Method for synthesizing 2-bromoethanol through selective electro-oxidation of ethylene by taking sodium bromide solution as bromine source mediation

Through a carbon paper electrode system mediated by sodium bromide solution, selective electrooxidation of ethylene is achieved to synthesize 2-bromoethanol, solving the problems of equipment corrosion and precious metal catalysts in traditional synthesis methods, and achieving efficient and safe 2-bromoethanol synthesis.

CN120591796APending Publication Date: 2025-09-05TIANJIN UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411831062.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-12-12
Publication Date
2025-09-05

AI Technical Summary

Technical Problem

The method of synthesizing 2-bromoethanol in the prior art needs to be carried out under acidic conditions, which has problems such as equipment corrosion, many by-products, complex operations, and the use of precious metal catalysts, and is not suitable for large-scale industrial production.

Method used

Sodium bromide solution is used as the bromine source, and constant potential electrochemical oxidation is performed in the tri-electrode system through carbon paper as working electrode. Inexpensive and easy-to-get carbon materials and water are used as solvents to achieve selective electrooxidation of ethylene to synthesize 2-bromoethanol. The reaction conditions are mild and the catalyst is easy to recover.

Benefits of technology

It realizes efficient and highly selective synthesis of 2-bromoethanol, avoids equipment corrosion and the use of precious metal catalysts, is easy to operate, has high yield, good selectivity and is environmentally friendly.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN120591796A_ABST
    Figure CN120591796A_ABST
Patent Text Reader

Abstract

The invention provides a method for synthesizing 2-bromoethanol through selective electrooxidation of ethylene by taking a sodium bromide solution as a bromine source mediation, which comprises the following steps: reacting ethylene gas as a raw material with a reaction system taking hydrophobic carbon paper as a working electrode, and carrying out constant-potential electrochemical selective oxidation to obtain a corresponding alcohol compound at the reaction potential of 0.5-1.3 V. According to the method, high-efficiency and high-selectivity synthesis of 2-bromoethanol can be realized in a relatively wide potential range, and the method takes a cheap, easily available and efficient carbon material as an electrode, is green and safe, takes sodium bromide as a bromine source and water as a hydrogen source, does not need an additional hydrogen source, is mild in reaction condition, does not need heating, is simple and convenient to operate, and is easy to recover a catalyst.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of electrocatalytic synthesis of 2-bromoethanol, and more particularly to a method for synthesizing 2-bromoethanol by selective electrooxidation of ethylene using a sodium bromide solution as a bromine source. Background Art

[0002] The unique combination of bromine atoms and hydroxyl groups in 2-bromoethanol gives it good reactivity and can be used to introduce different functional groups. Therefore, in many fields such as pharmaceutical pesticides and dye industries, 2-bromoethanol is an important synthetic intermediate for many compounds. So far, most researchers still use traditional methods to prepare 2-bromoethanol. The specific methods are as follows: (1) 2-bromoethanol is synthesized by reacting ethylene glycol with hydrobromic acid. This reaction is usually carried out under heating and acidic conditions. HO-CH2-CH2-OH+HBr→Br-CH2-CH2-OH+H2O

[0003] (2) Ethanol is reacted with hydrogen bromide (HBr) and sulfuric acid (H2SO4) to produce 2-bromoethanol. Ethanol is mixed with concentrated sulfuric acid and hydrobromic acid. The reaction needs to be carried out under heating conditions. CH3CH2OH+HBr→Br-CH2-CH2-OH

[0004] Above method all need to carry out under acidic conditions, and need to heat, and condition is relatively not gentle.In the reaction of traditional chemical reagent method synthesis 2-bromoethanol, there are some drawbacks, reaction mostly need to be carried out under the system of strong acid, and high temperature heating simultaneously, may cause product decomposition or produce more by products.In addition, hydrobromic acid and bromine gas have stronger corrosivity, and reaction unit (such as glass, metal) is had to significant corrosive effect.Particularly in industrial large-scale production, the anti-corrosion cost of equipment is high, and improper operation also may cause bromine gas leakage, harmful to operator and environment.

