Battery and method for manufacturing battery
The battery design employs a laminate film exterior with intersecting rising portions to enhance mechanical reliability and prevent moisture intrusion, addressing the challenges of miniaturization and structural integrity in conventional battery technologies.
Patent Information
- Application Number
- PCT/JP2023/035997
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-27
- Filing Date
- 2023-10-03
- Publication Date
- 2024-10-03
AI Technical Summary
Conventional battery technologies face challenges in achieving miniaturization and mechanical reliability, particularly when housed in a laminate film exterior body, as they struggle to effectively seal the power generation element and protect it from moisture intrusion while maintaining structural integrity.
A battery design that uses a laminate film exterior body with an overlapping portion surrounding the power generation element, featuring rising portions that intersect and are joined to form a strong structure, which reduces the projected area and enhances mechanical reliability by sealing the element under reduced pressure and heat-sealing the laminate films to prevent moisture intrusion.
The solution enables the creation of a battery that is both miniaturized and highly reliable, with improved protection against external forces and moisture, resulting in a compact, efficient, and durable battery suitable for practical use.
Smart Images

Figure JP2023035997_03102024_PF_FP_ABST
Abstract
Description
Battery and method for manufacturing the battery
[0001] The present disclosure relates to batteries and methods for manufacturing batteries.
[0002] Patent Documents 1 and 2 disclose folding the heat-sealed portion of a laminated battery cell.
[0003] JP 2000-200585 A JP 2002-319375 A
[0004] In the prior art, a practical battery is desired.
[0005] In particular, miniaturization and mechanical reliability of batteries housed in laminate film-type exterior bodies are important points in terms of practical characteristics.
[0006] Therefore, the present disclosure provides a battery suitable for practical use when an exterior body made of a laminate film is used, and a method for manufacturing the same.
[0007] A battery according to one embodiment of the present disclosure comprises a power generating element and an exterior body made of a laminate film that seals the power generating element, wherein the exterior body is positioned to surround the power generating element in a planar view relative to the main surface of the power generating element and has an overlapping portion where the laminate film is superimposed, and the overlapping portion includes a first raised portion where an end of the overlapping portion located on a first direction side of the power generating element in the planar view is raised, and a second raised portion where an end of the overlapping portion on a second direction side of the power generating element that intersects the first direction in the planar view is raised, and the first raised portion and the second raised portion are joined to each other.
[0008] A method for manufacturing a battery according to one aspect of the present disclosure includes the steps of: covering a power generating element with a laminate film; forming an overlapping portion by overlapping the laminate film at a position that surrounds the power generating element in a planar view relative to the main surface of the power generating element, thereby sealing the power generating element with an outer casing made of the laminate film; raising the ends of the overlapping portion to form a first raised portion where the end of the overlapping portion located on a first direction side of the power generating element in the planar view is raised; and forming a second raised portion where the end of the overlapping portion on a second direction side of the power generating element that intersects the first direction in the planar view is raised by raising the ends of the overlapping portion; and joining the first raised portion and the second raised portion.
[0009] According to the present disclosure, a battery using an exterior body made of a laminate film that is suitable for practical use can be provided.
[0010] FIG. 1 is a top view of a battery according to embodiment 1. FIG. 2 is a cross-sectional view of the battery according to embodiment 1. FIG. 3 is a side view of the battery according to embodiment 1. FIG. 4 is a side view showing another example of the height of the raised portion according to embodiment 1. FIG. 5 is a flowchart showing an example of a method for manufacturing a battery according to embodiment 1. FIG. 6A is a cross-sectional view of an example of a unit cell according to embodiment 1. FIG. 6B is a cross-sectional view of another example of a unit cell according to embodiment 1. FIG. 6C is a cross-sectional view of yet another example of a unit cell according to embodiment 1. FIG. 7 is a cross-sectional view of a power generating element having a plurality of battery cells according to embodiment 1. FIG. 8A is a top view of an electrode lead and a counter electrode lead according to embodiment 1. FIG. 8B is a side view of an electrode lead and a counter electrode lead according to embodiment 1. FIG. 9 is a top view of a battery in the middle of manufacture according to embodiment 1. FIG. 10 is a cross-sectional view of a battery in the middle of manufacture according to embodiment 1. FIG. 11 is a top view of a battery in the middle of manufacture after FIG. 10 . FIG. 12 is a top view of a battery in the middle of manufacture according to variation 1 of embodiment 1. FIG. 13 is a top view of a battery according to Modification 1 of Embodiment 1. FIG. 14 is a cross-sectional view of a battery in the process of being manufactured according to Modification 2 of Embodiment 1. FIG. 15 is a cross-sectional view of a battery according to Modification 2 of Embodiment 1. FIG. 16 is a side view of a battery according to Modification 2 of Embodiment 1. FIG. 17 is a side view showing another example of the height of the raised portion according to Modification 2 of Embodiment 1. FIG. 18 is a top view of a battery in the process of being manufactured according to Modification 3 of Embodiment 1. FIG. 19 is a top view of a battery according to Modification 3 of Embodiment 1. FIG. 20 is a top view of a battery in the process of being manufactured according to Modification 4 of Embodiment 1. FIG. 21 is a top view of a battery according to Modification 4 of Embodiment 1. FIG. 22 is a top view of a battery according to Embodiment 2. FIG. 23 is a top view of another battery according to Embodiment 2. FIG. 24 is a top view of a battery according to Modification 1 of Embodiment 2. FIG. 25 is a top view of a battery according to Embodiment 3. FIG. 26 is a top view of another battery according to Embodiment 3. FIG. 27 is a top view of a battery in the process of being manufactured according to Embodiment 3. Fig. 28 is a top view of another partially manufactured battery according to embodiment 3. Fig. 29 is a side view showing an example of a wiring board on which another battery according to embodiment 3 is mounted.
[0011] (Summary of the Present Disclosure) As an overview of the present disclosure, examples of a battery and a method for manufacturing a battery according to the present disclosure will be described below.
[0012] A battery according to a first aspect of the present disclosure comprises a power generating element and an exterior body made of a laminate film and sealing the power generating element, wherein the exterior body is positioned to surround the power generating element in a planar view relative to the main surface of the power generating element and has an overlapping portion where the laminate film is superimposed, and the overlapping portion includes a first raised portion where an end of the overlapping portion located on a first direction side of the power generating element in the planar view is raised, and a second raised portion where an end of the overlapping portion on a second direction side of the power generating element that intersects with the first direction in the planar view is raised, and the first raised portion and the second raised portion are joined to each other.
[0013] This makes it possible to provide a battery that is suitable for practical use, using an exterior body made of a laminate film.
[0014] Specifically, the overlapping portion surrounding the power generating element effectively prevents moisture from penetrating the exterior, which can cause deterioration of the power generating element, while the raised edges of the overlapping portion allow the battery's projected area to be reduced. Furthermore, the first raised portion and the second raised portion are joined, forming a strong structure that makes it easier for the first raised portion and the second raised portion to maintain their raised state even when subjected to external force. For example, the raised structure is maintained until the joint between the first raised portion and the second raised portion is broken, preventing external force from being applied to the power generating element. This improves the mechanical reliability of the battery.
[0015] Furthermore, for example, a battery according to a second aspect of the present disclosure may be the battery according to the first aspect, in which the power generating element is sealed under reduced pressure in the exterior body.
[0016] This allows the amount of moisture in the exterior body to be reduced, and also allows the thickness of the battery to be reduced.
[0017] Also, for example, a battery according to a third aspect of the present disclosure may be a battery according to the first or second aspect, in which the overlapping laminate films are heat-sealed to each other in the overlapping portion.
[0018] This further prevents moisture from entering the exterior.
[0019] Furthermore, for example, a battery according to a fourth aspect of the present disclosure may be a battery according to any one of the first to third aspects, in which the first raised portion and the second raised portion are joined by thermal fusion.
[0020] This allows the first rising portion and the second rising portion to be joined together without increasing the volume and weight of the battery.
[0021] Furthermore, for example, a battery according to a fifth aspect of the present disclosure may be a battery according to any one of the first to fourth aspects, wherein at least one of the first raised portion and the second raised portion rises to a position higher than the height of the battery at the point where the power generating element is present in the planar view.
[0022] This allows an external force acting in the height direction to be received by at least one of the first rising portion and the second rising portion, thereby reducing the application of the external force to the power generating element.
[0023] Furthermore, for example, a battery according to a sixth aspect of the present disclosure may be a battery according to any one of the first to fifth aspects, wherein the first raised portion and the second raised portion have a contact portion joined to each other in face-to-face contact and a non-contact portion not in contact with each other, and the contact portion may be located closer to the power generating element than the non-contact portion.
[0024] This allows the bulky contact portions joined in surface contact to be disposed inside the first rising portion and the second rising portion, thereby reducing the projected area of the exterior body.
[0025] Furthermore, for example, a battery according to a seventh aspect of the present disclosure may be a battery according to any one of the first to fifth aspects, wherein the first raised portion and the second raised portion have a contact portion joined to each other in face-to-face contact and a non-contact portion not in contact with each other, and the contact portion may be located farther from the power generating element than the non-contact portion.
[0026] This allows the contact portion to be disposed outside the first rising portion and the second rising portion, making it possible to easily form the contact portion without being restricted by other components in forming the contact portion.
[0027] Furthermore, for example, a battery according to an eighth aspect of the present disclosure may be a battery according to any one of the first to seventh aspects, wherein the first raised portion and the second raised portion have a contact portion that is joined in face-to-face contact with each other and a non-contact portion that is not in contact with each other, and the contact portion may be joined to the non-contact portion.
[0028] This makes it possible to further strengthen the structure of the first rising portion and the second rising portion.
[0029] Furthermore, for example, a battery according to a ninth aspect of the present disclosure may be a battery according to any one of the first to fifth aspects, and in the planar view, the first raised portion and the second raised portion may be joined to each other at their tips in a direction perpendicular to their thickness direction.
