Battery and battery manufacturing method

The battery design addresses the challenges of miniaturization and reliability by using a laminate film exterior body with a folded overlapping structure, creating a bonded adhesive region and non-adhesive region to reduce moisture intrusion and mechanical stress, thereby enhancing the battery's performance.

WO2024202138A1PCT designated stage expired Publication Date: 2024-10-03PANASONIC INTELLECTUAL PROPERTY MANAGEMENT CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2023/035996
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-27
Filing Date
2023-10-03
Publication Date
2024-10-03

AI Technical Summary

Technical Problem

Conventional battery technologies face challenges in miniaturization and reliability when housed in a laminate film exterior body, particularly in preventing moisture intrusion and protecting the power generation element from mechanical forces.

Method used

A battery design featuring a laminate film exterior body with an overlapping portion that is folded back to create a bonded adhesive region and a non-adhesive region, which reduces the battery's projected area, suppresses moisture intrusion, and enhances mechanical reliability by forming voids that buffer external forces.

Benefits of technology

The design achieves both miniaturization and high reliability by reducing moisture intrusion and mechanical stress on the battery, while maintaining effective moisture blocking and protecting the power generation element.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2023035996_03102024_PF_FP_ABST
    Figure JP2023035996_03102024_PF_FP_ABST
Patent Text Reader

Abstract

A battery of the present disclosure comprises: a power generation element; and a case that is configured from a laminate film and that seals the power generation element. The case is positioned so as to surround the power generation element in a plan view with respect to the main surface of the power generation element and has an overlapping section where portions of the laminate film overlap each other. The overlapping section has a folded-back section, which is the area of overlap between the overlapping portions in the plan view and which is obtained by folding back, toward the power generation element side, the end of the overlapping section on the opposite side to the power generation element side. The folded-back section includes: a bonding region in which the overlapping portions overlapping each other in the plan view are bonded to each other via inner surfaces thereof; and a non-bonding region, which is a region between the folding position of the overlapping section and the bonding region in the plan view and in which the overlapping portions overlapping each other in the plan view are not bonded to each other.
Need to check novelty before this filing date? Find Prior Art

Description

Battery and method for manufacturing the battery

[0001] The present disclosure relates to batteries and methods for manufacturing batteries.

[0002] Patent Document 1 discloses folding back the heat-sealed portion of a laminated battery cell.

[0003] Patent Document 2 discloses that the heat-sealed portion of a laminated battery cell is folded back multiple times.

[0004] JP 2000-251855 A Japanese Patent No. 5303974 A

[0005] In the prior art, a practical battery is desired.

[0006] In particular, miniaturization and reliability of batteries housed in laminate film-type exterior bodies are important points in terms of practical characteristics.

[0007] Therefore, the present disclosure provides a battery suitable for practical use when an exterior body made of a laminate film is used, and a method for manufacturing the same.

[0008] A battery according to one embodiment of the present disclosure comprises a power generating element and an exterior body made of a laminate film that seals the power generating element, wherein the exterior body is positioned to surround the power generating element in a planar view relative to the main surface of the power generating element and has an overlapping portion where the laminate film is overlapped, and the overlapping portion has a folded portion where the overlapping portions overlap in the planar view, with the end of the overlapping portion opposite the power generating element side folded back toward the power generating element side, and the folded portion includes an adhesive region where the overlapping portions that overlap in the planar view are adhered to each other's inner surfaces, and a non-adhesive region that is a region between the folded position of the overlapping portion in the planar view and the adhesive region, and where the overlapping portions that overlap in the planar view are not adhered to each other.

[0009] A method for manufacturing a battery according to one aspect of the present disclosure includes the steps of: covering a power generating element with a laminate film, and forming an overlapping portion by overlapping the laminate film at a position that surrounds the power generating element in a planar view relative to the main surface of the power generating element, thereby sealing the power generating element with an outer casing made of the laminate film; folding back the end of the overlapping portion opposite the power generating element side toward the power generating element side, thereby forming a folded portion where the overlapping portions overlap in the planar view; and forming in the folded portion an adhesive region where the overlapping portions that overlap in the planar view are adhered to each other's inner surfaces, and a non-adhesive region between the folded position of the overlapping portions in the planar view and the adhesive region, where the overlapping portions that overlap in the planar view are not adhered to each other.

[0010] According to the present disclosure, a battery using an exterior body made of a laminate film that is suitable for practical use can be provided.

[0011] FIG. 1 is a top view of a battery according to embodiment 1. FIG. 2 is a cross-sectional view of the battery according to embodiment 1. FIG. 3 is a flowchart showing an example of a manufacturing method for the battery according to embodiment 1. FIG. 4A is a cross-sectional view of an example of a unit cell according to embodiment 1. FIG. 4B is a cross-sectional view of another example of a unit cell according to embodiment 1. FIG. 4C is a cross-sectional view of yet another example of a unit cell according to embodiment 1. FIG. 5 is a cross-sectional view of a power generating element having a plurality of battery cells according to embodiment 1. FIG. 6A is a top view of an electrode lead and a counter electrode lead according to embodiment 1. FIG. 6B is a side view of an electrode lead and a counter electrode lead according to embodiment 1. FIG. 7 is a top view of a battery in the process of being manufactured according to embodiment 1. FIG. 8 is a top view of a battery according to variation 1 of embodiment 1. FIG. 9 is a top view of a battery in the process of being manufactured according to variation 1 of embodiment 1. FIG. 10 is a top view of a battery according to variation 2 of embodiment 1. FIG. 11 is a cross-sectional view of a battery according to variation 2 of embodiment 1. FIG. 12 is a top view of a battery in the process of being manufactured according to variation 2 of embodiment 1. Fig. 13 is a top view of a battery according to embodiment 2. Fig. 14 is a top view of a battery according to embodiment 3. Fig. 15 is a cross-sectional view of the battery according to embodiment 3.

[0012] (Summary of the Present Disclosure) As an overview of the present disclosure, examples of a battery and a method for manufacturing a battery according to the present disclosure will be described below.

[0013] A battery according to a first aspect of the present disclosure comprises a power generating element and an exterior body made of a laminate film that seals the power generating element, wherein the exterior body is positioned to surround the power generating element in a planar view relative to the main surface of the power generating element and has an overlapping portion where the laminate film is overlapped, and the overlapping portion has a folded portion where the overlapping portions overlap in the planar view, with the end of the overlapping portion opposite the power generating element side folded back toward the power generating element side, and the folded portion includes an adhesive region where the overlapping portions that overlap in the planar view are adhered to each other's inner surfaces, and a non-adhesive region that is a region between the folded position of the overlapping portion in the planar view and the adhesive region, and where the overlapping portions that overlap in the planar view are not adhered to each other.

[0014] This makes it possible to provide a battery that is suitable for practical use, using an exterior body made of a laminate film.

[0015] Specifically, the overlapping portion surrounding the power-generating element effectively prevents moisture from penetrating into the exterior, which can cause deterioration of the power-generating element. The overlapping portion is folded back toward the power-generating element, reducing the projected area of ​​the battery. Furthermore, if there is no non-adhesive region when bonding the folded portion to form the adhesive region, the bonding operation is performed up to the very edge of the folded portion, potentially damaging the metal layer in the laminate film. In this embodiment, the non-adhesive region exists between the folded portion and the adhesive region, preventing damage to the metal layer in the laminate film and reducing the degradation of the moisture-blocking effect of the exterior. Therefore, a battery using an exterior composed of a laminate film can be both compact and highly reliable, providing a battery suitable for practical use.

[0016] Furthermore, for example, a battery according to a second aspect of the present disclosure may be the battery according to the first aspect, in which the power generating element is sealed under reduced pressure in the exterior body.

[0017] This allows the amount of moisture in the exterior body to be reduced, and also allows the thickness of the battery to be reduced.

[0018] Also, for example, a battery according to a third aspect of the present disclosure may be a battery according to the first or second aspect, in which the overlapping laminate films are heat-sealed to each other in the overlapping portion.

[0019] This further prevents moisture from entering the exterior.

[0020] Also, for example, a battery according to a fourth aspect of the present disclosure may be a battery according to any one of the first to third aspects, and in the adhesive region, the overlapping portions may be bonded together by thermal fusion.

[0021] This allows the overlapping portions to be bonded together without increasing the volume and weight of the battery.

[0022] Furthermore, for example, a battery according to a fifth aspect of the present disclosure may be a battery according to any one of the first to fourth aspects, in which a gap is formed between the overlapping portions that overlap in the planar view in the non-adhesive region.

