Defect detection method and apparatus for composite insulator, and electronic device and storage medium

By calculating the peak-to-peak value and attenuation coefficient of the composite insulator detection area, we can accurately determine whether there are defects in the composite insulator, solve the problem of poor defect detection accuracy in the existing technology, and achieve the accurate determination and traceability analysis of composite insulator defects.

WO2024221888A1PCT designated stage expired Publication Date: 2024-10-31JIEYANG POWER SUPPLY BUREAU GUANGDONG POWER GRID CO LTD

Patent Information

Application Number
PCT/CN2023/133889
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-04-26
Filing Date
2023-11-24
Publication Date
2024-10-31

AI Technical Summary

Technical Problem

Existing composite insulator defect detection methods rely on defect echo signals, making it difficult to accurately determine the existence of defects. In addition, the attenuation and dispersion characteristics of ultrasonic waves in ultrasonic diagnostic technology are obvious, making it impossible to obtain defect signals and perform traceability analysis.

Method used

By determining the first peak value and the second peak value of the target detection area, calculate the detection attenuation coefficient, and compare it with the calibrated attenuation coefficient to determine whether there is a defect in the target detection area, and then accurately determine the defect type and service life.

Benefits of technology

It achieves the accurate determination of defects in composite insulators, solves the problem of relying on defect echo signals, improves the accuracy and reliability of detection, and can accurately determine defect types and service life.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN2023133889_31102024_PF_FP_ABST
    Figure CN2023133889_31102024_PF_FP_ABST
Patent Text Reader

Abstract

A defect detection method and apparatus for a composite insulator, and an electronic device and a storage medium. The method comprises: determining a target detection area of a target composite insulator, and collecting a first peak-to-peak value which is output from a target point on a first end of the target detection area and a second peak-to-peak value which is output from a calibration point on a second end (S110); determining a detection attenuation coefficient on the basis of the first peak-to-peak value and the second peak-to-peak value (S120); and on the basis of a result of comparison between the detection attenuation coefficient and a calibration attenuation coefficient, determining whether there is a defect in the target detection area (S130).
Need to check novelty before this filing date? Find Prior Art

Description

Composite insulator defect detection method, device, electronic device and storage medium

[0001] This application claims priority to the Chinese patent application filed with the China Patent Office on April 26, 2023, with application number 202310458488.1. The entire contents of the above application are incorporated herein by reference. Technical Field

[0002] The present application relates to the field of nondestructive testing technology, for example, to a composite insulator defect detection method, device, electronic device and storage medium. Background Art

[0003] As an important electrical insulation device in the transmission network, insulators play a vital role in ensuring the safe and stable operation of the power system. While achieving safe isolation of transmission lines, insulators also provide mechanical support for transmission line nodes and need to be able to operate safely and reliably under complex working conditions. Unlike traditional glass and porcelain insulators, composite insulators are made mainly of polymers such as rubber and fiberglass, and are widely used due to their excellent anti-pollution flashover performance. Composite insulators have advantages such as high mechanical strength and high environmental tolerance. However, due to long-term operation in wet, acidic, polluted, and electrical environments, defects and failures will inevitably occur, directly affecting the safety and reliability of transmission lines. Therefore, quality inspection of composite insulators is a necessary prerequisite for ensuring their safe operation.

[0004] Common methods for composite insulator defect detection include thermal imaging, radiographic testing, magnetic particle testing, and ultrasonic testing. Thermal imaging can only provide a preliminary estimate of the potential presence of defects, and field operations often require secondary testing to assess and trace defects. Radiographic testing primarily uses spectrum scanning to observe details within the composite insulator material for defect diagnosis, but this method requires precise testing equipment, making it difficult to use portable equipment for field operations. Similar to radiographic testing, magnetic particle testing often requires specialized laboratories and is not suitable for online testing in field operations. Ultrasonic testing has rapidly developed in recent years, but due to the unique layered structure of composite insulators and the unique material characteristics, the ultrasonic attenuation and dispersion characteristics of ultrasonic diagnostic technology are relatively significant. This can make it impossible to obtain defect signals during defect diagnosis and to perform traceability analysis of defect signals. Therefore, it is crucial to accurately determine the presence of defects based on ultrasonic testing to identify potential defects.

[0005] Summary of the Invention

[0006] The present application provides a composite insulator defect detection method, device, electronic device and storage medium to solve the problem of over-reliance on defect echo signals and achieve accurate determination of defects.

[0007] The present application provides a composite insulator defect detection method, the method comprising:

[0008] Determine a target detection area for a target composite insulator, and collect a first peak-to-peak value outputted by a target point at a first end of the target detection area and a second peak-to-peak value outputted by a calibration point at a second end; wherein the target detection area is determined based on a calibration detection distance, the calibration detection distance being the distance from a target point at a first end of a reference composite insulator to a target point at a second end, the target point being the center point of a longitudinal cross-section of the composite insulator, the calibration point being a position point obtained by mapping a position of a reference calibration point on a longitudinal cross-section of the second end of the reference composite insulator to the longitudinal cross-section of the second end of the target detection area, and the reference composite insulator being an unused composite insulator;

[0009] Determining a detection attenuation coefficient based on the first peak-to-peak value and the second peak-to-peak value; wherein the first peak-to-peak value includes a first longitudinal mode peak-to-peak value and a first torsional mode peak-to-peak value, the second peak-to-peak value includes a second longitudinal mode peak-to-peak value and a second torsional mode peak-to-peak value, and the detection attenuation coefficient includes a longitudinal mode detection attenuation coefficient and a torsional mode detection attenuation coefficient;

[0010] Based on the comparison result of the detection attenuation coefficient and the calibration attenuation coefficient, it is determined whether there is a defect in the target detection area.

[0011] The present application provides a composite insulator defect detection device, which includes:

[0012] a peak-to-peak value determination module configured to determine a target detection area of ​​a target composite insulator, and collect a first peak-to-peak value outputted by a target point at a first end of the target detection area and a second peak-to-peak value outputted by a calibration point at a second end; wherein the target detection area is determined based on a calibration detection distance, the calibration detection distance being the distance from a target point at a first end of a reference composite insulator to a target point at a second end, the target point being the center point of a longitudinal cross-section of the composite insulator, the calibration point being a position point obtained by mapping a position of a reference calibration point on a longitudinal cross-section at a second end of the reference composite insulator to the longitudinal cross-section at the second end of the target detection area, and the reference composite insulator being an unused composite insulator;

[0013] an attenuation coefficient determination module, configured to determine a detection attenuation coefficient based on the first peak-to-peak value and the second peak-to-peak value; wherein the first peak-to-peak value includes a first longitudinal mode peak-to-peak value and a first torsional mode peak-to-peak value, the second peak-to-peak value includes a second longitudinal mode peak-to-peak value and a second torsional mode peak-to-peak value, and the detection attenuation coefficient includes a longitudinal mode detection attenuation coefficient and a torsional mode detection attenuation coefficient;

[0014] The defect detection module is configured to determine whether there is a defect in the target detection area based on a comparison result of the detection attenuation coefficient and the calibration attenuation coefficient.

[0015] The present application provides an electronic device, comprising:

[0016] at least one processor; and

[0017] a memory communicatively coupled to the at least one processor;

[0018] The memory stores a computer program that can be executed by the at least one processor, and the computer program is executed by the at least one processor so that the at least one processor can execute the composite insulator defect detection method described in any embodiment of the present application.

[0019] The present application provides a computer-readable storage medium storing computer instructions, wherein the computer instructions are used to enable a processor to implement the composite insulator defect detection method described in any embodiment of the present application when executed.

[0020] It should be understood that the content described in this section is not intended to identify key or important features of the embodiments of the present application, nor is it intended to limit the scope of the present application. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] The following is a brief introduction to the drawings required for describing the embodiments.

