Foldable display module and foldable display device

By using a glass substrate with a thickness of less than or equal to 100 microns in a foldable display device, combined with the rigidity and flexibility of the glass substrate, a hybrid foldable display panel is formed, which solves the crease problem and achieves light or even no creases. The effect improves user experience and service life.

WO2024216686A1PCT designated stage expired Publication Date: 2024-10-24WUHAN CHINA STAR OPTOELECTRONICS SEMICONDUCTOR DISPLAY TECHNOLOGY CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
PCT/CN2023/093854
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-17
Filing Date
2023-05-12
Publication Date
2024-10-24

AI Technical Summary

Technical Problem

Foldable display devices are prone to creases during use, which affects the user experience.

Method used

A glass substrate is used as the carrier of the main display structure. The thickness of the part of the glass substrate corresponding to the foldable area is less than or equal to 100 microns. Combined with the rigidity and flexibility of the glass substrate, a hybrid foldable display panel is formed, omitting the backplane and backplane in traditional technology. Foam layer and glue layer, reduce the use of glue layer to avoid creases caused by plastic deformation.

Benefits of technology

It achieves light or even no creases for foldable display modules and devices, improving appearance and user experience and extending service life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023093854_24102024_PF_FP_ABST
    Figure CN2023093854_24102024_PF_FP_ABST
Patent Text Reader

Abstract

A foldable display module (200) and a foldable display device (300). The foldable display module (200) is provided with a foldable area (200a) and a non-foldable area (200b) adjacent to the foldable area (200a); the foldable display module (200) comprises a display main body structure (04) and a glass substrate (041); the glass substrate (041) is located on the back side of the light exit surface of the display main body structure (04); and the thickness (H1) of the part of the glass substrate (041) corresponding to the foldable area (200a) is less than or equal to 100 microns.
Need to check novelty before this filing date? Find Prior Art

Description

Foldable display module and foldable display device Technical Field

[0001] The present application relates to the field of display technology, and in particular to a foldable display module and a foldable display device. Background Art

[0002] Foldable display devices have become a mainstream development trend in the display industry. From small foldable phones to mid-to-large foldable laptops, foldable display devices are increasingly popular with users due to their easy storage and high portability. However, foldable display devices are prone to creases during use, which seriously affects the user experience.

[0003] Therefore, the fact that foldable display devices are prone to creases during use is an industry pain point that needs to be solved urgently. SUMMARY OF THE INVENTION

[0004] The purpose of the present application is to provide a foldable display module and a foldable display device to improve the problem that the foldable display module and the foldable display device are prone to creases during use.

[0005] In a first aspect, the present application provides a foldable display module, wherein the foldable display module has a foldable area and a non-foldable area adjacent to the foldable area, and the foldable display module includes:

[0006] Display the main structure; and

[0007] A glass substrate is located on the back side of the light-emitting surface of the display main structure, and the thickness of the portion of the glass substrate corresponding to the foldable area is less than or equal to 100 microns.

[0008] In a second aspect, the present application also provides a foldable display device, which includes: the above-mentioned foldable display module. Beneficial effects

[0009] Because a glass substrate serves as the carrier of the display main structure, the thickness of the portion of the glass substrate corresponding to the foldable area is less than or equal to 100 microns. This thinning allows the portion of the glass substrate corresponding to the foldable area to be flexible, allowing the portion of the glass substrate corresponding to the foldable area to be folded. Furthermore, the glass substrate itself is rigid, and the display main structure is disposed on the glass substrate, so that the glass substrate and the display main structure form a foldable display panel that is both rigid and flexible. In other words, the glass substrate and the display main structure form a hybrid foldable display panel. Furthermore, because the glass substrate provides rigid support, it is advantageous to omit supporting components such as the backplane and foam layer located on the back side of the flexible display panel in conventional technologies, thereby omitting the adhesive layer on the back side of the flexible display panel, thereby improving the crease problem caused by plastic deformation of the adhesive layer in the foldable display module. BRIEF DESCRIPTION OF THE DRAWINGS

[0010] FIG1 is a cross-sectional schematic diagram of a foldable display module in the related art;

[0011] FIG2 is a first cross-sectional schematic diagram of a foldable display module according to an embodiment of the present application;

[0012] FIG3 is a second cross-sectional schematic diagram of a foldable display module according to an embodiment of the present application;

[0013] FIG4 is a third cross-sectional schematic diagram of a foldable display module according to an embodiment of the present application;

[0014] FIG5 is a fourth cross-sectional schematic diagram of a foldable display module according to an embodiment of the present application;

[0015] FIG6 is a fifth cross-sectional schematic diagram of a foldable display module according to an embodiment of the present application;

[0016] FIG7 is a first cross-sectional schematic diagram of a foldable display module according to another embodiment of the present application;

[0017] FIG8 is a second cross-sectional schematic diagram of a foldable display module according to another embodiment of the present application;

[0018] FIG9 is a schematic cross-sectional view of a foldable display device according to an embodiment of the present application. Modes for Carrying Out the Invention

[0019] The following will be combined with the drawings in the embodiments of the present application to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the embodiments described are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by those skilled in the art without making creative efforts are within the scope of protection of this application.

[0020] Please refer to Figure 1, which is a cross-sectional schematic diagram of a foldable display module in the related art. Foldable display module 100 has a foldable area 100a and two non-foldable areas 100b, with the two non-foldable areas 100b adjacent to opposite sides of foldable area 100a. Foldable display module 100 includes a flexible display panel 01, a first module 02, and a second module 03. First module 02 is located on the light-emitting side of flexible display panel 01, and second module 03 is located on the back side of the light-emitting side of flexible display panel 01.

[0021] The flexible display panel 01 comprises a stacked flexible substrate 011, a driving circuit layer 012, a light-emitting device layer 013, and a thin-film encapsulation layer 014. The light-emitting device layer 013 includes multiple light-emitting devices, which are organic light-emitting diodes (OLEDs), but are not limited to these. Quantum light-emitting diodes (QLEDs) can also be used. Flexible substrate 011 is a polymer substrate.

[0022] The first module 02 includes a touch layer 021, a polarizer 022, an ultra-thin glass 023, a protective cover 024, a first adhesive layer 0251, a second adhesive layer 0252, a third adhesive layer 0253, and a fourth adhesive layer 0254. The first adhesive layer 0251, the second adhesive layer 0252, the third adhesive layer 0253, and the fourth adhesive layer 0254 are all transparent optical clear adhesives (OCAs).

[0023] First adhesive layer 0251 bonds touch layer 021 to thin film encapsulation layer 014 of flexible display panel 01. Second adhesive layer 0252 bonds touch layer 021 to polarizer 022. Third adhesive layer 0253 bonds polarizer 022 to ultra-thin glass 023. Fourth adhesive layer 0254 bonds ultra-thin glass 023 to protective cover 024. Protective cover 024 is a transparent polymer substrate.