[0030] This allows the battery to be made smaller.
[0031] Furthermore, for example, a battery according to a tenth aspect of the present disclosure may be a battery according to any one of the first to ninth aspects, further comprising an auxiliary material attached to the first rising portion and the second rising portion, and the first rising portion and the second rising portion may be joined via the auxiliary material.
[0032] This allows the power generating element to be protected by the auxiliary material as well.
[0033] Furthermore, for example, a battery according to an eleventh aspect of the present disclosure may be the battery according to the tenth aspect, wherein the auxiliary material is attached to the first rising portion and the second rising portion by a crimping mechanism.
[0034] This allows the reinforcing material to be easily and firmly attached to the first rising portion and the second rising portion.
[0035] Furthermore, for example, a battery according to a twelfth aspect of the present disclosure may be a battery according to any one of the first to eleventh aspects, wherein the overlapping portion is shifted to one side from the center of the power generating element in the thickness direction of the power generating element, and the first raised portion and the second raised portion may rise toward the other side in the thickness direction of the power generating element.
[0036] This allows the height of the first raised portion and the second raised portion to be ensured while preventing the volume occupied in the thickness direction of the battery from increasing, and protects the power generating element from external forces from both sides in the thickness direction of the battery.
[0037] Furthermore, for example, a battery according to a thirteenth aspect of the present disclosure may be the battery according to any one of the first to twelfth aspects, in which the power generating element is an all-solid-state battery.
[0038] This allows the exterior body to protect the all-solid-state battery, which is prone to material collapse and other problems.
[0039] Furthermore, for example, a battery according to a fourteenth aspect of the present disclosure may be a battery according to any one of the first to thirteenth aspects, wherein the first raised portion and the second raised portion are inclined at an angle of 45° or more with respect to the main surface of the power generating element.
[0040] This allows the projected area of the battery to be further reduced.
[0041] Furthermore, for example, a battery according to a fifteenth aspect of the present disclosure may be a battery according to any one of the first to fourteenth aspects, further comprising a lead connected to the power generating element and a portion of which is disposed within the outer casing, the lead being pulled out from the outer casing at the second rising portion, and the entire lead overlapping the outer casing in the planar view.
[0042] This allows the projected area of the entire battery, including the leads, to be reduced.
[0043] In addition, a method for manufacturing a battery according to a sixteenth aspect of the present disclosure includes the steps of: covering a power generating element with a laminate film; forming an overlapping portion by overlapping the laminate film at a position that surrounds the power generating element in a planar view relative to the main surface of the power generating element, thereby sealing the power generating element with an exterior body made of the laminate film; raising the ends of the overlapping portion to form a first raised portion where the end of the overlapping portion located on a first direction side of the power generating element in the planar view is raised; and forming a second raised portion where the end of the overlapping portion on a second direction side of the power generating element that intersects the first direction in the planar view is raised by raising the ends of the overlapping portion; and joining the first raised portion and the second raised portion.
[0044] This makes it possible to manufacture a battery that is both compact and highly reliable.
[0045] Furthermore, for example, a method for manufacturing a battery according to a seventeenth aspect of the present disclosure may be a method for manufacturing a battery according to the sixteenth aspect, in which, in the step of sealing the power generating element, the overlapping laminate films of the overlapping portions may be heat-sealed to each other to seal the power generating element with the outer casing.
[0046] This further prevents moisture from entering the exterior.
[0047] Furthermore, for example, a method for manufacturing a battery according to an eighteenth aspect of the present disclosure may be the method for manufacturing a battery according to the sixteenth or seventeenth aspect, in which the power generating element is an all-solid-state battery.
[0048] This allows the exterior body to protect the all-solid-state battery, which is prone to material collapse and other problems.
[0049] Furthermore, for example, a method for manufacturing a battery according to a 19th aspect of the present disclosure may be a method for manufacturing a battery according to any one of the 16th to 18th aspects, wherein in the step of forming the first raised portion and the second raised portion, before raising the end of the overlapping portion, a notch may be formed in the overlapping portion, and both sides of the notch may be raised to form the first raised portion and the second raised portion.
[0050] This makes it less likely that the first rising portion and the second rising portion will interfere with each other when they are formed, and the end of the overlapping portion can be easily raised.
[0051] Furthermore, for example, a method for manufacturing a battery according to a twentieth aspect of the present disclosure may be a method for manufacturing a battery according to any one of the sixteenth to eighteenth aspects, wherein in the step of forming the first raised portion and the second raised portion, before raising the end of the overlapping portion, a notch may be formed in the overlapping portion, and both sides of the notch may be raised to form the first raised portion and the second raised portion.
[0052] This makes it less likely that the first rising portion and the second rising portion will interfere with each other when they are formed, and the end of the overlapping portion can be easily raised.
[0053] Hereinafter, embodiments of the present disclosure will be described with reference to the drawings.
[0054] The embodiments described below are all comprehensive or specific examples. The numerical values, shapes, materials, components, component placement and connection configurations, steps, and step order shown in the following embodiments are merely examples and are not intended to limit the present disclosure. Furthermore, among the components in the following embodiments, components not described in independent claims are described as optional components.
[0055] Furthermore, each figure is a schematic diagram and is not necessarily an exact illustration. Therefore, for example, the scales of the figures do not necessarily match. Furthermore, in each figure, substantially the same components are given the same reference numerals, and redundant explanations are omitted or simplified.
[0056] Furthermore, in this specification, terms indicating the relationship between elements, such as parallelism, terms indicating the shape of elements, such as rectangle, and numerical ranges are not expressions that only express a strict meaning, but are expressions that also include a substantially equivalent range, for example, a difference of about a few percent.
[0057] In this specification and drawings, the x-axis, y-axis, and z-axis represent the three axes of a three-dimensional Cartesian coordinate system. When the shape of the power generating element of the battery in plan view is rectangular, the x-axis and y-axis are directions parallel to a first side of the rectangle and a second side perpendicular to the first side, respectively. The z-axis is a direction parallel to the thickness direction and stacking direction of the power generating element.
[0058] In this specification, the "stacking direction" of the power generating element corresponds to the direction normal to the principal surfaces of the current collector and each layer of the battery cell. In addition, in this specification, "plan view" refers to the view from a direction perpendicular to the principal surface of the power generating element, unless otherwise specified.
[0059] Furthermore, in this specification, the terms "upper" and "lower" do not refer to the upward direction (vertically upward) and downward direction (vertically downward) in absolute spatial recognition, but are used as terms defined by a relative positional relationship based on the stacking order in a stacked configuration. Furthermore, the terms "upper" and "lower" are used not only when two components are arranged with a gap between them and another component is present between them, but also when two components are arranged closely together and are in contact with each other. In the following description, the negative side of the z axis is referred to as "lower" or "lower side," and the positive side of the z axis is referred to as "upper" or "upper side."
[0060] Furthermore, in this specification, ordinal numbers such as "first" and "second" do not refer to the number or order of components unless otherwise specified, but are used to avoid confusion between similar components and to distinguish between components.
[0061] First Embodiment A battery according to a first embodiment will be described below.
[0062] [Configuration] First, the configuration of the battery according to the first embodiment will be described.
[0063] FIG. 1 is a top view of a battery 1 according to this embodiment. FIG. 2 is a cross-sectional view of the battery 1 according to this embodiment. FIG. 3 is a side view of the battery 1 according to this embodiment. Specifically, FIG. 1 is a plan view of the battery 1 when viewed from the positive side in the z-axis direction, that is, when viewed from the upper main surface 15 of the power-generating element 10. In FIG. 1, the planar shape of the power-generating element 10 and the boundary of the overlapping portion 30 in the exterior body 20 are indicated by dashed lines. FIG. 2 shows a cross section taken along line II-II in FIG. 1. In addition, FIG. 3 is a plan view of the battery 1 when viewed from the negative side in the y-axis direction. In the plan views of the battery in this disclosure, such as FIG. 1 and FIG. 3, the overlapping portion 30 in the exterior body 20 is marked with a dot pattern for ease of understanding. In addition, the rising portion of the overlapping portion 30 is marked with a dot pattern that is denser than other portions. In addition, in the plan views of the battery such as FIG. 1 and FIG. 3, the state in which the two laminate films are superimposed on each other at the end surface of the exterior body 20 is not shown.
[0064] As shown in FIGS. 1 to 3 , the battery 1 includes a power generating element 10 , an outer casing 20 , an electrode lead 91 , a counter electrode lead 92 , and a sleeve 93 .
[0065] The power generating element 10 has a structure in which one or more battery cells 100 and one or more current collectors are stacked in the thickness direction.
[0066] The shape of the power generating element 10 in a plan view is, for example, rectangular as shown in FIG. 1 . That is, the shape of the power generating element 10 is a flattened rectangular parallelepiped. Here, "flat" means that the thickness (i.e., the length in the z-axis direction) is shorter than each side of the main surface (i.e., the lengths in the x-axis direction and the y-axis direction) or the maximum width. The shape of the power generating element 10 in a plan view may be another polygon, such as a square, hexagon, or octagon, or may be a circle or an ellipse. Note that in cross-sectional views such as FIG. 2 , the thickness of each layer is exaggerated to make the layer structure of the power generating element 10 easier to understand.
[0067] 1 and 2 , the power-generating element 10 includes four side surfaces 11, 12, 13, and 14 and two main surfaces 15 and 16. The main surfaces 15 and 16 have the largest areas of the surfaces of the power-generating element 10. In this embodiment, the side surfaces 11, 12, 13, and 14 and the main surfaces 15 and 16 are all flat surfaces.