[0023] This allows the bending radius of the overlapping portion at the folded-back portion to be increased, further suppressing damage to the metal layer in the laminate film. In addition, the voids provide cushioning properties to the folded-back portion, mitigating external mechanical forces and protecting the power generating element from external mechanical forces.

[0024] Furthermore, for example, a battery according to a sixth aspect of the present disclosure may be the battery according to the fifth aspect, further comprising a first member that closes a portion of the gap.

[0025] This allows the overlapping portions sandwiching the gap in the non-adhesive region to be held by the first member, thereby increasing the strength of the folded portion.

[0026] Furthermore, for example, a battery according to a seventh aspect of the present disclosure may be a battery according to any one of the first to sixth aspects, and may further include a second member arranged between the overlapping portions that overlap in the planar view in the non-adhesive region.

[0027] This allows the folded portion to be reinforced by the second member, further improving the mechanical reliability of the battery.

[0028] Furthermore, for example, a battery according to an eighth aspect of the present disclosure is the battery according to the seventh aspect, wherein the second member may include at least one of a metal and a ceramic.

[0029] This increases the rigidity of the second member, further improving the mechanical reliability of the battery.

[0030] Furthermore, for example, a battery according to a ninth aspect of the present disclosure may be the battery according to any one of the first to eighth aspects, in which the power generating element is an all-solid-state battery.

[0031] This allows the exterior body to protect the all-solid-state battery, which is prone to material collapse and other problems.

[0032] In addition, a manufacturing method for a battery according to a tenth aspect of the present disclosure includes the steps of: covering a power generating element with a laminate film, and forming an overlapping portion by overlapping the laminate film at a position that surrounds the power generating element in a planar view relative to the main surface of the power generating element, thereby sealing the power generating element with an outer casing made of the laminate film; folding back an end of the overlapping portion opposite the power generating element side toward the power generating element side, thereby forming a folded portion where the overlapping portions overlap in the planar view; and forming in the folded portion an adhesive region where the overlapping portions that overlap in the planar view are adhered to each other's inner surfaces, and a non-adhesive region between the folded position of the overlapping portions in the planar view and the adhesive region, where the overlapping portions that overlap in the planar view are not adhered to each other.

[0033] This makes it possible to manufacture a battery that is both compact and highly reliable.

[0034] Furthermore, for example, a method for manufacturing a battery according to an eleventh aspect of the present disclosure may be the method for manufacturing a battery according to the tenth aspect, and in the step of sealing the power generating element, the power generating element may be sealed with the outer casing by heat-sealing the overlapping laminate films of the overlapping portions.

[0035] This further prevents moisture from entering the exterior.

[0036] Furthermore, for example, a method for manufacturing a battery according to a twelfth aspect of the present disclosure may be a method for manufacturing a battery according to the tenth or eleventh aspect, and in the step of forming the adhesive region and the non-adhesive region, the adhesive region may be formed by thermally fusing the overlapping portions together.

[0037] This allows the overlapping portions to be bonded together without increasing the volume and weight of the battery.

[0038] Furthermore, for example, a method for manufacturing a battery according to a thirteenth aspect of the present disclosure may be a method for manufacturing a battery according to any one of the tenth to twelfth aspects, and in the step of forming the adhesive region and the non-adhesive region, a gap may be formed between the overlapping portions that overlap in the planar view in the non-adhesive region.

[0039] This allows the bending radius of the overlapping portion at the folded-back portion to be increased, further suppressing damage to the metal layer in the laminate film. In addition, the voids provide cushioning properties to the folded-back portion, mitigating external mechanical forces and protecting the power generating element from external mechanical forces.

[0040] Also, for example, a method for manufacturing a battery according to a fourteenth aspect of the present disclosure may be the method for manufacturing a battery according to the thirteenth aspect, further including a step of blocking a portion of the void with a first member.

[0041] This allows the overlapping portions sandwiching the gap in the non-adhesive region to be held by the first member, thereby increasing the strength of the folded portion.

[0042] Furthermore, for example, a method for manufacturing a battery according to a fifteenth aspect of the present disclosure may be a method for manufacturing a battery according to any one of the tenth to fourteenth aspects, and may further include a step of placing a second member between the overlapping portions that overlap in the planar view in the non-adhesive region.

[0043] This allows the folded portion to be reinforced by the second member, further improving the mechanical reliability of the battery.

[0044] Furthermore, for example, a method for manufacturing a battery according to a sixteenth aspect of the present disclosure may be the method for manufacturing a battery according to any one of the tenth to fifteenth aspects, in which the power-generating element is an all-solid-state battery.

[0045] This allows the exterior body to protect the all-solid-state battery, which is prone to material collapse and other problems.

[0046] Hereinafter, embodiments of the present disclosure will be described with reference to the drawings.

[0047] The embodiments described below are all comprehensive or specific examples. The numerical values, shapes, materials, components, component placement and connection configurations, steps, and step order shown in the following embodiments are merely examples and are not intended to limit the present disclosure. Furthermore, among the components in the following embodiments, components not described in independent claims are described as optional components.

[0048] Furthermore, each figure is a schematic diagram and is not necessarily an exact illustration. Therefore, for example, the scales of the figures do not necessarily match. Furthermore, in each figure, substantially the same components are given the same reference numerals, and redundant explanations are omitted or simplified.

[0049] Furthermore, in this specification, terms indicating the relationship between elements, such as parallelism, terms indicating the shape of elements, such as rectangle, and numerical ranges are not expressions that only express a strict meaning, but are expressions that also include a substantially equivalent range, for example, a difference of about a few percent.

[0050] In this specification and drawings, the x-axis, y-axis, and z-axis represent the three axes of a three-dimensional Cartesian coordinate system. When the shape of the power generating element of the battery in plan view is rectangular, the x-axis and y-axis are directions parallel to a first side of the rectangle and a second side perpendicular to the first side, respectively. The z-axis is a direction parallel to the thickness direction and stacking direction of the power generating element.

[0051] In this specification, the "stacking direction" of the power generating element corresponds to the direction normal to the principal surfaces of the current collector and each layer of the battery cell. In addition, in this specification, "plan view" refers to the view from a direction perpendicular to the principal surface of the power generating element, unless otherwise specified.

[0052] Furthermore, in this specification, the terms "upper" and "lower" do not refer to the upward direction (vertically upward) and downward direction (vertically downward) in absolute spatial recognition, but are used as terms defined by a relative positional relationship based on the stacking order in a stacked configuration. Furthermore, the terms "upper" and "lower" are used not only when two components are arranged with a gap between them and another component is present between them, but also when two components are arranged closely together and are in contact with each other. In the following description, the negative side of the z axis is referred to as "lower" or "lower side," and the positive side of the z axis is referred to as "upper" or "upper side."

[0053] Furthermore, in this specification, ordinal numbers such as "first" and "second" do not refer to the number or order of components unless otherwise specified, but are used to avoid confusion between similar components and to distinguish between components.

[0054] First Embodiment A battery according to a first embodiment will be described below.

[0055] [Configuration] First, the configuration of the battery according to the first embodiment will be described.

[0056] FIG. 1 is a top view of a battery 1 according to this embodiment. FIG. 2 is a cross-sectional view of the battery 1 according to this embodiment. Specifically, FIG. 1 is a plan view of the battery 1 when viewed from the positive side in the z-axis direction, that is, a plan view of the upper main surface 15 of the power-generating element 10. In FIG. 1, the planar shapes of the power-generating element 10 and the voids 45, as well as the boundaries of the overlapping portions 30 in the exterior body 20, are indicated by dashed lines. FIG. 2 shows a cross section taken along line II-II in FIG. 1. In the present disclosure, in the plan views of the battery such as FIG. 1, the overlapping portions 30 in the exterior body 20 are marked with a dotted pattern for ease of understanding. Furthermore, the folded portion 40 of the overlapping portions 30 is marked with a dotted pattern that is denser than the other portions.

[0057] As shown in FIGS. 1 and 2 , the battery 1 includes a power generating element 10 , an outer casing 20 , an electrode lead 91 , a counter electrode lead 92 , and a sleeve 93 .

[0058] The power generating element 10 has a structure in which one or more battery cells 100 and one or more current collectors are stacked in the thickness direction.

[0059] The shape of the power generating element 10 in a plan view is, for example, rectangular as shown in FIG. 1 . That is, the shape of the power generating element 10 is a flattened rectangular parallelepiped. Here, "flat" means that the thickness (i.e., the length in the z-axis direction) is shorter than each side of the main surface (i.e., the lengths in the x-axis direction and the y-axis direction) or the maximum width. The shape of the power generating element 10 in a plan view may be another polygon, such as a square, hexagon, or octagon, or may be a circle or an ellipse. Note that in cross-sectional views such as FIG. 2 , the thickness of each layer is exaggerated to make the layer structure of the power generating element 10 easier to understand.

