Fatigue hysteresis loop prediction method, equipment and product for laminated ceramic matrix composites
By constructing the fiber axial stress distribution equation and the fracture mechanics interface debonding criterion, the fatigue load interface debonding and slip length equations are established, which solves the problem of insufficient prediction accuracy of the fatigue hysteresis loop of laminated ceramic matrix composites, and realizes the matrix The consideration of cracking and interface debonding factors provides effective monitoring of composite damage.
Patent Information
- Application Number
- CN202410961521.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-18
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2044-07-18
AI Technical Summary
The existing technology lacks research on the fatigue hysteresis loop of laminated ceramic matrix composites, especially the insufficient prediction accuracy under the influence of matrix cracking and interface debonding factors, making it difficult to effectively monitor the damage of composite materials caused by fatigue loads.
By constructing the unloading and reloading fiber axial stress distribution equation, the fracture mechanics interface debonding criterion is established, the fatigue load interface debonding and slip length equation is established, and then the fatigue hysteresis loop stress-strain relationship equation is established to accurately predict the laminated ceramic substrate. Fatigue hysteresis loop of composite materials.
It improves the prediction accuracy of the fatigue hysteresis loop of laminated ceramic matrix composites, provides an effective basis for monitoring the damage caused by fatigue load to composite materials, and enhances the reliability and safety of the structure.
Smart Images

Figure CN118506940B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of electrical digital data processing, and in particular to a method, equipment and product for predicting fatigue hysteresis loop of a laminated ceramic-based composite material. Background Art
[0002] Ceramic-based composites have the advantages of high temperature resistance, corrosion resistance, low density, high specific strength, and high specific modulus. Compared with high-temperature alloys, they can withstand higher temperatures, reduce cooling airflow, and improve turbine efficiency. They have been used in aircraft engine combustion chambers, turbine guide vanes, turbine casing rings, tail nozzles, etc. The LEAP (LeadingEdge Aviation Propulsion) series engines developed by CFM use ceramic-based composite components in their high-pressure turbines. The LEAP-1B engine provides power for the Airbus A320 and Boeing 737MAX.
[0003] In order to ensure the reliability and safety of ceramic matrix composites used in aircraft and aero-engine structures, the Federal Aviation Administration of the United States regards the development of ceramic matrix composite performance evaluation, damage evolution, strength and life prediction tools as the key to the airworthiness certification of ceramic matrix composite structural components. Under fatigue loads, laminated ceramic matrix composites experience multiple damage mechanisms such as matrix cracking, fiber / matrix interface debonding and slippage, resulting in obvious hysteresis in the stress-strain curve during unloading and reloading. The shape, position and area of the hysteresis loop can reflect the damage evolution inside the laminated ceramic matrix composite, and is a key technical means to monitor internal damage in laminated composites.
[0004] Currently, there is a lack of research on the fatigue hysteresis loop of laminated ceramic matrix composites. How to consider the influence of matrix cracking and interface debonding on the fatigue hysteresis loop of laminated ceramic matrix composites and monitor the damage caused by fatigue loads to composites are key technical issues that need to be solved in the actual engineering application of laminated ceramic matrix composite structures. Summary of the invention
[0005] The purpose of the present invention is to provide a method, equipment and product for predicting the fatigue hysteresis loop of a laminated ceramic matrix composite material, so as to improve the prediction accuracy of the fatigue hysteresis loop of the laminated ceramic matrix composite material under the condition of considering the factors of matrix cracking and interface debonding, thereby providing an effective basis for monitoring the damage caused by fatigue load to the composite material.
[0006] To achieve the above object, the present invention provides the following solutions:
[0007] A method for predicting fatigue hysteresis loop of a laminated ceramic matrix composite material, the method comprising:
[0008] The fiber axial stress distribution equations during unloading and reloading are constructed, and the microscopic stress field of the laminated ceramic matrix composite material after damage is obtained based on the fiber axial stress distribution equations during unloading and reloading; the fiber axial stress distribution equations during unloading and reloading include: the fiber axial stress distribution equation during unloading and the fiber axial stress distribution equation during reloading;
[0009] Based on the interface debonding criterion of fracture mechanics, the interface debonding and slip length equations of laminated ceramic matrix composite materials under fatigue load are established; the interface debonding and slip length equations of laminated ceramic matrix composite materials under fatigue load include: the reverse length equation of unloading interface and the slip length equation of reloading new interface;
[0010] Based on the microscopic stress field of the laminated ceramic matrix composite after damage, the interface debonding and slip length of the laminated ceramic matrix composite under fatigue load are obtained by using the interface debonding and slip length equation of the laminated ceramic matrix composite under fatigue load.