[0024] The second module 03 includes a back plate 031, a foam layer 032, a metal support layer 033, a fifth adhesive layer 0341, a sixth adhesive layer 0342, and a seventh adhesive layer 0343. The fifth adhesive layer 0341, the sixth adhesive layer 0342, and the seventh adhesive layer 0343 are all pressure-sensitive adhesive (PSA) layers.

[0025] The fifth adhesive layer 0341 bonds the flexible substrate 011 of the flexible display panel 01 to the backplane 031 . The sixth adhesive layer 0342 bonds the backplane 031 to the foam layer 032 . The seventh adhesive layer 0343 bonds the metal support layer 033 to the foam layer 032 .

[0026] Regarding the foldable display module 100 in the related art, creases are likely to appear on the foldable display module 100 after being folded multiple times, which affects the appearance of the foldable display module 100 .

[0027] After disassembling the foldable display module 100 in the related art, the inventors found through analysis that the presence of a film layer in the foldable display module 100 that is prone to plastic deformation is a key factor that causes creases to easily form. In particular, the optical adhesive layer and the pressure-sensitive adhesive layer in the foldable display module 100 are both prone to plastic deformation.

[0028] Based on the above findings and on the basis of related technologies, the present application improves the problem of creases in the foldable display module caused by plastic deformation of the glue layer by reducing the number of glue layers in the foldable display module or even completely removing the glue layers in the foldable display module.

[0029] The specific solution of the present application includes using a glass substrate as a carrier for the display main structure, wherein the thickness of the portion of the glass substrate corresponding to the foldable area is less than or equal to 100 microns, and then thinning the portion of the glass substrate corresponding to the foldable area to a degree that it is flexible, so that the portion of the glass substrate corresponding to the foldable area can be folded. In addition, the glass substrate itself has rigidity, and the display main structure is disposed on the glass substrate, so that the glass substrate and the display main structure constitute a foldable display panel that is both rigid and flexible. In other words, the glass substrate and the display main structure constitute a hybrid foldable display panel. In addition, because the glass substrate provides rigid support, it is advantageous to omit supporting components such as the backplane and foam layer located on the back side of the flexible display panel in traditional technology, thereby omitting the adhesive layer on the back side of the flexible display panel, thereby improving the crease problem caused by plastic deformation of the adhesive layer in the foldable display module.

[0030] The solution of this application is described below with reference to specific embodiments.

[0031] Please refer to FIG. 2 , which is a first cross-sectional schematic diagram of a foldable display module according to an embodiment of the present application.

[0032] In this embodiment, the foldable display module 200 includes a foldable region 200a and a non-foldable region 200b adjacent to the foldable region 200a. The two non-foldable regions 200b are located on opposite sides of the foldable region 200a. When the foldable region 200a and the non-foldable region 200b are coplanar, the foldable display module 200 is in a flattened state. When the foldable region 200a and the non-foldable region 200b are located in intersecting planes, the foldable display module 200 is in a folded state.

[0033] The number of the foldable areas 200a may be one or more. Specifically, the number of the foldable areas 200a is one, and the number of the non-foldable areas 200b is two.

[0034] In this embodiment, the foldable display module 200 includes a glass substrate 041 and a display main structure 04 stacked in sequence, and the glass substrate 041 is located on the back side of the light emitting surface of the display main structure 04 .

[0035] In this embodiment, the thickness H1 of the portion of the glass substrate 041 corresponding to the foldable area 200a is less than or equal to 100 microns, so that the thickness H1 of the portion of the glass substrate 041 corresponding to the foldable area 200a is thinned to be flexible, so that the portion of the glass substrate 041 corresponding to the foldable area 200a can be folded.

[0036] It should be noted that the glass substrate is generally used as a rigid substrate for the hard display panel in the related technology, and the thickness of the glass substrate is generally 480 microns to 600 microns. Due to the thick thickness of the glass substrate, the hard display panel cannot be folded. Moreover, since the glass substrate is thick and cannot be folded when used as a rigid substrate, it is not currently used in foldable display panels.

[0037] However, the present application innovatively uses an initial glass substrate with a thickness of 480 to 600 microns as a substrate. After forming the display main structure 04 and the like on the initial glass substrate, the initial glass substrate is thinned so that the thickness of the portion of the initial glass substrate corresponding to the foldable area is thinned to less than or equal to 100 microns, thereby ensuring that the portion of the glass substrate corresponding to the foldable area is foldable. Combined with the rigidity of the glass substrate itself, this is beneficial for the foldable display panel including the thinned glass substrate to have both flexibility and rigidity.

[0038] Furthermore, the ultra-thin glass 023 in the related art is too thin to be directly used as a carrier for the display main structure 04. Furthermore, when using the ultra-thin glass 023 as a rigid carrier, it must be attached to the back side of the light-emitting surface of the display main structure 04 with the aid of an adhesive layer. This adhesive layer increases the risk of creases forming during the folding process of the foldable display module 200.

[0039] In this embodiment, since the display main structure 04 is directly formed on the initial glass substrate, there is no adhesive layer between the display main structure 04 and the glass substrate 041 .

[0040] In this embodiment, the thickness H1 of the portion of the glass substrate 041 corresponding to the foldable region 200a is greater than 0 microns. This allows the portion of the glass substrate 041 corresponding to the foldable region 200a to be foldable while also providing rigid support and protection. The glass substrate 041 and the display main structure 04 constitute a hybrid foldable display panel. Furthermore, the portion of the glass substrate 041 corresponding to the foldable region 200a is made of a rigid material, and the portion of the glass substrate 041 corresponding to the foldable region 200a does not undergo plastic deformation.

[0041] Furthermore, the thickness H1 of the portion of the glass substrate 041 corresponding to the foldable area 200a is greater than or equal to 10 microns, so as to ensure that the portion of the glass substrate 041 corresponding to the foldable area 200a has rigid support while meeting the precision of the glass substrate thinning process.

[0042] It should be noted that, the thinner the thickness H1 of the portion of the glass substrate 041 corresponding to the foldable area 200 a is, the better the foldability of the portion of the glass substrate 041 corresponding to the foldable area 200 a is, and the more difficult the thinning process is.

[0043] It can be understood that the thickness H1 of the portion of the glass substrate 041 corresponding to the foldable area 200a may also be greater than or equal to 20 microns and less than or equal to 90 microns; alternatively, the thickness H1 of the portion of the glass substrate 041 corresponding to the foldable area 200a may also be greater than or equal to 30 microns and less than or equal to 80 microns; alternatively, the thickness H1 of the portion of the glass substrate 041 corresponding to the foldable area 200a may also be greater than or equal to 40 microns and less than or equal to 60 microns; alternatively, the thickness H1 of the portion of the glass substrate 041 corresponding to the foldable area 200a may be greater than or equal to 12 microns and less than or equal to 18 microns.

