Organic electroluminescent compound and light-emitting device
By introducing deuterium-substituted carbazole groups into organic electroluminescent materials, the problems of material stability and luminous efficiency were solved, thereby improving the stability and efficiency of the device, reducing the fabrication cost, and extending its service life.
Patent Information
- Application Number
- PCT/CN2026/093762
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-07
- Filing Date
- 2026-04-29
- Publication Date
- 2026-11-12
AI Technical Summary
Existing organic electroluminescent materials have poor stability and luminous efficiency. In particular, the P/N ratio of green light-emitting materials changes greatly during the evaporation process, leading to unstable device performance and affecting device lifespan and luminous efficiency.
Organic electroluminescent compounds with a specific structure, in which carbazole and the electron-rich group composed of the benzene ring attached thereto are replaced by deuterium, and combined with the deuterated P-type compound in the core region, form a Premix material with good solubility, which is used for the light-emitting layer and other organic layers to improve the chemical, photoelectric and thermal stability of the material.
This improves the stability and luminous efficiency of organic electroluminescent devices, reduces fabrication and cleaning costs, extends device lifespan, and enhances carrier mobility and mass production stability.
Smart Images

Figure CN2026093762_12112026_PF_FP_ABST
Abstract
Description
Organic electroluminescent compounds and light-emitting devices
[0001] Cross-references to related applications
[0002] This application claims priority to Chinese Patent Application No. 202510579667.X, filed on May 7, 2025, entitled "Organic Electroluminescent Compounds and Light-Emitting Devices", the entire contents of which are incorporated herein by reference. Technical Field
[0003] This disclosure belongs to the field of organic electroluminescence technology, specifically relating to organic electroluminescent compounds and light-emitting devices. Background Technology
[0004] Organic electroluminescent devices generally include a cathode, an anode, and an organic layer disposed between the two. When a voltage is applied between the two electrodes, holes are injected into the organic layer from the anode, and electrons are injected into the organic layer from the cathode. When holes and electrons meet, they form excitons. When the excitons re-transition to the ground state, they emit light.
[0005] In recent years, deuterated luminescent materials have been frequently used in organic light-emitting devices (OLEDs). The way deuterium atoms are introduced into luminescent materials can have different effects on device performance. For example, if deuteration does not occur at active sites or sites with high electron density in the material molecule, the material stability may not meet expectations, thus affecting the device's lifetime. Poor compatibility between the host luminescent materials in organic OLEDs may lead to inefficient energy transfer to the dopant materials, thus affecting luminous efficiency. Furthermore, we have found that the P / N ratio of current green host luminescent materials changes significantly with increasing deposition time, resulting in large fluctuations in device performance, poor stability, and low yield. Summary of the Invention
[0006] The technical objective of this disclosure is to develop organic electroluminescent materials with superior performance.
[0007] To achieve the above technical objectives, this disclosure provides the following technical solution:
[0008] The structural formula of the organic electroluminescent compound is shown in formula (1) below:
[0009] In the formula:
[0010] R0-R7 each independently represent deuterium, deuterated or unsubstituted C6-C30 aryl groups, provided that at least seven of R0-R7 are deuterium;
[0011] R8-R 11Each independently represents a C6-C30 aryl group, either hydrogen-, deuterium-, or deuterated or unsubstituted, under the condition R8-R. 11 At least one of them is deuterium;
[0012] L1 and L2 each represent a single bond independently;
[0013] Ar1 and Ar2 being the same or different represent C6-C30 aryl groups that are substituted or unsubstituted, provided that R0-R... 11 When none of Ar1 and Ar2 are deuterated or unsubstituted C6-C30 aryl groups, at least one of Ar1 and Ar2 is a biphenyl group that is substituted or unsubstituted; the substituents of Ar1 and Ar2 are each independently selected from one or more of deuterium, cyano, C6-C20 aryl, deuterated C6-C20 aryl, C5-C20 heteroaryl, C1-C4 straight-chain or branched alkyl, or deuterated C1-C4 straight-chain or branched alkyl, or a combination of multiple such substituents.