[0011] Establish the stress-strain relationship equation of fatigue hysteresis loop of laminated ceramic matrix composites;
[0012] Based on the slip length and the microscopic stress field of the laminated ceramic matrix composite material after damage, the fatigue hysteresis loop of the laminated ceramic matrix composite material is predicted by using the stress-strain relationship equation of the fatigue hysteresis loop of the laminated ceramic matrix composite material.
[0013] Optionally, the fiber axial stress distribution equation during unloading is expressed as:
[0014] ;
[0015] ;
[0016] In the formula, Half the thickness of the 0° ply. Half the thickness of the 90° ply. is the fiber volume content, For Axial stress of the ply at 90°, is the fiber / matrix interface shear stress, is the matrix crack spacing, is the interfacial debonding length at the right of the feature element, is the interfacial debonding length at the left of the feature element, is the reverse slip length of the unloading interface at the right of the feature element, is the reverse slip length of the unloading interface at the left of the feature element, is the transverse crack spacing of the 90° layer, and are damage parameters. is the fiber radius, , and are shear lag model parameters, is the fiber axial stress, is the transverse coordinate of the 90° ply, is the fiber axial stress in the interface bonding zone, is the lateral coordinate of the 0o ply, For stress.
[0017] Alternatively, the fiber axial stress distribution equation during reloading is expressed as:
[0018] ;
[0019] ;
[0020] In the formula, is the new sliding length of the reload interface at the right of the feature element, is the new slip length of the reload interface at the left side of the feature element.
[0021] Alternatively, the fracture mechanics interface debonding criterion is expressed as:
[0022] ;
[0023] ;
[0024] In the formula, is the interfacial debonding energy, is the fiber axial displacement at the matrix crack plane, is the axial displacement of the fiber relative to the matrix, The fibers in the matrix crack plane bear the load.
[0025] Optionally, the unloading interface reverse length equation is expressed as:
[0026] ;
[0027] ;
[0028] In the formula, is the matrix elastic modulus, is the axial elastic modulus of the 0° ply, is the lossless axial stress of the 90° ply, is the fiber elastic modulus, is the matrix volume content.
[0029] Optionally, the reloading new interface slip length equation is expressed as:
[0030] ;
[0031] .
[0032] Optionally, the stress-strain relationship equation of the fatigue hysteresis loop of the laminated ceramic matrix composite material is expressed as:
[0033] ;
[0034] ;
[0035] In the formula, To unload the strain, To reload the strain, is the thermal residual strain.
[0036] A computer device comprises: a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor executes the computer program to implement any of the above-mentioned methods for predicting fatigue hysteresis loops of laminated ceramic matrix composite materials.
[0037] A computer-readable storage medium stores a computer program, which, when executed by a processor, implements any of the above-mentioned methods for predicting fatigue hysteresis loops of laminated ceramic matrix composite materials.
[0038] A computer program product comprises a computer program, which, when executed by a processor, implements any of the above-mentioned methods for predicting fatigue hysteresis loops of laminated ceramic matrix composite materials.