[0060] 1 and 2 , the power-generating element 10 includes four side surfaces 11, 12, 13, and 14 and two main surfaces 15 and 16. The main surfaces 15 and 16 have the largest areas of the surfaces of the power-generating element 10. In this embodiment, the side surfaces 11, 12, 13, and 14 and the main surfaces 15 and 16 are all flat surfaces.

[0061] The side surfaces 11 and 13 are back-to-back and parallel to each other. The side surfaces 12 and 14 are back-to-back and parallel to each other. The front directions of the side surfaces 11 and 13 and the front directions of the side surfaces 12 and 14 intersect, specifically, are perpendicular to each other. The side surfaces 11, 12, 13, and 14 stand perpendicular to the main surfaces 15 and 16 from each side of the main surfaces 15 and 16. The side surfaces 11, 12, 13, and 14 are parallel to the stacking direction. The side surfaces 11 and 12, 12 and 13, 13 and 14, and 11 and 14 are adjacent to each other and intersect, specifically, are perpendicular to each other.

[0062] The main surfaces 15 and 16 are back-to-back and parallel to each other. The main surface 15 is the top surface of the power-generating element 10. The main surface 16 is the bottom surface of the power-generating element 10.

[0063] As shown in FIG. 2 , the power generating element 10 has a plurality of current collectors and battery cells 100. The plurality of current collectors include an electrode current collector 140 electrically connected to the electrode layer 110 and a counter electrode current collector 150 electrically connected to the counter electrode layer 120. In the power generating element 10, the electrode current collector 140, the battery cells 100, and the counter electrode current collector 150 are stacked in this order along the thickness direction (z-axis direction) of the power generating element 10. The battery cell 100 is the minimum configuration of the power generating section of a battery, and is also referred to as a unit cell. The battery cell 100 and the current collectors stacked on the battery cell 100 may also be collectively referred to as a unit cell.

[0064] 2, the power generating element 10 has one battery cell 100, but this is not particularly limited and may be two or more. In this case, the multiple battery cells 100 are stacked with current collectors interposed therebetween, and each battery cell 100 is sandwiched between the current collectors. In this case, the multiple battery cells 100 may be connected in series or in parallel.

[0065] The battery cell 100 includes an electrode layer 110, a counter electrode layer 120, and an electrolyte layer 130. The electrode layer 110 and the counter electrode layer 120 each contain an active material and are also referred to as an electrode active material layer and a counter electrode active material layer. In the battery cell 100, the electrode layer 110, the electrolyte layer 130, and the counter electrode layer 120 are stacked in this order along the z-axis direction.

[0066] The electrode layer 110 is one of the positive electrode layer and the negative electrode layer of the battery cell 100. The counter electrode layer 120 is the other of the positive electrode layer and the negative electrode layer of the battery cell 100. In the following, a case where the electrode layer 110 is the negative electrode layer and the counter electrode layer 120 is the positive electrode layer will be described as an example.

[0067] The electrode layer 110 is disposed on a main surface of the electrode current collector 140. The electrode layer 110 contains, for example, a negative electrode active material as an electrode material. The electrode layer 110 is disposed opposite the counter electrode layer 120.

[0068] The negative electrode active material contained in the electrode layer 110 may be, for example, graphite, metallic lithium, or the like. As the negative electrode active material, various materials capable of extracting and inserting ions such as lithium (Li) or magnesium (Mg) may be used.

[0069] Furthermore, as a material contained in the electrode layer 110, for example, a solid electrolyte such as an inorganic solid electrolyte may be further used. As the inorganic solid electrolyte, for example, a sulfide solid electrolyte or an oxide solid electrolyte may be used. As the sulfide solid electrolyte, for example, lithium sulfide (Li 2 S) and diphosphorus pentasulfide (P 2 S 5 The electrode layer 110 may further contain a conductive agent such as acetylene black or a binder such as polyvinylidene fluoride.

[0070] The electrode layer 110 is produced by applying a paste-like paint, in which the materials contained in the electrode layer 110 are kneaded together with a solvent, to the main surface of the electrode current collector 140, for example, and drying the paint. In order to increase the density of the electrode layer 110, the electrode current collector 140 (also referred to as an electrode plate) on which the electrode layer 110 is applied may be pressed after drying. The thickness of the electrode layer 110 is, for example, 5 μm or more and 300 μm or less, but is not limited to this.

[0071] The counter electrode layer 120 is disposed on a main surface of the counter electrode current collector 150. The counter electrode layer 120 is a layer containing a positive electrode material such as an active material. The positive electrode material is a material that constitutes a counter electrode for the negative electrode material. The counter electrode layer 120 contains, for example, a positive electrode active material.

[0072] Examples of the positive electrode active material that can be used in the counter electrode layer 120 include lithium cobalt oxide composite oxide (LCO), lithium nickel oxide composite oxide (LNO), lithium manganese oxide composite oxide (LMO), lithium-manganese-nickel composite oxide (LMNO), lithium-manganese-cobalt composite oxide (LMCO), lithium-nickel-cobalt composite oxide (LNCO), and lithium-nickel-manganese-cobalt composite oxide (LNMCO). Various materials that can extract and insert ions such as Li or Mg can be used as the positive electrode active material.

[0073] Furthermore, as a material contained in the counter electrode layer 120, for example, a solid electrolyte such as an inorganic solid electrolyte may be further used. As the inorganic solid electrolyte, a sulfide solid electrolyte or an oxide solid electrolyte may be used. As the sulfide solid electrolyte, for example, Li 2 S and P 2 S 5 A mixture of these materials may be used. The surface of the positive electrode active material may be coated with a solid electrolyte. The counter electrode layer 120 may further contain a conductive agent such as acetylene black or a binder such as polyvinylidene fluoride.

[0074] The counter electrode layer 120 is produced by applying a paste-like paint, in which the materials contained in the counter electrode layer 120 are kneaded together with a solvent, to the main surface of the counter electrode current collector 150, for example, and drying the paint. In order to increase the density of the counter electrode layer 120, the counter electrode current collector 150 (also referred to as a counter electrode plate) to which the counter electrode layer 120 is applied may be pressed after drying. The thickness of the counter electrode layer 120 is, for example, 5 μm or more and 300 μm or less, but is not limited to this.

[0075] The electrolyte layer 130 is disposed between the electrode layer 110 and the counter electrode layer 120. The electrolyte layer 130 is in contact with both the electrode layer 110 and the counter electrode layer 120. The electrolyte layer 130 has, for example, lithium ion conductivity. The electrolyte layer 130 is a layer containing an electrolyte material. A commonly known electrolyte for batteries can be used as the electrolyte material. The thickness of the electrolyte layer 130 may be 5 μm or more and 300 μm or less, or 5 μm or more and 100 μm or less.

[0076] The electrolyte layer 130 includes, for example, a solid electrolyte. In this case, the power generating element 10 is, for example, an all-solid-state battery. As the solid electrolyte, for example, a solid electrolyte such as an inorganic solid electrolyte can be used. As the inorganic solid electrolyte, a sulfide solid electrolyte or an oxide solid electrolyte can be used. As the sulfide solid electrolyte, for example, Li 2 S and P 2 S 5 The electrolyte layer 130 may contain, in addition to the electrolyte material, a binder such as polyvinylidene fluoride.

[0077] In this embodiment, the electrode layer 110, the counter electrode layer 120, and the electrolyte layer 130 are maintained in a parallel plate shape. This makes it possible to prevent cracking or collapse due to bending. Alternatively, the electrode layer 110, the counter electrode layer 120, and the electrolyte layer 130 may be smoothly curved together.

[0078] The electrode current collector 140 and the counter electrode current collector 150 are each conductive foil-like, plate-like, or mesh-like members. The electrode current collector 140 and the counter electrode current collector 150 may each be, for example, a conductive thin film. In the example shown in FIG. 1 , the electrode current collector 140 and the counter electrode current collector 150 are each made of a single metal foil. Note that the electrode current collector 140 and the counter electrode current collector 150 may each have a multilayer structure of multiple current collecting layers made of multiple metal foils or the like.

[0079] The electrode current collector 140 and the counter electrode current collector 150 may be made of a metal such as stainless steel (SUS), aluminum (Al), copper (Cu), or nickel (Ni). The electrode current collector 140 and the counter electrode current collector 150 may be made of different materials.

[0080] The thickness of each of the electrode current collector 140 and the counter electrode current collector 150 is, for example, not less than 5 μm and not more than 200 μm, but is not limited to this.