[0044] For example, the thickness H1 of the portion of the glass substrate 041 corresponding to the foldable area 200a can be 10 microns, 15 microns, 18 microns, 20 microns, 30 microns, 35 microns, 40 microns, 45 microns, 50 microns, 55 microns, 60 microns, 65 microns, 75 microns, 80 microns, 85 microns, 90 microns, 95 microns or 100 microns.

[0045] In this embodiment, the thickness H1 of the portion of the glass substrate 041 corresponding to the foldable area 200a is equal to the thickness H2 of the portion of the glass substrate 041 corresponding to the non-foldable area 200b, so as to ensure that the portion of the glass substrate 041 corresponding to the foldable area 200a is foldable while ensuring the flatness of the glass substrate 041, thereby ensuring the flatness of the foldable display module 200.

[0046] Specifically, the thickness H2 of the portion of the glass substrate 041 corresponding to the non-foldable area 200 b is greater than or equal to 10 micrometers and less than or equal to 100 micrometers.

[0047] For example, the thickness H2 of the portion of the glass substrate 041 corresponding to the non-foldable area 200b is 10 microns, 15 microns, 18 microns, 20 microns, 30 microns, 35 microns, 40 microns, 45 microns, 50 microns, 55 microns, 60 microns, 65 microns, 75 microns, 80 microns, 85 microns, 90 microns, 95 microns or 100 microns.

[0048] It should be noted that this application uses an initial glass substrate with a thickness of 480 to 520 microns as a substrate. After fabricating the display main structure 04 and other structures on the initial glass substrate, the surface of the initial glass substrate facing away from the display main structure 04 is thinned as a whole to obtain a glass substrate 041 with a thickness of 10 to 100 microns. The thickness H1 of the portion of the glass substrate 041 corresponding to the foldable area 200a is equal to the thickness H2 of the portion of the glass substrate 041 corresponding to the non-foldable area 200b. Methods for thinning the glass substrate include, but are not limited to, mechanical grinding and chemical etching.

[0049] In this embodiment, because the surface 041b of the glass substrate 041, which is remote from the display main structure 04, has been thinned, the surface 041b of the glass substrate 041, which is remote from the display main structure 04, is relatively rough. In contrast, the surface 041c of the glass substrate 041, which is near the display main structure 04, has not been treated and is relatively smooth. Therefore, along the thickness direction of the glass substrate 041, the roughness of the surface 041b of the glass substrate 041, which is remote from the display main structure 04, is greater than the roughness of the surface 041c of the glass substrate 041, which is near the display main structure 04.

[0050] In this embodiment, the display main structure 04 includes a display pixel layer 042 and a thin film encapsulation layer 043 .

[0051] In this embodiment, the display pixel layer 042 is located on one side of the glass substrate 041. Specifically, the display pixel layer 042 is located on the surface of the glass substrate 041. In other words, the display pixel layer 042 is in direct contact with the surface of the glass substrate 041.

[0052] In this embodiment, since the display pixel layer 042 is in direct contact with the surface of the glass substrate 041, there is no flexible substrate between the glass substrate 041 and the display pixel layer 042. This improves the foldable display module 200 from creases caused by plastic deformation of the flexible substrate. The flexible substrate can be made of, but not limited to, polyimide. Furthermore, since the glass substrate 041 can provide support, the flexible substrate can also be omitted.

[0053] It should be noted that, in the present application, direct contact between two film layers means that there is no other film layer between the two film layers, for example, there is no adhesive layer between the two film layers.

[0054] The display pixel layer 042 includes a driving circuit layer 0421 and a light-emitting device layer 0422. The light-emitting device layer 0422 is located on the surface of the driving circuit layer 0421 away from the glass substrate 041. The driving circuit layer 0421 includes multiple driving circuits, and the light-emitting device layer 0422 includes multiple light-emitting devices, which are electrically connected to the driving circuits. The light-emitting devices are organic light-emitting diodes, but are not limited to such. The light-emitting devices can also be quantum dot light-emitting diodes, etc.

[0055] In this embodiment, the thin film encapsulation layer 043 is used to encapsulate the display pixel layer 042 to extend the service life of the display main structure 04. The thin film encapsulation layer 043 is located on the side of the display pixel layer 042 away from the glass substrate 041 and covers the display pixel layer 042.

[0056] The thin film encapsulation layer 043 includes two inorganic layers and an organic layer located between the two inorganic layers. The inorganic layer is made of, but not limited to, at least one of silicon nitride, silicon oxide, and aluminum oxide. The organic layer is made of, but not limited to, at least one of polyimide and polyacrylate.

[0057] In this embodiment, since the glass substrate 041 can play a role of rigid support in both the foldable area 200a and the non-foldable area 200b, the foldable display module 200 of this embodiment does not include supporting bodies such as a back plate, a foam layer, and a metal layer that play a supporting role in the related art, so as to reduce the number of adhesive layers located on the back side of the light-emitting surface of the display main structure 04, or even completely remove the adhesive layer located on the back side of the light-emitting surface of the display main structure 04, thereby improving the crease problem caused by the plastic deformation of the adhesive layer of the foldable display module 200.

[0058] In this embodiment, the foldable display module 200 further includes a functional module 05 , which is located on the surface of the display main structure 04 away from the glass substrate 041 and includes at least two stacked functional layers 051 , with any two adjacent functional layers 051 in contact with each other.

[0059] Specifically, the functional module 05 is located on the surface of the thin film encapsulation layer 043 away from the display pixel layer 042. The functional module 05 includes at least two functional layers 051, and any two adjacent functional layers 051 are in direct contact with each other.

[0060] In this embodiment, functional module 05 is located on the surface of thin film encapsulation layer 043 away from display pixel layer 042, allowing direct contact between functional module 05 and thin film encapsulation layer 043. This eliminates the adhesive layer between functional module 05 and thin film encapsulation layer 043, thereby improving the folding problem caused by plastic deformation of the adhesive layer in foldable display module 200. Furthermore, direct contact between any two film layers in functional module 05 also eliminates the adhesive layer between any two film layers in functional module 05, reducing the adhesive layer in functional module 05 and further improving the folding problem caused by plastic deformation of the adhesive layer in foldable display module 200.

[0061] It should be noted that in the related art, the light-emitting side of the flexible display panel 01 has four adhesive layers. However, in this application, the functional module 05 is located on the surface of the thin-film encapsulation layer 043 away from the display pixel layer 042, and the functional module 05 includes at least two functional layers 051, with any two adjacent functional layers 051 in direct contact with each other, thus removing all four adhesive layers on the light-emitting side of the flexible display panel 01 in the related art.

[0062] The functional layer 051 includes, but is not limited to, at least one of a touch layer, an optical functional layer, and a light-transmitting protective layer. The optical functional layer includes, but is not limited to, a color filter layer and an optical lens layer. The light-transmitting protective layer includes, for example, a hard coating layer.

