Preparation method of N-type polymer transistor based on electrolyte gate dielectric
By using a solid electrolyte gate dielectric layer in N-type polymer transistors, combined with specific polymer semiconductor materials and electrode materials, high-performance N-type polymer transistors have been fabricated, solving the problem of insufficient gate control capability and achieving low power consumption and memory characteristics, making them suitable for flexible electronic devices.
Patent Information
- Application Number
- CN202511488089.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2025-10-17
- Publication Date
- 2026-01-20
AI Technical Summary
Existing N-type polymer transistors have insufficient gate control capability and lack memory characteristics, which limits their application in low-power and flexible electronic devices.
Using a solid electrolyte as the gate dielectric layer, combined with specific polymer semiconductor materials and electrode materials, an N-type polymer transistor is fabricated through a thermal evaporation process to form a top-gate bottom contact structure, which has short-range memory characteristics.
It significantly reduces the operating voltage of the device, improves gate control capability and device performance, exhibits short-range memory characteristics, and is suitable for low-power and flexible electronic devices.
Smart Images

Figure CN121368326A_ABST
Abstract
Description
TECHNICAL FIELD
[0001] The application belongs to the field of electronic information, and particularly relates to a preparation method of an N-type polymer transistor based on an electrolyte gate dielectric. BACKGROUND
[0002] Organic polymer transistors have made significant progress in the field of organic electronics, but most of them work at high voltages, which seriously affects the application of polymer transistors in low-power and flexible wearable devices. Through research, it is found that the general method for transistors to achieve low-power operation is to use a High-K gate dielectric or to introduce an intermediate layer at the gate dielectric interface. However, as a new type of dielectric material, the ion gate contains free-moving ions. Compared with traditional liquid electrolytes, the solid electrolyte mentioned in the application exhibits remarkable stability in transistor applications, can maintain electrochemical stability for a long time, and avoids the common problems of leakage and evaporation of liquid electrolytes. In addition, the solid electrolyte has high mechanical strength, which reduces the risk of damage to the device during use, especially suitable for application scenarios that require high reliability and durability. This feature enables the efficient integration of solid electrolytes with solid-state elements, promoting the miniaturization and performance improvement of compact and flexible electronic devices. These devices not only have the advantages of low power consumption and large current modulation, but also are widely used in the fields of sensors, actuators, energy storage and bioelectronics due to their low cost, multifunctionality and adaptability. SUMMARY
[0003] In order to solve the problem of insufficient gate control ability of the existing N-type polymer transistor and the lack of memory characteristics, the application provides a preparation method of an N-type polymer transistor based on an electrolyte gate dielectric.
[0004] The specific technical solutions are as follows: Firstly, the application provides a preparation method of an N-type polymer transistor based on an electrolyte gate dielectric, which comprises the following steps: Step S1: preparation of a solution: Step S1-1: preparation of a semiconductor solution: an N-type polymer semiconductor material is prepared into a solution with an organic solvent at a mass-volume ratio of 3-10 mg / mL, and is heated to be fully dissolved to obtain a semiconductor solution, The N-type polymer semiconductor material is a polymer DPPT-TT (CAS No. 1260685-66-2) of 1,4-dioxadipyrrone and thiophene, and the organic solvent is o-dichlorobenzene (DCB); The polymer DPPT-TT of 1,4-dioxadipyrrone and thiophene has a CAS No. of 1260685-66-2 and a molecular formula as follows: .
[0005] Step S1-2: Preparation of gate medium solution: polyvinylidene fluoride-trifluoroethylene copolymer P(VDF-co-TrFE) and 1-ethylimidazole bis(trifluoromethylsulfonyl) imidazole ([EMIM][TFSI]) are dissolved in acetone, polymethyl methacrylate (PMMA) is dissolved in n-butyl acrylate (N-BA), and then the two obtained solutions are mixed, followed by heating and complete dissolution to form a gate medium solution; the raw materials used for the gate medium are different from those in the prior art, so that the performance of the product device in the application is significantly improved. At the same time, it shows short-term memory characteristics, providing direction for chips applied to predictive computing systems. P(VDF-co-TrFE), CAS No.: 24937-79-9, molecular formula (CH2CF2) n Specifically as follows: .