[0039] According to the specific embodiments provided by the present invention, the present invention discloses the following technical effects:
[0040] The present invention obtains the microscopic stress field of the laminated ceramic matrix composite material after damage by establishing the axial stress distribution equation of the fiber under unloading and reloading. The interface debonding and slip length equation of the laminated ceramic matrix composite material under fatigue load is established based on the interface debonding criterion of fracture mechanics to obtain the interface debonding and slip length of the laminated ceramic matrix composite material under fatigue load. Under the condition of considering the factors of matrix cracking and interface debonding, by establishing the stress-strain relationship equation of the fatigue hysteresis loop of the laminated ceramic matrix composite material, the fatigue hysteresis loop of the laminated ceramic matrix composite material is predicted more accurately, thereby providing an effective basis for monitoring the damage caused by fatigue load to the composite material. BRIEF DESCRIPTION OF THE DRAWINGS
[0041] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0042] Figure 1 A flow chart of a fatigue hysteresis loop prediction method for a laminated ceramic matrix composite material provided in an embodiment of the present invention;
[0043] Figure 2 A schematic diagram of the prediction results of the hysteresis loop of a laminated ceramic matrix composite material under fatigue load provided in an embodiment of the present invention. DETAILED DESCRIPTION
[0044] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0045] The purpose of the present invention is to provide a method, equipment and product for predicting the fatigue hysteresis loop of a laminated ceramic matrix composite material, aiming to improve the prediction accuracy of the fatigue hysteresis loop of a laminated ceramic matrix composite material under the conditions of considering the factors of matrix cracking and interface debonding, thereby providing an effective basis for monitoring the damage caused to the composite material by fatigue load.
[0046] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, the present invention is further described in detail below with reference to the accompanying drawings and specific embodiments.
[0047] Example 1
[0048] This embodiment provides a method for predicting fatigue hysteresis loop of a laminated ceramic matrix composite material. Figure 1 As shown, the method includes:
[0049] Step 100: Construct the unloading and reloading fiber axial stress distribution equation, and obtain the microscopic stress field of the laminated ceramic matrix composite material after damage based on the unloading and reloading fiber axial stress distribution equation. This unloading and reloading fiber axial stress distribution equation is mainly constructed based on the fatigue damage microscopic stress field of the laminated ceramic matrix composite material, which includes: the fiber axial stress distribution equation during unloading and the fiber axial stress distribution equation during reloading. Among them, the fiber axial stress distribution equation during unloading is expressed as:
[0050] .
[0051] .
[0052] In the formula, Half the thickness of the 0° ply. Half the thickness of the 90° ply. is the fiber volume content, For Axial stress of the ply at 90°, is the fiber / matrix interface shear stress, is the matrix crack spacing, is the interfacial debonding length at the right of the feature element, is the interfacial debonding length at the left of the feature element, is the reverse slip length of the unloading interface at the right of the feature element, is the reverse slip length of the unloading interface at the left of the feature element, is the transverse crack spacing of the 90° layer, and are damage parameters. is the fiber radius, , and are shear lag model parameters, is the fiber axial stress, is the transverse coordinate of the 90° ply, is the fiber axial stress in the interface bonding zone, is the lateral coordinate of the 0o ply, For stress.
[0053] The fiber axial stress distribution equation during reloading is expressed as:
[0054] .
[0055] .
[0056] In the formula, is the new sliding length of the reload interface at the right of the feature element, is the new slip length of the reload interface at the left side of the feature element.
[0057] Step 101: Based on the fracture mechanics interface debonding criterion, establish the interface debonding and slip length equation of the laminated ceramic matrix composite material under fatigue loading. The interface debonding and slip length equation of the laminated ceramic matrix composite material under fatigue loading includes: an unloading interface reverse length equation and a reloading new interface slip length equation.
[0058] The fracture mechanics interface debonding criterion is expressed as:
[0059] .
[0060] .
[0061] In the formula, is the interfacial debonding energy, is the fiber axial displacement at the matrix crack plane, is the axial displacement of the fiber relative to the matrix, The fibers in the matrix crack plane bear the load.
[0062] The unloading interface reverse length equation is expressed as:
[0063] .
[0064] .
[0065] In the formula, is the matrix elastic modulus, is the axial elastic modulus of the 0° ply, is the lossless axial stress of the 90° ply, is the fiber elastic modulus, is the matrix volume content.
[0066] Optionally, reload the new interface slip length equation as:
[0067] .
[0068] .
[0069] Step 102: Based on the microscopic stress field of the laminated ceramic matrix composite material after damage, the laminated ceramic matrix composite material fatigue load interface debonding and slip length equation is used to obtain the laminated ceramic matrix composite material fatigue load interface debonding and slip length.
[0070] Step 103: Establishing a stress-strain relationship equation of a fatigue hysteresis loop of a laminated ceramic matrix composite material. The stress-strain relationship equation of a fatigue hysteresis loop of a laminated ceramic matrix composite material is expressed as:
[0071] .