[0081] The electrode layer 110 is in contact with the main surface of the electrode current collector 140. Of the multiple electrode current collectors 140, the electrode current collector 140 sandwiched between two battery cells 100 has the electrode layer 110 in contact with each of the two main surfaces. The electrode current collector 140 at the bottom has the electrode layer 110 in contact with only one of the two main surfaces (specifically, the upper surface). The electrode current collector 140 may include a connection layer that is a layer containing a conductive material and is provided in a portion that contacts the electrode layer 110.

[0082] The counter electrode layer 120 is in contact with a main surface of the counter electrode current collector 150. Of the multiple counter electrode current collectors 150, the counter electrode current collector 150 sandwiched between two battery cells 100 has the counter electrode layer 120 in contact with each of the two main surfaces. The counter electrode layer 120 is in contact with only one of the two main surfaces (specifically, the lower surface) of the uppermost counter electrode current collector 150. The counter electrode current collector 150 may include a connection layer that is a layer containing a conductive material and is provided in a portion that contacts the counter electrode layer 120.

[0083] The exterior body 20 seals the power generating element 10 contained therein. The power generating element 10 is, for example, vacuum sealed in the exterior body 20. Vacuum sealing can reduce the amount of moisture in the exterior body 20 and can also reduce the thickness of the battery 1.

[0084] The exterior body 20 is made of a laminate film. In the example shown in Fig. 2, the exterior body 20 is made of two laminate films 21a and 21b that are arranged to sandwich the power generating element 10 from above and below.

[0085] 1 , the rectangular shapes of the power generating element 10 and the exterior body 20 each have two sides parallel to the x-axis direction and facing each other, and two sides parallel to the y-axis direction and facing each other, in plan view.

[0086] As shown in FIGS. 1 and 2 , the exterior housing 20 has an overlapping portion 30 where the laminate films 21a and 21b are overlapped. In a plan view, the overlapping portion 30 is positioned so as to surround the power-generating element 10. In a plan view, the overlapping portion 30 extends outside the power-generating element 10. In a plan view, the power-generating element 10 is surrounded by the overlapping portion 30. A gap may be formed between the power-generating element 10 and the overlapping portion 30. In the overlapping portion 30, for example, the overlapping laminate films 21a and 21b are heat-sealed to each other to seal the overlapping portion 30. In FIG. 2 , the boundary between the overlapping laminate films 21a and 21b is shown by a solid line, but in reality, the boundary may not be visible due to heat fusion. This also applies to the other cross-sectional views described below. The exterior body 20 is not limited to the two laminate films 21a and 21b, but may be a single laminate film folded, or may be a single bag-shaped laminate film. In this case, the overlapping portion 30 near the folded edge and the edge other than the opening of the bag does not have to be heat-sealed because the power-generating element 10 can be sealed without heat fusion. The overlapping portion 30 does not have to completely surround the power-generating element 10. For example, the exterior body 20 may be made of a single laminate film, and this single laminate film may be folded back to cover the side surface 12 on the negative side of the power-generating element 10 in the y-axis direction.

[0087] Known laminate films can be used for the laminate films 21a and 21b. The laminate films 21a and 21b have a laminated structure consisting of a resin layer made of a thermoplastic resin such as a polyethylene resin or a polypropylene resin and a metal layer made of a metal such as aluminum. In the laminated structure, both ends in the stacking direction are made of resin layers, and a metal layer is disposed between the resin layers at both ends. The laminate films 21a and 21b have a three-layer structure, for example, in which a first resin layer, a metal layer, and a second resin layer are stacked in this order. The types of thermoplastic resin and metal used for the laminate films 21a and 21b are not particularly limited. The laminated structures of the laminate films 21a and 21b are not shown in the figures.

[0088] The thickness of the laminate films 21a and 21b is, for example, 50 μm or more and 300 μm or less, and the thickness of the metal layer in the laminate films 21a and 21b is, for example, 5 μm or more and 50 μm or less.

[0089] In a plan view, the overlapping portions 30 are located on the positive x-axis side, negative x-axis side, positive y-axis side, and negative y-axis side of the power-generating element 10. In a plan view, the overlapping portions 30 are provided along all side surfaces 11, 12, 13, and 14 of the power-generating element 10. Furthermore, the portion of the overlapping portions 30 inside a folded portion 40 described below is parallel to, for example, the main surfaces 15 and 16 of the power-generating element 10. In other words, the portion of the overlapping portions 30 adjacent to the power-generating element 10 is a planar region parallel to the main surfaces 15 and 16 of the power-generating element 10.

[0090] 2 , the portion of the overlapping portion 30 adjacent to the power generating element 10 is shifted in the negative z-axis direction from the center of the power generating element 10 in the thickness direction of the power generating element 10. Note that the portion of the overlapping portion 30 adjacent to the power generating element 10 may be shifted in the positive z-axis direction from the center of the power generating element 10 in the thickness direction of the power generating element 10, or may be located at the center of the power generating element 10.

[0091] The overlapping portions 30 have a folded-back portion 40 where the overlapping portions 30 overlap in a planar view, with the end of the overlapping portion 30 opposite the power-generating element 10 side folded back toward the power-generating element 10 side. In the folded-back portion 40, the portion of the overlapping portion 30 distal to the folded-back position R overlaps the portion of the overlapping portion 30 between the folded-back position R and the power-generating element 10 in a planar view. In the example shown in FIGS. 1 and 2 , the overlapping portion 30 is folded back only once in the folded-back portion 40, resulting in a double overlapping portion 30. Furthermore, in the folded-back portion 40, the overlapping portion 30 is folded back toward the power-generating element 10 side via the positive z-axis direction. Furthermore, the overlapping portion 30 is curved at the end of the folded-back portion 40 opposite the power-generating element 10 side, i.e., near the folded-back position R. In this specification, the term "folded" means to bend and turn, and includes curving the overlapping portion 30 as shown in FIG. 2 . The fold position R is the end of the folded portion 40 on the side where the overlapping portion 30 turns, i.e., the portion of the folded portion 40 farthest from the power-generating element 10 in a planar view. The shape of the folded portion 40 is fixed by bonding the overlapping portions 30 together at adhesive regions 41 (described below). The formation of the folded portion 40 allows the projected area (area in a planar view) of the battery 1 to be reduced. The width of the folded portion 40, i.e., the length of the folded portion 40 in the folding direction, is, for example, 1 mm or more and 10 mm or less. This allows for both good adhesion between the overlapping portions 30 at the folded portion 40 and a reduced area of ​​the battery 1.

[0092] In the example shown in FIGS. 1 and 2 , the overlapping portion 30 has two folded portions 40 that sandwich the power-generating element 10. The two folded portions 40 are located on the positive and negative sides of the power-generating element 10 in the x-axis direction. That is, both ends of the overlapping portion 30 in the x-axis direction are folded portions 40. One of the two folded portions 40 faces the side surface 11 without the power-generating element 10 in between, and the other of the two folded portions 40 faces the side surface 13 without the power-generating element 10 in between. Each of the two folded portions 40 extends along the y-axis direction in a plan view, and the folded portion 40 is provided over the entire end of the overlapping portion 30 in the x-axis direction. In a plan view, the two folded portions 40 are spaced apart from the power-generating element 10 and do not overlap with the power-generating element 10.

[0093] In the battery 1, no folded portion 40 is provided on the positive side of the y-axis direction of the power generating element 10 in the overlapping portion 30 where the electrode lead 91 and the counter electrode lead 92 are pulled out from the outer casing 20, and on the opposite side, on the negative side of the y-axis direction.

[0094] The folded portion 40 includes an adhesive region 41 and a non-adhesive region 42. In the example shown in Fig. 1, the adhesive region 41 and the non-adhesive region 42 extend along the y-axis direction in a plan view.

[0095] The adhesive region 41 is a region in the folded portion 40 where the overlapping portions 30 that overlap in a planar view are adhered to each other at their inner surfaces. In the example shown in FIG. 2 , the overlapping portions 30 are folded back at the folded portion 40 so that the laminate film 21a of the laminate films 21a and 21b is on the inside. Therefore, the inner surface of the overlapping portions 30 that overlap in a planar view at the adhesive region 41 is the surface of the laminate film 21a. Furthermore, the inner surface of the overlapping portions 30 that overlap in a planar view is the top surface of the overlapping portions 30 before folding. In the adhesive region 41, for example, the overlapping portions 30 that overlap in a planar view are adhered to each other by heat fusion. Therefore, the laminate films 21a and 21b are heat-fused in a four-layer structure in the adhesive region 41. In the adhesive region 41, the overlapping portions 30 that overlap in a planar view may be adhered to each other using a method other than heat fusion, such as an adhesive.