[0068] The side surfaces 11 and 13 are back-to-back and parallel to each other. The side surfaces 12 and 14 are back-to-back and parallel to each other. The front directions of the side surfaces 11 and 13 and the front directions of the side surfaces 12 and 14 intersect, specifically, are perpendicular to each other. The side surfaces 11, 12, 13, and 14 stand perpendicular to the main surfaces 15 and 16 from each side of the main surfaces 15 and 16. The side surfaces 11, 12, 13, and 14 are parallel to the stacking direction. The side surfaces 11 and 12, 12 and 13, 13 and 14, and 11 and 14 are adjacent to each other and intersect, specifically, are perpendicular to each other.
[0069] The main surfaces 15 and 16 are back-to-back and parallel to each other. The main surface 15 is the top surface of the power-generating element 10. The main surface 16 is the bottom surface of the power-generating element 10.
[0070] As shown in FIG. 2 , the power generating element 10 has a plurality of current collectors and battery cells 100. The plurality of current collectors include an electrode current collector 140 electrically connected to the electrode layer 110 and a counter electrode current collector 150 electrically connected to the counter electrode layer 120. In the power generating element 10, the electrode current collector 140, the battery cells 100, and the counter electrode current collector 150 are stacked in this order along the thickness direction (z-axis direction) of the power generating element 10. The battery cell 100 is the minimum configuration of the power generating section of a battery, and is also referred to as a unit cell. The battery cell 100 and the current collectors stacked on the battery cell 100 may also be collectively referred to as a unit cell.
[0071] 2, the power generating element 10 has one battery cell 100, but this is not particularly limited and may be two or more. In this case, the multiple battery cells 100 are stacked with current collectors interposed therebetween, and each battery cell 100 is sandwiched between the current collectors. In this case, the multiple battery cells 100 may be connected in series or in parallel.
[0072] The battery cell 100 includes an electrode layer 110, a counter electrode layer 120, and an electrolyte layer 130. The electrode layer 110 and the counter electrode layer 120 each contain an active material and are also referred to as an electrode active material layer and a counter electrode active material layer. In the battery cell 100, the electrode layer 110, the electrolyte layer 130, and the counter electrode layer 120 are stacked in this order along the z-axis direction.
[0073] The electrode layer 110 is one of the positive electrode layer and the negative electrode layer of the battery cell 100. The counter electrode layer 120 is the other of the positive electrode layer and the negative electrode layer of the battery cell 100. In the following, a case where the electrode layer 110 is the negative electrode layer and the counter electrode layer 120 is the positive electrode layer will be described as an example.
[0074] The electrode layer 110 is disposed on a main surface of the electrode current collector 140. The electrode layer 110 contains, for example, a negative electrode active material as an electrode material. The electrode layer 110 is disposed opposite the counter electrode layer 120.
[0075] The negative electrode active material contained in the electrode layer 110 may be, for example, graphite, metallic lithium, or the like. As the negative electrode active material, various materials capable of extracting and inserting ions such as lithium (Li) or magnesium (Mg) may be used.
[0076] Furthermore, as a material contained in the electrode layer 110, for example, a solid electrolyte such as an inorganic solid electrolyte may be further used. As the inorganic solid electrolyte, for example, a sulfide solid electrolyte or an oxide solid electrolyte may be used. As the sulfide solid electrolyte, for example, lithium sulfide (Li 2 S) and diphosphorus pentasulfide (P 2 S 5 The electrode layer 110 may further contain a conductive agent such as acetylene black or a binder such as polyvinylidene fluoride.
[0077] The electrode layer 110 is produced by applying a paste-like paint, in which the materials contained in the electrode layer 110 are kneaded together with a solvent, to the main surface of the electrode current collector 140, for example, and drying the paint. In order to increase the density of the electrode layer 110, the electrode current collector 140 (also referred to as an electrode plate) on which the electrode layer 110 is applied may be pressed after drying. The thickness of the electrode layer 110 is, for example, 5 μm or more and 300 μm or less, but is not limited to this.
[0078] The counter electrode layer 120 is disposed on a main surface of the counter electrode current collector 150. The counter electrode layer 120 is a layer containing a positive electrode material such as an active material. The positive electrode material is a material that constitutes a counter electrode for the negative electrode material. The counter electrode layer 120 contains, for example, a positive electrode active material.
[0079] Examples of the positive electrode active material that can be used in the counter electrode layer 120 include lithium cobalt oxide composite oxide (LCO), lithium nickel oxide composite oxide (LNO), lithium manganese oxide composite oxide (LMO), lithium-manganese-nickel composite oxide (LMNO), lithium-manganese-cobalt composite oxide (LMCO), lithium-nickel-cobalt composite oxide (LNCO), and lithium-nickel-manganese-cobalt composite oxide (LNMCO). Various materials that can extract and insert ions such as Li or Mg can be used as the positive electrode active material.
[0080] Furthermore, as a material contained in the counter electrode layer 120, for example, a solid electrolyte such as an inorganic solid electrolyte may be further used. As the inorganic solid electrolyte, a sulfide solid electrolyte or an oxide solid electrolyte may be used. As the sulfide solid electrolyte, for example, Li 2 S and P 2 S 5 A mixture of these materials may be used. The surface of the positive electrode active material may be coated with a solid electrolyte. The counter electrode layer 120 may further contain a conductive agent such as acetylene black or a binder such as polyvinylidene fluoride.
[0081] The counter electrode layer 120 is produced by applying a paste-like paint, in which the materials contained in the counter electrode layer 120 are kneaded together with a solvent, to the main surface of the counter electrode current collector 150, for example, and drying the paint. In order to increase the density of the counter electrode layer 120, the counter electrode current collector 150 (also referred to as a counter electrode plate) to which the counter electrode layer 120 is applied may be pressed after drying. The thickness of the counter electrode layer 120 is, for example, 5 μm or more and 300 μm or less, but is not limited to this.
[0082] The electrolyte layer 130 is disposed between the electrode layer 110 and the counter electrode layer 120. The electrolyte layer 130 is in contact with both the electrode layer 110 and the counter electrode layer 120. The electrolyte layer 130 has, for example, lithium ion conductivity. The electrolyte layer 130 is a layer containing an electrolyte material. A commonly known electrolyte for batteries can be used as the electrolyte material. The thickness of the electrolyte layer 130 may be 5 μm or more and 300 μm or less, or 5 μm or more and 100 μm or less.
[0083] The electrolyte layer 130 includes, for example, a solid electrolyte. In this case, the power generating element 10 is, for example, an all-solid-state battery. As the solid electrolyte, for example, a solid electrolyte such as an inorganic solid electrolyte can be used. As the inorganic solid electrolyte, a sulfide solid electrolyte or an oxide solid electrolyte can be used. As the sulfide solid electrolyte, for example, Li 2 S and P 2 S 5 The electrolyte layer 130 may contain, in addition to the electrolyte material, a binder such as polyvinylidene fluoride.
[0084] In this embodiment, the electrode layer 110, the counter electrode layer 120, and the electrolyte layer 130 are maintained in a parallel plate shape. This makes it possible to prevent cracking or collapse due to bending. Alternatively, the electrode layer 110, the counter electrode layer 120, and the electrolyte layer 130 may be smoothly curved together.
[0085] The electrode current collector 140 and the counter electrode current collector 150 are each conductive foil-like, plate-like, or mesh-like members. The electrode current collector 140 and the counter electrode current collector 150 may each be, for example, a conductive thin film. In the example shown in FIG. 1 , the electrode current collector 140 and the counter electrode current collector 150 are each made of a single metal foil. Note that the electrode current collector 140 and the counter electrode current collector 150 may each have a multilayer structure of multiple current collecting layers made of multiple metal foils or the like.
[0086] The electrode current collector 140 and the counter electrode current collector 150 may be made of a metal such as stainless steel (SUS), aluminum (Al), copper (Cu), or nickel (Ni). The electrode current collector 140 and the counter electrode current collector 150 may be made of different materials.
[0087] The thickness of each of the electrode current collector 140 and the counter electrode current collector 150 is, for example, not less than 5 μm and not more than 200 μm, but is not limited to this.
[0088] The electrode layer 110 is in contact with the main surface of the electrode current collector 140. Of the multiple electrode current collectors 140, the electrode current collector 140 sandwiched between two battery cells 100 has the electrode layer 110 in contact with each of the two main surfaces. The electrode current collector 140 at the bottom has the electrode layer 110 in contact with only one of the two main surfaces (specifically, the upper surface). The electrode current collector 140 may include a connection layer that is a layer containing a conductive material and is provided in a portion that contacts the electrode layer 110.
[0089] The counter electrode layer 120 is in contact with a main surface of the counter electrode current collector 150. Of the multiple counter electrode current collectors 150, the counter electrode current collector 150 sandwiched between two battery cells 100 has the counter electrode layer 120 in contact with each of the two main surfaces. The counter electrode layer 120 is in contact with only one of the two main surfaces (specifically, the lower surface) of the uppermost counter electrode current collector 150. The counter electrode current collector 150 may include a connection layer that is a layer containing a conductive material and is provided in a portion that contacts the counter electrode layer 120.
[0090] The exterior body 20 seals the power generating element 10 contained therein. The power generating element 10 is, for example, vacuum sealed in the exterior body 20. Vacuum sealing can reduce the amount of moisture in the exterior body 20 and can also reduce the thickness of the battery 1.
[0091] The exterior body 20 is made of a laminate film. In the example shown in Fig. 2, the exterior body 20 is made of two laminate films 21a and 21b that are arranged to sandwich the power generating element 10 from above and below.
[0092] 1 , the rectangular shapes of the power generating element 10 and the exterior body 20 each have two sides parallel to the x-axis direction and facing each other, and two sides parallel to the y-axis direction and facing each other, in plan view.