[0014] Furthermore, Ar1 and Ar2 being identical or different represent phenyl or biphenyl substituted or unsubstituted forms, wherein the substituents of Ar1 and Ar2 are each independently selected from one or more of deuterium, methyl, phenyl, deuterated methyl and deuterated phenyl, or a combination of multiple forms.
[0015] Furthermore, in the compound, R8-R 11 In the middle, R8 or R 10 It is a C6-C30 aryl group that is either deuterated or unsubstituted, and at least one of the other three R groups is deuterated.
[0016] Furthermore, in the compound, the seven R groups in R0-R7 are deuterium, and the other non-deuterium group is phenyl or deuterated phenyl.
[0017] In the preferred embodiments of this disclosure, the compounds are selected from the following compounds:
[0018] An organic electroluminescent device includes a first electrode, a second electrode, and an organic layer formed between the first electrode and the second electrode, the organic layer containing an organic electroluminescent compound as described in any of the preceding claims.
[0019] In a preferred embodiment of this disclosure, the organic layer includes a hole injection layer, a first hole transport layer, a second hole transport layer, a light-emitting layer, a hole blocking layer, an electron transport layer, and an electron injection layer, wherein the light-emitting layer contains an organic electroluminescent compound as described in any of the above embodiments.
[0020] Furthermore, in the organic electroluminescent device, the light-emitting layer contains a light-emitting host material, which is composed of a first compound and a second compound. The first compound is any of the organic electroluminescent compounds described above, and the structure of the second compound is shown in formula (2-1) or formula (2-2):
[0021] In the formula:
[0022] L3, L4, L5, and L6 each independently represent a single bond, or a C6-C20 arylene bond with or without deuteration substitution;
[0023] Ar3, Ar4, Ar5 and Ar6 each independently represent C6-C30 aryl groups that are substituted or unsubstituted, or C5-C30 heteroaryl groups that are substituted or unsubstituted; the substituents of Ar3, Ar4, Ar5 and Ar6 are each independently selected from deuterium, deuterated or undeuterated C6-C20 aryl groups.
[0024] R 12 and R 13 Let m1 be a deuterium, m2 be an integer selected from 0 to 3, and n be an integer selected from 0 to 4.
[0025] Furthermore, in the second compound, L3, L4, L5, and L6 are each independently a single bond, a phenylene group, or a deuterated phenylene group; Ar3, Ar4, Ar5, and Ar6 are each independently a substituted or unsubstituted phenyl, biphenyl, naphthyl, anthracene, phenanthrene, benzo[a]phenanthrene, or N-containing heteroaryl group, and the substituents of Ar3, Ar4, Ar5, and Ar6 are selected from one or more of deuterium, phenyl, and deuterated phenyl groups.
[0026] In a preferred embodiment of this disclosure, the second compound is selected from any one of the following compounds:
[0027] The beneficial effects of this disclosure are as follows:
[0028] 1) In the N-type compound structure disclosed herein, the electron-rich group consisting of carbazole and the benzene ring attached thereto is replaced by deuterium. Combined with the deuterated P-type compound in the core region (HOMO electron distribution region), the chemical stability, photoelectric stability and thermal stability of the luminescent material structure can be effectively improved, thereby improving the stability and service life of the luminescent device using the material.
[0029] 2) The N-type compound disclosed herein can form a good premix material with the deuterated P-type compound in the core region (HOMO electron distribution region). It has good P / N stability and mass production stability during the evaporation process, and the formed premix material has a more balanced carrier mobility, thereby greatly improving the efficiency and lifespan of the device.
[0030] 3) The compounds disclosed herein have good solubility, which can reduce the preparation cost of materials and the cleaning cost of masks. Attached Figure Description
[0031] To more clearly illustrate the technical solutions of the embodiments of this disclosure, the accompanying drawings used in the embodiments will be briefly described below. It should be understood that the following drawings only show some embodiments of this disclosure and should not be regarded as a limitation of the scope. For those skilled in the art, other related drawings can be obtained based on these drawings without creative effort.