[0022] FIG1 is a flow chart of a composite insulator defect detection method provided by an embodiment of the present application;

[0023] FIG2a is a schematic diagram of the structure of a composite insulator applicable to an embodiment of the present application and a schematic diagram of the structure of mapping at both ends of the composite insulator;

[0024] FIG2 b is a schematic diagram of a longitudinal cross-section of a first end of a composite insulator applicable to an embodiment of the present application;

[0025] FIG2 c is a schematic diagram of a longitudinal cross-section of a second end of a composite insulator applicable to an embodiment of the present application;

[0026] FIG3 is a flow chart of another composite insulator defect detection method provided in an embodiment of the present application;

[0027] FIG4 is a schematic structural diagram of a composite insulator defect detection device provided in an embodiment of the present application;

[0028] FIG5 is a schematic structural diagram of an electronic device for implementing the composite insulator defect detection method according to an embodiment of the present application. DETAILED DESCRIPTION

[0029] The technical solutions in the embodiments of the present application will be described below in conjunction with the drawings in the embodiments of the present application. The described embodiments are only part of the embodiments of the present application, rather than all the embodiments.

[0030] The terms "first", "second", "third", "fourth", "fifth" and the like in the specification and claims of the present application and the above-mentioned drawings are used to distinguish similar objects and are not necessarily used to describe a specific order or sequential order. It should be understood that the data used in this way can be interchangeable where appropriate, so that the embodiments of the present application described herein can be implemented in a sequence other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, in addition to the processes, methods, systems, products or devices that include a series of steps or units shown in the embodiments of the present application, other processes, methods, systems, products or devices that do not clearly list these series of steps or units, or other steps or units inherent to these processes, methods, systems, products or devices, may also be included.

[0031] Example 1

[0032] FIG1 is a flow chart of a composite insulator defect detection method provided by an embodiment of the present application. This embodiment is applicable to detecting defects in composite insulators. The method can be performed by a composite insulator defect detection device. The composite insulator defect detection device can be implemented in the form of hardware and / or software. The composite insulator defect detection device can be configured in an electronic device having the composite insulator defect detection method. As shown in FIG1 , the method includes:

[0033] S110 , determining a target detection area of ​​a target composite insulator, collecting a first peak-to-peak value outputted by a target point at a first end of the target detection area and a second peak-to-peak value outputted by a calibration point at a second end thereof.

[0034] The target detection area is determined based on the calibrated detection distance, which is the distance from a target point at the first end of the reference composite insulator to a target point at the second end. For example, if any of points b1, b2, and b3 in Figure 2a is used as the reference calibration point, then the distance from point a to point b is the calibrated detection distance. The target point is the center point of the longitudinal cross-section of the composite insulator, such as points a and b in Figure 2a. The calibration point is the position of the reference calibration point on the longitudinal cross-section of the second end of the reference composite insulator mapped to the longitudinal cross-section of the second end of the target detection area. The reference composite insulator is an unused composite insulator.

[0035] This application uses an ultrasonic excitation sensor A and an ultrasonic receiving sensor B to collect information. The ultrasonic excitation sensor A and the ultrasonic receiving sensor B use piezoelectric transducers of the same structure and size so that the signal types received at both ends are similar. The ultrasonic excitation sensor A is set at the first end of the composite insulator, such as the upper end of the detection point a in Figure 2b, and is used to generate the ultrasonic signal Aa required by this application. The ultrasonic receiving sensor B is set at the second end of the composite insulator, such as the upper end of the detection point b in Figure 2c, and is used to receive the ultrasonic signal B transmitted to point b. b . The ultrasonic excitation sensor A, the ultrasonic receiving sensor B and the outer surface of the composite insulator are matched with an arc surface, and the angle θ of the sensor arc surface structure ranges from 60 to 120° (as shown in Figure 2b). The ultrasonic excitation sensor A can generate the ultrasonic guided wave longitudinal mode L(0, 2) mode and the torsional mode T(0, 2) mode. This application uses the L(0, 2) mode and the T(0, 2) mode to evaluate the defects and hidden dangers of composite insulators, and the center frequency of the ultrasonic guided wave signal generated by the ultrasonic excitation sensor A can be set between 10-50kHz, and the number of cycles of the ultrasonic guided wave signal can be set to 10.

[0036] According to the calibration detection distance calibrated in advance, a detection area is selected on the target composite insulator as the target detection area so that the appropriate signal can be received. That is, the ultrasonic excitation sensor A is used to collect the first peak-to-peak value output by the target point at the first end of the target detection area, and the ultrasonic receiving sensor B is used to collect the second peak-to-peak value output by the calibration point at the second end of the target detection area.

[0037] In a feasible embodiment, optionally, in order to accurately determine the target detection area of ​​the target composite insulator, it is necessary to accurately determine the reference calibration point and the calibration detection distance. The following describes the process of determining the reference calibration point and the calibration detection distance, including steps A1-A5:

[0038] Step A1, determining the third peak-to-peak value of the target point at the first end of the reference composite insulator and the fourth peak-to-peak value of each detection point at the second end; wherein the spatial phases of the detection points differ from each other by a preset angle, and the detection points are on the circumference of the longitudinal cross-section of the second end.

[0039] When the distance between the target point at the first end of the reference composite insulator and the target point at the second end is selected for the first time, that is, the current detection distance l, can be determined according to a multiple n of the minimum periodic shed length l1, for example, according to l = n * l1 (n is 8-10), and then the third peak-to-peak value of the target point at the first end of the reference composite insulator and the fourth peak-to-peak value of each detection point at the second end are collected, where the detection points are points b1, b2 and b3 in Figure 2c.

[0040] Step A2: Compare the maximum peak-to-peak value among the fourth peak-to-peak values ​​of each detection point with a reference peak-to-peak value, where the reference peak-to-peak value is the product of a preset coefficient and the third peak-to-peak value. The preset coefficient can be determined based on actual conditions, such as any value between 0.6 and 0.8.

[0041] Step A3: If the maximum peak-to-peak value is greater than or equal to the reference peak-to-peak value, the detection point corresponding to the maximum peak-to-peak value is used as the reference calibration point, and the current detection distance is used as the calibration detection distance, where the current detection distance is the distance from the target point at the first end to the target point at the second end of the reference composite insulator.

[0042] Step A4: If the maximum peak-to-peak value is less than the reference peak-to-peak value, the current detection distance is shortened according to the preset reduction distance to determine the third peak-to-peak value of the target point at the first end of the reference composite insulator and the fourth peak-to-peak value of each detection point at the second end next time to determine the reference calibration point and the calibration detection distance.

[0043] The preset reduction distance can be determined according to actual conditions, that is, the position of the second end can be moved to shorten the current detection distance, and the reduced detection distance is used as the current detection distance again. The third peak-to-peak value and the fourth peak-to-peak value of each detection point are continued to be collected, and the maximum peak-to-peak value of the fourth peak-to-peak value of each detection point is compared with the reference peak-to-peak value until the calibrated detection distance is determined.

[0044] Step A5: If the current detection distance is equal to or less than the preset distance, and the maximum peak-to-peak value is less than the reference peak-to-peak value, the detection point corresponding to the maximum peak-to-peak value output at the preset distance is used as the reference calibration point, and the preset distance is used as the calibration detection distance. The preset distance is set based on actual conditions, for example, 0.4 meters.

[0045] Because the ultrasonic excitation sensor A can generate the ultrasonic guided wave longitudinal mode L(0, 2) mode and the torsional mode T(0, 2) mode, when calibrating the reference calibration point and the calibration detection distance, it will also be divided into the reference calibration point and calibration detection distance under the L mode and the T mode. However, because in the actual process, the difference between the reference calibration point and the calibration detection distance of the two modes is very small, the reference calibration point and calibration detection distance of one mode will be selected as the final reference calibration point and calibration detection distance, or the reference calibration point and calibration detection distance in the middle of the two modes will be selected as the final reference calibration point and calibration detection distance.