[0006] Step S2: cleaning of the substrate; Step S3: preparation of the device: Step S3-1: preparation of source-drain electrode: vacuum evaporation boat, source-drain mask and substrate are sequentially placed from top to bottom in the evaporation instrument cavity, gold metal particles are placed on the vacuum evaporation boat, and then the cleaned source-drain mask is placed on the substrate, the evaporation instrument cavity is evacuated to a vacuum of 10 -5 ~10 -4 Pa, and then hot evaporation is performed to form a source-drain electrode on the surface of the substrate; Step S3-2: preparation of polymer semiconductor layer: spin-coat the semiconductor solution obtained in step S1-1 on the surface of the sample obtained in step S3-1, and then perform annealing treatment after spin-coating to form a polymer semiconductor layer on the surface of the source-drain electrode; Step S3-3: preparation of solid-state electrolyte gate medium layer: spin-coat the gate medium solution obtained in step S1-2 on the surface of the sample obtained in step S3-2, and then perform annealing treatment after spin-coating to form a solid-state electrolyte gate medium layer on the surface of the polymer semiconductor layer; Step S3-4: preparation of gate electrode: first, place aluminum metal particles on the vacuum evaporation boat, then place the cleaned gate mask above the sample surface obtained in step S3-3, evacuate the evaporation instrument cavity to a vacuum of 10 -5 ~10 -4 Pa, and then perform hot evaporation to form an aluminum gate electrode on the surface of the solid-state electrolyte gate medium layer; compared with the conventional organic material PMMA as the gate medium of the polymer field effect transistor, the organic electrolyte gate transistor has better performance, stronger gate control ability, and short-term memory characteristics.
[0007] Step S4: preparing the transistor: adjusting the power of the two ends of the vacuum evaporation boat, filling the inert gas after cooling to room temperature, taking out after the pressure in the evaporation instrument cavity is reduced to balance with the outside, and obtaining the N-type polymer transistor based on the electrolyte gate dielectric.
[0008] Further, the ionic liquid in step S1-2 is 1-ethylimidazolium bis(trifluoromethylsulfonyl) imide ([EMIM][TFSI]), the polymer matrix is polymethyl methacrylate (PMMA), and the solvent is a mixed solvent of acetone and n-butyl acrylate (N-BA).
[0009] [EMIM][TFSI] is 1-ethylimidazolium bis(trifluoromethylsulfonyl) imide (ionic liquid), CAS number: 174899-82-2, molecular formula C8H 11 F6N3O4S2 Specifically as follows: , PMMA, CAS number: 9011-14-7, molecular formula [CH2C(CH3)(CO2CH3)] n Specifically as follows: .
[0010] Further, the specific steps of step S1-2 are: first, P(VDF-co-TrFE) and [EMIM][TFSI] are dissolved in acetone in a certain proportion, the weight ratio of P(VDF-co-TrFE), [EMIM][TFSI] and acetone is 1:4:7, and the P(VDF-co-TrFE)-[EMIM][TFSI] gel solution is obtained by heating and stirring at 70°C in an inert gas environment. Then, the gel solution is uniformly mixed with the N-BA solution of PMMA at a volume ratio of 2:98. Further, in steps S1-1 and S1-2, heating is carried out to 75-85°C to fully dissolve.
[0011] Further, the specific steps of step S2 are: sequentially placing the substrate in deionized water and alcohol, respectively, and removing surface impurities by ultrasonic cleaning, then blowing dry with inert gas, and then heating to evaporate the surface.