[0032] Figure 1 is a schematic diagram of the structure of the organic electroluminescent device provided in this disclosure;
[0033] Figure 2 is the HPLC chromatogram of compound N-1 disclosed herein;
[0034] Figure 3 is the HPLC chromatogram of compound N-3 disclosed herein;
[0035] Figure 4 is the HPLC chromatogram of compound N-60 disclosed herein;
[0036] Diagram: 1-Anode, 2-Hole injection layer, 3-First hole transport layer, 4-Second hole transport layer, 5-Light emission layer, 6-Hole blocking layer, 7-Electron transport layer, 8-Electron injection layer, 9-Cathode. Detailed Implementation
[0037] To make the objectives, technical solutions, and advantages of the embodiments of this disclosure clearer, the technical solutions in the embodiments of this disclosure will be clearly and completely described below. Where specific conditions are not specified in the embodiments, conventional conditions or conditions recommended by the manufacturer shall apply. Reagents or instruments whose manufacturers are not specified are all conventional products that can be purchased commercially.
[0038] In this document, the terms "substituted" or "unsubstituted" refer to the rearrangement of at least one hydrogen atom in a group with a substituent group such as deuterium, aryl, or heteroaryl. "Aryl" in this document refers to a group containing one or more aromatic rings, including but not limited to benzene, naphthalene, phenanthrene, fluorene, and acenaphthene. "Heteroaryl" in this document refers to a heteroaryl group obtained by substituting one or more carbon atoms in the structure of an aryl group with one or more heteroatoms. The terms "C6-C30," "C5-C30," "C1-C4," "C6-C20," and "C5-C20" respectively indicate that the modified group contains 6-30, 5-30, 1-4, 6-20, and 5-20 carbon atoms. "Deuterium" in this disclosure refers to a stable isotope of hydrogen, also known as heavy hydrogen, with the element symbol D.
[0039] Unless otherwise specified in the examples, the procedures should be performed under standard conditions or conditions recommended by the manufacturer. Reagents or instruments whose manufacturers are not specified are all commercially available products.
[0040] Example 1:
[0041] The synthesis method of compound N-1 is as follows:
[0042] Step 1: Under air atmosphere, add 25 ml of 3-bromo-4-fluorobiphenyl (25 g, 0.1 mol, 1 eq), 25 ml of toluene, 40 g of heavy water (2 mol, 20 eq), 5.6 g of silver carbonate (0.02 mol, 20% eq), 13.41 g of diphenylcyclohexylphosphine (0.05 mol, 50% eq), and 36 g of potassium carbonate (0.26 mol, 1 eq) to the reaction flask. After the addition is complete, heat the reaction solution to 120 °C and react for 24 h. Add 150 ml of toluene to the reaction solution, separate the liquids, concentrate the organic phase to dryness, and column chromatography to obtain approximately 21.5 g of intermediate 1, with a yield of 85%.
[0043] Step 2: Under nitrogen protection, deuterated carbazole (14.87 g, 0.085 mol, 1 eq), intermediate 1 (21.5 g, 0.085 mol, 1 eq), DMF (200 ml), and cesium carbonate (69 g, 0.2125 mol, 2.5 eq) were added to the reaction flask. After the addition was complete, the reaction solution was heated to reflux and reacted for 12 h. The reaction was detected by HPLC. After cooling, 200 ml of water was added for washing, and the mixture was filtered. The filter cake was dried and purified by column chromatography using a petroleum ether / dichloromethane system to obtain approximately 27.74 g of intermediate 2, with a yield of 80%.
[0044] Step 3: Under nitrogen protection, intermediate 2 (27.84 g, 0.068 mol, 1 eq) was added to the reaction flask, followed by 300 ml of ultra-dry tetrahydrofuran. The temperature was lowered to -78°C, and 2.5 M n-butyllithium (28.56 ml, 0.0714 mol, 1.05 eq) was added dropwise. After the addition was complete, the reaction was kept at this temperature for 1 h. Triisopropyl borate (15.34 g, 0.0816 mol, 1.2 eq) was added dropwise. After the addition was complete, the temperature was allowed to rise naturally to room temperature. A saturated ammonium chloride aqueous solution was added, and the mixture was separated. The organic phase was concentrated to dryness and recrystallized from ethyl acetate to obtain approximately 20.34 g of intermediate 3, with a yield of 80%.