[0072] .
[0073] In the formula, To unload the strain, To reload the strain, is the thermal residual strain.
[0074] Step 104: Based on the slip length and the microscopic stress field of the laminated ceramic matrix composite material after damage, the fatigue hysteresis loop of the laminated ceramic matrix composite material is predicted using the stress-strain relationship equation of the fatigue hysteresis loop of the laminated ceramic matrix composite material. The predicted hysteresis loop of the laminated ceramic matrix composite material under fatigue load is as follows: Figure 2 shown. Figure 2 The N in represents the fatigue load.
[0075] Based on the above description, the fatigue hysteresis loop prediction method of laminated ceramic matrix composite materials provided by the present invention calculates the strain of unloading and reloading the laminated ceramic matrix composite materials by introducing parameters such as matrix crack spacing and interface debonding length, so as to predict the fatigue hysteresis loop, thereby providing a strong basis for monitoring the damage evolution of laminated ceramic matrix composite materials under fatigue load.
[0076] Example 2
[0077] A computer device includes: a memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor executes the computer program to implement the fatigue hysteresis loop prediction method for laminated ceramic matrix composite materials in Example 1.
[0078] Example 3
[0079] A computer-readable storage medium stores a computer program, which, when executed by a processor, implements the fatigue hysteresis loop prediction method for a laminated ceramic matrix composite material in Example 1.
[0080] Example 4
[0081] A computer program product includes a computer program, which, when executed by a processor, implements the method for predicting fatigue hysteresis loop of a laminated ceramic matrix composite material in embodiment 1.
[0082] Example 5
[0083] A computer device, which can be a database. The computer device includes a processor, a memory, an input / output interface (Input / Output, referred to as I / O) and a communication interface. Wherein, the processor, the memory and the input / output interface are connected via a system bus, and the communication interface is connected to the system bus via the input / output interface. Wherein, the processor of the computer device is used to provide computing and control capabilities. The memory of the computer device includes a non-volatile storage medium and an internal memory. The non-volatile storage medium stores an operating system, a computer program and a database. The internal memory provides an environment for the operation of the operating system and the computer program in the non-volatile storage medium. The database of the computer device is used to store pending transactions. The input / output interface of the computer device is used to exchange information between the processor and an external device. The communication interface of the computer device is used to communicate with an external terminal via a network connection. When the computer program is executed by the processor, the fatigue hysteresis loop prediction method of the laminated ceramic matrix composite material in Example 1 is implemented.
[0084] It should be noted that the object information (including but not limited to object device information, object personal information, etc.) and data (including but not limited to data used for analysis, stored data, displayed data, etc.) involved in the present invention are all information and data authorized by the object or fully authorized by all parties, and the collection, use and processing of relevant data must comply with relevant laws, regulations and standards of relevant countries and regions.
[0085] Those skilled in the art can understand that all or part of the processes in the above-mentioned embodiments can be completed by instructing the relevant hardware through a computer program, and the computer program can be stored in a non-volatile computer-readable storage medium. When the computer program is executed, it can include the processes of the embodiments of the above-mentioned methods. Among them, any reference to the memory, database or other medium used in the embodiments provided by the present invention can include at least one of non-volatile and volatile memory. Non-volatile memory can include read-only memory (ROM), magnetic tape, floppy disk, flash memory, optical memory, high-density embedded non-volatile memory, resistive random access memory (ReRAM), magnetoresistive random access memory (MRAM), ferroelectric random access memory (FRAM), phase change memory (PCM), graphene memory, etc. Volatile memory can include random access memory (RAM) or external cache memory, etc. As an illustration and not limitation, RAM can be in various forms, such as static random access memory (SRAM) or dynamic random access memory (DRAM). The database involved in each embodiment provided by the present invention may include at least one of a relational database and a non-relational database. Non-relational databases may include distributed databases based on blockchains, etc., but are not limited to this. The processor involved in each embodiment provided by the present invention may be a general-purpose processor, a central processing unit, a graphics processor, a digital signal processor, a programmable logic device, a data processing logic device based on quantum computing, etc., but are not limited to this.
[0086] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.