[0096] 1 and 2 , the overlapping portions 30 in the adhesive region 41 are parallel to the main surfaces 15 and 16 of the power-generating element 10. In addition, the adhesive region 41 is formed over a certain range from the end of the folded portion 40 on the power-generating element 10 side in a plan view. Note that there may be an area in the end of the folded portion 40 on the power-generating element 10 side where the overlapping portions 30 are not adhered to each other.

[0097] The non-adhesive region 42 is a region in the folded portion 40 between the folding position R of the overlapping portion 30 and the adhesive region 41 in a planar view, and is a region where the overlapping portions 30 that overlap in a planar view are not adhered to each other. The folding position R of the overlapping portion 30 in the folded portion 40 is located at the end of the folded portion 40 on the side opposite the power-generating element 10. In the folded portion 40, the overlapping portion 30 is bent and folded back at the non-adhesive region 42. By forming a region where the overlapping portions 30 that overlap in a planar view are not adhered to each other for a predetermined distance from the folding position R, damage to the metal layers in the laminate films 21 a and 21 b can be suppressed, and a reduction in the moisture-blocking effect of the exterior body 20 can be suppressed.

[0098] In the non-adhesive region 42, the overlapping portions 30 that overlap in a plan view are not in contact with each other. A gap 45 is formed between the overlapping portions 30 that overlap in a plan view in the non-adhesive region 42. The overlapping portions 30 that overlap in a plan view in the non-adhesive region 42 face each other across the gap 45 in the thickness direction of the adhesive region 41. Therefore, the thickness of the non-adhesive region 42 is greater than the thickness of the adhesive region 41. These thicknesses are lengths in the z-axis direction in FIG. 2 .

[0099] 1 and 2 , the void 45 is a space surrounded by the inner surface of the overlapping portion 30 in the folded-back portion 40. In the example shown in Fig. 1 and 2 , the void 45 is a through-hole that extends in a plan view along the y-axis direction, which is a direction perpendicular to the direction in which the overlapping portion 30 is folded back, and penetrates the folded-back portion 40, and openings of the void 45 are formed at both ends of the folded-back portion 40 in the y-axis direction.

[0100] The formation of the voids 45 in the non-adhesive regions 42 allows the bending radius of the overlapping portions 30 in the folded-back portions 40 to be increased, further suppressing damage to the metal layers in the laminate films 21 a and 21 b. The voids 45 also provide cushioning properties to the folded-back portions 40, mitigating mechanical external forces and protecting the power-generating element 10 from such external forces. Furthermore, because the folded-back portions 40 have a pipe-like structure, the mechanical strength of the power-generating element 10 against external forces that bend it can be increased.

[0101] In the thickness direction of the adhesive region 41, the distance between the overlapping portions 30 facing each other across the gap 45 is, for example, 0.2 mm or more and 10 mm or less. The bending radius of the inner surface of the overlapping portion 30 at the folded portion 40 may be, for example, at least twice the thickness of one laminate film 21a or 21b, or at least four times the thickness of one laminate film 21a or 21b. Specifically, the bending radius of the inner surface of the overlapping portion 30 at the folded portion 40 may be, for example, at least 0.2 mm and 10 mm, at least 0.5 mm and 10 mm, or at least 2 mm and 10 mm. This further suppresses damage to the metal layers of the laminate films 21a and 21b at the folded portion 40.

[0102] The electrode lead 91 and the counter electrode lead 92 are extraction electrodes connected to the power generating element 10. The electrode lead 91 and the counter electrode lead 92 are each made of a conductor such as a metal. The electrode lead 91 is connected to the electrode current collector 140, for example, at the main surface 16. The counter electrode lead 92 is connected to the counter electrode current collector 150, for example, at the main surface 15. The electrode lead 91 and the counter electrode lead 92 may each be connected to an end surface of the current collector, or may be integral with the current collector. For example, the electrode current collector 140 and the counter electrode current collector 150 may have a portion that functions as a current collector and a portion that functions as a lead.

[0103] A portion of the electrode lead 91 and the counter electrode lead 92 are disposed within the exterior body 20. The electrode lead 91 and the counter electrode lead 92 are drawn out from the end of the exterior body 20 on the positive side in the y-axis direction via the overlapping portion 30 located on the positive side in the y-axis direction of the power-generating element 10. This allows charging and discharging of the power-generating element 10 from outside the exterior body 20.

[0104] The sleeve 93 is disposed between the electrode lead 91 and the exterior body 20 and between the counter electrode lead 92 and the exterior body 20 at positions where the electrode lead 91 and the counter electrode lead 92 are pulled out from the exterior body 20. The sleeve 93 is made of an insulating material that can be heat-sealed to both the electrode lead 91 and the counter electrode lead 92 and the exterior body 20. By disposing the sleeve 93 between the electrode lead 91 and the exterior body 20 and between the counter electrode lead 92 and the exterior body 20, airtightness and insulation between the electrode lead 91 and the counter electrode lead 92 and the exterior body 20 can be ensured.

[0105] [Manufacturing Method] Next, a method for manufacturing the battery 1 according to this embodiment will be described. Note that the manufacturing method described below is an example, and the manufacturing method for the battery 1 according to this embodiment is not limited to the following example.

[0106] FIG. 3 is a flowchart showing an example of a method for manufacturing the battery 1 according to this embodiment.

[0107] As shown in Fig. 3, first, the power generating element 10 is prepared (step S10). For example, a unit cell having a battery cell 100 is prepared. Since the power generating element 10 has one battery cell 100, the unit cell can be used as the power generating element 10 as is. Furthermore, when the power generating element 10 has a plurality of battery cells 100, the power generating element 10 is prepared by stacking the prepared unit cells. Figs. 4A to 4C are each a cross-sectional view of an example of a unit cell.

[0108] 4A , the unit cell 100a has one battery cell 100, an electrode current collector 140, and a counter electrode current collector 150. In the unit cell 100a, the battery cell 100 is disposed between the electrode current collector 140 and the counter electrode current collector 150, and the battery cell 100 is in contact with both the electrode current collector 140 and the counter electrode current collector 150. Specifically, the electrode layer 110 of the battery cell 100 is in contact with the electrode current collector 140, and the counter electrode layer 120 of the battery cell 100 is in contact with the counter electrode current collector 150. The unit cell 100a has the same configuration as the power generating element 10 described above.

[0109] 4B , the unit cell 100b has one battery cell 100 and one electrode current collector 140. In the unit cell 100b, the electrode current collector 140 is disposed on the electrode layer 110 side of the battery cell 100, facing the battery cell 100, and is in contact with the electrode layer 110. In the unit cell 100b, the main surface of the counter electrode layer 120 of the battery cell 100 opposite the electrolyte layer 130 side is exposed.

[0110] 4C , the unit cell 100c has one battery cell 100 and one counter electrode current collector 150. In the unit cell 100c, the counter electrode current collector 150 is disposed on the counter electrode layer 120 side of the battery cell 100, facing the battery cell 100, and is in contact with the counter electrode layer 120. In the unit cell 100c, the main surface of the electrode layer 110 of the battery cell 100 opposite to the electrolyte layer 130 side is exposed.

[0111] When stacking unit cells, at least one type of unit cell from the above-described unit cells 100a, 100b, and 100c is prepared according to the stack configuration of the power generating element to be included in the battery 1 to be manufactured. Fig. 5 is a cross-sectional view of a power generating element 10a having a plurality of battery cells 100 according to this embodiment. The battery 1 may include the power generating element 10a instead of the power generating element 10. Note that the batteries according to each of the modified examples and embodiments described below may also include the power generating element 10a.

[0112] The power generating element 10a is a stacked battery in which a plurality of battery cells 100 are connected in series by being stacked via bipolar current collectors 160. The power generating element 10a is, for example, an all-solid-state battery. When preparing the power generating element 10a, for example, one unit cell 100a and two unit cells 100b or 100c are prepared and stacked. The electrode current collector 140 or counter electrode current collector 150 sandwiched between the battery cells 100 functions as the bipolar current collector 160. It is also possible to stack only the unit cells 100a. In this case, two current collectors are placed between the battery cells 100. The unit cells may also be stacked so that the battery cells 100 can be connected in parallel.