[0012] Further, in step S3-1, the source-drain mask material is stainless steel, and the substrate is a glass sheet, and the source-drain electrode prepared in step S3-1 by thermal evaporation is prepared by the following steps: heating the vacuum evaporation boat, rotating the power control knob to make the thermal evaporation current reach 110-120 A, preparing a gold electrode with a thickness of 50-55 nm at a rate of 0.03-0.05 nm / s, then slowly reducing the power, waiting for the evaporation instrument cavity to cool to room temperature, filling with inert gas, and opening the evaporation instrument cavity to take out the prepared source-drain electrode.
[0013] Further, the gate electrode prepared in step S3-4 by thermal evaporation is prepared by the following steps: heating the evaporation boat, rotating the power control knob to make the thermal evaporation current reach 100-120 A, preparing an aluminum gate electrode with a thickness of 80-100 nm at a rate of 0.02-0.03 nm / s.
[0014] Further, the spin coating process in steps S3-2 and S3-3 is first pre-spin coating at 500-600 rpm for 3-5 seconds, and then spin coating at 2000-2100 rpm for 60-120 seconds; the annealing treatment in step S3-2 is annealing at 200-250 DEG C for 1-1.5 hours, and the annealing treatment in step S3-3 is annealing at 75-85 DEG C for 2-3 hours. Secondly, the application also provides an N-type polymer transistor prepared by any of the above-mentioned methods, which is a top-gate bottom-contact structure and sequentially comprises a gate electrode, a solid-state electrolyte gate dielectric layer, a polymer semiconductor layer, a source-drain electrode and a substrate from top to bottom.
[0015] Thirdly, the application also provides the use of the N-type polymer transistor in flexible electronics, sensors, low-power storage or neuromorphic computing devices.
[0016] Compared with the prior art, the application has the beneficial effects that: most of the current organic polymer transistors work at a large voltage, a high-performance N-type polymer device is prepared by using a new electrolyte gate dielectric layer, the working voltage of the device is greatly reduced, the performance of the device is improved, the device exhibits short-range memory characteristics, and the device has the characteristics of simple process, high stability and low cost. BRIEF DESCRIPTION OF DRAWINGS
[0017] Figure 1 FIG. 1 is a 3D structure schematic diagram of the polymer electrolyte gate transistor of the application; Figure 2 FIG. 2 is a comparison diagram of the transfer characteristics and output curves of the N-type polymer field effect transistor prepared by the electrolyte gate and the conventional polymer gate dielectric (PMMA) of the application; Figure 3The contrastive chart of capacitance-voltage (C-V) curves of N-type polymer field effect transistors prepared by the electrolyte gate and conventional polymer gate dielectric (PMMA) of the application; Figure 4 The forward and backward scan transfer characteristic curves and current response curves of the polymer electrolyte gate transistor of the application. DETAILED DESCRIPTION
[0018] The technical solutions of the application will be described in detail below through examples, but the protection scope of the application is not limited to the examples. EXAMPLE
[0019] Step S1: preparation of a solution: Step S1-1: preparation of a semiconductor pre-solution; a polymer DPPT-TT (CAS No. 1260685-66-2) of 1,4-dioxo-di-pyrrole and thiophene is prepared with o-dichlorobenzene (DCB) at a mass-volume ratio of 5 mg / mL to form a semiconductor solution with a concentration of 5 mg / mL.
[0020] Step S1-2: preparation of a gate dielectric pre-solution; P(VDF-co-TrFE) and [EMIM][TFSI] are first dissolved in acetone in a proportion, and the weight ratio of P(VDF-co-TrFE), [EMIM][TFSI] and acetone is 1:4:7; the mixture is heated and stirred at 70°C in a nitrogen-filled glove box for 24 hours to obtain a P(VDF-co-TrFE)-[EMIM][TFSI] gel solution; then the gel solution is uniformly mixed with a n-butyl acrylate (N-BA) solution of PMMA at a volume ratio of 2:98 to form a gate dielectric pre-solution.