[0063] In this embodiment, the functional module 05 includes a touch layer 052, a color filter layer 053, and a hard coating layer 054. The touch layer 052 is located on the surface of the display main structure 04 away from the glass substrate 041. The color filter layer 053 is located on the surface of the touch layer 052 away from the display main structure 04. The hard coating layer 054 is located on the surface of the color filter layer 053 away from the touch layer 052.

[0064] Specifically, the touch layer 052 is located on the surface of the thin film encapsulation layer 043 away from the display pixel layer 042. The color filter layer 053 is located on the surface of the touch layer 052 away from the thin film encapsulation layer 043. The hard coating layer 054 is located on the surface of the color filter layer 053 away from the touch layer 052.

[0065] In this embodiment, the touch layer 052 includes touch electrodes and touch electrode lines connected to the touch electrodes. The touch electrodes include either mutual capacitance touch electrodes or self-capacitance touch electrodes. The touch layer 052 is fabricated directly on the thin film encapsulation layer 043 and is therefore directly attached to the display main structure 04.

[0066] Color filter layer 053 includes a black matrix layer and multiple photoresist units. The black matrix layer includes multiple openings, and the photoresist units are disposed one-to-one within the openings. Color filter layer 053 is formed directly on touch layer 052, so color filter layer 053 is directly attached to touch layer 052.

[0067] It should be noted that this embodiment uses a color filter layer 053 to replace the polarizer in traditional technology. The color filter layer 053 can be directly formed on the touch layer 052 without the need for a glue layer, which is beneficial for reducing the glue layer in the functional module 05.

[0068] The hard coating layer 054 protects the underlying functional film layers. The material of the hard coating layer 054 includes a cured optical adhesive layer, ensuring that the hard coating layer 054 can be directly formed on the surface of the color filter layer 053 away from the touch layer 052 through a coating and curing process. The material of the cured optical adhesive layer includes, but is not limited to, at least one of an acrylic resin, an epoxy resin, and a polyurethane.

[0069] It is understandable that the hard coating 054 may also include an inorganic layer, and the material of the inorganic layer includes but is not limited to at least one of silicon nitride, silicon oxide and aluminum oxide.

[0070] It should be noted that the present application replaces the traditional ultra-thin glass and protective cover with a hard coating 054, so that the hard coating 054 plays a protective role for the functional layer below it. Moreover, ultra-thin glass and protective cover require an adhesive layer for attachment. Since the hard coating 054 can be formed on other film layers by coating or other methods without an adhesive layer, it is beneficial to reduce the adhesive layer in the functional module 05. In addition, in some related technologies, the hard coating is formed on a flexible substrate as a protective cover, but the flexible substrate is prone to creases during the folding process. In the present application, the hard coating 054 is directly formed on the color filter layer 053, and the flexible substrate can be omitted, which is more conducive to improving the problem of the foldable display module 200 being prone to creases during the folding process.

[0071] It should also be noted that the inventors of this application have also innovatively discovered that, because the glass substrate serves as the rigid support substrate for the display main structure 04, it is rigid and less susceptible to internal deformation under external forces. Therefore, when the material of the hard coating 054 includes a cured optical adhesive layer, the stress generated during the curing process has minimal impact on the underlying film layers. In contrast, in some related technologies, when only a polyimide layer is used as the substrate, the polyimide layer is more susceptible to deformation under external forces. Consequently, when a hard coating 054 including a cured optical adhesive layer is formed on the polyimide layer, the stress generated during the curing process can affect the performance of some underlying film layers.

[0072] In other embodiments, the functional module 05 may include only one or two of the touch layer 052 , the color filter layer 053 , and the hard coating layer 054 . Alternatively, at least one of the touch layer 052 and the color filter layer 053 may be integrated into the display main structure 04 .

[0073] In this embodiment, since there is no adhesive layer on the light-emitting side and the back side of the light-emitting side of the display main structure 04, there is no optical adhesive layer and pressure-sensitive adhesive layer in the foldable display module, thereby improving the problems of poor bubbles, bumps and concave-convex points, and bonding marks caused by the bonding of the adhesive layer in the foldable display module, and realizing that the foldable display module 200 has slight creases or even no creases during the folding process, thereby improving the appearance of the foldable display module 200 and thus improving the user experience.

[0074] It is understandable that in other embodiments, only the light-emitting side of the display main structure 04 may be free of an optical adhesive layer, or the back side of the light-emitting side of the display main structure 04 may be free of a pressure-sensitive adhesive layer, so as to improve problems such as bubbles, bumps and concave / convex points, and bonding marks caused by the bonding of the adhesive layer in the foldable display module.

[0075] Please refer to Figure 3, which is a second cross-sectional schematic diagram of a foldable display module according to an embodiment of the present application. The foldable display module 200 shown in Figure 3 is substantially similar to the foldable display module 200 shown in Figure 2, and the similarities are not repeated here. The differences include that the foldable display module 200 shown in Figure 3 further includes an elastic buffer layer 06. The elastic buffer layer 06 is located on the side of the glass substrate 041 away from the display pixel layer 042, and the elastic buffer layer 06 is in direct contact with the surface of the glass substrate 041 away from the display pixel layer 042, so that there is no adhesive layer between the elastic buffer layer 06 and the glass substrate 041. The elastic properties of the elastic buffer layer 06 not only protect the glass substrate 041, but also improve the problem of folding marks on the foldable display module 200 caused by the adhesive layer.

[0076] In this embodiment, the elastic buffer layer 06 is located in the foldable area 200 a and the non-foldable area 200 b .

[0077] In this embodiment, the elastic buffer layer 06 overlaps with the display area of ​​the foldable display module 200 to protect the display area of ​​the foldable display module 200 .

[0078] It is understood that the elastic buffer layer 06 can also overlap the non-display area of ​​the foldable display module 200. The elastic buffer layer 06 is made of at least one of an adhesive and an elastic resin. The adhesive includes, but is not limited to, at least one of liquid optical clear resin (OCR) and solid optical adhesive. Liquid optical adhesives include, but are not limited to, epoxy resins, acrylate resins, and polyurethanes. Solid optical adhesives include, but are not limited to, polysiloxanes, epoxy resins, and polyurethanes. Elastic resins include, but are not limited to, silicone and thermoplastic polyurethanes.

[0079] In this embodiment, the elastic buffer layer 06 is made of an elastic resin to ensure good cushioning performance. Furthermore, the elastic buffer layer 06 made of the elastic resin has good resilience and is less susceptible to plastic deformation than optical adhesive layers and pressure-sensitive adhesive layers. This helps alleviate creases in the foldable display module caused by plastic deformation of the adhesive layer.