[0113] Next, the electrode lead 91 and the counter electrode lead 92 are formed on the main surfaces of the power-generating element 10 (step S20). First, the electrode lead 91 and the counter electrode lead 92 are prepared. FIG. 6A is a top view of the electrode lead 91 and the counter electrode lead 92. FIG. 6B is a side view of the electrode lead 91 and the counter electrode lead 92. As shown in FIGS. 6A and 6B, the electrode lead 91 and the counter electrode lead 92 are inserted into a sleeve 93. The electrode lead 91 inserted into the sleeve 93 is connected to the electrode current collector 140 on the main surface 16, and the counter electrode lead 92 inserted into the sleeve 93 is connected to the counter electrode current collector 150 on the main surface 15.

[0114] Next, the power generating element 10 is sealed with the exterior body 20 (step S30). Fig. 7 is a top view of the battery 2 according to this embodiment during manufacture.

[0115] As shown in FIG. 7 , for example, a power generating element 10 having an electrode lead 91 and a counter electrode lead 92 formed thereon is sandwiched between two laminate films 21a and 21b constituting an exterior body 20, covering both sides of the power generating element 10 in the thickness direction, and the laminate films 21a and 21b are overlapped at a position surrounding the power generating element 10 in a planar view to form an overlapping portion 30. At this time, the tip sides of the electrode lead 91 and the counter electrode lead 92 are exposed. The laminate films 21a and 21b of the overlapping portion 30 are then heat-sealed to each other to seal the power generating element 10 with the exterior body 20. As shown in FIG. 7 , the overlapping portion 30 is formed in all directions outside the power generating element 10 in a planar view, such as the positive side, negative side, positive side, and negative side of the x-axis direction of the power generating element 10. As a result, the power generating element 10 is completely surrounded by the overlapping portion 30 in a planar view. For example, the overlapping portions 30 on the x-axis positive side, x-axis negative side, y-axis positive side, and y-axis negative side of the power-generating element 10 are heat-sealed in sequence using a sealer, etc. Note that, as described above, the overlapping portions 30 near the folded edges when the exterior body 20 is formed by folding a single laminate film, and near the edges other than the opening of the bag when the exterior body 20 is formed from a single bag-shaped laminate film, do not need to be heat-sealed.

[0116] Furthermore, the sealing of the power-generating element 10 with the exterior body 20 is performed in a reduced pressure atmosphere, such as in a vacuum chamber, thereby reducing the pressure and sealing the power-generating element 10 to the exterior body 20. When reducing the pressure and sealing the power-generating element 10, it is not necessary to perform all sealing operations in a reduced pressure atmosphere; it is sufficient that the operation is performed in a reduced pressure atmosphere at least until the heat fusion of all overlapping portions 30 is completed, that is, until the path between the power-generating element 10 in the exterior body 20 and the outside world is completely blocked.

[0117] Furthermore, in forming the battery 2, a cup-shaped laminate film with a recess formed in advance in the area that overlaps the power-generating element 10 in a planar view may be used as the laminate film 21a. This reduces stress on the corners of the power-generating element 10, where the laminate film 21a will bend significantly during sealing, suppresses damage to the power-generating element 10 or the laminate film 21a, and reduces the risk of short circuits. Using a cup-shaped laminate film with a recess formed in the exterior body 20 is particularly effective when the power-generating element 10 is thick, and may be applied to a stacked battery such as the power-generating element 10a, for example.

[0118] The sealing of the power-generating element 10 by the exterior body 20 prevents moisture (water vapor) and other substances that can cause deterioration of the power-generating element 10 from penetrating into the interior of the exterior body 20. The laminate films 21a and 21b contain a metal layer, such as an aluminum layer, and therefore have a high moisture-blocking effect in the thickness direction. On the other hand, moisture can penetrate into the exterior body 20 in a direction perpendicular to the thickness direction of the laminate films 21a and 21b without passing through the metal layer. For example, moisture is likely to penetrate into the exterior body 20 from the end faces of the laminate films 21a and 21b in a direction perpendicular to the thickness direction. In the battery 2, the overlapping portion 30 is formed to surround the power-generating element 10 and is heat-sealed for a certain length, thereby preventing moisture from penetrating from the end of the exterior body 20. However, in the battery 2 state, the projected area (i.e., the area in a plan view) of the exterior body 20 is large, which is disadvantageous for miniaturization.

[0119] Next, the ends of the overlapping portions 30 opposite the power-generating element 10 are folded back toward the power-generating element 10 to form the folded back portions 40, which are the portions where the overlapping portions 30 overlap in a planar view (step S40). Then, the overlapping portions 30 in the folded back portions 40 that overlap in a planar view are partially bonded together to form bonded regions 41 and non-bonded regions 42 in the folded back portions 40 (step S50).

[0120] For example, the two-dot chain line shown in FIG. 7 is used as the folding position, and the overlapping portions 30 on both sides of the power-generating element 10 in the x-axis direction are bent and curved, thereby folding back a region 50 of the overlapping portion 30 outside the two-dot chain line toward the power-generating element 10. In this case, as shown in FIGS. 1 and 2 , the overlapping portions 30 are folded back once so that the overlapping portions 30 contact each other on their inner surfaces at the folding back portion 40. Furthermore, the overlapping portions 30 are folded back so that the overlapping portions 30 that overlap in plan view near the folding back position R in the folding back portion 40 are spaced apart, so that the overlapping portions 30 are not folded back completely. A region is then secured a predetermined distance from the folding back position R in plan view where the overlapping portions 30 are not bonded, and the overlapping portions 30 that overlap in plan view at the folding back portion 40 are bonded together on their inner surfaces. For example, the overlapping portions 30 are heat-fused together by thermocompression bonding using a heater or the like. 1 and 2 are formed in the folded portion 40, thereby fixing the shape of the folded portion 40. Also, a gap 45 is formed between the overlapping portions 30 that overlap in the non-adhesive region 42 in a plan view. This results in the battery 1 shown in FIGS. 1 and 2.

[0121] By forming the folded portion 40 in this manner, the projected area of ​​the exterior body 20 can be reduced compared to the battery 2 before the folded portion 40 was formed. Specifically, the area is reduced by the area of ​​the region 50. Therefore, by reducing the projected area of ​​the exterior body 20 that does not directly contribute to power generation, the area efficiency of the battery 1 can be improved. Furthermore, if the folded portion 40 is bonded up to the non-bonded region 42 on the folding position R side, the bonding operation may apply large bending stress and heat to the laminate films 21a and 21b near the folding position R, which may damage the metal layers of the laminate films 21a and 21b. In particular, the metal layers of the laminate films 21a and 21b are typically very thin and therefore prone to damage. If the metal layers of the laminate films 21a and 21b are damaged near the folding position R, the moisture-blocking effect of the exterior body 20, which was enhanced by ensuring the width of the overlapping portion 30, will be significantly reduced. In battery 1, forming non-adhesive region 42 in folded portion 40 prevents damage to the metal layers of laminate films 21 a and 21 b and prevents a decrease in the moisture blocking effect of exterior body 20. Therefore, battery 1 using exterior body 20 can be made compact and highly reliable at the same time.

[0122] Furthermore, in the adhesive region 41, the overlapping portions 30 that overlap in a plan view in the folded portion 40 are adhered to each other at their inner surfaces, so that the folded portion 40 can be formed with a minimum number of folds.

[0123] Furthermore, in the battery 1, the formation of the gap 45 in the non-adhesive region 42 allows the bending radius of the overlapping portion 30 at the folded portion 40 to be increased, further suppressing damage to the metal layers in the laminate films 21a and 21b.

[0124] [Modification 1] Next, a description will be given of a battery according to Modification 1 of Embodiment 1. The following description will focus on differences from Embodiment 1, and description of commonalities will be omitted or simplified.

[0125] 8 is a top view of the battery 1a according to this modification. As shown in Fig. 8, the battery 1a according to this modification differs from the battery 1 according to the first embodiment in that the overlapping portion 30 further includes a folded portion 40a.

[0126] The folded portion 40a is a portion where the overlapping portions 30 overlap in a planar view, as the end of the overlapping portion 30 opposite the power-generating element 10 is folded back toward the power-generating element 10 on the negative side in the y-axis direction of the power-generating element 10. In the battery 1a, the end of the overlapping portion 30 on the negative side in the y-axis direction is the folded portion 40a. The folded portion 40a faces the side surface 12 without the power-generating element 10 in between. The folded portion 40a extends along the x-axis direction in a planar view, and a folded portion 40b is provided over the entire end of the overlapping portion 30 on the negative side in the y-axis direction.

