Simulation test method for on-site stray current corrosion environment of tower grounding body

Through computer simulation technology and the improved Miller box simulation platform, combined with electrochemical detection, the problem that the existing technology cannot accurately simulate the soil environment is solved, and accurate monitoring and early warning of the corrosion conditions of grounding conductors is achieved, and the time efficiency of corrosion detection is improved. Sex and accuracy.

CN118961565APending Publication Date: 2024-11-15STATE GRID GANSU ELECTRIC POWER RESEARCH INSTITUTE +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411418048.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-11
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

The prior art cannot accurately simulate the corrosion of the grounding conductors of the transmission line pole tower in the soil, and it is difficult to completely reproduce the soil environment in solution tests, resulting in the corrosion rate and product migration situation that do not match the actual situation, and lack of convenient on-site detection methods.

Method used

Computer simulation technology is used to evaluate the leakage current density distribution of grounding systems, and an improved version of Miller box and electrochemical detection platform is built, combining soil oxygen content, moisture and temperature sensors to simulate the on-site corrosion environment through a controllable DC current source, monitoring and Adjust the corrosion reaction rate of the specimen.

Benefits of technology

It realizes accurate dynamic monitoring and early warning of the corrosion conditions of grounded conductors, improves the timeliness of corrosion monitoring, provides simulation test results close to the on-site corrosion environment, and facilitates verification of anti-corrosion materials and measures of grounded conductors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118961565A_ABST
    Figure CN118961565A_ABST
Patent Text Reader

Abstract

The invention provides a simulation test method for an on-site stray current corrosion environment of a tower grounding body, which comprises the following steps: monitoring ground stray current to obtain leakage current density distribution Ji, selecting a central point of each branch as a test point, monitoring parameters of the corrosion environment of each branch, including soil oxygen content, pH value, moisture content and temperature parameter, and calculating the corrosion environment of each branch according to the parameters. And taking back the soil sample at the central point of each branch, building a simulation test platform of the stray current corrosion environment, monitoring the electrochemical potential change of the test piece by using a Miller box of an improved version, calculating the corrosion rate of the test piece, and carrying out a simulation test of the stray current corrosion environment. The method has the beneficial effects that the method for monitoring the corrosion environment parameters is provided, change data of the corrosion environment is accurately and dynamically tracked, and the simulation test platform can carry out a long-time corrosion simulation test to monitor the change of the corrosion parameters.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to a grounding body corrosion detection technology, and relates to a simulation of an on-site stray current corrosion environment of a tower grounding body. Background Art

[0002] The grounding conductors of transmission line towers are mostly made of steel and buried in the soil for many years, which is prone to electrolytic corrosion of the metal. The grounding resistance of the grounding conductor of the line tower is related to the lightning strike back overvoltage of the line and is an important factor affecting the line strike back tripping rate. The corrosion status of the tower grounding conductor can only be analyzed through excavation inspection at present, but the number of tower grounding bodies in the project is extremely large, and large-scale excavation inspection on site is not practical. Therefore, more convenient and effective transmission line tower grounding conductor corrosion detection methods and test methods are needed.

[0003] Conducting corrosion tests on grounding conductors of transmission line towers in the laboratory is currently a feasible engineering research method. On the one hand, the tests in the laboratory have a certain degree of credibility and can simulate corrosion factors more accurately to evaluate the corrosion rate and remaining life of the grounding conductor. On the other hand, the relevant corrosion simulation test platform can provide a simulation test environment for new anti-corrosion materials and new measures for grounding conductors, thereby verifying the application effect of new anti-corrosion materials and new measures.