[0045] Step 4: Under nitrogen protection, intermediate 3 (20.34 g, 0.0544 mol, 1 eq), triazine compound (14.5 g, 0.0544 mol, 1 eq), toluene (300 ml), ethanol (150 ml), potassium carbonate (18.63 g, 0.135 mol, 2.5 eq), and Pd(PPh3)4 (0.62 g, 0.00054 mol, 1% eq) were added to the reaction flask. After the addition was complete, the reaction solution was heated to reflux and reacted overnight. The reaction was sampled and detected by HPLC. After cooling, the reaction solution was washed with water, separated, and the organic phase was passed through silica gel and concentrated to dryness. Column chromatography was performed to obtain approximately 19.87 g of compound N-1, with a yield of 65%.
[0046] Other compounds were prepared using similar methods, as shown in Tables 1-1, 1-2, 1-3, 1-4, 1-5, 1-6, 1-7, 1-8, 1-9, 1-10, 1-11, 1-12, 1-13, 1-14, 1-15, 1-16, 1-17, 1-18, 1-19, 1-20, 1-21, 1-22, and 1-23 below.
[0047] Table 1-1
[0048] Table 1-2
[0049] Table 1-3
[0050] Table 1-4
[0051] Table 1-5
[0052] Table 1-6
[0053] Table 1-7
[0054] Table 1-8
[0055] Table 1-9
[0056] Table 1-10
[0057] Table 1-11
[0058] Table 1-12
[0059] Table 1-13
[0060] Table 1-14
[0061] Table 1-15
[0062] Table 1-16
[0063] Table 1-17
[0064] Table 1-18
[0065] Table 1-19
[0066] Table 1-20
[0067] Table 1-21
[0068] Table 1-22
[0069] Table 1-23
[0070] The synthetic identification results of the compounds prepared in Tables 1-1, 1-2, 1-3, 1-4, 1-5, 1-6, 1-7, 1-8, 1-9, 1-10, 1-11, 1-12, 1-13, 1-14, 1-15, 1-16, 1-17, 1-18, 1-19, 1-20, 1-21, 1-22, and 1-23 are shown in Table 2 below:
[0071] Table 2
[0072] Device performance testing:
[0073] Application Example 1:
[0074] ITO was used as the anode substrate material for the reflective layer, and its surface was sequentially treated with water, acetone, and N2 plasma. A 10 nm layer of HT-1 doped with 5% NDP-9 was deposited on top of the ITO anode substrate to form a hole injection layer (HIL). A 100 nm layer of HT-1 was evaporated on top of the hole injection layer (HIL) to form a first hole transport layer (HTL). GP-1 was vacuum-deposited on top of the first hole transport layer (HTL) to form a second hole transport layer (GPL) with a thickness of 10 nm. Compound N-1 (N-type) and compound P-19 (P-type) prepared in Example 1 of this disclosure were co-deposited as the light-emitting host material in a 5:5 ratio, and GD-1 was evaporated as a dopant (GD-1 amount was 8% of the total weight of compounds N-1 and P-19) onto the second hole transport layer (GPL) to form a 20 nm thick layer. The process involves: depositing HB-1 onto the light-emitting layer to obtain a hole blocking layer (HBL) with a thickness of 20 nm; co-depositing ET-1 and LiQ in a 5:5 ratio onto the hole blocking layer (HBL) to obtain an electron transport layer (ETL) with a thickness of 30 nm; depositing a mixture of magnesium (Mg) and silver (Ag) in a 9:1 ratio onto the electron transport layer (ETL) to form an electron injection layer (EIL) with a thickness of 50 nm; subsequently depositing silver (Ag) onto the electron injection layer to form a cathode with a thickness of 100 nm; depositing a 50 nm thick DNTPD on the cathode sealing layer; and sealing the cathode surface with a UV-curable adhesive and a sealing cap containing a desiccant to protect the organic electroluminescent device from atmospheric oxygen or moisture. This completes the fabrication of the organic electroluminescent device.