[0046] The technical solution of this embodiment selects the detection point corresponding to the maximum peak-to-peak value among the fourth peak-to-peak values ​​of each detection point as the reference calibration point to ensure the integrity of the signal, and then compares the maximum peak-to-peak value among the fourth peak-to-peak values ​​of each detection point with the reference peak-to-peak value. Based on the comparison results, the reference calibration point and the calibration detection distance are prepared to be selected, thereby achieving accurate determination of the reference calibration point and the calibration detection distance, thereby making the subsequent determination of the target detection area of ​​the target composite insulator based on the calibration detection distance more accurate, and making the signal collected from the reference calibration point more representative, so that the collected signal can be used more accurately for defect detection.

[0047] S120. Determine a detection attenuation coefficient based on the first peak-to-peak value and the second peak-to-peak value.

[0048] Because the ultrasonic excitation sensor A can generate the ultrasonic guided wave longitudinal mode L(0, 2) mode and the torsional mode T(0, 2) mode, the collected first peak-to-peak value includes the first longitudinal mode peak-to-peak value and the first torsional mode peak-to-peak value, the second peak-to-peak value includes the second longitudinal mode peak-to-peak value and the second torsional mode peak-to-peak value, and the detection attenuation coefficient includes the longitudinal mode detection attenuation coefficient and the torsional mode detection attenuation coefficient.

[0049] Based on the first peak-to-peak value and the second peak-to-peak value, the process of determining the detection attenuation coefficient can be as follows: the peak-to-peak value of the second longitudinal mode U Lb The peak-to-peak value of the first longitudinal mode U La The difference between the peak-to-peak value of the first longitudinal mode U La The ratio of the product of the calibrated detection distance l is taken as the longitudinal modal detection attenuation coefficient X L , which can be expressed as: X L =(U Lb -U La ) / (U La *l); the peak-to-peak value of the second torsional mode U Tb The peak-to-peak value of the first torsional mode U Ta The difference between the peak-to-peak value of the first torsional mode U Ta The ratio of the product of the calibrated detection distance l is taken as the torsional mode detection attenuation coefficient X T , which can be expressed as: X T =(U Tb -U Ta ) / (U Ta *l).

[0050] S130 : Determine whether there is a defect in the target detection area based on a comparison result of the detection attenuation coefficient and the calibration attenuation coefficient.

[0051] The calibration attenuation coefficient includes the longitudinal modal calibration detection attenuation coefficient and the torsional modal calibration detection attenuation coefficient.

[0052] The defect types of the composite insulators of the present application include core rod aging type, sheath debonding type and air hole / bubble type. Based on the comparison results of the detection attenuation coefficient and the calibrated attenuation coefficient, it can be accurately determined whether the target detection area has defects, may have defects or does not have defects, and then specific analysis can be performed on different situations to accurately determine the defect type in the target detection area, or to evaluate the service life of the target detection area.

[0053] Optionally, the process of determining the calibration attenuation coefficient includes steps B1-B5:

[0054] Step B1: Determine a preset number of candidate attenuation coefficients; wherein the preset number is determined based on a calibrated detection distance and a minimum periodic shed length.

[0055] After the calibration detection distance is determined, the number of candidate attenuation coefficients collected can be determined by the ratio of the calibration detection distance l and the minimum periodic shed length l1, that is, the preset number N. Then, by collecting the peak-to-peak values ​​of the first and second ends corresponding to the N nodes on the reference composite insulator, the candidate attenuation coefficients x[x1, x2, ...x N ], can be expressed as follows: x N =(U bN -U a ) / [U a *N*(l / l1)]

[0056] Step B2: determining an attenuation coefficient average, an attenuation coefficient average error, and an attenuation coefficient root mean square error based on the candidate attenuation coefficients.

[0057] Based on the candidate attenuation coefficients, the formulas for solving the attenuation coefficient average value X1, the attenuation coefficient average error X2, and the attenuation coefficient root mean square error X3 can be expressed as follows:

[0058] Step B3, determine whether the first parameter and the second parameter meet the first preset condition; wherein, the first parameter is the ratio of the average error of the attenuation coefficient to the average value of the attenuation coefficient, that is, X2 / X1, and the second parameter is the ratio of the root mean square error of the attenuation coefficient to the average value of the attenuation coefficient, that is, X3 / X1, and the first preset condition is that the first parameter is greater than the preset error value and the second parameter is greater than the preset error value; wherein, the preset error value can be determined according to actual conditions, such as being set to 0.25.

[0059] Step B4: If the first preset condition is met, the average value of the attenuation coefficient is used as the calibration attenuation coefficient.

[0060] Step B5: If the first preset condition is not met, a calibrated attenuation coefficient is determined according to an attenuation coefficient equation and a calibrated detection distance, wherein the attenuation coefficient equation is determined according to the candidate attenuation coefficient.

[0061] For example, the equation x can be calculated based on the candidate attenuation coefficients N =exp(-α*N*l1) for fitting, so as to determine the accurate α value and obtain the attenuation coefficient equation x=exp(-α*l). Then, the calibration detection distance l is input to obtain the calibration attenuation coefficient.

[0062] In this solution, a preset number of candidate attenuation coefficients are determined to calculate the candidate attenuation coefficients to determine the average value of the attenuation coefficient, the average error of the attenuation coefficient and the root mean square error of the attenuation coefficient. Then, by comparing whether the first parameter and the second parameter meet the first preset condition, a calibrated attenuation coefficient suitable for this application is accurately obtained, so as to facilitate subsequent comparison with the detection attenuation coefficient, thereby accurately detecting defects.

[0063] The technical solution of the embodiment of the present application determines the target detection area of ​​the target composite insulator, collects the first peak-to-peak value output by the target point at the first end of the target detection area and the second peak-to-peak value output by the calibration point at the second end; determines the detection attenuation coefficient based on the first peak-to-peak value and the second peak-to-peak value; and determines whether there is a defect in the target detection area based on the comparison result of the detection attenuation coefficient and the calibration attenuation coefficient. The technical solution of the present application accurately derives the detection attenuation coefficient by determining the first peak-to-peak value and the second peak-to-peak value, and then accurately determines whether there is a defect in the target detection area by comparing the detection attenuation coefficient with the calibration attenuation coefficient, thereby solving the problem of over-reliance on defect echo signals and achieving accurate determination of defects.

[0064] Example 2

[0065] FIG3 is a flow chart of another composite insulator defect detection method provided in an embodiment of the present application. This embodiment further describes S130 in the above embodiment. As shown in FIG3 , the method includes:

[0066] S210. Determine a target detection area of ​​a target composite insulator, collect a first peak-to-peak value outputted by a target point at a first end of the target detection area and a second peak-to-peak value outputted by a calibration point at a second end, and determine a detection attenuation coefficient based on the first peak-to-peak value and the second peak-to-peak value.

[0067] S220: Based on the detected attenuation coefficient and the calibrated attenuation coefficient, determine whether the relationship between the detected attenuation coefficient and the calibrated attenuation coefficient meets a second preset condition and / or a third preset condition.

[0068] The second preset condition is that the longitudinal modal detection attenuation coefficient is less than the first preset multiple of the longitudinal modal calibration detection attenuation coefficient, and the third preset condition is that the torsional modal detection attenuation coefficient is less than the first preset multiple of the torsional modal calibration detection attenuation coefficient; wherein, the first preset multiple can be determined according to actual conditions, such as it can be set to 2.

[0069] S230: If both the second preset condition and the third preset condition are satisfied, determine that there is no defect in the target detection area.