[0005] In recent years, electrocatalytic organic synthesis has emerged as a new method for electrically driven chemical reactions. Electrodes directly or indirectly participate in the reaction, replacing the chemical reagents used in traditional chemical reactions to achieve oxidation or reduction reactions. The core principle is to stimulate intermolecular electron transfer under mild conditions by regulating the electrode potential, thereby achieving the formation or breaking of specific chemical bonds. Therefore, electrocatalytic or promoted organic transformations have gradually become a hot research topic in synthetic chemistry. Given the limitations of the aforementioned synthetic methods, the electrooxidation of ethylene to 2-bromoethanol using aqueous electrolytes is crucial for the timely utilization of the bromine produced by the oxidation of bromide ions. Therefore, the search for inexpensive, efficient electrocatalysts to achieve high conversion and selectivity in electrocatalytic synthesis is crucial. Some researchers have used metal-based materials such as Ir, Co2O3, and NiO as catalytic materials in their research on the electrocatalytic oxidation of ethylene to 2-bromoethanol, but these materials are expensive and difficult to recycle. Summary of the Invention

[0006] The present invention aims to overcome the deficiencies in the prior art and provides a method for synthesizing 2-bromoethanol by selective electrooxidation of ethylene using a sodium bromide solution as a bromine source. The method can achieve efficient and highly selective synthesis of 2-bromoethanol within a wide potential range. Furthermore, the present invention uses inexpensive, readily available, and efficient carbon materials as electrodes and uses green, safe, and abundant water as a solvent and hydrogen source. The reaction conditions are mild, heating is not required, the operation is simple, and the catalyst is easily recyclable.

[0007] The technical purpose of the present invention is achieved through the following technical solutions.

[0008] A method for synthesizing 2-bromoethanol by selective electrooxidation of ethylene mediated by sodium bromide solution as a bromine source, wherein constant-potential electrochemical selective oxidation is carried out in a three-electrode system using carbon paper as a working electrode, wherein a cathode chamber and an anode chamber are separated by a proton exchange membrane, an aqueous sodium bromide solution is introduced into the two electrode chambers, ethylene passes from the gas chamber, penetrates the carbon paper, and forms a gas-liquid-solid three-phase interface on the carbon paper surface, and 2-bromoethanol is obtained in the anode liquid product through constant-potential electrochemical selective oxidation.

[0009] In the technical solution of the present invention, the reaction potential is 0.5-1.3V (Hg / Hg2Cl2).

[0010] In the technical solution of the present invention, a peristaltic pump is used to pump the sodium bromide aqueous solution into the bipolar chamber and its flow rate is controlled, such as 10-30 rpm.

[0011] In the technical solution of the present invention, a flow meter is used to control the flow rate of ethylene, such as 10-30 sccm.

[0012] In the technical solution of the present invention, the concentration of the sodium bromide solution is 0.25-1M.

[0013] In the technical solution of the present invention, nickel foam or platinum sheet is used as the counter electrode, and Hg / Hg2Cl2 (1.0M NaBr aqueous solution) is used as the reference electrode.

[0014] In the technical solution of the present invention, a flow cell electrolytic cell is used as a reaction container.

[0015] In the technical solution of the present invention, the reaction environment temperature is room temperature 20-25°C.

[0016] In the technical solution of the present invention, carbon paper is used as a catalyst to convert ethylene into 2-bromoethanol under the mediation of sodium bromide solution as a bromine source, and the carbon paper (CP) is a hydrophobic carbon paper 28BC model.

[0017] The present invention uses cheap, readily available, and efficient carbon materials as electrodes, and uses green, safe, and abundant water as a solvent and hydrogen source. The reaction conditions are mild, heating is not required, the operation is simple, the product is easy to separate, and the catalyst is easy to recover. The problems existing in other synthesis methods such as the use of precious metal catalysts, complex operation, long reaction time, low yield, poor selectivity, strong reagent toxicity, and environmental pollution caused by reaction by-products are effectively avoided. The carbon electrode has good stability and can be recycled multiple times. The Faradaic efficiency, yield, and selectivity of the generated 2-bromoethanol do not change significantly, the conversion rate and selectivity are high, and the influence of by-products is avoided. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 The figures are the nuclear magnetic resonance line spectra of standard samples of 2-bromoethanol at different concentrations in the present invention.

[0019] Figure 2 This is a linear relationship diagram between the concentration of 2-bromoethanol and the NMR peak area ratio of 2-bromoethanol to DMSO.

[0020] Figure 3 It is the nuclear magnetic resonance line spectrum of the product at different constant potentials in the embodiment of the patent of the present invention. DETAILED DESCRIPTION

[0021] The technical solution of the present invention is further described below with reference to specific embodiments.