[0075] The structural formulas of the compounds used in each application example are as follows:
[0076] Application Example 2-82:
[0077] Compounds N-3, N-4, N-5, N-7, N-10, N-17, N-30, N-36, N-38, N-40, N-49, N-57, N-59, N- 60. N-68, N-72, N-73, N-77, N-79, N-83, N-96, N-97, N-109, N-113, N-115, N-117, N-1 19. N-120, N-130, N-140, N-143, N-160, N-162, N-165, N-167, N-170, N-175, N-177, N -182, N-183, N-185, N-186, N-189, N-192, N-201, N-206, N-222, N-229, N-235, N-236 , N-244, N-253, N-259, N-262, N-267, N-269, N-307, N-313, N-315, N-320, N-328, N-3 29. N-337, N-339, N-345, N-347, N-351, N-353, N-359, N-361, N-363, N-372, N-379, N Replacing compound N-1 in the application examples with N-387, N-396, N-398, N-404, N-410, N-412, N-418, and N-422 respectively, and using them together with P-type compounds P-19 or P-40 as the light-emitting host material of the green light device by vapor deposition, the organic electroluminescent devices of application examples 2-82 were fabricated under the same conditions as application example 1.
[0078] Compare with Examples 1-5:
[0079] Compound N-1 in the application examples was replaced with control compounds D-1, D-2, D-3, D-4, and D-5, respectively. These compounds, along with compounds P-19 or P-40, were used as the main light-emitting materials for green light devices and were vapor-deposited. Under the same conditions as in application example 1, organic electroluminescent devices of control examples 1-5 were fabricated accordingly.
[0080] At a current density of 10 mA / cm 2 The characteristics of the organic electroluminescent devices manufactured under the application examples and the organic electroluminescent devices manufactured under the control examples were tested under the following conditions. The test results are shown in Tables 3-1, 3-2, 3-3, 3-4, and 3-5:
[0081] Table 3-1
[0082] Table 3-2
[0083] Table 3-3
[0084] Table 3-4
[0085] Table 3-5
[0086] As shown in Tables 3-1, 3-2, 3-3, 3-4, and 3-5, under the same current density, the N-type compound provided in this disclosure, when applied to organic electroluminescent devices and combined with a P-type compound with a deuterated core region, significantly improves the luminous efficiency of the device compared to existing compounds, reduces the device's start-up voltage to varying degrees, and relatively lowers the device's power consumption.
[0087] The organic electroluminescent devices prepared in Comparative Examples 1-5 and some application examples were subjected to luminescence lifetime tests at a current density of 10 mA / cm². 2 Under the test conditions, the luminescence lifetime T97% data (the time for the luminescence brightness to decrease to 97% of the initial brightness) was obtained. The test results are shown in Table 4 (with the lifetime data of Control Example 1 as a reference):
[0088] Table 4
[0089] As shown in the table above, when the N-type compound and the comparative compound provided in this disclosure are applied to organic electroluminescent devices in the same manner, under the same current density and other parameter conditions, the lifespan of the device in the application example of this disclosure is significantly improved compared to the comparative example.
[0090] Table 5. HPLC chromatographic data of compounds N-1, N-3, and N-60 disclosed herein. Industrial applicability
[0091] In this disclosure, the electron-rich groups consisting of carbazole and the phenyl group linked to it are replaced by deuterium in the N-type compound structure. Combined with the deuterated P-type compound in the core region, this effectively improves the chemical, photoelectric, and thermal stability of the luminescent material structure, thereby enhancing the stability and lifespan of the luminescent devices using this material. Simultaneously, this N-type compound can form a premix material with the P-type compound, resulting in a more balanced carrier mobility, which significantly improves the efficiency and lifespan of the device, demonstrating industrial application value.