[0080] In other embodiments, the material of the elastic buffer layer 06 may also include an adhesive material, so that the elastic buffer layer 06 has both cushioning properties and adhesive properties. The adhesive property ensures better adhesion between the elastic buffer layer 06 and the glass substrate 041. During the folding process of the foldable display module 200, the elastic buffer layer 06 and the glass substrate 041 are less likely to delaminate, thereby extending the service life of the foldable display module 200. In addition, the adhesive property of the elastic buffer layer 06 can also reduce the risk of direct fracture of the glass substrate 041.

[0081] The thickness of the elastic buffer layer 06 is greater than or equal to 100 microns and less than or equal to 400 microns. For example, the thickness of the elastic buffer layer 06 can be 100 microns, 120 microns, 140 microns, 160 microns, 180 microns, 200 microns, 220 microns, 240 microns, 260 microns, 280 microns, 300 microns, 320 microns, 360 microns, 380 microns, or 400 microns.

[0082] It should be noted that unlike related art foldable display modules that use a foam layer as a buffer layer, this foam layer requires a pressure-sensitive adhesive layer to be attached to the back side of the flexible display panel. This results in the introduction of a pressure-sensitive adhesive layer, which increases the risk of creases in the foldable display module. Furthermore, unlike related art, the back side of the flexible substrate that supports the display main structure 04 has multiple support layers, including a backplane, a foam layer, and a metal support layer.

[0083] In this embodiment, the elastic buffer layer 06 is made of at least one of a glue material and an elastic resin. Both the glue material and the elastic resin can be formed into films through coating or other processes, eliminating the need for a glue layer, thereby reducing the number of glue layers in the foldable display module 200. Furthermore, the foldable display module 200 of this application comprises only the elastic buffer layer 06 below the glass substrate 041.

[0084] In this embodiment, when the elastic buffer layer 06 is made of an elastic resin, there is no adhesive layer on either the light-emitting side or the back side of the display main structure 04. When the elastic buffer layer 06 is made of an adhesive material, there is no adhesive layer on the light-emitting side of the display main structure 04, but there is an adhesive layer on the back side.

[0085] In other embodiments, in the foldable display module 200, the number of adhesive layers on the light-emitting side of the display main structure 04 is less than the number of adhesive layers on the back side of the light-emitting side of the display main structure 04, so as to reduce the number of adhesive layers on the light-emitting side of the foldable display module 200, which is beneficial to improving the crease problem of the foldable display module 200 caused by plastic deformation of the adhesive layer on the light-emitting side.

[0086] In this embodiment, the foldable display module 200 further includes a chip-on-film 091 , a flexible circuit board 092 , and an adhesive layer 093 .

[0087] In this embodiment, one end of the chip-on-film (CFO) 091 is bonded to the non-display area of ​​the display main structure 04, thereby connecting the CFO 091 to the display main structure 04. The CFO 091 is bent so that the other end of the CFO 091 is located on the side of the glass substrate 041 away from the display main structure 04. The CFO 091 includes a flexible substrate and a driver chip located on the flexible substrate.

[0088] In this embodiment, one end of flexible circuit board 092 is connected to the other end of chip-on-film 091. Adhesive layer 093 bonds the other end of flexible circuit board 092 to elastic buffer layer 06, thereby securing the other end of flexible circuit board 092 to elastic buffer layer 06. Flexible circuit board 092 includes a flexible substrate and a control chip located on the flexible substrate.

[0089] It should be noted that, unlike the related art, the back side of the light-emitting side of the foldable display module is a metal layer, a buffer layer and other film layers, and the flexible circuit board needs to be fixed on the metal layer and the buffer layer. In this application, the flexible circuit board is fixed on the elastic buffer layer 06.

[0090] In this embodiment, adhesive layer 093 is a reinforced double-sided adhesive tape. Adhesive layer 093 comprises a flexible substrate, a first adhesive layer, and a second adhesive layer, with the flexible substrate positioned between the first and second adhesive layers. The flexible substrate provides stiffness to adhesive layer 093 and is made of materials such as polyethylene terephthalate.

[0091] In this embodiment, the elastic buffer layer 06 overlaps with the chip-on-film 091 and the flexible circuit board 092 , so that the elastic buffer layer 06 also protects the chip-on-film 091 and the flexible circuit board 092 .

[0092] Please refer to Figure 4, which is a third cross-sectional schematic diagram of a foldable display module according to an embodiment of the present application. The foldable display module shown in Figure 4 is substantially similar to the foldable display module shown in Figure 3, and similarities are not repeated here. The differences include: one end of the chip-on-film (CFF) 091 is bound to the non-display area of ​​the display main structure 04, thereby connecting the CFF 091 to the display main structure 04; the CFF 091 is bent so that the other end of the CFF 091 is located on the side of the glass substrate 041 away from the display main structure 04; one end of the flexible circuit board 092 is connected to the other end of the CFF 091; the elastic buffer layer 06 further includes an opening 06a located in the non-foldable area 200b, which penetrates the elastic buffer layer 06 and exposes the glass substrate 041; the adhesive layer 093 is located in the opening 06a and bonds the other end of the flexible circuit board 092 to the glass substrate 041, thereby securing the other end of the flexible circuit board 092 to the glass substrate 041.

[0093] Since the adhesive layer 093 is located in the opening 06a of the elastic buffer layer 06 and bonds the other end of the flexible circuit board 092 to the glass substrate 041, the thickness of the adhesive layer 093 is thicker to ensure the adhesion of the adhesive layer 093 and ensure that the other end of the flexible circuit board 092 can be better fixed.

[0094] In this embodiment, the opening 06 a overlaps the COF 091 and the flexible printed circuit board 092 to reduce the bending diameter of the COF 091 and prevent the circuits on the COF 091 from being damaged due to excessive bending.

[0095] Please refer to Figure 5, which is a fourth cross-sectional schematic diagram of a foldable display module according to an embodiment of the present application. The foldable display module 200 shown in Figure 5 is substantially similar to the foldable display module 200 shown in Figure 3, and the similarities are not repeated here. The differences include that the foldable display module 200 shown in Figure 5 further includes a flexible substrate 07, which is positioned between the glass substrate 041 and the main display structure 04, and is in contact with both the glass substrate 041 and the main display structure 04.

[0096] Since the flexible substrate 07 is located between the glass substrate 041 and the display main structure 04 , the flexible substrate 07 flattens the surface of the glass substrate 041 , reducing the impact of impurities on the glass substrate 041 or defects in the glass substrate 041 on the display pixel layer 042 of the display main structure 04 .

[0097] Specifically, the flexible substrate 07 includes a first flexible substrate 071 , which is located between the glass substrate 041 and the display pixel layer 042 of the display main structure 04 , and the first flexible substrate 071 is in direct contact with the surface of the glass substrate 041 and the display pixel layer 042 .