[0070] When the second preset condition and the third preset condition are met at the same time, it is determined that there is no defect in the target detection area. Then, the longitudinal modal group velocity and the torsional modal group velocity can be determined based on the first center time output by the target point at the first end of the target detection area and the second center time output by the calibration point at the second end, as well as the calibrated detection distance. The minimum value of the longitudinal modal group velocity and the torsional modal group velocity is selected as the target group velocity. Then, according to the calibrated elastic modulus E and the group velocity C p The elastic modulus is calculated by the relationship between the two, and the service life is predicted and outputted by combining the accelerated aging fitting curve E(t), so as to accurately determine the service life of the target detection area of ​​the composite insulator. Among them, the elastic modulus E and the group velocity C p The relationship between can be expressed as:

[0071] Among them, μ is Poisson's ratio, ρ is material density, both are equivalent values ​​under the original value E0, and C is the calibration coefficient.

[0072] S240: If both the second preset condition and the third preset condition are not satisfied, determine that there is a defect in the target detection area.

[0073] If both the second preset condition and the third preset condition are not satisfied, it is determined that a defect exists in the target inspection area, and then it is necessary to analyze what type of defect it is.

[0074] Optionally, after determining that a defect exists in the target detection area, determining the defect type of the target detection area includes steps C1-C7:

[0075] Step C1: Determine a first center time output by a target point at a first end of the target detection area and a second center time output by a calibration point at a second end.

[0076] Step C2: determining a target elastic modulus based on the first center time, the second center time, and a relationship between the elastic modulus and the group velocity; wherein the target elastic modulus includes a longitudinal modal elastic modulus and a torsional modal elastic modulus.

[0077] The group velocity is determined based on the first center time, the second center time, and the calibrated detection distance, and then the group velocity is input into a relationship between the elastic modulus and the group velocity, thereby accurately determining the target elastic modulus.

[0078] Step C3: determining a target debonding angle based on the second peak-to-peak value and a first calibration equation; wherein the target debonding angle includes a longitudinal modal debonding angle and a torsional modal debonding angle, and the first calibration equation represents the relationship between the debonding length and the peak-to-peak value.

[0079] The first calibration relationship can be expressed as: U b ′=U b *exp(-k1β)-k2*(0.5*l)

[0080] Among them, U b is the peak-to-peak value of the second-end signal when there is no debonding, k1 and k2 are the calibration correction parameters, and β is the debonding angle.

[0081] Step C4: determining a target pore depth based on the second peak-to-peak value and a second calibration equation; wherein the target pore depth includes a longitudinal modal pore depth and a torsional modal pore depth, and the second calibration equation represents a relationship between the pore depth and the peak-to-peak value.

[0082] The second calibration relationship can be expressed as: U b ″=U b *exp(-k3h)*exp[-k4(h-R2+R1)]

[0083] Among them, U b is the peak-to-peak value of the second-end signal when there is no air hole, k3 and k4 are calibrated correction parameters, and h is the depth from the surface to the inside of the composite insulator.

[0084] Step C5: normalize the target elastic modulus, the target degumming angle, and the target pore depth to determine the elastic modulus probability, the degumming angle probability, and the pore depth probability, wherein the sum of the elastic modulus probability, the degumming angle probability, and the pore depth probability is one.

[0085] Step C6: If a candidate probability greater than a preset probability value exists among the elastic modulus probability, the debonding angle probability, and the pore depth probability, the defect type corresponding to the candidate probability is determined as the target defect type. The preset probability is set according to actual conditions, for example, 0.6.

[0086] The defect types include core rod aging type, sheath debonding type and pore / bubble type; the core rod aging type is determined according to the elastic modulus probability, the sheath debonding type is determined according to the debonding angle probability, and the pore / bubble type is determined according to the pore depth probability.

[0087] Step C7: If there is no candidate probability greater than a preset probability value among the elastic modulus probability, the debonding angle probability, and the pore depth probability, the defect type of the target detection area is the core rod aging type, the sheath debonding type, and the pore / bubble type.

[0088] This technical solution accurately analyzes the specific defect type of the target inspection area of ​​the target composite insulator by comparing the elastic modulus probability, debonding angle probability and pore depth probability with the preset probability values, thereby tracing the defect and facilitating subsequent maintenance work by staff.

[0089] S250: If only any one of the second preset condition and the third preset condition is met, determine that there may be a defect in the target detection area.

[0090] When only one of the second preset condition and the third preset condition is met, it means that it is not possible to accurately determine whether there is a defect in the target detection area. In order to ensure accurate determination of the defect, further analysis is required to avoid misjudgment of the defect.

[0091] Optionally, after determining that a defect may exist in the target inspection area, further analysis of the defect detection may include steps D1-D4:

[0092] Step D1: determining the measured modal attenuation coefficient according to the second peak-to-peak value.

[0093] The ratio of the peak-to-peak value of the second longitudinal mode to the peak-to-peak value of the second torsional mode is taken as the measured modal attenuation coefficient.

[0094] Step D2: If the measured modal attenuation coefficient is greater than the calibrated modal attenuation coefficient of the second preset multiple, and the peak-to-peak value of the second torsional mode is less than the peak-to-peak value of the calibrated torsional mode of the third preset multiple, the defect type in the target detection area is the sheath debonding type.

[0095] The modal attenuation coefficient is calibrated after the reference calibration point and calibration detection distance are determined. The ratio of the longitudinal modal peak-to-peak value and the torsional modal peak-to-peak value outputted by the reference composite insulator at the reference calibration point is collected, and the calibration modal attenuation coefficient is calculated. The second and third preset multiples can be set based on actual conditions, for example, the second preset multiple can be set to 1.5 and the third preset multiple can be set to 0.5.

[0096] Step D3: If the measured modal attenuation coefficient is less than the calibrated modal attenuation coefficient of the fourth preset multiple, and the peak-to-peak value of the second longitudinal modal is less than the peak-to-peak value of the calibrated longitudinal modal attenuation coefficient of the third preset multiple, then the defect type in the target detection area is a pore / bubble type; wherein the fourth preset multiple can be set according to actual conditions, such as setting the fourth preset multiple to 0.5.

[0097] Step D4: If the measured modal attenuation coefficient is greater than the calibrated modal attenuation coefficient at a fourth preset multiple, and is less than the calibrated modal attenuation coefficient at a second preset multiple, and the target elastic modulus meets a fourth preset condition, then the defect type in the target inspection area is a core rod aging defect. The fourth preset condition is that the longitudinal modal elastic modulus is less than the original elastic modulus at a fifth preset multiple, and the torsional modulus is less than the original elastic modulus at a fifth preset multiple, where the original elastic modulus is the elastic modulus of the reference composite insulator. The fifth preset multiple can be set based on actual conditions, such as setting the fifth preset multiple to 0.9.

[0098] This technical solution compares the measured modal attenuation coefficient with the calibrated modal attenuation coefficient, and based on the comparison result, accurately determines whether there is a defect in the target detection area and the defect type when there may be a defect in the target detection area.

[0099] The technical solution of the embodiment of the present application determines the target detection area of ​​the target composite insulator, collects the first peak-to-peak value output by the target point at the first end of the target detection area and the second peak-to-peak value output by the calibration point at the second end, determines the detection attenuation coefficient based on the first peak-to-peak value and the second peak-to-peak value, and then analyzes whether the relationship between the detection attenuation coefficient and the calibration attenuation coefficient meets the second preset condition and / or the third preset condition, thereby accurately determining the possibility of defects in the target detection area, and further analyzing the defect type of the defect, solving the problem of over-reliance on defect echo signals, and achieving accurate determination of defects.

[0100] Example 3

[0101] This embodiment describes the determination of the relationship between the elastic modulus and the group velocity, the first calibration relationship, and the second calibration relationship.

[0102] Because the above relationship needs to be accurately determined by collecting data output from the designed defect samples, the process of making defect samples is described first. The process is as follows:

[0103] This application uses a new composite insulator to design and produce defect samples. Small-sized internal defects that are difficult to diagnose are selected to produce samples, and only one defect is produced in a single sample. The designed defect samples mainly include three types of samples: core rod aging, sheath debonding, and pores / bubbles in composite insulators.

[0104] Core rod aging samples of composite insulators are obtained through laboratory accelerated aging tests. The calculated elastic modulus E = σ / ε is selected as the observation index for evaluating the mechanical aging of the core rod, that is, the ratio of stress σ to strain ε. The value range of the calculated elastic modulus E in sample preparation is 0.7 to 1 times the original value E0, that is, samples with a core rod mechanical strength value range of (0.7 to 1) times E0 are obtained through aging tests, among which the sample data of (0.9 to 1) times E0 are not less than 30, and the sample data of (0.7 to 0.9) times E0 are not less than 10. During the preparation of the core rod aging samples, the relationship E(t) between the aging time and the calculated elastic modulus is recorded.

[0105] The sheath debonding sample is processed by the debonding process in the composite insulator sheath bonding. The debonding length in the axial direction is calibrated to 0.5*i*l1 (i=1, 2, 3, 4), and the debonding angle β in the radial direction ranges from 30 degrees to 120 degrees. No less than 10 debonding samples with different angles under a debonding length are prepared.

[0106] The pore / bubble samples are made by electro-corrosion punching, and electro-corrosion holes with a diameter of 2 mm are uniformly made. The number of samples with a defect sample depth h ranging from 0 to (R2-R1) (the defect hole is in the shed area) is not less than 20, and the number of samples with a defect sample depth h ranging from (R2-R1) to R2 (the defect hole is in the core rod area) is not less than 10. R1 is the core rod radius and R2 is the sheath radius.

[0107] After the defect samples are prepared, the sample characteristic quantities of the core rod aging sample, the sheath debonding sample, and the pore / bubble sample are calibrated respectively to determine the above relationship. The process is as follows:

[0108] The first end ultrasonic signal A is still collected during the experiment a [L / T, f, U a , t a ] and the second end ultrasonic signal B b [L / T, f, U b , t b ] is used to calibrate the sample feature quantity.

[0109] In the calibration of the mandrel aging sample, the mathematical relationship E(t) for calculating the elastic modulus attenuation is obtained by curve fitting. At the same time, The group velocity of each sample in L mode and T mode is calculated by Complete the equation fitting between elastic modulus and group velocity, where μ is Poisson's ratio and ρ is material density. Both are equivalent values ​​under the original value E0. C is the coefficient that needs to be calibrated. That is, C can be accurately determined by fitting. Once the group velocity result of a sample is obtained, the formula can be used. Calculate the corresponding elastic modulus E.

[0110] In the calibration of sheath debonding samples, the formula U b ′=U b *exp(-k1β)-k2*(0.5*i*l i ) to fit the axial debonding length 0.5*i*l1 and the radial debonding angle β, where U b is the peak-to-peak value of the signal at point b without debonding, k1 and k2 are the correction parameters that need to be fitted, that is, k1 and k2 can be accurately determined by fitting, thereby determining the first calibration relationship.

[0111] In the calibration of pore / bubble samples, the following formula is used to fit the peak-to-peak value of the signal at different depths from 0 to R2: U b ″=U b *exp(-k3h)*exp[-k4(h-R2+R1)]

[0112] Among them, exp(-k3h) is the fitting of the peak-to-peak attenuation at a depth of 0 to (R2-R1) in the sheath area, and exp[-k4(h-R2+R1)] is the fitting of the peak-to-peak attenuation at a depth of (R2-R1) to R2 in the core rod area. When the depth is 0 to (R2-R1), k4=0. By fitting, k3 and k4 can be accurately determined, thereby accurately determining the second calibration relationship.

[0113] After the defect sample is produced, this technical solution accurately determines the characteristic parameters of various samples by collecting the ultrasonic signals output by the defect sample, analyzing the output ultrasonic signals, and fitting them in combination with formulas, thereby accurately determining the relationship between the elastic modulus and the group velocity, the first calibration relationship, and the second calibration relationship, so as to facilitate subsequent use in defect detection and make the determination of defects more accurate.

[0114] Example 4

[0115] Figure 4 is a schematic diagram of the structure of a composite insulator defect detection device provided by an embodiment of the present application. As shown in Figure 4, the device includes: a peak-to-peak value determination module 310, configured to determine a target detection area of ​​a target composite insulator, collect a first peak-to-peak value outputted by a target point at a first end of the target detection area, and a second peak-to-peak value outputted by a calibration point at a second end; wherein the target detection area is determined based on a calibration detection distance, which is the distance from the target point at the first end of the reference composite insulator to the target point at the second end. The target point is the center point of the longitudinal section of the composite insulator, and the calibration point is a position point obtained by mapping the position of the reference calibration point on the longitudinal section of the second end of the reference composite insulator to the longitudinal section of the second end of the target detection area, and the reference composite insulator is an unused composite insulator; the attenuation coefficient determination module 320 is configured to determine the detection attenuation coefficient based on the first peak-to-peak value and the second peak-to-peak value; wherein the first peak-to-peak value includes the first longitudinal mode peak-to-peak value and the first torsional mode peak-to-peak value, the second peak-to-peak value includes the second longitudinal mode peak-to-peak value and the second torsional mode peak-to-peak value, and the detection attenuation coefficient includes the longitudinal mode detection attenuation coefficient and the torsional mode detection attenuation coefficient; the defect detection module 330 is configured to determine whether there is a defect in the target detection area based on the comparison result of the detection attenuation coefficient and the calibration attenuation coefficient.

[0116] Optionally, the composite insulator defect detection device further includes a parameter determination module configured to: determine a third peak-to-peak value of a target point at the first end of the reference composite insulator and a fourth peak-to-peak value of each detection point at the second end; wherein the spatial phases of the detection points differ by a preset angle, and the detection points are on the circumference of the longitudinal cross-section of the second end; compare the maximum peak-to-peak value among the fourth peak-to-peak values ​​of the detection points with a reference peak-to-peak value, where the reference peak-to-peak value is the product of a preset coefficient and the third peak-to-peak value; when the maximum peak-to-peak value is greater than or equal to the reference peak-to-peak value, the detection point corresponding to the maximum peak-to-peak value is used as a reference calibration point, and the current detection distance is used as a calibration point. A detection distance is determined, where the current detection distance is the distance from the target point at the first end of the reference composite insulator to the target point at the second end; when the maximum peak-to-peak value is less than the reference peak-to-peak value, the current detection distance is shortened according to the preset reduction distance to determine the third peak-to-peak value of the target point at the first end of the reference composite insulator and the fourth peak-to-peak value of each detection point at the second end next time, so as to determine the reference calibration point and the calibration detection distance; when the current detection distance is equal to or less than the preset distance and the maximum peak-to-peak value is less than the reference peak-to-peak value, the detection point corresponding to the maximum peak-to-peak value output at the preset distance is used as the reference calibration point, and the preset distance is used as the calibration detection distance.

[0117] Optionally, the composite insulator defect detection device also includes a calibration attenuation coefficient determination module, which is configured to: determine a preset number of candidate attenuation coefficients; wherein the preset number is determined based on the calibration detection distance and the minimum periodic shed length; determine the attenuation coefficient average value, the attenuation coefficient average error and the attenuation coefficient root mean square error based on the candidate attenuation coefficients; judge whether the first parameter and the second parameter meet a first preset condition; wherein the first parameter is the ratio of the attenuation coefficient average error to the attenuation coefficient average value, and the second parameter is the ratio of the attenuation coefficient root mean square error to the attenuation coefficient average value, and the first preset condition is that the first parameter is greater than a preset error value and the second parameter is greater than a preset error value; in response to the judgment result that the first parameter and the second parameter meet the first preset condition, use the attenuation coefficient average value as the calibration attenuation coefficient; in response to the judgment result that the first parameter and the second parameter do not meet the first preset condition, determine the calibration attenuation coefficient according to the attenuation coefficient equation and the calibration detection distance, and the attenuation coefficient equation is determined according to the candidate attenuation coefficients.

[0118] Optionally, the attenuation coefficient determination module 320 is configured to: use the ratio of the difference between the second longitudinal mode peak-to-peak value and the first longitudinal mode peak-to-peak value to the product of the first longitudinal mode peak-to-peak value and the calibrated detection distance as the longitudinal mode detection attenuation coefficient; and use the ratio of the difference between the second torsional mode peak-to-peak value and the first torsional mode peak-to-peak value to the product of the first torsional mode peak-to-peak value and the calibrated detection distance as the torsional mode detection attenuation coefficient.

[0119] Optionally, the calibration attenuation coefficient includes a longitudinal modal calibration detection attenuation coefficient and a torsional modal calibration detection attenuation coefficient, and the defect detection module 330 includes: a judgment unit, configured to determine whether the relationship between the detection attenuation coefficient and the calibration attenuation coefficient meets a second preset condition and / or a third preset condition based on the detection attenuation coefficient and the calibration attenuation coefficient, the second preset condition being that the longitudinal modal detection attenuation coefficient is less than the longitudinal modal calibration detection attenuation coefficient of a first preset multiple, and the third preset condition being that the torsional modal detection attenuation coefficient is less than the torsional modal calibration detection attenuation coefficient of a first preset multiple; a first defect determination unit, configured to determine that there is no defect in the target detection area when the relationship between the detection attenuation coefficient and the calibration attenuation coefficient satisfies both the second preset condition and the third preset condition; a second defect determination unit, configured to determine that there is a defect in the target detection area when the relationship between the detection attenuation coefficient and the calibration attenuation coefficient does not meet both the second preset condition and the third preset condition; and a third defect determination unit, configured to determine that there may be a defect in the target detection area when the relationship between the detection attenuation coefficient and the calibration attenuation coefficient satisfies only any one of the second preset condition and the third preset condition.

[0120] Optionally, the second defect determination unit also includes a first defect type determination unit, which is configured to: determine a first center time output by a target point at the first end of the target detection area and a second center time output by a calibration point at the second end; determine a target elastic modulus based on the first center time, the second center time, and a relationship between the elastic modulus and the group velocity; wherein the target elastic modulus includes a longitudinal modal elastic modulus and a torsional modal elastic modulus; determine a target debonding angle based on the second peak-to-peak value and a first calibration relationship; wherein the target debonding angle includes a longitudinal modal debonding angle and a torsional modal debonding angle, and the first calibration relationship represents the relationship between the debonding angle and the peak-to-peak value; determine a target pore depth based on the second peak-to-peak value and the second calibration relationship; wherein the target pore depth includes a longitudinal modal pore depth and a torsional modal pore depth, and the second calibration relationship represents the relationship between the pore depth and the peak-to-peak value; The target debonding angle and the target pore depth are normalized to determine the elastic modulus probability, the debonding angle probability and the pore depth probability, and the sum of the elastic modulus probability, the debonding angle probability and the pore depth probability is one; when there is a candidate probability greater than a preset probability value among the elastic modulus probability, the debonding angle probability and the pore depth probability, the defect type corresponding to the candidate probability is determined as the target defect type; wherein the defect types include core rod aging type, sheath debonding type and pore / bubble type; the core rod aging type is determined according to the elastic modulus probability, the sheath debonding type is determined according to the debonding angle probability, and the pore / bubble type is determined according to the pore depth probability; when there is no candidate probability greater than the preset probability value among the elastic modulus probability, the debonding angle probability and the pore depth probability, the defect type of the target detection area is the core rod aging type, the sheath debonding type and the pore / bubble type.

[0121] Optionally, the third defect determination unit also includes a second defect type determination unit, which is configured to: determine the measured modal attenuation coefficient based on the second peak-to-peak value; when the measured modal attenuation coefficient is greater than the calibrated modal attenuation coefficient of the second preset multiple, and the second torsional mode peak-to-peak value is less than the calibrated torsional mode peak-to-peak value of the third preset multiple, the defect type of the target detection area is the sheath debonding type; when the measured modal attenuation coefficient is less than the calibrated modal attenuation coefficient of the fourth preset multiple, and the second longitudinal mode peak-to-peak value is less than the calibrated longitudinal mode peak-to-peak value of the third preset multiple, the target detection area is a sheath debonding type. The defect type of the target detection area is a pore / bubble type; when the measured modal attenuation coefficient is greater than the calibrated modal attenuation coefficient of the fourth preset multiple, the measured modal attenuation coefficient is less than the calibrated modal attenuation coefficient of the second preset multiple, and the target elastic modulus meets the fourth preset condition, the defect type of the target detection area is a core rod aging type; wherein the fourth preset condition is that the longitudinal modal elastic modulus is less than the original elastic modulus of the fifth preset multiple, and the torsional modulus is less than the original elastic modulus of the fifth preset multiple, and the original elastic modulus is the elastic modulus of the reference composite insulator.

[0122] The composite insulator defect detection device provided in the embodiment of the present application can execute the composite insulator defect detection method provided in any embodiment of the present application, and has the corresponding functional modules and effects of the execution method.

[0123] Example 5

[0124] According to an embodiment of the present disclosure, the present disclosure also provides an electronic device, a readable storage medium, and a computer program product.

[0125] FIG5 shows a block diagram of an electronic device that can be used to implement an embodiment of the present application. The electronic device 10 can be various forms of digital computers, such as laptop computers, desktop computers, workstations, personal digital assistants, servers, blade servers, mainframe computers, and other suitable computers. The electronic device 10 can also represent various forms of mobile devices, such as personal digital processing, cellular phones, smart phones, wearable devices (such as helmets, glasses, watches, etc.) and other similar computing devices. The components shown herein, their connections and relationships, and their functions are merely examples and are not intended to limit the implementation of the present application described and / or required herein.

[0126] As shown in FIG5 , the electronic device 10 includes at least one processor 11 and a memory, such as a read-only memory (ROM) 12 and a random access memory (RAM) 13, that is communicatively connected to the at least one processor 11. The memory stores a computer program that can be executed by the at least one processor, and the processor 11 can perform various appropriate actions and processes according to the computer program stored in the ROM 12 or loaded from the storage unit 18 into the RAM 13. Various programs and data required for the operation of the electronic device 10 can also be stored in the RAM 13. The processor 11, ROM 12, and RAM 13 are connected to each other via a bus 14. An input / output (I / O) interface 15 is also connected to the bus 14.

[0127] Multiple components in the electronic device 10 are connected to the I / O interface 15, including an input unit 16, such as a keyboard, a mouse, etc.; an output unit 17, such as various types of displays, speakers, etc.; a storage unit 18, such as a magnetic disk, an optical disk, etc.; and a communication unit 19, such as a network card, a modem, a wireless communication transceiver, etc. The communication unit 19 allows the electronic device 10 to exchange information / data with other devices via a computer network such as the Internet and / or various telecommunication networks.

[0128] The processor 11 can be any general-purpose and / or specialized processing component with processing and computing capabilities. Some examples of the processor 11 include, but are not limited to, a central processing unit (CPU), a graphics processing unit (GPU), various specialized artificial intelligence (AI) computing chips, various processors running machine learning model algorithms, a digital signal processor (DSP), and any suitable processor, controller, microcontroller, etc. The processor 11 executes the various methods and processes described above, such as the composite insulator defect detection method.