Claims
1. An organic electroluminescent compound, characterized by The structural formula is shown in the following formula (1): wherein: R0 to R7 each independently represent deuterium, deuterium-substituted or unsubstituted C6-C30 aryl, provided that at least seven of R0 to R7 are deuterium; R8-R 11 each independently represents hydrogen, deuterium, deuterium-substituted or unsubstituted C6-C30 aryl, provided that at least one of R8-R 11 is deuterium; L1 and L2 each independently represent a single bond; Ar1and Ar2, which are identical or different, represent a substituted or unsubstituted C6-C30aryl group, with the proviso that when any one of R0-R 11 at least one of Ar1and Ar2is a substituted or unsubstituted biphenyl group, provided that when any one of R0-R the substituents of Ar1 and Ar2 each independently are selected from one or more, or a combination of a plurality of, deuterium, cyano, C6-C20 aryl, deuterium-substituted C6-C20 aryl, C5-C20 heteroaryl, C1-C4 linear or branched alkyl, deuterium-substituted C1-C4 linear or branched alkyl.
2. The organic electroluminescent compound according to claim 1, wherein: Ar1 and Ar2 each independently represent a substituted or unsubstituted phenyl or biphenyl; and the substituents of Ar1 and Ar2 each independently are selected from one or more of deuterium, methyl, phenyl, deuterium-substituted methyl, deuterium-substituted phenyl.
3. The organic electroluminescent compound according to claim 1, wherein R8-R 11 In particular, R8or R 10 is a C6-C30aryl group which is substituted by deuterium or unsubstituted, and at least one of the remaining three R groups is deuterium.
4. The organic electroluminescent compound according to claim 1, wherein seven R groups in R0 to R7 are deuterium, and the other group other than deuterium is phenyl or deuterium-substituted phenyl.
5. The organic electroluminescent compound according to claim 1, wherein selected from the group consisting of:
6. An organic electroluminescent device, characterized by An organic electroluminescent device including a first electrode, a second electrode, and an organic layer formed between the first electrode and the second electrode, the organic layer containing the organic electroluminescent compound according to any one of claims 1 to 5.
7. The organic electroluminescent device according to claim 6, wherein The organic layer includes a hole injection layer, a first hole transport layer, a second hole transport layer, a light-emitting layer, a hole blocking layer, an electron transport layer, and an electron injection layer, and the light-emitting layer contains the organic electroluminescent compound according to any one of claims 1 to 5.
8. The organic electroluminescent device according to claim 7, wherein The light-emitting layer contains a light-emitting host material, the light-emitting host material is composed of a first compound and a second compound, the first compound is an organic electroluminescence compound according to any one of claims 1-5, and the second compound has a structure represented by formula (2-1) or formula (2-2): wherein: L3, L4, L5, and L6 each independently represent a single bond, or a C6-C20 arylene group which is substituted with deuterium or unsubstituted; Ar5, Ar6, Ar3, and Ar4 each independently represent a substituted or unsubstituted C6-C30 aryl group, or a substituted or unsubstituted C5-C30 heteroaryl group; and the substituents of Ar5, Ar6, Ar3, and Ar4 each independently are selected from deuterium, a C6-C20 aryl group which is substituted with deuterium or unsubstituted; R 12 and R 13 is deuterium, m1 is an integer selected from 0-3, m2 is an integer selected from 0-4, and n is an integer selected from 0-4.
9. The organic electroluminescent device according to claim 8, wherein: L3, L4, L5, and L6 each independently are a single bond, a phenylene group, or a deuterium-substituted phenylene group; and Ar5, Ar6, Ar3, and Ar4 each independently are a substituted or unsubstituted phenyl group, a biphenyl group, a naphthyl group, an anthryl group, a phenanthryl group, a phenanthrenyl group, or an N-containing heteroaryl group, and the substituents of Ar5, Ar6, Ar3, and Ar4 are selected from one or more of deuterium, a phenyl group, and a deuterium-substituted phenyl group.