[0021] Step S1-3: dissolution of the solution; the semiconductor pre-solution prepared in step S1-1 is placed on a heating table at 80°C for 48 hours, and the gate dielectric pre-solution prepared in step S1-2 is placed on a heating table at 80°C for 24 hours, and then fully dissolved to obtain a semiconductor solution and a gate dielectric solution; Step S2: cleaning of the substrate; the substrate is sequentially placed in deionized water and alcohol, and cleaned with an ultrasonic cleaner for 20 minutes, and then dried with a nitrogen gun and placed on a heating table at 100°C for 15 minutes.
[0022] Step S3: preparation of a device: Step S3-1: preparation of a source-drain electrode; titanium metal particles and aluminum metal particles are first placed on a vacuum evaporation boat, and then a cleaned stainless steel source-drain mask is placed on a glass sheet and sent into an evaporation instrument cavity, and the cavity is pumped to a vacuum of 4×10 -4Pa, then the evaporation boat was heated by thermal evaporation, and the power control knob was rotated to make the thermal evaporation current reach 120 A. A gold electrode with a thickness of 50 nm was prepared at a rate of 0.03 nm / s, and then the power was slowly reduced. After the cavity was cooled to room temperature for 30 minutes, nitrogen was filled to open the cavity and take out the sample, and the source-drain electrode was prepared. Step S3-2: Preparation of a polymer semiconductor layer: using the semiconductor solution obtained in step S1-3, i.e., the N2200 solution, the substrate was pre-spun at 500 rpm for 3 seconds, then spun at 2000 rpm for 60 seconds, and annealed at 200°C for 1 hour to form a polymer semiconductor layer. After cooling for 40 minutes, the process was completed.
[0023] Step S3-3: Preparation of a solid-state electrolyte gate dielectric layer: using the gate dielectric solution obtained in step S1-3, the semiconductor layer obtained in step S3-2 was pre-spun at 500 rpm for 3 seconds, then spun at 2000 rpm for 60 seconds, and annealed at 80°C for 2 hours to form a solid-state electrolyte gate dielectric layer.
[0024] Step S3-4: Preparation of a gate electrode: first, aluminum metal particles were placed on a vacuum evaporation boat, then a cleaned source-drain mask was placed on the substrate and sent into the cavity of the evaporation instrument. The cavity of the evaporation instrument was pumped to a vacuum of 4×10 -4 Pa, then the evaporation boat was heated by thermal evaporation, and the power control knob was rotated to make the thermal evaporation current reach 120 A. A gold electrode with a thickness of 50 nm was prepared at a rate of 0.03 nm / s, and then the power was slowly reduced. After the cavity was cooled to room temperature for 30 minutes, nitrogen was filled to open the cavity and take out the sample, and the source-drain electrode was prepared.
[0025] Step S4: Preparation of a transistor: the power at both ends of the vacuum evaporation boat was adjusted and reduced, and after cooling for 30 minutes, nitrogen was filled to take out the N-type polymer transistor based on the electrolyte gate dielectric. The transistor structure is shown in Figure 1 .
[0026] A polymer field effect transistor using traditional organic material PMMA as the gate dielectric layer.
[0027] Step S1: Preparation of a solution: Step S1-1: Preparation of a semiconductor pre-solution: 1,4-dioxadipyrrone and thienyl polymer DPPT-TT (CAS No.: 1260685-66-2) were prepared with o-dichlorobenzene (DCB) at a mass-volume ratio of 5 mg / mL to form a semiconductor solution with a concentration of 5 mg / mL.
[0028] Step S1-2: Preparation of a gate dielectric pre-solution: PMMA and n-butyl acrylate (N-BA) solution were prepared at a mass-volume ratio of 80 mg / mL to form a gate dielectric pre-solution. This is different from the examples.