[0098] The first flexible substrate 071 is yellow. The material of the first flexible substrate 071 includes, but is not limited to, polyimide. The thickness of the first flexible substrate 071 is greater than or equal to 8 micrometers and less than or equal to 10 micrometers.

[0099] For example, the thickness of the first flexible substrate 071 is 8.5 micrometers, 9 micrometers, 9.4 micrometers, 9.8 micrometers, or 10 micrometers.

[0100] It should be noted that the first flexible substrate 071 is formed on the aforementioned initial glass substrate (480 to 520 microns thick) through coating and other processes, ensuring good adhesion between the first flexible substrate 071 and the thinned glass substrate 041. Furthermore, other structures, such as the display main structure 04, are also formed on the first flexible substrate 071, and then the initial glass substrate is thinned to form the foldable display module 200.

[0101] Please refer to Figure 6, which is a fifth cross-sectional schematic diagram of a foldable display module according to an embodiment of the present application. The foldable display module 200 shown in Figure 6 is substantially similar to the foldable display module 200 shown in Figure 5, and the similarities are not repeated here. The differences include that the flexible substrate 07 of the foldable display module 200 shown in Figure 6 also includes a second flexible substrate 072. The second flexible substrate 072 is located between the display pixel layer 042 and the first flexible substrate 071, and the second flexible substrate 072 is in direct contact with both the first flexible substrate 071 and the display pixel layer 042. The material of the first flexible substrate 071 is the same as that of the second flexible substrate 072, and the thickness of the first flexible substrate 071 is greater than that of the second flexible substrate 072.

[0102] It should be noted that the second flexible substrate 072 also serves to isolate the first flexible substrate 071 from the display pixel layer 042 , thereby reducing the impact of the first flexible substrate 071 on the performance of devices in the display pixel layer 042 .

[0103] The second flexible substrate 072 is used as a flexible substrate and is a transparent polyimide layer.

[0104] The thickness of the second flexible substrate 072 is greater than or equal to 4.5 micrometers and less than or equal to 7.5 micrometers. For example, the thickness of the second flexible substrate 072 is 4.5 micrometers, 5.5 micrometers, 6.5 micrometers, and 7 micrometers.

[0105] Please refer to FIG7, which is a first cross-sectional view of another embodiment of the foldable display module of the present application. The foldable display module 200 shown in FIG7 is substantially similar to the foldable display module 200 shown in FIG2.

[0106] The similarities are not repeated here, and the differences include: the glass substrate 041 of the foldable display module 200 shown in FIG. 7 includes a groove 041 a , which is located in the foldable area 200 a , and the groove 041 a is arranged on the surface of the glass substrate 041 away from the display main structure 04 .

[0107] Since the glass substrate 041 includes a groove 041a, the groove 041a is located in the foldable area 200a. The groove 041a is arranged on the surface of the glass substrate 041 away from the display pixel layer 042, thereby further thinning the thickness of the portion of the glass substrate 041 corresponding to the foldable area 200a, thereby ensuring that the portion of the glass substrate 041 corresponding to the foldable area 200a is easier to fold.

[0108] In this embodiment, when the groove 041a is located in the foldable area 200a, the thickness H1 of the portion of the glass substrate 041 corresponding to the foldable area 200a is greater than 0 microns. In other words, the groove 041a penetrates the portion of the glass substrate 041 in the foldable area 200a, so that a portion of the glass substrate 041 is retained in the foldable area 200a, thereby protecting the display pixel layer 042 while providing rigid support for the display pixel layer 042. The characteristic of the glass substrate 041 not to undergo plastic deformation can also be used to improve the crease problem of the foldable display module 200 caused by the plastic deformation of the film layer.

[0109] Specifically, when the groove 041a is located in the foldable area 200a, the thickness of the portion of the glass substrate 041 corresponding to the foldable area 200a is greater than or equal to 10 microns, and the thickness of the portion of the glass substrate 041 corresponding to the foldable area 200a is less than 100 microns.

[0110] The cross-section of the groove 041a is rectangular, trapezoidal, or inverted trapezoidal in the thickness direction of the glass substrate 041. The cross-section of the groove 041a is rectangular in the direction perpendicular to the thickness of the glass substrate 041.

[0111] Specifically, the number of the groove 041 a is one. The cross-section of the groove 041 a is rectangular in the thickness direction of the glass substrate 041. The cross-section of the groove 041 a is rectangular in the direction perpendicular to the thickness of the glass substrate 041.

[0112] The sum of the depth S1 of the groove 041a and the thickness H1 of the portion of the glass substrate 041 corresponding to the foldable area 200a is equal to the thickness H2 of the portion of the glass substrate 041 corresponding to the non-foldable area 200b. The depth S1 of the groove 041a is greater than the thickness H1 of the portion of the glass substrate 041 corresponding to the foldable area 200a.

[0113] In this embodiment, the thickness H2 of the portion of the glass substrate 041 corresponding to the non-foldable area 200 b is greater than or equal to 10 microns and less than or equal to 600 microns, so as to ensure that the portion of the glass substrate 041 corresponding to the non-foldable area 200 b has good rigidity.

[0114] Specifically, the thickness H2 of the portion of the glass substrate 041 corresponding to the non-foldable region 200b is greater than or equal to 300 micrometers and less than or equal to 600 micrometers. For example, the thickness H2 of the portion of the glass substrate 041 corresponding to the non-foldable region 200b is 300 micrometers, 320 micrometers, 340 micrometers, 360 micrometers, 400 micrometers, 420 micrometers, 440 micrometers, 460 micrometers, 480 micrometers, 500 micrometers, 520 micrometers, or 600 micrometers.

[0115] It should be noted that this embodiment uses an initial glass substrate with a thickness of 480 microns to 520 microns as a substrate. After the display pixel layer 042, the thin film encapsulation layer 043 and the functional module 05 are prepared in sequence on the initial glass substrate, the surface of the initial glass substrate facing away from the display main structure 04 is locally thinned to form a groove 041a, and a glass substrate 041 is obtained.

[0116] In this embodiment, the groove 041a is formed by local thinning, and the roughness of the inner wall 041a1 of the groove 041a is greater than the roughness of the surface 041c of the glass substrate 041 close to the display main structure 04. The roughness of the inner wall 041a1 of the groove 041a is also greater than the roughness of the surface of the glass substrate 041 located in the non-folding area and away from the display main structure 04.

[0117] In this embodiment, the foldable display module 200 also includes an elastic filling layer 08, which is filled in the groove 041a. The filling thickness of the elastic filling layer 08 in the groove 041a is equal to the depth S1 of the groove 041a, so as to improve the flatness of the back of the display main structure 04 and make it more difficult for the elastic filling layer 08 to produce plastic deformation, thereby improving the crease problem caused by the plastic deformation of the film layer of the foldable display module 200.