[0004] At present, the electrochemical corrosion detection industry mostly uses the method of placing grounding conductors in corrosion solutions to simulate the influence of the soil environment (including pH value, oxygen content, resistivity, electrolyte composition and other factors) of the grounding grid on the corrosion rate of the grounding conductor. The current research method has the following disadvantages: First, the solution corrosion test method is different from the actual situation where the soil water content is not high. The oxygen content in the solution is different from the oxygen content in the soil. The soil has a loose structure, so the oxygen content is high, which has the effect of accelerating corrosion. Second, it is difficult to completely simulate the physical and chemical composition of the soil in the solution. The soil includes complex components such as soluble salts and insoluble salts. The migration and dissolution of steel conductor corrosion products in the soil are also different from the corrosion in the solution. Based on the current research situation, the solution test method in the laboratory cannot accurately simulate the corrosion of the grounding conductor of the transmission line tower in the soil. Summary of the invention

[0005] The purpose of the present invention is to provide a simulation test method for the on-site stray current corrosion environment of a tower grounding body, so as to obtain corrosion observation results close to those in the field.

[0006] The technical solution of the present invention is a simulation test method for the on-site stray current corrosion environment of a tower grounding body. The first step is to detect the ground current of the tower grounding body, and then use computer simulation technology to evaluate the leakage current density distribution at different positions of the grounding system. 1.1 Use flexible stray current sensors to continuously monitor the stray current entering the ground of the tower grounding body; 1.2 Separate all the conductor branches of the tower grounding body { L}, assuming there is B branch road; 1.3 Separate all conductor nodes of the tower grounding body { E}, assuming there is N nodes, and the node injection current column vector [ F ]; 1.4 Calculate the correlation matrix of the tower grounding body from the conductor branches and conductor nodes [ K ] and its transposed matrix [ K T ]; Correlation Matrix[ K ]for N × B Order matrix, incidence matrix[ K ] is the transposed matrix [ K T ]for B × N If the matrix i #Node and j #Branches are associated, then [ K ] i,j = [ K T ] j,i = 0.5, temporary integer variable i =1,2,…,N,j=1,2,…,N like i #Node and j # If the branches are not related, then [ K ] i,j = [ K T ] j,i = 0; Temporary integer variable i =1, 2, ..., N, temporary integer variable j = 1, 2, ..., N; The association criteria between nodes and branches are: If the distance between the three-dimensional coordinates of the starting point of the branch and the three-dimensional coordinates of the node is less than 0.01m, the node and the branch are considered to be associated; if the distance between the three-dimensional coordinates of the end point of the branch and the three-dimensional coordinates of the node is less than 0.01m, the node and the branch are considered to be associated; otherwise, the node and the branch are not associated.

[0007] 1.5 Solve the mutual resistance matrix [ M ] Mutual resistance matrix[ M ]for B ×B The diagonal elements of the matrix are (1) in, ρ is the equivalent earth resistivity, L i For the i The length of the conductor, a i is the radius of the conductor, dist is the function for finding the distance, for L i Mirror image, [ M ]The off-diagonal elements are (2) in, ρ is the equivalent earth resistivity, L i For the i The length of the conductor, L j For the j The length of the conductor, dist is the function of finding the distance, for L j Mirror image of, temporary integer variable j =1, 2, …, N; 1.6 Solve for the node voltage column vector [ V ] Node voltage column vector[ V ]for N The order column vector is obtained by solving the following equation: 1.7 Solve for the branch leakage current column vector [ I ] Branch leakage current column vector [ I ]for N The order column vector is calculated as follows: 1.8 Obtain the leakage current density distribution at different locations of the grounding system For conductor L i , the leakage current density distribution is the leakage current divided by the conductor surface area, thus obtaining the leakage current density distribution J i ; Temporary integer variable i =1, 2,…, N.

[0008] Step 2: Monitor the parameters of the corrosion environment of each branch 2.1 Select the center point of each branch as the test point, and install an electrochemical oxygen sensor and an integrated soil pH-moisture-temperature sensor 20 cm above the conductor; 2.2 Continuously monitor and transmit the parameters of the corrosion environment every 1 minute, including soil oxygen content, pH value, moisture content, and temperature parameters.

