications, improvements, etc. are possible within the scope that does not deviate from the gist of the present disclosure.
[0081] As described above, the electrochemical cell (cell 1) according to the embodiment includes the element unit 4, the metal body 2, and an oxide coating material. The metal body 2 contains chromium and supports the element unit 4. The oxide coating material covers the surface of the metal body 2 and is exposed to an oxidizing atmosphere. The oxide coating material suppresses the release of chromium into the oxidizing atmosphere. The oxide coating material has at least the conductive first coating material (first coating 31). This can improve the performance of the cell 1.
[0082] Furthermore, the electrochemical cell device (cell stack device 10) according to the embodiment includes a cell stack 11 that includes electrochemical cells, thereby enabling the performance of the cell stack device 10 to be improved.
[0083] Moreover, the module 100 according to the embodiment includes the electrochemical cell device described above and a container 101 that houses the electrochemical cell device, thereby improving the performance of the module 100.
[0084] Furthermore, the module housing device 110 according to the embodiment includes the above-described module 100, accessories for operating the module 100, and an exterior case for housing the module 100 and the accessories. This can improve the performance of the module housing device 110.
[0085] The disclosed embodiments should be considered in all respects as illustrative and not restrictive. Indeed, the above-described embodiments may be embodied in various forms. Furthermore, the above-described embodiments may be omitted, substituted, or modified in various ways without departing from the scope and spirit of the appended claims.
[0086] REFERENCE SIGNS LIST 1 cell 2 metal body 4 element portion 8 sealing material 9 oxide coating 10 cell stack device 11 cell stack 31 first coating 32 second coating 100 module 110 module housing device
Claims
1. An element portion; a metal body containing chromium and electrically connected to the element portion; an oxide coating material that covers the metal body, is exposed to an oxidizing atmosphere, and suppresses the release of chromium into the oxidizing atmosphere; Equipped with The oxide coating material has at least a conductive first coating material. Electrochemical cell.
2. The oxide coating material further includes an insulating second coating material.
10. The electrochemical cell of claim 1.
3. The second covering material is disposed between the element portion and the first covering material.
3. The electrochemical cell of claim 2.
4. the element portion includes a first electrode, a solid electrolyte layer, and a second electrode; The electrical conductivity of the second coating material is 1 / 10 or less of the electrical conductivity of the solid electrolyte layer.
3. The electrochemical cell of claim 2.
5. The second coating material has a porosity of 10% or less.
3. The electrochemical cell of claim 2.
6. The second coating material includes forsterite.
3. The electrochemical cell of claim 2.
7. The first coating material contains manganese.
10. The electrochemical cell of claim 1.
8. A cell stack comprising an electrochemical cell according to any one of claims 1 to 7. Electrochemical cell setup.
9. The electrochemical cell device according to claim 8 ; A container for housing the electrochemical cell device; A module comprising:
10. A module according to claim 9; Auxiliary equipment for operating the module; an exterior case that houses the module and the auxiliary equipment; A module housing device comprising: