Antibacterial fabric and preparation method therefor
By using a mixed solution soaking process of a blend of left-handed polylactic acid and right-handed polylactic acid and antibacterial nanoparticles on fiber materials, an antibacterial fabric with a stereoscopic cross-linked network is formed, which solves the problem of antibacterial coating adhesion and antibacterial coating in the existing technology. It solves the problem of insufficient mechanical strength and achieves efficient antibacterial performance and stability. It is suitable for a variety of fiber materials and expands its application scope.
Patent Information
- Application Number
- PCT/CN2024/093529
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-04-26
- Filing Date
- 2024-05-16
- Publication Date
- 2024-10-31
AI Technical Summary
The antibacterial coating of existing medical protective fiber materials has low adhesion, weak mechanical strength, and limited bonding ability, which limits its durability and cannot achieve the function of actively inactivating pathogenic microorganisms. As a result, it is easy to cause sequelae when worn and handled improperly. Infection occurs.
Using a mixed solution composed of a blend of L-polylactic acid and D-polylactic acid and antibacterial nanoparticles (such as zinc oxide-silver nanoparticles), the fabric is soaked and dried to form an antibacterial fabric with a stereoscopic cross-linked network, which enhances the nanoparticles. The binding force between particles and fiber surface.
It significantly improves the antibacterial performance of antibacterial fabrics, enhances the binding force between nanoparticles and fibers, is suitable for a variety of fabrics, has low cost, simple process, is suitable for mass production, and has broad application prospects in the fields of medical, military and home textiles.
Smart Images

Figure CN2024093529_31102024_PF_FP_ABST
Abstract
Description
Antibacterial fabric and preparation method thereof Technical Field
[0001] The present invention relates to the technical field of new materials, in particular to an antibacterial fabric and a preparation method thereof. Background Art
[0002] Wearing personal protective equipment (PPE) has been shown to be an effective way to prevent the spread of pathogens. However, existing medical protective fiber materials only provide protection by blocking pathogens and cannot actively inactivate them. If the wearer's hands or other body parts come into contact with contaminated PPE, or if discarded PPE is improperly handled, secondary infection can easily occur. The introduction of antimicrobial nanomaterials could enable the active protective properties of these fiber materials.
[0003] The current mainstream strategy for developing antimicrobial medical protective fiber materials is to load antimicrobial nanomaterials onto fiber materials through vapor deposition, evaporation, sputtering, and spraying, as shown in patents CN111549521A and CN103015166B. However, the antimicrobial coatings suffer from low adhesion, weak mechanical strength, and limited bonding capacity (e.g., weak electrostatic interactions), which limit the durability of these medical protective fiber materials. Therefore, there is an urgent need to develop antimicrobial fabrics with excellent antimicrobial properties and high stability to expand their application.
[0004] Summary of the Invention
[0005] The object of the present invention is to provide an antibacterial fabric with good antibacterial properties. The preparation process of the antibacterial fabric is simple, the preparation efficiency is high, the cost is low, and it is suitable for batch production.
[0006] In order to achieve the purpose of the present invention, the preparation method of the antibacterial fabric provided by the present invention specifically comprises the following steps in parts by weight:
[0007] (1) Preparation of polylactic acid solution: 0.1 to 30 parts of polylactic acid are added to 100 parts of solvent, and the mixture is stirred and dissolved at a speed of 200 to 1000 rpm at room temperature to 100° C. for 0.5 to 5 hours to obtain a polylactic acid solution with a mass concentration of 0.1 to 30%.
[0008] (2) Preparation of mixed solution: 0.01 to 20 parts of antibacterial nanoparticles are added to the above polylactic acid solution and stirred for 0.1 to 12 hours to obtain a mixed solution.
[0009] (3) Preparation of antibacterial fabric: soak the fabric in the above mixed solution. After a period of time, take out the fabric and dry it to obtain the antibacterial fabric.
[0010] Furthermore, in step (1), the polylactic acid is a blend of L-polylactic acid and D-polylactic acid, wherein the D-polylactic acid accounts for 10 to 50% of the total mass of the polylactic acid.