[0009] Step 3: Take soil samples from the center of each branch and build a simulation test platform for stray current corrosion environment 3.1 Take back sufficient soil samples from the center point of each branch; 3.2 A square test piece is made of a plate made of the same material as the grounding body. The welding area of ​​the insulated signal line connected to the test piece is encapsulated with epoxy resin. The number of test pieces is 16 times the number of test points. 3.3 The number of the improved version of the Miller box is the same as the number of measuring points. The inner core of the Miller box is a graphite electrode, and the outer shell is a stainless steel conductor. There are two capillaries between the outer shell and the graphite electrode, which are used to adjust the soil moisture and oxygen content. 3.4 The improved version of the Miller box is divided into four layers, each layer contains the test piece, soil oxygen sensor, pH sensor, moisture sensor, temperature sensor, soil sample, and a platinum wire electrode is arranged 2 cm near the test piece; The test piece is installed 10 cm away from the outer shell. The upper and lower covers of the Miller box are encapsulated by non-conductive insulating materials, and the insulated signal wires, as well as the signal wires of the soil oxygen sensor, pH sensor, moisture sensor, temperature sensor and platinum wire electrode are led out; 3.5 The insulated signal line and the signal line of the platinum wire electrode are connected to the electrochemical workstation, which monitors the change of the electrochemical potential of the test piece and calculates the corrosion rate of the test piece.

[0010] Step 4: Conduct a simulation test of the stray current corrosion environment 4.1 Miller cell connected to a controllable DC current source The core rod of the Miller box is connected to the positive electrode of the current source, and the stainless steel shell is connected to the negative electrode of the current source; 4.2 Leakage current surface density distribution J i Adjusting the output current of a controllable DC power supply I oi , I oi It is derived from the following formula: , a temporary integer variable i =1,2,…,B 4.3 Adjust the gas volume in the capillary tube according to the test data of the oxygen content of the soil on site. If the test result of the oxygen content in the Miller box is less than the situation on site, oxygen is introduced into the capillary tube to increase the oxygen content of the soil sample. On the contrary, if the test result of the oxygen content in the Miller box is greater than the situation on site, inert gas is introduced into the capillary tube to reduce the oxygen content of the soil sample. 4.4 Adjust the deionized water output of the capillary according to the test data of the soil moisture content on site. If the moisture content test result in the Miller box is less than the on-site situation, deionized water is introduced into the capillary to increase the moisture content of the soil sample. Conversely, if the moisture content test result in the Miller box is greater than the on-site situation, dry air is introduced into the capillary to reduce the moisture content of the soil sample. 4.5 The insulated signal wire of the specimen and the signal wire of the platinum wire electrode are connected to the electrochemical workstation, which gives the corrosion reaction rate of each specimen; 4.6 Perform real-time corrosion rating based on the corrosion reaction rate of each specimen given by the electrochemical workstation; Record the corrosion rate of 16 specimens in the same Miller box; the unit of corrosion rate is g / (dm 2 ﹒ a).

[0011] Step 5: Continue to conduct simulated corrosion tests and conduct corrosion warnings 5.1 Real-time corrosion rating at 1-minute intervals; 5.2 Corrosion warning is carried out by simulated corrosion test. If the corrosion rate classification is above a certain level for a certain period of time, a corresponding predetermined warning signal will be issued; 5.3 Every other year, all specimens are taken out of the Miller box for surface corrosion product analysis, scanning electron microscopy analysis, and weight loss measurement. The data are collated to give the annual average corrosion rate of different locations of the grounding conductor.

[0012] Preferably, the overall height of the Miller box is 500 mm, the graphite electrode is Φ100 mm, and the outer shell diameter is 300 mm.

[0013] Preferably, the specimen size is 10 mm×10 mm×4 mm.

[0014] Preferably, the height positions of each layer in step 3.4 are 10 cm, 20 cm, 30 cm, and 40 cm.