[0093] As shown in FIGS. 1 and 2 , the exterior housing 20 has an overlapping portion 30 where the laminate films 21a and 21b are overlapped. In a plan view, the overlapping portion 30 is positioned so as to surround the power-generating element 10. In a plan view, the overlapping portion 30 extends outside the power-generating element 10. In a plan view, the power-generating element 10 is surrounded by the overlapping portion 30. A gap may be formed between the power-generating element 10 and the overlapping portion 30. In the overlapping portion 30, for example, the overlapping laminate films 21a and 21b are heat-sealed to each other to seal the overlapping portion 30. In FIG. 2 , the boundary between the overlapping laminate films 21a and 21b is shown by a solid line, but in reality, the boundary may not be visible due to heat fusion. This also applies to the other cross-sectional views described below. The laminate film constituting the exterior body 20 is not limited to the two laminate films 21a and 21b, but may be a single laminate film folded, or may be a single bag-shaped laminate film. In this case, the overlapping portion 30 near the folded side and the side other than the opening of the bag does not need to be heat-sealed because the power generating element 10 can be sealed without heat-sealing.
[0094] Known laminate films can be used for the laminate films 21a and 21b. The laminate films 21a and 21b have a laminated structure consisting of a resin layer made of a thermoplastic resin such as a polyethylene resin or a polypropylene resin and a metal layer made of a metal such as aluminum. In the laminated structure, both ends in the stacking direction are made of resin layers, and a metal layer is disposed between the resin layers at both ends. The laminate films 21a and 21b have a three-layer structure, for example, in which a first resin layer, a metal layer, and a second resin layer are stacked in this order. The types of thermoplastic resin and metal used for the laminate films 21a and 21b are not particularly limited. The laminated structures of the laminate films 21a and 21b are not shown in the figures.
[0095] In a plan view, the overlapping portions 30 are located on the positive x-axis side, negative x-axis side, positive y-axis side, and negative y-axis side of the power-generating element 10. In a plan view, the overlapping portions 30 are provided along all side surfaces 11, 12, 13, and 14 of the power-generating element 10. Furthermore, the overlapping portions 30 are parallel to the main surfaces 15 and 16 of the power-generating element 10, except for, for example, the rising portions 31, 32, and 33 described below. In other words, the portions of the overlapping portions 30 adjacent to the power-generating element 10 are planar regions parallel to the main surfaces 15 and 16 of the power-generating element 10.
[0096] 2 , the portion of the overlapping portion 30 adjacent to the power generating element 10 is positioned at the center of the power generating element 10 in the thickness direction of the power generating element 10. This reduces the amount of bending required for each of the laminate films 21a and 21b to conform to the shape of the power generating element 10 and the stress on the corners of the power generating element 10 due to sealing with the laminate films 21a and 21b, thereby suppressing damage to the power generating element 10 or the laminate films 21a and 21b and reducing the risk of short circuits.
[0097] The overlapping portion 30 includes rising portions 31, 32, and 33, which are portions where the ends of the overlapping portion 30 rise. In the exterior body 20, the overlapping portion 30 extends up to the end of the exterior body 20, and therefore the end of the overlapping portion 30 is also the end of the exterior body 20. The rising portions 31, 32, and 33 are each formed by bending the outer peripheral end of the overlapping portion 30 and rising toward the positive side in the z-axis direction. The rising portion 31 is located on the negative side of the power-generating element 10 in the x-axis direction and faces the side surface 11 without the power-generating element 10 in between. The rising portion 32 is located on the negative side of the power-generating element 10 in the y-axis direction and faces the side surface 12 without the power-generating element 10 in between. The rising portion 33 is located on the positive side of the power-generating element 10 in the x-axis direction and faces the side surface 13 without the power-generating element 10 in between. In the battery 1, the end of the overlapping portion 30 on the positive side of the y-axis direction of the power-generating element 10, where the electrode lead 91 and the counter electrode lead 92 are pulled out from the exterior body 20, does not rise and remains parallel to the main surfaces 15 and 16 of the power-generating element 10. In this embodiment, the rising portion 31 is an example of a first rising portion, and the rising portion 32 is an example of a second rising portion. The x-axis direction is an example of a first direction, and the y-axis direction is an example of a second direction.
[0098] In a plan view, rising portions 31 and 33 extend along the y-axis direction, and rising portion 32 extends along the x-axis direction. In a plan view, rising portions 31 and 33 and rising portion 32 extend in intersecting directions, specifically, in directions perpendicular to each other. In battery 1, rising portions 31, 32, and 33 form three sides of the rectangle of exterior body 20 in a plan view.
[0099] The rising portions 31, 32, and 33 are inclined at an angle θ with respect to the main surfaces 15 and 16 of the power-generating element 10 (the rising portion 32 is not shown in FIG. 2 ). While the angle θ is not particularly limited, an angle θ of 45° or greater can effectively reduce the projected area of the exterior body 20. In the example shown in FIG. 2 , the angle θ is 90°. Furthermore, from the viewpoint of effectively increasing the strength of the rising portions 31, 32, and 33, the angle θ may be 90° or less. The angles θ of the rising portions 31, 32, and 33 are, for example, the same, but two or more of these angles may be different from each other. In FIG. 2 , an imaginary plane parallel to the main surfaces 15 and 16 of the power-generating element 10 is indicated by a dashed line. As shown in FIG. 2 , the angle θ is the angle formed by the outer surfaces of the rising portions 31, 32, and 33 with respect to the imaginary plane.
[0100] 2 and 3 , in the battery 1, for example, the rising portions 31, 32, and 33 rise to a position higher than the height of the battery 1 at the location of the power-generating element 10 in a plan view. The height here refers to the length in the thickness direction of the power-generating element 10 from the bottom of the rising portions 31, 32, and 33 to the top surface of the battery 1 at the location of the power-generating element 10 in a plan view. This allows the rising portions 31, 32, and 33 to protect the power-generating element 10 from impacts from the height direction.
[0101] 4, the height to which the rising portions 31, 32, and 33 rise in the battery 1 may be lower than the height of the battery 1 at the location of the power-generating element 10 in a plan view. This allows the volume occupied in the thickness direction of the battery 1 to be reduced. FIG. 4 is a side view showing another example of the height of the rising portion 32. Although only the rising portion 32 is shown in FIG. 4, the rising portions 31 and 33 also rise to the same height as the rising portion 32. The heights of the rising portions 31, 32, and 33 may be the same, or two or more of them may be different from each other.
[0102] The heights of the rising portions 31, 32, and 33 can be adjusted, for example, by the bending position of the overlapping portion 30. The rising heights of the rising portions 31, 32, and 33 can also be adjusted by the angle θ.
[0103] As shown in Fig. 1, two adjacent rising portions among the rising portions 31, 32, and 33 are joined to each other by thermal fusion. In Fig. 1, the boundaries between the rising portions 31, 32, and 33 are schematically shown by solid lines, but in reality, the boundaries may not be visible due to the thermal fusion. This also applies to the other top views described below.
[0104] In battery 1, two adjacent rising portions among rising portions 31, 32, and 33 are two rising portions that form two adjacent sides in a planar view of exterior body 20. Each of rising portions 31, 32, and 33 is joined to the adjacent rising portion at an end in the direction in which it extends in a planar view.
[0105] Specifically, rising portions 31 and 32 are joined to each other, and rising portions 32 and 33 are joined to each other. In battery 1, rising portions 31 and 32, and rising portions 32 and 33 are joined to each other at the rectangular corners of exterior body 20 in a plan view. Note that this joining is not limited to thermal fusion, and may be performed by a method other than thermal fusion, such as adhesion with an adhesive, caulking using a caulking mechanism, or screw fastening.
[0106] Two adjacent rising portions among the rising portions 31, 32, and 33 have contact portions 42a and 42b that are joined in surface contact with each other, and non-contact portions 41a, 41b, and 41c that are not in contact with each other. In this specification, surface contact means contact on surfaces perpendicular to the thickness direction.
[0107] The contact portions 42a and 42b are joined to the non-contact portion 41b. In the battery 1, the contact portions 42a and 42b are located farther from the power-generating element 10 than the non-contact portions 41a, 41b, and 41c. This positions the contact portions 42a and 42b on the outer sides of the rising portions 31, 32, and 33, making it possible to easily form the contact portions 42a and 42b without being restricted by other components.
[0108] The contact portion 42a is a portion where the inner surfaces of the rising portions 31 and 32 are in surface contact with each other. The contact portion 42b is a portion where the inner surfaces of the rising portions 32 and 33 are in surface contact with each other. Here, the inner surfaces are the surfaces that face the power generating element 10 when the rising portions 31, 32, and 33 are raised.
[0109] The non-contact portion 41a is a portion of the rising portion 31 that is not in contact with other rising portions. The non-contact portion 41b is a portion of the rising portion 32 that is not in contact with other rising portions. The non-contact portion 41c is a portion of the rising portion 33 that is not in contact with other rising portions.
[0110] The electrode lead 91 and the counter electrode lead 92 are extraction electrodes connected to the power generating element 10. The electrode lead 91 and the counter electrode lead 92 are each made of a conductor such as a metal. The electrode lead 91 is connected to the electrode current collector 140, for example, at the main surface 16. The counter electrode lead 92 is connected to the counter electrode current collector 150, for example, at the main surface 15. The electrode lead 91 and the counter electrode lead 92 may each be connected to an end surface of the current collector, or may be integral with the current collector. For example, the electrode current collector 140 and the counter electrode current collector 150 may have a portion that functions as a current collector and a portion that functions as a lead.
[0111] A portion of the electrode lead 91 and the counter electrode lead 92 are disposed within the exterior body 20. The electrode lead 91 and the counter electrode lead 92 are drawn out from the end of the exterior body 20 on the positive side in the y-axis direction via the overlapping portion 30 located on the positive side in the y-axis direction of the power-generating element 10. This allows charging and discharging of the power-generating element 10 from outside the exterior body 20.
[0112] The sleeve 93 is disposed between the electrode lead 91 and the exterior body 20 and between the counter electrode lead 92 and the exterior body 20 at positions where the electrode lead 91 and the counter electrode lead 92 are pulled out from the exterior body 20. The sleeve 93 is made of an insulating material that can be heat-sealed to both the electrode lead 91 and the counter electrode lead 92 and the exterior body 20. By disposing the sleeve 93 between the electrode lead 91 and the exterior body 20 and between the counter electrode lead 92 and the exterior body 20, airtightness and insulation between the electrode lead 91 and the counter electrode lead 92 and the exterior body 20 can be ensured.