[0011] Furthermore, in step (1), the solvent is any one of dimethyl carbonate, dichloromethane or chloroform, or a combination of two or more thereof.
[0012] Furthermore, in step (2), the antibacterial nanoparticles are any one of heterostructured zinc oxide-silver nanoparticles, cuprous oxide nanoparticles, copper oxide nanoparticles, ferric oxide nanoparticles, ferrous oxide nanoparticles, zinc oxide nanoparticles, zinc sulfide nanoparticles, titanium dioxide nanoparticles, silver nanoparticles or bismuth oxide nanoparticles, or a combination of two or more thereof.
[0013] Furthermore, in step (3), the fabric is any one of nylon fabric, vinylon fabric, polyester fabric, polypropylene fabric, spandex fabric, polyethylene fiber fabric, and cotton fiber fabric, or a combination of two or more thereof.
[0014] Furthermore, in step (3), the soaking method is to stand or stir at a speed lower than 2000 rpm for 0.01 to 12 hours.
[0015] The present invention also provides antibacterial fabric prepared by adopting the preparation method of the antibacterial fabric.
[0016] The present invention has achieved the following beneficial effects:
[0017] 1. The present invention uses a stereocomposite cross-linked network formed by an appropriate proportion of L-polylactic acid and D-polylactic acid to stably and evenly disperse the nanoparticles on the fabric surface, and the stereocomposite cross-linked network can enhance the binding force between the antibacterial nanoparticles and the fiber fabric surface.
[0018] 2. The antibacterial fabric prepared by the present invention has significantly high antibacterial properties and has broad application prospects in the fields of medical equipment, military industry, home textiles, medical protection, etc.
[0019] 3. The polylactic acid / antibacterial nanoparticle mixed solution system used in the antibacterial fabric prepared by the present invention is suitable for soaking most fabrics, such as nylon fabric, vinylon fabric, polyester fabric, polypropylene fabric, spandex fabric, polyethylene fiber fabric, and cotton fiber fabric.
[0020] 4. The antibacterial fabric of the present invention is prepared by soaking the fiber fabric in a mixed solution composed of L-polylactic acid, D-polylactic acid and antibacterial nanoparticles. The raw materials are widely available, the preparation process is simple, the cost is low, the efficiency is high, and it has good prospects for industrial application. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] FIG1 is a physical diagram of an antibacterial polyethylene fiber fabric according to an embodiment of the present invention;
[0022] FIG2 is a physical picture of an antibacterial polyester fabric according to an embodiment of the present invention;
[0023] FIG3 is a physical picture of an antibacterial cotton fiber fabric according to an embodiment of the present invention;
[0024] FIG4 is a diagram showing the antibacterial performance of an antibacterial polyethylene fiber fabric against Escherichia coli according to an embodiment of the present invention;
[0025] FIG5 is a diagram showing the antibacterial performance of the antibacterial polyester fabric against Escherichia coli according to an embodiment of the present invention;
[0026] FIG6 is a diagram showing the antibacterial performance of an antibacterial cotton fiber fabric against Escherichia coli according to an embodiment of the present invention;
[0027] FIG7 is a comparison diagram of the antibacterial polyethylene fiber fabric with a stereo-crosslinked network prepared by the present invention and the antibacterial polyethylene fiber fabric without a stereo-crosslinked network. DETAILED DESCRIPTION
[0028] The specific embodiments of the present invention are described in detail below. All features disclosed in this specification, or steps in all methods or processes disclosed, except for mutually exclusive features and / or steps, can be combined in any manner.
[0029] Example 1
[0030] The preparation method of the antibacterial fabric of this embodiment is:
[0031] (1) Preparation of polylactic acid solution: 0.5 g of polylactic acid (wherein the mass ratio of L-polylactic acid to D-polylactic acid is 1:1) was added to 10 g of dichloromethane, and the mixture was stirred and dissolved at 25°C and 600 rpm for 3 h to obtain a polylactic acid solution with a mass concentration of 5%.