[0022] A flow cell electrolytic cell was used as the reaction vessel. The cathode and anode chambers of the electrolytic cell were separated by a proton exchange membrane. 20ml of 1M sodium bromide solution was placed in an electrolyte bottle and injected into the anode and cathode chambers using a peristaltic pump at 20 rpm. Ethylene was introduced into the gas chamber at 20 sccm. Hydrophobic carbon paper (model 28BC) was placed between the gas chamber and the anode chamber. Ethylene gas could pass through the carbon paper, but the electrolyte in the anode chamber could not. The carbon paper served as the working electrode, nickel foam as the counter electrode, and a (Hg / Hg2Cl2) electrode as the reference electrode. The cell was connected to an electrochemical workstation and subjected to constant potential for IT testing. After a ten-minute reaction, the anode liquid product was collected and analyzed by NMR to obtain 2-bromoethanol, which was then quantitatively analyzed by NMR.

[0023] After cleaning the anode electrolyte bottle and adding new electrolyte, you can proceed to the next potential test.

[0024] In order to perform quantitative analysis of the product 2-bromoethanol, different concentrations of 2-bromoethanol standards were purchased for nuclear magnetic resonance testing. The concentration of 2-bromoethanol and the ratio of the nuclear magnetic peak area of ​​dibromoethanol to DMSO were linearly programmed, as shown in the following example: Figure 1 and Figure 2Then the anode liquid products obtained at different constant potentials were subjected to nuclear magnetic resonance testing, and it was found that the products at different potentials were all the target product 2-bromoethanol. Figure 2 The linear relationship presented is used to calculate the concentration of the target product. In the test of the product of the present invention, the charge utilization efficiency (Faradaic efficiency, %) of the product is calculated based on:

[0025]

[0026] Where n is the number of electrons transferred, m is the amount of substance of the product, and F is the Faraday constant 96485 Cmol -1 , C is the total charge consumed by the reaction.

[0027]

[0028]

[0029] The above analysis shows that the test results are not greatly affected by the potential, and the target product 2-bromoethanol can be prepared, and the Faradaic efficiency reaches 60%-73%.

[0030] By adjusting the process parameters according to the present invention, the synthesis of 2-bromoethanol can be achieved, and the performance is substantially consistent with that of the present invention. The above is an exemplary description of the present invention. It should be noted that any simple variation, modification, or equivalent substitution that can be made by other skilled in the art without inventive effort falls within the scope of protection of the present invention without departing from the core of the present invention.

Claims

1. A method for synthesizing 2-bromoethanol by selective electrooxidation of ethylene mediated by sodium bromide solution as a bromine source, characterized in that: Constant potential electrochemical selective oxidation is carried out in a three-electrode system with carbon paper as the working electrode. The cathode chamber and the anode chamber are separated by a proton exchange membrane. A sodium bromide aqueous solution is passed into the two electrode chambers. Ethylene passes through the gas chamber, penetrates the carbon paper and forms a gas-liquid-solid three-phase interface on the carbon paper surface. 2-bromoethanol is obtained in the anode liquid product through constant potential electrochemical selective oxidation.

2. The method for synthesizing 2-bromoethanol by selective electrooxidation of ethylene mediated by sodium bromide solution as a bromine source according to claim 1, characterized in that: The reaction potential is 0.5-1.3V (Hg / Hg2Cl2).

3. The method for synthesizing 2-bromoethanol by selective electrooxidation of ethylene mediated by sodium bromide solution as a bromine source according to claim 1, characterized in that: Use a flow meter to control the flow rate of ethylene, such as 10-30 sccm.

4. The method for synthesizing 2-bromoethanol by selective electrooxidation of ethylene mediated by sodium bromide solution as a bromine source according to claim 1, characterized in that: Use a peristaltic pump to pump the sodium bromide aqueous solution into the bipolar chamber and control its flow rate, such as 10-30 rpm.

5. The method for synthesizing 2-bromoethanol by selective electrooxidation of ethylene mediated by sodium bromide solution as a bromine source according to claim 1, characterized in that: The concentration of sodium bromide solution is 0.25-1M.

6. The method for synthesizing 2-bromoethanol by selective electrooxidation of ethylene mediated by sodium bromide solution as a bromine source according to claim 1, characterized in that: Nickel foam or platinum sheet is used as the counter electrode, and Hg / Hg2Cl2 is used as the reference electrode.

7. The method for synthesizing 2-bromoethanol by selective electrooxidation of ethylene mediated by sodium bromide solution as a bromine source according to claim 1, characterized in that: A flow cell electrolytic cell was used as the reaction vessel.

8. The method for synthesizing 2-bromoethanol by selective electrooxidation of ethylene mediated by sodium bromide solution as a bromine source according to claim 1, characterized in that: The reaction environment temperature is room temperature 20-25°C.

9. Application of carbon paper as catalyst in the conversion of ethylene to 2-bromoethanol mediated by sodium bromide solution as bromine source.

10. The use according to claim 9, characterized in that The carbon paper is hydrophobic carbon paper.