[0015] The beneficial effects of the present invention are as follows: 1. An analytical method for evaluating the distribution of leakage current density at different positions of a grounding system using computer simulation technology is proposed to determine the position of the maximum corrosion rate of the grounding conductor; 2. From the perspective of on-site corrosion environment detection, the center point of each branch is selected as the test point, and a method for monitoring corrosion environment parameters is proposed to accurately and dynamically track the changing data of the corrosion environment; 3. Build a simulation test platform for stray current corrosion environment with "improved version of Miller box + electrochemical detection platform + soil oxygen content, moisture content, temperature control system + controllable DC current source", which can carry out long-term corrosion simulation tests and monitor changes in corrosion parameters; 4. The corrosion amount is rated by the corrosion reaction rate of each specimen, which greatly improves the timeliness of corrosion monitoring and facilitates ground corrosion early warning. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a schematic diagram of the monitored stray current entering the ground; Figure 2 This is an example diagram of conductor branch numbering; Figure 3 is an example diagram of a conductor node; Figure 4 It is a schematic diagram of the positions of two arbitrarily placed conductors; Figure 5 It is a schematic diagram of the processing scheme of the square specimen; Figure 6 This is a schematic diagram of the improved version of the Miller box structure; Figure 7 This is a schematic diagram of the layer section of the improved version of the Miller box. DETAILED DESCRIPTION

[0017] Definitions of Abbreviations and Key Terms: Tower Grounding Electrode - An interconnected electrical network consisting of metal structures such as steel located underground below the line tower, used for safety protection and lightning protection purposes;

[0018] Stray current refers to abnormal current components found outside the designed path. In this patent, it specifically refers to low-frequency component current with a frequency less than 5Hz. Among them, stray current with an amplitude greater than 0 flowing into the grounding body will cause electrolytic corrosion of the grounding body, while negative current will not.

[0019] A simulation test method for the on-site stray current corrosion environment of a tower grounding body, the technical solution is: The first step is to detect the ground current of the tower grounding body, and then use computer simulation technology to evaluate the leakage current density distribution at different locations of the grounding system. 1.1 Continuously monitor the stray current entering the tower grounding body, as shown in the schematic diagram Figure 1 ,The test device is as follows: a flexible stray current sensor; 1.2 Separate all the conductor branches of the tower grounding body { L} (Assuming there is B branches), see the example diagram Figure 2 ; 1.3 Separate all conductor nodes of the tower grounding body { E} (assuming there is N nodes, see the example diagram Figure 3 ), and the node injection current column vector [ F ]; 1.4 Calculation of the correlation matrix of the tower grounding body from the conductor branches and nodes [ K ] and its transpose[ K T ]; Correlation Matrix[ K ]for N × B Order matrix, incidence matrix[ K ] is the transposed matrix [ K T ]for B × N If i #Node and j #Branches are associated, then [ K ] i,j = [ K T ] j,i = 0.5, temporary integer variable i =1, 2, …, N, j =1,2,…,N like i #Node and j # If the branches are not related, then [ K ] i,j = [ K T ] j,i = 0, temporary integer variable i =1, 2, ..., N, temporary integer variable j =1, 2, …, N; illustrate: i , j , N specifically means an integer, where i and j It is just a reference symbol for a temporary integer variable, N is the total number of nodes; 1.5 Solve the mutual resistance matrix [ M ], Mutual resistance matrix[ M ]for B × B The diagonal elements of the matrix are (1) in, ρ is the equivalent earth resistivity, L i For the i The length of the conductor,a i is the conductor radius, dist is the function for finding the distance, L i Mirror image, [ M ]The off-diagonal elements are (2) in, L j is the length of the conductor, L i For the i The length of the conductor, L j For the j The length of the conductor, dist is the function of finding the distance, which is L j Temporary integer variable j = 1, 2, ..., N; Formulas (1) and (2) involve the double integral of the inverse of the line conductor distance. Figure 4 The two arbitrarily placed conductors shown in FIG. L AB and L EF , the analytical formula for the distance reciprocal double conductor integral is: (3) (4) in, CG yes L AB and L EF The common perpendicular line, and It is a straight line EF In plane S The two endpoints of the projected line segment on the straight line AB The projection on this plane S Through the straight line AB and parallel to the straight line EF of, and The meaning and and Same meaning. θ Non-coplanar straight lines L AB and L EF The angle between the two points. The variables without brackets in the above formula represent the distance between the two points and are taken as positive values. The variables with brackets have the same direction as AB and EF When the directions are consistent, it is positive, otherwise it is negative; Substituting formula (3) and (4) into formula (1) and (2) can complete [ M ] solution; 1.6 Solve for the node voltage column vector [ V ], node voltage column vector [ V ]for N The order column vector is obtained by solving the following equation: (5) 1.7 Solve for the branch leakage current column vector [ I ], Branch leakage current column vector [ I ]for N The order column vector is calculated as follows: (6) 1.8 Obtain the leakage current density distribution at different locations of the grounding system; For conductor L i , the leakage current density distribution is the leakage current divided by the conductor surface area, thus obtaining the leakage current density distribution J i ; Temporary integer variable i =1, 2,…, N.