[0113] [Manufacturing Method] Next, a method for manufacturing the battery 1 according to this embodiment will be described. Note that the manufacturing method described below is an example, and the manufacturing method for the battery 1 according to this embodiment is not limited to the following example.
[0114] FIG. 5 is a flowchart showing an example of a method for manufacturing the battery 1 according to this embodiment.
[0115] As shown in Fig. 5, first, the power generating element 10 is prepared (step S10). For example, a unit cell having a battery cell 100 is prepared. Since the power generating element 10 has one battery cell 100, the unit cell can be used as the power generating element 10 as is. Furthermore, when the power generating element 10 has a plurality of battery cells 100, the power generating element 10 is prepared by stacking the prepared unit cells. Figs. 6A to 6C are each a cross-sectional view of an example of a unit cell.
[0116] 6A , the unit cell 100a has one battery cell 100, an electrode current collector 140, and a counter electrode current collector 150. In the unit cell 100a, the battery cell 100 is disposed between the electrode current collector 140 and the counter electrode current collector 150, and the battery cell 100 is in contact with both the electrode current collector 140 and the counter electrode current collector 150. Specifically, the electrode layer 110 of the battery cell 100 is in contact with the electrode current collector 140, and the counter electrode layer 120 of the battery cell 100 is in contact with the counter electrode current collector 150. The unit cell 100a has the same configuration as the power generating element 10 described above.
[0117] 6B , the unit cell 100b has one battery cell 100 and one electrode current collector 140. In the unit cell 100b, the electrode current collector 140 is disposed on the electrode layer 110 side of the battery cell 100, facing the battery cell 100, and is in contact with the electrode layer 110. In the unit cell 100b, the main surface of the counter electrode layer 120 of the battery cell 100 opposite the electrolyte layer 130 side is exposed.
[0118] 6C , a unit cell 100c has one battery cell 100 and one counter electrode current collector 150. In the unit cell 100c, the counter electrode current collector 150 is disposed on the counter electrode layer 120 side of the battery cell 100, facing the battery cell 100, and is in contact with the counter electrode layer 120. In the unit cell 100c, the main surface of the electrode layer 110 of the battery cell 100 opposite the electrolyte layer 130 side is exposed.
[0119] When stacking unit cells, at least one type of unit cell from the above-described unit cells 100a, 100b, and 100c is prepared according to the stack configuration of the power generating element to be included in the battery 1 to be manufactured. Fig. 7 is a cross-sectional view of a power generating element 10a having a plurality of battery cells 100 according to this embodiment. The battery 1 may include the power generating element 10a instead of the power generating element 10. Note that the batteries according to each of the modified examples and embodiments described below may also include the power generating element 10a.
[0120] The power generating element 10a is a stacked battery in which a plurality of battery cells 100 are connected in series by being stacked via bipolar current collectors 160. The power generating element 10a is, for example, an all-solid-state battery. When preparing the power generating element 10a, for example, one unit cell 100a and two unit cells 100b or 100c are prepared and stacked. The electrode current collector 140 or counter electrode current collector 150 sandwiched between the battery cells 100 functions as the bipolar current collector 160. It is also possible to stack only the unit cells 100a. In this case, two current collectors are placed between the battery cells 100. The unit cells may also be stacked so that the battery cells 100 can be connected in parallel.
[0121] Next, the electrode lead 91 and the counter electrode lead 92 are formed on the main surfaces of the power-generating element 10 (step S20). First, the electrode lead 91 and the counter electrode lead 92 are prepared. FIG. 8A is a top view of the electrode lead 91 and the counter electrode lead 92. FIG. 8B is a side view of the electrode lead 91 and the counter electrode lead 92. As shown in FIGS. 8A and 8B, the electrode lead 91 and the counter electrode lead 92 are inserted into a sleeve 93. The electrode lead 91 inserted into the sleeve 93 is connected to the electrode current collector 140 on the main surface 16, and the counter electrode lead 92 inserted into the sleeve 93 is connected to the counter electrode current collector 150 on the main surface 15.
[0122] Next, the power generating element 10 is sealed with the exterior body 20 (step S30). Fig. 9 is a top view of a battery 2a in the process of being manufactured according to this embodiment. Fig. 10 is a cross-sectional view of a battery 2a in the process of being manufactured according to this embodiment. Fig. 10 shows a cross section taken along line X-X shown in Fig. 9.
[0123] As shown in FIGS. 9 and 10 , for example, a power generating element 10 having an electrode lead 91 and a counter electrode lead 92 formed thereon is sandwiched between two laminate films 21a and 21b constituting an exterior body 20, covering both sides of the power generating element 10 in the thickness direction. The laminate films 21a and 21b are overlapped at a position surrounding the power generating element 10 in a planar view to form an overlapping portion 30. At this time, the tip sides of the electrode lead 91 and the counter electrode lead 92 are exposed. The laminate films 21a and 21b of the overlapping portion 30 are then heat-sealed to each other to seal the power generating element 10 with the exterior body 20. As shown in FIG. 9 , the overlapping portion 30 is formed in all directions outside the power generating element 10 in a planar view, such as the positive side, negative side, positive side, and negative side of the x-axis direction of the power generating element 10. As a result, the power generating element 10 is completely surrounded by the overlapping portion 30 in a planar view. For example, the overlapping portions 30 on the x-axis positive side, x-axis negative side, y-axis positive side, and y-axis negative side of the power-generating element 10 are heat-sealed in sequence using a sealer, etc. Note that, as described above, the overlapping portions 30 near the folded edges when the exterior body 20 is formed by folding a single laminate film, and near the edges other than the opening of the bag when the exterior body 20 is formed from a single bag-shaped laminate film, do not need to be heat-sealed.
[0124] As shown in FIG. 10 , the overlapping portion 30 is formed so as to be positioned at the center of the power generating element 10 in the thickness direction of the power generating element 10 .
[0125] Furthermore, the sealing of the power-generating element 10 with the exterior body 20 is performed in a reduced pressure atmosphere, such as in a vacuum chamber, thereby reducing the pressure and sealing the power-generating element 10 to the exterior body 20. When reducing the pressure and sealing the power-generating element 10, it is not necessary to perform all sealing operations in a reduced pressure atmosphere; it is sufficient that the operation is performed in a reduced pressure atmosphere at least until the heat fusion of all overlapping portions 30 is completed, that is, until the path between the power-generating element 10 in the exterior body 20 and the outside world is completely blocked.
[0126] The sealing of the power-generating element 10 by the exterior body 20 prevents moisture (water vapor) and other substances that can cause deterioration of the power-generating element 10 from penetrating into the interior of the exterior body 20. The laminate films 21a and 21b contain a metal layer, such as an aluminum layer, and therefore have a high moisture-blocking effect in the thickness direction. On the other hand, moisture can penetrate into the exterior body 20 in a direction perpendicular to the thickness direction of the laminate films 21a and 21b without passing through the metal layer. For example, moisture is likely to penetrate into the exterior body 20 from the end faces perpendicular to the thickness direction of the laminate films 21a and 21b. In the battery 2a, the overlapping portion 30 is formed to surround the power-generating element 10 and is heat-sealed for a certain length, thereby preventing moisture and other substances from penetrating through the end of the exterior body 20. However, in the state of the battery 2a, the projected area (i.e., the area in a plan view) of the exterior body 20 is large, which is disadvantageous for miniaturization.
[0127] Next, the ends of the overlapping portion 30 are raised to form raised portions 31, 32, and 33 (step S40). For example, the raised portions 31, 32, and 33 are formed by bending the overlapping portion 30 along the two-dot chain lines shown in FIG. 9. This allows the projected area of the exterior body 20 to be smaller than that of the battery 2a before the ends of the overlapping portion 30 are raised. Therefore, by reducing the projected area of the exterior body 20, which does not directly contribute to power generation, the area efficiency of the battery 1 can be improved.
[0128] Specifically, in plan view, the end of the overlapping portion 30 located on the negative side of the x-axis direction of the power generating element 10 is bent and raised to form the raised portion 31. As a result, the region ABCD in FIG. 9 is raised to form the raised portion 31.
[0129] In addition, in plan view, the end of the overlapping portion 30 located on the negative side of the power-generating element 10 in the y-axis direction is bent and raised to form a rising portion 32. As a result, the region BCFE in FIG. 9 rises, forming the rising portion 32.
[0130] In addition, in plan view, the end of the overlapping portion 30 located on the positive side of the power-generating element 10 in the x-axis direction is bent and raised to form a rising portion 33. As a result, the region EFHG in FIG. 9 rises, forming the rising portion 33.
[0131] Figure 11 is a top view of battery 2b in the middle of manufacture after Figure 10. As shown in Figure 11, raised portions 31, 32, and 33 are formed by raising the ends of overlapping portion 30. At this time, corners of exterior body 20 are folded outward in a planar view to form contact portion 42a where the inner surfaces of raised portions 31 and 32 are in surface contact with each other, and contact portion 42b where the inner surfaces of raised portions 32 and 33 are in surface contact with each other. In battery 2b, contact portions 42a and 42b protrude outward at the corners of exterior body 20 in a planar view.
[0132] After the rising portions 31, 32, and 33 are formed, the shapes of the rising portions 31, 32, and 33 may be stabilized by applying a backing plate or the like to the rising portions 31, 32, and 33 and heating them.