[0032] (2) Preparation of polylactic acid mixed solution: 0.02 g of heterostructured zinc oxide-silver nanoparticles was added to the above polylactic acid solution and stirred for 8 h to obtain a polylactic acid mixed solution.
[0033] (3) Preparation of antibacterial fabric: The polyethylene fiber fabric was immersed in the above mixed solution and stirred at a speed of 1000 rpm for 12 h. The polyethylene fiber fabric was taken out and dried to obtain the antibacterial polyethylene fiber fabric, as shown in FIG1 .
[0034] The obtained product was tested by a colony counter, and the antibacterial rate against Escherichia coli was 99.99%, as shown in FIG4 .
[0035] Comparative Example 1
[0036] The preparation method of the antibacterial fabric of this comparative example 1 is:
[0037] (1) Preparation of polylactic acid solution: 0.5 g of L-polylactic acid was added to 10 g of dichloromethane, and the mixture was stirred and dissolved at 25° C. and 600 rpm for 3 h to obtain a polylactic acid solution with a mass concentration of 5%.
[0038] (2) Preparation of polylactic acid mixed solution: 0.02 g of heterostructured zinc oxide-silver nanoparticles was added to the above polylactic acid solution and stirred for 8 h to obtain a polylactic acid mixed solution.
[0039] (3) Preparation of antibacterial fabric: The polyethylene fiber fabric was immersed in the above mixed solution and stirred at a speed of 1000 rpm for 12 h. The polyethylene fiber fabric was taken out and dried to obtain the antibacterial polyethylene fiber fabric.
[0040] The resulting product was tested using a colony counter and found to have an antibacterial rate of 98.58% against E. coli. However, the interfacial bonding strength between the polylactic acid film, which lacks a stereo-crosslinked network, and the polyethylene fiber fabric was very weak, resulting in easy peeling, as shown in Figure 7.
[0041] As shown in Figure 7, an antibacterial polyethylene fiber fabric prepared through step (3) of the specific embodiment is a physical comparison of an antibacterial polyethylene fiber fabric with a stereo-crosslinked network (Example 1, as shown in the left figure of Figure 7) and an antibacterial polyethylene fiber fabric without a stereo-crosslinked network (Comparative Example 1, as shown in the right figure of Figure 7). The interfacial bonding strength between the antibacterial polyethylene fiber fabric with a stereo-crosslinked network and the polylactic acid / nanoparticle film is significantly better than the interfacial bonding strength between the antibacterial polyethylene fiber fabric without a stereo-crosslinked network and the polylactic acid / nanoparticle film.
[0042] Example 2
[0043] The preparation method of the antibacterial fabric of this embodiment is:
[0044] (1) Preparation of polylactic acid solution: 0.2 g of polylactic acid (wherein the mass ratio of L-polylactic acid to D-polylactic acid is 1:1) was added to 10 g of dichloromethane, and the mixture was stirred and dissolved at 60°C and 900 rpm for 1 h to obtain a polylactic acid solution with a mass concentration of 2%.
[0045] (2) Preparation of polylactic acid mixed solution: 0.005 g of heterostructured zinc oxide-silver nanoparticles was added to the above polylactic acid solution and stirred for 2 h to obtain a polylactic acid mixed solution.
[0046] (3) Preparation of antibacterial fabric: The polyester fiber fabric was immersed in the above mixed solution and stirred at a speed of 1200 rpm for 10 h. The polyester fiber fabric was taken out and dried to obtain the antibacterial polyester fabric, as shown in FIG2 .
[0047] The obtained product was tested by a colony counter, and the antibacterial rate against Escherichia coli was 99.91%, as shown in FIG5 .
[0048] Example 3
[0049] The preparation method of the antibacterial fabric of this embodiment is:
[0050] (1) Preparation of polylactic acid solution: 0.5 g of polylactic acid (wherein the mass ratio of L-polylactic acid to D-polylactic acid is 1:1) was added to 10 g of dichloromethane, and the mixture was stirred and dissolved at 40°C and 800 rpm for 2 h to obtain a polylactic acid solution with a mass concentration of 5%.