[0020] Step 2: Select the center point of each branch as the test point to monitor the parameters of the corrosion environment. 2.1 Select the center point of each branch as the test point and install an electrochemical oxygen sensor 20cm above the conductor; 2.2 Select the center point of each branch as the test point and install an integrated soil pH-moisture-temperature sensor 20 cm above the conductor; 2.3 Continuously monitor and transmit the parameters of the corrosion environment every 1 minute, including soil oxygen content, pH value, moisture content, temperature and other parameters.

[0021] Step 3: Take the soil samples from the center of each branch and build a simulation test platform for stray current corrosion environment. 3.1 Take sufficient soil samples (at least 0.01m 3 ); 3.2 The plate of the same material as the grounding body is processed into a 10mm×10mm×4mm square specimen (see Figure 5 ), the number is 16 times the number of test points; 3.3 The number of the improved version of the Miller box is consistent with the number of measuring points. The structural diagram of a single Miller box is shown in Figure 6 ; The overall height of the improved version of the Miller box is 500mm. The inner core of the Miller box is a Φ100 graphite electrode, and the outer shell is a stainless steel conductor with a diameter of 300mm. The Miller box accessories are two capillaries for adjusting soil moisture and oxygen content; The improved version of the Miller box is divided into four layers, with specific layer heights of 10cm, 20cm, 30cm, and 40cm. Each layer contains test pieces, soil oxygen sensor, pH sensor, moisture sensor, temperature sensor, and soil sample. See the cross-sectional diagram of each layer. Figure 6 The soil oxygen sensor, pH sensor, moisture sensor, and temperature sensor are collectively referred to as soil environmental parameter sensors. A platinum wire electrode (including signal lead wire) is arranged 2 cm near the test piece. An improved version of the Miller box can be installed with 16 test pieces, 16 sets of soil environmental parameter sensors, and 16 platinum wire electrodes. The test piece is installed 10 cm away from the outer shell. The upper and lower covers of the Miller box need to be encapsulated with non-conductive insulating materials to prevent soil sample leakage and lead out the insulated signal lines of the test piece and the signal lines of the soil oxygen sensor, pH sensor, moisture content sensor, temperature sensor and platinum wire electrode; 3.5 The insulated signal line and the signal line of the platinum wire electrode are connected to the electrochemical workstation, which monitors the change of the electrochemical potential of the test piece and calculates the corrosion rate of the test piece.

[0022] Step 4: Conduct simulation test of stray current corrosion environment. 4.1 The Miller cell is connected to a controllable DC current source; The core rod of the Miller box is connected to the positive electrode of the current source, and the stainless steel shell is connected to the negative electrode of the current source; 4.2 Leakage current surface density distribution J i Adjusting the output current of a controllable DC power supply I oi ; (7), temporary integer variable i =1, 2, …, B; 4.3 Adjust the gas output of the capillary according to the test data of the oxygen content of the soil on site. If the test result of the oxygen content in the Miller box is less than the situation on site, oxygen is introduced into the capillary to increase the oxygen content of the soil sample. Conversely, if the test result of the oxygen content in the Miller box is greater than the situation on site, nitrogen is introduced into the capillary to reduce the oxygen content of the soil sample; 4.4 Adjust the deionized water output of the capillary according to the test data of the soil moisture content on site. If the moisture content test result in the Miller box is less than the on-site situation, deionized water is introduced into the capillary to increase the moisture content of the soil sample. Conversely, if the moisture content test result in the Miller box is greater than the on-site situation, dry air is introduced into the capillary to reduce the moisture content of the soil sample; 4.5 The insulated signal wire of the specimen and the signal wire of the platinum wire electrode are connected to the electrochemical workstation, which gives the corrosion reaction rate of each specimen; 4.6 Perform real-time corrosion rating based on the corrosion reaction rate of each specimen given by the electrochemical workstation; The corrosion reaction rate rating table of the specimens is as follows: Table 1 Corrosion reaction rate rating table

[0023] The corrosion rates of 16 specimens in the same Miller box were recorded.