[0133] Next, two adjacent rising portions of the rising portions 31, 32, and 33 are joined (step S50). For example, in battery 2b, the contact portion 42a is sandwiched between heaters to join the rising portions 31 and 32 by thermal fusion, and the contact portion 42b is sandwiched between heaters to join the rising portions 32 and 33 by thermal fusion. Furthermore, the contact portions 42a and 42b are folded toward the non-contact portion 41b, bringing the contact portions 42a and 42b into contact with the non-contact portion 41b. Then, the contact portions 42a and 42b are joined to the non-contact portion 41b by thermal fusion using a heater or the like. This results in the battery 1 shown in FIGS. 1 to 3 .
[0134] In this way, in the battery 1, two adjacent rising portions among the rising portions 31, 32, and 33 are joined. This not only reduces the projected area of the exterior body 20, but also allows the rising portions 31, 32, and 33 to form a strong structure, improving the mechanical reliability of the battery 1. If the rising portions 31, 32, and 33 were simply bent but not joined, the rising structure would not be maintained when an external force of the same magnitude as that required for bending were applied. As a result, the power-generating element 10 would be more susceptible to external forces, increasing the risk of damage to the power-generating element 10. In contrast, by joining two adjacent rising portions among the rising portions 31, 32, and 33, the rising structure is maintained to the extent that the joints are broken, and the propagation of external forces to the power-generating element 10 can be suppressed until the joints are broken. Therefore, the battery 1 using the exterior body 20 can be made both compact and highly reliable.
[0135] Before joining the contact portions 42a and 42b, the contact portions 42a and 42b may be folded toward the non-contact portion 41b, and the joining of the two adjacent rising portions and the joining of the contact portions 42a and 42b and the non-contact portion 41b may be performed all at once. Furthermore, the joining is not limited to thermal fusion, and may be performed by a method other than thermal fusion, such as adhesion with an adhesive, caulking using a caulking mechanism, or screw fastening.
[0136] Alternatively, the contact portion 42a may be folded toward the non-contact portion 41a, and the contact portion 42b may be folded toward the non-contact portion 41c, and the contact portion 42a and the non-contact portion 41a may be joined together, and the contact portion 42b and the non-contact portion 41c may be joined together.
[0137] [Modification 1] Next, a description will be given of a battery according to Modification 1 of Embodiment 1. The following description will focus on differences from Embodiment 1, and description of commonalities will be omitted or simplified.
[0138] The manufacturing process of the battery according to this modification differs from that of the first embodiment in that, in forming the rising portions 31, 32, and 33 (step S40 described above), the corners of the exterior body 20 in plan view are folded inward. FIG. 12 is a top view of a battery 2c in the process of being manufactured according to this modification. As shown in FIG. 12 , by folding inward the corners of the exterior body 20 in plan view, the battery 2a shown in FIG. 10 above forms a contact portion 42c where the outer surfaces of the rising portions 31 and 32 are in surface contact with each other, and a contact portion 42d where the outer surfaces of the rising portions 32 and 33 are in surface contact with each other. Here, the outer surfaces are the surfaces that face away from the power-generating element 10 when the rising portions 31, 32, and 33 are raised. In the battery 2c, the contact portions 42c and 42d protrude inward at the corners of the exterior body 20 in plan view.
[0139] Then, in step S50, two adjacent rising portions of the rising portions 31, 32, and 33 are joined. For example, in battery 2c, rising portions 31 and 32 are joined at contact portion 42c, and rising portions 32 and 33 are joined at contact portion 42d. Furthermore, contact portions 42c and 42d are folded toward non-contact portion 41b, bringing the contact portions 42c and 42d into contact with non-contact portion 41b. Then, contact portions 42c and 42d are joined with non-contact portion 41b. This results in the battery 1a shown in FIG. 13. FIG. 13 is a top view of battery 1a according to this modification.
[0140] 13 , battery 1a has a configuration in which contact portions 42a and 42a of battery 1 according to embodiment 1 are replaced with contact portions 42c and 42d, respectively. Contact portions 42c and 42d are joined to non-contact portion 41b. In battery 1a, contact portions 42c and 42d are located closer to power generating element 10 than non-contact portions 41a, 41b, and 41c. This further reduces the projected area of exterior body 20, enabling battery 1a to be made even more compact.
[0141] [Modification 2] Next, a description will be given of a battery according to Modification 2 of Embodiment 1. The following description will focus on the differences from Embodiment 1 and Modification 1 of Embodiment 1, and description of commonalities will be omitted or simplified.
[0142] The manufacturing process of the battery according to this modification differs from that of embodiment 1 in that, when sealing the power-generating element 10 (step S30 described above), the overlapping portion 30 is formed offset from the center of the power-generating element 10 in the thickness direction. Fig. 14 is a cross-sectional view of a battery 2d according to this modification during manufacturing. As shown in Fig. 14 , the power-generating element 10 is sandwiched between two laminate films 21a and 21b that constitute the exterior body 20, and the overlapping portion 30 is formed offset from the center of the power-generating element 10 to the negative side in the z-axis direction in the thickness direction of the power-generating element 10. In addition, in battery 2d, the laminate film 21b below the power-generating element 10 is entirely parallel to the main surface 16 of the power-generating element 10.
[0143] In forming the battery 2d, a cup-shaped laminate film with a recess formed in advance at the location where it overlaps the power-generating element 10 in a planar view may be used as the laminate film 21a. This reduces stress on the corners of the power-generating element 10, where the laminate film 21a would be significantly bent during sealing, thereby suppressing damage to the power-generating element 10 or the laminate film 21a and reducing the risk of short circuits. Using a cup-shaped laminate film with a recess formed in the exterior body 20 is particularly effective when the power-generating element 10 is thick, and may be applied to a stacked battery such as the power-generating element 10a. Furthermore, as in the above-described battery 2a, cup-shaped laminate films may be used as the laminate films 21a and 21b even when the overlapping portion 30 is located at the center of the power-generating element 10 in the thickness direction.
[0144] The battery 1b shown in FIGS. 15 and 16 is obtained by forming rising portions 31, 32, and 33 on the battery 2d and joining adjacent rising portions of the rising portions 31, 32, and 33. FIG. 15 is a cross-sectional view of the battery 1b according to this modification. FIG. 16 is a side view of the battery 1b according to this modification. The top view of the battery 1b is the same as that of the battery 1 shown in FIG. 1, for example. The top view of the battery 1b may also be the same as that of the battery 1a shown in FIG. 13.
[0145] 15 and 16 , battery 1b differs from battery 1 according to embodiment 1 in the position of overlapping portion 30 in the thickness direction of power generating element 10. In battery 1b, the portion of overlapping portion 30 adjacent to power generating element 10 is shifted toward the negative z-axis direction, which is one side of the center of power generating element 10, in the thickness direction of power generating element 10. In addition, rising portions 31, 32, and 33 rise toward the positive z-axis direction, which is the other side of power generating element 10 in the thickness direction.
[0146] 15 and 16 , the height of the rising portions 31, 32, and 33 is lower than the height of the battery 1 at the location of the power-generating element 10 in a plan view. This reduces the volume occupied by the battery 1b in the thickness direction. Furthermore, because the overlapping portion 30 is offset from the center of the power-generating element 10 in the thickness direction, the height of the rising portions 31, 32, and 33 can be ensured while preventing the volume occupied by the battery 1b in the thickness direction from increasing.
[0147] Furthermore, as shown in Fig. 17 , in battery 1b, rising portions 31, 32, and 33 may rise to a position higher than the height of battery 1 at the location of power-generating element 10 in a plan view. Fig. 17 is a side view showing another example of the height of rising portion 32. Although only rising portion 32 is shown in Fig. 17 , rising portions 31 and 33 also rise to the same height as rising portion 32. This allows rising portions 31, 32, and 33 to protect power-generating element 10 against impacts from both sides in the height direction. In particular, when power-generating element 10 is thick, the entire power-generating element 10 can be effectively protected.
[0148] In the batteries of each modified example and each embodiment described below, the overlapping portion 30 may be positioned offset from the center of the thickness direction of the power generating element 10, as in battery 1b, or may be positioned at the center of the thickness direction of the power generating element 10, as in battery 1.
[0149] [Modification 3] Next, a description will be given of a battery according to Modification 3 of Embodiment 1. The following description will focus on the differences from Embodiment 1 and the modifications of Embodiment 1, and description of commonalities will be omitted or simplified.
[0150] The manufacturing process of the battery according to this modification differs from that of the first embodiment in that, in forming the raised portions 31, 32, and 33 (step S40 described above), notches are formed in the overlapping portion 30 before the end of the overlapping portion 30 is raised. FIG. 18 is a top view of a battery 2e in the process of being manufactured according to this modification. As shown in FIG. 18 , notches 35 are formed in the corners of the overlapping portion 30 in a planar view of the battery 2a shown in FIG. 10 described above. In the example shown in FIG. 18 , the notches 35 extend from the corners of the overlapping portion 30 (points C and F in FIG. 18 ) toward the power-generating element 10 in a planar view. Note that the notches 35 do not necessarily need to extend from the corners of the overlapping portion 30 toward the power-generating element 10 in a planar view; for example, they may extend inward from the outer periphery of the overlapping portion 30 near the corners of the overlapping portion 30.
[0151] Then, the overlapping portion 30 is bent along the two-dot chain lines shown in FIG. 18 to form raised portions 31, 32, and 33. Specifically, the region ABCD in FIG. 18 is raised to form raised portion 31. The region BCFE in FIG. 18 is raised to form raised portion 32. The region EFHG in FIG. 18 is raised to form raised portion 33. In this way, the raised portions 31, 32, and 33 are formed by raising the regions on both sides of the notch 35 in a plan view, using the notch 35 as a boundary. By raising the regions on both sides of the notch 35, the regions on both sides of the notch 35 do not interfere with each other when raising the ends of the overlapping portion 30, and the ends of the overlapping portion 30 can be easily raised.