[0051] (2) Preparation of polylactic acid mixed solution: 0.01 g of heterostructured zinc oxide-silver nanoparticles was added to the above polylactic acid solution and stirred for 5 h to obtain a polylactic acid mixed solution.
[0052] (3) Preparation of antibacterial fabric: Cotton fiber fabric was immersed in the above mixed solution and stirred at a speed of 900 rpm for 5 h. The cotton fiber fabric was taken out and dried to obtain antibacterial cotton fiber fabric, as shown in FIG3 .
[0053] The obtained product was tested by a colony counter, and the antibacterial rate against Escherichia coli was 99.99%, as shown in FIG6 .
[0054] The above-described embodiments merely represent specific implementations of the present invention. While the descriptions are relatively specific and detailed, they should not be construed as limiting the scope of the present invention. It should be noted that a person skilled in the art would be able to make numerous variations and improvements without departing from the spirit of the present invention, and all such variations and improvements fall within the scope of protection of the present invention.
Claims
1. A method for preparing an antibacterial fabric, characterized in that: By weight, the method specifically comprises the following steps: (1) Preparation of polylactic acid solution: 0.1 to 30 parts of polylactic acid are added to 100 parts of a solvent, and the mixture is stirred and dissolved at a speed of 200 to 1000 rpm for 0.5 to 5 hours at room temperature to 100° C. to obtain a polylactic acid solution with a mass concentration of 0.1 to 30%; (2) Preparation of mixed solution: adding 0.01 to 20 parts of antibacterial nanoparticles to the above polylactic acid solution, stirring for 0.1 to 12 hours, to obtain a mixed solution; (3) Preparation of antibacterial fabric: soaking the fabric in the mixed solution, taking out the fabric after a period of time, and drying it to obtain the antibacterial fabric; In the step (1), the polylactic acid is a blend of left-handed polylactic acid and right-handed polylactic acid, wherein the right-handed polylactic acid accounts for 10 to 50% of the total mass of the polylactic acid.
2. The method for preparing the antibacterial fabric according to claim 1, characterized in that: In the step (1), the solvent is any one of dimethyl carbonate, dichloromethane or chloroform, or a combination of two or more thereof.
3. The method for preparing the antibacterial fabric according to claim 1, characterized in that: In the step (2), the antibacterial nanoparticles are any one of heterostructured zinc oxide-silver nanoparticles, cuprous oxide nanoparticles, cupric oxide nanoparticles, ferric oxide nanoparticles, ferrous oxide nanoparticles, zinc oxide nanoparticles, zinc sulfide nanoparticles, titanium dioxide nanoparticles, silver nanoparticles or bismuth oxide nanoparticles, or a combination of two or more thereof.
4. The method for preparing the antibacterial fabric according to claim 1, characterized in that: In the step (3), the fabric is any one of nylon fabric, vinyl fabric, polyester fabric, polypropylene fabric, spandex fabric, polyethylene fiber fabric, and cotton fiber fabric, or a combination of two or more thereof.
5. The method for preparing the antibacterial fabric according to claim 1, characterized in that: In the step (3), the soaking method is to stand or stir at a speed lower than 2000 rpm for 0.01 to 12 hours.
6. An antibacterial fabric prepared by the method for preparing antibacterial fabric according to any one of claims 1 to 5.
Citation Information
Patent Citations
Nanometer traditional chinese medicine microcapsule fabric finishing agent, preparation and fabric finishing method
CN101324026A
Non-migration type efficient antibacterial composite material and preparation method thereof
CN109553939A
Antibacterial fabric and preparation method thereof
CN116356569A
Nanometer material dispersion liquid with steric cross-linked network stably dispersed and preparation method of nanometer material dispersion liquid
CN116789988A
Porous polylactic acid antibacterial nanofiber and preparation method thereof
CN116791233A