[0118] The elastic filling layer 08 is made of at least one of an adhesive and an elastic resin to ensure good elasticity. The adhesive includes, but is not limited to, liquid optical clear resin (OCR) and solid optical adhesive. Liquid optical adhesives include, but are not limited to, epoxy resins, acrylate resins, and polyurethane. Solid optical adhesives include, but are not limited to, polysiloxane, epoxy resin, and polyurethane. Elastic resins include, but are not limited to, silicone and thermoplastic polyurethane.

[0119] In this embodiment, the elastic filling layer 08 is made of a glue material, which provides both elasticity and viscosity. This viscosity ensures better adhesion between the elastic filling layer 08 and the glass substrate 041. During the folding process, the elastic filling layer 08 and the glass substrate 041 are less likely to separate, thereby extending the service life of the foldable display module 200. Furthermore, the viscosity of the elastic filling layer 08 reduces the risk of fracture in the portion of the glass substrate 041 corresponding to the foldable region 200a. It also acts as a bonding agent when cracks occur in the portion of the glass substrate 041 corresponding to the foldable region 200a, preventing the cracks from spreading further.

[0120] In other embodiments, the material of the elastic filling layer 08 may also include elastic resin.

[0121] In this embodiment, the elastic buffer layer 06 is located on a side of the glass substrate 041 away from the display pixel layer 042 , and is in direct contact with the surface of the glass substrate 041 away from the display pixel layer 042 and the elastic filling layer 08 .

[0122] In this embodiment, the elastic buffer layer 06 is made of the same material as the elastic filling layer 08, and the elastic buffer layer 06 and the elastic filling layer 08 are integrally formed. This allows the elastic buffer layer 06 and the elastic filling layer 08 to be formed in a single process, simplifying the process of manufacturing the foldable display module 200 and reducing the risk of delamination between the elastic buffer layer 06 and the elastic filling layer 08. Specifically, the elastic buffer layer 06 and the elastic filling layer 08 are both made of elastic resin.

[0123] In other embodiments, the material of the elastic buffer layer 06 and the material of the elastic filling layer 08 may also be different. For example, the material of the elastic filling layer 08 includes a plastic material, and the material of the elastic buffer layer 06 includes an elastic resin. This allows the elastic filling layer 08 to perform a filling function while also reducing the risk of partial fracture of the foldable area 200a corresponding to the glass substrate 041. The buffering function of the elastic buffer layer 06 provides good protection for the glass substrate 041.

[0124] It is understandable that, in other embodiments, when the material of the elastic buffer layer 06 is different from the material of the elastic filling layer 08 , the material of the elastic buffer layer 06 may also include glue, and the material of the elastic filling layer 08 may include elastic resin.

[0125] In this embodiment, the glass substrate 041 is in direct contact with the display pixel layer 042 , and there is no flexible substrate between the glass substrate 041 and the display pixel layer 042 , which is beneficial for improving the crease problem of the foldable display module 200 caused by plastic deformation of the flexible substrate.

[0126] In this embodiment, the foldable display module 200 shown in FIG7 may further include a first flexible substrate 071, which is located between the glass substrate 041 and the display pixel layer 042, and is in direct contact with both the glass substrate 041 and the display pixel layer 042. For details about the first flexible substrate 071, reference may be made to FIG5 and its related description, which will not be repeated here. Alternatively, the foldable display module 200 shown in FIG7 may further include a first flexible substrate 071 and a second flexible substrate 072, which is located between the glass substrate 041 and the display pixel layer 042, and is in direct contact with the surface of the glass substrate 041. The second flexible substrate 072 is located between the display pixel layer 042 and the first flexible substrate 071, and is in direct contact with both the first flexible substrate 071 and the display pixel layer 042. For details about the first flexible substrate 071 and the second flexible substrate 072, reference may be made to FIG6 and its related description, which will not be repeated here.

[0127] Please refer to Figure 8, which is a second cross-sectional schematic diagram of another embodiment of the foldable display module of the present application. The foldable display module 200 shown in Figure 8 is substantially similar to the foldable display module 200 shown in Figure 7, and the similarities are not repeated here. The differences include that the groove 041a of the foldable display module 200 shown in Figure 8 penetrates the glass substrate 041 along the thickness direction of the glass substrate 041. In other words, the portion of the glass substrate 041 corresponding to the foldable region 200a is completely removed.

[0128] Since the portion of the glass substrate 041 corresponding to the foldable area 200 a is completely removed, it can be ensured that the portion of the foldable display module 200 corresponding to the foldable area 200 a has good foldability.

[0129] In this embodiment, the foldable display module 200 further includes a first flexible substrate 071, which is located between the glass substrate 041 and the display pixel layer 042. The first flexible substrate 071 is in direct contact with both the glass substrate 041 and the display pixel layer 042. This allows the first flexible substrate 071 to protect the display pixel layer 042 when the portion of the glass substrate 041 corresponding to the foldable area 200a is removed, thereby reducing the impact of the local thinning process on the display pixel layer 042.

[0130] In this embodiment, the foldable display module 200 shown in FIG8 may further include the second flexible substrate 072 shown in FIG6 . The second flexible substrate 072 is located between the first flexible substrate 071 and the display pixel layer 042 , and the second flexible substrate 072 is in contact with the first flexible substrate 071 and the display pixel layer 042 to further protect the display pixel layer 042 .

[0131] It should be noted that the foldable display module shown in Figures 2, 5, 6, 7 and 8 also includes the cover chip film 091, flexible circuit board 092 and adhesive layer 093 in Figures 5 and 6. The relevant design refers to Figures 5 and 6 and the corresponding description, which will not be repeated here.

[0132] It should also be noted that the compatible technical features in the above embodiments can be combined with each other arbitrarily.

[0133] 9 is a cross-sectional view of a foldable display device according to an embodiment of the present invention. The foldable display device 300 includes any of the foldable display modules 200 described above, a folding mechanism 30 , and adhesive. The foldable display module 200 is fixed to the folding mechanism 30 by adhesive.

[0134] The folding mechanism 30 includes a first support plate 301 and a second support plate 302. The first support plate 301 and the second support plate 302 are rotatably connected via a hinge mechanism (not shown).

[0135] The sealant includes a first sealant 401 and a second sealant 402. The first sealant 401 bonds the portion of the foldable display module 200 corresponding to one non-foldable area 200b to the first support plate 301, and the second sealant 402 bonds the portion of the foldable display module 200 corresponding to the other non-foldable area 200b to the second support plate 302.

[0136] Specifically, the first sealant 401 bonds the glass substrate 041 of one non-foldable area 200b to the first support plate 301, and the first sealant 401 contacts the glass substrate 041. The second sealant 402 bonds the glass substrate 041 of the other non-foldable area 200b to the second support plate 302, and the second sealant 402 contacts the glass substrate 041.