[0129] In some embodiments, the composite insulator defect detection method can be implemented as a computer program tangibly embodied in a computer-readable storage medium, such as storage unit 18. In some embodiments, part or all of the computer program can be loaded and / or installed on electronic device 10 via ROM 12 and / or communication unit 19. When the computer program is loaded into RAM 13 and executed by processor 11, one or more steps of the composite insulator defect detection method described above can be performed. Alternatively, in other embodiments, processor 11 can be configured to execute the composite insulator defect detection method in any other suitable manner (e.g., via firmware).

[0130] Various embodiments of the systems and techniques described herein can be implemented in digital electronic circuit systems, integrated circuit systems, field programmable gate arrays (FPGAs), application specific integrated circuits (ASICs), application specific standard products (ASSPs), systems on chips (SOCs), complex programmable logic devices (CPLDs), computer hardware, firmware, software, and / or combinations thereof. These various embodiments can include being implemented in one or more computer programs that are executable and / or interpreted on a programmable system that includes at least one programmable processor, which can be a special purpose or general purpose programmable processor that can receive data and instructions from a storage system, at least one input device, and at least one output device, and transmit data and instructions to the storage system, the at least one input device, and the at least one output device.

[0131] Computer programs for implementing the methods of the present application may be written in any combination of one or more programming languages. These computer programs may be provided to a processor of a general-purpose computer, a special-purpose computer, or other programmable data processing device, such that when the computer program is executed by the processor, the functions / operations specified in the flowcharts and / or block diagrams are implemented. The computer program may be executed entirely on the machine, partially on the machine, as a stand-alone software package, partially on the machine and partially on a remote machine, or entirely on a remote machine or server.

[0132] In the context of the present application, a computer-readable storage medium can be a tangible medium that can contain or store a computer program for use by an instruction execution system, device or equipment or used in combination with an instruction execution system, device or equipment. A computer-readable storage medium can include, but is not limited to, electronic, magnetic, optical, electromagnetic, infrared or semiconductor systems, devices or equipment, or any suitable combination of the foregoing. Alternatively, a computer-readable storage medium can be a machine-readable signal medium. A machine-readable storage medium can include an electrical connection based on one or more lines, a portable computer disk, a hard disk, a random access memory (RAM), a read-only memory (ROM), an erasable programmable read-only memory (EPROM) or a flash memory, an optical fiber, a portable compact disc read-only memory (CD-ROM), an optical storage device, a magnetic storage device, or any suitable combination of the foregoing.

[0133] To provide for user interaction, the systems and techniques described herein can be implemented on an electronic device 10 having a display device (e.g., a cathode ray tube (CRT) or a liquid crystal display (LCD) monitor) configured to display information to the user, and a keyboard and pointing device (e.g., a mouse or trackball) through which the user can provide input to the electronic device. Other types of devices can also be configured to provide for user interaction; for example, the feedback provided to the user can be any form of sensory feedback (e.g., visual feedback, auditory feedback, or tactile feedback); and input from the user can be received in any form (including acoustic input, voice input, or tactile input).

[0134] The systems and techniques described herein can be implemented in a computing system that includes back-end components (e.g., a data server), or a computing system that includes middleware components (e.g., an application server), or a computing system that includes front-end components (e.g., a user computer with a graphical user interface or a web browser through which a user can interact with implementations of the systems and techniques described herein), or a computing system that includes any combination of such back-end components, middleware components, or front-end components. The components of the system can be interconnected by any form or medium of digital data communication (e.g., a communication network). Examples of communication networks include: a local area network (LAN), a wide area network (WAN), a blockchain network, and the Internet.

[0135] A computing system may include a client and a server. The client and server are generally remote from each other and typically interact via a communication network. This client-server relationship is established by running computer programs on the respective computers. The server may be a cloud server, also known as a cloud computing server or cloud host. This server is a host product within a cloud computing service ecosystem that addresses the management difficulties and limited scalability of traditional physical hosts and virtual private server (VPS) services.

[0136] The steps described in this application can be executed in parallel, sequentially, or in different orders, as long as the expected results of the technical solution of this application can be achieved. This document does not impose any restrictions here.

Claims

1. A composite insulator defect detection method, include: Determine a target detection area of ​​a target composite insulator, collect a first peak-to-peak value outputted by a target point at a first end of the target detection area and a second peak-to-peak value outputted by a calibration point at a second end; wherein the target detection area is determined according to a calibration detection distance, the calibration detection distance is a distance from a target point at a first end of a reference composite insulator to a target point at a second end, the target point is a center point of a longitudinal cross section of the composite insulator, the calibration point is a position point obtained by mapping a position of a reference calibration point on a longitudinal cross section of a second end of the reference composite insulator to a longitudinal cross section of a second end of the target detection area, and the reference composite insulator is an unused composite insulator; Based on the first peak-to-peak value and the second peak-to-peak value, determining a detection attenuation coefficient; wherein the first peak-to-peak value includes a first longitudinal mode peak-to-peak value and a first torsional mode peak-to-peak value, the second peak-to-peak value includes a second longitudinal mode peak-to-peak value and a second torsional mode peak-to-peak value, and the detection attenuation coefficient includes a longitudinal mode detection attenuation coefficient and a torsional mode detection attenuation coefficient; Based on the comparison result of the detection attenuation coefficient and the calibration attenuation coefficient, it is determined whether there is a defect in the target detection area.

2. The method according to claim 1, in, The process of determining the reference calibration point and the calibration detection distance includes: Determine a third peak-to-peak value of a target point at a first end of a reference composite insulator and a fourth peak-to-peak value of each detection point at a second end; wherein the spatial phases of the detection points differ from each other by a preset angle, and the detection points are on the circumference of a longitudinal cross section of the second end; Compare the maximum peak-to-peak value among the fourth peak-to-peak values ​​of each detection point with a reference peak-to-peak value, where the reference peak-to-peak value is the product of a preset coefficient and the third peak-to-peak value; When the maximum peak-to-peak value is greater than or equal to the reference peak-to-peak value, the detection point corresponding to the maximum peak-to-peak value is used as the reference calibration point, and the current detection distance is used as the calibration detection distance, where the current detection distance is the distance from the target point at the first end to the target point at the second end of the reference composite insulator; When the maximum peak-to-peak value is less than the reference peak-to-peak value, shorten the current detection distance according to the preset reduction distance, so as to determine the third peak-to-peak value of the target point at the first end of the reference composite insulator and the fourth peak-to-peak value of each detection point at the second end next time, so as to determine the reference calibration point and the calibration detection distance; When the current detection distance is equal to or less than the preset distance and the maximum peak-to-peak value is less than the reference peak-to-peak value, the detection point corresponding to the maximum peak-to-peak value output at the preset distance is used as the reference calibration point, and the preset distance is used as the calibration detection distance.

3. The method according to claim 2, in, The process of determining the calibration attenuation coefficient includes: Determine a preset number of candidate attenuation coefficients; wherein the preset number is based on the calibration detection distance and The minimum periodic shed length is determined; Determine an attenuation coefficient average, an attenuation coefficient average error, and an attenuation coefficient root mean square error based on the candidate attenuation coefficients; Determine whether the first parameter and the second parameter meet a first preset condition; wherein the first parameter is the ratio of the average error of the attenuation coefficient to the average value of the attenuation coefficient, the second parameter is the ratio of the root mean square error of the attenuation coefficient to the average value of the attenuation coefficient, and the first preset condition is that the first parameter is greater than a preset error value and the second parameter is greater than a preset error value; In response to a judgment result that the first parameter and the second parameter satisfy a first preset condition, taking the average value of the attenuation coefficient as a calibration attenuation coefficient; In response to a judgment result that the first parameter and the second parameter do not satisfy the first preset condition, a calibrated attenuation coefficient is determined according to an attenuation coefficient equation and a calibrated detection distance, wherein the attenuation coefficient equation is determined according to the candidate attenuation coefficients.