[0087] The principles and implementation methods of the present invention are described in this article using specific examples. The description of the above embodiments is only used to help understand the method and core ideas of the present invention. The same and similar parts between the embodiments can be referred to each other. At the same time, for those skilled in the art, according to the ideas of the present invention, there will be changes in the specific implementation methods and application scope. In summary, the content of this specification should not be understood as limiting the present invention.
Claims
1. A method for predicting fatigue hysteresis loop of laminated ceramic matrix composite materials, characterized in that: The method comprises: Step 100: constructing an unloading and reloading fiber axial stress distribution equation, and obtaining a microscopic stress field of the laminated ceramic matrix composite material after damage based on the unloading and reloading fiber axial stress distribution equation; the unloading and reloading fiber axial stress distribution equation includes: an unloading fiber axial stress distribution equation and a reloading fiber axial stress distribution equation; The fiber axial stress distribution equation during unloading is expressed as: ; ; In the formula, Half the thickness of the 0° ply. Half the thickness of the 90° ply. is the fiber volume content, For Axial stress of the ply at 90°, is the fiber / matrix interface shear stress, is the matrix crack spacing, is the interfacial debonding length at the right of the feature element, is the interfacial debonding length at the left of the feature element, is the reverse slip length of the unloading interface at the right of the feature element, is the reverse slip length of the unloading interface at the left of the feature element, is the transverse crack spacing of the 90° layer, and are damage parameters. is the fiber radius, , and are shear lag model parameters, is the fiber axial stress, is the transverse coordinate of the 90° ply, is the fiber axial stress in the interface bonding zone, is 0 o The transverse coordinate of the ply, for stress; The fiber axial stress distribution equation during reloading is expressed as: ; ; In the formula, is the new sliding length of the reload interface at the right of the feature element, is the new slip length of the reload interface at the left of the feature element; Step 101: Based on the fracture mechanics interface debonding criterion, establish the interface debonding and slip length equation of the laminated ceramic matrix composite material under fatigue load; the interface debonding and slip length equation of the laminated ceramic matrix composite material under fatigue load includes: an unloading interface reverse length equation and a reloading new interface slip length equation; the fracture mechanics interface debonding criterion is expressed as: ; ; In the formula, is the interfacial debonding energy, is the fiber axial displacement at the matrix crack plane, is the axial displacement of the fiber relative to the matrix, The fibers in the matrix crack plane bear the load; The unloading interface reverse length equation is expressed as: ; ; In the formula, is the matrix elastic modulus, is the axial elastic modulus of the 0° ply, is the lossless axial stress of the 90° ply, is the fiber elastic modulus, is the matrix volume content; The reloaded new interface slip length equation is expressed as: ; ; Step 102: Based on the microscopic stress field of the laminated ceramic matrix composite material after damage, the laminated ceramic matrix composite material fatigue load interface debonding and slip length equation is used to obtain the laminated ceramic matrix composite material fatigue load interface debonding and slip length; Step 103: Establishing a stress-strain relationship equation of a fatigue hysteresis loop of a laminated ceramic matrix composite material; the stress-strain relationship equation of a fatigue hysteresis loop of a laminated ceramic matrix composite material is expressed as: ; ; In the formula, To unload the strain, To reload the strain, is the thermal residual strain; Step 104: Based on the slip length and the microscopic stress field of the laminated ceramic matrix composite material after damage, a fatigue hysteresis loop stress-strain relationship equation of the laminated ceramic matrix composite material is used to complete the prediction of the fatigue hysteresis loop of the laminated ceramic matrix composite material.
2. A computer device comprising: A memory, a processor, and a computer program stored in the memory and executable on the processor, wherein the processor executes the computer program to implement the fatigue hysteresis loop prediction method for laminated ceramic matrix composite materials as described in claim 1.
3. A computer-readable storage medium having a computer program stored thereon, characterized in that: When the computer program is executed by a processor, the fatigue hysteresis loop prediction method of the laminated ceramic matrix composite material described in claim 1 is implemented.
4. A computer program product, comprising a computer program, characterized in that When the computer program is executed by a processor, the fatigue hysteresis loop prediction method of the laminated ceramic matrix composite material described in claim 1 is implemented.