[0029] Step S1-3: Dissolution of the solution: the semiconductor pre-solution prepared in step S1-1 was heated on a heating table at 80℃ for 48 hours, and the gate medium pre-solution prepared in step S1-2 was heated on a heating table at 80℃ for 24 hours, and were fully dissolved respectively to obtain a semiconductor solution and a gate medium solution; Step S2: Cleaning of the substrate; the substrate was sequentially placed in deionized water and alcohol, and was cleaned by an ultrasonic cleaner for 20 minutes respectively, and was then dried by a nitrogen gun and was heated on a heating table at 100℃ for 15 minutes.
[0030] Step S3: Preparation of the device: Step S3-1: Preparation of the source-drain electrode: gold metal particles were first placed on a vacuum evaporation boat, and then a cleaned stainless steel source-drain mask was placed on the glass sheet and was sent into the cavity of the evaporation instrument, a mechanical pump and a molecular pump were used to evacuate the cavity of the evaporation instrument to a vacuum of 4x10 -4 Pa, and then a hot evaporation method was used to heat the evaporation boat, a power control knob was rotated to make the hot evaporation current reach 120 A, a gold electrode with a thickness of 50 nm was prepared at a rate of 0.03 nm / s, and then the power was slowly reduced, the cavity was cooled to room temperature for 30 minutes, nitrogen was filled, the cavity was opened, and the sample was taken out to prepare the source-drain electrode; Step S3-2: Preparation of the polymer semiconductor layer: the surface of the glass sheet was cleaned by air blowing, the semiconductor solution obtained in step S1-3, i.e. the DPPT-TT solution, was used, the glass sheet was pre-spun at 500 rpm for 3 seconds by a pipette gun, and was then spun at 2000 rpm for 60 seconds, and was annealed at 200℃ for 1 hour to form a polymer semiconductor layer, and was then cooled for 40 minutes; Step S3-3: Preparation of the solid-state electrolyte gate medium layer: the surface of the glass sheet was cleaned by air blowing, the gate medium solution obtained in step S1-3 was used, and was first pre-spun at 500 rpm for 3 seconds on the semiconductor layer obtained in step S3-2 by a pipette gun, and was then spun at 2000 rpm for 60 seconds, and was annealed at 80℃ for 2 hours to form a solid-state electrolyte gate medium layer.
[0031] Step S3-4: Preparation of the gate electrode: aluminum metal particles were first placed on a vacuum evaporation boat, and then a cleaned source-drain mask was placed on the substrate and was sent into the cavity of the evaporation instrument, a mechanical pump and a molecular pump were used to evacuate the cavity of the evaporation instrument to a vacuum of 4x10 -4 Pa, and then a hot evaporation method was used to heat the evaporation boat, a power control knob was rotated to make the hot evaporation current reach 120 A, an aluminum gate electrode with a thickness of 80 nm was prepared at a rate of 0.02 nm / s.
[0032] Step S4: Obtaining the transistor: Adjust and reduce the power at both ends of the vacuum evaporation boat, and after cooling, fill it with nitrogen gas to remove the N-type polymer transistor based on the electrolyte gate dielectric.
[0033] Figure 2 This is a comparison graph showing the n-type saturation region transfer characteristic curves and output characteristic curves of the polymer field-effect transistors obtained in the comparative examples and embodiments. Figure 2 As can be seen, the polymer field-effect transistor fabricated using a solid electrolyte as the gate dielectric layer in the embodiments outperforms the traditional transistor using PMMA as the gate dielectric layer in terms of transfer and output characteristics, and its main basic electrical parameters are superior. Table 1 below lists the threshold voltage and mobility of the two devices: Table 1 Gate dielectric layer Threshold voltage (V) Mobility (cm 2 / V·s)]]> Electrolyte gate 1.58 0.26 PMMA 8.31 0.12 For the comparative polymer field-effect transistor, its threshold voltage is 8.31V and its mobility is 0.12cm. 2 For the polymer field-effect transistor of this embodiment, the threshold voltage is 1.58V and the mobility is 0.26 cm⁻¹. 2 / V·s. Therefore, it can be seen from the above electrical parameters that the electrical performance of the polymer electrolyte gate transistor prepared by this invention has been significantly improved.