[0024] Step 5: Continue to carry out simulated corrosion tests and conduct corrosion warnings. 5.1 Carry out simulated corrosion tests continuously and rate the corrosion amount in real time at 1-minute intervals; 5.2 Corrosion early warning by simulated corrosion test; If the corrosion rate is above level V for 60 minutes, a red warning signal will be issued; If the corrosion rate is graded as III or IV for 60 minutes, a yellow warning signal will be issued; No warning signals are issued for other situations; 5.3 Every other year, all specimens are taken out of the Miller box and the corrosion products on the surface of the specimens are analyzed, the scanning electron microscope is analyzed, and the weight loss is measured. The data is collated to give the annual average corrosion rate of different positions of the grounding conductor, and the test is terminated.

Claims

1. A simulation test method for the on-site stray current corrosion environment of a tower grounding body, characterized by: Step 1, carrying out the detection of the ground current of the tower grounding body, and then using computer simulation technology to evaluate the leakage current density distribution at different positions of the grounding system, 1.

1. Use flexible stray current sensors to continuously monitor the stray current entering the ground of the tower grounding body; 1.

2. Separate all the conductor branches of the tower grounding body { L }, assuming there is B branch road; 1.

3. Separate all conductor nodes of the tower grounding body { E }, assuming there is N nodes, and the node injection current column vector [ F ]; 1.

4. Calculate the correlation matrix of the tower grounding body from the conductor branches and conductor nodes [ K ] and its transposed matrix [ K T ]; Correlation Matrix[ K ]for N × B Order matrix, incidence matrix[ K ] is the transposed matrix [ K T ]for B × N If the matrix i #Node and j #Branches are associated, then [ K ] i,j = [ K T ] j,i = 0.5, temporary integer variable i =1, 2, …, N, j =1, 2, …, N, like i #Node and j # If the branches are not related, then [ K ] i,j = [ K T ] j,i = 0, temporary integer variable i =1, 2, ..., N, temporary integer variable j =1, 2, …, N; 1.

5. Solve the mutual resistance matrix [ M ]; 1.

6. Solve the node voltage column vector [ V ]: Node voltage column vector[ V ]for N The order column vector is obtained by solving the following equation: ; 1.

7. Solve for the branch leakage current column vector [ I ]: Branch leakage current column vector [ I ]for N The order column vector is calculated as follows: ; 1.

8. Obtain the leakage current density distribution at different locations of the grounding system: For conductor L i , the leakage current density distribution is the leakage current divided by the conductor surface area, thus obtaining the leakage current density distribution J i ;temporary Integer variables i =1, 2, …, N; Step 2: Monitor the parameters of the corrosion environment of each branch. 2.

1. Select the center point of each branch as the test point, and install an electrochemical oxygen sensor and an integrated soil pH-moisture-temperature sensor 20 cm above the conductor; 2.

2. Continuously monitor and transmit the parameters of the corrosion environment every 1 minute, including soil oxygen content, pH value, moisture content, and temperature parameters; Step 3: Take the soil samples from the center of each branch and build a simulation test platform for stray current corrosion environment. 3.

1. Take back sufficient soil samples from the center point of each branch; 3.

2. A square test piece is made of a plate made of the same material as the grounding body. The welding area of ​​the insulated signal line connected to the test piece is encapsulated with epoxy resin. The number of test pieces is 16 times the number of test points. 3.

3. The number of the improved version of the Miller box is consistent with the number of measuring points. The inner core of the Miller box is a graphite electrode, and the outer shell is a stainless steel conductor. There are two capillaries between the outer shell and the graphite electrode, which are used to adjust the soil moisture and oxygen content. 3.