4. The method according to claim 1, in, Determining a detection attenuation coefficient based on the first peak-to-peak value and the second peak-to-peak value includes: The ratio of the difference between the peak-to-peak value of the second longitudinal mode and the peak-to-peak value of the first longitudinal mode to the product of the peak-to-peak value of the first longitudinal mode and the calibrated detection distance is taken as the longitudinal mode detection attenuation coefficient; The ratio of the difference between the peak-to-peak value of the second torsion mode and the peak-to-peak value of the first torsion mode to the product of the peak-to-peak value of the first torsion mode and the calibrated detection distance is taken as the torsion mode detection attenuation coefficient.

5. The method according to claim 1, in, The calibration attenuation coefficient includes a longitudinal modal calibration detection attenuation coefficient and a torsional modal calibration detection attenuation coefficient. Based on a comparison result of the detection attenuation coefficient and the calibration attenuation coefficient, determining whether there is a defect in the target detection area includes: Based on the detection attenuation coefficient and the calibration attenuation coefficient, determining whether the relationship between the detection attenuation coefficient and the calibration attenuation coefficient satisfies a second preset condition and / or a third preset condition, wherein the second preset condition is that the longitudinal modal detection attenuation coefficient is less than a first preset multiple of the longitudinal modal calibration detection attenuation coefficient, and the third preset condition is that the torsional modal detection attenuation coefficient is less than a first preset multiple of the torsional modal calibration detection attenuation coefficient; When the relationship between the detection attenuation coefficient and the calibration attenuation coefficient satisfies both the second preset condition and the third preset condition, determining that there is no defect in the target detection area; When the relationship between the detection attenuation coefficient and the calibration attenuation coefficient does not satisfy both the second preset condition and the third preset condition, determining that a defect exists in the target detection area; When the relationship between the detection attenuation coefficient and the calibration attenuation coefficient only satisfies any one of the second preset condition and the third preset condition, it is determined that the target detection area may exist defect.

6. The method according to claim 5, after determining that there is a defect in the target detection area, further include: Determine a first center time output by a target point at a first end of the target detection area and a second center time output by a calibration point at a second end; Determining a target elastic modulus based on the first center time, the second center time, and a relationship between the elastic modulus and the group velocity; wherein the target elastic modulus includes a longitudinal modal elastic modulus and a torsional modal elastic modulus; Determine a target debonding angle based on the second peak-to-peak value and a first calibration relationship; wherein the target debonding angle includes a longitudinal modal debonding angle and a torsional modal debonding angle, and the first calibration relationship represents a relationship between the debonding angle and the peak-to-peak value; Determine a target pore depth based on the second peak-to-peak value and a second calibration relationship; wherein the target pore depth includes a longitudinal modal pore depth and a torsional modal pore depth, and the second calibration relationship represents a relationship between the pore depth and the peak-to-peak value; Normalizing the target elastic modulus, the target degumming angle, and the target pore depth to determine the elastic modulus probability, the degumming angle probability, and the pore depth probability, wherein the elastic modulus probability, the degumming angle probability, and the pore depth probability sum to one; In the case that there is a candidate probability greater than a preset probability value among the elastic modulus probability, the debonding angle probability and the pore depth probability, the defect type corresponding to the candidate probability is determined as the target defect type; wherein the defect types include a core rod aging type, a sheath debonding type and a pore / bubble type; the core rod aging type is determined according to the elastic modulus probability, the sheath debonding type is determined according to the debonding angle probability, and the pore / bubble type is determined according to the pore depth probability; When there is no candidate probability greater than a preset probability value among the elastic modulus probability, the debonding angle probability and the pore depth probability, the defect types of the target detection area are core rod aging type, sheath debonding type and pore / bubble type.

7. The method according to claim 5, after determining that the target detection area may have defects, further include: Determine the measured modal attenuation coefficient based on the second peak-to-peak value; When the measured modal attenuation coefficient is greater than the calibrated modal attenuation coefficient of the second preset multiple, and the peak-to-peak value of the second torsional mode is less than the peak-to-peak value of the calibrated torsional mode of the third preset multiple, the defect type of the target detection area is the sheath debonding type; When the measured modal attenuation coefficient is less than the calibrated modal attenuation coefficient of the fourth preset multiple, and the second longitudinal When the modal peak-to-peak value is less than the third preset multiple of the calibrated longitudinal modal peak-to-peak value, the defect type of the target inspection area is a pore / bubble-containing type; When the measured modal attenuation coefficient is greater than the calibrated modal attenuation coefficient of the fourth preset multiple, the measured modal attenuation coefficient is less than the calibrated modal attenuation coefficient of the second preset multiple, and the target elastic modulus satisfies the fourth preset condition, the defect type of the target detection area is the core rod aging type; wherein the fourth preset condition is that the longitudinal modal elastic modulus is less than the original elastic modulus of the fifth preset multiple, and the torsional modulus is less than the original elastic modulus of the fifth preset multiple, and the original elastic modulus is the elastic modulus of the reference composite insulator.

8. A composite insulator defect detection device, include: a peak-to-peak value determination module, configured to determine a target detection area of ​​a target composite insulator, and collect a first peak-to-peak value outputted by a target point at a first end of the target detection area and a second peak-to-peak value outputted by a calibration point at a second end; wherein the target detection area is determined according to a calibration detection distance, the calibration detection distance is a distance from a target point at a first end of a reference composite insulator to a target point at a second end, the target point is a center point of a longitudinal cross section of the composite insulator, the calibration point is a position point obtained by mapping a position of a reference calibration point on a longitudinal cross section of a second end of the reference composite insulator to a longitudinal cross section of a second end of the target detection area, and the reference composite insulator is an unused composite insulator; an attenuation coefficient determination module, configured to determine a detection attenuation coefficient based on the first peak-to-peak value and the second peak-to-peak value; wherein the first peak-to-peak value includes a first longitudinal mode peak-to-peak value and a first torsional mode peak-to-peak value, the second peak-to-peak value includes a second longitudinal mode peak-to-peak value and a second torsional mode peak-to-peak value, and the detection attenuation coefficient includes a longitudinal mode detection attenuation coefficient and a torsional mode detection attenuation coefficient; The defect detection module is configured to determine whether there is a defect in the target detection area based on a comparison result of the detection attenuation coefficient and the calibration attenuation coefficient.

9. An electronic device, include: at least one processor; as well as a memory communicatively coupled to the at least one processor; The memory stores a computer program executable by the at least one processor, and the computer program is executed by the at least one processor so that the at least one processor can execute the composite insulator defect detection method according to any one of claims 1 to 7.

10. A computer-readable storage medium storing computer instructions, wherein the computer instructions are used to enable a processor to implement the composite insulator defect detection method according to any one of claims 1 to 7 when executed.

Citation Information

Patent Citations

  • Torsional mode ultrasonic guided-wave based composite insulator debonding detection method

    CN107085040A

  • Terahertz wave based internal defect imaging device and method and readable storage medium

    CN110579483A

  • Composite insulator defect detection method, device, equipment and system

    CN111856190A

  • Composite insulator detection method and device, terminal equipment and readable storage medium

    CN114065811A

  • Composite insulator defect detection method and device, electronic equipment and storage medium

    CN116165279A

Cited By

  • Method and system for calculating crisp and decayed length of crisp and decayed composite insulator

    CN120298477A

  • Lightning arrester insulation protection method

    CN120804794A