[0152] Then, two adjacent rising portions 31, 32, and 33 are joined to obtain the battery 1c shown in FIG. 19 . FIG. 19 is a top view of the battery 1c according to this modification. In the battery 1c, two adjacent rising portions 31, 32, and 33 have contact portions 42e and 42f that are joined in surface contact with each other. Contact portion 42e is the portion where the inner surface of rising portion 31 and the outer surface of rising portion 32 are in surface contact with each other. Contact portion 42f is the portion where the outer surface of rising portion 32 and the inner surface of rising portion 33 are in surface contact with each other. Because contact portions 42e and 42f are formed without folding the corners of the overlapping portion 30, the reduction in the joint area between the rising portions due to folding can be suppressed. For example, contact portions 42e and 42f are more likely to have a larger surface contact area than contact portions 42a, 42b, 42c, and 42d.
[0153] [Modification 4] Next, a battery according to Modification 4 of Embodiment 1 will be described. The following description will focus on the differences from Embodiment 1 and the modifications of Embodiment 1, and description of commonalities will be omitted or simplified.
[0154] The manufacturing of a battery according to this modification differs from that of the first embodiment in that, in forming the rising portions 31, 32, and 33 (step S40 described above), notches are formed in the overlapping portion 30 before the end of the overlapping portion 30 is raised. Figure 19 is a top view of a battery 2f in the process of being manufactured according to this modification. As shown in Figure 19, notches 36 are formed in the corners of the overlapping portion 30 in a plan view of the battery 2a shown in Figure 10 described above. In the example shown in Figure 19, notches 36 are formed in the two corners on the negative side in the y-axis direction.
[0155] Then, the overlapping portion 30 is bent along the two-dot chain lines shown in FIG. 19 to form raised portions 31, 32, and 33. Specifically, the region ABCD in FIG. 19 is raised to form raised portion 31. The region BGFE in FIG. 19 is raised to form raised portion 32. The region EJIH in FIG. 19 is raised to form raised portion 33. In this way, raised portions 31, 32, and 33 are formed by raising the regions on both sides of the cutout 36 in a plan view, with the cutout 36 as a boundary. By raising the regions on both sides of the cutout 36, the regions on both sides of the cutout 36 do not interfere with each other when raising the ends of the overlapping portion 30, and the ends of the overlapping portion 30 can be easily raised.
[0156] Thereafter, two adjacent rising portions among the rising portions 31, 32, and 33 are joined to obtain the battery 1d shown in FIG. 21 . FIG. 21 is a top view of the battery 1d according to this modification. In the battery 1d, two adjacent rising portions among the rising portions 31, 32, and 33 are joined by contacting each other at their tips in a direction perpendicular to their thickness direction in a plan view, for example. In the battery 1d, the adjacent rising portions 31 and 32, and the adjacent rising portions 32 and 33, respectively, do not overlap each other in the thickness direction. This allows the battery 1d to be made smaller and lighter. Furthermore, stacking of the batteries 1d is improved when arranging them side by side.
[0157] Depending on the shape of the notch 36, two adjacent rising portions among the rising portions 31, 32, and 33 may be joined in surface contact with each other.
[0158] (Embodiment 2) Next, a battery according to embodiment 2 will be described. In the battery according to embodiment 2, adjacent rising portions are joined via a relay joining member. The following description will focus on the differences from embodiment 1 and the modifications of embodiment 1, and description of commonalities will be omitted or simplified.
[0159] Fig. 22 is a top view of battery 201 according to the present embodiment. Fig. 23 is a top view of another battery 201a according to the present embodiment. As shown in Figs. 22 and 23, batteries 201 and 201a according to the present embodiment differ from battery 1d according to Variation 4 of Embodiment 1 in that they further include relay joint member 60. Relay joint member 60 is an example of an auxiliary material.
[0160] The relay joint members 60 are attached to the adjacent rising portions 31 and 32, and the adjacent rising portions 32 and 33, respectively. In the batteries 201 and 201a, the adjacent rising portions 31 and 32, and the adjacent rising portions 32 and 33, are joined via the relay joint members 60, respectively. This allows the power generating element 10 to be protected by the relay joint members 60 as well. In the batteries 201 and 201a, the adjacent rising portions 31 and 32, and the adjacent rising portions 32 and 33, respectively, may or may not be directly joined by heat fusion or the like.
[0161] Each relay joint member 60 extends along the shape of the joint between adjacent rising portions 31 and 32 or the joint between adjacent rising portions 32 and 33. In the example shown in Figures 22 and 23, adjacent rising portions 31 and 32, and rising portions 32 and 33 are joined at corners of exterior body 20 in a plan view, and therefore relay joint member 60 is an L-shaped plate member in a plan view.
[0162] 22 , in the battery 201, the relay joining member 60 is provided at a position farther from the power generating element 10 than the rising portions 31, 32, and 33, and the inner surface of the relay joining member 60 is in contact with two adjacent rising portions of the rising portions 31, 32, and 33. In the battery 201, the relay joining member 60 easily protects the power generating element 10 from external forces, and the shape and size of the relay joining member 60 have a high degree of freedom.
[0163] 23 , in the battery 201a, the relay joint member 60 is provided at a position closer to the power generating element 10 than the rising portions 31, 32, and 33, and the outer surface of the relay joint member 60 contacts two adjacent rising portions among the rising portions 31, 32, and 33. The provision of the relay joint member 60 does not increase the size of the battery 201a, making it easy to miniaturize the battery 201a.
[0164] The rising portions 31, 32, and 33 are respectively joined to the relay joining member 60 by, for example, heat fusion or adhesion with an adhesive. In order to improve the joining property between the relay joining member 60 and the rising portions 31, 32, and 33, the surface of the relay joining member 60 may be uneven, or holes may be formed in the relay joining member 60.
[0165] The relay joint member 60 has, for example, higher rigidity than the exterior body 20. The material forming the relay joint member 60 is, for example, metal, ceramic, or resin, or a composite containing two or more of these.
[0166] In batteries 201 and 201a, battery 1d according to variant 4 of embodiment 1 is configured to further include relay joint member 60, but the above-mentioned batteries 1, 1a, 1b, or 1c may also further include relay joint member 60.
[0167] [Variation 1] Next, a description will be given of a battery according to Variation 1 of Embodiment 2. The following description will focus on Embodiment 2, each variation of Embodiment 1, and differences from Embodiment 2, and will omit or simplify the description of commonalities.
[0168] Fig. 24 is a top view of a battery 201b according to this modification. As shown in Fig. 24, the battery 201b according to this modification differs from the batteries 201 and 201a according to embodiment 2 in that it further includes a fastening member 63 for attaching the relay joint member 60. The fastening member 63 is an example of a crimping mechanism. In Fig. 24, the invisible portion of the fastening member 63 is indicated by a dashed line.
[0169] Battery 201b includes a pair of relay joint members 60 that sandwich the joint between adjacent rising portions 31 and 32, and another pair of relay joint members 60 that sandwich the joint between adjacent rising portions 32 and 33. Each pair of relay joint members 60 is attached to adjacent rising portions 31 and 32 or rising portions 32 and 33 by fastening members 63. As a result, adjacent rising portions 31 and 32 or rising portions 32 and 33 are joined to each other via the relay joint members 60.
[0170] The fastening member 63 is a member that can be fastened by, for example, a rivet, etc. This allows the relay joining member 60 to be attached to the rising portions 32 and 33 easily and firmly.
[0171] The fastening member 63 may be a member that can be fastened with a screw, such as a bolt and a nut. The battery 201b may include only one of the relay joint members 60 that are farther from the power generating element 10 than the rising portions 31, 32, and 33 and the relay joint members 60 that are closer to the power generating element 10 than the rising portions 31, 32, and 33.
[0172] (Embodiment 3) Next, a battery according to embodiment 3 will be described. In the battery according to embodiment 3, the overlapping portions where the leads are pulled out are raised. The following description will focus on the differences from embodiments 1 and 2 and the modifications of embodiments 1 and 2, and will omit or simplify the description of the commonalities.
[0173] Fig. 25 is a top view of battery 301 according to the present embodiment. As shown in Fig. 25, battery 301 according to the present embodiment differs from battery 201 according to embodiment 2 in that overlapping portion 30 further includes rising portion 34. In the present embodiment, rising portion 31 is an example of a first rising portion, and rising portion 34 is an example of a second rising portion.
[0174] In the battery 301, the overlapping portion 30 includes rising portions 31, 32, 33, and 34, which are portions of the overlapping portion 30 at their ends that rise. The rising portions 31, 32, 33, and 34 are each formed by bending the ends of the overlapping portion 30 and rising toward the positive side in the z-axis direction. In a plan view, the rising portions 31 and 33 extend along the y-axis direction, and the rising portions 32 and 34 extend along the x-axis direction. In a plan view, the rising portions 31 and 33 and the rising portions 32 and 34 extend in intersecting directions, specifically, perpendicular to each other. In the battery 301, the rising portions 31, 32, 33, and 34 form the four sides of the rectangular exterior body 20 in a plan view. In the battery 301, the power generating element 10 is completely surrounded by the rising portions 31, 32, 33, and 34 in a plan view.
[0175] The rising portion 34 is located on the positive side of the power-generating element 10 in the y-axis direction, and faces the side surface 14 without the power-generating element 10 in between. Although not shown, the angle θ at which the rising portion 34 is inclined with respect to the main surfaces 15 and 16 of the power-generating element 10 and the rising height are similar to the angle θ and the rising height of the rising portions 31, 32, and 33 described in the first embodiment above, respectively.
[0176] The adjacent rising portions 31 and 34, and the adjacent rising portions 33 and 34, are joined via an intermediate joining member 60, respectively.
[0177] In the battery 301, the electrode lead 91 and the counter electrode lead 92 are each drawn out from the exterior body 20 at the rising portion 34. Furthermore, the electrode lead 91 and the counter electrode lead 92 drawn out from the exterior body 20 at the rising portion 34 each extend toward the power-generating element 10 side of the rising portion 34 in a plan view. The electrode lead 91 and the counter electrode lead 92 each entirely overlap the exterior body 20 in a plan view.