4. The improved version of the Miller box is divided into four layers. Each layer contains the test piece, soil oxygen sensor, pH sensor, moisture sensor, temperature sensor, and soil sample. A platinum wire electrode is arranged 2 cm near the test piece. The test piece is installed 10 cm away from the outer shell. The upper and lower covers of the Miller box are encapsulated by non-conductive insulating materials, and the insulated signal wires, as well as the signal wires of the soil oxygen sensor, pH sensor, moisture sensor, temperature sensor and platinum wire electrode are led out; 3.

5. The insulated signal line and the signal line of the platinum wire electrode are connected to the electrochemical workstation, which monitors the electrochemical potential change of the test piece and calculates the corrosion rate of the test piece; Step 4: Conduct simulation test of stray current corrosion environment. 4.

1. Connect the Miller box to the controllable DC current source: the core rod of the Miller box is connected to the positive electrode of the current source, and the stainless steel shell is connected to the negative electrode of the current source; 4.

2. Leakage current surface density distribution J i Adjusting the output current of a controllable DC power supply I oi ; I oi It is derived from the following formula: , a temporary integer variable i =1,2,…,B, 4.

3. Adjust the gas volume in the capillary tube according to the test data of the oxygen content of the soil on site. If the test result of the oxygen content in the Miller box is less than the situation on site, oxygen is introduced into the capillary tube to increase the oxygen content of the soil sample. On the contrary, if the test result of the oxygen content in the Miller box is greater than the situation on site, inert gas is introduced into the capillary tube to reduce the oxygen content of the soil sample. 4.

4. Adjust the deionized water output of the capillary according to the test data of the on-site soil moisture content. If the moisture content test result in the Miller box is less than the on-site situation, deionized water is introduced into the capillary to increase the moisture content of the soil sample. Conversely, if the moisture content test result in the Miller box is greater than the on-site situation, dry air is introduced into the capillary to reduce the moisture content of the soil sample. 4.

5. The insulated signal wire of the specimen and the signal wire of the platinum wire electrode are connected to the electrochemical workstation, which gives the corrosion reaction rate of each specimen; 4.

6. Perform real-time corrosion rating based on the corrosion reaction rate of each specimen given by the electrochemical workstation; Record the corrosion rate of 16 specimens in the same Miller box; the unit of corrosion rate is g / (dm 2 ﹒ a); Step 5: Continue to carry out simulated corrosion tests and conduct corrosion warnings. 5.

1. Real-time corrosion rating at 1-minute intervals; 5.

2. Corrosion early warning is carried out by simulated corrosion test. If the corrosion rate classification is above a certain level for a certain period of time, a corresponding predetermined form of early warning signal will be issued; 5.

3. Every other year, all specimens are taken out of the Miller box for surface corrosion product analysis, scanning electron microscopy analysis, and weight loss measurement. The data are collated to give the annual average corrosion rate of different locations of the grounding conductor.

2. The simulation test method for the on-site stray current corrosion environment of the tower grounding body according to claim 1 is characterized by: The overall height of the Miller box is 500mm, the graphite electrode is Φ100mm, and the shell diameter is 300mm.

3. The simulation test method for the on-site stray current corrosion environment of the tower grounding body according to claim 1 is characterized by: The specimen size is 10mm×10mm×4mm.

4. The simulation test method for the on-site stray current corrosion environment of the tower grounding body according to claim 2 is characterized by: Step 3.4: The heights of each layer are 10cm, 20cm, 30cm, and 40cm.

5. The simulation test method for the on-site stray current corrosion environment of the tower grounding body according to claim 1 is characterized by: Step 1.5 Mutual resistance matrix [ M ]for B × B The diagonal elements of the matrix are: , in, ρ is the equivalent earth resistivity, L i For the i The length of the conductor, a i is the radius of the conductor, dist is the function for finding the distance, for L i Mirror image, [ M ]The off-diagonal elements are: , in, L j For the j The length of the conductor, for L j Mirror image of, temporary integer variable j =1, 2,…, N.