[0137] In this embodiment, the foldable display device 300 further includes an elastic buffer layer 06 , which overlaps with the non-foldable area 200 b and is located between the first support plate 301 and the glass substrate 041 and between the second support plate 302 and the glass substrate 041 .

[0138] Specifically, the elastic buffer layer 06 includes a first elastic buffer layer 061 and a second elastic buffer layer 062. The first elastic buffer layer 061 is fixed to the first support plate 301, the first elastic buffer layer 061 is located between the first support plate 301 and the glass substrate 041 and contacts the glass substrate 041, and the first sealant 401 is arranged around the first elastic buffer layer 061. The second elastic buffer layer 062 is fixed to the second support plate 302, the second elastic buffer layer 062 is located between the second support plate 302 and the glass substrate 041 and contacts the glass substrate 041, and the second sealant 402 is arranged around the second elastic buffer layer 062. In this embodiment, the elastic buffer layer 06 also includes a third elastic buffer layer 603 located outside the first sealant 401 and the second sealant 402. The third elastic buffer layer 603 is located between the first support plate 301 and the glass substrate 041, and / or, the third elastic buffer layer 603 is located between the second support plate 302 and the glass substrate 041. Specifically, the third elastic buffer layer 603 is located between the first support plate 301 and the glass substrate 041 .

[0139] The elastic buffer layer 06 includes a substrate and an elastic buffer film on the substrate. The surface of the substrate away from the elastic buffer film is sticky, and the sticky surface of the substrate is bonded to the first support plate 301 and the second support plate 302 .

[0140] It should be noted that the elastic buffer layer 06 is removed at the position where the first sealant 401 and the second sealant 402 are bonded to the glass substrate 041 , so as to better fix the foldable display module 200 on the folding mechanism 30 .

[0141] The description of the above embodiments is only used to help understand the technical solutions and core ideas of this application; ordinary technicians in this field should understand that they can still modify the technical solutions recorded in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein; and these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of this application.

Claims

1. A foldable display module, wherein: The foldable display module has a foldable area and a non-foldable area adjacent to the foldable area, and the foldable display module includes: Display the main structure; and A glass substrate is located on the back side of the light emitting surface of the display main structure, and the thickness of the portion of the glass substrate corresponding to the foldable area is less than or equal to 100 micrometers.

2. The foldable display module according to claim 1, wherein: The foldable display module further includes: The elastic buffer layer is located at a side of the glass substrate away from the display main structure and is in contact with a surface of the glass substrate away from the display main structure.

3. The foldable display module according to claim 2, wherein: The glass substrate comprises: The groove is located in the foldable area and is arranged on the surface of the glass substrate away from the display main structure.

4. The foldable display module according to claim 3, wherein: The roughness of the inner wall of the groove is greater than the roughness of the surface of the glass substrate close to the display main structure; The thickness of the portion of the glass substrate corresponding to the non-foldable area is greater than or equal to 300 micrometers and less than or equal to 600 micrometers; The foldable display module further includes: The elastic filling layer is filled in the groove.

5. The foldable display module according to claim 4, wherein: The material of the elastic filling layer is the same as that of the elastic buffer layer.

6. The foldable display module according to claim 5, wherein: The material of the elastic buffer layer includes elastic resin, and the material of the elastic filling layer includes at least one of a glue material and an elastic resin.

7. The foldable display module according to claim 1, wherein: There is no glue layer between the display main structure and the glass substrate.

8. The foldable display module according to claim 1, wherein: The thickness of a portion of the glass substrate corresponding to the foldable area is equal to the thickness of a portion of the glass substrate corresponding to the non-foldable area.

9. The foldable display module according to claim 1, wherein: In the thickness direction of the glass substrate, the roughness of a surface of the glass substrate away from the display main structure is greater than the roughness of a surface of the glass substrate close to the display main structure.

10. The foldable display module according to claim 1, wherein: The thickness of the portion of the glass substrate corresponding to the foldable area is greater than 10 micrometers.

11. The foldable display module according to claim 1, wherein: The foldable display module further includes: The flexible substrate is located between the glass substrate and the display main structure, and is in contact with the glass substrate and the display main structure.

12. The foldable display module according to claim 1, wherein: The glass substrate is in contact with the display main structure.

13. The foldable display module according to claim 1, wherein: The display main structure comprises: A display pixel layer, located on one side of the glass substrate; and The thin film encapsulation layer is located on a side of the display pixel layer away from the glass substrate and covers the display pixel layer.

14. The foldable display module according to claim 1, wherein: The foldable display module further includes: The functional module is located on a surface of the display main structure away from the glass substrate and includes at least two stacked functional layers, and any two adjacent functional layers are in contact with each other.

15. The foldable display module according to claim 14, wherein: The functional modules include: A touch layer, located on a surface of the display main structure away from the glass substrate; A color filter layer is located on the surface of the touch layer away from the display main structure; and The hard coating layer is located on the surface of the color filter layer away from the touch layer.

16. The foldable display module according to claim 2, wherein: The foldable display module further includes: A chip-on-chip film, one end of which is connected to the display main structure, and the chip-on-chip film is bent so that the other end of the chip-on-chip film is located on a side of the glass substrate away from the display main structure; A flexible circuit board, one end of which is connected to the other end of the chip-on-film; and The bonding layer bonds the other end of the flexible circuit board to the elastic buffer layer.

17. The foldable display module according to claim 2, wherein: The elastic buffer layer further comprises an opening located in the non-foldable area, wherein the opening penetrates the elastic buffer layer and exposes the glass substrate; The foldable display module further includes: A chip-on-chip film, one end of which is connected to the display main structure, and the chip-on-chip film is bent so that the other end of the chip-on-chip film is located on a side of the glass substrate away from the display main structure; A flexible circuit board, one end of which is connected to the other end of the chip-on-film; and The bonding layer is located in the opening and bonds the other end of the flexible circuit board to the glass substrate.

18. A foldable display device, wherein: The foldable display device comprises: The foldable display module as claimed in claim 1.

19. The foldable display device according to claim 18, wherein: The two non-foldable areas are adjacent to two opposite sides of one foldable area, and the foldable display device further includes: a first support plate; and A second support plate, rotatably connected to the first support plate; A first sealant is used to bond the glass substrate in the non-foldable area to the first support plate; and The second frame glue is used to bond the glass substrate in the other non-foldable area to the second supporting plate.

20. The foldable display device according to claim 19, wherein: The foldable display device further comprises: The elastic buffer layer overlaps the non-foldable area and is located between the first support plate and the glass substrate and between the second support plate and the glass substrate.

Citation Information

Patent Citations

  • Display module, fabrication method thereof and display device

    CN108807474A

  • Display panel and display device

    CN111081742A

  • Flexible display panel, display device and preparation method of display device

    CN111276518A

  • Display panel and display device

    CN111986575A

  • Flexible display panel

    CN113889512A