[0127] The folded portion 40a has a similar configuration to the folded portion 40, except that it is located on the negative side of the power-generating element 10 in the y-axis direction. Specifically, like the folded portion 40, the folded portion 40a includes an adhesive region 41 and a non-adhesive region 42, and a void 45 is formed between the overlapping portions 30 that overlap in a planar view in the non-adhesive region 42. In the folded portion 40a, the adhesive region 41 and the non-adhesive region 42 extend along the x-axis direction in a planar view. Furthermore, in the folded portion 40a, the void 45 is a through-hole that extends along the x-axis direction and penetrates the folded portion 40a in a planar view, and openings of the void 45 are formed at both ends of the folded portion 40a in the x-axis direction.

[0128] In the battery 1a, the overlapping portion 30 includes the folded portion 40a in addition to the folded portion 40, which further improves the mechanical reliability of the battery 1a. In addition, the area of ​​the exterior body 20 is further reduced, which allows the battery 1a to be further miniaturized.

[0129] The battery 1a is manufactured, for example, via the partially manufactured battery 2a shown in Fig. 9. Fig. 9 is a top view of the partially manufactured battery 2a according to this modification. The battery 2a is manufactured, for example, by forming notches 36 in two corners of the overlapping portion 30 on the negative side in the y-axis direction in the battery 2 shown in Fig. 7 in a plan view. This makes it possible to form the folded portions 40 on both sides in the x-axis direction of the power-generating element 10 and the folded portion 40a on the negative side in the y-axis direction so that they do not overlap each other.

[0130] For example, the two-dot chain line shown in FIG. 9 is used as the folding position, and the overlapping portion 30 on the negative side of the y-axis direction of the power-generating element 10 is bent and curved, thereby folding back the region 50a of the overlapping portion 30 outside the two-dot chain line toward the power-generating element 10. In this case, the overlapping portion 30 is folded back once so that the overlapping portions 30 contact each other on their inner surfaces at the folded back portion 40a. Furthermore, the overlapping portions 30 are folded back so that the overlapping portions 30 that overlap in plan view near the folding position R at the folded back portion 40a are spaced apart, so that the overlapping portions 30 are not folded back completely. A predetermined distance from the folding position R in plan view is then secured between the overlapping portions 30 that overlap in plan view, and the overlapping portions 30 that overlap in plan view at the folded back portion 40a are bonded to each other on their inner surfaces. As a result, the folded back portion 40a is formed with an adhesive region 41 and a non-adhesive region 42 as shown in FIG. 8, and the shape of the folded back portion 40a is fixed. Furthermore, gaps 45 are formed between overlapping portions 30 that overlap in plan view in the non-adhesive regions 42. The folded portions 40 are formed in the same manner as in the battery 1. In this way, the battery 1a shown in FIG. 8 is obtained.

[0131] 8 and 9 , in the power-generating element 10, the ridge between two adjacent side surfaces 11, 12, 13, and 14 may be chamfered. That is, the corners of the power-generating element 10 in plan view may be chamfered. This causes the corners of the power-generating element 10 to recede inward in plan view, ensuring the distance of the overlapping portion 30 between the notch 36 and the power-generating element 10. As a result, it is possible to suppress the intrusion of moisture into the exterior body 20.

[0132] [Modification 2] Next, a description will be given of a battery according to Modification 2 of Embodiment 1. The following description will focus on the differences from Embodiment 1 and Modification 1 of Embodiment 1, and description of commonalities will be omitted or simplified.

[0133] Fig. 10 is a top view of battery 1b according to this modification. Fig. 11 is a cross-sectional view of battery 1b according to this modification. Fig. 11 shows a cross section taken along line XI-XI in Fig. 10. As shown in Figs. 10 and 11, battery 1b according to this modification differs from battery 1a according to Modification 1 of Embodiment 1 in that overlapping portion 30 further includes folded-back portion 40b.

[0134] The folded portion 40b is a portion where the overlapping portions 30 overlap in a planar view, as the end of the overlapping portion 30 opposite the power-generating element 10 side is folded back toward the power-generating element 10 side on the positive side in the y-axis direction of the power-generating element 10. In battery 1b, the end of the overlapping portion 30 on the positive side in the y-axis direction is the folded portion 40b. The folded portion 40b faces the side surface 14 without the power-generating element 10 in between. The folded portion 40b extends along the x-axis direction in a planar view, and is provided over the entire end of the overlapping portion 30 on the positive side in the y-axis direction.

[0135] The folded portion 40b has a similar configuration to the folded portion 40, except that it is located on the positive side of the y-axis direction of the power-generating element 10. Specifically, like the folded portion 40, the folded portion 40b includes an adhesive region 41 and a non-adhesive region 42, and a void 45 is formed between the overlapping portions 30 that overlap in a planar view in the non-adhesive region 42. In the folded portion 40b, the adhesive region 41 and the non-adhesive region 42 extend along the x-axis direction in a planar view. Furthermore, in the folded portion 40b, the void 45 is a through-hole that extends along the x-axis direction and penetrates the folded portion 40b in a planar view, and openings of the void 45 are formed at both ends of the folded portion 40b in the x-axis direction.

[0136] In battery 1b, overlapping portion 30 includes folded portion 40b in addition to folded portions 40 and 40a, which further improves the mechanical reliability of battery 1b. In addition, the area of ​​exterior body 20 is further reduced, which allows battery 1b to be further miniaturized.

[0137] In battery 1b, the electrode lead 91 and the counter electrode lead 92 are pulled out from the exterior body 20 at the folded portion 40b. Furthermore, at the folded portion 40b, the electrode lead 91 and the counter electrode lead 92 are also folded back together with the overlapping portion 30. Therefore, in battery 1b, the pulled-out portions of the electrode lead 91 and the counter electrode lead 92 extend to the negative side in the y-axis direction and overlap with the power-generating element 10 in a planar view. Furthermore, the electrode lead 91 and the counter electrode lead 92 each entirely overlap with the exterior body 20 in a planar view.

[0138] Battery 1b is manufactured, for example, via battery 2b in the process of being manufactured as shown in Fig. 12. Fig. 12 is a top view of battery 2b in the process of being manufactured according to this modified example. Battery 2b is manufactured, for example, by forming notches 36 in two corners of overlapping portion 30 on the positive side in the y-axis direction in plan view of battery 2a shown in Fig. 9. This makes it possible to form folded portions 40 on both sides in the x-axis direction of power-generating element 10 and folded portion 40b on the positive side in the y-axis direction so that they do not overlap each other.

[0139] For example, the two-dot chain line shown in FIG. 12 is used as the folding position, and the overlapping portion 30 on the positive side of the y-axis direction of the power-generating element 10 is bent and curved, thereby folding back the region 50b of the overlapping portion 30 outside the two-dot chain line toward the power-generating element 10. At this time, the overlapping portion 30 is folded back so that the overlapping portions 30 contact each other on their inner surfaces at the folding back portion 40b. Furthermore, the overlapping portions 30 are folded back so that the overlapping portions 30 that overlap in plan view near the folding back position R are spaced apart, so that the overlapping portions 30 are not folded back completely. A predetermined distance from the folding back position R in plan view is then secured between the overlapping portions 30 that overlap in plan view, and the overlapping portions 30 that overlap in plan view in the folding back portion 40b are bonded to each other on their inner surfaces. As a result, the folding back portion 40b is formed with an adhesive region 41 and a non-adhesive region 42 as shown in FIG. 10, and the shape of the folding back portion 40b is fixed. Furthermore, gaps 45 are formed between overlapping portions 30 that overlap in plan view in the non-adhesive regions 42. The folded portion 40 is formed in the same manner as in battery 1, and the folded portion 40a is formed in the same manner as in battery 1a. This results in battery 1b shown in Figures 10 and 11.

[0140] (Embodiment 2) Next, a battery according to embodiment 2 will be described. The following description will focus on the differences from embodiment 1 and the modifications of embodiment 1, and description of commonalities will be omitted or simplified.

[0141] Fig. 13 is a top view of a battery 201 according to the present embodiment. As shown in Fig. 13, the battery 201 according to the present embodiment differs from the battery 1 according to the first embodiment in that it further includes a blocking member 60. The blocking member 60 is an example of a first member.

[0142] The blocking member 60 is a member that blocks a portion of the gap 45. At least a portion of the blocking member 60 enters the gap 45 from an opening at the end of the folded portion 40 in the y-axis direction, and blocks the opening. This allows the overlapping portions 30 that face each other across the gap 45 in the non-bonded region 42 to be held by the blocking member 60, thereby increasing the strength of the folded portion 40.

[0143] 13 , two blocking members 60 are provided at both ends of one gap 45 in the y-axis direction. Therefore, the openings on both sides of the gap 45 in the y-axis direction are blocked, forming an enclosed space. This increases the repulsive force of the folded portion 40 against an external force, further improving the mechanical reliability of the battery 201.