[0034] Figure 3 For comparison with the polymer field-effect transistors obtained in the examples C - V Curve comparison chart. (From...) Figure 3 As can be seen, the polymer field-effect transistor fabricated using electrolyte as the gate dielectric layer in the embodiments has a higher capacitance per unit area than the transistor using PMMA as the gate dielectric layer. This indicates that the electrolyte-gate transistor has better gate control capability.
[0035] Figure 4 The scan-through transfer characteristic curves and current response curves of the polymer field-effect transistor obtained in this embodiment are shown. The scan-through transfer characteristic curves reveal a hysteresis window in the device. Simultaneously, when a pulse signal is applied to the device gate, the drain current in this embodiment exhibits a non-linear increase with each pulse applied to the gate, gradually approaching saturation. A significant delay occurs before the current returns to its initial level after each pulse. This short-term memory effect can significantly enhance the current peak, which is particularly important for reservoir computing systems processing time-series data.
[0036] The results show that devices using solid electrolytes as the gate dielectric layer exhibit improved performance compared to devices using PMMA as the gate dielectric, while also demonstrating short-range memory characteristics, providing direction for chips applied to predictive computing systems.
[0037] The above-mentioned technologies not specifically mentioned are referred to the state of the art.
[0038] As mentioned above, although the application has been represented and described with reference to specific preferred embodiments, it is not to be construed as being limited thereto. Various changes in form and detail can be made thereto without departing from the spirit and scope of the application as defined in the following claims.
Claims
1. A method for fabricating an N-type polymer transistor based on an electrolyte gate dielectric, characterized in that, The method includes the following steps: Step S1: Solution preparation: Step S1-1: Preparation of the semiconductor solution: The N-type polymer semiconductor material and an organic solvent are mixed at a mass-to-volume ratio of 3-10 mg / mL to prepare a solution, which is then heated to fully dissolve the semiconductor solution. The N-type polymer semiconductor material is a polymer DPPT-TT of 1,4-dioxodipyrrole and thiophene (CAS No.: 1260685-66-2), and the organic solvent is o-dichlorobenzene (DCB). Step S1-2: Preparation of gate dielectric solution: Polyvinylidene fluoride-trifluoroethylene copolymer P(VDF-co-TrFE) and 1-ethylimidazolium bis(trifluoromethanesulfonyl)imide ([EMIM][TFSI]) are dissolved in acetone, and polymethyl methacrylate (PMMA) is dissolved in n-butyl acrylate (N-BA). The two solutions are then mixed, heated and fully dissolved to form the gate dielectric solution. Step S2: Cleaning the substrate; Step S3: Device fabrication: Step S3-1: Fabrication of source / drain electrodes: Place the vacuum evaporation boat, source / drain mask, and substrate sequentially into the vapor deposition apparatus chamber from top to bottom. First, place the gold metal particles on the vacuum evaporation boat, then cover the substrate with the cleaned source / drain mask. Evaporate the vapor deposition apparatus chamber to a vacuum level of 10. -5 ~10 -4 Pa, followed by thermal evaporation to form source and drain electrodes on the substrate surface; Step S3-2: Preparation of polymer semiconductor layer: Spin-coat the semiconductor solution obtained in step S1-1 onto the sample surface obtained in step S3-1. After spin-coating, perform annealing treatment to form a polymer semiconductor layer on the source and drain electrode surfaces. Step S3-3: Preparation of solid electrolyte gate dielectric layer: The gate dielectric solution obtained in step S1-2 is spin-coated onto the sample surface obtained in step S3-2. After spin-coating, annealing is performed to form a solid electrolyte gate dielectric layer on the polymer semiconductor layer surface. Step S3-4: Gate electrode fabrication: First, place aluminum metal particles on a vacuum evaporation boat, then place the cleaned gate mask above the sample surface obtained in step S3-3, and evacuate the vapor deposition chamber to a vacuum level of 10. -5 ~10 -4 Pa, followed by thermal evaporation to form an aluminum gate electrode on the surface of the solid electrolyte gate dielectric layer; Step S4: Obtaining a transistor: Adjust and reduce the power at both ends of the vacuum evaporation boat, and after cooling to room temperature, fill it with inert gas. After the gas pressure in the vapor deposition chamber drops to equilibrium with the outside, take it out to obtain an N-type polymer transistor based on an electrolyte gate dielectric.