[0178] 25 , the electrode lead 91 and the counter electrode lead 92 are each entirely bent on the distal end side of the sleeve 93 and extend toward the power-generating element 10 in plan view. The electrode lead 91 and the counter electrode lead 92 may each extend toward the opposite side from the power-generating element 10 in plan view.
[0179] The manner in which the electrode lead 91 and the counter electrode lead 92 are pulled out is not limited to the example shown in Fig. 25 . Fig. 26 is a top view of another battery 301a according to the present embodiment. As shown in Fig. 26 , in the battery 301a, the end of the rising portion 34 in the rising direction is further bent and extends toward the power-generating element 10. Therefore, the electrode lead 91 and the counter electrode lead 92 pulled out from the exterior body 20 at the rising portion 34 each extend toward the power-generating element 10 side of the rising portion 34 in a plan view without being bent. In the battery 301a, the electrode lead 91 and the counter electrode lead 92 pulled out from the exterior body 20 each overlap with the power-generating element 10 in a plan view.
[0180] The electrode lead 91 and the counter electrode lead 92 do not have to be drawn out from the exterior body 20 at the rising portion 34. For example, the electrode lead or the counter electrode lead may be drawn out from at least one of the main surfaces 15 or 16 to at least one of the positive side or negative side in the z-axis direction.
[0181] Battery 301 is manufactured, for example, from battery 302 in the process of manufacture shown in Fig. 27, and battery 301a is manufactured, for example, from battery 302a in the process of manufacture shown in Fig. 28. Fig. 27 is a top view of battery 302 in the process of manufacture according to this embodiment. Fig. 28 is a top view of another battery 302a in the process of manufacture according to this embodiment.
[0182] Batteries 302 and 302a are formed by adjusting the size of the overlapping portion 30 of battery 2f shown in Figure 20 and further forming notches 36 at two corners on the positive side of the y axis direction. The area KAHL of batteries 302 and 302a is raised toward the positive side of the z axis direction to form raised portions 34. Because the area KAHL of battery 302a is larger than that of battery 302, it is possible to further bend the end of the raised portion 34 in the raised direction.
[0183] For example, the batteries 301 and 301a allow for miniaturization of the wiring board. FIG. 29 is a side view showing an example of a wiring board 180 on which the battery 301a is mounted. In FIG. 24, the shapes of the power generating element 10, electrode lead 91, counter electrode lead 92, and sleeve 93 are indicated by dashed lines. In the example shown in FIG. 29, the battery 301a is mounted on the wiring board 180 with its main surfaces 15 and 16 parallel to the wiring board 180 and with the electrode lead 91 and counter electrode lead 92 drawn out from the outer casing 20 closer to the wiring board 180. Mounting the battery 301a, which can reduce the projected area, allows for miniaturization of the wiring board 180. Furthermore, an electronic component 182 that receives power from the battery 301a is mounted on the wiring board 180.
[0184] The electrode lead 91 and the counter electrode lead 92 are joined to the wiring board 180 via a joining member 181 such as solder. At least one of the rising portions 31, 32, 33, and 34 may be joined to the wiring board 180. This further improves the mechanical reliability of the battery 301a. In addition, the distance between the electronic component 182 mounted on the wiring board 180 and the battery 301a can be shortened, which is advantageous for forming a high-frequency circuit.
[0185] In batteries 301 and 301a, the overlapping portion 30 of battery 201 according to embodiment 2 further includes a rising portion 34, but the overlapping portion 30 of the above-mentioned batteries 1, 1a, 1b, 1c, 1d, 201a or 201b may further include a rising portion 34.
[0186] While the batteries and battery manufacturing methods according to one or more aspects have been described above based on the embodiments and modifications, the present disclosure is not limited to these embodiments. As long as they do not deviate from the gist of the present disclosure, various modifications that would occur to a person skilled in the art to the present embodiments and modifications, and configurations constructed by combining components of different embodiments and modifications, are also included within the scope of the present disclosure.
[0187] For example, although the power generating element 10 is an all-solid-state battery in the above embodiment, the power generating element 10 is not limited to this and may be a liquid battery including an electrolyte and a separator.
[0188] Furthermore, various modifications, substitutions, additions, omissions, etc. can be made to each of the above-described embodiments within the scope of the claims or their equivalents.
[0189] Batteries according to the present disclosure can be used as batteries for a variety of applications, such as electronic devices, electrical appliances, and electric vehicles.
[0190] DESCRIPTION OF SYMBOLS 1, 1a, 1b, 1c, 1d, 2a, 2b, 2c, 2d, 2e, 2f, 201, 201a, 201b, 301, 301a, 302, 302a Battery 10, 10a Power generating element 11, 12, 13, 14 Side surface 15, 16 Main surface 20 Exterior body 21a, 21b Laminate film 30 Overlapping portion 31, 32, 33, 34 Rising portion 35 Cutout 36 Notch 41a, 41b, 41c Non-contact portion 42a, 42b, 42c, 42d, 42e, 42f Contact portion 60 Relay joining member 63 Fastening member 91 Electrode lead 92 Counter electrode lead 93 Sleeve 100 Battery cell 100a, 100b, 100c Unit cell 110 Electrode layer 120 Counter electrode layer 130 Electrolyte layer 140 Electrode current collector 150 Counter electrode current collector 160 Bipolar current collector 180 Wiring substrate 181 Bonding member 182 Electronic component
Claims
1. A battery comprising: a power generating element; and an exterior body made of a laminate film and sealing the power generating element, wherein the exterior body is positioned to surround the power generating element in a plan view relative to the main surface of the power generating element, and has an overlapping portion where the laminate film is overlapped, wherein the overlapping portion includes: a first raised portion where an end of the overlapping portion located on a first direction side of the power generating element in the plan view is raised; and a second raised portion where an end of the overlapping portion on a second direction side of the power generating element that intersects with the first direction in the plan view is raised, and the first raised portion and the second raised portion are joined to each other.
2. The battery according to claim 1, wherein the power generating element is sealed in the exterior body under reduced pressure.
3. The battery according to claim 1, wherein the laminate films are heat-sealed together at the overlapping portions.
4. The battery according to claim 1, wherein the first raised portion and the second raised portion are joined by thermal fusion.
5. The battery according to claim 1, wherein at least one of the first raised portion and the second raised portion rises to a position higher than the height of the battery at a point where the power generating element is present in the plan view.
6. The battery according to claim 1, wherein the first raised portion and the second raised portion have a contact portion joined to each other in face-to-face contact and a non-contact portion not in contact with each other, and the contact portion is located closer to the power generating element than the non-contact portion.
7. The battery according to claim 1, wherein the first raised portion and the second raised portion have a contact portion joined to each other in face-to-face contact and a non-contact portion not in contact with each other, and the contact portion is provided at a position farther from the power generating element than the non-contact portion.
8. The battery according to claim 1, wherein the first raised portion and the second raised portion have a contact portion joined to each other in face-to-face contact and a non-contact portion not in contact with each other, and the contact portion is joined to the non-contact portion.
9. The battery according to claim 1, wherein, in the plan view, the first raised portion and the second raised portion are joined to each other at their tips in a direction perpendicular to the thickness direction of the first raised portion and the second raised portion.
10. The battery according to claim 1, further comprising an auxiliary material attached to said first raised portion and said second raised portion, said first raised portion and said second raised portion being joined via said auxiliary material.
11. The battery according to claim 10, wherein the auxiliary material is attached to the first raised portion and the second raised portion by a crimping mechanism.
12. A battery as described in any one of claims 1 to 11, wherein the overlapping portion is offset to one side from the center of the power generating element in the thickness direction of the power generating element, and the first raised portion and the second raised portion rise toward the other side in the thickness direction of the power generating element.
13. The battery according to any one of claims 1 to 11, wherein the power generating element is an all-solid-state battery.
14. The battery according to any one of claims 1 to 11, wherein the first raised portion and the second raised portion are inclined at an angle of 45° or more with respect to the main surface of the power generating element.
15. A battery as described in any one of claims 1 to 11, further comprising a lead connected to the power generating element and a portion of which is disposed within the exterior body, the lead being pulled out from the exterior body at the second raised portion, and the entire lead overlapping with the exterior body in the planar view.
16. A method for manufacturing a battery, comprising: covering a power generating element with a laminate film and forming an overlapping portion by overlapping the laminate film at a position surrounding the power generating element in a planar view with respect to a main surface of the power generating element, thereby sealing the power generating element with an exterior body composed of the laminate film; raising ends of the overlapping portion to form a first raised portion at the raised end of the overlapping portion located on the first direction side of the power generating element in the planar view, and a second raised portion at the raised end of the overlapping portion on the second direction side of the power generating element that intersects with the first direction in the planar view; and joining the first raised portion and the second raised portion.
17. The method for manufacturing a battery as described in claim 16, wherein in the step of sealing the power generating element, the overlapped laminate films in the overlapping portions are heat-sealed to seal the power generating element in the exterior body.
18. The method for producing a battery according to claim 16, wherein the power generating element is an all-solid-state battery.
19. A method for manufacturing a battery as described in any one of claims 16 to 18, wherein in the step of forming the first raised portion and the second raised portion, a notch is formed in the overlapping portion before raising the end of the overlapping portion, and the first raised portion and the second raised portion are formed by raising both sides of the notch.
20. A method for manufacturing a battery as described in any one of claims 16 to 18, wherein in the step of forming the first raised portion and the second raised portion, a notch is formed in the overlapping portion before raising the end of the overlapping portion, and the first raised portion and the second raised portion are formed by raising both sides of the notch.
Citation Information
Patent Citations
Battery and battery pack
JP2001256933A
Electrochemical device and manufacturing method therefor
JP2002260601A
Plate-shaped battery
JP2005038613A
Electrochemical cell
JP2015165460A
Manufacturing method of laminate all-solid battery
JP2018133175A