[0144] Examples of materials that can be used to form the blocking member 60 include metals, ceramics, and resins, as well as composite materials that include two or more of these.

[0145] In addition to the method for manufacturing the battery 1, the method for manufacturing the battery 201 further includes a step of blocking a part of the gap 45 with a blocking member 60. For example, the battery 201 is formed by blocking the gap 45 of the battery 1 with the blocking member 60. The blocking member 60 may be adhered to the folded portion 40.

[0146] In the battery 201, the battery 1 further includes the blocking member 60, but the above-described battery 1a or 1b may further include the blocking member 60. In this case, the gap 45 of the folded portion 40a or 40b may also be blocked by the blocking member 60.

[0147] (Embodiment 3) Next, a battery according to embodiment 3 will be described. The following description will focus on the differences from embodiments 1 and 2 and the modifications of embodiment 1, and description of commonalities will be omitted or simplified.

[0148] Fig. 14 is a top view of battery 301 according to the present embodiment, and Fig. 15 is a cross-sectional view of battery 301 according to the present embodiment. Fig. 15 shows a cross section taken along line XV-XV shown in Fig. 14. As shown in Figs. 14 and 15, battery 301 according to the present embodiment differs from battery 1 according to embodiment 1 in that it further includes a reinforcing member 70. Reinforcing member 70 is an example of a second member.

[0149] The reinforcing member 70 is disposed between the overlapping portions 30 that overlap in a plan view in the non-adhesive region 42. The upper and lower surfaces of the reinforcing member 70 are in contact with the overlapping portions 30, and the reinforcing member 70 holds the upper overlapping portion 30 in the non-adhesive region 42.

[0150] The reinforcing member 70 is, for example, a rod-shaped member extending in the same direction as the non-bonded region 42. The reinforcing member 70 may also be a pipe-shaped member with a hollow center formed in the rod. The length of the reinforcing member 70 in the extending direction may be longer than the length of the power-generating element 10 in that direction. By providing the battery 301 with the reinforcing member 70, the reinforcing member 70 reinforces the folded portion 40, thereby further improving the mechanical reliability of the battery 301.

[0151] The reinforcing member 70 has higher rigidity than, for example, the exterior body 20. Examples of materials that form the reinforcing member 70 include metal, ceramic, and resin, as well as composite materials that include two or more of these. The reinforcing member 70 includes, for example, at least one of metal and ceramic.

[0152] In addition to the manufacturing method of the battery 1, the manufacturing method of the battery 301 further includes a step of arranging a reinforcing member 70 between the overlapping portions 30 that overlap in a planar view in the non-adhesive region 42. For example, when forming the folded-back portion 40, the overlapping portions 30 are folded back so as to sandwich the reinforcing member 70 between the overlapping portions 30. Also, for example, after forming the gap 45 as in the battery 1, the reinforcing member 70 is inserted into the gap 45.

[0153] 14 , the battery 301 is configured such that the void 45 in the battery 1 is completely occupied by the reinforcing member 70, but the reinforcing member 70 may be disposed so that a portion of the void 45 remains in the battery 1. Furthermore, at least a portion of the void 45 in at least one of the folded portions 40, 40a, and 40b in the above-described batteries 1a, 1b, or 201 may be occupied by the reinforcing member 70.

[0154] While the batteries and battery manufacturing methods according to one or more aspects have been described above based on the embodiments and modifications, the present disclosure is not limited to these embodiments. As long as they do not deviate from the gist of the present disclosure, various modifications that would occur to a person skilled in the art to the present embodiments and modifications, and configurations constructed by combining components of different embodiments and modifications, are also included within the scope of the present disclosure.

[0155] For example, although the power generating element 10 is an all-solid-state battery in the above embodiment, the power generating element 10 is not limited to this and may be a liquid battery including an electrolyte and a separator.

[0156] Furthermore, for example, in the above embodiment, the void 45 is formed in the non-adhesive region 42, but this is not limited thereto. In the non-adhesive region 42, as long as the overlapping portions 30 that overlap in a planar view are not adhered to each other, the void 45 does not need to be formed, and the overlapping portions 30 that overlap in a planar view may be in contact with each other.

[0157] Furthermore, various modifications, substitutions, additions, omissions, etc. can be made to each of the above-described embodiments within the scope of the claims or their equivalents.

[0158] Batteries according to the present disclosure can be used as batteries for a variety of applications, such as electronic devices, electrical appliances, and electric vehicles.

[0159] REFERENCE SIGNS LIST 1, 1a, 1b, 2, 2a, 2b, 201, 301 Battery 10, 10a Power generating element 11, 12, 13, 14 Side surface 15, 16 Main surface 20 Exterior body 21a, 21b Laminate film 30 Overlapping portion 36 Notch 40, 40a, 40b Folded portion 41 Adhesion area 42 Non-adhesion area 45 Void 50, 50a, 50b Area 60 Closing member 70 Reinforcing member 91 Electrode lead 92 Counter electrode lead 93 Sleeve 100 Battery cell 100a, 100b, 100c Unit cell 110 Electrode layer 120 Counter electrode layer 130 Electrolyte layer 140 Electrode current collector 150 Counter electrode current collector 160 Bipolar current collector

Claims

1. A battery comprising: a power generating element; and an exterior body made of a laminate film and sealing the power generating element, wherein the exterior body has an overlapping portion where the laminate film is overlapped and is positioned so as to surround the power generating element in a planar view relative to the main surface of the power generating element, and the overlapping portion has a folded-back portion where the overlapping portions overlap in the planar view, with an end of the overlapping portion opposite the power generating element being folded back towards the power generating element, and the folded-back portion includes: an adhesive region where the overlapping portions that overlap in the planar view are adhered to each other's inner surfaces, and a non-adhesive region that is a region between the folded-back position of the overlapping portions in the planar view and the adhesive region, where the overlapping portions that overlap in the planar view are not adhered to each other.

2. The battery according to claim 1, wherein the power generating element is sealed in the exterior body under reduced pressure.

3. The battery according to claim 1, wherein the laminate films are heat-sealed together at the overlapping portions.

4. The battery according to claim 1, wherein in the bonding region, the overlapping portions are bonded together by thermal fusion.

5. The battery according to claim 1, wherein a gap is formed between the overlapping portions that overlap in the planar view in the non-bonded region.

6. The battery according to claim 5, further comprising a first member that closes a portion of the gap.

7. The battery according to claim 1, further comprising a second member disposed between the overlapping portions that overlap in the planar view in the non-bonded region.

8. The battery according to claim 7, wherein the second member includes at least one of a metal and a ceramic.

9. The battery according to any one of claims 1 to 8, wherein the power generating element is an all-solid-state battery.

10. A method for manufacturing a battery, comprising the steps of: covering a power generating element with a laminate film, and forming an overlapping portion by overlapping the laminate film at a position that surrounds the power generating element in a planar view relative to a main surface of the power generating element, thereby sealing the power generating element with an exterior body composed of the laminate film; folding back an end of the overlapping portion opposite the power generating element side toward the power generating element side, thereby forming a folded back portion where the overlapping portions overlap in the planar view; and forming in the folded back portion an adhesive region where the overlapping portions that overlap in the planar view are adhered to each other's inner surfaces, and a non-adhesive region that is a region between the folded back position of the overlapping portions in the planar view and the adhesive region, where the overlapping portions that overlap in the planar view are not adhered to each other.

11. The method for manufacturing a battery as described in claim 10, wherein in the step of sealing the power generating element, the overlapped laminate films in the overlapping portions are heat-sealed to seal the power generating element in the exterior body.

12. The method for manufacturing a battery according to claim 10, wherein in the step of forming the adhesive region and the non-adhesive region, the adhesive region is formed by heat fusing the overlapping portions together.

13. The method for manufacturing a battery according to claim 10, wherein in the step of forming the adhesive region and the non-adhesive region, a gap is formed between the overlapping portions of the non-adhesive region that overlap in the planar view.

14. The method for manufacturing a battery according to claim 13, further comprising the step of blocking a portion of the gap with a first member.

15. The method for manufacturing a battery according to claim 10, further comprising the step of disposing a second member between the overlapping portions that overlap in the planar view in the non-bonded region.

16. The method for producing a battery according to any one of claims 10 to 15, wherein the power generating element is an all-solid-state battery.

Citation Information

Patent Citations

  • Battery package

    JP2000200585A

  • Laminated battery, protection member and battery unit for the laminated battery

    JP2005116278A

  • Nonaqueous electrolyte battery, and nonaqueous electrolyte battery module

    JP2010218756A

  • Lithium ion secondary battery

    JP2015185416A

  • Laminate outer package battery

    JP2020140874A