2. The preparation method according to claim 1, characterized in that, The specific steps of steps S1-2 are as follows: First, polyvinylidene fluoride-trifluoroethylene copolymer P(VDF-co-TrFE) and 1-ethylimidazolium bis(trifluoromethanesulfonyl)imide [EMIM][TFSI] are dissolved together in acetone in a certain proportion. The weight ratio of P(VDF-co-TrFE), [EMIM][TFSI] and acetone is 1:4:
7. The mixture is heated and stirred at 70°C under an inert gas environment to obtain a P(VDF-co-TrFE)-[EMIM][TFSI] gel solution. PMMA and n-butyl acrylate (N-BA) solution are mixed at a mass-volume ratio of 80 mg / mL to prepare an N-BA solution of PMMA. Then, the gel solution and the N-BA solution of PMMA are mixed evenly at a volume ratio of 2:
98.
3. The preparation method according to claim 1, characterized in that, In both steps S1-1 and S1-2, the temperature is heated to 75-85°C to ensure complete dissolution.
4. The preparation method according to claim 1, characterized in that, Step S2 is as follows: The substrate is placed in deionized water and alcohol in sequence, and surface impurities are removed by ultrasonic cleaning. Then, it is dried with inert gas and heated to evaporate the surface.
5. The preparation method according to claim 1, characterized in that, In step S3-1, the source / drain mask is made of stainless steel, and the substrate is a glass sheet. The specific steps for obtaining the source / drain electrodes by thermal evaporation in step S3-1 are as follows: the vacuum evaporation boat is heated, the power control knob is rotated to make the thermal evaporation current reach 110~120A, and a gold electrode with a thickness of 50-55 nm is prepared at a rate of 0.03-0.05nm / s. Then the power is slowly reduced, and after the evaporation chamber cools to room temperature, inert gas is filled in. The evaporation chamber is then opened and the obtained source / drain electrodes are taken out.
6. The preparation method according to claim 5, characterized in that, The specific steps for obtaining the gate electrode by thermal evaporation in step S3-4 are as follows: heating the vacuum evaporation boat, rotating and adjusting the power control knob to make the thermal evaporation current reach 100~120A, and preparing an aluminum gate electrode with a thickness of 80~100nm at a rate of 0.02~0.03nm / s.
7. The preparation method according to claim 1, characterized in that, The spin coating process described in steps S3-2 and S3-3 involves first pre-spin coating at 500-600 rpm for 3-5 seconds, and then spin coating at 2000-2100 rpm for 60-120 seconds; the annealing treatment described in step S3-2 is annealing at 200-250℃ for 1-1.5 hours, and the annealing treatment described in step S3-3 is annealing at 75-85℃ for 2-3 hours.
8. An N-type polymer transistor prepared by any one of the methods of claims 1-7, wherein the transistor has a top-gate bottom contact structure and comprises, from top to bottom, a gate electrode, a solid electrolyte gate dielectric layer, a polymer semiconductor layer, source and drain electrodes, and a substrate.
9. The application of the N-type polymer transistor of claim 8 in flexible electronics, sensors, low-power storage, or neuromorphic computing devices.